Semiconductor device structure and manufacturing method thereof

By forming an electrically connected multi-layer conductive via structure on the substrate, the aspect ratio problem in the through silicon via process is solved, efficient device design is achieved, and the requirements for high aspect ratio and device performance are met.

CN118738020APending Publication Date: 2024-10-01SHANGHAI MICROWELL ELECTRONIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410800670.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-20
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

The existing through silicon via process encounters problems such as difficulty in etching, rough sidewalls, and filling of voids when achieving high aspect ratios, and reducing the process difficulty by increasing the width will lead to area loss in the device area and thinning of the substrate thickness. , affecting device performance.

Method used

A first conductive via hole and a second conductive via hole are respectively formed on two opposite surfaces of the substrate, and their bottoms are electrically connected. By adjusting the etching tilt angle and the design of the dielectric barrier layer, an aspect ratio is greater than 10: 1’s conductive via structure avoids the problems of process difficulty and area loss.

Benefits of technology

It achieves higher aspect ratio through silicon vias that break through the 10:1 aspect ratio on conventional thickness substrates that meet device performance, meets application requirements that require high substrate thickness and device area loss, and avoids process difficulties. and performance impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738020A_ABST
    Figure CN118738020A_ABST
Patent Text Reader

Abstract

The invention discloses a semiconductor device structure and a manufacturing method thereof. The semiconductor device structure comprises a conductive through hole structure arranged in a substrate in a penetrating manner; the conductive through hole structure comprises a first conductive through hole and a second conductive through hole which enter the substrate from two opposite surfaces of the substrate respectively, and the bottom of the first conductive through hole and the bottom of the second conductive through hole are electrically connected in the substrate. The conductive through hole structure provided by the invention can be applied to forming a silicon through hole integrated structure with a higher aspect ratio, and can enable the substrate to have a relatively thicker thickness so as to better meet the application requirements of some products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit technology, and in particular to a semiconductor device structure and a manufacturing method thereof. Background Art

[0002] With the development of semiconductor ultra-large-scale integrated circuits, existing technology and processes have reached physical limits. Driven by the goal of further miniaturization and multifunctionality of electronic products, other new technologies, new materials, and new technologies have been explored. Three-dimensional stacking technology is one of them. Three-dimensional stacking technology stacks silicon wafers through bonding technology to achieve a metal interconnection structure on a three-dimensional level, which can reduce the interconnection distance, increase the transmission speed, reduce the device size, and provide the possibility of heterogeneous structure integration.

[0003] One of the key processes of the existing three-dimensional stacking technology is the through silicon via process. There are three main existing through silicon via process integration schemes, including through silicon via first manufacturing process, through silicon via later manufacturing process, and back through silicon via process. Among them, the through silicon via first manufacturing process is to form a through silicon via structure between two adjacent active areas by performing processes such as photolithography, etching and deposition on the silicon substrate when the conventional active area is formed. The through silicon via later manufacturing process is to etch the dielectric layer and the silicon substrate together from the front of the silicon substrate after the conventional back-end process to form a through silicon via structure. However, the through silicon vias formed by the above two processes ultimately need to be led out from the back of the silicon substrate. This process is usually called the through silicon via back exposure process. The back through silicon via process will turn over the silicon substrate that has completed the back process for bonding with the carrier and thinning the back of the silicon substrate, and then perform processes such as photolithography, etching, and deposition from the back of the silicon substrate to form a through silicon via structure.

[0004] All current TSV integration solutions have certain requirements for the aspect ratio of the TSV structure, but the aspect ratio is usually no more than 10:1. If you want to achieve a TSV with a higher aspect ratio, such as a 20:1 aspect ratio, you will often encounter a series of process problems, mainly including: in terms of etching, under a certain opening size, the deeper the etching goes into the through hole, the smaller the amount and speed of the etching gas that can reach the bottom of the through hole will be, making the deep through hole part prone to various problems, such as rough sidewall surface (grass), size changes, etc. At the same time, the etching time will also double; in terms of filling, the higher the aspect ratio, the higher the copper filling requirements, the greater the process difficulty, and it is easy to have problems such as filling voids at the bottom of the through hole.

[0005] Taking various process factors into consideration, the aspect ratio of TSV is limited under normal process. However, for some applications, the aspect ratio of TSV of 10:1 cannot effectively meet the demand. If the process difficulty is reduced by increasing the width of the TSV to increase the aspect ratio, the excessive width of the TSV will cause area loss in the device area. For TSVs with smaller widths, such as the common 10μm width TSV, the substrate thickness is only 100μm, and the thin substrate thickness of 100μm will affect the device performance.

[0006] Therefore, if a TSV with a higher aspect ratio can be achieved on a thicker substrate that meets device performance, such as a TSV with a width of 10μm and a depth of 200μm, it can better meet the application needs of some products that have high requirements on substrate thickness and device area loss. Summary of the invention

[0007] The purpose of the present invention is to overcome the above-mentioned defects in the prior art and to provide a semiconductor device structure and a manufacturing method thereof.

[0008] To achieve the above object, the technical solution of the present invention is as follows:

[0009] The present invention provides a semiconductor device structure, comprising:

[0010] A conductive via structure penetrating the substrate;

[0011] The conductive via structure includes a first conductive via and a second conductive via respectively entering the substrate from two opposite surfaces of the substrate, and the bottom of the first conductive via and the bottom of the second conductive via are electrically connected in the substrate.

