Preparation method and application of high-water-resistance zinc dialkyl dithiophosphate additive

By preparing a highly water-resistant zinc dialkyl dithiophosphate additive in oil film bearing oil, utilizing the batch reaction of alkyl alcohol and phosphorus pentasulfide, combined with a high flash point aromatic solvent and zinc oxide, the hydrolysis stability in oil film bearing oil is solved. and poor water separation performance, achieving excellent anti-wear performance and a safe and environmentally friendly preparation process.

CN118725935AActive Publication Date: 2024-10-01PETROCHINA CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202310334462.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-01
Estimated Expiration
2043-03-31

AI Technical Summary

Technical Problem

It is difficult to achieve high hydrolysis stability and excellent water separation performance in oil film bearing oil with the existing technology, and the preparation process has potential safety hazards and environmental impacts caused by hydrogen sulfide overflow.

Method used

Alkyl alcohol and phosphorus pentasulfide are added in batches under rapid stirring conditions, and then the temperature is raised to react and distilled under reduced pressure to obtain the intermediate dialkyl dithiophosphate, and then high flash point aromatic hydrocarbon solvents and Zinc oxide, combined with fatty acid salt accelerator and sulfide, undergoes a multi-step reaction to prepare a highly water-resistant zinc dialkyl dithiophosphate additive.

Benefits of technology

It achieves excellent water separation performance, anti-wear performance and filtration performance in oil film bearing oil, and the process is stable and environmentally friendly, avoiding the safety hazard of hydrogen sulfide overflow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004155932060000091
    Figure BDA0004155932060000091
Patent Text Reader

Abstract

The invention discloses a preparation method of a high-water-resistance zinc dialkyl dithiophosphate additive, which specifically comprises the following steps: firstly, weighing alkyl alcohol, adding phosphorus pentasulfide into the alkyl alcohol in batches under a stirring condition, heating for reaction after adding, and then carrying out reduced pressure distillation, cooling and filtering to obtain dialkyl dithiophosphoric acid; the preparation method comprises the following steps: stirring an aromatic solvent and zinc oxide to form a homogeneous phase, adding a fatty acid salt accelerant and an intermediate dialkyl dithiophosphoric acid, stirring, then adding zinc oxide in batches, carrying out a heating reaction and a reduced pressure reaction after charging is completed, then cooling, adding sulfide, carrying out a heating reaction, carrying out reduced pressure distillation, and filtering to obtain the zinc sulfide. The high-water-resistance zinc dialkyl dithiophosphate additive is obtained. The high-water-resistance zinc dialkyl dithiophosphate additive disclosed by the invention can be used for preparing high-performance oil film bearing oil, so that an oil product has excellent water diversion performance and wear resistance, and the oil film bearing oil has excellent filterability, hydrolytic stability and outstanding bearing capacity.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of chemical material preparation, and in particular relates to a preparation method of a highly water-resistant dialkyl zinc dithiophosphate additive, and also relates to the application of the additive. Background Art

[0002] Zinc dialkyl dithiophosphate (ZDDP) is widely used due to its excellent properties of anti-oxidation, anti-wear and anti-corrosion. Since its introduction in the 1940s, it has been an indispensable additive component in oil products such as internal combustion engine oils, and has also been widely used in industrial oils such as gear oils and hydraulic oils.

[0003] The dosage of ZDDP in engine oil is usually 0.5-1.0%, and the dosage in industrial lubricating oil is usually 0.2-0.8%. In engine oil, ZDDP products with neutral salt as the main component are used; in industrial oil under water conditions, such as hydraulic oil, oil film bearing oil, etc., ZDDP products with basic salt as the main component are used. In the past 30 years, most neutral ZDDP products are mainly primary alkyl and secondary alkyl of single alkyl or mixed alkyl of carbon 3-8, and most basic ZDDP products are mainly primary alkyl products.

