Memory device, semiconductor device and preparation method thereof
By forming a doped nitride insulating layer and isolation layer on the top surface and sidewalls of the gate structure of the semiconductor device, the spacing between adjacent gate structures is increased, which solves the problem of increased parasitic capacitance and improves the performance and speed of the device.
Patent Information
- Application Number
- CN202410797120.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-19
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2044-06-19
AI Technical Summary
As the integration level of semiconductor chips increases, the spacing between gate structures of adjacent transistors shrinks, resulting in an increase in parasitic capacitance and affecting device performance and speed.
Design a semiconductor device that increases the spacing between adjacent gate structures and reduces parasitic capacitance by forming a doped nitride insulating layer on the top surface and sidewalls of the gate structure, and setting an isolation layer on the sidewalls. The device includes a substrate, a gate structure, a sidewall structure and an insulating layer. The sidewall structure includes a first sidewall and a second sidewall. The insulating layer covers the gate structure and the sidewall, and the insulating layer is doped nitride. layer to improve etching resistance.
It effectively reduces the parasitic capacitance between adjacent gate structures, improves the etching resistance of the insulating layer, ensures the integrity of the interconnect layer in subsequent processes, and improves device performance and speed.
Smart Images

Figure CN118738094A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present disclosure relate to the semiconductor field, and in particular to a memory device, a semiconductor device, and a method for manufacturing the same. Background Art
[0002] As semiconductor chips develop towards higher integration, the characteristic size of semiconductor devices is gradually shrinking, the spacing between the gate structures of adjacent transistors is getting smaller and smaller, and the parasitic capacitance is also increasing, which may lead to the performance or operation speed of the semiconductor device being degraded. At present, it is necessary to propose a new semiconductor device and its preparation method. Summary of the invention
[0003] According to some embodiments of the present disclosure, on one hand, an embodiment of the present disclosure provides a semiconductor device, including:
[0004] substrate;
[0005] A gate structure, located on the substrate, the gate structure comprising a gate oxide layer and a gate conductive layer stacked in sequence;
[0006] A sidewall structure covering the sidewall of the gate structure, wherein the sidewall structure comprises a first sidewall and a second sidewall;
[0007] an insulating layer, wherein the insulating layer covers a top surface of the gate structure, a top surface of the first sidewall and a first surface of the second sidewall, and the insulating layer is a doped nitride layer;
[0008] The source and the drain are located in the substrate on both sides of the gate structure.
[0009] In some embodiments, the spacer structure further includes an isolation layer located on the second surface of the second spacer, the isolation layer includes a first isolation layer and a second isolation layer, and the first isolation layer is located between the second spacer and the second isolation layer.
[0010] In some embodiments, the semiconductor device also includes a contact structure, and in a direction parallel to the substrate, the total width of the insulating layer and the contact structure located in the insulating layer is greater than the width of the gate structure, and is smaller than the total width of the gate structure and the isolation layer, the first side wall and the second side wall perpendicular to the substrate direction.
[0011] In some embodiments, in a direction parallel to the substrate, a total width of the insulating layer and the contact structure within the insulating layer is equal to a total width of the gate structure and the first isolation layer, the first side wall and the second side wall perpendicular to the substrate direction.
[0012] In some embodiments, the second isolation layer is the doped nitride layer, and the doping elements of the gate insulation layer and the second isolation layer are one or more of boron, phosphorus, arsenic or carbon.
[0013] In some embodiments, the first isolation layer is the doped nitride layer, and the first isolation layer and the second isolation layer have a concentration gradient of doping elements in a direction parallel to the substrate.
[0014] In some embodiments, materials of the first spacer and the second spacer are silicon nitride and silicon oxide, respectively.
[0015] According to some embodiments of the present disclosure, another aspect of the present disclosure further provides a method for preparing a semiconductor device, comprising:
[0016] providing a substrate;
[0017] forming a gate structure, the gate structure being located on the substrate, the gate structure comprising a stacked gate oxide layer and a gate conductive layer;
[0018] forming an insulating layer, wherein the insulating layer covers the top surface of the gate structure, the top surface of the first sidewall and the first surface of the second sidewall, and the insulating layer is a doped nitride layer;
[0019] A source and a drain are formed, wherein the source and the drain are located in the substrate at both sides of the gate structure.
[0020] In some embodiments, the steps of forming a gate structure and a sidewall structure include: depositing and patterning a stacked gate oxide material layer and a first gate conductive material layer on the substrate in sequence to form the gate oxide layer and the first gate conductive layer, the gate oxide layer and the first gate conductive layer constituting an initial gate structure; depositing a first sidewall material layer and a second sidewall material layer on the initial gate structure and the substrate in sequence, removing a portion of the first sidewall material layer and the second sidewall material layer located on the top surface of the gate structure and the substrate to form the first sidewall and the second sidewall covering the sidewall of the gate structure and a portion of the substrate; depositing a metal layer on the top surface of the initial gate structure, and annealing to form a second gate conductive layer, the gate oxide layer, the first gate conductive layer and the second gate conductive layer constituting the gate structure.
