An etching method

By performing feature analysis of photoresist and photomask patterns and adjusting exposure parameters, the problem of photoresist edge unevenness is solved and the etching effect is improved.

CN118782508BActive Publication Date: 2024-11-12XUZHOU MEIXING OE TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411269158.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-12
Estimated Expiration
2044-09-11

AI Technical Summary

Technical Problem

The prior art does not consider the material properties of the photoresist and the influence of the photomask pattern pattern pattern characteristics on the exposure process, resulting in uneven stress, affecting the uniformity of the photoresist edge and subsequent etching effect.

Method used

By conducting irradiation hardness change experiments on the photoresist, combining the texture feature calculation process in the photomask pattern to stably characterize the parameters, adjust the exposure intensity and preheating temperature, ensure the stability of the photoresist during the exposure process, and the adaptive adjustment process Parameters to improve uniformity of photoresist edges.

Benefits of technology

By considering the properties and texture characteristics of the photoresist, the exposure parameters are adaptively adjusted, the uniformity of the photoresist edge is improved, the impact on subsequent development and etching effects is reduced, and the etching effect is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118782508B_ABST
    Figure CN118782508B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of semiconductor technology, and in particular to an etching method. The invention conducts an irradiation hardness change experiment on a required photoresist to determine the hardness change amount, calculates process stability characterization parameters in combination with texture features in a photomask pattern, determines the stability category of the photoresist in the exposure process, performs photomask exposure on the silicon wafer based on the stability category of the photoresist in the exposure process, and when the photoresist is of a weak stability category, adaptively adjusts the exposure intensity for exposure, and determines whether the exposure process meets the stability standard through the axial height discrete difference of each feature point in a specific observation area, so as to correct the exposure intensity. The invention considers the influence of the photoresist properties and the photomask texture on the exposure process through the above process, adaptively adjusts the process parameters, improves the uniformity of the photoresist edge after exposure, reduces the influence on subsequent development and etching effects, and improves the etching effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of semiconductor technology, and in particular to an etching method. Background Art

[0002] Etching is a very important step in semiconductor processing. It selectively removes materials on the substrate surface according to the mask shape obtained by photolithography to form circuit patterns. The existing technology improves the etching efficiency by controlling the surface temperature of the substrate below -70°C to volatilize the by-products generated by etching. However, it does not consider the impact of complex photomask patterns on the exposed photoresist.

[0003] Chinese patent publication number: CN111584360A, discloses an etching method, including the steps of placing a substrate containing a silicon oxide film on a mounting table; controlling the surface temperature of the substrate to a temperature below -70°C; after the above control step, supplying high-frequency electric power for plasma generation to generate plasma from a gas containing fluorine and hydrogen to etch the silicon oxide film; and raising the surface temperature of the substrate to volatilize the by-products generated by the above etching. The invention can increase the etching rate.

[0004] However, the prior art still has the following problems:

[0005] In the prior art, the influence of the material properties of the photoresist and the texture features in the mask pattern on the exposure process is not considered. In actual situations, the change in the properties of the photoresist at the intersection of the textures may cause uneven stress, affecting the uniformity of the photoresist edge and the subsequent etching effect. Summary of the invention

[0006] To this end, the present invention provides an etching method to overcome the problem that the prior art does not consider the influence of the material properties of the photoresist and the texture features in the photomask pattern on the exposure process. In actual situations, the change in the properties of the photoresist at the intersection of the textures may cause uneven stress, affect the uniformity of the edge of the photoresist, and affect the subsequent etching effect.

