A TAIKO wafer vacuum film laminating device and method

By using a movable vacuum cavity to adsorb the wafer in the TAIKO wafer vacuum filming device and combining laser circumcision and vacuum film, the problems of complexity and low efficiency of Taiko wafer filming are solved, and efficient and low-cost circumcision are achieved. and filming process.

CN118692959BActive Publication Date: 2024-11-08YUNZHE SEMICON TECH (ZHEJIANG) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411196684.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-11-08
Estimated Expiration
2044-08-29

AI Technical Summary

Technical Problem

Taiko wafers need to be filmed before cutting, but due to different edge thicknesses, the existing film pasting methods are complex, numerous equipment, high cost and low efficiency, making it difficult to achieve efficient circumcision and film pasting processes.

Method used

A TAIKO wafer vacuum film patching device including an circumcision station and a film patching station was designed. The wafer is adsorbed by a movable vacuum cavity, combined with laser circumcision and vacuum patching to achieve continuous processing of circumcision and film patching. Avoid wafer warping and reduce equipment costs through split structures.

Benefits of technology

It improves the efficiency and quality of wafer circumcision and filming, reduces equipment and management costs, saves space, and realizes efficient filming process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118692959B_ABST
    Figure CN118692959B_ABST
Patent Text Reader

Abstract

The present invention discloses a TAIKO wafer vacuum film pasting device and method, including a ring cutting station and a film pasting station, wherein the ring cutting station is provided with a ring cutting table, and a hollow wafer placement position is provided on the ring cutting table; the film pasting station is provided with a sealing cover, a sheet ring placement table and a vacuum chamber that work together, and the sealing cover, the sheet ring placement table and the vacuum chamber constitute a vacuum film pasting mechanism; the vacuum chamber can be driven by a first driving mechanism to reciprocate between the film pasting station and the ring cutting station; a liftable wafer adsorption table is provided in the vacuum chamber, and during ring cutting, the vacuum chamber moves to the bottom of the ring cutting table, and the wafer adsorption table can rise to the wafer placement position. The present invention uses a movable vacuum chamber to adsorb wafers, so that the wafer is adsorbed by the wafer adsorption table in the vacuum chamber throughout the process from ring cutting to film pasting, and the wafer will not have a warping problem, thereby ensuring film pasting efficiency and film pasting quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of wafer film pasting, and in particular to a TAIKO wafer vacuum film pasting device and method. Background Art

[0002] The Taiko process means that when the wafer is thinned, the edge of the wafer is retained, and only the inner circle of the wafer is ground and thinned. The thinned wafer is disc-shaped, and the edge of the wafer has high-strength support to prevent the wafer from warping. Generally, the wafer needs to be electroplated, cut and other processes after thinning. Before the cutting process, the wafer needs to be affixed with a protective film on the back. However, because the edge of the Taiko wafer has a thick step support, the thickness of the entire film surface is different, and the ring needs to be removed first, and the film process cannot be carried out directly. This makes it very difficult to cut and film the Taiko wafer.

[0003] At present, the film lamination method used by Taiko wafers is: first vacuum lamination, then ring cutting of the wafer to separate the step from the wafer; then UV irradiation, control of UV light so that only the step part is irradiated by UV light, and then use a scraper to remove the step ring; finally, high-temperature baking is performed to make the wrinkled film at the step ring stretch and flatten. This film lamination method has more and more complicated overall processes, high management costs, and requires multiple devices to work together, which occupies a larger area, increasing production costs, and the procurement cost of these devices is high, and the overall film lamination efficiency is low. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a TAIKO wafer vacuum film laminating device and method, which can quickly complete the wafer ring cutting and film laminating processes with good film laminating quality and high efficiency.

[0005] To this end, the technical solution of the present invention is: a TAIKO wafer vacuum film pasting device, including a ring cutting station and a film pasting station, the ring cutting station is provided with a ring cutting table, and the ring cutting table is provided with a hollow wafer placement position; the film pasting station is provided with a sealing cover, a sheet ring placement table and a vacuum chamber that work together, the sheet ring placement table is located below the sealing cover, and the sealing cover, the sheet ring placement table and the vacuum chamber constitute a vacuum film pasting mechanism; the vacuum chamber can be driven by a first driving mechanism to move back and forth between the film pasting station and the ring cutting station; the vacuum chamber is provided with a liftable wafer adsorption table, during ring cutting, the vacuum chamber moves to below the ring cutting table, and the wafer adsorption table can rise to the wafer placement position.

[0006] On the basis of the above scheme and as a preferred scheme of the above scheme: a sheet ring placement groove is provided above the sheet ring placement table, and the sheet ring placement table is installed on a lifting mechanism, and the lifting mechanism drives the sheet ring placement table to move up and down.

