Dredged mud dewatering method free of tail water treatment

By pre-adding trivalent metal ion-modified zeolite and flocculant to the dredging mud, the problem of high nitrogen content in the tail water and low nitrogen content in the mud cake is solved, achieving rapid dehydration and effective utilization of nitrogen resources, and satisfying the surface water environment Quality standards and soil resource utilization needs.

CN118833982APending Publication Date: 2024-10-25JIANGSU UNIV OF SCI & TECH
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202410791200.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-19
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

The nitrogen content in the tail water during the existing dredging mud dehydration process is high, which leads to the need for expensive and inefficient denitrification treatment. Moreover, the nitrogen content in the dewatered mud cake is low, which is not conducive to its resource utilization.

Method used

Trivalent metal ion-modified zeolite is added before dewatering the dredging mud, and through stirring and flocculant treatment, particle aggregation and nitrogen adsorption are promoted to achieve rapid dehydration and tailwater nitrogen reduction, thereby obtaining a mud cake with high nitrogen content.

Benefits of technology

It realizes denitrification-free treatment of dewatered tailwater, improves dehydration efficiency, makes the dehydrated mud cake suitable as planting soil, meets surface water environmental quality standards, reduces the total nitrogen concentration of tailwater, and improves the resource utilization of mud cake. Utilization.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118833982A_ABST
    Figure CN118833982A_ABST
Patent Text Reader

Abstract

The invention discloses a tail water treatment-free dredged mud dewatering method which comprises the following steps: (1) pretreating mud: adding an acidic additive or an alkaline additive into the mud, fully stirring, adding modified zeolite, fully stirring, adding a flocculating agent, fully stirring, standing, discharging supernate after standing, and filtering to obtain filtrate; sediment is obtained; and (2) filtering and dehydrating the sediment to obtain a solid mud cake and liquid tail water. According to the method disclosed by the invention, the dehydrated tail water can be directly discharged without denitrification treatment, the dehydration efficiency of the mud can be effectively improved, and finally, the dehydrated mud cake can be used as planting soil, so that resource utilization of the mud cake is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for processing dredging mud. Background Art

[0002] Eutrophication of rivers, lakes and reservoirs will promote the excessive growth of algae and other plant plankton, also known as algal bloom. Algal bloom will reduce the transparency of the water body and hinder the photosynthesis of underwater plants, thus destroying the ecological balance. Since the bottom mud of rivers, lakes and reservoirs is rich in nutrients such as nitrogen and phosphorus, it is an "endogenous pollutant" of eutrophication and needs to be removed urgently. It is currently a common practice to remove the bottom mud rich in nutrients by suction dredging. At present, there are three main problems in the dehydration of dredged mud:

[0003] (1) After the mud is dehydrated, the nitrogen originally enriched in the bottom mud will be transferred to the tailwater, resulting in a high concentration of nitrogen in the tailwater. Therefore, the tailwater needs to be treated to reduce the nitrogen content to the relevant water quality requirements before it can be discharged. (2) If traditional physical, chemical, biological and other methods are used to denitrify the tailwater, on the one hand, the treatment time is long and it will occupy a lot of space. On the other hand, the treatment cost is high and the treatment effect is limited. (3) After the mud is dehydrated, most of the nitrogen is transferred to the tailwater, making the nitrogen content in the mud cake lower. The loss of nitrogen means the loss of nutrients, which is not conducive to the subsequent resource utilization of the mud cake as planting soil.

[0004] Therefore, the basic idea of ​​existing technologies for dredging tailwater treatment is to perform secondary treatment on the tailwater after it is generated, and there is currently no technology that can directly discharge the tailwater. Summary of the invention

[0005] Purpose of the invention: The purpose of the present invention is to provide a method for dewatering dredged mud without tailwater treatment. The method can make the dewatered tailwater be discharged directly without denitrification treatment, and can also effectively improve the dewatering efficiency of the mud. Finally, the dewatered mud cake can be used as planting soil to realize its resource utilization.

[0006] Technical solution: The dredged mud dewatering method without tailwater treatment of the present invention comprises the following steps:

[0007] (1) Pre-treating the mud: adding an acidic admixture or an alkaline admixture to the mud, stirring it fully, then adding a modified zeolite thereto, stirring it fully, and finally adding a flocculant thereto, stirring it fully and letting it stand, and then discharging the supernatant after standing to obtain a sediment;

[0008] (2) The sediment is filtered and dehydrated to obtain a solid mud cake and liquid tail water.

