A preparation process and forming device of environmentally friendly bricks
By designing a molding device with a vanishable mold cavity and a front and rear permeable sintering cover, the problems of low operation efficiency and transfer risk during the environmentally friendly brick forming process are solved, efficient drying and sintering are achieved, and water permeability is tested. Improves molding quality and efficiency.
Patent Information
- Application Number
- CN202411245570.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-06
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-06
AI Technical Summary
In the existing environmentally friendly brick forming process, the operation efficiency of wet or semi-dry embryos is low, resulting in low molding efficiency, and there are transfer risks and unevenness problems during drying and sintering.
Design a forming device, including a vanishable mold cavity and a front-and-back permeable sintering cover, to achieve molding, drying, sintering and permeable coating applications of bricks through sliding modules and drivers, and to use a shaped frame for permeability. Performance detection.
It improves drying efficiency and quality, reduces the risk of brick transfer, realizes efficient sintering and permeability detection, and simplifies the process process.
Smart Images

Figure CN118752590B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of environmentally friendly brick forming, in particular to a preparation process and a forming device for environmentally friendly bricks. Background Art
[0002] Environmentally friendly bricks are a new type of building material, which are mainly made of construction waste or industrial waste. They can be used as wall materials or floor materials. The molding process of environmentally friendly bricks generally includes demoulding, drying, sintering and cooling treatment.
[0003] In the prior art, when the environmentally friendly bricks are wet or semi-dry after demolding, the embryos need to be transferred to a drying room and then transported to a sintering kiln. During the molding process, the operation of the environmentally friendly bricks greatly affects the molding efficiency. Summary of the invention
[0004] The present invention provides a preparation process and a forming device for an environmentally friendly brick, which can not only form, dry and sinter a brick body, but also coat a water-permeable coating on one side of the brick body, and can also complete the detection of the water permeability of the brick body.
[0005] In order to achieve the above object, the present invention provides the following technical solutions:
[0006] A forming device for environmentally friendly bricks, comprising:
[0007] A first mold and a second mold integrally formed on its top, the first mold is connected to the second mold, a partition is installed on the second mold, a bearing module is slidably installed inside the first mold in the vertical direction, when the top of the bearing module isolates the connection between the first mold and the second mold, a shaping cavity is formed between the second mold, the partition and the bearing module; the internal space of the first mold is larger than the shaping cavity; when the bearing module slides downward to a preset position, the top of the brick blank to be dried and its four continuous sides will be exposed to the inside of the first mold; the bearing module includes two bearing seats slidably installed on the inner wall of the first mold, both of the bearing seats are controllably hinged with assembly plates, the two assembly plates are symmetrically designed, and the two assembly plates remain horizontal in the initial state, and their free ends fit each other when the two assembly plates remain horizontal.
[0008] Furthermore, the assembly plate is penetrated by a plurality of air holes, which are distributed in a matrix pattern. A blocking plate is slidably mounted on the bottom of the assembly plate, and a plurality of piston columns are distributed in a matrix pattern on the top of the blocking plate. The piston columns are filled in the air holes one by one. When the blocking plate slides away from the assembly plate, the air holes are released. During the shaping process, the end of the piston column remains in the same plane as the surface of the assembly plate. A first driver for controlling the displacement of the blocking plate is also mounted on the assembly plate.
[0009] Further, the first mold is designed with a structure that is permeable from front to back. A sintering cover can slide into the interior of the first mold. When the assembly plate and the dried brick blank are displaced downward to the sintering position, the sintering cover can slide to the top of the assembly plate, and a sintering channel is formed between the sintering cover and the two assembly plates. The two ends of the sintering channel are in circular communication with an external sintering kiln. The sintering kiln can continuously input high-temperature air flow into the sintering channel. Both the sintering cover and the assembly plate are made of high-temperature resistant materials.
[0010] Further, the depth of the second mold is greater than the height of the sintered brick blank. A frame-shaped flange that does not interfere with the shaping of the brick blank to be dried is installed inside the second mold. When the shaping space is formed, the bottom of the frame-shaped flange covers the top edge of the sintered brick blank, and an external spraying device can coat a water-permeable coating on the top of the sintered brick blank.
[0011] Further, assembly grooves are formed on both side walls of the first mold. Two U-shaped frames are slidably installed in the assembly grooves. The ends of the two U-shaped frames are close to and fit with each other to form a limiting frame. The limiting frame can lock and limit the sintered brick blank, and a flexible member is installed inside the limiting frame. A water storage pool is formed between the limiting frame and the top of the cooled sintered brick blank. The assembly plate releases the load on the sintered brick blank and releases the bottom of the sintered brick blank.