[0007] On the basis of the above scheme and as a preferred scheme of the above scheme: a circular opening is provided on the wafer placement position of the ring cutting table, and the diameter of the circular opening is the same as the diameter of the thinned part of the wafer; a circle of annular support surface is provided on the circular opening, and the annular support surface is opposite to the step ring position of the wafer.

[0008] On the basis of the above scheme and as a preferred scheme of the above scheme: a vacuum suction nozzle is provided on the annular support surface for adsorbing the step ring of the wafer.

[0009] On the basis of the above scheme and as a preferred scheme of the above scheme: the wafer adsorption table covers the thinned portion of the wafer, that is, the wafer adsorption table can completely adsorb the thinned portion of the wafer.

[0010] Another technical solution of the present invention is: a TAIKO wafer vacuum film bonding method, comprising the following steps:

[0011] S1. Place the wafer on the circular cutting table, wherein the step ring of the wafer is placed on the circular support surface, and the thinned wafer body is completely exposed at the circular opening;

[0012] S2, the vacuum chamber moves to the bottom of the circular cutting table, the wafer adsorption table rises to the circular opening, and vacuum adsorbs the wafer body;

[0013] S3, laser ring cutting is performed to remove the step ring of the wafer, and the step ring remains on the ring cutting table, and the main body of the wafer is driven downward by the wafer adsorption table;

[0014] S4. The vacuum chamber drives the wafer body to move to the bottom of the wafer ring placement table and cooperates with the sealing cover to complete the vacuum film bonding.

[0015] On the basis of the above scheme and as a preferred scheme of the above scheme: the vacuum film lamination in step S4 comprises the following steps:

[0016] S4.1. Fix the cutting film and the sheet ring together in advance, place the sheet ring on the sheet ring placement table, and fix it;

[0017] S4.2, the vacuum chamber moves to below the wafer ring placement table, and the wafer ring placement table is lowered to be fixedly connected to the vacuum chamber, and the wafer body is located below the cutting film;

[0018] S4.3. Move the sealing cover downwards and seal it with the ring placement table and the vacuum chamber to start vacuuming and film lamination.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] A movable vacuum chamber is used to adsorb the wafer, so that the wafer is in an adsorbed state from ring cutting to film pasting, and the wafer is adsorbed by the wafer adsorption table in the vacuum chamber throughout the process. During the ring cutting and film pasting process, the wafer will not warp, thereby ensuring the film pasting efficiency and quality.

[0021] The vacuum chamber and the wafer ring placement table are set as a split structure to facilitate the vacuum chamber to move to the ring cutting station to adsorb the wafer body. The vacuum chamber is used instead of the vacuum suction cup to avoid the warping problem that may occur during the wafer transfer process, which is more efficient to use.

[0022] Combining laser circular cutting and vacuum film lamination together can not only meet the film lamination needs and ensure product safety, but also reduce equipment costs, save management costs, save clean room space, and be economical and practical. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a structural schematic diagram of the feeding stage of the present invention;

[0024] Figure 2 It is a structural front view of the present invention at the loading stage;

[0025] Figure 3 It is a structural schematic diagram of the circumcision stage of the present invention;

[0026] Figure 4 It is a front view of the structure of the circumcision stage of the present invention;

[0027] Figure 5 It is a structural schematic diagram of the film-sticking stage of the present invention;

[0028] Figure 6 It is a front view of the structure of the present invention at the film-sticking stage;

[0029] Figure 7 It is a schematic diagram of the working principle of the present invention.

[0030] The accompanying drawings are marked as: loading station 1, circular cutting station 2, laser circular cutting machine 21, circular cutting table 22, third driving mechanism 23, circular mouth 24, annular supporting surface 25, film pasting station 3, sealing cover 31, sheet ring placement table 32, sheet ring placement groove 321, vacuum chamber 33, wafer adsorption table 331, lifting mechanism 34, first driving mechanism 35, wafer 4, wafer body 41, step ring 42. DETAILED DESCRIPTION

[0031] In the description of the present invention, it should be noted that directional words, such as the terms "center", "lateral (X)", "longitudinal (Y)", "vertical (Z)", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", etc., indicating directions and positional relationships are based on the directions or positional relationships shown in the accompanying drawings, which are only for the convenience of narrating the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and cannot be understood as limiting the specific scope of protection of the present invention.

[0032] In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features. Therefore, the definition of "first" and "second" features can explicitly or implicitly include one or more of the features. In the description of the present invention, "several" and "a number" mean two or more, unless otherwise clearly and specifically defined.

