Computer numerical simulation method for high-temperature oxidation behavior of ultra-pure ferritic stainless steel
Through computer numerical simulation methods, the evolution of oxide morphology of ultra-pure ferritic stainless steel at high temperatures is simulated, which solves the problem of difficulty in experimental observation, achieves rapid optimization of alloy composition and process, and improves high-temperature oxidation resistance. understanding and productivity.
Patent Information
- Application Number
- CN202410773947.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2024-10-01
AI Technical Summary
In high-temperature environments, it is extremely difficult to directly observe the evolution of surface and internal oxides on the surface of ultrapure ferritic stainless steel through experiments, resulting in serious delays in research, development, production and application. There is a lack of effective computer numerical simulation methods to accelerate new high-temperature resistant stainless steels. Ultra-pure ferritic stainless steel alloy composition design and process development.
Computer numerical simulation methods are used, including model geometry settings, boundary condition settings, mesh division, temperature field calculations, concentration field calculations, oxide nucleation calculations, growth kinetics calculations and other steps to simulate ultrapure ferrite stainless steel at high temperatures. The evolution process of surface and internal oxide morphologies in the environment, predicting and optimizing alloy composition and production process.
It realizes the intuitive description and prediction of the high-temperature oxidation behavior of ultra-pure ferritic stainless steel, quickly optimizes the alloy composition and process, and improves the understanding of high-temperature oxidation resistance and production efficiency.
Smart Images

Figure CN118737304A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of material numerical simulation, and relates to a computer numerical simulation method for high-temperature oxidation behavior of ultrapure ferrite stainless steel. Background Art
[0002] Ultrapure ferritic stainless steel refers to ferritic stainless steel with extremely low content of interstitial elements such as carbon and nitrogen (C+N≤0.03%). The thickness, composition and properties of the oxide generated on the surface of ultrapure ferritic stainless steel under high temperature environment play an important role in its surface quality control and application as a functional structural material.
[0003] In the hot rolling process, the oxide scale has a higher hardness than the matrix. Therefore, an oxide layer with a certain thickness can prevent the ultra-pure ferritic stainless steel matrix from direct contact with the working roll and protect it from damage from the roll or oxide scale fragments. At the same time, it plays a role in increasing rolling lubrication and reducing the phenomenon of rolling sticking.
[0004] The oxide scale produced during annealing needs to be removed in the subsequent pickling process and the substrate is passivated to produce a new passivation film. Accurately understanding the composition and structure of the annealing oxide scale and the depth of the subcutaneous chromium-poor area is the key to improving the energy efficiency of annealing and pickling, controlling the surface quality of stainless steel, and producing excellent corrosion-resistant products.
[0005] The welding process during the processing of ultra-pure ferritic stainless steel products is one of the key factors restricting its application. A deep understanding of the composition and evolution of the oxide layer in the heat-affected zone of welding plays an important guiding role in improving the corrosion resistance of the weld.
[0006] However, directly observing the evolution of the surface and internal oxides of ultra-pure ferritic stainless steel in high-temperature environments through experiments is not only extremely difficult but also extremely time-consuming and expensive, which has seriously delayed the research, development, and production application of advanced ferritic stainless steel materials with excellent high-temperature oxidation resistance.
[0007] Therefore, computer numerical simulation and prediction of the high-temperature oxidation behavior of ultra-pure ferritic stainless steel are of great significance for strengthening the deep understanding of the high-temperature oxidation behavior of stainless steel materials and accelerating the design optimization and process development of new high-temperature resistant ultra-pure ferritic stainless steel alloy compositions. Summary of the invention
[0008] The purpose of the present invention is to provide a computer numerical simulation method for the high temperature oxidation behavior of ultrapure ferritic stainless steel. Based on the theory of internal / external oxidation and selective oxidation of alloys, a computer program is used to simulate and intuitively describe the morphological evolution of surface oxides and internal oxides of ultrapure ferritic stainless steel under high temperature environment. The data simulated by the present invention can predict, analyze and optimize the alloy composition and production process of high temperature oxidation resistant ultrapure ferritic stainless steel.