[0012] Further, a water retaining strip is installed at the inner bottom of the first mold. A measuring cavity is formed between the water retaining strip and the inner bottom of the first mold. Scales are marked in the measuring cavity. A water level measuring instrument is installed at the inner bottom of the first mold. A second driver for controlling the deflection of the assembly plate is installed on the bearing seat.
[0013] Further, a guide rod is fixedly installed between the inner top and the inner bottom of the first mold. The bearing seat is vertically slidably installed on the outer wall of the guide rod. A screw rod is rotatably installed between the inner top and the inner bottom of the first mold. The bearing seat is threadedly connected to the screw rod. A third driver for controlling the rotation of the screw rod is installed on the top of the first mold. When the screw rod rotates, the bearing seat can be displaced in the vertical direction.
[0014] A preparation process for an environmentally friendly brick, which includes the above-mentioned forming device for the environmentally friendly brick, and includes the following steps:
[0015] S1: Forming. The brick blank to be dried is formed in the shaping die cavity, and the brick body is a wet blank or a semi-dry blank.
[0016] S2: Drying. The brick blank to be dried is transferred downward through the assembly plate, and the top and four consecutive side surfaces of the brick blank to be dried are exposed. At the same time, the air holes on the assembly plate are released.
[0017] S3: Sintering. Transfer the dried brick embryo to the sintering position. Meanwhile, the sintering hood slides in and forms a sintering channel between the assembly plates. The external sintering kiln operates and continuously circulates high-temperature airflows.
[0018] S4: Surface treatment. Apply a water-permeable coating on the top of the sintered brick embryo on one side.
[0019] S5: Water permeability test. After the water-permeable coating dries and cures, conduct a water permeability test on the sintered brick embryo.
[0020] Furthermore, in S5, it also includes:
[0021] V1: Use the limiting frame formed by two C-shaped frames to lock the sintered brick embryo, and control the downward displacement of the bearing module to release the shielding of the bottom of the sintered brick embryo.
[0022] V2: A water storage pool is formed between the limiting frame and the top of the sintered brick embryo. Inject water into the water storage pool, and use a scale or water level measuring instrument to confirm the water permeability in the measuring cavity per unit time, and calculate the water permeability coefficient or water permeability ability of the sintered brick embryo.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] By designing a disappearable shaping cavity, when the bearing module moves upward, it blocks the first mold and the second mold. Meanwhile, a shaping cavity is formed between the top of the bearing module, the second mold and the partition board. After the green brick embryo is formed, just control the downward displacement of the bearing module to make the shaping cavity disappear. At the same time, the top and its four continuous sides of the green brick embryo will be exposed inside the first mold, increasing the contact area between the green brick embryo and the external environment, and improving the drying efficiency and quality.
[0025] When drying is required, move the sealing plate and the piston column away from the assembly plate, so that the piston column completely disengages from the air vent holes. At this time, part of the bottom of the green brick embryo will be in contact with the environment inside the first mold, further improving the drying quality and efficiency.
[0026] After drying is completed, transfer the brick body to the sintering position through the assembly plate. At this time, the sintering hood will slide in and form a sintering channel with the assembly plate. The sintering kiln will operate and continuously output high-temperature airflows to the sintering channel. The high-temperature airflows will cause the particles in the brick body to melt, recrystallize and closely adhere to each other, completing the sintering of the brick body.
[0027] When surface treatment is required, the bottom of the frame-shaped flange will cover the top edge of the sintered brick embryo, and the external spraying equipment can apply a water-permeable coating on the top of the sintered brick embryo.
[0028] By utilizing the limiting frame formed by the close fitting of two C-shaped frames, the limiting frame can not only lock the brick body, but also surround the top of the brick body to form a water storage pool. At the same time, the assembly plate moves downward to release the bottom of the brick body, and calculating the amount of water passing through the brick body per unit time can complete the test of the water permeability of the brick body. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 Schematic perspective view of the forming device of the present invention;
[0030] Figure 2 Internal cross-sectional view of the forming device of the present invention;
[0031] Figure 3 Schematic perspective view of the forming device when the sintering channel is formed in the present invention;
[0032] Figure 4 In the present invention Figure 3 Internal structure schematic diagram;
[0033] Figure 5 Internal cross-sectional view of the forming device when the sintering channel is formed in the present invention;
[0034] Figure 6 Internal cross-sectional view of the forming device when the water permeability of the brick body is detected in the present invention;
[0035] Figure 7 Internal cross-sectional view of the forming device when the green brick blank to be dried is dried in the present invention;
[0036] Figure 8 Internal cross-sectional view of the forming device when the sintered brick blank is coated on one side in the present invention.
