Application method of an application structure of a flared bolt
By combining flaring bolts and locking nuts in fasteners in aerospace fields, combined with heat treatment and flaring assembly design, the problems of mechanical properties and anti-loosening performance of fasteners in high temperature environments are solved, and the blades are realized Stable connection with the inner ring and reliability at high temperatures.
Patent Information
- Application Number
- CN202411148165.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-08-21
AI Technical Summary
In the aerospace field, it is difficult for fasteners to maintain good mechanical properties and anti-loosening properties in high temperature environments, especially in compact and narrow spaces, making it difficult to achieve effective connection between the blades and the inner ring.
Using the application structure of flared bolts, threaded connection between locking nuts and flared bolts, and rectangular grooves and through holes are designed on the flared bolts to achieve stable connection between the blade and the inner ring, combining solid solution heat treatment and stress-removing heat treatment To improve the thermal fatigue performance and plasticity of the bolt, and flar the bolt tail through the flaring assembly to ensure tightness.
It realizes good mechanical properties and anti-loosening performance of the flared bolt under high temperature environment, ensures stable connection and assembly quality between the blade and the inner ring, avoids deformity and cracking of the bolts during use, and ensures the stability of the fastening assembly. and reliability.
Smart Images

Figure CN118650392B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an application method of an application structure of a flared bolt, belonging to the technical field of aerospace fasteners. Background Art
[0002] In the field of aerospace fastener technology, fasteners used to connect important components in high-temperature environments need to maintain good mechanical properties and anti-loosening properties in high-temperature environments, and have the characteristics of installation, fixation, and easy maintenance. In the assembly process of the high-temperature end blades and inner rings of aircraft engines, fasteners are often used to connect the blades and the inner ring. However, since the space at the fastener installation location is very compact and narrow, fasteners with conventional structures cannot meet the use requirements. Therefore, how to achieve the assembly connection between the blades and the inner ring through fasteners in a compact and narrow space, and ensure that the fasteners have good mechanical properties and anti-loosening properties in a high-temperature environment, is a technical problem that needs to be solved urgently by technical personnel in this field. Summary of the invention
[0003] In order to solve the above technical problems, the present invention provides an application method of an application structure of a flared bolt.
[0004] The present invention is achieved through the following technical solutions:
[0005] An application method of an application structure of an expansion bolt, the application structure of the expansion bolt comprises an inner ring and a blade, the blade portion extends into the inner ring and is connected to the inner ring through a fastening assembly, the fastening assembly comprises a locking nut and an expansion bolt, the locking nut is threadedly connected to the expansion bolt, and an end of the expansion bolt away from the bolt head is expanded to prevent the locking nut from loosening;
[0006] The bottom of the inner ring is provided with a rectangular groove A in the longitudinal direction, and the top of the inner ring is provided with a rectangular groove B in the longitudinal direction on one side of the rectangular groove A, a through hole A is provided on the side wall of the inner ring between the rectangular groove A and the rectangular groove B, a through hole B is provided on the side wall of the rectangular groove B away from the rectangular groove A, the through hole B is coaxially arranged with the through hole A, and the diameter of the through hole B is greater than the diameter of the through hole A, a through hole C is provided on the blade at a position corresponding to the through hole A, and the diameters of the through hole C and the through hole A are adapted to the diameter of the matching section on the expansion bolt;
[0007] The application method of the expansion bolt application structure comprises the following steps:
[0008] Step A, insert the blade part into the rectangular groove B on the inner ring, align the through hole C on the blade with the through hole A on the inner ring, and then pass the flaring section of the flaring bolt through the through hole A and through hole C in sequence;
[0009] Step B, install and fix the fixture to the inner ring, and make the fixture cover the bolt head of the expansion bolt;