[0033] like Figure 1 to Figure 6 As shown, the TAIKO wafer vacuum film laminating device described in this embodiment includes a loading station 1, a ring cutting station 2 and a film laminating station 3. The TAIKO wafer 4 includes a wafer body 41 thinned in the middle and a step ring 42 not thinned at the edge.

[0034] The circular cutting station 2 is provided with a laser circular cutting machine 21, a circular cutting table 22, and a third driving mechanism 23 for driving the circular cutting table 22 to translate; the circular cutting table 22 is located below the laser circular cutting machine 21, and a hollow wafer placement position is provided on the circular cutting table 22, and a circular opening 24 is provided on the wafer placement position of the circular cutting table 22, and the diameter of the circular opening 24 is the same as the diameter of the thinned wafer body 41; a circle of annular support surface 25 is provided on the edge of the circular opening 24, and the annular support surface 25 is opposite to the step ring 42 of the wafer. At the same time, there is a vacuum suction nozzle on the annular support surface 25, which can adsorb the wafer on the step ring 42 to position the wafer.

[0035] The third driving mechanism 23 includes a third slide rail, a third slider, a third screw rod, and a third screw rod motor. The third slider is slidably mounted on the third slide rail below the circular cutting table 22, and the slider is threadedly engaged with the third screw rod. The third screw rod motor drives the third screw rod to rotate, so that the circular cutting table 22 moves back and forth between the loading station 1 and the circular cutting station 2. The manipulator of the loading station 1 places the positioned wafer on the circular cutting table 22, and then the circular cutting table 22 brings it back to the circular cutting station 2 for laser circular cutting.

[0036] The film-sticking station 3 is provided with a sealing cover 31, a sheet ring placement table 32 and a vacuum chamber 33 that work together. The sheet ring placement table 32 is located below the sealing cover 31. The sealing cover 31, the sheet ring placement table 32 and the vacuum chamber 33 constitute a vacuum film-sticking mechanism. The sheet ring placement table 32 is provided with a sheet ring placement groove 321, which can be used to place the cutting film and the sheet ring, and the sheet ring placement table 32 is set on a lifting mechanism 34. The lifting mechanism 34 includes a lifting cylinder and a guide block. A lifting slider is provided on the side of the sheet ring placement table 32. The lifting slider is connected to the cylinder rod of the lifting cylinder. Guide rods are fixed on both sides of the lifting slider. The guide rods are inserted into the guide blocks, so that the sheet ring placement table 32 can be lifted and lowered smoothly, and it is convenient to connect and fix with the vacuum chamber. The vacuum chamber 33 is provided with a liftable wafer adsorption table 331. The wafer adsorption table 331 can cover the thinned wafer body 41, that is, the wafer adsorption table 331 can completely adsorb the wafer body 41.

[0037] The vacuum chamber 33 is mounted on the first driving mechanism 35 and can move between the film laminating station 3 and the ring cutting station 2; the first driving mechanism 35 includes a first slide rail, a first slider, a first screw rod, and a first screw rod motor. Both sides of the vacuum chamber 33 are slidably mounted on the first slide rail through the first slider, and the first slider is threadedly matched with the first screw rod. During ring cutting, the vacuum chamber 33 moves to the bottom of the ring cutting table 22, and the wafer adsorption table 331 can rise to the wafer placement position, so that the wafer adsorption table 331 can adsorb the thinned wafer body 41 before ring cutting; after ring cutting, the vacuum chamber 33 can drive the wafer body 41 to move to the bottom of the sealing cover 31 for vacuum laminating.

[0038] like Figure 7 As shown, the film pasting method includes the following steps:

[0039] S1. Place the wafer 4 on the circular cutting table 22, wherein the wafer step ring 42 is placed on the circular support surface 25, and the thinned wafer body 41 is completely exposed at the circular opening 24. The wafer can be taken out from the wafer box by a robot, and after being positioned by a positioning mechanism and flipped by a flipping mechanism, it is placed on the circular cutting table at the loading station.

[0040] S2. Driven by the third driving mechanism 23, the circular cutting table 22 returns to the circular cutting station 2 and is opposite to the position of the laser circular cutting machine 21; at this time, the vacuum chamber 33 moves to the bottom of the circular cutting table 22, and the wafer adsorption table 331 rises to the circular opening 24 and vacuum adsorbs the thinned wafer body 41.

[0041] S3, laser ring cutting is performed to remove the step ring 42 of the wafer, and the step ring 42 remains on the ring cutting table 22, and the wafer body 41 is driven downward by the wafer adsorption table 331. The laser ring cutting mechanism performs the laser ring cutting process, which is a mature technology and will not be described in detail.