[0021] In some embodiments, the step of forming an insulating layer includes: forming an initial insulating layer on the substrate, the gate structure, the first side wall and the second side wall, removing the initial insulating layer located on the side wall of the gate structure, and retaining the initial insulating layer on the surface of the substrate, the top surface of the gate structure, the top surface of the first side wall and the first surface of the second side wall to form the insulating layer.
[0022] In some embodiments, the step of forming an initial insulating layer on the substrate, the gate structure, the first sidewall and the second sidewall includes: performing a deposition process to form the nitride layer covering the first surface of the substrate, the gate structure, the first sidewall and the second sidewall, the nitride layer including silicon nitride; performing an ion implantation process on the nitride layer to form the initial insulating layer of the nitride layer including doped elements, wherein the initial insulating layer located on the substrate, the top surface of the gate structure, the top surface of the first sidewall and the first surface of the second sidewall has a different concentration of doped elements from the initial insulating layer located on the sidewall of the gate structure.
[0023] In some embodiments, the deposition process and the ion implantation process are performed alternately and cyclically.
[0024] In some embodiments, the step of removing the initial insulating layer located on the sidewall of the gate structure, retaining the initial insulating layer on the surface of the substrate, the top surface of the gate structure, the top surface of the first sidewall, and the first surface of the second sidewall to form the insulating layer includes: removing the initial insulating layer located on the sidewall of the gate structure by wet etching, retaining the initial insulating layer on the surface of the substrate, the top surface of the gate structure, the top surface of the first sidewall, and the first surface of the second sidewall, wherein the etching selectivity of the initial insulating layer located on the surface of the substrate and the top surface of the gate structure to the initial insulating layer located on the top surface of the gate structure, the top surface of the first sidewall, and the first surface of the second sidewall in the wet etching is in the range of 1:3 to 1:10.
[0025] In some embodiments, the spacer structure further includes an isolation layer located on the second surface of the second spacer, and the isolation layer is formed by the same process as that of the insulating layer.
[0026] According to some embodiments of the present disclosure, a third aspect of the embodiments of the present disclosure further provides a storage device, which is formed by bonding a target wafer containing the semiconductor device and a bonding wafer; the bonding wafer includes a control circuit and a bonding interface, and the storage device is bonded to the bonding interface of the bonding wafer through the bonding layer of the target wafer.
[0027] According to an embodiment of the present disclosure, an insulating layer is provided on the top surface of the gate structure, the top surface of the first side wall, and the first surface of the second side wall, and the insulating layer is a doped nitride layer, thereby effectively improving the etching resistance of the insulating layer. Thus, a side wall structure including a first side wall and a second side wall can be formed in a subsequent process, thereby effectively increasing the spacing between adjacent gate structures, thereby reducing the parasitic capacitance between adjacent gate structures. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] One or more embodiments are exemplarily illustrated by pictures in the corresponding drawings, and these exemplified descriptions do not constitute a limitation on the embodiments. Unless otherwise specified, the pictures in the drawings do not constitute a scale limitation. In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the traditional technology, the drawings required for use in the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0029] Figure 1 It is a schematic diagram of the structure of a semiconductor device in one embodiment of the present disclosure.
[0030] Figure 2 A schematic flow chart of a method for preparing a semiconductor device is provided.
[0031] Figures 3 to 10 A schematic structural diagram corresponding to each step of a method for preparing a semiconductor device provided in one embodiment of the present disclosure.
[0032] Fig.11 Schematic diagram of the process steps for bonding to form a memory device. DETAILED DESCRIPTION
[0033] The following will describe the various embodiments of the present disclosure in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present disclosure, many technical details are provided in order to enable the reader to better understand the present disclosure. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solutions claimed in the present disclosure can be implemented.
[0034] An embodiment of the present disclosure provides a semiconductor device, which will be described below in conjunction with the accompanying drawings.
[0035] Figure 1 It is a schematic diagram of the structure of a semiconductor device in one embodiment of the present disclosure; Figure 2 A schematic diagram of a process for preparing a semiconductor device is provided; Figures 3 to 10 A schematic structural diagram corresponding to each step of a method for preparing a semiconductor device provided in one embodiment of the present disclosure; Fig.11 Schematic diagram of the process steps for bonding to form a memory device.
[0036] refer to Figure 1The semiconductor device 10 provided by the embodiment of the present disclosure includes: a substrate 100; a gate structure 102, located on the substrate 100, the gate structure 102 includes a gate oxide layer 1021 and a gate conductive layer 1022 stacked in sequence; a sidewall structure SW, covering the sidewall of the gate structure 102, the sidewall structure includes a first sidewall 103 and a second sidewall 104; an insulating layer 110, the insulating layer 110 covers the top surface of the gate structure 102, the top surface of the first sidewall 103 and the first surface S1 of the second sidewall 104, and the insulating layer 110 is a doped nitride layer; a source 105 and a drain 106, located in the substrate on both sides of the gate structure. The following will be described in detail with reference to the accompanying drawings.
[0037] Continue to refer Figure 1 The substrate 100 includes a shallow trench isolation (STI) 101 and an active area AA. In some embodiments, the material of the semiconductor substrate 100 may include semiconductor materials such as silicon, germanium, silicon germanium, gallium arsenide, etc., or may be a composite structure such as silicon on insulator, which is not limited here.
