Semiconductor device and method of manufacturing the same

By alternately arranging first conductivity type and second conductivity type pillars in the semiconductor device, and optimizing the pillar spacing using multi-level zigzag outer portions and impurity layers, trench clogging and on-resistance problems are solved, achieving stable manufacturing and low conductivity. Super-junction structure with pass resistance.

CN118738089APending Publication Date: 2024-10-01SANAN JAPAN TECH CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410312876.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-19
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

In existing semiconductor devices, when the second conductivity type layer is epitaxially grown, the slot opening is easily blocked, resulting in internal voids remaining, making it impossible to manufacture stably. In addition, the distance between adjacent conductivity type layers in the superjunction structure is uneven, resulting in an increase in on-resistance. .

Method used

A plurality of first conductive type pillars and a plurality of second conductive type pillars are alternately arranged. The second conductive type pillars have multi-level zigzag outer portions and are fitted with the zigzag outer portions of adjacent pillars. Through ion implantation and etching, The process forms an impurity layer and a filling layer, and optimizes the column spacing and impurity concentration.

Benefits of technology

Achieved stable manufacturing of superjunction structure semiconductor elements with improved on-resistance characteristics, reduced on-resistance, and improved impurity concentration and voltage resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738089A_ABST
    Figure CN118738089A_ABST
Patent Text Reader

Abstract

The invention provides a semiconductor device and a manufacturing method thereof. A semiconductor device includes: a drain layer formed of a first conductivity type semiconductor; a drift layer formed of a first conductivity type semiconductor on one surface of the drain layer; and a pillar structure in which a plurality of first conductivity-type pillars and a plurality of second conductivity-type pillars are alternately arranged in the drift layer, the second conductivity-type pillars having a multi-stage serrated outer portion in a cross-sectional view, the multi-stage serrated outer portion of the second conductivity-type pillars having a super junction structure, and the first conductivity-type pillars and the second conductivity-type pillars having a super junction structure in a cross-sectional view. The super junction structure is configured to be embedded with the outer side part of the multi-stage zigzag shape of the adjacent second conductive type column.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a semiconductor device and a method for manufacturing the same. Background Art

[0002] Patent Documents 1 and 2 disclose semiconductor devices having a super junction structure. In the semiconductor device described in Patent Document 1, a groove is formed in a first conductive type semiconductor by etching. A second conductive type layer is formed in the groove by epitaxial growth. As a result, a super junction SJ structure is obtained.

[0003] Japanese Patent Laid-Open No. 2013-102087;

[0004] U.S. Patent No. 8,476,698;

[0005] However, in the semiconductor device described in Patent Document 1, when the second conductivity type layer is formed in the groove by epitaxial growth, the opening of the groove is easily clogged. Therefore, voids are likely to remain inside the groove, making stable manufacturing impossible.

[0006] In addition, in the semiconductor device described in Patent Document 2, when viewed in cross section, the distance between adjacent first conductivity types and the distance between adjacent second conductivity types in the super junction structure differ depending on the position in the thickness direction. Therefore, the impurity concentration cannot be increased, resulting in an increase in on-resistance. Summary of the invention

[0007] The present disclosure is intended to solve the above-mentioned problems. An object of the present invention is to provide a semiconductor device having a super junction structure and a method for manufacturing the same, the super junction structure being able to be stably manufactured and having improved on-resistance characteristics.

[0008] In a first aspect, a semiconductor device is provided in this embodiment, including:

[0009] a drain layer, wherein the drain layer is formed of a first conductive type semiconductor;

[0010] a drift layer, wherein the drift layer is formed of a first conductive type semiconductor on one side of the drain layer; and

[0011] A column structure, wherein in the drift layer, a plurality of first conductive type columns and a plurality of second conductive type columns are alternately arranged;

[0012] The second conductive type column has a multi-stage sawtooth outer portion when viewed in cross section;

[0013] The multi-stage sawtooth outer portion of the second conductive type pillar has a super junction structure, and the super junction structure is configured to be embedded with the multi-stage sawtooth outer portion of another adjacent second conductive type pillar.

[0014] In some embodiments, the second conductive column has:

[0015] a second conductivity type impurity layer; and

[0016] A filling layer is formed inside the impurity layer.

[0017] In some of the embodiments, the filling layer is formed of an insulator or a semiconductor.

[0018] In some embodiments, the impurity concentration of the impurity layer is 1.0×10 17 cm -3 Above and 1.0×10 20 cm -3 the following.

[0019] In some of the embodiments, a distance between any adjacent second conductive type pillars is less than 4 μm.

[0020] In some of the embodiments, the first conductive type pillar is formed of first conductive type silicon carbide;

[0021] The impurity layer is formed of second conductivity type silicon carbide.