[0007] To achieve the above object, the present invention provides an etching method, comprising:

[0008] Step S1, performing an irradiation hardness change experiment on the desired photoresist, including irradiating the photoresist surface with a predetermined exposure intensity after coating the photoresist, and recording the hardness change of the photoresist before and after the exposure;

[0009] Step S2, obtaining a photomask pattern of a desired photomask, determining texture features in the photomask pattern, and calculating process stability characterization parameters in combination with the hardness variation to determine the stability category of the photoresist during the exposure process, wherein the texture features include the number of texture intersections and the mean value of the texture gaps;

[0010] Step S3, determining a preheating temperature based on the process stability characterization parameter to preheat the silicon wafer coated with the photoresist, and performing photomask exposure on the silicon wafer based on the stability category of the photoresist during the exposure process, including:

[0011] Adjusting the exposure intensity for exposure, determining a specific observation area based on the texture of the photomask pattern, and determining whether the exposure process meets the stability standard according to the axial height discrete difference of each feature point in the specific observation area on the photoresist surface during the exposure process, so as to correct the exposure intensity;

[0012] Or, maintaining the initial exposure intensity to complete the photomask exposure;

[0013] Step S4, developing and etching the exposed silicon wafer and removing the photoresist on the silicon wafer to obtain an etched silicon wafer.

[0014] Furthermore, the process stability characterization parameter is calculated based on formula (1):

[0015] ,

[0016] In formula (1), Z is the process stability characterization parameter, P represents the number of grain intersections, P0 represents the preset grain intersection number threshold, D represents the grain gap mean, D0 represents the preset grain gap standard threshold, F represents the hardness change, and F0 represents the preset hardness change threshold.

[0017] Further, the stability category of the photoresist during the exposure process is determined according to the process stability characterization parameter, wherein:

[0018] If the process stability characterization parameter is greater than or equal to a preset process stability characterization parameter standard threshold, determining that the stability category of the photoresist is a weak stability category;

[0019] If the process stability characterization parameter is less than the preset process stability characterization parameter standard threshold, the stability category of the photoresist is determined to be a strong stability category.

[0020] Further, the preheating temperature is determined based on the process stability characterization parameter, wherein:

[0021] The preset temperature is positively correlated with the preset process stability characterization parameter.

[0022] Furthermore, in step S3, a photomask exposure is performed on the silicon wafer based on the stability category of the photoresist during the exposure process, wherein:

[0023] If the photoresist is of a weakly stable type, the exposure intensity to be adjusted is selected for exposure, a specific observation area is determined based on the texture of the photomask pattern, and whether the exposure process meets the stability standard is determined according to the axial height discrete difference of each feature point in the specific observation area on the surface of the photoresist during the exposure process, so as to correct the exposure intensity;

[0024] If the photoresist is of a strong stable type, it is selected to maintain the initial exposure intensity to complete the photomask exposure.

[0025] Furthermore, in step S3, adjusting the exposure intensity for exposure includes:

[0026] increasing the exposure intensity based on the process stability characterization parameter;

[0027] Among them, the increase in exposure intensity is positively correlated with the process stability characterization parameters.

[0028] Further, determining a specific observation area based on the texture of the photomask pattern includes:

[0029] Performing grayscale processing on the photomask pattern;

[0030] Dividing the photomask pattern into a number of observation areas;

[0031] The area ratio of each grain gap in each observation area is calculated, and the observation area with an area ratio higher than the preset area ratio is recorded as a special observation area.

[0032] Further, whether the exposure process meets the stability standard is determined based on the discrete difference in the axial height of each feature point in each specific observation area of ​​the photoresist surface during the exposure process, wherein:

[0033] If the discrete difference is greater than or equal to the preset discrete difference standard threshold, it is determined that the exposure process does not meet the stability standard;

[0034] If the discrete difference is less than the preset discrete difference standard threshold, it is determined that the exposure process meets the stability standard.

[0035] Furthermore, in step S3, the process of calculating the discrete difference includes:

[0036] Establishing a three-dimensional model of each specific observation area to determine the axial height of each characteristic point in each specific observation area;

[0037] Calculate the variance of the axial height of each feature point for each specific observation area;

[0038] The mean of the variance corresponding to each specific observation area is determined as the discrete difference.