[0038] The gate structure 102 includes a gate oxide layer 1021 and a gate conductive layer 1022 stacked in sequence. In some embodiments, the gate conductive layer 1022 may also include a first gate conductive layer CT1 and a second gate conductive layer CT2, wherein the material of the gate oxide layer 1021 may be silicon oxide, silicon oxynitride or a high-k dielectric material; the first gate conductive layer CT1 and the second gate conductive layer CT2 may be polysilicon, metal or metal silicide, wherein the metal may be titanium Ti, cobalt Co, nickel Ni, aluminum Al, tungsten W, etc., and the metal silicide may be cobalt silicide CoSi, nickel silicide NiSi, etc., which are not limited here. In other embodiments, a work function adjustment layer or a diffusion barrier layer, such as titanium nitride TiN, may also be provided between the gate oxide layer 1021 and the gate conductive layer 1022.
[0039] The spacer structure SW covers the sidewall of the gate structure 102 . The spacer structure 102 includes a first spacer 103 and a second spacer 104 . In some embodiments, the materials of the first spacer 103 and the second spacer 104 can be silicon nitride or silicon oxide, respectively.
[0040] In some embodiments, the spacer structure SW further includes an isolation layer 111 located on the second surface S2 of the second spacer SW, the isolation layer 111 includes a first isolation layer 1111 and a second isolation layer 1112, and the first isolation layer 1111 is located between the second spacer 104 and the second isolation layer 1112. The spacer structure SW includes only the first spacer 103 and the second spacer 104, which effectively increases the spacing between adjacent gate structures 102, thereby reducing the parasitic capacitance between adjacent gate structures 102.
[0041] In some embodiments, the materials of the first sidewall 103 and the second sidewall 104 may be silicon nitride and silicon oxide, respectively. In other embodiments, the material of the second sidewall 104 may also be other materials with high dielectric constants. Since the material of the second sidewall 104 is silicon oxide, which has a dielectric constant greater than that of silicon nitride, the parasitic capacitance between the gate structures 102 can be further reduced by setting the material of the second sidewall 104 to silicon oxide.
[0042] The insulating layer 110 covers the top surface of the gate structure 102, the top surface of the first sidewall 103, and the first surface S1 of the second sidewall 104, wherein the insulating layer 110 may be a doped nitride layer, exemplarily, the nitride layer may be silicon nitride, and the doping element may be one or more of boron, phosphorus, arsenic, or carbon. By setting the insulating layer 110 on the top surface of the gate structure 102, the top surface of the first sidewall 103, and the first surface S1 of the second sidewall 104, and the insulating layer 110 is a doped nitride layer, the doping element may be one or more of boron B, phosphorus P, arsenic As, or carbon C. Exemplarily, when the doping element is boron, as the boron content increases, the etching resistance will also increase. Therefore, by setting the insulating layer 110 as a doped nitride layer, the etching resistance of the insulating layer 110 can be effectively improved, and when performing subsequent processes, the insulating layer 110 can be completely retained as a stop layer when forming an interconnection layer. In some embodiments, the molar concentration range of the doping element of the insulating layer 110 is 5% to 8%. For example, when the doping element is boron and the molar concentration of doped boron is 5% to 8%, the etching resistance of the insulating layer 110 can be maintained within a reasonable range and can be effectively removed when it is necessary to remove the insulating layer 110.
[0043] In some embodiments, the second isolation layer 1112 may also be a doped nitride layer, and the doping element may be one or more of boron B, phosphorus P, arsenic As or carbon C. For example, when the doping element is boron, as the boron content increases, the etching resistance will also increase. Therefore, by setting the second isolation layer 1112 as a doped nitride layer, the etching resistance of the second isolation layer 1112 can be effectively improved. When performing subsequent processes, it can be used together with the insulating layer 110 as a stop layer when forming an interconnection layer and can be completely retained. In some embodiments, the molar concentration of the doping element of the second isolation layer 1112 is in the range of 5% to 8%. For example, when the doping element is boron, when the molar concentration of the doped boron is 5% to 8%, the etching resistance of the second isolation layer 1112 can be maintained within a reasonable range, and the second isolation layer 1112 can be effectively removed when it is necessary to remove it.
[0044] In some embodiments, the first isolation layer 1111 may also be a doped nitride layer, and the doping element may be one or more of boron B, phosphorus P, arsenic As or carbon C. Exemplarily, the molar concentration of the doping element of the first isolation layer 1111 may be in the range of 1% to 3%. Exemplarily, when the doping element is boron, when the molar concentration of doped boron is in the range of 1% to 3%, the etching resistance of the first isolation layer 1111 can be maintained within a reasonable range, so that the first isolation layer 1111 and the second sidewall 104 have a certain etching selectivity ratio. In the subsequent process, when the first isolation layer 1111 needs to be removed, the second sidewall 104 is prevented from being over-etched. In other embodiments, the doping element concentrations of the first isolation layer 1111 and the second isolation layer 1112 may also be set in a gradient, that is, the first isolation layer 1111 decreases uniformly toward the second isolation layer 1112, thereby effectively preventing the second sidewall 104 from being over-etched.