[0010] Step C, threading the locking nut to the flared bolt, and tightening the locking nut to a specified torque value using a torque wrench;
[0011] Step D, installing the flaring assembly on the fixture, and flaring the tail of the flaring bolt through the flaring assembly;
[0012] Step E, remove the flaring assembly and the fixture in turn, check the flaring cone surface and its edge, if there is no crack, it is qualified, that is, the assembly of the blade and the inner ring is completed;
[0013] The clamp comprises a clamp block, a rectangular groove C is longitudinally provided on the top of the clamp block, a square groove is provided on one side wall of the rectangular groove C, a coaxially arranged sliding hole and a threaded hole A are provided on the other side wall at a position corresponding to the square groove, one end of the threaded hole A is connected to one end of the sliding hole, and the sliding hole is located between the threaded hole A and the rectangular groove C, and fixing bolts are threadedly connected on both sides of the threaded hole A on the clamp block, and the fixing bolts are located on the opposite side of the square groove;
[0014] The left side wall of the square groove is a plane, and the width of the square groove is adapted to the distance between the two planes of the bolt head, the length is greater than the diameter of the bolt head, and the depth is adapted to the axial length of the bolt head;
[0015] The process of fixing the fixture to the inner ring in step B is as follows: first, partially extend the fixture block into the rectangular groove A at the bottom of the inner ring, and make the square groove on the fixture block cover the bolt head, then make the side wall with the square groove on the rectangular groove C keep in contact with the side wall between the rectangular groove A and the rectangular groove B on the inner ring, and make the bottom surface of the rectangular groove C keep in contact with the side wall on the lower side of the rectangular groove B on the inner ring, and then simultaneously tighten all the fixing bolts on the fixture block to tighten against the inner ring, so that the fixture can be fixed to the inner ring;
[0016] The processing method of the flared bolt comprises the following steps:
[0017] Step 1: Material preparation: Select solid solution strengthened nickel-based oxidation-resistant alloy GH3044 bar as the blank for making flared bolts;
[0018] Step 2: Heat treatment A: subjecting the blank to solution heat treatment;
[0019] Step 3: Turning: Turn the outer circle of the bolt head, matching section, fastening section and flaring section on the blank to the designed size, then drill the flaring hole, turn the external thread of the fastening section, and chamfer and polish the blank. Next, turn the blank over and turn the spherical surface of the bolt head;
[0020] Step 4: Milling: Mill two planes on the outer surface of the bolt head to obtain a semi-finished product;
[0021] Step 5, heat treatment B: perform stress relief heat treatment on the semi-finished product to obtain the finished expanded bolt;
[0022] Step 6: Packaging and warehousing: After wrapping the flared bolts with electrolytic paper, place them in vacuum packaging bags for vacuum packaging;
[0023] The process of performing solution heat treatment on the blank in step 2 is as follows: placing the blank in a vacuum oil quenching heat treatment furnace with an entry temperature lower than 500°C, slowly heating the blank to 850°C-860°C, preheating for 30min-40min, and controlling the vacuum degree in the vacuum oil quenching heat treatment furnace to be below 20Pa; then heating the blank to 1130°C±10°C, keeping the temperature for 120min-180min, and controlling the vacuum degree in the vacuum oil quenching heat treatment furnace to be below 13.3Pa, and then cooling the blank with vacuum oil in the vacuum oil quenching heat treatment furnace, while passing argon gas into the vacuum oil quenching heat treatment furnace to cool the blank, and raising the pressure in the furnace to (6-8)×10 4 Pa;
[0024] The process of stress relief heat treatment of the semi-finished product in step 5 is as follows: the semi-finished product is placed in a vacuum tempering heat treatment furnace with the furnace temperature lower than 300°C, the semi-finished product is heated to 860°C±10°C, and argon is introduced into the furnace at the same time, and the argon pressure in the furnace is controlled at (7.5~9)×10 4 Pa, keep warm for 180 min, and then increase the argon pressure in the furnace to (1~1.4)×10 5 Pa, the semi-finished product is slowly cooled to room temperature by air cooling in the furnace; the hardness value HB of the finished product of the expanded bolt 1 is less than 285, and the tensile strength σ b Reaching a strength grade of 685MPa.
[0025] After step 3 is completed, the verticality between the end surface of the bolt head close to the mating section and the center axis of the expanded bolt is no more than 0.05 mm;
[0026] The symmetry between the two planes in step 4 is no greater than 0.01 mm.