[0039] Further, when it is determined that the exposure process does not meet the stability standard, the exposure intensity is reduced based on the discrete difference, and the reduction amount of the exposure intensity is positively correlated with the discrete difference.

[0040] Compared with the prior art, the present invention conducts an irradiation hardness change experiment on the required photoresist to determine the hardness change amount, calculates the process stability characterization parameters in combination with the texture features in the photomask pattern, determines the stability category of the photoresist in the exposure process, and performs photomask exposure on the silicon wafer based on the stability category of the photoresist in the exposure process. When the photoresist is of a weakly stable category, the exposure intensity is adaptively adjusted for exposure, and whether the exposure process meets the stability standard is determined by the axial height discrete difference of each feature point in a specific observation area to correct the exposure intensity. The present invention takes into account the effects of the photoresist properties and the photomask texture on the exposure process through the above process, adaptively adjusts the process parameters, improves the uniformity of the photoresist edge after exposure, reduces the effects on subsequent development and etching effects, and improves the etching effect.

[0041] In particular, the stability characterization parameters of the calculation process of the present invention take into account the texture characteristics and hardness change. In actual situations, the texture of the photomask pattern corresponds to the photoresist texture. During the exposure process, when the photoresist texture is relatively complex and the texture gaps are relatively close, the exposed area of ​​the photoresist undergoes property changes under exposure, which causes stress interference to the surrounding photoresist texture areas. If the texture areas are dense and the textures are relatively close, multi-directional stress interference and uneven stress are generated, which can easily lead to uneven edges of the photoresist texture areas and poor stability. In addition, if the hardness change of the photoresist during the exposure process is large, the above phenomenon will be aggravated. Therefore, the present invention characterizes the above situation through the texture characteristics and hardness change calculation process stability characterization parameters, provides data support for the subsequent determination of the stability category of the photoresist during the exposure process, thereby improving the uniformity of the photoresist edge and ensuring the subsequent etching effect.

[0042] In particular, for weakly stable photoresists, since the texture areas are dense and the textures are relatively close, it is considered to adaptively increase the exposure intensity to expose the local photoresist derived from stress interference and stress unevenness, thereby improving the edge unevenness phenomenon. In addition, the present invention considers determining the discrete differences in axial heights of each feature point in the specific observation area to characterize the uniformity of the property changes of the photoresist in the specific observation area during the exposure process. In actual situations, if the property changes are uneven and there is multi-directional stress interference, slight undulations may occur on the surface of the specific observation area of ​​the photoresist, affecting the exposure process. Based on this, it is determined whether the exposure process meets the standards, and the exposure intensity is adaptively adjusted to improve the uniformity of the photoresist edge and ensure the subsequent etching effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 is a flow chart of the etching method of the present invention;

[0044] Figure 2 A flow chart for determining the stability category of the photoresist during the exposure process of the present invention;

[0045] Figure 3 A flow chart for determining a process for photomask exposure of a silicon wafer;

[0046] Figure 4 Flowchart for determining whether the exposure process meets the stability standard. DETAILED DESCRIPTION

[0047] In order to make the objects and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with embodiments; it should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0048] The preferred embodiments of the present invention are described below with reference to the accompanying drawings. It should be understood by those skilled in the art that these embodiments are only used to explain the technical principles of the present invention and are not intended to limit the protection scope of the present invention.

[0049] It should be noted that, in the description of the present invention, terms such as "up", "down", "left", "right", "inside" and "outside" indicating directions or positional relationships are based on the directions or positional relationships shown in the drawings. This is merely for the convenience of description and does not indicate or imply that the device or element must have a specific orientation, be constructed and operated in a specific orientation. Therefore, it cannot be understood as a limitation on the present invention.