[0045] In some embodiments, the thickness of the insulating layer 110 and the isolation layer 111 may be in the range of 15 nm to 30 nm, which can ensure that they are completely retained when used as stop layers in subsequent processes.
[0046] In some embodiments, the semiconductor device 10 further includes a contact structure CP. In a direction parallel to the substrate 100, a total width d1 of the insulating layer 110 and the contact structure CP in the insulating layer 110 may be greater than a width d2 of the gate structure 102, and less than a total width d3 of the gate structure 102 and the isolation layer, the first sidewall 103, and the second sidewall 104 perpendicular to the substrate 100. Thus, when used as a stop layer in subsequent processes, the integrity of the gate structure 102 and the sidewall structure SW can be effectively protected. The contact structure CP may include a transition layer 114 and a metal layer 115. The contact structure CP is used to realize electrical connection between the gate structure 102, the source 105, and the drain 106 and other devices or control circuits. The material of the transition layer 114 may include titanium nitride, metal silicide, etc., and the material of the metal layer 115 may include one or more of metal silicide, metal compound, metal alloy, and metal. In other embodiments, a contact layer may also be provided between the contact structure CP and the gate structure 102, the source 105 and the drain 106, for example, a source contact layer 107, a drain contact layer 108 and a second gate conductive layer CT2. By way of example, the material of the contact layer may include metal silicide, such as cobalt silicide CoSi, nickel silicide NiSi, etc., to reduce the contact resistance between the contact structure CP and the gate structure 102, the source 105 and the drain 106.
[0047] In some embodiments, in a direction parallel to the substrate 100, a width d1 of the insulating layer 110 is equal to a total width d4 of the gate structure 102 and the first isolation layer 1111, the first sidewall 103, and the second sidewall 104 perpendicular to the substrate 100, to ensure that the sidewall structure SW is not over-etched in subsequent processes.
[0048] The source 105 and the drain 106 are located in the substrate 100 on both sides of the gate structure 102, and together with the gate structure 102 constitute a transistor. Exemplarily, the transistor can be a MOSFET (metal-oxide-semiconductor field-effect transistor), and can further be divided into NMOS or PMOS according to the different doping elements of the source 105 or the drain 106.
[0049] In some embodiments, the semiconductor device 10 further includes a dielectric layer 113 for isolating different functional devices, wherein the material of the dielectric layer 113 may include silicon oxide, and the dielectric layer 113 is partially filled between the gate structures 102, thereby further reducing the parasitic capacitance between the gate structures 102.
[0050] Correspondingly, another embodiment of the present disclosure provides a method for preparing a semiconductor device, which can be used to form the above-mentioned semiconductor device.
[0051] Figure 2 A flowchart of a method for preparing a semiconductor structure provided by an embodiment of the present disclosure is provided. Figure 3-Figure 10 This is a structural schematic diagram corresponding to each step of a semiconductor device preparation method provided in one embodiment of the present disclosure. The preparation method of the semiconductor structure provided in this embodiment will be described in detail in conjunction with the accompanying drawings. The parts that are the same or corresponding to the above-mentioned embodiments will not be described in detail below.
[0052] In step S100 , a substrate 100 is provided.
[0053] In some embodiments, reference Figure 3 , a plurality of active areas AA and shallow isolation trenches 101 arranged at intervals are formed in the substrate 100, wherein the material of the substrate 100 may be single crystal silicon (Si), single crystal germanium (Ge), or silicon germanium (GeSi), silicon carbide (SiC), or silicon on insulator (SOI), germanium on insulator (GOI); or other materials, such as III-V compounds such as gallium arsenide. The shallow isolation trenches 101 may be formed by the following steps: forming a trench in the substrate 100, and filling the trench with an insulating material such as silicon oxide (SiO2) or silicon nitride (SiN).
[0054] In step S200 , a gate structure 102 is formed. The gate structure 102 is located on the substrate 100 . The gate structure 102 includes a gate oxide layer 1021 and a gate conductive layer 1022 that are stacked.
[0055] In step S300 , a spacer structure SW is formed. The spacer structure SW covers the sidewall of the gate structure 102 . The spacer structure 102 includes a first spacer 103 and a second spacer 104 .
[0056] Step S400: forming an insulating layer 110, the insulating layer 110 covers the top surface of the gate structure 102, the top surface of the first spacer 103 and the first surface S1 of the second spacer 104, and the insulating layer 110 is a doped nitride layer;
[0057] In step S500 , a source 105 and a drain 106 are formed. The source 105 and the drain 106 are located in the substrate 100 on both sides of the gate structure 102 .
[0058] In some embodiments, reference Figure 3-Figure 10 , a stacked gate oxide material layer and a first gate conductive material layer can be deposited in sequence on the active area AA, and then a patterned etching process is performed to form a gate oxide layer 1021 and a first gate conductive layer CT1 stacked in a direction perpendicular to the substrate 100, and the gate oxide layer 1021 and the first gate conductive layer CT1 constitute an initial gate structure.