[0012] Further, a top size of the first conductive via corresponds to a top size of the second conductive via.

[0013] Furthermore, the top size and bottom size of the first conductive via are consistent, the top size of the second conductive via is larger than the bottom size, the first conductive via and the second conductive via correspond in position, and the bottom size of the second conductive via is smaller than the bottom size of the first conductive via, so that the bottom of the second conductive via is located within the area occupied by the bottom of the first conductive via.

[0014] Further, a first dielectric barrier layer is provided on the side wall of the first conductive through hole, and a first through hole metal layer is filled in the first dielectric barrier layer; a second dielectric barrier layer is provided on the side wall of the second conductive through hole, and a second through hole metal layer is filled in the second dielectric barrier layer; the second dielectric barrier layer located at the bottom of the second conductive through hole is connected to the first dielectric barrier layer located at the bottom of the first conductive through hole; the second through hole metal layer sequentially passes through the second dielectric barrier layer at the bottom of the second conductive through hole and the first dielectric barrier layer at the bottom of the first conductive through hole to enter the bottom of the first conductive through hole and connect with the first through hole metal layer; and / or the substrate is located on the side of the first conductive through hole A first dielectric protection layer is provided on the first surface of the substrate, the top of the first conductive via is located on a side surface of the first dielectric protection layer away from the first surface, and the bottom of the first conductive via passes through the first dielectric protection layer to enter the substrate, a second dielectric protection layer is provided on the second surface of the substrate located on the second conductive via side, the top of the second conductive via is located on a side surface of the second dielectric protection layer away from the second surface, and the bottom of the second conductive via passes through the second dielectric protection layer to enter the substrate, and a third dielectric protection layer is further provided on a side surface of the first dielectric protection layer away from the first surface, and the third dielectric protection layer covers the top of the first conductive via.

[0015] Further, the substrate comprises a silicon substrate, and the first conductive via and the second conductive via comprise silicon vias; and / or the aspect ratio of the first conductive via and the aspect ratio of the second conductive via are greater than 5:1, or the aspect ratio of the conductive via structure is greater than 10:1.

[0016] The present invention also provides a method for manufacturing a semiconductor device structure, comprising:

[0017] providing a substrate;

[0018] A first conductive via and a second conductive via are formed on two opposite surfaces of the substrate, respectively, and the bottom of the first conductive via and the bottom of the second conductive via are electrically connected in the substrate to form a conductive via structure penetrating the substrate.

[0019] Furthermore, the method for forming the conductive via structure specifically includes:

[0020] Forming a first conductive via on the first surface of the substrate, the bottom of which is located in the substrate, and making the top size and bottom size of the first conductive via consistent with each other;

[0021] Thinning a second surface of the substrate opposite to the first surface, so that the substrate is thinned to a target thickness greater than the depth of the first conductive through hole;

[0022] A second conductive via is formed on the second surface of the thinned substrate, the bottom of which is located in the substrate and electrically connected to the bottom of the first conductive via, so that the second conductive via corresponds to the position of the first conductive via, the top size of the second conductive via corresponds to the top size of the first conductive via, the top size of the second conductive via is larger than the bottom size, and the bottom size of the second conductive via is smaller than the bottom size of the first conductive via, so that the bottom of the second conductive via is located within the area occupied by the bottom of the first conductive via, thereby forming a conductive via structure by the connected second conductive via and the first conductive via.

[0023] Furthermore, the method for forming the first conductive via specifically includes:

[0024] Using a silicon substrate, forming a first dielectric protection layer on a first surface of the silicon substrate;

[0025] Using photolithography and etching processes, a first through hole with a bottom located in the silicon substrate is formed on the surface of the first dielectric protection layer, and by adjusting the etching inclination angle, a top size of the first through hole is made consistent with a bottom size;

[0026] Forming a first dielectric barrier layer on the inner wall of the first through hole, and filling a first through hole metal layer in the first through hole within the first dielectric barrier layer, thereby forming a first conductive through hole of a through silicon via structure;

[0027] The method for forming the second conductive via specifically includes:

[0028] forming a third dielectric protection layer on the surface of the first dielectric protection layer to cover the top of the first conductive through hole;

[0029] Turning over the silicon substrate, and thinning the second surface of the silicon substrate, so that the silicon substrate is thinned to a target thickness that is twice the depth of the first conductive through hole;

[0030] forming a second dielectric protection layer on the second surface of the silicon substrate;

[0031] Using photolithography and etching processes, a second through hole is formed on the surface of the second dielectric protection layer, and the bottom of the second through hole is stopped on the first dielectric barrier layer at the bottom of the first conductive through hole, wherein the bottom size of the second through hole is smaller than the top size by adjusting the etching tilt angle, so that the bottom of the second conductive through hole is located within the area occupied by the bottom of the first conductive through hole;

[0032] Forming a second dielectric barrier layer on the inner wall of the second through hole, and performing back etching to remove the second dielectric barrier layer at the bottom of the second conductive through hole and the first dielectric barrier layer at the bottom of the first conductive through hole, forming openings at the bottom of the second through hole and the bottom of the first conductive through hole, exposing the first through hole metal layer in the first conductive through hole;

[0033] A second through-hole metal layer is filled in the second through-hole within the second dielectric barrier layer, so that the second through-hole metal layer is connected to the first through-hole metal layer through the opening, thereby forming a second conductive through-hole of a silicon via structure connected to the first conductive through-hole.