[0027] The flaring assembly includes a flaring core rod and a pushing bolt. A conical head is provided at one end of the flaring core rod, and the cone angle of the conical head is 90°. A threaded hole B is coaxially provided at the other end. One end face of the pushing bolt abuts against the end face of the flaring core rod with the threaded hole B.
[0028] The method for expanding the tail of the expanded bolt in step D comprises the following steps:
[0029] Step 1, determining the torque required for expanding the expansion bolt through an experiment, and setting the torque as the test torque value;
[0030] Step 1: Pass one end of the flaring mandrel with a conical head through the sliding hole on the clamp block and the through hole B on the inner ring in sequence, and partially push it into the flaring hole at the tail of the flaring bolt, then thread the push bolt with the threaded hole A on the clamp block, and rotate the push bolt until it contacts the flaring mandrel;
[0031] Step 1: Use a torque wrench to rotate the push bolt, push the flaring mandrel to move along its axial direction to flare the tail of the flaring bolt. When the torque wrench tightens the push bolt, the actual torque value of the push bolt is 5N∙m greater than the test torque value.
[0032] The beneficial effects of the present invention are:
[0033] 1. Improve the thermal fatigue performance of the expanded bolts through solution heat treatment, and then ensure the tensile strength of the expanded bolts σ b On the premise of reaching the strength grade of 685MPa, the plasticity of the flared bolt is improved through stress relief heat treatment, so that the hardness value HB of the flared bolt is less than 285, and the residual stress of the flared bolt in the machining process is eliminated to avoid deformity of the flared bolt during use or cracking during flaring, ensuring that the flared bolt has good mechanical properties and anti-loosening performance in a high temperature environment.
[0034] 2. The verticality between the end face of the bolt head close to the fitting section and the center axis of the flared bolt is limited to no more than 0.05 mm, ensuring that the end face of the bolt head close to the fitting section can be well contacted with the inner ring, and that the fitting section on the flared bolt can be well matched with the through hole A on the inner ring and the through hole C on the blade, which helps to ensure the assembly quality of the flared bolt and the locking nut to the blade and the inner ring.
[0035] 3. Since the bolt head is provided with a spherical surface, the left side wall of the square groove is a plane, and the length of the square groove is greater than the diameter of the bolt head, the square groove makes way for the bolt head, and the bolt head can be properly deflected in the Y direction, ensuring that during the process of connecting and tightening the flared bolt with the locking nut, the flared bolt is not affected by other additional external forces, thereby improving the assembly quality of the blade, inner ring and fastening components.
[0036] 4. Since the locking nut has a self-locking function, the locking nut is restricted by expanding the tail of the expanding bolt. The two anti-loosening methods ensure that the fastening assembly is always in a fastened state in a high temperature environment, ensuring the stability and reliability of the blade and the inner ring after assembly. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 It is a structural schematic diagram of the expansion bolt of the present invention;
[0038] Figure 2 for Figure 1 Left view of
[0039] Figure 3 It is a partial schematic diagram of the assembly of the blade, inner ring, fastening assembly, fixture and flaring assembly of the present invention;
[0040] Figure 4 for Figure 3 Section view along AA;
[0041] Figure 5 for Figure 3 Sectional view along BB;
[0042] Figure 6 It is a schematic diagram of the main structure of the card block of the present invention;
[0043] Figure 7 for Figure 6 Sectional view along CC;
[0044] Figure 8 It is a structural schematic diagram of the expanding mandrel of the present invention;
[0045] Fig. 9 It is a structural schematic diagram of the push bolt of the present invention;
[0046] Fig.10 It is a schematic diagram of the assembly structure of the blades, inner ring and fastening components of the present invention.
[0047] In the figure: 1-flared bolt, 11-bolt head, 111-spherical surface, 112-plane, 12-matching section, 13-fastening section, 14-flared section, 15-flared hole, 2-blade, 3-inner ring, 31-rectangular groove A, 32-rectangular groove B, 4-locking nut, 5-block, 51-rectangular groove C, 52-square groove, 53-sliding hole, 54-threaded hole A, 6-tightening bolt, 7-flared mandrel, 71-threaded hole B, 8-pushing bolt. DETAILED DESCRIPTION
[0048] The technical solution of the present invention is further described below, but the scope of protection claimed is not limited to the description.