[0037] In the figure: 1, first mold; 2, second mold; 3, assembly plate; 4, bearing seat; 5, sealing plate; 6, C-shaped frame; 7, partition plate; 8, sintering cover; 9, screw; 11, piston rod; 12, frame flange; 13, water level measuring instrument; 14, guide rod. DETAILED DESCRIPTION OF THE EMBODIMENTS
[0038] The following will clearly and completely describe the technical solutions in the embodiments of the present invention with reference to the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. All other embodiments obtained by those of ordinary skill in the art based on the embodiments of the present invention without creative efforts shall fall within the protection scope of the present invention.
[0039] Please refer to Figures 1 to 8 , the present invention provides a technical solution: a forming device for environmentally friendly bricks, comprising:
[0040] A first mold 1 and a second mold 2 integrally formed on its top, the first mold 1 is connected to the second mold 2, a partition 7 is installed on the second mold 2, a supporting module is slidably installed in the vertical direction inside the first mold 1, when the top of the supporting module isolates the connection between the first mold 1 and the second mold 2, a shaping cavity is formed between the second mold 2, the partition 7 and the supporting module; the internal space of the first mold 1 is larger than the shaping cavity; when the supporting module slides downward to a preset position, the top of the brick blank to be dried and its four continuous sides are exposed to the inside of the first mold 1.
[0041] In the prior art, the wet embryo needs to be taken out of the mold after being formed. However, due to factors such as the strength of the wet embryo, unexpected deformation may occur during the removal process, and transferring the wet embryo to a drying kiln will increase the number of process steps. In the present invention, a disappearing shaping cavity is designed. When the shaping cavity is needed to form the brick embryo, the supporting module can be displaced upward to block the first mold 1 and the second mold 2. At the same time, a shaping cavity is formed between the top of the supporting module, the second mold 2 and the partition 7. After the dried brick embryo is formed, the shaping cavity can be made to disappear by controlling the supporting module to move downward. At the same time, the top of the dried brick embryo and its four continuous sides are exposed to the inside of the first mold 1, thereby increasing the contact area between the dried brick embryo and the external environment, improving the efficiency of natural or mechanical drying, and avoiding the risk of transfer of the dried brick embryo.
[0042] In a preferred embodiment, the bearing module comprises two bearing seats 4 slidably mounted on the inner wall of the first mold 1, and the two bearing seats 4 are controllably hinged with mounting plates 3. The two mounting plates 3 are symmetrically designed, and the two mounting plates 3 are both kept horizontal in the initial state. When the two mounting plates 3 are kept horizontal, their free ends are in contact with each other. Please refer to Figures 1 to 8 In this embodiment, the cooperation of the two assembly plates 3 can form a tray for supporting the brick body. The two assembly plates 3 remain horizontal in the initial state, which can ensure the flatness of the bottom of the brick body when forming the shaping cavity. Secondly, the two assembly plates 3 can also rotate in opposite directions, which can effectively demold the brick body after sintering or drying. The two bearing seats 4 are slidably installed in the first mold 1, thereby driving the assembly plates 3 to move in the vertical direction.
[0043] On the basis of the embodiment of the bearing module, a plurality of air holes are formed on the assembly plate 3, and the plurality of air holes are arranged in a matrix. A blocking plate 5 is slidably mounted on the bottom of the assembly plate 3, and a plurality of piston rods 11 are arranged in a matrix on the top of the blocking plate 5. The piston rods 11 are filled in the air holes one by one. When the blocking plate 5 slides away from the assembly plate 3, the air holes are released. During the shaping process, the end of the piston rod 11 maintains the same plane as the surface of the assembly plate 3. A first driver for controlling the displacement of the blocking plate 5 is also installed on the assembly plate 3. Please refer to Figure 4 and Figure 7 In this embodiment, the first driver can control the displacement of the blocking plate 5, so that the blocking plate 5 can be moved away from or close to the assembly plate 3, so that the piston column 11 can be movably installed in the air vent. When the brick body needs to be shaped, the top of the piston column 11 is placed in the same plane as the bearing surface of the assembly plate 3 to ensure the quality of the bearing and shaping of the assembly plate 3. Secondly, when drying is required, the blocking plate 5 and the piston column 11 are moved away from the assembly plate 3, so that the piston column 11 is completely separated from the air vent. At this time, the bottom of the brick blank to be dried can also be effectively dried to reduce uneven drying. Secondly, the separation of the piston column 11 is also the mutual distance between the bottom of the brick blank to be dried, which can help the subsequent demolding.