[0034] Further, when the second surface of the silicon substrate is thinned, the second surface is roughly ground by first using a grinding process to grind the silicon substrate to an intermediate thickness close to the target thickness, and then a combination of a wet etching process, a dry etching process and a planarization process is used to finally thin the silicon substrate to the target thickness, so as to reduce the total thickness deviation of the silicon substrate reflected on the second surface;

[0035] When performing a photolithography process to form the second through hole, photolithography alignment is performed using infrared light to control the coverage accuracy of the second through hole relative to the first conductive through hole within a target accuracy, thereby achieving position alignment of the second conductive through hole with the first conductive through hole;

[0036] When performing the etching process for forming the second through hole, the etching rate of the silicon substrate material is made greater than the etching rate of the first dielectric barrier layer material, so that the bottom of the formed second through hole stops on the first dielectric barrier layer at the bottom of the first conductive through hole, so as to avoid exposing the first through hole metal layer in the first conductive through hole;

[0037] The second dielectric protection layer having a certain thickness is used as a hard mask layer during back etching and as a top protection layer located on the second surface of the silicon substrate.

[0038] Furthermore, when forming the first through hole, the etching process menu is adjusted so that the aspect ratio of the first through hole is greater than 5:1, so that the aspect ratio of the conductive through hole structure of the finally formed silicon through via structure is greater than 10:1.

[0039] It can be seen from the above technical scheme that the present invention forms a first conductive via and a second conductive via entering the substrate on two opposite surfaces of the substrate respectively, and makes the bottom of the first conductive via and the bottom of the second conductive via electrically connected in the substrate, so that a conductive via structure with a higher aspect ratio exceeding 10:1 can be formed in the substrate for application in a through silicon via (TSV) integrated structure, thereby avoiding the existing method of reducing the process difficulty when increasing the aspect ratio by increasing the width of the through silicon via, and the problem that the excessive through silicon via width will cause the area loss of the device area, and the existing problem that the substrate thickness will be thinned accordingly to form a through silicon via with a smaller width, which will affect the device performance. Therefore, the present invention can realize a through silicon via with a higher aspect ratio on a substrate of conventional thickness that meets the device performance, thereby better meeting some application requirements with high requirements on substrate thickness and device area loss. BRIEF DESCRIPTION OF THE DRAWINGS

[0040] Figure 1 A schematic diagram of a semiconductor device structure according to a preferred embodiment of the present invention.

[0041] Figure 2 The present invention is a flowchart of a method for manufacturing a semiconductor device structure according to a preferred embodiment of the present invention.

[0042] Figure 3-Figure 9 A preferred embodiment of the present invention is based on Figure 2 The invention discloses a schematic diagram of the process steps for manufacturing a semiconductor device structure. DETAILED DESCRIPTION

[0043] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Unless otherwise defined, the technical terms or scientific terms used herein should be understood by people with general skills in the field to which the present invention belongs. "Including" and similar words used in this article mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects.

[0044] In order to solve the problem that the existing method of increasing the width of silicon via to reduce the process difficulty when increasing the aspect ratio causes the excessively large width of the silicon via to cause the area loss of the device region, and the existing method of forming silicon vias with a smaller width will cause the substrate thickness to become thinner accordingly, which will affect the device performance, the present invention provides a semiconductor device structure and a manufacturing method thereof.

[0045] A semiconductor device structure of the present invention comprises:

[0046] A conductive via structure penetrating the substrate;

[0047] The conductive via structure includes a first conductive via and a second conductive via respectively entering the substrate from two opposite surfaces of the substrate, and the bottom of the first conductive via and the bottom of the second conductive via are electrically connected in the substrate.

[0048] A method for manufacturing a semiconductor device structure of the present invention comprises:

[0049] providing a substrate;

[0050] A first conductive via and a second conductive via are formed on two opposite surfaces of the substrate, respectively, and the bottom of the first conductive via and the bottom of the second conductive via are electrically connected in the substrate to form a conductive via structure penetrating the substrate.

[0051] The present invention forms a first conductive via and a second conductive via into the substrate on two opposite surfaces of the substrate, respectively, and connects the bottom of the first conductive via and the bottom of the second conductive via in the substrate, so that a conductive via structure with a higher aspect ratio exceeding 10:1 can be formed in the substrate for application in a through silicon via (TSV) integrated structure, thereby avoiding the above-mentioned problems existing in the prior art, so that the present invention can realize a through silicon via with a higher aspect ratio on a substrate of a conventional thickness that meets the device performance, thereby better meeting some application requirements that have higher requirements on substrate thickness and device area loss.

[0052] The specific implementation modes of the present invention are further described in detail below in conjunction with the accompanying drawings.

[0053] refer to Figure 1 A semiconductor device structure of the present invention includes a conductive via structure 13 penetrating through a substrate 10 .

[0054] The substrate 10 has a first surface 101 (upper surface / front side) and a second surface 102 (lower surface / back side) opposite to each other. The conductive via structure 13 includes a first conductive via 14 that enters the substrate 10 from the first surface 101 of the substrate 10, and a second conductive via 15 that enters the substrate 10 from the second surface 102 of the substrate 10. Furthermore, the first conductive via 14 is located at the bottom of the substrate 10 and the second conductive via 15 is located at the bottom of the substrate 10 and is electrically connected to each other, so that the conductive via structure 13 is formed by the electrical connection between the first conductive via 14 and the second conductive via 15 in the substrate 10.