[0022] In a second aspect, a method for manufacturing a semiconductor device is provided in this embodiment, comprising:

[0023] a drift layer forming step of forming a first conductivity type drift layer by epitaxial growth on a drain layer formed of a first conductivity type semiconductor; and

[0024] A second conductive type pillar forming step, in which a plurality of second conductive type pillars are formed in the drift layer so as to have a multi-stage sawtooth outer portion in cross-sectional view;

[0025] The second conductive type column forming step comprises:

[0026] A first step, the first step comprising: an etching process, in which etching is performed using a first mask having an opening formed therein at a position corresponding to a region where a plurality of second conductive type pillars that are not adjacent to each other are formed among the plurality of second conductive type pillars;

[0027] The second step includes: an ion implantation process, in which impurities are implanted using a second mask, the second mask is formed with an opening position, and the opening position corresponds to the area formed by the multiple second conductive type columns formed in the first step and the multiple second conductive type columns adjacent thereto; and an etching process, in which the second mask is still used to etch a portion of the ion implantation area.

[0028] In some embodiments, the depth of etching performed by the etching process in the first step is half of the depth of etching performed by the etching process in the second step.

[0029] In some embodiments, by repeatedly performing the ion implantation process and the etching process in the second step, a plurality of second conductive type pillars are formed in a manner that the outer portion has a multi-level sawtooth shape in cross-section.

[0030] In some of the embodiments, in the ion implantation step, ion implantation is performed in such a manner that a portion of a region where the impurities exist extends further outward than an opening of the mask when viewed from above.

[0031] In some embodiments, after repeating the ion implantation process and the etching process in the second step, a filling process is further included, in which the grooves formed by the etching process are filled with an insulator or a semiconductor.

[0032] According to the present disclosure, a semiconductor element having a super junction structure with improved on-resistance characteristics can be stably manufactured.

[0033] Details of one or more embodiments of the present application are set forth in the following drawings and description to make other features, objects, and advantages of the present application more readily apparent. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] The drawings described herein are used to provide further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute improper limitations on the present application.

[0035] Figure 1 is a cross-sectional view of the semiconductor device in Embodiment 1;

[0036] Figure 2 is a cross-sectional view of a comparative example;

[0037] Figure 3 is a graph showing the relationship between the SJ pitch P and the on-resistance;

[0038] Figure 4 is a cross-sectional view for explaining the method for manufacturing the semiconductor device in the first embodiment;

[0039] Figure 5 This is a diagram for explaining a method for forming a second conductivity type impurity layer in the semiconductor device in the first embodiment.

[0040] In the figure: 1. semiconductor device; 2. drain layer; 3. drift layer; 4. main layer; 5. source layer; 6. main contact layer; 7. gate insulating layer; 8. gate electrode layer; 9. interlayer insulating layer; 10. source electrode layer; 11. wiring electrode layer; 12. drain electrode layer; 13. impurity layer; 14. filling layer; 15, 16, silicon dioxide layer. DETAILED DESCRIPTION

[0041] In order to more clearly understand the purpose, technical solutions and advantages of the present application, the present application is described and illustrated below in conjunction with the accompanying drawings and embodiments.

[0042] Unless otherwise defined, the technical terms or scientific terms involved in this application shall have the general meaning understood by people with ordinary skills in the technical field to which this application belongs. The words "one", "a", "a", "the", "these" and the like in this application do not represent quantitative restrictions, and they can be singular or plural. The terms "include", "comprise", "have" and any variants thereof involved in this application are intended to cover non-exclusive inclusions; for example, a process, method and system, product or device comprising a series of steps or modules (units) is not limited to the listed steps or modules (units), but may include unlisted steps or modules (units), or may include other steps or modules (units) inherent to these processes, methods, products or devices. The words "connect", "connected", "coupled" and the like involved in this application are not limited to physical or mechanical connections, but may include electrical connections, whether directly or indirectly. The "multiple" involved in this application refers to two or more. "And / or" describes the association relationship of associated objects, indicating that there can be three relationships. For example, "A and / or B" can mean: A exists alone, A and B exist at the same time, and B exists alone. Usually, the character " / " indicates that the objects associated with each other are in an "or" relationship. The terms "first", "second", "third", etc. involved in this application are only used to distinguish similar objects and do not represent a specific ordering of the objects.

[0043] Implementation 1:

[0044] Figure 1 This is a cross-sectional view of the semiconductor device 1 in the first embodiment.

[0045] exist Figure 1 In the embodiment, the semiconductor device 1 is a planar MOSFET having a superjunction structure of silicon carbide. The semiconductor device 1 includes a drain layer 2, a drift layer 3, a plurality of body layers 4, a plurality of source layers 5, a plurality of body contact layers 6, a plurality of gate insulating layers 7, a plurality of interlayer insulating layers 9, a plurality of source electrode layers 10, a wiring electrode layer 11, a drain electrode layer 12, a plurality of impurity layers 13, and a plurality of filling layers 14.

