Wafer packaging structure, power device and bonding method of wafer packaging structure
By setting an elastic transition layer in the nanomaterial film and optimizing the design of the nanomaterial layer, the problem of wafer warpage and deformation is solved, the thermal resistance management and reliability of the device are improved, and the application of low-temperature bonding technology is promoted.
Patent Information
- Application Number
- CN202410772567.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-14
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-06-14
AI Technical Summary
Traditional low-temperature bonding technology causes serious warping and deformation of the wafer during the entire wafer packaging process of GCT power devices, affecting the thermal resistance optimization effect and reliability.
A transition layer with elastic deformation capability is provided in the nanomaterial film. The transition layer absorbs the warpage deformation stress of the wafer, releases the warpage deformation stress, reduces the degree of warpage deformation, and optimizes the thickness and particle size distribution of the nanomaterial layer. Increase the elastic modulus of a specific area.
It effectively reduces the degree of wafer warpage and deformation, improves the thermal resistance management and long-term reliability of the device, and promotes the application of low-temperature bonding technology in the field of whole-wafer packaging.
Smart Images

Figure CN118738003A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of semiconductor devices, and in particular to a wafer packaging structure, a power device, and a bonding method for a wafer packaging structure. Background Art
[0002] Integrated Gate-Commutated Thyristor (IGCT), as the fully controlled power device with the largest single-tube capacity, is widely used in DC transmission, smart grid, power converter, power inverter and other fields. With the continuous improvement of IGCT device power level, higher requirements are placed on the thermal resistance of device packaging, requiring more effective device heat management.
[0003] At present, the whole wafer of GCT power devices is usually packaged through nano-silver low-temperature bonding technology, while the traditional low-temperature bonding technology uses silver film and silver paste to coat the whole wafer for packaging. However, the degree of wafer warping and deformation after bonding is serious, which seriously affects the thermal resistance optimization effect and reliability of the wafer.
[0004] Therefore, how to reduce the degree of wafer warping and deformation during the bonding process has become an urgent problem to be solved in the current field of semiconductor technology. Summary of the invention
[0005] Based on this, it is necessary to provide a wafer packaging structure, a power device and a bonding method for a wafer packaging structure that can reduce the degree of wafer warping deformation in order to address the above technical problems.
[0006] In a first aspect, the present application provides a wafer packaging structure, which includes: a cathode metal sheet, a wafer, a nanomaterial film and an anode metal sheet stacked in sequence; the nanomaterial film includes at least one transition layer; the material of the transition layer is an elastic material.
[0007] In one embodiment, the surface of the transition layer close to the wafer is convex.
[0008] In one embodiment, the surface of the transition layer close to the anode metal sheet is convex.
[0009] In one embodiment, the thickness of the transition layer is 50-100 microns; the difference in thickness between the thickness of the middle protrusion of the convex surface and the thickness of the two edges is 20-50 microns.
[0010] In one embodiment, the material of the transition layer includes a metal material with conductive properties; preferably, the metal material with conductive properties includes at least one of a silver foil material and a copper foil surface-plated silver material.
[0011] In one embodiment, the nanomaterial film further includes at least two nanomaterial layers; each transition layer is disposed between two adjacent nanomaterial layers.
[0012] In one embodiment, the nanomaterial layer has different particle sizes.
[0013] In one embodiment, the nano material layer includes a central region and an edge region; the particle size of the material in the edge region gradually increases in a direction away from the central region.
[0014] In one embodiment, the particle size of the material in the central area is 0.05-0.1 micrometers; the particle size of the material in the edge area is 0.5-1 micrometers.
[0015] In one embodiment, the thickness of the nanomaterial layer is 75-50 microns.
[0016] In one embodiment, the material of the nanomaterial layer includes a second metal material with conductive properties; preferably, the second metal material with conductive properties includes at least one of nanosilver material, nanocopper material, and nanosilver / copper composite material.
[0017] In a second aspect, the present application further provides a power device, which includes a packaging structure as in any one of the embodiments of the first aspect.
[0018] In a third aspect, the present application further provides a method for bonding a wafer packaging structure, the method being applied to a packaging structure as in any one of the embodiments of the first aspect, the method comprising:
[0019] Through a preset coating process, the nano material layer and the transition layer are coated on the surface of the wafer close to the anode metal sheet in an alternating manner to form a nano material film;
[0020] Bonding the structure consisting of the coated wafer and the nano material film at a first preset pressure and a first preset temperature;
[0021] coating an anode metal sheet on the surface of the nanomaterial film facing away from the wafer;
[0022] The structure consisting of the coated wafer, the nano material film and the anode metal sheet is set at a second preset pressure and a second preset temperature for bonding.
