A method for preparing a trench MOSFET

By using two-layer photomasks and sidewall residual technology in the preparation of trench MOSFETs, the process flow is simplified, the problem of high production costs caused by multiple photomask layers is solved, and smaller device resistance and higher device resistance are achieved. production efficiency.

CN118658788BActive Publication Date: 2024-10-22NANJING RONGXIN MICROELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411147659.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-10-22
Estimated Expiration
2044-08-21

AI Technical Summary

Technical Problem

In the existing trench MOSFET preparation process, the large number of mask layers results in high production costs, and it is still difficult to effectively reduce costs by omitting the mask layer AA.

Method used

The preparation of trench MOSFET can be completed by using two layers of photomasks. Polysilicon is left on the sidewall of the silicon nitride layer and etched to form a smaller trench structure. This simplifies the process without affecting the static characteristics of the device.

Benefits of technology

It greatly reduces the production cost of MOSFET devices, shortens production time, improves work efficiency, and achieves smaller device resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118658788B_ABST
    Figure CN118658788B_ABST
Patent Text Reader

Abstract

The present invention belongs to the field of semiconductor technology, and discloses a method for preparing a trench MOSFET, and the specific preparation steps are as follows: S1 forms polysilicon on the surface of an epitaxial layer and a silicon nitride layer; S2 leaves sidewall polysilicon on both side walls of the silicon nitride layer, etches a trench I on the epitaxial layer, and generates a gate oxide layer; S3 fills the trench I with gate polysilicon; S4 removes the sidewall polysilicon and the gate polysilicon, and deposits a shielding oxide layer; S5 forms a P-type well region I and an N-type well region; S6 deposits a dielectric layer; S7 ions are implanted into the P-type well region II in the trench II; S8 deposits metal to form an electrode. Under the premise of ensuring that the static characteristics of the device are not affected, the present invention only needs to use a two-layer mask to realize the production of the trench MOSFET, which not only greatly reduces the production cost of the MOSFET device, but also further reduces the production time of the MOSFET device, and greatly improves the work efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of semiconductor technology, and in particular relates to a method for preparing a trench MOSFET. Background Art

[0002] The structure of power metal oxide semiconductor field effect transistor (Power MOSFET) can be divided into trench structure and planar structure. The trench structure can obtain better resistance because of the smaller cell pitch. In the conventional preparation process of trench MOSFET, the number of mask layers required is five, excluding the passivation layer, namely Trench, AA, Source, Contact, and Metal. The production cost of MOSFET mainly depends on the number of mask layers. At present, the most commonly used method on the market is to reduce production costs by omitting the mask layer AA, that is, using four layers of mask to complete the trench MOSFET device, but even so, the production cost savings are still limited. Summary of the invention

[0003] In order to further reduce the production cost of MOSFET devices, the present invention provides a method for preparing trench MOSFET. Under the premise of ensuring that the static characteristics of the MOSFET device are not affected, the trench MOSFET can be produced by only using two layers of masks, which not only greatly reduces the production cost of the MOSFET device, but also further shortens the production time of the MOSFET device, greatly improving work efficiency.

[0004] The main technical solutions adopted in the present invention are:

[0005] A method for preparing a trench MOSFET, the specific preparation steps are as follows:

[0006] S1: depositing a layer of silicon nitride on the epitaxial layer, etching a part of the silicon nitride region based on the first mask layer using a photolithography process to form a plurality of silicon nitride layers distributed at intervals, and depositing polysilicon on the surface of the epitaxial layer and the silicon nitride layer;

[0007] S2: using a dry etching process to remove the polysilicon on the surface, the process will leave polysilicon on both sides of the silicon nitride layer, which is recorded as sidewall polysilicon, and then using a dry etching process to etch a trench I on the epitaxial layer between the adjacent sidewall polysilicon, and generate a gate oxide layer on the surface of the trench I;

[0008] S3: Filling the gate polysilicon into the trench I so that it covers the entire upper surface of the device, and flattening the surface of the gate polysilicon;

[0009] S4: using a wet etching process to simultaneously remove the sidewall polysilicon and the gate polysilicon, and etching the gate polysilicon to below the surface of the epitaxial layer to ensure that no polysilicon remains on the surface of the epitaxial layer, and then depositing a shielding oxide layer on the surface of the gate polysilicon, the silicon nitride layer and the epitaxial layer;