[0050] In addition, it should be noted that in the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0051] See also Figures 1 to 4 As shown, Figure 1 is a flow chart of the etching method of the present invention, Figure 2 The flowchart of the present invention for determining the stability category of the photoresist during the exposure process, Figure 3 A flow chart for determining the processing method for photomask exposure of silicon wafers. Figure 4 A flowchart for determining whether an exposure process meets a stability standard. The etching method according to an embodiment of the present invention includes:

[0052] Step S1, performing an irradiation hardness change experiment on the desired photoresist, including irradiating the photoresist surface with a predetermined exposure intensity after coating the photoresist, and recording the hardness change of the photoresist before and after the exposure;

[0053] Step S2, obtaining a photomask pattern of a desired photomask, determining texture features in the photomask pattern, and calculating process stability characterization parameters in combination with the hardness variation to determine the stability category of the photoresist during the exposure process, wherein the texture features include the number of texture intersections and the mean value of the texture gaps;

[0054] Step S3, determining a preheating temperature based on the process stability characterization parameter to preheat the silicon wafer coated with the photoresist, and performing photomask exposure on the silicon wafer based on the stability category of the photoresist during the exposure process, including:

[0055] Adjusting the exposure intensity for exposure, determining a specific observation area based on the texture of the photomask pattern, and determining whether the exposure process meets the stability standard according to the axial height discrete difference of each feature point in the specific observation area on the photoresist surface during the exposure process, so as to correct the exposure intensity;

[0056] Or, maintaining the initial exposure intensity to complete the photomask exposure;

[0057] Step S4, developing and etching the exposed silicon wafer and removing the photoresist on the silicon wafer to obtain an etched silicon wafer.

[0058] Specifically, there is no limitation on the specific material of the photoresist, and those skilled in the art may select the material of the photoresist according to specific needs, which will not be elaborated here.

[0059] Specifically, there is no limitation on the specific method of measuring the surface hardness of the photoresist. For example, a nanoindentation experiment can be used to detect the photoresist coated on the silicon wafer to determine the hardness. Of course, other methods can also be used, which will not be repeated here.

[0060] Specifically, the process stability characterization parameter is calculated based on formula (1):

[0061] ,

[0062] In formula (1), Z is the process stability characterization parameter, P represents the number of grain intersections, P0 represents the preset grain intersection number threshold, D represents the grain gap mean, D0 represents the preset grain gap standard threshold, F represents the hardness change, and F0 represents the preset hardness change threshold.

[0063] Specifically, in this embodiment, the preset standard threshold value D0 of the texture gap is obtained in advance, and a number of photomask samples are obtained, the texture gaps of different photomasks are recorded, and the texture gap mean △D is solved, and D0=α×△D is set, α represents the first accuracy coefficient, 0.75<α<0.85.

[0064] Specifically, in this embodiment, the preset threshold value P0 of the number of texture intersections is obtained in advance, and a number of photomask samples are obtained, the number of texture intersections of different photomasks is recorded, and the mean number of texture intersections △P is solved, and P0=β×△P is set, β represents the second precision coefficient, 0.68<β<0.82.

[0065] Specifically, in this embodiment, the preset hardness variation threshold F0 is obtained by pre-measurement, and an irradiation hardness variation experiment is performed on a number of photoresist samples to determine the hardness variation mean value, which is set as the hardness variation threshold value.

[0066] Specifically, there is no limitation on the method of identifying the intersections and gaps of grains. An image processing algorithm or model that can identify the intersections and gaps of grains can be pre-trained and imported into a computer to process the mask sample to achieve the corresponding function, which will not be elaborated here.

[0067] See also Figure 2 As shown, it is a flow chart of determining the stability category of the photoresist during the exposure process of the present invention.

[0068] Specifically, the stability category of the photoresist during the exposure process is determined according to the process stability characterization parameters, wherein:

[0069] If the process stability characterization parameter is greater than or equal to a preset process stability characterization parameter standard threshold, determining that the stability category of the photoresist is a weak stability category;

[0070] If the process stability characterization parameter is less than the preset process stability characterization parameter standard threshold, the stability category of the photoresist is determined to be a strong stability category.