[0009] The technical solution adopted by the present invention to achieve the above-mentioned purpose is:
[0010] A computer numerical simulation method for high temperature oxidation behavior of ultrapure ferrite stainless steel comprises the following steps:
[0011] S1. Model geometry setting, boundary condition setting and meshing: intercept a representative area of the ultrapure ferritic stainless steel to be analyzed, set the geometric size information of the simulation area to establish a geometric model, set the boundary conditions of the geometric area, and mesh the selected simulation area;
[0012] S2, model initialization, initializing parameters to the simulation area of the geometric model established in S1, the parameters are high temperature oxidation weight gain test conditions, including ambient temperature, oxygen concentration, oxidation time, thermophysical parameters and thermodynamic parameters of ultrapure ferritic stainless steel materials;
[0013] S3, temperature field calculation, setting the temperature field of the simulation area to a uniform temperature field, and assigning the temperature to the grid nodes of the grid divided into the simulation area described in S1;
[0014] S4, concentration field calculation, discretizing the concentration field equation to the grid nodes described in S3, and solving the concentration field distribution in the simulation area;
[0015] S5. Oxide nucleation calculation, establish the control equation of metal oxide nucleation in ultra-pure ferritic stainless steel under high temperature environment, and solve the nucleation process;
[0016] S6, judging whether the solute around the oxide crystal nucleus can provide sufficient solute to enable the oxide to grow, if it cannot provide sufficient solute to enable the oxide to grow, returning to S3;
[0017] S7, calculation of oxide growth kinetics. If it is determined that sufficient solute can be provided in S6 to allow the oxide to grow, then the growth rate control equation at the front edge of the metal oxide growth interface is established and solved;
[0018] S8, based on the ratio of the volume of the metal to its oxide, the volume of the metal oxide that completely occupies a single cell is expanded toward the air / oxide interface by the number of cells of the corresponding ratio to simulate the change caused by the difference between the volume of the metal oxide and the volume of the matrix;
[0019] S9, calculation of oxidation increment per unit area, updating of temperature field, concentration field, metal oxidation volume fraction in the simulation area, and output of oxidation weight gain data per unit area;
[0020] S10, judging whether the simulation time reaches the set oxidation time, if not, repeating S3 to S8, and completing the simulation when the set oxidation time is reached.
[0021] The technical solution of the present invention has the following beneficial effects:
[0022] The present invention can intuitively describe the morphological evolution process of surface oxides and internal oxides of ultrapure ferritic stainless steel under high temperature environment;
[0023] The present invention can use simulation results to quickly predict, analyze and optimize the alloy composition and production process of high-temperature oxidation-resistant ultra-pure ferritic stainless steel. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 is a flow chart of the method of the present invention;
[0025] Figure 2 This is the simulation result of high temperature oxide layer of ultrapure ferritic stainless steel at 1123K;
[0026] Figure 3 This is the experimental result of high temperature oxide layer of ultrapure ferritic stainless steel at 1123K;
[0027] Figure 4 It is the time evolution process of the high temperature oxide layer of ultra-pure ferritic stainless steel simulated at 1073K.
[0028] Figure 5 This is the simulation result of high temperature oxide layer of ultrapure ferritic stainless steel at 1073K;
[0029] Figure 6 It is the simulated curve of the mass increase of ultra-pure ferritic stainless steel during high temperature oxidation over time;
[0030] Figure 7 This is the simulated curve of the high-temperature oxidation mass increase rate of ultra-pure ferritic stainless steel changing with time. DETAILED DESCRIPTION
[0031] The method of the present invention is further described below in conjunction with embodiments and drawings:
[0032] Embodiment 1:
[0033] The computer numerical simulation of the high temperature oxidation behavior of ultrapure ferritic stainless steel includes the following steps:
[0034] S1. The geometric model area size of the simulation using orthogonal meshing is 20μm×8μm×2μm, and the boundary conditions are set as periodic boundary conditions;
[0035] S2, the initialization environment temperature is 1123K, the oxygen concentration is 21%, the oxidation time is 10min, and the alloy composition of the ultra-pure ferritic stainless steel material is: C: 0.0046wt%, N: 0.0093wt%, Cr: 18.9wt%, Ti: 0.004wt%, Al: 0.04wt%, Si<0.05wt%, Mn: <0.05wt%, P: <0.01wt%, S: <0.0003wt%. The thermodynamic parameters of the material are calculated and input by Thermo-Calc software. The material physical properties are shown in Table 1.
[0036] S3, the temperature field of the simulation area is set to a uniform temperature of 1123K;
[0037] S4, discretize the concentration field equation based on Fick's second law and the finite volume method (FVM), and use the tridiagonal matrix (TDMA) solution method to solve the concentration field equation implicitly and iteratively;
[0038] S5. Based on the experimentally observed oxide grain size, the control algorithm of metal oxide nucleation process is established in combination with the classical nucleation theory: the nucleation probability P of a single cell is i Set to P i =I i / ∑I i ,i=1,…,n CA Where, I i is the nucleation rate of metal oxide in the ith unit cell, n CA is the total number of cells in the calculation area; when P i ≥Δn v / n CA , and when the number of nuclei is greater than 1, a new crystal nucleus can be formed there; where Δn v is the number of grains that will be generated within the iteration time interval; the total number of grains is obtained by inferring the experimentally determined grain size.