[0023] The wafer packaging structure, power device and bonding method of the wafer packaging structure are as follows: the packaging structure includes a cathode metal sheet, a wafer, a nanomaterial film and an anode metal sheet stacked in sequence; the nanomaterial film includes at least one transition layer; the material of the transition layer is an elastic material. In the packaging structure, by arranging a transition layer with elastic deformation ability in the nanomaterial film, the transition layer can absorb the warping deformation stress of the wafer to release the warping deformation stress, thereby achieving the effect of reducing the degree of warping deformation, further reducing the thermal resistance of the device, improving the long-term reliability of the device, and promoting the application of low-temperature bonding technology in the field of whole wafer packaging. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the technical solutions in the embodiments of the present application or the conventional technology, the drawings required for use in the embodiments or the conventional technology descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0025] Figure 1 is a schematic diagram of a wafer packaging structure in one embodiment;
[0026] Figure 2 is a schematic diagram of the structure of a transition layer in one embodiment;
[0027] Figure 3 A schematic diagram of the structure of a nanomaterial film in one embodiment;
[0028] Figure 4 A top view of the structure of a nanomaterial layer in one embodiment;
[0029] Figure 5 A bonding method for a wafer packaging structure in an embodiment;
[0030] Description of reference numerals:
[0031] Cathode metal sheet 10; Wafer 20; Nano material film 30;
[0032] Anode metal sheet 40; Transition layer 301; Nano material layer 302;
[0033] Central area 3021; Edge area 3022. DETAILED DESCRIPTION
[0034] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are given in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.
[0035] It should be understood that when an element or layer is referred to as being "connected to," it may be directly connected to other elements or layers, or there may be intervening elements or layers. It should be understood that although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, doping types, and / or portions, these elements, components, regions, layers, doping types, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, doping type, or portion from another element, component, region, layer, doping type, or portion.
[0036] Spatial relational terms such as "above..." may be used herein to describe the relationship of one element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, spatial relational terms also include different orientations of the device in use and operation. For example, if the device in the drawings is flipped, the feature described as "above..." will be oriented "below...". Therefore, the exemplary term "above..." may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.
[0037] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that when the terms "consisting of" and / or "comprising" are used in this specification, the presence of the features, integers, steps, operations, elements and / or parts can be determined, but the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups is not excluded. At the same time, when used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0038] Unless otherwise defined, the technical terms or scientific terms involved in this application should be understood by people with ordinary skills in the technical field to which this application belongs. The words "one", "a", "a", "the" and the like involved in this application do not indicate a quantitative limitation and may represent the singular or plural. The terms "including", "comprising", "having" and any of their variations involved in this application are intended to cover non-exclusive inclusions; for example, a process, method, system, product or device that includes a series of steps or modules (units) is not limited to the listed steps or units, but may also include unlisted steps or units, or may also include other steps or units inherent to these processes, methods, products or devices. The "multiple" involved in this application means greater than or equal to two. "And / or" describes the association relationship of associated objects, indicating that there may be three relationships, for example, "A and / or B" can represent: A exists alone, A and B exist at the same time, and B exists alone. The terms "first", "second" and the like involved in this application are only used to distinguish similar objects and do not represent a specific ordering of objects.
[0039] First of all, before specifically introducing the technical solution of the embodiment of the present disclosure, the technical background or technical evolution context on which the embodiment of the present disclosure is based is introduced. As a fully controlled power device with the largest single-tube capacity, the integrated gate-commutated thyristor device (IGCT) is widely used in DC transmission, smart grid, power converter, power inverter and other fields. With the continuous improvement of the power level of IGCT devices, higher requirements are put forward for the thermal resistance of device packaging, and the heat of the device needs to be managed more effectively. At present, the whole wafer of the GCT power device is usually packaged by nano-silver low-temperature bonding technology, while the traditional low-temperature bonding technology is to use nano-material film and silver paste to coat the whole wafer for packaging. However, the degree of wafer warping and deformation after bonding is serious, which seriously affects the thermal resistance optimization effect and reliability of the wafer. Therefore, how to reduce the degree of wafer warping and deformation during the bonding process has become a problem to be solved in the current field of semiconductor technology.