[0010] S5: using an ion implantation process to form a P-type well region I and an N-type well region in the epitaxial layer on both sides of the trench I;

[0011] S6: depositing a dielectric layer on the entire device surface, and planarizing the surface of the dielectric layer so that the surface of the dielectric layer is flush with or lower than the surface of the shielding oxide layer on the silicon nitride layer;

[0012] S7: using a dry etching process to sequentially remove the shielding oxide layer, the silicon nitride layer, and a portion of the epitaxial layer corresponding to the vertical projection surface of the silicon nitride layer on the surface of the silicon nitride layer to form a trench II, and performing ion implantation in the trench II to form a P-type well region II, wherein both sides of the P-type well region II are connected to the P-type well region I and the N-type well region at the same time;

[0013] S8: Deposit metal on the surface of the dielectric layer and in the groove II to form electrodes, and use a photolithography process to separate the surface electrodes based on the second mask layer to obtain the gate and the source, thus completing the production of the trench MOSFET.

[0014] Preferably, in S5, P-type doping ions are implanted into the epitaxial layer on both sides of the trench I at an angle of 7°-9°, and a P-type well region I is formed after high-temperature activation at 1000°C-1100°C.

[0015] Preferably, the P-type doping ions are boron ions.

[0016] Preferably, in S5, N-type doping ions are implanted into the epitaxial layer on both sides of the trench I at an angle of 0°, and annealing is performed at 900° C.-950° C. to form an N-type well region.

[0017] Preferably, the N-type doping ions are arsenic ions or phosphorus ions.

[0018] Preferably, in S3, a CMP process is used to planarize the surface of the gate polysilicon.

[0019] Preferably, in S6, a CMP process is used to planarize the surface of the dielectric layer.

[0020] Preferably, in S7, an ion implantation process is used to implant boron difluoride ions or boron ions at an angle of 0° into the bottom of the trench II to form a P-type well region II.

[0021] Beneficial effects: The present invention provides a method for preparing a trench MOSFET, which has the following advantages:

[0022] (1) In the present invention, during the entire preparation process of the trench MOSFET, without affecting the static characteristics of the device and ensuring that the size of the unit cell and the area of ​​the device are not increased, only two layers of mask layers are used to complete the production of the trench MOSFET, thereby reducing the number of mask layers used, greatly reducing the production cost, simplifying the production process, and being conducive to improving the production efficiency of the wafer.

[0023] (2) The present invention adopts the sidewall residual technology, which provides the possibility of realizing a smaller trench structure by leaving polysilicon on the sidewall of the silicon nitride layer, and is conducive to obtaining a smaller device resistance value. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 This is a schematic diagram of the structure of step S1 in Example 1;

[0025] Figure 2 This is a schematic diagram of the structure of step S2 in Example 1;

[0026] Figure 3 This is a schematic diagram of the structure of step S3 in Example 1;

[0027] Figure 4 This is a schematic diagram of the structure of step S4 in Example 1;

[0028] Figure 5 This is a schematic diagram of the structure of step S5 in Example 1;

[0029] Figure 6 This is a schematic diagram of the structure of step S6 in Example 1;

[0030] Figure 7 This is a schematic diagram of the structure of step S7 in Example 1;

[0031] Figure 8 This is a schematic diagram of the structure of step S8 in Example 1;

[0032] In the figure: epitaxial layer 100, silicon nitride layer 101, polysilicon 102a, sidewall polysilicon 102b, gate polysilicon 102c, gate oxide layer 103a, shielding oxide layer 103b, P-type well region I 104, N-type well region 105, dielectric layer 106, P-type well region II 107, metal 108, trench I 109a, trench II 109b. DETAILED DESCRIPTION

[0033] In order to enable those skilled in the art to better understand the technical solutions in this application, the technical solutions in the embodiments of this application are clearly and completely described below. Obviously, the described embodiments are only part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of this application.

[0034] Embodiment 1, a method for preparing a trench MOSFET, the specific preparation steps are as follows:

[0035] S1: Figure 1 As shown, a layer of silicon nitride is deposited on the epitaxial layer 100, and a part of the silicon nitride region is etched using a photolithography process based on the first mask layer to form a plurality of silicon nitride layers 101 distributed at intervals, and polysilicon 102a is deposited on the surface of the epitaxial layer 100 and the silicon nitride layer 101. In this embodiment 1, the specific distribution interval of the silicon nitride layer 101 and the specific thickness of the polysilicon 102a can be selectively designed by those skilled in the art according to actual device design requirements.

