Metal liquid continuous production system and method

Through the continuous metal liquid production system with a double melting pool structure, the problems of high CO2 emissions and high production costs in the traditional steelmaking process are solved, and a low-carbon smelting process is realized, which meets the quality requirements of high-end products and reduces production costs.

CN118726680APending Publication Date: 2024-10-01SHOUGANG JINGTANG IRON & STEEL CO LTD +2
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410768999.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-14
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

Traditional steelmaking processes have high CO2 emissions, and existing new processes such as electric furnace smelting and hydrogen-based reduction furnace smelting have problems such as difficulty in controlling residual harmful elements in molten steel and high production costs.

Method used

A continuous metal liquid production system with a double melting pool structure is used to preheat ferrite resources and carbon raw materials through a mixing heating furnace, use a hot blast furnace to recover hot flue gas for energy reuse, and perform carburizing and mixing in the second melting pool. Uniformly separate slag and gold to achieve continuous process production of molten iron.

Benefits of technology

It reduces carbon emissions, meets the quality requirements for low nitrogen content of high-end products, improves process energy efficiency, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118726680A_ABST
    Figure CN118726680A_ABST
Patent Text Reader

Abstract

The invention relates to a metal liquid continuous production system and method, and the system comprises a mixing heating furnace which is used for mixing an iron resource and a carbon raw material; the first molten pool is used for roughly melting the mixture of the iron resource and the carbon raw material to obtain molten iron and furnace slag; the first molten pool is connected with the mixed heating furnace; the second molten pool is used for carrying out carburization, uniform mixing and slag-metal separation on the molten iron and the slag; the second molten pool is connected with the first molten pool; the hot blast stove is used for recycling the hot flue gas generated by the mixed heating furnace; and the hot-blast stove is connected with the mixed heating furnace. According to the continuous production system and method for the molten metal, a unique double-molten-pool structure is utilized, the problem that a dead stock column structure is formed when waste steel adopts a vertical preheating and continuous smelting mode is effectively solved, and molten iron and slag which are non-uniformly molten in a short time are accumulated in the second molten pool; and short-process continuous steel scrap feeding, preheating and tapping processes are realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of metallurgical industry, and in particular to a metal liquid continuous production system and method. Background Art

[0002] Traditional long-process steelmaking uses the blast furnace-converter process as the production process of the main raw material for steelmaking. This process is the main source of CO2 emissions, and the LCA carbon emissions are as high as about 3.0 / t of finished product.

[0003] At present, steel enterprises are actively exploring the traditional long-process extreme carbon reduction process, while also actively researching new green steel smelting processes. There are two main new process paths currently being explored: the first path is to use electric furnaces as the core equipment for producing finished molten steel, which can be smelted in electric furnaces with all scrap steel or in hydrogen-based direct reduced iron plus electric furnaces; the second path is to use a hydrogen-based reduction furnace plus a smelting furnace at the front end to provide low-carbon emission liquid iron, and the converter is still used as the core equipment for producing finished molten steel in the back process.

[0004] Electric furnace smelting is a relatively mature steelmaking process. The use of all scrap steel and green electricity mode can reduce carbon emissions to a lower level. However, it is difficult to control the residual harmful elements and N content in the molten steel, which cannot meet the requirements of high-end products such as automobile outer panels, and the production cost is long and the process is high. At present, companies such as ThyssenKrupp and Posco have developed the vertical furnace-melting furnace-converter process. The molten iron produced is connected to the converter process to meet the quality requirements of high-end products. However, since the vertical furnace production uses natural gas and coke oven gas, the carbon emission reduction is limited, and the production cost is higher than or close to that of the electric furnace, which is significantly higher than the existing blast furnace-converter process. Although the use of hydrogen and green electricity can significantly reduce carbon emissions, the production cost is higher, so it needs to be improved. Summary of the invention

[0005] In view of this, the present invention provides a metal liquid continuous production system and method.