[0046] The drain layer 2 is formed of first conductive type silicon carbide. For example, the drain layer 2 is formed of n+ type 4H silicon carbide. For example, the drain layer 2 is formed with nitrogen as an impurity. The drift layer 3 is formed on the first surface ( Figure 1 The drift layer 3 is an upper surface. The drift layer 3 is formed of first conductivity type silicon carbide having a lower impurity concentration than the drain layer 2. For example, the drift layer 3 is an n-type layer. For example, the drift layer 3 is formed on the drain layer 2 by epitaxial growth.

[0047] A plurality of main body layers 4 are formed on the drift layer 3. The plurality of main body layers 4 are formed of second conductive type silicon carbide. For example, the plurality of main body layers 4 are p-type layers. For example, the plurality of main body layers 4 are formed by ion implantation using aluminum as an impurity. A plurality of source layers 5 are formed on the plurality of main body layers 4, respectively. The plurality of source layers 5 are formed of first conductive type silicon carbide having a higher impurity concentration than the drift layer 3. For example, the plurality of source layers 5 are n+ type layers. For example, the plurality of source layers 5 are formed by ion implantation using nitrogen as an impurity. A plurality of main body contact layers 6 are formed on the plurality of main body layers 4, respectively. In each of the plurality of main body layers 4, the main body contact layer 6 is surrounded by the source layer 5. The plurality of main body contact layers 6 are formed of second conductive type silicon carbide having a higher impurity concentration than the plurality of main body layers 4. For example, the plurality of main body contact layers 6 are p+ type layers. For example, the plurality of main body contact layers 6 are formed by ion implantation using aluminum as an impurity.

[0048] The plurality of gate insulating layers 7 are formed so as to contact the source layers 5 of the respective adjacent main layers 4. Specifically, the plurality of gate insulating layers 7 are formed so as to span the main layers 4 adjacent to the drift layer 3 and the respective source layers 5 existing inside the main layers 4. For example, the plurality of gate insulating layers 7 are formed into silicon dioxide layers by thermal oxidation. The plurality of gate electrode layers 8 are respectively formed on the plurality of gate insulating layers 7. For example, the plurality of gate electrode layers 8 are formed of polycrystalline silicon by CVD method.

[0049] A plurality of interlayer insulating layers 9 are formed to cover the plurality of gate electrode layers 8, respectively. For example, the plurality of interlayer insulating layers 9 are formed of silicon dioxide by a CVD method. A plurality of source electrode layers 10 are formed corresponding to the plurality of main body layers 4, respectively. The source electrode layer 10 is formed to be in contact with the source layer 5. The source electrode layer 10 may also be formed to straddle the main body contact layer 6. For example, the plurality of source electrode layers 10 are formed by forming a film of a material such as Ni by a method such as a sputtering method, and then subjecting the film to a heat treatment. The wiring electrode layer 11 is formed to cover the plurality of source electrode layers 10. For example, the wiring electrode layer 11 is formed of a material such as an aluminum alloy by a method such as a sputtering method.

[0050] The drain electrode layer 12 is formed on the second surface of the drain layer 2 ( Figure 1 For example, the drain electrode layer 12 is formed by forming a film of a material such as Ni by a method such as sputtering and then subjecting it to heat treatment.

[0051] In this embodiment, a column configuration C is formed in the drift layer 3. In the column configuration C, a plurality of first conductive type columns C1 and a plurality of second conductive type columns C2 are arranged alternately. The plurality of first conductive type columns C1 are formed as part of the drift layer 3. The plurality of second conductive type columns C2 are formed separately from the layer formed as the drift layer 3.

[0052] A plurality of second conductive type columns C2 are respectively formed below the source electrode layer 10. In each of the plurality of second conductive type columns C2, the upper portion is surrounded by the main layer 4, the source layer 5 and the main contact layer 6. Each of the plurality of second conductive type columns C2 has a multi-level sawtooth outer portion when viewed in cross section. Specifically, in each of the plurality of second conductive type columns C2, a plurality of first inclined portions A1 and a plurality of second inclined portions A2 are alternately arranged in the thickness direction of the drift layer 3. The first inclined portion A1 extends from one side of the drain layer 2 (at Figure 1 The upper surface in the middle) toward the other side (in Figure 1 The second inclined portion A2 is formed by gradually narrowing laterally from one side of the drain layer 2 toward the other side. At this time, the second inclined portion A2 is formed to be narrowed more sharply than the expansion degree of the first inclined portion A1.

[0053] More specifically, each of the plurality of second conductive type columns C2 includes an impurity layer 13 and a filling layer 14. The impurity layer 13 forms the outer portion of the second conductive type column C2. The impurity layer 13 is formed of second conductive type silicon carbide. The impurity layer 13 is a p-type layer. For example, the impurity layer 13 is formed by ion implantation using aluminum as an impurity. The impurity concentration of the impurity layer 13 is 1.0×10 17 cm-3 or more and 1.0×10 20 The filling layer 14 is formed inside the impurity layer 13. The filling layer 14 is formed of an insulator or a semiconductor. For example, the filling layer 14 is formed of silicon dioxide.