[0049] like Figures 1 to 10 As shown, an application method of an application structure of a flared bolt described in the present invention, the application structure of the flared bolt includes an inner ring 3 and a blade 2, the blade 2 partially extends into the inner ring 3, and is connected to the inner ring 3 through a fastening assembly, the fastening assembly includes a locking nut 4 and a flared bolt 1, the locking nut 4 is threadedly connected to the flared bolt 1, and the end of the flared bolt 1 away from the bolt head 11 is flared to prevent the locking nut 4 from loosening.
[0050] A rectangular groove A31 is longitudinally provided at the bottom of the inner ring 3, and a rectangular groove B32 is longitudinally provided at the top of the inner ring 3 on one side of the rectangular groove A31, a through hole A is provided on the side wall of the inner ring 3 between the rectangular groove A31 and the rectangular groove B32, a through hole B is provided on the side wall of the rectangular groove B32 away from the rectangular groove A31, the through hole B is coaxially arranged with the through hole A, and the diameter of the through hole B is larger than the diameter of the through hole A, a through hole C is provided on the blade 2 at a position corresponding to the through hole A, and the diameters of the through hole C and the through hole A are adapted to the diameter of the mating section 12 on the expansion bolt 1.
[0051] The application method of the expansion bolt application structure comprises the following steps:
[0052] Step A, partially insert the blade 2 into the rectangular groove B32 on the inner ring 3, and align the through hole C on the blade 2 with the through hole A on the inner ring 3, and then pass the flaring section 14 of the flaring bolt 1 through the through hole A and the through hole C in sequence;
[0053] Step B, installing and fixing the fixture on the inner ring 3, and making the fixture cover the bolt head 11 of the flared bolt 1;
[0054] Step C, threading the locking nut 4 to the flared bolt 1, and tightening the locking nut 4 to a specified torque value using a torque wrench;
[0055] Step D, installing the flaring assembly on the fixture, and flaring the tail of the flaring bolt 1 through the flaring assembly;
[0056] Step E: Remove the flaring assembly and the fixture in turn, check the flaring cone surface and its edge, and if there is no crack, it is qualified, that is, the assembly of the blade 2 and the inner ring 3 is completed.
[0057] The clamp includes a clamp block 5, a rectangular groove C51 is longitudinally provided on the top of the clamp block 5, a square groove 52 is provided on one side wall of the rectangular groove C51, a coaxially arranged sliding hole 53 and a threaded hole A54 are provided on the other side wall at a position corresponding to the square groove 52, one end of the threaded hole A54 is connected to one end of the sliding hole 53, and the sliding hole 53 is located between the threaded hole A54 and the rectangular groove C51, and fixing bolts 6 are threadedly connected on both sides of the threaded hole A54 on the clamp block 5, and the fixing bolts 6 are located on the opposite side of the square groove 52;
[0058] The left side wall of the square groove 52 is a plane, and the width of the square groove 52 matches the distance between the two planes 112 of the bolt head 11 , the length is greater than the diameter of the bolt head 11 , and the depth matches the axial length of the bolt head 11 .
[0059] The process of installing and fixing the fixture to the inner ring 3 in step B is as follows: first, partially extend the block 5 into the rectangular groove A31 at the bottom of the inner ring 3, and make the square groove 52 on the block 5 cover the bolt head 11, and then make the side wall of the rectangular groove C51 with the square groove 52 keep in contact with the side wall between the rectangular groove A31 and the rectangular groove B32 on the inner ring 3, and make the bottom surface of the rectangular groove C51 keep in contact with the side wall on the lower side of the rectangular groove B32 on the inner ring 3, and then simultaneously tighten all the fixing bolts 6 on the block 5 to tighten them on the inner ring 3, so that the fixture can be installed and fixed to the inner ring 3.