[0055] refer to Figure 1 In some embodiments, the first conductive via 14 and the second conductive via 15 correspond to each other in upper and lower positions, and the top width dimension of the first conductive via 14 on the first surface 101 corresponds to the top width dimension of the second conductive via 15 on the second surface 102. That is, the first conductive via 14 and the second conductive via 15 have the same critical via dimension design specifications.

[0056] In some embodiments, the top width dimension and the bottom width dimension of the first conductive via 14 are consistent, that is, the sidewall of the first conductive via 14 is perpendicular or substantially perpendicular to the first surface 101. The top width dimension of the second conductive via 15 is greater than the bottom width dimension, that is, the angle α between the sidewall of the second conductive via 15 and the second surface 102 is an obtuse angle. In addition, the bottom width dimension of the second conductive via 15 is smaller than the bottom width dimension of the first conductive via 14, so that at the connection between the bottom of the first conductive via 14 and the bottom of the second conductive via 15, the bottom of the second conductive via 15 is located within the area occupied by the bottom of the first conductive via 14.

[0057] In some embodiments, a first dielectric barrier layer 141 is disposed on the sidewall of the first conductive via 14, and a first via metal layer 142 is filled in the first dielectric barrier layer 141. A second dielectric barrier layer 151 is disposed on the sidewall of the second conductive via 15, and a second via metal layer 152 is filled in the second dielectric barrier layer 151.

[0058] Furthermore, the second dielectric barrier layer 151 at the bottom of the second conductive via 15 is connected to the first dielectric barrier layer 141 at the bottom of the first conductive via 14. The second through-hole metal layer 152 sequentially passes through the second dielectric barrier layer 151 at the bottom of the second conductive via 15 and the first dielectric barrier layer 141 at the bottom of the first conductive via 14, enters the bottom of the first conductive via 14, and is connected to the first through-hole metal layer 142 at the bottom of the first conductive via 14.

[0059] In some embodiments, the second dielectric barrier layer 151 located at the bottom of the second conductive via 15 and the first dielectric barrier layer 141 located at the bottom of the first conductive via 14 jointly form an opening 154 at the bottom of the second conductive via 15 and the first conductive via 14, and the second through-hole metal layer 152 is connected to the first through-hole metal layer 142 through the opening 154, so that the second conductive via 15 and the first conductive via 14 are electrically connected through the connection between the second through-hole metal layer 152 and the first through-hole metal layer 142 at their respective bottoms, and the second through-hole metal layer 152 and the first through-hole metal layer 142 are surrounded by the connection between the second dielectric barrier layer 151 and the first dielectric barrier layer 141 at their respective bottoms to be insulated from the substrate 10.

[0060] refer to Figure 1 In some embodiments, a first dielectric protection layer 11 is disposed on the first surface 101 of the substrate 10, the top of the first conductive via 14 is located on a side surface of the first dielectric protection layer 11 away from the first surface 101, and the bottom of the first conductive via 14 passes through the first dielectric protection layer 11 into the substrate 10. The first through-hole metal layer 142 in the first conductive via 14 is exposed on a side surface of the first dielectric protection layer 11 away from the first surface 101.

[0061] A second dielectric protection layer 16 is provided on the second surface 102 of the substrate 10, the top of the second conductive via 15 is located on a side surface of the second dielectric protection layer 16 away from the second surface 102, and the bottom of the second conductive via 15 passes through the second dielectric protection layer 16 into the substrate 10. The second through-hole metal layer 152 in the second conductive via 15 is exposed on a side surface of the second dielectric protection layer 16 away from the second surface 102.

[0062] In some embodiments, a third dielectric protection layer 12 is further disposed on a surface of the first dielectric protection layer 11 away from the first surface 101 , and the third dielectric protection layer 12 covers the top of the first conductive via 14 .

[0063] In some embodiments, the substrate 10 includes a silicon substrate 10, and the first conductive via 14 and the second conductive via 15 include through silicon vias (TSVs). Thus, a new through silicon via integrated structure is formed through the conductive via structure 13 of the present invention.

[0064] In some embodiments, the aspect ratio of the first conductive via 14 and the aspect ratio of the second conductive via 15 are greater than 5:1. Alternatively, the aspect ratio of the entire conductive via structure 13 is greater than 10:1.

[0065] In this embodiment, the critical size of the through silicon via of the first conductive via 14 and the critical size of the through silicon via of the second conductive via 15 (measured by the top opening width) are 10 μm, and the through silicon via depth of the first conductive via 14 and the through silicon via depth of the second conductive via 15 are 100 μm, so that the through silicon via depth-to-width ratio of the first conductive via 14 and the through silicon via depth-to-width ratio of the second conductive via 15 reach 10:1. Therefore, through the combination of the two through silicon vias of the first conductive via 14 and the second conductive via 15, the formed conductive via structure 13 reaches a higher depth-to-width ratio of 20:1. That is, the through silicon via integrated structure formed by the conductive via structure 13 of the present invention achieves a depth-to-width ratio twice that of the 10:1 depth-to-width ratio of the existing through silicon via, and ensures the required thickness of the silicon substrate 10 required to meet the device performance, thereby fully meeting some application requirements with high requirements on substrate thickness and device area loss.