[0036] S2: Figure 2 As shown, a dry etching process is used to remove the polysilicon 102a on the upper surface of the epitaxial layer 100 and the silicon nitride layer 101. This process leaves polysilicon on both side walls of the silicon nitride layer 101, which is recorded as sidewall polysilicon 102b. Subsequently, a dry etching process is used to etch a groove I 109a on the epitaxial layer 100 between the adjacent sidewall polysilicon 102b, and a gate oxide layer 103a is generated on the surface of the groove I 109a. The gate oxide layer is generated in a high-temperature oxygen-containing environment, which is a conventional technical means, so it is not described in detail.

[0037] In this embodiment 1, the specific parameters of the trench I 109a, such as depth and width, are selectively designed by those skilled in the art according to actual device design requirements. In this embodiment 1, the thickness of the gate oxide layer 103a is preferably 20-100nm, and the specific value can be selectively designed by those skilled in the art according to actual requirements.

[0038] S3: Figure 3 As shown, the gate polysilicon 102c is filled into the groove I 109a so as to cover the entire upper surface of the device, and the surface of the gate polysilicon 102c is planarized by using a CMP process (chemical mechanical polishing process).

[0039] S4: Figure 4As shown, the sidewall polysilicon 102b and the gate polysilicon 102c are removed simultaneously by a wet etching process, and the gate polysilicon 102c is etched to a height slightly lower than the surface of the epitaxial layer 100 (the height difference is not greater than 0.1 μm) to ensure that there is no polysilicon residue on the surface of the epitaxial layer 100, and then a shielding oxide layer 103b is deposited on the surface of the gate polysilicon 102c, the silicon nitride layer 101 and the epitaxial layer 100. In this embodiment 1, the thickness of the shielding oxide layer 103b is preferably 20-30 nm.

[0040] S5: Figure 5 As shown, an ion implantation process is used to form a P-type well region Ⅰ104 and an N-type well region 105 in the epitaxial layer 100 on both sides of the trench Ⅰ109a.

[0041] In this embodiment 1, P-type doping ions (preferably boron ions) are implanted into the epitaxial layer 100 on both sides of the trench Ⅰ109a at an angle of 7°-9°, and after high-temperature activation at 1000°C-1100°C, a P-type well region Ⅰ104 is formed. N-type doping ions (preferably arsenic ions or phosphorus ions) are implanted into the epitaxial layer 100 on both sides of the trench Ⅰ109a at an angle of 0°, and annealed at 950°C to form an N-type well region 105. In this embodiment 1, the concentrations of the P-type doping ions and the N-type doping ions are preferably 1e12-1e13 cm -2 .

[0042] S6: Figure 6 As shown, a dielectric layer 106 is deposited on the entire device surface, and the surface of the dielectric layer 106 is planarized by a CMP process (chemical mechanical polishing process), so that the surface of the dielectric layer 106 is flush with the surface of the shielding oxide layer 103b on the silicon nitride layer 101 or slightly lower than the surface of the shielding oxide layer 103b on the silicon nitride layer 101;

[0043] S7: Figure 7 As shown, a dry etching process is used to sequentially remove the shielding oxide layer 103b on the surface of the silicon nitride layer 101, the silicon nitride layer 101, and a portion of the epitaxial layer 100 corresponding to the vertical projection surface of the silicon nitride layer 101 to form a trench II 109b, and an ion implantation process is used in the trench II 109b to implant difluoroboride ions or monoboron ions at an angle of 0° into the bottom of the trench II 109b to form a P-type well region II 107, and both sides of the P-type well region II 107 are connected to the P-type well region I 104 and the N-type well region 105.

[0044] In this embodiment 1, the width of the groove II 109b can be selectively designed according to the actual device design requirements, which is a conventional technical means, and generally a width of 0.6-2um is applicable. In this embodiment 1, the concentration of the boron difluoride ion or the monoboron ion is preferably 1e14-5e15 cm -2 .

[0045] In the present invention, since the two P-type well regions I 104 are separated, a P-type well region II 107 is filled in the trench II 109 b to connect the two P-type well regions I 104 .