[0060] The processing method of the flared bolt comprises the following steps:
[0061] Step 1, material preparation: select solid solution strengthened nickel-based oxidation-resistant alloy GH3044 bar as the blank for making the flared bolt 1;
[0062] Step 2: Heat treatment A: subjecting the blank to solution heat treatment;
[0063] Step 3: Turning: Turn the outer circles of the bolt head 11, the fitting section 12, the fastening section 13 and the flaring section 14 on the blank to the designed size, then drill the flaring hole 15, turn the outer thread of the fastening section 13, and chamfer and polish the blank. Next, turn the blank around and turn the spherical surface 111 of the bolt head 11;
[0064] Step 4: Milling: Mill two planes 112 on the outer circumferential surface of the bolt head 11 to obtain a semi-finished product;
[0065] Step 5, heat treatment B: performing stress relief heat treatment on the semi-finished product to obtain a finished product of the expanded bolt 1;
[0066] Step 6, packaging and storage: After wrapping the finished expanded bolt 1 with electrolytic paper, place it in a vacuum packaging bag for vacuum packaging. When in use, the expanded bolt 1 includes a bolt head 11, a matching section 12, a fastening section 13 and an expanded section 14, one end of the matching section 12 is connected to one end of the bolt head 11, and the other end is connected to one end of the fastening section 13, one end of the expanded section 14 is connected to the end of the fastening section 13 away from the matching section 12, the end face of the bolt head 11 away from the matching section 12 is a spherical surface 111, and two planes 112 are evenly and symmetrically arranged on the outer circumferential surface of the bolt head 11, and the end of the expanded bolt 1 away from the bolt head 11 is coaxially provided with an expanded hole 15. The diameter of the bolt head 11>the diameter of the matching section 12=the diameter of the fastening section 13>the diameter of the expanded section 14. Select the solid solution strengthened nickel-based anti-oxidation alloy GH3044 bar to make the expanded bolt 1, ensure that the bar has good processing performance, and ensure that the expanded bolt 1 has good mechanical properties under high temperature environment. After step 4, the semi-finished product is first deburred, cleaned and inspected, and then the semi-finished product is heat treated B in step 5. After step 5, the finished product of the expanded bolt 1 is first cleaned, and after cleaning, the surface of the expanded bolt 1 is allowed to be blackened, and then the expanded bolt 1 is generally inspected, and then the expanded bolt 1 is vacuum packaged in step 6.
[0067] The process of performing solution heat treatment on the blank in step 2 is as follows: placing the blank in a vacuum oil quenching heat treatment furnace with an entry temperature lower than 500°C, slowly heating the blank to 850°C-860°C, preheating for 30min-40min, and controlling the vacuum degree in the vacuum oil quenching heat treatment furnace to be below 20Pa; then heating the blank to 1130°C±10°C, keeping the temperature for 120min-180min, and controlling the vacuum degree in the vacuum oil quenching heat treatment furnace to be below 13.3Pa, and then cooling the blank with vacuum oil in the vacuum oil quenching heat treatment furnace, while passing argon gas into the vacuum oil quenching heat treatment furnace to cool the blank, and raising the pressure in the furnace to (6-8)×10 4 Pa. Improve the thermal fatigue performance of the blank through solution heat treatment. When in use, the blanks of the same material and the same furnace batch number are heat treated in the same furnace.
[0068] The process of stress relief heat treatment of the semi-finished product in step 5 is as follows: the semi-finished product is placed in a vacuum tempering heat treatment furnace with the furnace temperature lower than 300°C, the semi-finished product is heated to 860°C±10°C, and argon is introduced into the furnace at the same time, and the argon pressure in the furnace is controlled at (7.5~9)×10 4 Pa, keep warm for 180 min, and then increase the argon pressure in the furnace to (1~1.4)×10 5 Pa, the semi-finished product is slowly cooled to room temperature by air cooling in the furnace; the hardness value HB of the finished product of the expanded bolt 1 is less than 285, and the tensile strength σ bReaching the strength grade of 685MPa. b On the premise of reaching the strength grade of 685MPa, the plasticity of the flared bolt 1 is improved through stress relief heat treatment, so that the hardness value HB of the flared bolt 1 is less than 285, and the residual stress of the flared bolt 1 in the machining process is eliminated to avoid deformity of the flared bolt 1 during use or cracking during flaring, thereby ensuring that the flared bolt 1 has good mechanical properties and anti-loosening performance in a high temperature environment.