[0039] S6. Determine the sum of the solutes at the 51 nodes adjacent to the three-dimensional region around the oxide nucleus Whether sufficient solute can be provided to allow the oxide to grow to the next stage, and the solute required for growth ΔC g ,Right now If yes, proceed to the next step, otherwise return to S3; is the coordinate distance from the oxide nucleus , Δx is the size of a single grid / cell.
[0040] S7. Establish and solve the growth rate control equation of the metal oxide growth interface front;
[0041] S8. Based on the ratio of the metal volume to the oxide volume (PBR value), the volume of the metal oxide that completely occupies a single cell is expanded toward the air / oxide interface by a corresponding ratio of the cell unit to simulate the expansion of the metal oxide volume: PBR_Cr2O3≈2.0, PBR_Al2O3≈1.0;
[0042] S9, updating the temperature field, concentration field, and volume fraction of metal oxides in the simulation area, and outputting the oxidation weight gain data per unit area;
[0043] S10, judging whether the simulation time reaches the set oxidation time, if not, continue to repeat S3 to S8, if yes, end the simulation. Finally, use data processing software to process the simulated data.
[0044] The simulation results of Example 1 are as follows Figure 2 As shown in the experimental results, Figure 3 The comparison shown is basically consistent.
[0045] Example 2
[0046] The computer numerical simulation of the high temperature oxidation behavior of ultrapure ferritic stainless steel includes the following steps:
[0047] S1. The geometric model area size of the simulation using orthogonal meshing is 20μm×8μm×2μm, and the boundary conditions are set as periodic boundary conditions;
[0048] S2, the initialization environment temperature is 1073K, the oxygen concentration is 21%, the oxidation time is 10min, and the alloy composition of the ultra-pure ferritic stainless steel material is: C: 0.0046wt%, N: 0.0093wt%, Cr: 18.9wt%, Ti: 0.004wt%, Al: 0.04wt%, Si<0.05wt%, Mn: <0.05wt%, P: <0.01wt%, S: <0.0003wt%; the material thermodynamic parameters are calculated and input by Thermo-Calc software. The material physical properties are shown in Table 1.
[0049] S3, the temperature field of the simulation area is set to a uniform temperature of 1123K;
[0050] S4, discretize the concentration field equation based on Fick's second law and finite volume method (FVM), and use the tridiagonal matrix (TDMA) solution method to solve the concentration field equation implicitly and iteratively;
[0051] S5. Based on the experimentally observed oxide grain size, the metal oxide nucleation process control algorithm is established in combination with the classical nucleation theory: the nucleation probability P of a single cell is i Set to P i =I i / ∑Ii ,i=1,…,n CA In the formula, I i is the nucleation rate of metal oxide in the ith unit cell, n CA is the total number of cells in the calculation area; when P i ≥Δn v / n CA , and when the number of nuclei is greater than 1, a new crystal nucleus can be formed there; where Δn v is the number of grains that will be generated within the iteration time interval; the total number of grains is obtained by inferring the experimentally determined grain size.
[0052] S6. Determine the sum of the solutes at the 51 nodes adjacent to the three-dimensional region around the oxide nucleus Whether sufficient solute can be provided to allow the oxide to grow to the next stage, and the solute required for growth ΔC g ,Right now If yes, proceed to the next step, otherwise return to S3; is the coordinate distance from the oxide nucleus , Δx is the size of a single grid / cell.
[0053] S7. If the solute around the oxide nucleus can provide sufficient solute to allow the oxide to grow, then establish the growth rate control equation at the front edge of the metal oxide growth interface and solve it;
[0054] S8. Based on the ratio of the metal volume to the oxide volume (PBR value), the volume of the metal oxide that completely occupies a single cell is expanded toward the air / oxide interface by a corresponding ratio of the cell unit to simulate the expansion of the metal oxide volume: PBR_Cr2O3≈2.0, PBR_Al2O3≈1.0;
[0055] S9, updating the temperature field, concentration field, and metal oxidation volume fraction in the simulation area, and outputting the oxidation weight gain data per unit area;
[0056] S10, judging whether the simulated oxidation time reaches the set oxidation time, if not, continue to repeat S3 to S8, if yes, end the simulation.
[0057] Finally, the simulated data are processed using data processing software.
[0058] The simulation results of Example 2 are as follows Figure 4 As shown, the process of the surface oxide layer of ultra-pure ferritic stainless steel from formation to covering the entire surface is intuitively described. Figure 5 It shows the alloy composition and oxide distribution after the surface of ultra-pure ferritic stainless steel is completely covered by oxides.
[0059] The high temperature oxide weight gain curves of ultrapure ferrite stainless steel in Example 1 and Example 2 are as follows: Figure 6 As shown, the high temperature oxide weight gain rate curve of ultra-pure ferrite stainless steel is as follows Figure 7 shown.