[0006] Specifically, the present invention is achieved through the following technical solutions:

[0007] According to a first aspect of the present invention, there is provided a system for continuous production of liquid metal, comprising:

[0008] Mixing heating furnace, used to mix ferrous resources and carbon raw materials;

[0009] A first molten pool, used for roughly melting the mixture of the ferrous resource and the carbon raw material to obtain molten iron and slag; the first molten pool is connected to the mixed heating furnace;

[0010] A second molten pool is used for carburizing, mixing and slag-metal separation of the molten iron and slag; the second molten pool is connected to the first molten pool;

[0011] The hot blast furnace is used to recycle the hot flue gas generated by the mixed heating furnace; the hot blast furnace is connected to the mixed heating furnace.

[0012] Optionally, the first molten pool and the second molten pool are connected via a connecting pipe.

[0013] Optionally, the angle between the connecting pipe and the horizontal direction is 10-60°.

[0014] Optionally, electromagnetic induction coils are arranged on the outer side walls of the first molten pool, the second molten pool and the connecting pipe.

[0015] According to a second aspect of the present invention, there is provided a method for continuous production of liquid metal, which is implemented based on any of the above-mentioned continuous production systems for liquid metal, and the method comprises the steps of:

[0016] Mixing the ferrous resource and the carbon raw material by the mixing heating furnace;

[0017] Roughly melting the mixture of the ferrous resource and the carbon raw material in the first molten pool to obtain molten iron and slag;

[0018] Carburizing, mixing and slag-metal separation of the molten iron and slag are performed through the second molten pool;

[0019] The hot flue gas generated by the mixed heating furnace is recovered and utilized by the hot blast furnace.

[0020] Optionally, the total iron mass fraction of the ferrous resource is 30% to 100%.

[0021] Optionally, the mass fraction of carbon element in the carbon raw material is 30% to 99%.

[0022] Optionally, the mass of the carbon raw material is 2% to 20% of the ferrous solid waste.

[0023] Optionally, the outlet temperature of the hybrid heating furnace is 400-800°C.

[0024] Optionally, the temperature of the first molten pool is in the range of 800-1500°C, and the temperature of the second molten pool is in the range of 1400-1600°C.

[0025] The technical solution provided by the present invention brings at least the following beneficial effects:

[0026] The present application provides a continuous production system for liquid metal, which mixes ferrous resources and carbon raw materials to obtain a mixture; hot air is used to preheat and carburize the descending mixture, and the preheated ferrous resources and lime and other materials are added to the first melting pool for smelting, and the molten iron and slag are continuously flowed into the second melting pool for carburization, mixing and slag separation, and then the iron and steel are tapped respectively to obtain molten iron, semi-steel or steel with different carbon contents, and slag with specific components. The hot air generates hot gas in the mixed heating furnace, and the recycled coal gas generates hot air in the hot blast furnace, which is sprayed into the mixed heating furnace as a physical heat source and combustion-supporting gas to realize energy recycling. Compared with the current process, the present application uses a unique double melting pool structure to effectively solve the dead material column structure formed when the scrap steel adopts the vertical preheating and continuous smelting mode, and accumulates the molten iron and slag that are unevenly melted in a short time in the second melting pool, realizing a short-process continuous scrap steel feeding, preheating and iron-tapping process.

[0027] The present application provides a continuous production system and method for liquid metal to develop a new low-carbon smelting process, improve the energy efficiency of the process, utilize zero-carbon raw materials, and produce molten iron to connect the main process of the converter. The molten iron is processed in the converter to meet the quality requirements of high-end products for low nitrogen content, thereby reducing carbon emissions while meeting product quality, and is of great significance to reducing production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.

[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or related technical descriptions are briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.

[0030] Figure 1 A schematic structural diagram of a metal liquid continuous production system provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0031] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0032] Figure 1The schematic diagram shows the structure of a metal liquid continuous production system applicable to an embodiment of the present invention.