[0059] Continue to form a first sidewall 103 and a second sidewall 104 on the sidewall surface of the initial gate structure. The formation method includes: forming a first sidewall material layer and a second sidewall material layer on the surface of the substrate 100 and the surface of the initial gate structure, and then etching the first sidewall material layer and the second sidewall material layer using a maskless etching process to remove the first sidewall material layer and the second sidewall material layer located on the surface of the substrate 100 and the top surface of the initial gate structure to form the first sidewall 103 and the second sidewall 104 located on the sidewall surface of the initial gate structure. Exemplarily, the materials of the first sidewall 103 and the second sidewall 104 can be silicon nitride and silicon oxide, respectively. The thickness of the first sidewall 103 can be 2nm to 15nm, and the thickness of the second sidewall 104 can be 1nm to 10nm. The formation process of the first sidewall 103 and the second sidewall 104 can be chemical vapor deposition (CVD), atomic layer deposition (ALD) or physical vapor deposition (PVD). The first sidewall 103 and the second sidewall 104 are used to protect the sidewalls of the initial gate structure and can define the area for ion implantation when the source and drain are subsequently formed. Since the thickness range of the first sidewall 103 and the second sidewall 104 is small, the spacing between the initial gate structures can be increased, which is beneficial to reducing the parasitic capacitance between the initial gate structures. At the same time, since the material of the second sidewall 104 is silicon oxide, the dielectric constant of which is greater than that of silicon nitride, therefore, by setting the material of the second sidewall 104 to be silicon oxide, the parasitic capacitance between the initial gate structures can also be further reduced.
[0060] In some embodiments, after forming the first side wall 103, the initial gate structure and the first side wall 103 are used as masks to perform lightly doped ion implantation in the substrate 100 on both sides of the initial gate structure to form a lightly doped drain (LDD) to improve the short channel effect of the formed semiconductor device, and then form the second side wall 104, which is not limited here.
[0061] A source 105 and a drain 106 are formed in the substrate 100 on both sides of the initial gate structure. Specifically, the drain 106 can be formed in the substrate 100 between the two initial gate structures, and the source 105 is formed on both sides of the two initial gate structures, wherein the source 105 and the drain 106 can be interchangeable according to actual applications and device functions, and are not limited here. Exemplarily, the process of forming the source 105 and the drain 106 can be an ion implantation process, using the initial gate structure, the first sidewall 103 and the second sidewall 104 as masks, performing P-type or N-type ion implantation on the substrate 100 on both sides of the initial gate structure, and performing annealing to form the source 105 and the drain 106.
[0062] In some embodiments, after forming the source 105 and the drain 106, a contact layer is further formed on the source 105, the drain 106 and the top surface of the initial gate structure, for example, a source contact layer 107, a drain contact layer 108 and a second gate conductive layer CT2, wherein the material of the contact layer may be a metal silicide layer, for example, cobalt silicide CoSi, nickel silicide NiSi, etc., to reduce the contact resistance between the contact structure CP formed in the subsequent process and the gate structure 102, the source 105 and the drain 106. Exemplarily, the method for forming the contact layer may include: forming a metal layer covering the source 105, the drain 106 and the top surface of the initial gate structure and performing an annealing treatment, so that metal atoms in the metal layer react with atoms on the top surface of the initial gate structure and the surfaces of the source 105 and the drain 106, and forming the second gate conductive layer CT2, the source contact layer 107 and the drain contact layer 108 on the top surface of the initial gate structure and the surfaces of the source 105 and the drain 106, and then removing the remaining metal layer. Specifically, an evaporation or sputtering process may be used to form a metal layer covering the source 105, the drain 106 and the top surface of the initial gate structure, and a furnace tube or other high-temperature annealing equipment may be used to rapidly anneal in a high-purity nitrogen environment at a temperature of 300°C to 500°C to form a metal silicide, and then wet or dry etching may be used to remove excess metal to form a source contact layer 107, a drain contact layer 108 and a second gate conductive layer CT2. Exemplarily, the material of the metal layer may also be one or more metals including Ni, Ta, Ti, W, Co, Pt or Pd, and the material of the formed metal silicide may be SiNi, SiTa, SiTi or NiSiPt, wherein the first gate conductive layer CT1 and the second gate conductive layer CT2 together constitute the gate conductive layer 102, and in other embodiments, the gate conductive layer 102 may also only include the first gate conductive layer CT1 or the second gate conductive layer CT2, which is not limited here, and the gate conductive layer 1022 and the gate oxide layer 1021 together constitute the gate structure 102.
[0063] In some embodiments, reference Figure 6-Figure 10 An initial insulating layer 109 can be formed on the substrate 100, the gate structure 102, the top surface of the first spacer 103 and the second spacer 104, and the initial insulating layer 109 located on the side wall of the gate structure 102 is removed, and the initial insulating layer 109 on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first spacer 103 and the first surface S1 of the second spacer 104 is retained to form an insulating layer 110.