[0066] In some embodiments, the materials of the first dielectric barrier layer 141 and the second dielectric barrier layer 151 include silicon dioxide. The materials of the first through-hole metal layer 142 and the second through-hole metal layer 152 include metal copper. Further, a first seed layer and a first metal barrier layer are sequentially provided between the first through-hole metal layer 142 and the first dielectric barrier layer 141; a second seed layer and a second metal barrier layer are sequentially provided between the second through-hole metal layer 152 and the second dielectric barrier layer 151. The materials of the first seed layer and the second seed layer include copper, and the materials of the first metal barrier layer and the second metal barrier layer include at least one of Ta and TaN. But it is not limited to the above materials.

[0067] The materials of the first dielectric protection layer 11 to the third dielectric protection layer 12 include conventional interlayer dielectric materials, such as silicon dioxide, silicon nitride, etc., but are not limited to the above materials.

[0068] A method for manufacturing a semiconductor device structure of the present invention is further described in detail below through specific implementations and in conjunction with the accompanying drawings.

[0069] refer to Figure 2 A method for manufacturing a semiconductor device structure of the present invention can be used to manufacture the semiconductor device structure of the present invention, and comprises the following steps:

[0070] Step S1: providing a substrate.

[0071] like Figure 3 As shown, a substrate 10, such as a silicon substrate 10 wafer, is used to form a semiconductor device structure of the present invention.

[0072] Step S2: forming a first conductive via into the substrate on the first surface of the substrate.

[0073] like Figure 3As shown, first, a conventional CMOS front-end process is completed on a silicon substrate 10. Then, a first conductive via 14 with its bottom located in the silicon substrate 10 is formed on the front side (first surface 101) of the silicon substrate 10, and the top width dimension of the first conductive via 14 is made consistent with the bottom width dimension.

[0074] In some embodiments, a first dielectric protection layer 11 is formed on the front surface of the silicon substrate 10 by using a deposition process.

[0075] Next, a first through hole 143 with a bottom located in the silicon substrate 10 is formed on the surface of the first dielectric protection layer 11 by using a photolithography and etching process. The top width dimension (CD) of the first through hole 143 is made consistent with the bottom width dimension by adjusting the inclination angle when etching the first through hole 143. In addition, when forming the first through hole 143, the etching process menu is adjusted so that the aspect ratio of the first through hole 143 is greater than 5:1, so that the aspect ratio of the conductive through hole structure 13 finally formed is greater than 10:1.

[0076] In this embodiment, a conventional through silicon via formation process is adopted to etch a first through hole 143 with a top width of 10 μm and a depth of 100 μm on the surface of the first dielectric protection layer 11, and by adjusting the inclination angle during etching, the bottom width of the first through hole 143 is also about 10 μm, thereby forming a first through hole 143 with an aspect ratio of 10:1. Since the key width dimension of the first through hole 143 is a smaller 10 μm formed under conventional process conditions, no additional area loss of the device region is caused.

[0077] Next, a deposition process, such as ALD or CVD, is used to form a first dielectric barrier layer 141, such as silicon dioxide, on the inner wall of the first through hole 143. Then, a first metal barrier layer, such as TaN and a first seed layer of copper are sequentially formed on the surface of the first dielectric barrier layer 141, and then a copper electroplating process is used to form a first through hole metal layer 142 of copper on the surface of the first seed layer of copper, and the first through hole 143 is filled. Since the width critical dimension of the first through hole 143 is a conventional 10 μm, it can meet the requirement of good filling of the through hole metal, and avoid the generation of void defects at the bottom of the first through hole 143 caused by insufficient filling.

[0078] Then, a planarization process, such as a chemical mechanical polishing process, is used to remove the excess copper first through-hole metal layer 142, the copper first seed layer and the TaN first metal barrier layer material on the surface of the first dielectric protection layer 11 to form a flat surface of the first dielectric protection layer 11, thereby forming a first conductive via 14 with a through-silicon via structure having an aspect ratio of 10:1 on the front side of the silicon substrate 10, and exposing the top of the first conductive via 14 from the surface of the first dielectric protection layer 11.

[0079] After that, the subsequent CMOS process flow, such as CMOS back-end process, is completed.

[0080] Step S3: forming a second conductive via into the substrate on a second surface of the substrate opposite to the first surface, so that the bottom of the second conductive via is electrically connected to the bottom of the first conductive via to form a conductive via structure penetrating the substrate.

[0081] like Figure 4 As shown, a deposition process is used to form a third dielectric protection layer 12 on the surface of the first dielectric protection layer 11, covering the top of the first conductive via 14. Next, a bonding process is used to bond a surface of a carrier wafer with a bonding medium to the surface of the third dielectric protection layer 12, so as to form a carrier wafer layer 17 by bonding on the surface of the third dielectric protection layer 12.

[0082] Then, the silicon substrate 10 bonded with the carrier wafer layer 17 is turned over so that the back side of the silicon substrate 10 is placed upward. The back side of the silicon substrate 10 is thinned so that the silicon substrate 10 is thinned to a target thickness greater than the depth of the first conductive via 14. In this embodiment, the back side of the silicon substrate 10 is thinned so that the silicon substrate 10 is thinned to a target thickness about twice the depth of the first conductive via 14. For example, for the first conductive via 14 with a width of 10 μm and a depth of 100 μm completed on the front side of the silicon substrate 10, the silicon substrate 10 can be thinned to a thickness of about 200 μm. The back side of the thinned silicon substrate 10 forms a second surface 102.