[0040] The present application provides a wafer packaging structure, such as Figure 1 As shown, the packaging structure includes: a cathode metal sheet 10, a wafer 20, a nano material film 30 and an anode metal sheet 40 stacked in sequence; the nano material film 30 includes at least one transition layer 301; the material of the transition layer 301 is an elastic material.
[0041] The elastic material has a certain elastic deformation capability and is used to absorb the warping deformation stress of the wafer 20. The elastic material is a highly elastic metal and its composite material with a certain electrical and thermal conductivity. The elastic modulus of the elastic material can be set according to actual needs.
[0042] The thickness of the above-mentioned transition layer 301 is 50-100 microns. The material of the transition layer 301 is a material that can be directly pre-sintered with nanosilver, including a metal material with conductive properties; preferably, the metal material with conductive properties includes at least one of a silver foil material and a copper foil surface-plated silver material. The material selection of the transition layer 301 must follow the principle of being able to complete the bonding process. Specifically, the material of the transition layer 301 and the surface metallization material are selected based on the principle of being bondable with the nanomaterial layer. It is preferably the same material as the nanomaterial layer or a gold material with excellent performance. The specific material type can be set according to actual needs. Among them, the nanomaterial layer is the material layer to be bonded with the transition layer 301. The shapes of the upper surface and the lower surface of the transition layer 301 can be the same or different.
[0043] The packaging structure of the wafer provided in the embodiment of the present application, by setting a transition layer with elastic deformation ability in the nanomaterial film, can absorb the warping deformation stress of the wafer through the transition layer to release the warping deformation stress, thereby achieving the effect of reducing the degree of warping deformation, thereby further reducing the thermal resistance of the device, improving the long-term reliability of the device, and promoting the application of low-temperature bonding technology in the field of whole wafer packaging.
[0044] In one embodiment, the surface of the transition layer 301 close to the wafer 20 is convex and / or the surface of the transition layer 301 close to the anode metal sheet 40 is convex.
[0045] The surface of the transition layer 301 close to the wafer 20 is the upper surface of the transition layer 301 , and the surface of the transition layer 301301 close to the anode metal sheet 40 is the lower surface of the transition layer 301 .
[0046] In the embodiment of the present application, the upper surface of the transition layer 301 can be a plane or a convex surface; the lower surface of the transition layer 301 can be a plane or a convex surface. There are four situations. The first one is that the upper surface and the lower surface of the transition layer 301 are both planes; the second one is that the upper surface and the lower surface of the transition layer 301 are both convex surfaces. For details, please refer to Figure 2 The transition layer 301 structure shown in the figure; the third type, the upper surface of the transition layer 301 is a plane, and the lower surface is a convex surface; the fourth type, the upper surface of the transition layer 301 is a convex surface, and the lower surface is a plane. In the packaging structure described in the embodiment of the present application, by setting the surface of the transition layer to a convex surface, since the convex direction of the convex surface is opposite to the direction of the wafer warping deformation, when the wafer is about to warp, the convex surface can offset the wafer warping deformation stress, thereby achieving the effect of reducing the degree of warping deformation.
[0047] In one embodiment, the nanomaterial film 30 further includes at least two nanomaterial layers 302 ; each transition layer 301 is disposed between two adjacent nanomaterial layers 302 .
[0048] The thickness of the nano material layer 302 is 75-50 microns. The material of the nano material layer 302 includes a second metal material with conductive properties; preferably, the second metal material with conductive properties includes at least one of nano silver material, nano copper material and nano silver composite material. For example, the nano material film 30 can be a silver film. The nano material layer 302 is printed on both sides of the transition layer 301.
[0049] In the embodiment of the present application, the nano material film may be composed of at least one transition layer 301 and a nano material layer 302, for example, Figure 3 As shown, the nanomaterial film can be a "sandwich structure", which includes nanomaterial layer 302-transition layer 301-nanomaterial layer 302 in sequence. Optionally, it can also be a multilayer structure, which includes nanomaterial layer 302-transition layer 301-nanomaterial layer 302-transition layer 301-...-nanomaterial layer 302 in sequence. Optionally, it can also include nanomaterial layer 302-transition layer 301-transition layer 301-...-transition layer 301-nanomaterial layer 302 in sequence. The above packaging structure can release the warpage stress by increasing the overall thickness of the entire nanomaterial.