[0033] Reference Figure 1 As shown, the present application provides a metal liquid continuous production system, the method comprising the steps of:

[0034] A metal liquid continuous production system is provided, comprising:

[0035] A mixing heating furnace 1, used for mixing ferrous resources and carbon raw materials;

[0036] A first molten pool 2 is used for roughly melting a mixture of the ferrous resource and the carbon raw material to obtain molten iron and slag; the first molten pool 2 is connected to the mixed heating furnace 1;

[0037] A second molten pool 3 is used for carburizing, mixing and slag-metal separation of the molten iron and slag; the second molten pool 3 is connected to the first molten pool 2;

[0038] The hot blast furnace 4 is used to recycle the hot flue gas generated by the mixed heating furnace 1 ; the hot blast furnace 4 is connected to the mixed heating furnace 1 .

[0039] In an embodiment of the present application, ferrous resources and carbon raw materials are mixed in a mixing heating furnace 1 to obtain a mixture, and hot air is used in the mixing heating furnace 1 to preheat and carburize the descending mixture, and the preheated ferrous resources and lime and other materials are added to the first melting pool 2 for smelting, and the molten iron and slag continuously flow into the second melting pool 3 for carburizing, mixing and slag-metal separation, and then the iron and steel are tapped respectively; hot coal gas is generated in the mixing heating furnace 1, and the recycled coal gas is generated in the hot blast furnace 4 to generate hot air, which is sprayed into the mixing heating furnace 1 as a physical heat source and combustion-supporting gas to achieve energy recycling.

[0040] Exemplarily, the first molten pool 2 and the second molten pool 3 are connected via a connecting pipe 5 .

[0041] In the embodiment of the present application, the molten iron and slag continuously flow into the second molten pool 3 through the connecting pipe 5 for carburizing, mixing and slag-metal separation, and then the iron and steel are tapped respectively.

[0042] Exemplarily, the angle between the connecting pipe 5 and the horizontal direction is 10-60°. Exemplarily, the angle between the connecting pipe 5 and the horizontal direction can be 10°, 30°, 50°, 60°, etc.

[0043] In the embodiment of the present application, the angle between the connecting pipe 5 and the horizontal direction is 10-60°, which can satisfy the requirement that the molten iron and slag continuously flow into the second molten pool 3 through the connecting pipe 5 for carburizing, mixing and slag-metal separation.

[0044] Exemplarily, electromagnetic induction coils 6 are arranged on the outer side walls of the first molten pool 2 , the second molten pool 3 and the connecting pipe 5 .

[0045] In the embodiment of the present application, the electromagnetic induction coil 6 can heat the first molten pool 2, the second molten pool 3 and the connecting pipe 5 after being energized.

[0046] The present application also provides a method for continuous production of liquid metal, which is implemented based on the continuous production system for liquid metal as described above, and the method comprises the steps of:

[0047] Mixing the ferrous resource and the carbon raw material by the mixing heating furnace 1;

[0048] The first molten pool 2 is used to roughly melt the mixture of the ferrous resource and the carbon raw material to obtain molten iron and slag;

[0049] Carburizing, mixing and slag-metal separation of the molten iron and slag are performed through the second molten pool 3;

[0050] The hot flue gas generated by the mixed heating furnace is recovered and utilized by the hot blast furnace 4 .

[0051] In an embodiment of the present application, ferrous resources and carbon raw materials are mixed in a mixing heating furnace 1 to obtain a mixture, and hot air is used in the mixing heating furnace 1 to preheat and carburize the descending mixture, and the preheated ferrous resources and lime and other materials are added to the first melting pool 2 for smelting, and the molten iron and slag continuously flow into the second melting pool 3 for carburizing, mixing and slag-metal separation, and then the iron and steel are tapped respectively; hot coal gas is generated in the mixing heating furnace 1, and the recycled coal gas is generated in the hot blast furnace 4 to generate hot air, which is sprayed into the mixing heating furnace 1 as a physical heat source and combustion-supporting gas to achieve energy recycling.

[0052] Furthermore, the total iron mass fraction of the ferrous resource is 30% to 100%, and the ferrous resource includes at least one of scrap steel, metallurgical solid waste, sponge iron, and pellets. Exemplarily, the total iron mass fraction of the ferrous resource can be 30%, 50%, 80%, 100%, etc.