[0009] Wherein, in step (1), the acidic admixture is any one of acetic acid, citric acid, oxalic acid, lactic acid, formic acid, ferric chloride, aluminum sulfate, aluminum chloride, calcium chloride, magnesium chloride, manganese chloride, ammonium sulfate, calcium hydrogen phosphate or sodium citrate; the alkaline admixture is any one of sodium hydroxide, potassium hydroxide, calcium hydroxide, magnesium hydroxide, sodium carbonate, sodium bicarbonate, potassium carbonate, calcium oxide or magnesium oxide. The acidic and alkaline admixtures are used to adjust the pH value of the mud to improve the precipitation conditions.

[0010] Wherein, in step (1), the modified zeolite is a trivalent metal ion modified zeolite, and the trivalent metal ions may include but are not limited to the following: Fe 3+ or Al 3+ Any one of; the particle size of the modified zeolite is 200 to 400 mesh.

[0011] The modified zeolite is prepared by the following method: adding zeolite to a salt solution containing trivalent metal ions, placing the solution containing zeolite in a constant temperature water bath, stirring while reacting, and after the reaction is completed, washing and drying the obtained solid product to obtain a trivalent metal ion modified zeolite. The zeolite particles are chemically modified to change their zeta potential, giving them a positive potential. This modified zeolite not only adsorbs nitrogen more effectively due to the change in its charge properties, but also has a higher positive potential. After being added to the mud in advance, it can promote particle aggregation, improve the flocculation effect, and thus increase the dehydration rate.

[0012] The particle size of the zeolite is 200-400 meshes to ensure the modification effect and application efficiency.

[0013] The water bath temperature is 80-90°C, the stirring time is 90-100 min, and the rotation speed is 110-130 rpm.

[0014] After the reaction is completed, the zeolite is washed several times with distilled water to remove surface residues, and then placed in an oven at a drying temperature of 50 to 90°C.

[0015] Wherein, in step (1), the flocculant is any one of ferric chloride, polyacrylamide, polyaluminum sulfate, polyaluminum chloride, polyaluminum silicate, polyaluminum sulfate, polyaluminum passivated polymer, polyiron passivated polymer, polyaluminum passivated silicate, polyferric sulfate, polyferric chloride, polyammonium ferric chloride, polyammonium aluminum silicate, aluminum sulfate, ferrous sulfate, chitosan or guar gum.

[0016] Wherein, in step (1), the water content of the mud is higher than the mud liquid limit; the mass ratio of the acidic admixture or the alkaline admixture to the mud dry matter is 45:1000-1200; the stirring speed is 600-650rpm, and the stirring time is 20-25min.

[0017] Wherein, in step (1), the mass ratio of modified zeolite to mud dry matter is 50:1000-1200; the stirring speed is 500-550 rpm, and the stirring time is 15-20 min.

[0018] Wherein, in step (1), the mass ratio of flocculant to mud dry matter is 2:1000-1200; the stirring speed is 500-550rpm, the stirring time is 5-10min; and the standing time is 10-15min.

[0019] Wherein, in step (2), a high-pressure plate frame is used to filter and dehydrate the sediment, the pressure is not less than 1.0 MPa, and the moisture content of the obtained mud cake is not higher than 35%.

[0020] The method of the present invention achieves the "triple effect" of rapid dehydration of mud, no treatment of dehydration tail water, and soil resource utilization of dehydrated mud cake by pre-adding modified zeolite before dehydration of dredged mud. Through trivalent metal ion modification, zeolite not only maintains excellent pore structure, but also enhances its ion exchange capacity, especially adsorbing negatively charged nitrogen compounds; in addition, modified zeolite with smaller particle size has more adsorption sites due to its large specific surface area, thereby significantly improving its nitrogen adsorption capacity; trivalent metal ion modified zeolite can also promote the aggregation of particles into larger flocs, which are easy to dehydrate and separate.

[0021] Beneficial effects: Compared with the prior art, the present invention has the following significant advantages: (1) The method of the present invention can achieve denitrification-free treatment of dewatered tail water. By adding modified zeolite to the mud in advance, the ammonia nitrogen concentration in the tail water generated by the dredged mud during the dewatering process can be reduced to 2 mg / L or below, meeting the Class V water standard in the surface water environmental quality standard, so that it can be safely discharged; (2) The method of the present invention can improve the efficiency of mud dewatering. The small-particle zeolite modified by trivalent metal ions has a large specific surface area, positive potential, high ion exchange capacity and excellent pore structure, thereby effectively improving the dewatering rate of the mud; (3) The method of the present invention can realize the resource utilization of the dewatered mud cake as planting soil. By pre-treating nitrogen during the dewatering process of the dredged mud, the nitrogen element is converted from a dissolved state to an adsorbed state in the solid phase, so that the dewatered tail water is low in nitrogen and the dewatered mud cake is rich in nitrogen, which is suitable for use as planting soil; and it can also achieve long-term slow release of nitrogen to maintain the lasting nutritional properties of the soil. Therefore, the method of the present invention can effectively reduce the total nitrogen concentration in the tail water during the dehydration process and increase the nitrogen content in the mud cake, thereby eliminating the need for tail water treatment and improving the resource utilization rate of the mud cake, and also improving the mud dehydration efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a process flow chart of the method of the present invention. DETAILED DESCRIPTION