[0004] Oil film bearings have the characteristics of large load-bearing capacity, small friction coefficient, and strong impact resistance. It is a radial sliding bearing that uses lubricating oil as the lubricating medium. The operating temperature of its oil film oil system varies greatly, making the oil easy to oxidize and deteriorate, and it needs to bear impact loads. In view of these oil characteristics, foreign companies have developed three generations of oil film bearing oils. Oil film bearing oil will inevitably mix with industrial water during use, so the oil film bearing oil is required to have good wear resistance in the presence of water, and good oil-water separation ability is required when it is static. Based on the special performance requirements of oil film bearing oil, domestic lubricating oil research institutions and manufacturers have found it difficult to break through the bottleneck and make significant progress. Among them, ZDDP plays a key role in improving load-bearing capacity, wear resistance, and oxidation resistance in oil film bearing oil, and ZDDP products are required to have good water separation performance.

[0005] A Chinese patent (application number: 201110231801.5, publication number: CN102250139A) discloses a method for preparing alkyl thiophosphates, wherein phosphorus pentasulfide is dispersed in a high boiling point solvent, alcohol is added under vacuum conditions to react to obtain thiophosphoric acid, and then the thiophosphoric acid and zinc oxide react to obtain the product. The solvent used does not need to be removed and can be directly retained in the application system of the alkyl thiophosphate as a solvent; however, when hydrogen sulfide is extracted under vacuum conditions, the alkyl alcohol and hydrogen sulfide are easily separated from the reaction system, so that phosphorus pentasulfide cannot react completely, and the prepared product cannot achieve high hydrolysis stability and cannot be used in oil film bearing oil; Chinese patent (application number: 201711327221.X, publication number: CN107955035B) discloses a method for preparing a diisooctyl dithiophosphate additive for hydraulic oil, wherein isooctyl alcohol is added dropwise to an excess proportion of phosphorus pentasulfide; after the reaction, the solid phosphorus pentasulfide is filtered out; excess zinc oxide is added; the prepared thiophosphoric acid is added; after the reaction, the reagent is filtered to obtain diisooctyl dithiophosphate; the diisooctyl dithiophosphate prepared by this method improves its water separation performance in hydraulic oil, but the product does not mention the application in oil film bearing oil. Most of the existing technologies focus on the anti-wear and antioxidant properties of zinc dialkyl dithiophosphate products, but rarely pay attention to the basic salt structure and its use in oil film bearing oil under water conditions. Summary of the invention

[0006] The object of the present invention is to provide a method for preparing a highly water-resistant zinc dialkyl dithiophosphate additive, which has excellent water separation performance, load-bearing capacity and anti-wear performance in oil film bearing oil.

[0007] Another object of the present invention is to provide the use of the above-mentioned zinc dialkyl dithiophosphate additive in oil film bearing oil.

[0008] The technical solution adopted by the present invention is a method for preparing a highly water-resistant dialkyl dithiophosphate zinc additive, which is specifically implemented according to the following steps:

[0009] Step 1, weighing an alkyl alcohol, adding phosphorus pentasulfide to the alkyl alcohol in batches under rapid stirring conditions, heating the reaction after the phosphorus pentasulfide is added, then distilling under reduced pressure, cooling, and filtering to obtain an intermediate dialkyl dithiophosphoric acid;

[0010] Step 2, stirring a certain amount of high flash point aromatic solvent and a certain amount of zinc oxide to form a homogeneous phase, the reaction system is still carried out under the condition of an alkali solution absorption device, under certain conditions, a fatty acid promoter and an intermediate dialkyl dithiophosphate are added, and then zinc oxide is added in batches. After the addition is completed, the temperature is raised to a certain temperature condition, the reaction is carried out for a certain time, and then the pressure is reduced to react for a certain time, and then the temperature is lowered to add a certain amount of sulfide, and the temperature is continued to be raised for a certain time. After the reaction is completed, the high water-resistant dialkyl dithiophosphate zinc additive is obtained by filtration.

[0011] The present invention is also characterized in that:

[0012] In step 1, phosphorus pentasulfide is added in 5 to 10 batches; the molar ratio of alkyl alcohol to phosphorus pentasulfide is 4.0 to 5.0:1.0; when adding phosphorus pentasulfide, the temperature of the reaction system is controlled not to exceed 60° C., and maintained at a negative pressure of -0.005 MPa to -0.02 MPa, and a sodium hydroxide solution absorption bottle is connected to the reaction system.

[0013] In step 1, the reaction temperature is 95-110° C., the reaction time is 2-4 h, and the reduced pressure distillation time is 2 h.