[0054] Thus, in this embodiment, in the drift layer 3, a plurality of first conductive type columns C1 and a plurality of second conductive type columns C2 are alternately arranged to form a groove structure. When a reverse voltage is applied to the structure, the depletion layer expands laterally. As a result, a depletion layer equivalent to the depth of the groove is formed. At this time, only the depletion layer of half the groove interval expands, and a depletion layer with a thickness equivalent to the depth of the groove is formed.

[0055] In the super junction structure, it is preferred that the grooves and the groove intervals are as thin and deep as possible. Figure 1The column C shown indicates that it has been formed halfway to the drift layer 3, but it can also be formed throughout the entire drift layer 3. As a result, the on-resistance can be further reduced. Compared with the case of a non-super junction structure, the impurity concentration of the drift layer 3 can be increased to about 5 times. As described above, in the super junction structure, the withstand voltage is ensured by a mechanism different from that of the existing MOSFET. Therefore, it is possible to exert performance beyond the so-called silicon limit and SiC limit, and to reduce the on-resistance.

[0056] Here, if Figure 1 As shown, the adjacent second conductive type columns C2 are arranged in a manner that their respective multi-stage sawtooth outer portions are interlocked. That is, the adjacent second conductive type columns C2 are arranged to be offset from each other by half of a section of the sawtooth outer portion in the depth direction. In other words, when viewed in cross section, the lateral expansion portions and the narrowing portions of the impurity layers 13 of the adjacent second conductive type columns C2 are arranged in a substantially corresponding positional relationship.

[0057] Figure 1 The impurity layer 13 shown has a maximum width 13MaxW of 0.3 μm when viewed in cross section. Figure 1 The impurity layer 13 shown has a minimum width 13MinW of 0.1 μm when viewed in cross section.

[0058] Here, Figure 1 The super junction structure pitch (hereinafter referred to as “SJ pitch”) P shown represents the interval between adjacent second conductive type pillars C2. Figure 1 The distance L1 shown in the figure indicates the direction of the Figure 1 The lateral extension portion of the second conductive column C2 on the left side is Figure 1 The distance between the narrowed parts of the right second conductive type column C2.

[0059] Figure 1 The distance L2 shown in the figure represents the direction of the corresponding position relationship. Figure 1 The narrowed portion of the second conductive column C2 on the left side and the Figure 1 When the SJ pitch P is 4 μm and the groove width W of the filling layer 14 is 1 μm, the distance L1 and the distance L2 are both 2.6 μm. These distances are the maximum distances between the pillars.

[0060] Next, comparative examples will be described. Figure 2 is a cross-sectional view of a comparative example. Figure 2As shown, in the comparative example, between adjacent second conductive type columns C2, the respective multi-level sawtooth outer portions are not configured to fit together. That is, the adjacent second conductive type columns C2 are not configured to be offset from each other by half of a section of the sawtooth outer portion in the depth direction. In other words, in the cross-sectional view, as shown by the distance L5, the lateral extension portions of the impurity layer 13 between adjacent second conductive type columns C2 are configured to correspond to each other, and as shown by the distance L4, the narrowing portions of the impurity layer 13 are configured to correspond to each other. In the comparative example, when the SJ pitch P is 4μm and the groove width W of the filling layer 14 is 1μm, the distance between the narrowing portions of the impurity layer 13 between adjacent second conductive type columns C2, that is, the maximum distance L4 between the columns, is 2.8μm. In addition, the distance between the extension portions of the impurity layer 13 between adjacent second conductive type columns C2, that is, L5, is 2.4μm.

[0061] Table 1 shows the parameters when the SJ pitch P of the present invention and the comparative example is set to 2 μm, 4 μm, and 10 μm when the withstand voltage of the semiconductor element is set to about 1200 V.

[0062] Table 1

[0063]

[0064] As shown in Table 1, in the present invention and the comparative example, in any SJ pitch P, the inter-pillar distance of the present invention is smaller than the inter-pillar distance L4 of the comparative example. When the same reverse voltage is applied, according to the present invention, even if the concentration of the impurity layer 13 is increased and the extension of the depletion layer is reduced, the depletion layer between adjacent pillars C2 can be in a pinched-off state. By increasing the concentration of the impurity layer 13, the on-resistance can be further reduced.