[0071] Specifically, the preset process stability characterization parameter standard threshold value Z0 is selected between the interval [1.4, 1.6].

[0072] The present invention calculates the process stability characterization parameters taking into account the texture characteristics and the hardness variation. In actual situations, the texture of the photomask pattern is in a corresponding relationship with the photoresist texture. During the exposure process, when the photoresist texture is relatively complex and the texture gaps are relatively close, the exposed area of ​​the photoresist undergoes property changes under exposure, which causes stress interference to the surrounding photoresist texture areas. If the texture areas are dense and relatively close, multi-directional stress interference and uneven stress are generated, which can easily lead to uneven edges of the photoresist texture areas and poor stability. Furthermore, if the hardness variation of the photoresist during the exposure process is large, the above phenomenon will be aggravated. Therefore, the present invention calculates the process stability characterization parameters through the texture characteristics and the hardness variation to characterize the stability of the edge of the photoresist pattern under complex patterns.

[0073] See also Figure 3 As shown, it is a flow chart for determining a processing method for photomask exposure for a silicon wafer.

[0074] Specifically, in step S3, a photomask exposure is performed on the silicon wafer based on the stability category of the photoresist during the exposure process, wherein:

[0075] If the photoresist is of a weakly stable type, the exposure intensity to be adjusted is selected for exposure, a specific observation area is determined based on the texture of the photomask pattern, and whether the exposure process meets the stability standard is determined according to the axial height discrete difference of each feature point in the specific observation area on the surface of the photoresist during the exposure process, so as to correct the exposure intensity;

[0076] If the photoresist is of a strong stable type, it is selected to maintain the initial exposure intensity to complete the photomask exposure.

[0077] Specifically, in step S3, adjusting the exposure intensity for exposure includes:

[0078] increasing the exposure intensity based on the process stability characterization parameter;

[0079] Among them, the increase in exposure intensity is positively correlated with the process stability characterization parameters.

[0080] In this embodiment, optionally,

[0081] The process stability characterization parameter Z is compared with a preset first process stability characterization parameter standard threshold value Z1 and a second process stability characterization parameter standard threshold value Z2,

[0082] If Z≤Z1, increase the first exposure intensity Q1 and set Q1=0.2×Q0;

[0083] If Z1<Z≤Z2, increase the second exposure intensity Q2 and set Q2=0.25×Q0;

[0084] If Z2<Z, increase the third exposure intensity Q3 and set Q3=0.3×Q0;

[0085] Where Q0 is the initial exposure intensity, Z1=1.1×Z0, Z2=1.3×Z0.

[0086] Specifically, the specific observation area is determined based on the texture of the photomask pattern, including:

[0087] Performing grayscale processing on the photomask pattern;

[0088] Dividing the photomask pattern into a number of observation areas;

[0089] The area ratio of each grain gap in each observation area is calculated, and the observation area with an area ratio higher than the preset area ratio is recorded as a special observation area.

[0090] Specifically, in this embodiment, the preset area ratio is selected between the interval [0.45, 0.75].

[0091] See also Figure 4 As shown, it is a flow chart for determining whether the exposure process meets the stability standard.

[0092] Specifically, whether the exposure process meets the stability standard is determined based on the discrete differences in the axial heights of each feature point in each specific observation area on the photoresist surface during the exposure process, wherein:

[0093] If the discrete difference is greater than or equal to the preset discrete difference standard threshold, it is determined that the exposure process does not meet the stability standard;

[0094] If the discrete difference is less than the preset discrete difference standard threshold, it is determined that the exposure process meets the stability standard.

[0095] It is understandable that the feature points need to be set in areas not covered by the photomask, such as in the gaps between the textures of the photomask.