[0014] In step 2, the temperature is lower than 80° C. when a fatty acid salt promoter is added, and the fatty acid salt promoter is one or more of sodium salts, calcium salts, and magnesium salts of normal or isomeric butyric acid, valeric acid, caproic acid, heptanoic acid, caprylic acid, nonanoic acid, capric acid, lauric acid, myristic acid, palmitic acid, oleic acid, and stearic acid.

[0015] In step 2, the stirring time is 10 to 60 minutes; zinc oxide is added in 3 to 5 batches.

[0016] In step 2, after the addition of zinc oxide is completed, the reaction temperature is 95-105° C., the reaction time is 2-4 hours, the reduced pressure reaction temperature is 100° C., and the reduced pressure reaction time is 1-2 hours.

[0017] In step 2, after the sulfide is added, the reaction temperature is 95-105° C., the reaction time is 1-2 h, the vacuum distillation temperature is 100-130° C., and the vacuum distillation time is 2-3 h.

[0018] In step 2, the high flash point aromatic solvent is aromatic oil or alkyl naphthalene solvent oil having a flash point greater than 130° C., and the mass ratio of the aromatic solvent to zinc oxide is 0.50-1.5:1.0.

[0019] In step 2, the sulfide is any one of sulfur, ammonium sulfide, sodium sulfide, molybdenum sulfide, and tungsten sulfide; and the molar ratio of the sulfide to zinc oxide is 0.01-0.2:1.0.

[0020] The beneficial effects of the present invention are:

[0021] (1) The highly water-resistant dialkyl dithiophosphate zinc additive of the present invention can be used to prepare high-performance oil film bearing oil, so that the oil product has excellent water separation performance, anti-wear performance, and the oil film bearing oil has excellent filterability, hydrolysis stability and outstanding load-bearing capacity. The additive can also be used in lubricating materials such as engine oil, industrial lubricating oil, and grease.

[0022] (2) The highly water-resistant dialkyl dithiophosphate zinc additive of the present invention has a simple preparation process, good process stability, an environmentally friendly reaction system, and mild reaction conditions. DETAILED DESCRIPTION

[0023] The present invention is described in detail below through specific implementation modes.

[0024] The preparation method of the highly water-resistant dialkyl dithiophosphate zinc additive of the present invention is specifically implemented according to the following steps:

[0025] Step 1, weighing an alkyl alcohol, adding phosphorus pentasulfide to the alkyl alcohol in 5 to 10 portions under rapid stirring, controlling the temperature of the reaction system not to exceed 60° C., maintaining a negative pressure of -0.005 MPa to -0.02 MPa, and connecting a sodium hydroxide solution absorption bottle with a mass concentration of 15% to the reaction system, heating to 95 to 110° C. after adding phosphorus pentasulfide, keeping the temperature for reaction for 2 to 4 hours, and then distilling under reduced pressure for 2 hours under the temperature condition, cooling, filtering, and obtaining an intermediate dialkyl dithiophosphoric acid;

[0026] The alkyl alcohol is one or more normal or isomeric alkyl alcohols having 4 to 12 carbon atoms;

[0027] The molar ratio of alkyl alcohol to phosphorus pentasulfide is 4.0-5.0:1.0;

[0028] Step 2, stirring a high flash point aromatic solvent and zinc oxide to form a homogeneous phase, adding a fatty acid salt promoter under the condition of less than 80°C, then adding an intermediate dialkyl dithiophosphoric acid, stirring for 10 to 60 minutes, and connecting a sodium hydroxide solution absorption bottle with a mass concentration of 15% in the reaction system, and then adding zinc oxide in 3 to 5 batches. After the addition is completed, a temperature reaction and a pressure reduction reaction are carried out, and then the temperature is reduced to below 80°C, and a sulfide is added, and then a temperature reaction is carried out.

[0029] Distill under reduced pressure and filter to obtain a highly water-resistant zinc dialkyl dithiophosphate additive;

[0030] After the addition of zinc oxide is completed, the reaction temperature is 95-105°C, the reaction time is 2-4h, the reduced pressure reaction temperature is 100°C, and the reduced pressure reaction time is 1-2h;

[0031] After the sulfide is added, the reaction temperature is 95-105°C, the reaction time is 1-2h, the vacuum distillation temperature is 100-130°C, and the vacuum distillation time is 2-3h;

[0032] The fatty acid salt promoter is one or more of the sodium salt, calcium salt, and magnesium salt of normal or isomeric butyric acid, valeric acid, caproic acid, heptanoic acid, caprylic acid, nonanoic acid, capric acid, lauric acid, myristic acid, palmitic acid, oleic acid, and stearic acid.