[0050] In one embodiment, the particle sizes of the nanomaterial layer are not uniform.
[0051] In the embodiment of the present application, the setting of the material particle size of the nano material layer needs to be aimed at reducing the degree of wafer warpage deformation, and can be specifically determined according to the degree of wafer warpage deformation at each position. Optionally, the middle material particle size of the nano material layer can be larger or smaller than the edge material particle size. Optionally, the material particle size of the nano material layer can gradually increase or decrease from the middle to the edge, showing a gradual change process.
[0052] Preferably, the nanomaterial layer 302 includes a central region 3021 and an edge region 3022; the particle size of the material in the edge region 3022 gradually increases in the direction away from the central region 3021. The particle size of the material in the central region is 0.05-0.1 microns; the particle size of the material in the edge region is 0.5-1 microns. The shapes of the central region 3021 and the edge region 3022 can be circular, square, or polygonal. The specific shapes are set according to actual needs and are not limited in the embodiments of the present application. For example, Figure 4The top view of the nano material layer 302 is shown, wherein the central area 3021 and the edge area 3022 are both circular, wherein the central area 3021 is a dense ring and the edge area 3022 is a loose ring. The packaging structure described in the embodiment of the present application optimizes the radial looseness / density of the nano material, increases the elastic modulus of a specific area, and releases the warping deformation stress. The material particle size of the nano material layer can be that the material particle size of the middle layer is smaller than that of the edge layer, and the material particle size gradually increases from the middle to the edge. The material particle size at a specific position is
[0053] Based on the wafer packaging structures described in all the above embodiments, the present application further provides a wafer packaging structure, which includes: a cathode metal sheet 10, a wafer 20, a nano material film 30 and an anode metal sheet 40 stacked in sequence;
[0054] The nanomaterial film 30 includes at least one transition layer. The material of the transition layer 301 is an elastic material. The elastic material has a certain elastic deformation ability and is used to absorb the warping deformation stress of the wafer 20. The elastic modulus of the elastic material can be set according to actual needs. The surface of the transition layer 301 close to the wafer 20 is a convex surface, and the surface of the transition layer 301 close to the anode metal sheet 40 is a convex surface. The thickness difference between the thickness of the middle convex surface and the thickness of the two edges is 20-50 microns, and the thickness of the transition layer 301 is 50-100 microns. The material of the transition layer 301 is a material that can be directly pre-sintered with nanosilver, including a metal material with conductive properties; preferably, the metal material with conductive properties includes at least one of a silver foil material and a copper foil surface silver-plated material. The shape of the upper surface of the transition layer 301 can be the same or different. The upper surface of the transition layer 301 can be a plane or a convex surface; the lower surface of the transition layer 301 can be a plane or a convex surface. There are four situations. The first one is that both the upper surface and the lower surface of the transition layer 301 are planes. The second one is that both the upper surface and the lower surface of the transition layer 301 are convex. The third one is that the upper surface of the transition layer 301 is plane and the lower surface is convex. The fourth one is that the upper surface of the transition layer 301 is convex and the lower surface is plane.
[0055] The nano material film 30 also includes at least two nano material layers 302, each transition layer 301 is arranged between each two adjacent nano material layers 302, and the nano material layer 302 includes a central area 3021 and an edge area 3022. The material particle size of the edge area 3022 gradually increases in the direction away from the central area 3021. The material particle size of the central area 3021 is 0.05-0.1 microns, and the material particle size of the edge area 3022 is 0.5-1 microns. The shapes of the central area 3021 and the edge area 3022 can be circular, square, or polygonal. The specific shapes are set according to actual needs and are not limited in the embodiment of the present application. The thickness of the nano material layer 302 is 75-50 microns, and the material of the nano material layer 302 includes a second metal material with conductive properties; preferably, a second metal material with conductive properties. The nano material film can be a "sandwich structure", which includes a nano material layer 302-transition layer 301-nano material layer 302 in sequence. Optionally, it can also be a multilayer structure, which sequentially includes nano material layer 302-transition layer 301-nano material layer 302-transition layer 301-…-nano material layer 302. Optionally, it can also sequentially include nano material layer 302-transition layer 301-transition layer 301-…-transition layer 301-nano material layer 302.