[0064] Specifically, a deposition process may be first performed to form a nitride layer covering the substrate 100, the gate structure 102, the first sidewall 103 and the first surface S1 of the second sidewall 104. Exemplarily, the nitride layer may include silicon nitride, the deposition process may be CVD, ALD or PVD, the reaction gas may be ammonia NH3 and dichlorosilane SiH2Cl2, and the reaction temperature may range from 300°C to 500°C; an ion implantation process may be performed on the nitride layer to form an initial insulating layer 109 of the nitride layer including doped elements. Exemplarily, the ion implanted elements may be one or more of boron B, phosphorus P, arsenic As or carbon C. The initial insulating layer 109 located on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first spacer 103, and the first surface S1 of the second spacer 104 has a different concentration of doping elements from the initial insulating layer 109 located on the sidewall of the gate structure 102. For example, since the ion implantation process is implanted perpendicular to the substrate direction, the initial insulating layer 109 located on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first spacer 103, and the first surface S1 of the second spacer 104 has a different concentration of doping elements from the initial insulating layer 109 located on the sidewall of the gate structure 102. 2, the top surface of the first sidewall 103 and the first surface S1 of the second sidewall 104, the molar concentration range of the doping element of the initial insulating layer 109 is 5% to 8%, and the molar concentration range of the doping element of the initial insulating layer 109 located on the side wall of the gate structure 102 is 1% to 3%; when the doping element is boron, as the boron content increases, the etching resistance will also increase accordingly. By setting the molar concentration range of the doping element of the initial insulating layer 109 located on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first sidewall 103 and the first surface S1 of the second sidewall 104 to 5% to 8%, the etching resistance of the initial insulating layer 109 can be effectively improved.
[0065] In some embodiments, the deposition process and the ion implantation process are performed alternately and cyclically. For example, a nitride layer may be deposited, followed by an ion implantation process to form a doped nitride layer, and the above process is repeated to form an initial insulating layer 109 with uniformly distributed doped elements on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first sidewall 103, and the first surface S1 of the second sidewall 104. In other embodiments, a nitride layer may be deposited once, followed by high-energy ion implantation to form an initial insulating layer 109 including a doped nitride layer.
[0066] In some embodiments, the initial insulating layer 109 located on the sidewall of the gate structure 102 can be removed by wet etching, and the initial insulating layer 109 located on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first sidewall 103, and the first surface S1 of the second sidewall 104 is retained. Exemplarily, the etching solution of the wet etching process is a phosphoric acid solution, and the etching selectivity of the initial insulating layer 109 located on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first sidewall 103, and the first surface S1 of the second sidewall 104 to the initial insulating layer 109 located on the sidewall of the gate structure 102 is in the range of 3:1 to 10:1, that is, the etching resistance of the initial insulating layer 109 located on the sidewall of the gate structure 102 is weaker than that of the initial insulating layer 109 located on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first sidewall 103, and the first surface S1 of the second sidewall 104. The semiconductor device structure after wet etching is as follows: Figure 8 As shown, since only the first spacer 103 and the second spacer 104 of the sidewalls of the gate structure 102 are retained, the spacing between the gate structures 102 is effectively increased and the parasitic capacitance is reduced.
[0067] In some embodiments, the sidewall structure SW also includes an isolation layer 111 located on the second surface S2 of the second sidewall 104, the isolation layer 111 includes a first isolation layer 1111 and a second isolation layer 1112, the first isolation layer 1111 is located between the second sidewall 104 and the second isolation layer 1112, wherein the formation process of the isolation layer 111 and the insulating layer 110 can be the same, that is, while forming the insulating layer 110, the initial insulating layer 109 located on the second surface S2 of the second sidewall 104 is also retained as the isolation layer 1111. Exemplarily, when the initial insulating layer 109 located on the side wall of the gate structure 102 is removed and the initial insulating layer 109 on the surface of the substrate 100, the top surface of the gate structure 102, the top surface of the first side wall 103 and the first surface S1 of the second side wall 104 is retained, it also includes retaining the initial insulating layer 109 located on the second surface S2 of the second side wall 104, wherein the retained initial insulating layer 109 on the second surface S2 of the second side wall 104 also includes a portion of the initial insulating layer 109 located on the side wall of the gate structure 102, which constitutes a first isolation layer 1111, and the remaining initial insulating layer 109 on the second surface S2 of the second side wall 104 constitutes a second isolation layer 1112. Since the concentration of the doping elements in the portion of the initial insulating layer 109 located on the side wall of the gate structure 102 is less than the concentration of the doping elements in the initial insulating layer 109 located on the second surface S2 of the second side wall 104, correspondingly, the concentration of the doping elements in the first isolation layer 1111 is also less than the concentration of the doping elements in the second isolation layer 1112. Exemplarily, the molar concentration range of the doping elements in the first isolation layer 1111 is 1% to 3%, and the molar concentration range of the doping elements in the second isolation layer 1112 is 5% to 8%. In other embodiments, the concentrations of the doping elements in the first isolation layer 1111 and the second isolation layer 1112 can also be set in a gradient, that is, the first isolation layer 1111 decreases uniformly toward the second isolation layer 1112, thereby effectively preventing the second side wall 104 from being over-etched.