[0069] After the step 3 is completed, the perpendicularity between the end surface of the bolt head 11 close to the fitting section 12 and the central axis of the expanded bolt 1 is no more than 0.05 mm;
[0070] The symmetry of the two planes 112 in step 4 is no greater than 0.01 mm.
[0071] The flaring assembly includes a flaring core rod 7 and a pushing bolt 8. A conical head is provided at one end of the flaring core rod 7, and the cone angle of the conical head is 90°. A threaded hole B71 is coaxially provided at the other end. One end face of the pushing bolt 8 abuts against the end face of the flaring core rod 7 provided with the threaded hole B71.
[0072] The method for expanding the tail of the expanded bolt 1 in step D comprises the following steps:
[0073] Step 1, determining the torque required for expanding the expansion bolt 1 through an experiment, and setting the torque as the test torque value;
[0074] Step 2, pass one end of the flaring mandrel 7 with a conical head through the sliding hole 53 on the clamping block 5 and the through hole B on the inner ring 3 in sequence, and partially push it into the flaring hole 15 at the tail of the flaring bolt 1, then thread the push bolt 8 with the threaded hole A54 on the clamping block 5, and rotate the push bolt 8 until it contacts the flaring mandrel 7;
[0075] Step 3: Use a torque wrench to rotate the push bolt 8, push the flaring mandrel 7 to move along its axial direction to flare the tail of the flaring bolt 1. When the torque wrench tightens the push bolt 8, the actual torque value of the push bolt 8 is 5N∙m greater than the test torque value.
[0076] Since the installation space is very compact and narrow, a flared bolt 1 is designed, which is very different from the shape and function of ordinary fastening bolts. Figure 4As shown, during assembly, due to the compact and narrow space at the installation position of the flared bolt 1, the contact surface between the bolt head 11 and the inner ring 3 cannot be observed. For this reason, the present invention limits the perpendicularity between the end face of the bolt head 11 close to the mating section 12 and the center axis of the flared bolt 1 to no more than 0.05 mm, ensuring that the end face of the bolt head 11 close to the mating section 12 can be well in contact with the inner ring 3, and ensuring that the mating section 12 on the flared bolt 1 can be well matched with the through hole A on the inner ring 3 and the through hole C on the blade 2, which helps to ensure the assembly quality of the flared bolt 1 and the locking nut 4 to the blade 2 and the inner ring 3.
[0077] In addition, in order to prevent the bolt head 11 from being constrained by other additional loads during assembly, the end face of the bolt head 11 away from the mating section 12 is designed as a spherical surface 111, and two planes 112 are evenly and symmetrically milled on the outer circumferential surface of the bolt head 11; during assembly, the bolt head 11 falls into the square groove 52 on the block 5, and the spherical surface 111 is in point contact with the left side wall of the square groove 52. Since the bolt head 11 is provided with a spherical surface 111, the left side wall of the square groove 52 is a plane, and the length of the square groove 52 is greater than the diameter of the bolt head 11, the square groove 52 makes way for the bolt head 11, and the bolt head 11 can be appropriately deflected in the Y direction (i.e., the radial direction parallel to the plane 112), ensuring that the flared bolt 1 is not affected by other additional external forces during the process of connecting and tightening the flared bolt 1 and the locking nut 4, thereby improving the assembly quality of the blade 2, the inner ring 3 and the fastening assembly. Assuming that the square groove 52 completely restricts the bolt head 11, during the process of tightening the locking nut 4, the bolt head 11 will be affected by other additional external forces and cause the flared bolt 1 to deform. When the external force is removed, the flared bolt 1 recovers its deformation, which will cause its preload force to change, that is, the locking nut 4 is not tightened, thereby failing to ensure the assembly quality of the blade 2, inner ring 3 and fastening assembly.