[0042] S4, Vacuum film:

[0043] S4.1, the vacuum chamber 33 is moved to the bottom of the wafer ring placement table 32, the cutting film and the wafer ring are fixed together, and the wafer ring is placed on the wafer ring placement groove 321 and fixed; at this time, the wafer body 41 is located below the cutting film, and there is a certain distance between the two;

[0044] S4.2, the wafer ring placement table 32 moves down to be sealed and fixed with the vacuum chamber 33. The sealing cover 31 moves down to be sealed and fixed with the wafer ring placement table 32, and starts to evacuate; when the vacuum value reaches the required value, the wafer adsorption table 331 rises, so that the main surface of the wafer and the upper surface of the wafer ring are level;

[0045] S4.3, the vacuum chamber 33 and the sealing cover 31 release the atmospheric pressure at the same time, and use the atmospheric pressure to remove the bubbles between the wafer and the cutting film, so that the cutting film at the edge of the wafer is more docile;

[0046] S4.4, the sealing cover 31 moves up and separates from the vacuum chamber 33, the negative pressure of the ring placement groove and the wafer adsorption table 331 stops, and the robot can remove the wafer with the cutting film attached from the wafer adsorption table 331, thereby completing the wafer film attachment work.

[0047] The above is only a preferred embodiment of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention. It should be pointed out that for ordinary technicians in this technical field, some improvements and modifications without departing from the principle of the present invention should also be regarded as the protection scope of the present invention.

Claims

1. A TAIKO wafer vacuum laminating device, characterized in that: The invention comprises a ring cutting station and a film pasting station, wherein the ring cutting station is provided with a ring cutting table, and a hollow wafer placement position is provided on the ring cutting table; the film pasting station is provided with a sealing cover, a sheet ring placement table and a vacuum chamber that cooperate with each other, and the sheet ring placement table is located below the sealing cover, and the sealing cover, the sheet ring placement table and the vacuum chamber constitute a vacuum film pasting mechanism; the vacuum chamber can be driven by a first driving mechanism to move back and forth between the film pasting station and the ring cutting station; a liftable wafer adsorption table is provided in the vacuum chamber, and when ring cutting is performed, the vacuum chamber moves to the bottom of the ring cutting table, and the wafer adsorption table can rise to the wafer placement position; the movable vacuum chamber is used to adsorb the wafer, and the wafer is in an adsorbed state from the ring cutting to the film pasting process, and the wafer is adsorbed by the wafer adsorption table in the vacuum chamber throughout the process.

2. A TAIKO wafer vacuum laminating device as claimed in claim 1, characterized in that: A sheet ring placement groove is arranged above the sheet ring placement table, and the sheet ring placement table is installed on a lifting mechanism, and the lifting mechanism drives the sheet ring placement table to move up and down.

3. A TAIKO wafer vacuum laminating device as claimed in claim 1, characterized in that: A circular opening is provided on the wafer placement position of the circular cutting table, and the diameter of the circular opening is the same as the diameter of the thinned part of the wafer; a circle of annular supporting surface is provided on the circular opening, and the annular supporting surface is opposite to the step ring position of the wafer.

4. A TAIKO wafer vacuum laminating device as claimed in claim 3, characterized in that: The annular support surface is provided with a vacuum suction nozzle for adsorbing the step ring of the wafer.

5. The TAIKO wafer vacuum laminating device according to claim 1, characterized in that: The wafer adsorption table covers the thinned portion of the wafer, that is, the wafer adsorption table can completely adsorb the thinned portion of the wafer.

6. A TAIKO wafer vacuum film lamination method, characterized in that: Using the film sticking device according to any one of claims 1 to 5 comprises the following steps: S1. Place the wafer on the circular cutting table, wherein the step ring of the wafer is placed on the circular support surface, and the thinned wafer body is completely exposed at the circular opening; S2, the vacuum chamber moves to the bottom of the circular cutting table, the wafer adsorption table rises to the circular opening, and vacuum adsorbs the wafer body; S3, laser ring cutting is performed to remove the step ring of the wafer, and the step ring remains on the ring cutting table, and the main body of the wafer is driven downward by the wafer adsorption table; S4. The vacuum chamber drives the wafer body to move to the bottom of the wafer ring placement table and cooperates with the sealing cover to complete the vacuum film bonding.

7. A TAIKO wafer vacuum lamination method as claimed in claim 6, characterized in that: The vacuum film lamination in step S4 comprises the following steps: S4.

1. Fix the cutting film and the sheet ring together in advance, place the sheet ring on the sheet ring placement table, and fix it; S4.2, the vacuum chamber moves to below the wafer ring placement table, and the wafer ring placement table is lowered to be fixedly connected to the vacuum chamber, and the wafer body is located below the cutting film; S4.

3. Move the sealing cover downwards and seal it with the ring placement table and the vacuum chamber to start vacuuming and film lamination.