[0068] In some embodiments, the preparation method of the semiconductor device 10 also includes, after forming the insulating layer 110, depositing a dielectric layer 113 for isolating different functional devices; illustratively, the deposition process can be CVD, ALD or PVD, the material of the dielectric layer 113 can be silicon oxide, and the dielectric layer 113 is partially filled between the gate structures 102, thereby further reducing the parasitic capacitance between the gate structures 102. At the same time, since the side walls of the gate structure 102 are only provided with the first side wall 103 and the second side wall 104, the spacing between the gate structures 102 is increased. When filling the dielectric layer 113 between the gate structures 102, the filling effect can be effectively improved to avoid the formation of air gaps.
[0069] In some embodiments, reference Figure 1 and Fig.10, patterning the dielectric layer 113 to form a first groove T1 and a second groove T2, the first groove T1 exposes the second gate conductive layer CT2 of the gate structure 102, and is used to form a contact structure corresponding to the gate structure 102, and the second groove T2 exposes the source contact layer 107 of the source 105 or the drain contact layer 108 of the drain 106, and is used to form a contact structure of the source 105 or the drain 106, and the patterning process can be dry etching, wherein the insulating layer 110 and the isolation layer 111 can be used as an etching stop layer to protect the gate structure 102, the source contact layer 107 of the source 105 or the drain contact layer 108 of the drain 106 from being over-etched. A transition layer 114 and a metal layer 115 are sequentially deposited in the first groove T1 and the second groove T2 to form a contact structure CP, wherein the contact structure CP is used to realize electrical connection between the gate structure, the source 105 or the drain 106 and other functional devices or control circuits; exemplarily, the material of the transition layer 114 may include titanium nitride, metal silicide, etc., and the material of the metal layer 115 may include one or more of metal silicide, metal compounds, metal alloys and metals.
[0070] This embodiment also provides a memory device, which is formed by bonding a target wafer 20 including a semiconductor device 10 and a bonding wafer 30, such as Fig.11 As shown, the bonding wafer 30 includes a control circuit and a bonding interface, and the memory device is formed by bonding the bonding layer of the target wafer 20 including the semiconductor device 10 to the bonding interface of the bonding wafer 30 .
[0071] In some embodiments, the target wafer 20 may include a semiconductor chip, which may be a memory semiconductor chip, and the memory semiconductor chip includes a memory device. For example, the memory device includes a non-volatile memory device, such as at least one of a flash memory, a phase change random access memory (PRAM), a magnetoresistive random access memory (MRAM), a ferroelectric random access memory (FeRAM), and a resistive random access memory (RRAM). For example, the flash memory includes a NAND flash memory or a V-NAND flash memory. In some embodiments, the memory device includes a volatile memory device, such as a dynamic random access memory (DRAM) or a static random access memory (SRAM). Among them, the memory semiconductor chip may include a functional device, and the functional device includes a plurality of individual devices of various types. The plurality of individual devices include various semiconductor devices 10, such as a metal oxide semiconductor field effect transistor (MOSFET) including a CMOS transistor, a system large-scale integrated circuit (LSI), an active device, or a passive device.
[0072] In some embodiments, taking DRAM as an example, the storage structure may include a peripheral circuit and a storage area, and the peripheral circuit area may include a semiconductor device 10. Exemplarily, the contact structure CP may be directly connected to the source-drain area or the gate structure to achieve transmission of electrical signals, or the contact structure CP may also be used as an intermediate connection structure to achieve indirect connection with the source-drain area or the gate structure through connection with other metal layers of different layers. In addition, the contact structure CP is also electrically connected to the bonding layer of the target wafer 20 to achieve signal transmission with the bonded wafer 30.
[0073] Those skilled in the art can understand that the above-mentioned embodiments are specific examples for implementing the present disclosure, and in practical applications, various changes can be made to them in form and detail without departing from the spirit and scope of the embodiments of the present disclosure. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the embodiments of the present disclosure, so the protection scope of the embodiments of the present disclosure shall be based on the scope defined in the claims.
Claims
1. A semiconductor device, characterized in that: include: substrate; A gate structure, located on the substrate, the gate structure comprising a gate oxide layer and a gate conductive layer stacked in sequence; A sidewall structure covering the sidewall of the gate structure, wherein the sidewall structure comprises a first sidewall and a second sidewall; an insulating layer, wherein the insulating layer covers a top surface of the gate structure, a top surface of the first sidewall and a first surface of the second sidewall, and the insulating layer is a doped nitride layer; The source and the drain are located in the substrate on both sides of the gate structure.
2. The semiconductor device according to claim 1, wherein: The sidewall structure further includes an isolation layer located on the second surface of the second sidewall. The isolation layer includes a first isolation layer and a second isolation layer. The first isolation layer is located between the second sidewall and the second isolation layer.
3. The semiconductor device according to claim 2, characterized in that The semiconductor device also includes a contact structure. In a direction parallel to the substrate, the total width of the insulating layer and the contact structure located in the insulating layer is greater than the width of the gate structure, and is smaller than the total width of the gate structure and the isolation layer, the first side wall and the second side wall perpendicular to the substrate direction.