[0078] When the locking nut 4 is threadedly connected to the flaring bolt 1 and the locking nut 4 is tightened to the specified torque value using a torque wrench, the locking nut 4 cannot be loosened, and then the tail of the flaring bolt 1 is flared 90° through the flaring core rod 7 and the push bolt 8 to limit the locking nut 4 in the axial direction. Since the locking nut 4 has a self-locking function, the locking nut 4 is limited by flaring the tail of the flaring bolt 1. The two anti-loosening methods ensure that the fastening assembly is always in a fastened state in a high temperature environment, thereby ensuring the stability and reliability of the blade 2 and the inner ring 3 after assembly.
Claims
1. An application method of an application structure of a flared bolt, characterized in that: The application structure of the flared bolt comprises an inner ring (3) and a blade (2), wherein the blade (2) partially extends into the inner ring (3) and is connected to the inner ring (3) via a fastening assembly, wherein the fastening assembly comprises a locking nut (4) and a flared bolt (1), wherein the locking nut (4) is threadedly connected to the flared bolt (1), and an end of the flared bolt (1) away from the bolt head (11) is flared to prevent the locking nut (4) from loosening; The bottom of the inner ring (3) is provided with a rectangular groove A (31) in the longitudinal direction, and the top of the inner ring (3) is provided with a rectangular groove B (32) in the longitudinal direction on one side of the rectangular groove A (31); a through hole A is provided on the side wall of the inner ring (3) between the rectangular groove A (31) and the rectangular groove B (32); a through hole B is provided on the side wall of the rectangular groove B (32) away from the rectangular groove A (31); the through hole B is coaxially arranged with the through hole A, and the diameter of the through hole B is larger than the diameter of the through hole A; a through hole C is provided on the blade (2) at a position corresponding to the through hole A, and the diameters of the through hole C and the through hole A are adapted to the diameter of the matching section (12) on the expansion bolt (1); The application method of the expansion bolt application structure comprises the following steps: Step A, partially inserting the blade (2) into the rectangular groove B (32) on the inner ring (3), aligning the through hole C on the blade (2) with the through hole A on the inner ring (3), and then passing the flared section (14) of the flared bolt (1) through the through hole A and the through hole C in sequence; Step B, installing and fixing the fixture on the inner ring (3), and making the fixture cover the bolt head (11) of the expansion bolt (1); Step C, threading the locking nut (4) to the flared bolt (1), and tightening the locking nut (4) to a specified torque value using a torque wrench; Step D, installing the flaring assembly on the fixture, and flaring the tail of the flaring bolt (1) through the flaring assembly; Step E, dismantling the flaring assembly and the fixture in turn, inspecting the flaring cone surface and its edge, and if there are no cracks, it is qualified, that is, the assembly of the blade (2) and the inner ring (3) is completed; The clamp comprises a clamping block (5), a rectangular groove C (51) is longitudinally provided on the top of the clamping block (5), a square groove (52) is provided on one side wall of the rectangular groove C (51), a coaxially arranged sliding hole (53) and a threaded hole A (54) are provided on the other side wall at a position corresponding to the square groove (52), one end of the threaded hole A (54) is connected to one end of the sliding hole (53), and the sliding hole (53) is located between the threaded hole A (54) and the rectangular groove C (51), and fixing bolts (6) are threadedly connected on both sides of the threaded hole A (54) on the clamping block (5), and the fixing bolts (6) are located on the opposite side of the square groove (52); The left side wall of the square groove (52) is a plane, and the width of the square groove (52) is adapted to the distance between the two planes (112) of the bolt head (11), the length is greater than the diameter of the bolt head (11), and the depth is adapted to the axial length of the bolt head (11); The process of fixing the fixture to the inner ring (3) in step B is as follows: first, partially extend the fixture block (5) into the rectangular groove A (31) at the bottom of the inner ring (3), and make the square groove (52) on the fixture block (5) cover the bolt head (11), then make the side wall of the rectangular groove C (51) with the square groove (52) keep in contact with the side wall between the rectangular groove A (31) and the rectangular groove B (32) on the inner ring (3), and make the bottom surface of the rectangular groove C (51) keep in contact with the side wall on the lower side of the rectangular groove B (32) on the inner ring (3), and then simultaneously tighten all the fixing bolts (6) on the fixture block (5) to press against the inner ring (3), so that the fixture can be fixed to the inner ring (3); The processing method of the flared bolt comprises the following steps: Step 1: material preparation: select solid solution strengthened nickel-based oxidation-resistant alloy GH3044 bar as the blank for making the flared bolt (1); Step 2: Heat treatment A: subjecting the blank to solution heat treatment; Step 3: Turning: Turn the outer diameters of the bolt head (11), the fitting section (12), the fastening section (13) and the flaring section (14) on the blank to the designed size, then drill the flaring hole (15), turn the outer thread of the fastening section (13), and chamfer and polish the blank. Next, turn the blank around and turn the spherical surface (111) of the bolt head (11); Step 4: Milling: Mill two planes (112) on the outer circumferential surface of the bolt head (11) to obtain a semi-finished product; Step 5, heat treatment B: performing stress relief heat treatment on the semi-finished product to obtain a finished expanded bolt (1); Step 6: Packaging and warehousing: After the flared bolt (1) is wrapped with electrolytic paper, it is placed in a vacuum packaging bag for vacuum packaging; The process of performing solution heat treatment on the blank in step 2 is as follows: placing the blank in a vacuum oil quenching heat treatment furnace with an entry temperature lower than 500°C, slowly heating the blank to 850°C-860°C, preheating for 30min-40min, and controlling the vacuum degree in the vacuum oil quenching heat treatment furnace to be below 20Pa; then heating the blank to 1130°C±10°C, keeping the temperature for 120min-180min, and controlling the vacuum degree in the vacuum oil quenching heat treatment furnace to be below 13.3Pa, and then cooling the blank with vacuum oil in the vacuum oil quenching heat treatment furnace, while passing argon gas into the vacuum oil quenching heat treatment furnace to cool the blank, and raising the pressure in the furnace to (6-8)×10 4 Pa; The process of stress relief heat treatment of the semi-finished product in step 5 is as follows: the semi-finished product is placed in a vacuum tempering heat treatment furnace with the furnace temperature lower than 300°C, the semi-finished product is heated to 860°C±10°C, and argon is introduced into the furnace at the same time, and the argon pressure in the furnace is controlled at (7.5~9)×10 4 Pa, keep warm for 180 min, and then increase the argon pressure in the furnace to (1~1.4)×10 5 Pa, the semi-finished product is slowly cooled to room temperature by air cooling in the furnace; the hardness value of the expanded bolt (1) is less than 285, and the tensile strength σ b Reaching a strength grade of 685MPa.
2. The method for applying the expansion bolt application structure according to claim 1, characterized in that: After step 3 is completed, the perpendicularity between the end surface of the bolt head (11) close to the fitting section (12) and the center axis of the expanded bolt (1) is no more than 0.05 mm; The symmetry of the two planes (112) in step 4 is no greater than 0.01 mm.
3. The method for applying the expansion bolt application structure according to claim 1, characterized in that: The flaring assembly comprises a flaring core rod (7) and a pushing bolt (8); one end of the flaring core rod (7) is provided with a conical head, and the conical angle of the conical head is 90 degrees; the other end is coaxially provided with a threaded hole B (71); one end face of the pushing bolt (8) abuts against one end face of the flaring core rod (7) provided with the threaded hole B (71).
4. The method for applying the expansion bolt application structure according to claim 1, characterized in that: The method for expanding the tail of the expanded bolt (1) in step D comprises the following steps: Step 1, determining the torque required for expanding the expansion bolt (1) through an experiment, and setting the torque as the test torque value; Step 2: Pass one end of the flaring mandrel (7) with the conical head through the sliding hole (53) on the clamping block (5) and the through hole B on the inner ring (3) in sequence, and partially push it into the flaring hole (15) at the tail of the flaring bolt (1), then thread the push bolt (8) into the threaded hole A (54) on the clamping block (5), and rotate the push bolt (8) until it contacts the flaring mandrel (7); Step 3: Use a torque wrench to rotate the push bolt (8), push the flaring mandrel (7) to move along its axial direction to flare the tail of the flaring bolt (1). When the torque wrench tightens the push bolt (8), the actual torque value of the push bolt (8) is 5 N∙m greater than the test torque value.