[0053] Furthermore, the mass fraction of carbon in the carbon raw material is 30% to 99%, and the carbon raw material includes at least one of biomass particles and coal. Exemplarily, the mass fraction of carbon in the carbon raw material can be 30%, 50%, 80%, 99%, etc.

[0054] Furthermore, the mass of the carbon raw material is 2% to 20% of the ferrous solid waste. For example, the mass of the carbon raw material can be 2%, 10%, 15%, 20% and the like to the ferrous solid waste.

[0055] Exemplarily, the outlet temperature of the hybrid heating furnace 1 is 400-800° C. Exemplarily, the outlet temperature of the hybrid heating furnace 1 can be 400° C., 500° C., 600° C., 800° C., etc.

[0056] In the embodiment of the present application, 400-800°C can meet the heating needs of ferrous resources and carbon raw materials.

[0057] Exemplarily, the temperature of the first molten pool 2 is in the range of 800-1500° C. Exemplarily, the temperature of the first molten pool 2 may be in the range of 800° C., 1000° C., 1200° C., 1500° C., and the like.

[0058] In the embodiment of the present application, the temperature setting of 800-1500° C. can meet the heating requirements of the first molten pool 2 .

[0059] Exemplarily, the temperature of the second molten pool 3 ranges from 1400 to 1600° C. Exemplarily, the temperature of the second molten pool 3 can range from 1400° C., 1500° C., 1600° C., and the like.

[0060] In the embodiment of the present application, the temperature setting of 1400-1600° C. can meet the heating requirements of the second molten pool 3 .

[0061] Furthermore, the amount of carbon raw materials such as carbon powder and coal powder added to the second molten pool 3 is 2-10 kg / t to facilitate carburizing.

[0062] Furthermore, the temperature of the molten iron, semi-molten steel or molten steel in the second molten pool 3 is 1300-1650°C, and the carbon content is 0.5%-5.0%. For example, the temperature of the molten iron, semi-molten steel or molten steel can be 1300°C, 1500°C, 1650°C, etc.

[0063] Further, the hot air flow rate of the hot air furnace 4 is 50-100Nm3 / t iron, and the hot air temperature is 500-1300° C. For example, the hot air flow rate of the hot air furnace 4 can be 50Nm3 / t iron, 80Nm3 / t iron, 100Nm3 / t iron, etc., and the hot air temperature can be 500° C., 1000° C., 1300° C., etc.

[0064] In the embodiment of the present application, scrap steel and biomass are preheated to 700-800°C in the mixed heating furnace 1, induction heating and melting are carried out in the first melting pool 2, and the melted molten iron and slag enter the second melting pool 3 through the connecting pipe 5, and the separation of molten iron and slag is completed in the slag-iron separation furnace. The preheating vertical furnace uses biomass particles as fuel. The first melting pool 2 for induction melting is installed at the bottom of the mixed heating furnace 1, and the upper flange of the first melting pool 2 is sealed and connected with the lower flange of the mixed heating furnace 1. Scrap steel from the mixed heating furnace 1 enters the first melting pool 2 one after another. A steel outlet is set in the middle of the first melting pool 2, and when the liquid level reaches the steel outlet, the molten steel flows out of the steel outlet. The molten iron mixed with slag and iron flowing out of the steel outlet of the first melting pool 2 enters the slag-iron separation furnace. In the second melting pool 3, due to the large difference in density between slag and molten iron, a natural separation process of slag floating and iron sinking is presented. The slag-iron separation furnace adopts the method of tapping steel from the bottom and tapping slag from the top. The molten iron enters the next ladle or mixed railway through the teapot spout flow channel. The second melting pool 3 has a temperature-raising effect to ensure that the molten iron in the teapot spout flow channel has sufficient fluidity. During the entire production process, it is only necessary to continuously add materials from the top of the mixed heating furnace 1. After being burned and heated by biomass particles, it is melted in the first melting pool 2 and the iron is continuously tapped. The slag and iron are continuously separated through the second melting pool 3. If the power supply for the first melting pool 2 and the second melting pool 3 comes from green electricity such as solar power generation or wind power. Then the entire melting process of the scrap steel return material only uses biomass particles and green electricity, completely achieving zero carbon emissions.