[0056] The packaging structure described in the embodiment of the present application, by setting a transition layer with elastic deformation ability in the nano material film, can absorb the wafer warping deformation stress through the transition layer to release the warping deformation stress, so as to achieve the effect of reducing the degree of warping deformation, thereby further reducing the thermal resistance of the device, improving the long-term reliability of the device, and promoting the application of low-temperature bonding technology in the whole wafer packaging field. By setting the surface of the transition layer as a convex surface, since the convex direction of the convex surface is opposite to the direction of the wafer warping deformation, when the wafer is about to produce warping deformation, the convex surface can offset the wafer warping deformation stress, thereby achieving the effect of reducing the degree of warping deformation. By increasing the overall thickness of the whole nano material, the warping deformation stress can be released. By optimizing the radial looseness / density of the nano material, the elastic modulus of a specific area is increased, and the warping deformation stress is released.
[0057] Based on the wafer packaging structure described in all the above embodiments, the present application also provides a power device, which includes the packaging structure of any one of the above embodiments.
[0058] The power device described in the embodiment of the present application, by setting a transition layer with elastic deformation ability in the nano material film in the packaging structure, can absorb the wafer warping deformation stress through the transition layer to release the warping deformation stress, so as to achieve the effect of reducing the degree of warping deformation, thereby further reducing the thermal resistance of the device, improving the long-term reliability of the device, and promoting the application of low-temperature bonding technology in the whole wafer packaging field. By setting the surface of the transition layer as a convex surface, since the convex direction of the convex surface is opposite to the direction of the wafer warping deformation, when the wafer is about to produce warping deformation, the convex surface can offset the wafer warping deformation stress, thereby achieving the effect of reducing the degree of warping deformation. By increasing the overall thickness of the whole nano material, the warping deformation stress can be released. By optimizing the radial looseness / density of the nano material, the elastic modulus of a specific area is increased, and the warping deformation stress is released.
[0059] Based on the wafer packaging structures described in all the above embodiments, the present application also provides a bonding method for a wafer packaging structure, which is applied to the packaging structure of any of the above embodiments, such as Figure 5 As shown, the method includes:
[0060] S101, through a preset coating process, the nano material layer and the transition layer are coated on the surface of the wafer close to the anode metal sheet in an alternating manner to form a nano material film to achieve a pre-bonding operation.
[0061] S102, setting the structure consisting of the coated wafer and the nano material film at a first preset pressure and a first preset temperature for bonding.
[0062] S103, coating an anode metal sheet on the surface of the nanomaterial film facing away from the wafer.
[0063] S104, setting the structure consisting of the coated wafer, the nanomaterial film and the anode metal sheet at a second preset pressure and a second preset temperature for bonding.
[0064] The preset coating process may be to coat the nanomaterial layer on the surface of the transition layer by screen printing. The first preset pressure and the second preset pressure may be the same or different. The first preset temperature and the second preset temperature may be the same or different. The process parameters may be: 150-180°C / 3-5MPa / 30-60s. The pre-bonded nanomaterial film may be stored in a vacuum.
[0065] In the embodiment of the present application, the anode metal sheet / wafer can be assembled by a specially designed fixture, and a low-temperature bonding process can be completed using specific bonding equipment.
[0066] Optionally, a nano material film (e.g., a silver film) may be prepared in advance, and then the prepared nano material film may be used to complete the wafer packaging process. Specifically, the following steps may be included: first, the nano material is coated on the transition layer by heating and pressurizing bonding to complete the preparation of the silver film. Then, the surface of the anode metal sheet is metallized. The metallization material in this process may be a material that can be wetted by a composite silver film material such as silver or gold. Finally, the anode metal sheet, the silver film, and the wafer are bonded to realize the wafer packaging process.