[0060] Table 1 Material properties used in the simulation
[0061]
Claims
1. A computer numerical simulation method for high temperature oxidation behavior of ultrapure ferritic stainless steel, Features: The following steps are involved: S1. Model geometry setting, boundary condition setting and meshing: intercept a representative area of the ultrapure ferritic stainless steel to be analyzed, set the geometric size information of the simulation area to establish a geometric model, set the boundary conditions of the geometric area, and mesh the selected simulation area; S2. Model initialization: initializing parameters to the simulation area of the geometric model established in S1. The parameters are high-temperature oxidation weight gain test conditions, including ambient temperature, oxygen concentration, oxidation time, thermophysical parameters of ultrapure ferritic stainless steel materials, and thermodynamic parameter information calculated by third-party thermodynamic software; S3, temperature field calculation, setting the temperature field of the simulation area to a uniform temperature field, and assigning the temperature to the grid nodes of the grid divided into the simulation area described in S1; S4, concentration field calculation, discretizing the concentration field equation to the grid nodes described in S3, and solving the concentration field distribution in the simulation area; S5. Oxide nucleation calculation, establish the control equation of metal oxide nucleation in ultra-pure ferritic stainless steel under high temperature environment, and solve the nucleation process; S6, judging whether the solute around the oxide crystal nucleus can provide sufficient solute to enable the oxide to grow, if it cannot provide sufficient solute to enable the oxide to grow, returning to S3; S7, calculation of oxide growth kinetics. If it is determined that sufficient solute can be provided in S6 to allow the oxide to grow, then the growth rate control equation at the front edge of the metal oxide growth interface is established and solved; S8, according to the ratio of the volume of the metal of the oxide to its oxide, the volume of the metal oxide that completely occupies a single cell is expanded toward the air / oxide interface by a cell unit of a corresponding ratio to simulate the expansion of the metal oxide volume; S9, calculating the oxidation increment per unit area, updating the temperature field, concentration field, and metal oxidation volume fraction information of the simulation area, and outputting the oxidation weight gain data per unit area; S10, judging whether the simulation time reaches the set oxidation time, if not, continuing to repeat S3 to S8, and ending the simulation when the set oxidation time is reached.
2. A computer numerical simulation method for high temperature oxidation behavior of ultrapure ferritic stainless steel according to claim 1, Features: The geometric size range of the region in S1 is 1 nm to 1 mm, and the boundary condition of the geometric region is a periodic boundary.
3. A computer numerical simulation method for high temperature oxidation behavior of ultrapure ferritic stainless steel according to claim 1, Features: The temperature of the S2 medium-high temperature oxidation environment ranges from 973K to 1473K, and the oxygen concentration ranges from 0-100%.
4. The computer numerical simulation method for high temperature oxidation behavior of ultrapure ferritic stainless steel according to claim 1, Features: The composition range of the ultrapure ferritic stainless steel in S2 is: C: <0.015wt%, N: <0.015wt%, Cr: 14.0-30.0wt%, Ti: <1.0wt%, Nb: <1.0wt%, Al: <1.0wt%, Si: <1.0wt%, Mn: <1.0wt%, P: <0.04wt%, S: <0.03wt%, Ni: <6.0wt%, Mo: <6.0wt%.
5. The computer numerical simulation method for high temperature oxidation behavior of ultrapure ferritic stainless steel according to claim 1, Features: The metal oxide nucleation control algorithm in the ultrapure ferritic stainless steel under high temperature environment established in S5 is: the nucleation probability P of a single cell is i Set to P i =I i / ∑I i ,i=1,…,n CA Where, I i is the nucleation rate of metal oxide in the ith unit cell, n CA is the total number of cells in the calculation area; when P i ≥Δn v / n CA , and when the number of nuclei is greater than 1, a new crystal nucleus can be formed there; where Δn v is the number of grains that will be generated within the iteration time interval; the total number of grains is obtained by inferring the experimentally determined grain size.
6. The computer numerical simulation method for high temperature oxidation behavior of ultrapure ferritic stainless steel according to claim 1, Features: The algorithm for determining whether the solute around the oxide crystal nucleus can provide sufficient solute in S6 is: the sum of the solutes at the 51 nodes adjacent to the three-dimensional region around the oxide crystal nucleus is determined. Whether sufficient solute can be provided to allow the oxide to grow to the next stage, and the solute required for growth ΔC g ,Right now If yes, proceed to the next step, otherwise return to S3; is the coordinate distance from the oxide nucleus , Δx is the size of a single grid / cell.
Citation Information
Patent Citations
Ultra-pure ferritic stainless steel smelting method
CN113106322A
Numerical simulation method for microstructure evolution of magnesium alloy selective laser melting
CN113807033A
Numerical simulation method for predicting liquid / liquid two-phase interface reaction phase change process
CN114141313A
Systems and methods for multi-purpose analysis
US20130078624A1