[0065] Figure 3 : is a graph showing the relationship between the SJ pitch P and the on-resistance. The solid line represents the on-resistance value of each SJ pitch P of the present invention, and the dotted line represents the on-resistance value of each SJ pitch P of the comparative example. Figure 3 As shown in FIG. 1 , in any SJ pitch P, the on-resistance value of the present invention is lower than that of the comparative example. Here, the dot-dash line represents the improvement ratio of the on-resistance value of the present invention relative to the comparative example. Figure 3 As shown, it can be seen that the smaller the SJ pitch P is, the higher the improvement ratio is. That is, as the miniaturization of semiconductor devices continues to advance, the present invention will achieve better effects.

[0066] Next, Figure 1 A method for manufacturing the semiconductor device 1 shown will be described.

[0067] First, a drift layer formation process is performed. In the drift layer formation process, the drift layer 3 is formed on the drain layer 2. Then, three ion implantation processes are performed. In each ion implantation process, first, a resist pattern is formed. Then, ion implantation is performed. Then, the resist pattern is removed. As a result, a p-type ion implantation portion, an n+ type ion implantation portion, and a p+ type ion implantation portion are formed. The p-type ion implantation portion becomes the main body layer 4. The n+ type ion implantation portion becomes the source layer 5. The p+ type ion implantation portion becomes the main body contact layer 6.

[0068] After that, a mask pattern forming step is performed. Figure 4 The steps after the mask pattern forming step will be described. Figure 4 1 is a cross-sectional view for explaining a method for manufacturing a semiconductor device 1. In addition, the second conductive type column is formed in a region where the body layer 4, the source layer 5, and the body contact layer 6 are formed. Figure 4 It is omitted in .

[0069] like Figure 4 As shown in (a), in the mask pattern forming step, a silicon dioxide layer is formed on the drift layer 3. Then, a resist pattern is formed. Then, dry etching is performed. Then, the resist pattern is removed. As a result, a first mask pattern 15 of silicon dioxide is formed.

[0070] The first mask pattern 15 is formed with an opening portion, and the opening portion is located at a position corresponding to a region of a plurality of second conductive type pillars that are not adjacent to each other among a plurality of second conductive type pillars formed in a subsequent process.

[0071] Here, if Figure 4 As shown in (a), a portion of the drift layer 3 is etched. The etching amount at this time is half the amount of a section of the multi-stage sawtooth shape of the outer portion when the second conductive type column formed in the subsequent process is cross-sectionally viewed. For example, the etching amount can be set to 0.25μm. Although not shown, it is also possible to ion-implant impurities before etching the drift layer 3 using the first mask pattern 15. Thereafter, the first mask pattern 15 is removed.

[0072] Next, if Figure 4 As shown in (b), a second mask pattern 16 of silicon dioxide is formed. The second mask pattern 16 is formed thicker than the first mask pattern 15.

[0073] For example, when silicon carbide etching is performed using ICP-RIE in an SF6-O2-Ar atmosphere, the selectivity between the first mask pattern 15 and silicon dioxide as the raw material of the second mask pattern 16 can be 8. In this case, even if the second mask pattern 16 is reduced during the etching process, the ion implantation process and the etching process can still be repeated multiple times using the same mask pattern. For example, when the film thickness of the second mask pattern 16 is set to 2μm, since the selectivity is 8, the silicon carbide layer can be etched until the film thickness reaches 16μm. This means that it is possible to etch deeper than the thickness (about 10μm) of the drift layer 3 of a silicon carbide semiconductor device with a withstand voltage of about 1200V without a super junction structure. Here, not only the etching selectivity should be considered, but also the depth of impurities intruding (penetrating) into the second mask pattern 16 by ion implantation. The thickness of the second mask pattern 16 needs to be appropriately set to prevent impurities from penetrating the second mask pattern 16 and intruding into the drift layer 3. For example, the drift layer 3 is etched by 10 μm using the second mask pattern 16 with a selectivity of 8, and the reduction amount of the second mask pattern 16 is 1.25 μm. In addition, when the second mask pattern 16 acts as a mask during ion implantation, when the mask material is silicon dioxide, its necessary thickness is about 1 μm. In this case, the thickness of the second mask pattern 16 needs to be at least 2.25 μm. Taking into account the manufacturing margin, the thickness of the second mask pattern 16 is preferably 2.5 μm, for example. When the drift layer 3 is 10 μm, the film thickness of the second mask pattern 16 can be, for example, 2.5 μm, so that a semiconductor device 1 with improved on-resistance characteristics can be manufactured more stably.

[0074] The second mask pattern 16 is formed with openings located at positions corresponding to regions where the plurality of second conductive type pillars formed according to the first mask pattern 15 and the plurality of second conductive type pillars adjacent thereto are formed.

[0075] Then, if Figure 4 As shown in (c), an ion implantation process is performed. Specifically, in the ion implantation process, impurities such as aluminum are implanted into the drift layer 3 at a position corresponding to the opening of the second mask pattern 16. At this time, when viewed from above, the ion implantation is performed in such a manner that a portion of the region where the impurities exist extends further outward than the opening of the mask pattern. As a result, a p-type impurity layer 13 is formed.