[0033] Aromatic solvents with high flash points refer to aromatic oils or alkyl naphthalene solvent oils with a flash point greater than 130°C, and the mass ratio of aromatic solvents to zinc oxide is 0.50-1.5:1.0;

[0034] The sulfide is any one of sulfur, ammonium sulfide, sodium sulfide, molybdenum sulfide and tungsten sulfide; the molar ratio of the sulfide to zinc oxide is 0.01-0.2:1.0.

[0035] The preparation method of the dialkyl dithiophosphate zinc additive of the present invention has excellent water separation performance, load-bearing capacity and anti-wear performance in oil film bearing oil. At the same time, the preparation process of the present invention is simple, the process is stable, and the reaction system is safe, environmentally friendly, and has high controllability and mild reaction conditions.

[0036] Example 1

[0037] The preparation method of the highly water-resistant dialkyl zinc dithiophosphate additive of the present invention is specifically as follows:

[0038] Add 110.4g of 2,2-dimethylbutanol into a four-necked flask, and add 55.6g of phosphorus pentasulfide evenly in 5 portions under rapid stirring; control the temperature of the reaction system not to exceed 60°C, maintain the reaction flask under a negative pressure of -0.005Mpa to -0.015Mpa, and connect the negative pressure system to a 15% sodium hydroxide solution absorption bottle. After the addition of phosphorus pentasulfide, heat to 100°C, stir and react for 2.5h, and then distill under reduced pressure at this temperature for 2h to distill out 7.6g of light components to obtain an intermediate dialkyl dithiophosphoric acid;

[0039] In a four-necked reaction flask, 28 g of aromatic solvent S270 and 9 g of zinc oxide were stirred to form a homogeneous phase. The reaction system was still carried out under the condition of an alkali solution absorption device. At 65° C., 5.8 g of sodium laurate was added as a promoter. After stirring for 40 minutes, the intermediate dialkyl dithiophosphoric acid (about 146 g) was added, and then 40 g of zinc oxide was added in 3 portions. After the addition was completed, the temperature was raised to 102° C. for reaction for 3.5 hours, and then the reduced pressure reaction was carried out at the temperature for 1.5 hours, and then the temperature was lowered and 3.8 g of molybdenum sulfide was added, the temperature was raised to 105° C. for reaction for 2 hours, and then the reduced pressure distillation was carried out at 120° C. for 1.5 hours. After the reaction was completed, it was filtered to obtain a highly water-resistant dialkyl dithiophosphoric acid zinc additive; the yield was about 91.5%.

[0040] Example 2

[0041] The preparation method of the highly water-resistant dialkyl zinc dithiophosphate additive of the present invention is specifically as follows:

[0042] 145.6 g of 2-ethylhexanol was added to a four-necked flask, and 55.6 g of phosphorus pentasulfide was added evenly in 5 portions under rapid stirring; the temperature of the reaction system was controlled not to exceed 60° C., the reaction flask was kept under a negative pressure of -0.005 MPa to -0.015 MPa, and the negative pressure system was connected to a 15% sodium hydroxide solution absorption bottle. After the addition of phosphorus pentasulfide was completed, the temperature was raised to 105° C., stirred for reaction for 2.5 h, and then distilled under reduced pressure at the same temperature for 2 h to distill out 9.3 g of light components to obtain an intermediate dialkyl dithiophosphoric acid;

[0043] In a four-necked reaction flask, 30 g of aromatic solvent S270 and 12 g of zinc oxide were stirred to form a homogeneous phase. The reaction system was still carried out under the condition of an alkali solution absorption device. At 60°C, 7.2 g of sodium stearate was added as a promoter. After stirring for 50 minutes, the aforementioned synthesized intermediate dialkyl dithiophosphate (about 176 g) was added, and then 38 zinc oxide was added in 4 portions. After the addition was completed, the temperature was raised to 105°C for reaction for 3 hours, and then the reaction was carried out under reduced pressure at the temperature for 2 hours. Then, the temperature was lowered and 2.7 g of ammonium sulfide was added. The temperature was raised to 105°C for reaction for 2 hours, and then the reaction was carried out under reduced pressure at 125°C for 1.5 hours. After the reaction was completed, it was filtered to obtain a highly water-resistant dialkyl dithiophosphate zinc additive with a yield of about 90.2%.