[0083] In some embodiments, when thinning the back side of the silicon substrate 10, a grinding process is first used to roughly grind the back side of the silicon substrate 10, and the silicon substrate 10 is ground to an intermediate thickness (e.g., 210 μm) close to the target thickness of, for example, 200 μm. Then, a combination of a wet etching process, a dry etching process, and a chemical mechanical polishing process is used to further thin the silicon substrate 10 to a target thickness of 200 μm, so as to reduce the total thickness deviation (TTV) of the silicon substrate 10 reflected on the back side of the silicon substrate 10, and control the overall TTV within the required range. For example, for a 200 μm thick silicon substrate 10, the TTV is controlled to be below 10 μm.

[0084] like Figure 5 As shown, a deposition process is then used to form a second dielectric protection layer 16 on the back side (second surface 102) of the thinned silicon substrate 10. The second dielectric protection layer 16 is used as a hard mask layer for subsequent etching back of the second dielectric barrier layer 151 at the bottom of the second through hole.

[0085] The second dielectric protection layer 16 can be grown by, for example, CVD-deposited silicon dioxide, and its thickness needs to be sufficient to meet the consumption of subsequent back etching. For example, the total thickness required for etching the second dielectric barrier layer 151 at the bottom of the second through hole is set to When the thickness of the second dielectric protection layer 16 is about.

[0086] Then, a photoresist layer is formed on the surface of the second dielectric protection layer 16, and a photolithography process is used to form a photoresist pattern 18 on the surface of the second dielectric protection layer 16, so as to form a second through hole that is consistent with (or close to) the CD of the first through hole 143 and relatively aligned in position downward through the window 19 between the photoresist patterns 18.

[0087] Among them, when performing the photolithography process to form the second through hole, since the thickness of the silicon substrate 10 is relatively thick, infrared light can be used to perform photolithography alignment between the second through hole to be formed and the first conductive through hole 14 that has been formed, so as to control the overlay accuracy (Overlay) of the second through hole relative to the first conductive through hole 14 to be within a target accuracy of, for example, 1 μm, thereby achieving position alignment between the subsequently formed second conductive through hole 15 and the first conductive through hole 14.

[0088] like Figure 6 As shown, then, an etching process is used to etch the second dielectric protection layer 16 and the back side of the silicon substrate 10, and a second through hole is formed on the surface of the second dielectric protection layer 16 into the silicon substrate 10, and the bottom of the second through hole 153 stops on the first dielectric barrier layer 141 at the bottom of the first conductive through hole 14. In this embodiment, the second through hole 153 is formed by etching using the BOSCH process. The etching process menu is adjusted, such as adjusting the ratio of etching to deposition to adjust the etching inclination angle, so that the bottom width of the second through hole 153 is smaller than the top width, so that the bottom of the second through hole 153 is located within the area occupied by the bottom of the first conductive through hole 14. For example, if the bottom CD of the first conductive through hole 14 is 10 μm, the bottom CD of the second through hole 153 can be 9 μm.

[0089] Among them, when executing the etching process for forming the second through hole 153, a menu with a high Si-SiO2 selectivity ratio is adopted, so that the etching rate of the silicon substrate 10 material is greater than the etching rate of the first dielectric barrier layer 141 material, and the first dielectric barrier layer 141 located at the bottom of the first conductive through hole 14 is over-etched to a certain extent, so that the bottom of the formed second through hole 153 stops on the first dielectric barrier layer 141 at the bottom of the first conductive through hole 14 and is in full contact with the first dielectric barrier layer 141, but the first dielectric barrier layer 141 is not etched through, so as to avoid exposing the first through hole metal layer 142 in the first conductive through hole 14.

[0090] It should be noted that the purpose of not etching through the first dielectric barrier layer 141 is that if the first via metal layer 142 in the first conductive via 14 is exposed due to excessive etching, metal may be sputtered onto the Si material on the side wall of the second via 153, thereby causing leakage.

[0091] After the above etching is completed, the stripping and cleaning processes are performed.

[0092] like Figure 7 As shown, a deposition process with high sidewall coverage, such as ALD, is then used to form a second dielectric barrier layer 151 of, for example, silicon dioxide on the inner wall of the second through hole 153. The thickness of the second dielectric barrier layer 151 needs to meet the leakage performance requirements and also facilitate the subsequent removal of the second dielectric barrier layer 151 at the bottom of the second through hole 153. For example, the thickness of the second dielectric barrier layer 151 is If the thickness of the first dielectric barrier layer 141 at the bottom of the first conductive via 14 is also If , then the bottom of the second through hole 153 has a total of about Thickness of silicon dioxide.

[0093] Then, without performing a photolithography process, the second dielectric barrier layer 151 and the first dielectric barrier layer 141 at the bottom of the second through hole 153 are etched back (Blanket etch) to remove the second dielectric barrier layer 151 and the first dielectric barrier layer 141 at the bottom of the second through hole 153, thereby forming an opening 154 on the second dielectric barrier layer 151 at the bottom of the second through hole 153 and the first dielectric barrier layer 141 at the bottom of the first conductive through hole 14, exposing the first through hole metal layer 142 in the first conductive through hole 14. At the same time, the second dielectric barrier layer 151 located on the side wall of the second through hole 153 can also retain a sufficient thickness, such as Figure 8 At this time, the second dielectric protection layer 16 on the back side of the silicon substrate 10 will also be etched away to a certain thickness, and the remaining portion of the second dielectric protection layer 16 can be used as a top protection layer of the Si material on the back side of the silicon substrate 10 .