[0065] The present application will be further described below in conjunction with specific embodiments. It should be understood that these embodiments are intended only to illustrate the present application and are not intended to limit the scope of the present application. The experimental methods for which specific conditions are not specified in the following examples are usually measured according to national standards. If there is no corresponding national standard, then the conditions recommended by the manufacturer are followed.

[0066] Example 1

[0067] In a 100t / h industrial plant, scrap steel and biomass pellets are loaded into the hopper in a ratio of 10:1. The hot air flow rate is 8000Nm 3 / h, the temperature is 900℃, the thermophysical heat carried by the hot air heats the scrap steel, the oxygen in the hot air reacts with the C in the biomass particles to release heat and further heat the scrap steel, and the outlet temperature of the scrap steel in the preheating section is 700℃. The connecting pipe between the first molten pool 2 and the second molten pool 3 is 10° at an angle to the horizontal direction, the temperature range of the first molten pool 2 is 1250℃, and the temperature of the second molten pool 3 is 1550℃; the carbon powder added to the second molten pool 3 is 5kg / t for carburization; the carbon content of the output molten iron is 2.0%.

[0068] Example 2

[0069] In a 100t / h industrial device, DRI and biomass pellets are loaded into the hopper at a ratio of 8:1. The hot air flow rate is 9000Nm 3 / h, the temperature is 1000℃, the hot air carries the thermal physical heat to heat the scrap steel, the oxygen in the hot air reacts with the C in the biomass particles to release heat to further heat the scrap steel, and the scrap steel outlet temperature in the preheating section is 820℃. : The connecting pipe between the first molten pool 2 and the second molten pool 3 is 20° with the horizontal direction, the temperature range of the first molten pool 2 is 1230℃, and the temperature of the second molten pool 3 is 1570℃; the carbon powder added to the second molten pool 3 is 9kg / t for carburization; the carbon content of the output molten iron is 3.7%.

[0070] The present application provides a continuous production system for liquid metal, which mixes ferrous resources and carbon raw materials to obtain a mixture; hot air is used to preheat and carburize the descending mixture, and the preheated ferrous resources and lime and other materials are added to the first melting pool for smelting, and the molten iron and slag are continuously flowed into the second melting pool for carburization, mixing and slag separation, and then the iron and steel are tapped respectively to obtain molten iron, semi-steel or steel with different carbon contents, and slag with specific components. The hot air generates hot gas in the mixed heating furnace, and the recycled coal gas generates hot air in the hot blast furnace, which is sprayed into the mixed heating furnace as a physical heat source and combustion-supporting gas to realize energy recycling. Compared with the current process, the present application uses a unique double melting pool structure to effectively solve the dead material column structure formed when the scrap steel adopts the vertical preheating and continuous smelting mode, and accumulates the molten iron and slag that are unevenly melted in a short time in the second melting pool, realizing a short-process continuous scrap steel feeding, preheating and iron-tapping process.

[0071] The present application provides a metal liquid continuous production system to develop a new low-carbon smelting process, improve the energy efficiency of the process, utilize zero-carbon raw materials, and produce molten iron to connect the main process of the converter. The molten iron is processed in the converter to meet the quality requirements of high-end products for low nitrogen content, thereby reducing carbon emissions while meeting product quality, and is of great significance to reducing production costs.

[0072] It should be noted that, in the present application, the terms "upper", "lower", "left", "right", "front", "back", "top", "bottom", "inner", "outer", "vertical", "horizontal", "lateral", "longitudinal" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings. These terms are mainly used to better describe the present application and its embodiments, and are not used to limit the indicated devices, elements or components to have a specific orientation, or to be constructed and operated in a specific orientation.

[0073] In addition, some of the above terms may be used to express other meanings in addition to indicating orientation or positional relationship. For example, the term "on" may also be used to express a certain dependency or connection relationship in some cases. For those of ordinary skill in the art, the specific meanings of these terms in this application can be understood according to specific circumstances.