[0044] On the basis of the embodiment of the bearing module, the first mold 1 is designed as a front-to-back transparent structure, and a sintering cover 8 can be slid into the first mold 1. When the assembly plate 3 and the dried brick embryo are moved downward to the sintering position, the sintering cover 8 can slide to the top of the assembly plate 3, and a sintering channel is formed between the sintering cover 8 and the two assembly plates 3. The two ends of the sintering channel are circulated and connected with the external sintering kiln. The sintering kiln can continuously input high-temperature airflow into the sintering channel. The sintering cover 8 and the assembly plate 3 are made of high-temperature resistant materials. Please refer to Figures 3 to 5 In this embodiment, after the brick body is dried, it is necessary to perform high-temperature sintering on the brick body. During the heat treatment process, the high temperature will cause the particles in the brick body to melt, recrystallize and fit tightly. When the drying is completed, the brick body is transferred to the sintering position through the assembly plate 3. At this time, the sintering cover 8 will slide in and form a sintering channel between the assembly plate 3. At this time, the sintering kiln will work and continuously output high-temperature airflow to the sintering channel. At the same time, the heated airflow after heat exchange will return to the sintering kiln. At the same time, the sintering cover 8 and the assembly plate 3 can be made of high-temperature resistant ceramic materials to reduce the waste of sintering high temperature.
[0045] Furthermore, the depth of the second mold 2 is greater than the height of the fired brick blank. A frame-shaped flange 12 is installed inside the second mold 2 so as not to interfere with the shaping of the brick blank to be dried. When the shaping space is formed, the bottom of the frame-shaped flange 12 covers the top edge of the fired brick blank. The external spraying equipment can apply a water-permeable coating to the top of the fired brick blank. Please refer to Figure 8 In this embodiment, after sintering is completed, the brick body needs to be surface treated, and the environmentally friendly brick can also be used as a floor paving material or a single-sided exposed material, so only one side of the brick body needs to be coated with a water-permeable coating to improve wear resistance and water permeability.
[0046] Further, assembly grooves are formed on both side walls of the first mold 1. Two U-shaped frames 6 are slidably installed in the assembly grooves. The ends of the two U-shaped frames 6 are close to and fit with each other to form a limiting frame. The limiting frame can lock and limit the sintered brick blank. A flexible member is installed inside the limiting frame. A water storage pool is formed between the limiting frame and the top of the cooled sintered brick blank. The assembly plate 3 releases the load on the sintered brick blank and releases the bottom of the sintered brick blank. Please refer to Figure 6 , in this embodiment, after the permeable coating is coated and cured, the water permeability of the brick body can be detected. It is necessary to expose and release the bottom of the brick body, and at the same time, accumulate aqueous solution on the top of the brick body, and record the amount of water passing through the brick body within a certain period of time. This method is the fixed head method. In the present invention, by using the limiting frame formed by the close fitting of the two U-shaped frames 6, the limiting frame can not only lock the brick body, surround the top of the brick body in a circle, and form a water storage pool. At the same time, the assembly plate 3 also needs to move downward to release the bottom of the brick body.
[0047] Further, a water retaining strip is installed at the inner bottom of the first mold 1. A measuring cavity is formed between the water retaining strip and the inner bottom of the first mold 1. Scales are marked in the measuring cavity. A water level measuring instrument 13 is installed at the inner bottom of the first mold 1. A second driver for controlling the deflection of the assembly plate 3 is installed on the bearing seat 4. Please refer to Figure 6 and Figure 7 , in this embodiment, the water retaining strip and the inner bottom of the first mold 1 are used to form a structure that can receive the water permeated from the brick body, so that the water collection amount per unit time can be counted by using the scales or the water level measuring instrument 13. Secondly, the second driver can make the two assembly plates 3 deflect in an object shape to form a V-shaped water guide plate, so as to guide the water droplets permeating from the bottom of the brick body.