[0096] For weakly stable photoresists, since the texture areas are dense and the textures are relatively close, it is considered to adaptively increase the exposure intensity to expose the local photoresist derived from stress interference and stress unevenness, thereby improving the edge unevenness phenomenon. In addition, the present invention considers determining the discrete differences in the axial heights of each feature point in the specific observation area to characterize the uniformity of the property changes of the photoresist in the specific observation area during the exposure process. In actual situations, if the property changes are uneven and there is multi-directional stress interference, slight undulations may occur on the surface of the specific observation area of ​​the photoresist, affecting the exposure process. Based on this, it is determined whether the exposure process meets the standards, and the exposure intensity is adaptively adjusted to improve the uniformity of the photoresist edge and ensure the subsequent etching effect.

[0097] Specifically, in this embodiment, the preset discrete difference standard threshold L0 is obtained by pre-measurement, and the discrete differences in the historical photomask exposure process are collected to solve the discrete difference mean △L, and set L0=γ×△L, γ represents the third precision coefficient, 0.65<γ<0.85.

[0098] Specifically, in step S3, the process of calculating the discrete difference includes:

[0099] Establishing a three-dimensional model of each specific observation area to determine the axial height of each characteristic point in each specific observation area;

[0100] Calculate the variance of the axial height of each feature point for each specific observation area;

[0101] The mean of the variance corresponding to each specific observation area is determined as the discrete difference.

[0102] There is no limitation on the method of constructing the three-dimensional model. For example, a laser scanning device can be used to obtain point cloud data of a specific observation area, and a three-dimensional model can be constructed accordingly to obtain the axial height of each feature point. This will not be elaborated here.

[0103] Specifically, when it is determined that the exposure process does not meet the stability standard, the exposure intensity is reduced based on the discrete difference, and the reduction amount of the exposure intensity is positively correlated with the discrete difference.

[0104] In this embodiment, optionally,

[0105] The discrete difference L is compared with a preset first discrete difference standard threshold L1 and a preset second discrete difference standard threshold L2,

[0106] If L≤L1, reduce the first reduction amount Qe1 and set Qe1=0.1×Qe0;

[0107] If L1<L≤L2, then reduce the second reduction amount Qe2 and set Qe2=0.15×Qe0;

[0108] If L2<L, the third reduction amount Qe3 is reduced, and Qe3=0.2×Qe0 is set;

[0109] Among them, L1=1.12×L0, L2=1.25×L0, and Qe0 represents the current exposure intensity.

[0110] When the exposure intensity is too strong, it causes slight undulations on the surface of the photoresist in the specific observation area, affecting the exposure process. The exposure intensity should be adaptively corrected to alleviate the above phenomenon.

[0111] So far, the technical solutions of the present invention have been described in conjunction with the preferred embodiments shown in the accompanying drawings. However, it is easy for those skilled in the art to understand that the protection scope of the present invention is obviously not limited to these specific embodiments. Without departing from the principle of the present invention, those skilled in the art can make equivalent changes or substitutions to the relevant technical features, and the technical solutions after these changes or substitutions will fall within the protection scope of the present invention.

Claims

1. An etching method, characterized in that: include: Step S1, performing an irradiation hardness change experiment on the desired photoresist, including irradiating the photoresist surface with a predetermined exposure intensity after coating the photoresist, and recording the hardness change of the photoresist before and after the exposure; Step S2, obtaining a photomask pattern of a desired photomask, determining texture features in the photomask pattern, and calculating process stability characterization parameters in combination with the hardness variation to determine the stability category of the photoresist during the exposure process, wherein the texture features include the number of texture intersections and the mean value of the texture gaps; Step S3, determining a preheating temperature based on the process stability characterization parameter to preheat the silicon wafer coated with the photoresist, and performing photomask exposure on the silicon wafer based on the stability category of the photoresist during the exposure process, including: Adjusting the exposure intensity for exposure, determining a specific observation area based on the texture of the photomask pattern, and determining whether the exposure process meets the stability standard according to the axial height discrete difference of each feature point in the specific observation area on the photoresist surface during the exposure process, so as to correct the exposure intensity; Or, maintaining the initial exposure intensity to complete the photomask exposure; Step S4, developing and etching the exposed silicon wafer and removing the photoresist on the silicon wafer to obtain an etched silicon wafer.