[0044] Example 3

[0045] The preparation method of the highly water-resistant dialkyl zinc dithiophosphate additive of the present invention is specifically as follows:

[0046] 55.0 g of hexanol and 72 g of octanol were added to a four-necked flask. Under rapid stirring, 55.6 g of phosphorus pentasulfide was added evenly in 5 portions. The temperature of the reaction system was controlled not to exceed 60°C, and the reaction flask was kept under a negative pressure of -0.005 MPa to -0.02 MPa. The negative pressure system was connected to a 15% sodium hydroxide solution absorption bottle. After the addition of phosphorus pentasulfide, the temperature was raised to 102°C, stirred for reaction for 3 hours, and then distilled under reduced pressure for 2 hours under the temperature condition to distill out 7.4 g of light components to obtain the intermediate dialkyl dithiophosphoric acid.

[0047] In a four-necked reaction flask, 28 g of aromatic solvent S270 and 10 g of zinc oxide were stirred to form a homogeneous phase. The reaction system was still carried out under the condition of an alkali solution absorption device. At 70°C, 4.2 g of sodium laurate was added as a promoter. After stirring for 40 minutes, the aforementioned synthesized intermediate dialkyl dithiophosphate (about 161 g) was added, and then 40 g of zinc oxide was added in 4 portions. After the addition was completed, the temperature was raised to 105°C for reaction for 3 hours, and then the reaction was carried out under reduced pressure at the temperature for 2 hours. Then, the temperature was lowered and 3.6 g of molybdenum sulfide was added. The temperature was raised to 105°C for reaction for 2 hours, and then the reaction was carried out under reduced pressure at 120°C for 1.5 hours. After the reaction was completed, it was filtered to obtain a highly water-resistant dialkyl dithiophosphate zinc additive with a yield of about 91.7%.

[0048] The highly water-resistant zinc dialkyl dithiophosphate additives prepared in Examples 1-3 of the present invention were compared with conventional ZDDP products, as shown in Table 1;

[0049] Table 1 Product analysis data of different dialkyl dithiophosphate zinc additives

[0050] project Example 1 Example 2 Example 3 T202 T204 Comparative Example 1 Appearance Yellow liquid Light yellow liquid Light yellow liquid Amber liquid Light yellow liquid Yellow liquid Chroma(undiluted) 1.5 1.0 1.0 2.0 1.5 1.5 Base value, mgKOH / g 18.4 20.1 20.3 Unable to detect 5.02 Unable to detect Acid value, mgKOH / g 89.2 83.6 84.5 131.6 121.0 129.8 Sulfur content, % 15.44 14.56 14.88 16.18 14.99 15.96 Phosphorus content, % 7.29 7.21 7.33 7.74 7.48 7.70 Zinc content, % 9.04 8.82 8.98 8.55 9.55 8.21

[0051] Note: T202 is n-butyl n-octyl zinc dithiophosphate; T204 is basic diisooctyl zinc dithiophosphate; Comparative Example 1 is didecyl zinc dithiophosphate (implemented with reference to patent 201110231801.5);

[0052] The performance of Example 1, T204 and Comparative Example 1 was investigated in oil film bearing oil, and the results are shown in Table 2;

[0053] Table 2 Performance of ZDDP in oil film bearing oil

[0054]

[0055] From the results in Table 2, it can be seen that the product of the present invention has excellent effects in water separation performance, antioxidant performance, load-bearing capacity, anti-wear performance, etc. compared with the conventional T204 product. Compared with the performance of foreign oil film bearing oil, the product of the present invention has equivalent or better performance. Due to the special structure of the zinc dialkyl dithiophosphate product in the present invention, the stability and emulsification ability are well balanced under the condition of water, so the product has excellent comprehensive performance.