[0094] like Fig. 9As shown, then, first, a second metal barrier layer such as TaN is formed on the surface of the second dielectric barrier layer 151, and the second metal barrier layer is contacted with the first through-hole metal layer 142 exposed on the bottom of the first conductive through-hole 14 below through the opening 154 on the bottom surface of the second through-hole 153 to form an electrical connection; then, a copper second seed layer is grown on the surface of the second metal barrier layer, and then a copper electroplating process is used to fill the second through-hole 153 within the surface of the copper second seed layer to form a copper second through-hole metal layer 152, and fill the second through-hole 153. Since the width critical dimension of the second through-hole 153 is the conventional 10μm, and the bottom has a width dimension of 9μm, it can meet the requirement of good through-hole metal filling, and also avoid the void defect caused by insufficient filling at the bottom of the second through-hole 153. Thus, the second through-hole metal layer 152 is connected to the first through-hole metal layer 142 through the opening 154 to form a metal contact.

[0095] Finally, a planarization process, such as a chemical mechanical polishing process, is used to remove the excess copper second via metal layer 152, the copper second seed layer and the TaN second metal barrier layer material on the surface of the second dielectric protection layer 16 to form a flat surface of the second dielectric protection layer 16, thereby forming a second conductive via 15 having a through silicon via structure with an aspect ratio of 10:1 on the back side of the silicon substrate 10 according to the target thickness of 200 μm obtained after the silicon substrate 10 is thinned, and the top of the second conductive via 15 is exposed from the surface of the second dielectric protection layer 16. The carrier wafer layer 17 can be removed or retained.

[0096] The second conductive via 15 formed by the above method corresponds to the position of the first conductive via 14, the top size of the second conductive via 15 corresponds to the top size of the first conductive via 14, and the top size of the second conductive via 15 is larger than the bottom size, so that the bottom of the second conductive via 15 is completely located within the area occupied by the bottom of the first conductive via 14. Thus, a conductive via structure 13 consisting of the connected second conductive via 15 and the first conductive via 14 and having a complete silicon via structure with an aspect ratio of 20:1 is formed.

[0097] In summary, the present invention forms a conductive through-hole structure 13 with a higher aspect ratio that exceeds the aspect ratio of 10:1 on a silicon substrate 10 to form a through-silicon via (TSV) integrated structure. This can avoid the existing method of reducing the process difficulty when increasing the aspect ratio by increasing the width of the through-silicon via, which causes the area loss of the device region due to the excessively large through-silicon via width, and the existing problem of forming a through-silicon via with a smaller width, which causes the silicon substrate thickness to become thinner accordingly, thereby affecting the device performance. Therefore, a through-silicon via with a higher aspect ratio can be realized on a silicon substrate 10 of a conventional thickness that meets the device performance, thereby better meeting some application requirements that have high requirements on substrate thickness and device area loss.

[0098] Although the embodiments of the present invention are described in detail above, it is obvious to those skilled in the art that various modifications and variations can be made to these embodiments. However, it should be understood that such modifications and variations are within the scope and spirit of the present invention as described in the claims. Moreover, the present invention described herein may have other embodiments and may be implemented or realized in a variety of ways.

Claims

1. A semiconductor device structure, It is characterized in that include: A conductive via structure penetrating the substrate; The conductive via structure includes a first conductive via and a second conductive via respectively entering the substrate from two opposite surfaces of the substrate, and the bottom of the first conductive via and the bottom of the second conductive via are electrically connected in the substrate.

2. The semiconductor device structure according to claim 1, It is characterized in that A top dimension of the first conductive via corresponds to a top dimension of the second conductive via.

3. The semiconductor device structure according to claim 2, It is characterized in that The top size and bottom size of the first conductive via are consistent, the top size of the second conductive via is larger than the bottom size, the first conductive via and the second conductive via correspond in position, and the bottom size of the second conductive via is smaller than the bottom size of the first conductive via, so that the bottom of the second conductive via is located within the area occupied by the bottom of the first conductive via.

4. The semiconductor device structure according to claim 3, It is characterized in that A first dielectric barrier layer is provided on the side wall of the first conductive through hole, and a first through hole metal layer is filled in the first dielectric barrier layer; a second dielectric barrier layer is provided on the side wall of the second conductive through hole, and a second through hole metal layer is filled in the second dielectric barrier layer; the second dielectric barrier layer located at the bottom of the second conductive through hole is connected to the first dielectric barrier layer located at the bottom of the first conductive through hole; the second through hole metal layer sequentially passes through the second dielectric barrier layer at the bottom of the second conductive through hole and the first dielectric barrier layer at the bottom of the first conductive through hole to enter the bottom of the first conductive through hole and connect with the first through hole metal layer; and / or the substrate is located at a second dielectric barrier layer on the side of the first conductive through hole. A first dielectric protection layer is provided on one surface, the top of the first conductive via is located on a side surface of the first dielectric protection layer away from the first surface, and the bottom of the first conductive via passes through the first dielectric protection layer to enter the substrate, a second dielectric protection layer is provided on a second surface of the substrate located on the second conductive via side, the top of the second conductive via is located on a side surface of the second dielectric protection layer away from the second surface, and the bottom of the second conductive via passes through the second dielectric protection layer to enter the substrate, and a third dielectric protection layer is also provided on a side surface of the first dielectric protection layer away from the first surface, and the third dielectric protection layer covers the top of the first conductive via.