[0076] Then, if Figure 4 As shown in (d), the etching step is performed directly using the second mask pattern 16. In the etching step, the impurity layer 13 is etched at a position corresponding to the opening of the second mask pattern 16. At this time, the second mask pattern 16 is also reduced according to the etching selectivity.

[0077] Then, if Figure 4As shown in (e), the second mask pattern 16 is directly used to perform the ion implantation step again. Figure 4 (c) is the same as described above. Figure 4 (d) is an etching step having the same contents as described above.

[0078] Afterwards, it will be Figure 4 (c) and the ion implantation step described in Figure 4 The etching step described in (d) is repeated as many times as required. In this way, the ion implantation step and the etching step are performed alternately for a plurality of times. Figure 4 When the last etching step described in (d) is completed, Figure 1 As shown, a multi-level sawtooth impurity layer 13 is formed. Thereafter, a step of removing the second mask pattern 16 is performed. In the mask pattern removing step, the second mask pattern 16 is removed.

[0079] After that, a carbon cap forming step is performed. In the carbon cap forming step, a carbon cap layer is formed. After that, an annealing step is performed. In the annealing step, an annealing treatment is performed in a high temperature atmosphere in order to activate the impurity elements (dopants) implanted by ions. After that, a carbon cap removing step is performed. In the carbon cap removing step, the carbon cap layer is removed.

[0080] Then, a filling process is performed. In the filling process, silicon dioxide is used to fill the groove formed by the etching process, for example, by a method such as a CVD method. Then, an etch-back process is performed. In the etch-back process, silicon dioxide is removed to the upper surface of the drift layer 3. As a result, a filling layer 14 is formed.

[0081] Then, a gate insulating layer forming step is performed. In the gate insulating layer forming step, a gate insulating film is formed by a method such as a thermal oxidation method. Then, a resist pattern is formed. Then, the gate insulating film is etched. Then, the resist pattern is removed. As a result, a gate insulating layer 7 is formed.

[0082] Thereafter, a gate electrode layer forming step is performed. In the gate electrode layer forming step, a polysilicon film is formed by a method such as a CVD method. Thereafter, a resist pattern is formed. Thereafter, the polysilicon film is etched. Thereafter, the resist pattern is removed. As a result, a gate electrode layer 8 is formed. Thereafter, a source electrode layer forming step is performed. In the source electrode layer forming step, a metal film such as Ni is formed by a method such as a sputtering method. Thereafter, a resist pattern is formed. Thereafter, the metal film is etched. Thereafter, the resist pattern is removed. Thereafter, a heat treatment such as metal sintering is performed. As a result, a source electrode layer 10 is formed.

[0083] After that, an interlayer insulating layer forming step is performed. In the interlayer insulating layer forming step, an interlayer insulating layer 9 of silicon dioxide or the like is formed by a method such as a CVD method. After that, a wiring electrode layer forming step is performed. In the wiring electrode layer forming step, a wiring electrode layer 11 of aluminum alloy or the like is formed by a method such as a sputtering method. After that, a drain electrode layer forming step is performed. In the drain electrode layer forming step, a metal film of Ni or the like is formed by a method such as a sputtering method. After that, a heat treatment such as laser annealing is performed. As a result, a drain electrode layer 12 is formed.

[0084] Next, use Figure 5 , a method for forming the second conductivity type impurity layer 13 is described.

[0085] Figure 5 This is a diagram for explaining a method for forming a second conductivity type impurity layer in the semiconductor device in the first embodiment.

[0086] Figure 5 1 shows the profile of the silicon carbide drift layer 3 when ion implantation is performed from the top of the figure, and aluminum is implanted as an impurity into a central point of the silicon carbide drift layer 3. Figure 5 As shown in FIG. 1 , in each ion implantation step, the impurities radially spread into the drift layer 3 of silicon carbide. At this time, the impurities reach a depth of, for example, about 0.5 μm to 0.7 μm. In addition, the lateral expansion of the impurities is, for example, 0.2 μm to 0.3 μm. Figure 5 Although not shown, by etching the drift layer 3 of silicon carbide as described above, this ion implantation is repeatedly performed at different depths, so that in each of the plurality of second conductive type columns C2, the plurality of first inclined portions A1 and the plurality of second inclined portions A2 on the outer side are alternately arranged along the thickness direction of the drift layer 3 and are formed into a multi-level serrated shape.

[0087] According to the embodiment 1 described above, the plurality of second conductive type columns C2 have a multi-level sawtooth outer portion when viewed in cross section, and the multi-level sawtooth outer portions of the plurality of second conductive type columns C2 are configured to be interlocked with the multi-level sawtooth outer portions of other adjacent second conductive type columns. That is, the adjacent second conductive type columns C2 are configured to be offset from each other by half of a section of the sawtooth outer portion in the depth direction. The second conductive type columns C2 are formed by the impurity layer 13 and the filling layer 14. Therefore, it is possible to easily manufacture a semiconductor device 1 having a super junction structure with improved on-resistance characteristics.