[0046] S8: Deposit metal 108 on the surface of dielectric layer 106 and in trench II 109b to form electrodes, and separate the surface electrodes into gate and source electrodes based on the second mask layer using photolithography process, and finally complete the production of trench MOSFET. Figure 8 shown.

[0047] In the present invention, the sidewall polysilicon 102b is close to a triangular shape, and the width of the trench 1109a depends on the height of the silicon nitride layer 101. This is because the higher the height of the silicon nitride layer 101, the larger the triangular sidewall polysilicon 102b, resulting in a smaller width of the trench 1109a. Therefore, to complete a smaller trench, a higher silicon nitride layer 101 is required.

[0048] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A method for preparing a trench MOSFET, characterized in that: The specific preparation steps are as follows: S1: depositing a layer of silicon nitride on the epitaxial layer (100), etching a portion of the silicon nitride region using a photolithography process based on a first mask layer to form a plurality of silicon nitride layers (101) distributed at intervals, and depositing polysilicon (102a) on the surface of the epitaxial layer (100) and the silicon nitride layer (101); S2: using a dry etching process to remove the polysilicon (102a) on the surface, the process will leave polysilicon on both side walls of the silicon nitride layer (101), which is recorded as side wall polysilicon (102b), and then using a dry etching process to etch a groove I (109a) on the epitaxial layer (100) between adjacent side wall polysilicon (102b), and generate a gate oxide layer (103a) on the surface of the groove I (109a); S3: Filling the gate polysilicon (102c) into the groove I (109a) so as to cover the entire upper surface of the device, and flattening the surface of the gate polysilicon (102c); S4: using a wet etching process to simultaneously remove the sidewall polysilicon (102b) and the gate polysilicon (102c), and etching the gate polysilicon (102c) to below the surface of the epitaxial layer (100) to ensure that no polysilicon remains on the surface of the epitaxial layer (100), and then depositing a shielding oxide layer (103b) on the surfaces of the gate polysilicon (102c), the silicon nitride layer (101) and the epitaxial layer (100); S5: using an ion implantation process to form a P-type well region I (104) and an N-type well region (105) in the epitaxial layer (100) on both sides of the trench I (109a); S6: depositing a dielectric layer (106) on the entire device surface, and flattening the surface of the dielectric layer (106) so that the surface of the dielectric layer (106) is flush with or lower than the surface of the shielding oxide layer (103b) on the silicon nitride layer (101); S7: using a dry etching process to sequentially remove the shielding oxide layer (103b), the silicon nitride layer (101), and a portion of the epitaxial layer (100) corresponding to the vertical projection surface of the silicon nitride layer (101) on the surface of the silicon nitride layer (101) to form a trench II (109b), and performing ion implantation in the trench II (109b) to form a P-type well region II (107), wherein both sides of the P-type well region II (107) are connected to the P-type well region I (104) and the N-type well region (105); S8: Depositing metal (108) on the surface of the dielectric layer (106) and in the groove II (109b) to form electrodes, using a photolithography process based on a second mask layer to separate the surface electrodes to obtain a gate and a source, thereby completing the production of a trench MOSFET.

2. The method for preparing a trench MOSFET according to claim 1, characterized in that: In the above S5, P-type doping ions are implanted into the epitaxial layer (100) on both sides of the trench I (109a) at an angle of 7°-9°, and after high-temperature activation at 1000°C-1100°C, a P-type well region I (104) is formed.

3. The method for preparing a trench MOSFET according to claim 2, characterized in that: The P-type doping ions are boron ions.

4. The method for preparing a trench MOSFET according to claim 1, characterized in that: In the above S5, N-type doping ions are implanted into the epitaxial layer (100) on both sides of the trench I (109a) at an angle of 0°, and annealing is performed at 900°C-950°C to form an N-type well region (105).

5. The method for preparing a trench MOSFET according to claim 4, characterized in that: The N-type doping ions are arsenic ions or phosphorus ions.

6. The method for preparing a trench MOSFET according to claim 1, characterized in that: In the S3, a CMP process is used to planarize the surface of the gate polysilicon (102c).

7. The method for preparing a trench MOSFET according to claim 1, characterized in that: In S6, a CMP process is used to planarize the surface of the dielectric layer (106).

8. The method for preparing a trench MOSFET according to claim 1, characterized in that: In the above-mentioned S7, an ion implantation process is used to implant boron difluoride ions or monoboron ions at an angle of 0° into the bottom of the trench II (109b) to form a P-type well region II (107).