[0067] The bonding method of the wafer packaging structure described in the embodiment of the present application is to coat the surface of the wafer near the anode metal sheet with the nano material layer and the transition layer in an alternating stacking manner through a preset coating process to form a nano material film to achieve a pre-bonding operation, and then set the structure composed of the coated wafer and the nano material film at a first preset pressure and a first preset temperature for bonding, and then coat the anode metal sheet on the surface of the nano material film away from the wafer, and finally set the structure composed of the coated wafer, the nano material film and the anode metal sheet at a second preset pressure and a second preset temperature for bonding. In the above method, by setting a transition layer with elastic deformation ability in the nano material film in the packaging structure, the transition layer can absorb the warping deformation stress of the wafer to release the warping deformation stress, thereby achieving the effect of reducing the degree of warping deformation, thereby further reducing the thermal resistance of the device, improving the long-term reliability of the device, and promoting the application of low-temperature bonding technology in the field of whole wafer packaging. By setting the surface of the transition layer to a convex surface, since the convex direction is opposite to the direction of the wafer warpage, when the wafer is about to warp, the convex surface can offset the wafer warpage stress and reduce the degree of warpage. By increasing the overall thickness of the nanomaterial, the warpage stress can be released. By optimizing the radial looseness / density of the nanomaterial, the elastic modulus of a specific area is increased to release the warpage stress.
[0068] It should be understood that, although the various steps in the flowcharts involved in the above-mentioned embodiments are displayed in sequence according to the indication of the arrows, these steps are not necessarily executed in sequence according to the order indicated by the arrows. Unless there is a clear explanation in this article, the execution of these steps does not have a strict order restriction, and these steps can be executed in other orders. Moreover, at least a part of the steps in the flowcharts involved in the above-mentioned embodiments can include multiple steps or multiple stages, and these steps or stages are not necessarily executed at the same time, but can be executed at different times, and the execution order of these steps or stages is not necessarily to be carried out in sequence, but can be executed in turn or alternately with other steps or at least a part of the steps or stages in other steps.
[0069] In the description of this specification, the description with reference to the terms "some embodiments", "other embodiments", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic description of the above terms does not necessarily refer to the same embodiment or example.
[0070] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0071] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the present application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.
Claims
1. A wafer packaging structure, characterized in that: The packaging structure comprises: a cathode metal sheet, a wafer, a nano material film and an anode metal sheet stacked in sequence; the nano material film comprises at least one transition layer; the material of the transition layer is an elastic material.
2. The packaging structure according to claim 1, characterized in that: The surface of the transition layer close to the wafer is convex.
3. The packaging structure according to claim 1, characterized in that: The surface of the transition layer close to the anode metal sheet is convex.
4. The packaging structure according to claim 2, characterized in that: The thickness of the transition layer is 50-100 microns; the difference between the thickness of the middle protrusion of the convex surface and the thickness of the two edges is 20-50 microns.
5. The packaging structure according to claim 1, characterized in that: The material of the transition layer includes a first metal material with conductive properties; preferably, the first metal material with conductive properties includes at least one of a silver foil material and a copper foil surface-plated silver material.
6. The packaging structure according to any one of claims 1 to 5, characterized in that: The nano material film also includes at least two nano material layers; each transition layer is arranged between two adjacent nano material layers.
7. The packaging structure according to claim 6, characterized in that: The material particle sizes of the nano material layer are inconsistent.
8. The packaging structure according to claim 7, characterized in that: The nano material layer includes a central area and an edge area; the material particle size of the edge area gradually increases in a direction away from the central area.
9. The packaging structure according to claim 8, characterized in that: The particle size of the material in the central area is 0.05-0.1 micrometers; the particle size of the material in the edge area is 0.5-1 micrometers.
10. The packaging structure according to claim 6, characterized in that: The thickness of the nano material layer is 75-50 microns.
11. The packaging structure according to claim 6, characterized in that: The material of the nano material layer includes a second metal material with conductive properties; preferably, the second metal material with conductive properties includes at least one of nano silver material, nano copper material, and nano silver / copper composite material.
12. A power device, characterized in that: The power device comprises a packaging structure as claimed in any one of claims 1 to 11.
13. A bonding method for a wafer packaging structure, characterized in that: The method is applied to the packaging structure according to any one of claims 1 to 11, and the method comprises: Through a preset coating process, the nano material layer and the transition layer are coated on the surface of the wafer close to the anode metal sheet in an alternating manner to form a nano material film; Bonding the coated wafer and the structure formed by the nano material film at a first preset pressure and a first preset temperature; Coating the anode metal sheet on the surface of the nanomaterial film facing away from the wafer; The structure consisting of the coated wafer, the nano material film and the anode metal sheet is set at a second preset pressure and a second preset temperature for bonding.
Citation Information
Patent Citations
Sintered silver preformed sheet and preparation method thereof
CN115132590A
Semiconductor device and connection structure, and manufacturing methods thereof
JP2014003339A