[0088] Furthermore, in a cross-sectional view of the plurality of second conductivity type columns C2, there may be no impurity layer 13 above the body layer 4 or the body contact layer 6. In this case, the number of ion implantation steps is reduced, and the semiconductor device 1 with improved on-resistance characteristics can be manufactured at a lower cost.

[0089] In addition, the filling layer 14 is formed of an insulator or a semiconductor. Therefore, the semiconductor device 1 having improved on-resistance characteristics can be manufactured more easily.

[0090] In addition, the impurity concentration of the impurity layer 13 is 1.0×10 17 cm -3 Above and 1.0×10 20 cm -3 Therefore, it is possible to obtain improved on-resistance characteristics more reliably.

[0091] In addition, the first conductivity type column C1 is formed of the first conductivity type silicon carbide, and the impurity layer 13 is formed of the second conductivity type silicon carbide. Therefore, in the silicon carbide semiconductor device 1, the on-resistance characteristics are improved, and stable manufacturing is possible.

[0092] In addition, a plurality of second conductivity type columns C2 are formed in the drift layer 3 so that the outer portion thereof has a multi-stage sawtooth shape in cross-sectional view. Therefore, the semiconductor device 1 having improved on-resistance characteristics can be easily manufactured.

[0093] In addition, by repeatedly performing the etching process and the ion implantation process, a plurality of second conductive type columns C2 are formed, so that the outer portion thereof becomes a multi-level sawtooth shape when viewed in cross section. In the etching process, the mask pattern is repeatedly used. Therefore, it is not necessary to perform film formation of a mask silicon dioxide layer, photolithography, etching, resist removal, and mask removal at each stage.

[0094] Without using the present invention, one method of forming an impurity layer in the groove sidewall portion of the column C2 in the area with a higher aspect ratio is to perform ion implantation obliquely from the opening. As the aspect ratio of the groove increases, the ion implantation angle gradually approaches the horizontal direction from the direction perpendicular to the groove sidewall of the column C2. In this case, the ions are reflected at the surface and it is difficult to penetrate into the groove sidewall, resulting in low efficiency of ion implantation. In order to make the impurity layer 13 reach the necessary impurity concentration, it is necessary to increase the dose instead of performing ion implantation vertically, which will result in a longer processing time and reduce production efficiency. In addition, it becomes difficult to equalize the concentration of the impurity layer 13 in the upper and lower parts of the column C2.

[0095] In the ion implantation method of the present invention, lateral diffusion in the silicon carbide drift layer 3 by vertical ion implantation can be utilized. Therefore, the difficulty of the above-mentioned ion implantation process is reduced. As a result, a semiconductor device 1 with improved on-resistance characteristics can be easily manufactured.

[0096] Furthermore, in the ion implantation step, ions are implanted into a region partially containing impurities in a plan view, so that the ions extend outward beyond the opening of the mask pattern. Therefore, the semiconductor device 1 having improved on-resistance characteristics can be easily manufactured.

[0097] In addition, after the ion implantation process and the etching process are repeated, the groove formed by the etching process is filled with an insulator or a semiconductor. Therefore, compared with filling the second conductive type silicon carbide by epitaxy, it is more difficult to generate a void. As a result, it is possible to easily manufacture a semiconductor device 1 with improved on-resistance characteristics.

[0098] In addition, the semiconductor device 1 may also be a trench MOSFET of silicon carbide having a super junction structure. In the trench MOSFET semiconductor device 1, the plurality of second conductive type columns C2 also have a multi-level sawtooth outer portion when viewed in cross section, and the multi-level sawtooth outer portions of the plurality of second conductive type columns C2 are configured to be interlocked with the multi-level sawtooth outer portions of other adjacent second conductive type columns. That is, the adjacent second conductive type columns C2 are configured to be offset from each other by half of a section of the sawtooth outer portion in the depth direction. The second conductive type column C2 is formed by an impurity layer 13 and a filling layer 14. Therefore, it is possible to easily manufacture a trench MOSFET semiconductor device 1 having a super junction structure with improved on-resistance characteristics.

[0099] In the semiconductor device 1 of the first embodiment, the first conductivity type may be the p-type and the second conductivity type may be the n-type. In this case, improved on-resistance characteristics can be obtained as well.

[0100] Furthermore, the structure of the first embodiment can also be applied to a semiconductor device 1 mainly composed of silicon. In this case, improved on-resistance characteristics can be obtained as well.

[0101] Although some aspects of at least one embodiment have been described above, it should be understood that various changes, modifications and improvements may be easily conceived by those skilled in the art. The changes, modifications and improvements involved are intended to become part of this disclosure and are intended to be within the scope of this disclosure.