5. The semiconductor device structure according to claim 1, It is characterized in that The substrate comprises a silicon substrate, and the first conductive via and the second conductive via comprise silicon vias; and / or the aspect ratio of the first conductive via and the aspect ratio of the second conductive via are greater than 5:1, or the aspect ratio of the conductive via structure is greater than 10:

1.

6. A method for manufacturing a semiconductor device structure, It is characterized in that include: providing a substrate; A first conductive via and a second conductive via are formed on two opposite surfaces of the substrate, respectively, and the bottom of the first conductive via and the bottom of the second conductive via are electrically connected in the substrate to form a conductive via structure penetrating the substrate.

7. The method for manufacturing a semiconductor device structure according to claim 6, It is characterized in that The method for forming the conductive via structure specifically comprises: Forming a first conductive via on the first surface of the substrate, the bottom of which is located in the substrate, and making the top size and bottom size of the first conductive via consistent with each other; Thinning a second surface of the substrate opposite to the first surface, so that the substrate is thinned to a target thickness greater than the depth of the first conductive through hole; A second conductive via is formed on the second surface of the thinned substrate, the bottom of which is located in the substrate and electrically connected to the bottom of the first conductive via, so that the second conductive via corresponds to the position of the first conductive via, the top size of the second conductive via corresponds to the top size of the first conductive via, the top size of the second conductive via is larger than the bottom size, and the bottom size of the second conductive via is smaller than the bottom size of the first conductive via, so that the bottom of the second conductive via is located within the area occupied by the bottom of the first conductive via, thereby forming a conductive via structure by the connected second conductive via and the first conductive via.

8. The method for manufacturing a semiconductor device structure according to claim 7, It is characterized in that The method for forming the first conductive via specifically includes: Using a silicon substrate, forming a first dielectric protection layer on a first surface of the silicon substrate; Using photolithography and etching processes, a first through hole with a bottom located in the silicon substrate is formed on the surface of the first dielectric protection layer, and by adjusting the etching inclination angle, a top size of the first through hole is made consistent with a bottom size; Forming a first dielectric barrier layer on the inner wall of the first through hole, and filling a first through hole metal layer in the first through hole within the first dielectric barrier layer, thereby forming a first conductive through hole of a through silicon via structure; The method for forming the second conductive via specifically includes: forming a third dielectric protection layer on the surface of the first dielectric protection layer to cover the top of the first conductive through hole; Turning over the silicon substrate, and thinning the second surface of the silicon substrate, so that the silicon substrate is thinned to a target thickness that is twice the depth of the first conductive through hole; forming a second dielectric protection layer on the second surface of the silicon substrate; Using photolithography and etching processes, a second through hole is formed on the surface of the second dielectric protection layer, and the bottom of the second through hole is stopped on the first dielectric barrier layer at the bottom of the first conductive through hole, wherein the bottom size of the second through hole is smaller than the top size by adjusting the etching tilt angle, so that the bottom of the second conductive through hole is located within the area occupied by the bottom of the first conductive through hole; Forming a second dielectric barrier layer on the inner wall of the second through hole, and performing back etching to remove the second dielectric barrier layer at the bottom of the second conductive through hole and the first dielectric barrier layer at the bottom of the first conductive through hole, forming openings at the bottom of the second through hole and the bottom of the first conductive through hole, exposing the first through hole metal layer in the first conductive through hole; A second through-hole metal layer is filled in the second through-hole within the second dielectric barrier layer, so that the second through-hole metal layer is connected to the first through-hole metal layer through the opening, thereby forming a second conductive through-hole of a silicon via structure connected to the first conductive through-hole.

9. The method for manufacturing a semiconductor device structure according to claim 8, It is characterized in that When thinning the second surface of the silicon substrate, the second surface is roughly ground by first using a grinding process to grind the silicon substrate to an intermediate thickness close to a target thickness, and then a combination of a wet etching process, a dry etching process and a planarization process is used to finally thin the silicon substrate to a target thickness, so as to reduce a total thickness deviation of the silicon substrate reflected on the second surface; When performing a photolithography process to form the second through hole, photolithography alignment is performed using infrared light to control the coverage accuracy of the second through hole relative to the first conductive through hole within a target accuracy, thereby achieving position alignment of the second conductive through hole with the first conductive through hole; When performing the etching process for forming the second through hole, the etching rate of the silicon substrate material is made greater than the etching rate of the first dielectric barrier layer material, so that the bottom of the formed second through hole stops on the first dielectric barrier layer at the bottom of the first conductive through hole, so as to avoid exposing the first through hole metal layer in the first conductive through hole; The second dielectric protection layer having a certain thickness is used as a hard mask layer during back etching and as a top protection layer located on the second surface of the silicon substrate.

10. The method for manufacturing a semiconductor device structure according to claim 8, It is characterized in that When forming the first through hole, the etching process menu is adjusted so that the aspect ratio of the first through hole is greater than 5:1, so that the aspect ratio of the conductive through hole structure of the finally formed silicon through via structure is greater than 10:1.