[0056] The above is an embodiment of the present invention, taking into account the poor water separation performance, poor wear resistance and oxidation stability of the dialkyl dithiophosphate zinc additives used in the prior art oil film bearing oil products, and the hazards such as hydrogen sulfide overflow that may cause harm or even poisoning to operators, as well as impact on the environment. The present invention provides a method for preparing highly water-resistant dialkyl dithiophosphate zinc, which, when used in conjunction with other additives in oil film bearing oil, enables the oil film bearing oil to have excellent water separation performance, load-bearing capacity and wear resistance. At the same time, the preparation process of the present invention is simple, the process is stable, and the reaction system is safe, environmentally friendly, and has high controllability and mild reaction conditions. This type of additive can also be used in lubricating materials such as engine oil, industrial lubricating oil, and grease.

Claims

1. A method for preparing a highly water-resistant zinc dialkyl dithiophosphate additive, characterized in that: Follow the steps below to implement it: Step 1, weighing an alkyl alcohol, adding phosphorus pentasulfide to the alkyl alcohol in batches under rapid stirring conditions, heating the reaction after the phosphorus pentasulfide is added, then distilling under reduced pressure, cooling, and filtering to obtain an intermediate dialkyl dithiophosphoric acid; Step 2, stirring a high flash point aromatic solvent and zinc oxide to form a homogeneous phase, adding a fatty acid salt promoter and an intermediate dialkyl dithiophosphate, stirring, and then adding zinc oxide in batches, after the addition is completed, performing a temperature reaction and a reduced pressure reaction, then cooling, adding a sulfide, and then performing a temperature reaction, distilling under reduced pressure, filtering, and obtaining a highly water-resistant dialkyl dithiophosphate zinc additive.

2. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 1, phosphorus pentasulfide is added in 5 to 10 batches; the molar ratio of alkyl alcohol to phosphorus pentasulfide is 4.0 to 5.0:1.0; when adding phosphorus pentasulfide, the temperature of the reaction system is controlled not to exceed 60° C., and maintained at a negative pressure of -0.005 MPa to -0.02 MPa, and a sodium hydroxide solution absorption bottle is connected to the reaction system.

3. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 1, the reaction temperature is 95-110° C., the reaction time is 2-4 hours, and the reduced pressure distillation time is 2 hours.

4. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 2, the temperature is lower than 80° C. when the fatty acid salt promoter is added, and the fatty acid salt promoter is one or more of the sodium salt, calcium salt, and magnesium salt of normal or isomeric butyric acid, valeric acid, caproic acid, heptanoic acid, caprylic acid, nonanoic acid, capric acid, lauric acid, myristic acid, palmitic acid, oleic acid, and stearic acid.

5. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 2, the stirring time is 10 to 60 minutes; and the zinc oxide is added in 3 to 5 batches.

6. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 2, after the zinc oxide is added, the reaction temperature is 95-105° C., the reaction time is 2-4 hours, the reduced pressure reaction temperature is 100° C., and the reduced pressure reaction time is 1-2 hours.

7. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 2, after the sulfide is added, the reaction temperature is 95-105° C., the reaction time is 1-2 hours, the vacuum distillation temperature is 100-130° C., and the vacuum distillation time is 2-3 hours.

8. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In the step 2, the high flash point aromatic solvent is aromatic oil or alkyl naphthalene solvent oil having a flash point greater than 130° C., and the mass ratio of the aromatic solvent to zinc oxide is 0.50-1.5:1.

0.

9. The method for preparing the highly water-resistant zinc dialkyl dithiophosphate additive according to claim 1, characterized in that: In step 2, the sulfide is any one of sulfur, ammonium sulfide, sodium sulfide, molybdenum sulfide, and tungsten sulfide; and the molar ratio of the sulfide to zinc oxide is 0.01-0.2:1.

0.

10. Use of the highly water-resistant zinc dialkyl dithiophosphate additive according to any one of claims 1 to 9 in oil film bearing oil.

Citation Information

Patent Citations

  • Preparation method of alkyl thiophosphate

    CN102250139A

  • Preparation method of diisooctyl dithiophosphate additive for hydraulic oil

    CN107955035B

  • Extreme pressure antiwear agent and preparation method thereof and lubricating oil combination

    CN101724492A

  • A lubricating oil composition

    CN102459540A

  • Low-impurity content zinc dialkyl dithiophosphate and preparation method and application thereof

    CN106699806A