[0102] It should be understood that the implementation of the method and apparatus described herein is not limited to the details of the structure and arrangement of the components described in the above description or illustrated in the accompanying drawings. The method and apparatus can be implemented in other embodiments and implemented or executed in various ways.

[0103] The specific embodiments are provided herein only by way of example and are not meant to be limiting.

[0104] The expressions and terms used in this disclosure are for illustrative purposes only and should not be considered as limiting. The use of "includes," "having," "having," "comprising," and variations thereof as used herein means the inclusion of the following listed items, their equivalents, and additional items.

[0105] Reference to "or" may be interpreted as one or more of any terms recited using "or", as well as interpretation of all terms.

[0106] References to front, back, left, right, top, bottom, up, down, horizontal, vertical, inside and outside are for convenience of description. Such references do not mean that the constituent elements of the present disclosure are limited to any particular position or spatial orientation. Therefore, the above description and drawings are only for illustration.

[0107] In addition, it is needless to say that the present disclosure is not limited to the embodiments described above, but includes all embodiments that can achieve the purpose of the present invention.

[0108] The term "embodiment" in this disclosure refers to specific features, structures, or characteristics described in conjunction with the embodiment that may be included in at least one embodiment of the present application. The appearance of this phrase in various locations in the specification does not necessarily mean the same embodiment, nor does it mean that it is mutually exclusive with other embodiments and is independent or optional. It is clearly or implicitly understood by those of ordinary skill in the art that the embodiments described in this application can be combined with other embodiments without conflict.

[0109] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of patent protection. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the scope of protection of the present application. Therefore, the scope of protection of the present application shall be subject to the attached claims.

Claims

1. A semiconductor device, characterized in that: include: a drain layer, wherein the drain layer is formed of a first conductive type semiconductor; a drift layer, wherein the drift layer is formed of a first conductive type semiconductor on one side of the drain layer; as well as A column structure, wherein in the drift layer, a plurality of first conductive type columns and a plurality of second conductive type columns are alternately arranged; The second conductive type column has a multi-stage sawtooth outer portion when viewed in cross section; The multi-stage sawtooth outer portion of the second conductive type pillar has a super junction structure, and the super junction structure is configured to be embedded with the multi-stage sawtooth outer portion of another adjacent second conductive type pillar.

2. The semiconductor device according to claim 1, wherein: The second conductive column has: a second conductivity type impurity layer; and A filling layer is formed inside the impurity layer.

3. The semiconductor device according to claim 2, wherein: The filling layer is formed of an insulator or a semiconductor.

4. The semiconductor device according to claim 2 or 3, characterized in that The impurity concentration of the impurity layer is 1.0×10 17 cm -3 Above and 1.0×10 20 cm -3 the following.

5. The semiconductor device according to claim 1, wherein: The distance between any adjacent second conductive type pillars is less than 4 μm.

6. The semiconductor device according to claim 2 or 3, characterized in that: The first conductive type column is formed of first conductive type silicon carbide; The impurity layer is formed of second conductivity type silicon carbide.

7. A method for manufacturing a semiconductor device, characterized in that: include: a drift layer forming step of forming a first conductivity type drift layer by epitaxial growth on the drain layer formed of the first conductivity type semiconductor; as well as, A second conductive type pillar forming step, in which a plurality of second conductive type pillars are formed in the drift layer so as to have a multi-stage sawtooth outer portion in cross-sectional view; The second conductive type column forming step comprises: A first step, the first step comprising: an etching process, in which etching is performed using a first mask having an opening formed therein at a position corresponding to a region where a plurality of second conductive type pillars that are not adjacent to each other are formed among the plurality of second conductive type pillars; The second step includes: an ion implantation process, in which impurities are implanted using a second mask, the second mask is formed with an opening position, and the opening position corresponds to the area formed by the multiple second conductive type columns formed in the first step and the multiple second conductive type columns adjacent thereto; and an etching process, in which the second mask is still used to etch a portion of the ion implantation area.

8. The method for manufacturing a semiconductor device according to claim 7, wherein: The depth of etching performed by the etching process in the first step is half the depth of etching performed by the etching process in the second step.

9. The method for manufacturing a semiconductor device according to claim 7, wherein: By repeatedly performing the ion implantation step and the etching step in the second step, a plurality of second conductive type pillars are formed so that the outer portion has a multi-stage sawtooth shape in cross-sectional view.

10. The method for manufacturing a semiconductor device according to claim 7 or 9, characterized in that: In the ion implantation step, ion implantation is performed so that a portion of a region where the impurity exists extends outward from an opening of the mask when viewed from above.

11. The method for manufacturing a semiconductor device according to claim 9 or 10, characterized in that: After repeatedly performing the ion implantation process and the etching process in the second step, a filling process is further included in which the groove formed by the etching process is filled with an insulator or a semiconductor.