[0048] Further, a guide rod 14 is fixedly installed between the inner top and the inner bottom of the first mold 1. The bearing seat 4 is vertically slidably installed on the outer wall of the guide rod 14. A screw rod 9 is rotatably installed between the inner top and the inner bottom of the first mold 1. The bearing seat 4 is threadedly connected with the screw rod 9. A third driver for controlling the rotation of the screw rod 9 is installed on the top of the first mold 1. When the screw rod 9 rotates, the bearing seat 4 can be displaced in the vertical direction. In this embodiment, when the third driver works, it can drive the screw rod 9 to rotate. Due to the threaded connection relationship between the bearing seat 4 and the screw rod 9 and the vertical limiting relationship between the bearing seat 4 and the water level measuring instrument 13, the bearing seat 4 can be displaced in the vertical direction, thereby controlling the displacement of the assembly plate 3 and the brick body on its top.
[0049] A preparation process of an environmentally friendly brick, which includes the above-mentioned forming device for the environmentally friendly brick, and includes the following steps:
[0050] S1: Forming. The dry brick blank is formed in the shaping die cavity, and the brick body is a wet blank or a semi-dry blank;
[0051] S2: Drying. Transfer the green bricks to be dried downward through the assembly plate 3, and expose the top and its four consecutive sides of the green bricks to be dried. Meanwhile, the air-permeable holes on the assembly plate 3 will be released.
[0052] S3: Sintering. Transfer the dried green bricks to the sintering position. Meanwhile, the sintering hood 8 slides in and forms a sintering channel between the assembly plate 3. The external sintering kiln works and continuously circulates high-temperature air flow.
[0053] S4: Surface treatment. Apply a single-sided water-permeable coating to the top of the sintered green bricks.
[0054] S5: Water permeability test. After the water-permeable coating is dried and cured, conduct a water permeability test on the sintered green bricks.
[0055] In S1 - S5, compared with the existing processes, directly integrating the drying and sintering processes in the molding device reduces the transfer risk. Meanwhile, when performing progressive processes, the green bricks can maintain the state after each process is completed. Secondly, the disposable plastic mold cavity can reduce the structure and optimize the processes and devices.
[0056] Furthermore, in S5, it also includes:
[0057] V1: Use the limiting frame formed by two C-shaped frames 6 to lock the sintered green bricks, and control the downward displacement of the bearing module to release the shielding of the bottom of the sintered green bricks.
[0058] V2: A water storage pool is formed between the limiting frame and the top of the sintered green bricks. Inject water into the water storage pool, and use the scale or water level measuring instrument 13 to confirm the water permeability in the measuring cavity per unit time, and calculate the water permeability coefficient or water permeability of the sintered green bricks.
[0059] With the cooperation of the above structures, it is possible to both mold, dry and sinter the bricks, and also apply a single-sided water-permeable coating to the bricks, and at the same time complete the detection of the water permeability of the bricks.
[0060] The standard parts used in this embodiment can be directly purchased from the market. For the non-standard structural components described in the specification and drawings, they can also be directly processed without any doubt according to the existing technical knowledge. Meanwhile, the connection methods of each component adopt the mature conventional means in the existing technology, and the machinery, parts and equipment all adopt the conventional models in the existing technology, so no specific description will be made here.