4. The semiconductor device according to claim 3, characterized in that In a direction parallel to the substrate, a total width of the insulating layer and the contact structure in the insulating layer is equal to a total width of the gate structure and the first isolation layer, the first sidewall and the second sidewall perpendicular to the substrate.
5. The semiconductor device according to claim 2, wherein: The second isolation layer is the doped nitride layer, and the doping elements of the insulating layer and the second isolation layer are one or more of boron, phosphorus, arsenic or carbon.
6. The semiconductor device according to claim 5, characterized in that The first isolation layer is the doped nitride layer, and the first isolation layer and the second isolation layer have a concentration gradient of the doping element in a direction parallel to the substrate.
7. The semiconductor device according to claim 1, wherein: The materials of the first sidewall spacer and the second sidewall spacer are silicon nitride and silicon oxide respectively.
8. A method for preparing a semiconductor device, characterized in that: include: providing a substrate; forming a gate structure, the gate structure being located on the substrate, the gate structure comprising a stacked gate oxide layer and a gate conductive layer; forming a sidewall spacer structure, wherein the sidewall spacer structure covers the sidewall of the gate structure, and the sidewall spacer structure comprises a first sidewall spacer and a second sidewall spacer; forming an insulating layer, wherein the insulating layer covers the top surface of the gate structure, the top surface of the first sidewall and the first surface of the second sidewall, and the insulating layer is a doped nitride layer; A source and a drain are formed, wherein the source and the drain are located in the substrate at both sides of the gate structure.
9. The method for preparing a semiconductor device according to claim 8, characterized in that: The steps of forming the gate structure and the spacer structure include: Sequentially depositing and patterning a stacked gate oxide material layer and a first gate conductive material layer on the substrate to form the gate oxide layer and the first gate conductive layer, wherein the gate oxide layer and the first gate conductive layer constitute an initial gate structure; Depositing a first spacer material layer and a second spacer material layer on the initial gate structure and the substrate in sequence, and removing a portion of the first spacer material layer and the second spacer material layer located on the top surface of the gate structure and the substrate to form the first spacer and the second spacer covering the sidewall of the gate structure and a portion of the substrate; A metal layer is deposited on the top surface of the initial gate structure and annealed to form a second gate conductive layer. The gate oxide layer, the first gate conductive layer and the second gate conductive layer constitute the gate structure.
10. The method for preparing a semiconductor device according to claim 8, characterized in that: The step of forming an insulating layer includes: forming an initial insulating layer on the substrate, the gate structure, the first side wall and the second side wall, removing the initial insulating layer located on the side wall of the gate structure, and retaining the initial insulating layer on the surface of the substrate, the top surface of the gate structure, the top surface of the first side wall and the first surface of the second side wall to form the insulating layer.
11. The method for preparing a semiconductor device according to claim 10, characterized in that: The step of forming an initial insulating layer on the substrate, the gate structure, the first sidewall spacer and the second sidewall spacer comprises: Performing a deposition process to form the nitride layer covering the first surface of the substrate, the gate structure, the first spacer and the second spacer, wherein the nitride layer includes silicon nitride; An ion implantation process is performed on the nitride layer to form an initial insulating layer of the nitride layer including doped elements, wherein the concentration of the doped elements in the initial insulating layer located on the substrate, the top surface of the gate structure, the top surface of the first side wall and the first surface of the second side wall is different from that in the initial insulating layer located on the side wall of the gate structure.
12. The method for preparing a semiconductor device according to claim 11, characterized in that: The deposition process and the ion implantation process are performed alternately and cyclically.
13. The method for preparing a semiconductor device according to claim 10, characterized in that: The step of removing the initial insulating layer located on the sidewall of the gate structure and retaining the initial insulating layer on the surface of the substrate, the top surface of the gate structure, the top surface of the first sidewall and the first surface of the second sidewall to form the insulating layer comprises: The initial insulating layer located on the side wall of the gate structure is removed by wet etching, and the initial insulating layer on the substrate surface, the top surface of the gate structure, the top surface of the first side wall and the first surface of the second side wall is retained, wherein the etching selectivity ratio of the initial insulating layer located on the surface of the substrate and the top surface of the gate structure to the initial insulating layer located on the top surface of the gate structure, the top surface of the first side wall and the first surface of the second side wall in the wet etching is in the range of 1:3 to 1:
10.
14. The method for preparing a semiconductor device according to claim 11, characterized in that: The sidewall structure further includes an isolation layer located on the second surface of the second sidewall. The isolation layer is formed by the same process as that of the insulating layer.
15. A storage device, characterized in that: The target wafer comprising the semiconductor device as claimed in any one of claims 1 to 7 is bonded to a bonding wafer; the bonding wafer comprises a control circuit and a bonding interface, and the storage device is bonded to the bonding interface of the bonding wafer via the bonding layer of the target wafer.
Citation Information
Patent Citations
Fabricating method of semiconductor device
CN101599459A
Manufacturing method of semiconductor device
CN109872970A
Semiconductor structure and manufacturing method thereof
CN117199072A
Silicon oxycarbide and silicon carbonitride based materials for MOS devices
US20050236694A1
Method of manufacturing a semiconductor
US20100081246A1