2. The etching method according to claim 1, characterized in that: The process stability characterization parameter is calculated based on formula (1): , In formula (1), Z is the process stability characterization parameter, P represents the number of grain intersections, P0 represents the preset grain intersection number threshold, D represents the grain gap mean, D0 represents the preset grain gap standard threshold, F represents the hardness change, and F0 represents the preset hardness change threshold.

3. The etching method according to claim 1, characterized in that: The stability category of the photoresist during the exposure process is determined according to the process stability characterization parameters, wherein: If the process stability characterization parameter is greater than or equal to a preset process stability characterization parameter standard threshold, determining that the stability category of the photoresist is a weak stability category; If the process stability characterization parameter is less than the preset process stability characterization parameter standard threshold, the stability category of the photoresist is determined to be a strong stability category.

4. The etching method according to claim 3, characterized in that: The preheating temperature is determined based on the process stability characterization parameter, wherein: The preset temperature is positively correlated with the preset process stability characterization parameter.

5. The etching method according to claim 1, characterized in that: In step S3, a photomask exposure is performed on the silicon wafer based on the stability category of the photoresist during the exposure process, wherein: If the photoresist is of a weakly stable type, the exposure intensity to be adjusted is selected for exposure, a specific observation area is determined based on the texture of the photomask pattern, and whether the exposure process meets the stability standard is determined according to the axial height discrete difference of each feature point in the specific observation area on the surface of the photoresist during the exposure process, so as to correct the exposure intensity; If the photoresist is of a strong stable type, it is selected to maintain the initial exposure intensity to complete the photomask exposure.

6. The etching method according to claim 1, characterized in that: In step S3, adjusting the exposure intensity for exposure includes: increasing the exposure intensity based on the process stability characterization parameter; Among them, the increase in exposure intensity is positively correlated with the process stability characterization parameters.

7. The etching method according to claim 1, characterized in that: Determine specific observation areas based on the texture of the photomask pattern, including: Performing grayscale processing on the photomask pattern; Dividing the photomask pattern into a number of observation areas; The area ratio of each grain gap in each observation area is calculated, and the observation area with an area ratio higher than the preset area ratio is recorded as a special observation area.

8. The etching method according to claim 1, characterized in that: Whether the exposure process meets the stability standard is determined based on the discrete differences in the axial heights of each feature point in each specific observation area on the photoresist surface during the exposure process, wherein: If the discrete difference is greater than or equal to the preset discrete difference standard threshold, it is determined that the exposure process does not meet the stability standard; If the discrete difference is less than the preset discrete difference standard threshold, it is determined that the exposure process meets the stability standard.

9. The etching method according to claim 8, characterized in that: In step S3, the process of calculating the discrete difference includes: Establishing a three-dimensional model of each specific observation area to determine the axial height of each characteristic point in each specific observation area; Calculate the variance of the axial height of each feature point for each specific observation area; The mean of the variance corresponding to each specific observation area is determined as the discrete difference.

10. The etching method according to claim 9, characterized in that: When it is determined that the exposure process does not meet the stability standard, the exposure intensity is reduced based on the discrete difference, and the reduction amount of the exposure intensity is positively correlated with the discrete difference.

Citation Information

Patent Citations

  • Etching method

    CN111584360A

  • Transfer printing method, photomask for transfer printing and manufacturing method thereof

    CN101782718A

  • Method for verifying photoresist defect

    CN114609868A

  • Method and apparatus for modification of chemically amplified photoresist by electron beam exposure