[0074] In addition, the terms "installed", "set", "provided with", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0075] In addition, the terms "first", "second", etc. are mainly used to distinguish different devices, elements or components (the specific types and structures may be the same or different), and are not used to indicate or imply the relative importance and quantity of the indicated devices, elements or components. Unless otherwise specified, "plurality" means two or more.

[0076] Various embodiments of the present application may be presented in the form of a range; it should be understood that the description in the form of a range is only for convenience and brevity, and should not be understood as a rigid limitation on the scope of the present application; therefore, the range description should be considered to have specifically disclosed all possible sub-ranges and single numerical values ​​within the range. For example, the range description from 1 to 6 should be considered to have specifically disclosed sub-ranges, such as from 1 to 3, from 1 to 4, from 1 to 5, from 2 to 4, from 2 to 6, from 3 to 6, etc., as well as single numbers within the range, such as 1, 2, 3, 4, 5 and 6, which apply regardless of the range. In addition, whenever a numerical range is indicated herein, it is meant to include any cited number (fractional or integer) within the indicated range.

[0077] The foregoing is merely a specific embodiment of the present invention, which enables those skilled in the art to understand or implement the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features claimed herein.

Claims

1. A metal liquid continuous production system, characterized in that: include: Mixing heating furnace, used to mix ferrous resources and carbon raw materials; A first molten pool, used for roughly melting the mixture of the ferrous resource and the carbon raw material to obtain molten iron and slag; the first molten pool is connected to the mixed heating furnace; The second molten pool is used for carburizing, mixing and slag-metal separation of the molten iron and slag; The second molten pool is connected to the first molten pool; The hot blast furnace is used to recycle the hot flue gas generated by the mixed heating furnace; the hot blast furnace is connected to the mixed heating furnace.

2. The metal liquid continuous production system according to claim 1, characterized in that: The first molten pool and the second molten pool are connected via a connecting pipe.

3. The metal liquid continuous production system according to claim 2, characterized in that: The angle between the communicating pipe and the horizontal direction is 10-60°.

4. The metal liquid continuous production system according to claim 2, characterized in that: Electromagnetic induction coils are arranged on the outer side walls of the first molten pool, the second molten pool and the connecting pipe.

5. A method for continuous production of liquid metal, characterized in that: Based on the metal liquid continuous production system as described in any one of claims 1 to 4, the method comprises the steps of: Mixing the ferrous resource and the carbon raw material by the mixing heating furnace; Roughly melting the mixture of the ferrous resource and the carbon raw material in the first molten pool to obtain molten iron and slag; Carburizing, mixing and slag-metal separation of the molten iron and slag are performed by the second molten pool; The hot flue gas generated by the mixed heating furnace is recovered and utilized by the hot blast furnace.

6. The method for continuous production of liquid metal according to claim 5, characterized in that: The total iron mass fraction of the ferrite resource is 30% to 100%.

7. The method for continuous production of liquid metal according to claim 5, characterized in that: The mass fraction of carbon element in the carbon raw material is 30% to 99%.

8. The method for continuous production of liquid metal according to claim 5, characterized in that: The mass of the carbon raw material is 2% to 20% of the ferrous solid waste.

9. The method for continuous production of liquid metal according to claim 5, characterized in that: The outlet temperature of the mixed heating furnace is 400-800°C.

10. The metal liquid continuous production system according to claim 5, characterized in that: The temperature of the first molten pool is in the range of 800-1500°C, and the temperature of the second molten pool is in the range of 1400-1600°C.

Citation Information

Patent Citations

  • Baking-melting reduction iron smelting method, apparatus and raw amterial

    CN101070558A

  • Process and device for continuous steelmaking from ferriferous material

    CN101445848A

  • Ironmaking equipment and process for direct smelting reduction of iron ore

    CN102127610A

  • Near-zero carbon emission treatment method and system for iron element solid waste

    CN117587182A

  • Method and apparatus for producing metal from materials containing iron oxides

    WO2014035276A1