Claims
1. A forming device for environmentally friendly bricks, characterized in that: include: A first mold (1) and a second mold (2) integrally formed on its top, the first mold (1) being connected to the second mold (2), a partition (7) being installed on the second mold (2), a bearing module being slidably installed in the interior of the first mold (1) in a vertical direction, and when the top of the bearing module isolates the first mold (1) from the second mold (2), a shaping cavity is formed between the second mold (2), the partition (7) and the bearing module; The internal space of the first mold (1) is larger than the shaping mold cavity; When the supporting module slides downward to a preset position, the top of the brick to be dried and its four continuous sides are exposed inside the first mold (1); The bearing module comprises two bearing seats (4) slidably mounted on the inner wall of the first mold (1), and the two bearing seats (4) are controllably hinged with mounting plates (3), the two mounting plates (3) are symmetrically designed, and the two mounting plates (3) are both kept horizontal in an initial state, and the free ends of the two mounting plates (3) are in contact with each other when the two mounting plates (3) are kept horizontal; The assembly plate (3) is provided with a plurality of air holes, the plurality of air holes being arranged in a matrix pattern, a blocking plate (5) being slidably mounted on the bottom of the assembly plate (3), a plurality of piston rods (11) being arranged in a matrix pattern on the top of the blocking plate (5), the piston rods (11) being filled in the air holes one by one, when the blocking plate (5) slides away from the assembly plate (3), the air holes are released, during the shaping process, the end of the piston rod (11) remains in the same plane as the surface of the assembly plate (3), and a first driver for controlling the displacement of the blocking plate (5) is also mounted on the assembly plate (3); The first mold (1) has a transparent structure from front to back, and a sintering cover (8) can be slid into the first mold (1). When the assembly plate (3) and the dried brick embryo are moved downward to the sintering position, the sintering cover (8) can slide to the top of the assembly plate (3), and a sintering channel is formed between the sintering cover (8) and the two assembly plates (3). The two ends of the sintering channel are in circulation communication with an external sintering kiln, and the sintering kiln can continuously input high-temperature airflow into the sintering channel. The sintering cover (8) and the assembly plate (3) are both made of high-temperature resistant materials. The depth of the second mold (2) is greater than the height of the fired brick blank. The second mold (2) is internally provided with a frame-shaped flange (12) which does not interfere with the shaping of the brick blank to be dried. When the shaping space is formed, the bottom of the frame-shaped flange (12) covers the top edge of the fired brick blank, and the external spraying equipment can apply a water-permeable coating to the top of the fired brick blank.
2. The environmentally friendly brick forming device according to claim 1 is characterized in that: Both side walls of the first mold (1) are provided with assembly grooves, and two U-shaped frames (6) are slidably installed in the assembly grooves. The ends of the two U-shaped frames (6) are close to and fit with each other to form a limiting frame. The limiting frame can lock and limit the sintered brick blank, and a flexible member is installed inside the limiting frame. A water storage pool is formed between the limiting frame and the top of the cooled sintered brick blank. The assembly plate (3) releases the bearing of the sintered brick blank and releases the bottom of the sintered brick blank.
3. The environmentally friendly brick forming device according to claim 2 is characterized in that: A water retaining strip is installed at the inner bottom of the first mold (1). A measuring cavity is formed between the water retaining strip and the inner bottom of the first mold (1). Scales are marked in the measuring cavity. A water level measuring instrument (13) is installed at the inner bottom of the first mold (1). A second driver for controlling the deflection of the assembly plate (3) is installed on the bearing seat (4).
4. The environmentally friendly brick forming device according to claim 3 is characterized in that: A guide rod (14) is fixedly installed between the inner top and the inner bottom of the first mold (1). The bearing seat (4) is vertically slidably installed on the outer wall of the guide rod (14). A screw rod (9) is rotatably installed between the inner top and the inner bottom of the first mold (1). The bearing seat (4) is threadedly connected to the screw rod (9). A third driver for controlling the rotation of the screw rod (9) is installed on the top of the first mold (1). When the screw rod (9) rotates, the bearing seat (4) can be displaced in the vertical direction.
5. A process for preparing environmentally friendly bricks, comprising the forming device for environmentally friendly bricks according to claim 4, characterized in that: Including the following steps: S1: Forming. The to-be-dried brick blank is formed in the shaping die cavity, and the brick body is a wet blank or a semi-dry blank. S2: Drying. The to-be-dried brick blank is transferred downward through the assembly plate (3), and the top and four consecutive side surfaces of the to-be-dried brick blank are exposed. At the same time, the air holes on the assembly plate (3) are released. S3: Sintering. The dried brick blank is transferred to the sintering position. At the same time, the sintering cover (8) slides in and forms a sintering channel between the assembly plate (3). The external sintering kiln works and continuously circulates high-temperature air flow. S4: Surface treatment. A single-sided permeable coating is applied to the top of the sintered brick blank. S5: Permeability test. After the permeable coating is dried and cured, the permeability performance of the sintered brick blank is tested.
6. The process for preparing the environmentally friendly brick according to claim 5, characterized in that: In S5, it also includes: V1: Using the limiting frame formed by two U-shaped frames (6) to lock the sintered brick blank, and controlling the downward displacement of the bearing module to release the shielding of the bottom of the sintered brick blank. V2: A water storage pool is formed between the limiting frame and the top of the sintered brick blank. Water is injected into the water storage pool. The water permeability in the measuring cavity is confirmed per unit time by using the scale or the water level measuring instrument (13), and the water permeability coefficient or water permeability of the sintered brick blank is calculated.