[0023] Example 1

[0024] The dredging mud dehydration method without tailwater treatment of the present invention is applied to Taihu dredging mud with a water content of 400%, wherein the initial TN content of free water in the mud is 31.2 mg / L, and specifically comprises the following steps:

[0025] (1) Add the acidic admixture ferric chloride and the mud dry matter in a mass ratio of 45:1000 to the mud with a water content higher than the mud liquid limit, set the stirring speed to 600 rpm, and stir for 20 minutes;

[0026] (2) Then, Al 3+ Modified zeolite particles and mud dry matter were added to the mud at a mass ratio of 50:1000 (the amount of zeolite added was equivalent to 5% of the mud dry matter mass), the stirring speed was set to 500 rpm, and stirring was carried out for 15 min;

[0027] (3) Finally, cationic polyacrylamide and mud dry matter were added to the mud with a water content of 400% in a mass ratio of 2:1000, the stirring speed was set to 500 rpm, stirred for 5 minutes, and then allowed to stand for 10 minutes, and the supernatant was discharged to obtain sediment;

[0028] (4) The sediment was subjected to high-pressure plate and frame filtration dehydration for 40 min at a pressure of 1.0 MPa. The mud was quickly dehydrated to obtain a mud cake with a pH of 7.3 and a water content of 35%. The solid mud cake and liquid tail water were effectively separated, and the TN (total nitrogen) concentration in the tail water was 1.1 mg / L.

[0029] Based on the above steps, it can be seen that the total reaction time from the addition of zeolite to the production of tail water is 70 minutes (15+5+10+40=70), and the time for filtration and dehydration is 40 minutes.

[0030] Among them, Al 3+ The modified zeolite is prepared by the following method, specifically:

[0031] (1.1) Add 200 g of zeolite with a particle size of 200 mesh into 1 L of Al 3+ In a 1M aluminum ion solution, place the beaker containing zeolite in a constant temperature water bath, set the temperature to 90°C, set the stirrer speed to 120 rpm, and continue stirring evenly for 90 minutes;

[0032] (1.2) After stirring, the zeolite was washed twice with distilled water to remove surface residues, then placed in an oven (temperature set at 50°C) for drying, and sealed for subsequent use.

[0033] Comparative Example 1

[0034] The difference between Comparative Example 1 and Example 1 is mainly that the order of adding zeolite is different, that is, in Comparative Example 1, the modified zeolite is directly added to the tail water, while in Example 1, the modified zeolite is added to the mud before the mud is dehydrated; the specific steps are as follows:

[0035] (1) Add the acidic admixture ferric chloride and the mud dry matter in a mass ratio of 45:1000 to the mud with a water content higher than the mud liquid limit, set the stirring speed to 600 rpm, and stir for 20 minutes;

[0036] (2) cationic polyacrylamide and mud dry matter were added to the mud with a water content of 400% at a mass ratio of 2:1000, the stirring speed was set to 500 rpm, stirred for 5 minutes, and then allowed to stand for 10 minutes, and the supernatant was discharged to obtain a sediment;

[0037] (3) The sediment was dehydrated by high-pressure plate and frame filtration. The dehydration time was 75 min and the pressure was set to 1.0 MPa. The mud was quickly dehydrated to obtain a mud cake with a pH of 7.3 and a water content of 35%. The solid mud cake and liquid tail water were separated.

[0038] (4) Add 7% (7% is defined as the mass ratio of modified zeolite particles to mud dry matter is 70:1000) of Al2O3 with a particle size of 200 mesh to the dehydrated tail water. 3+ The modified zeolite particles were stirred at a speed of 500 rpm for 120 min. The nitrogen content in the tail water was detected and the TN concentration was 2.5 mg / L.

[0039] Based on the above steps, it can be seen that the total reaction time of adding zeolite to tail water is 120 minutes, and the time for filtration and dehydration is 75 minutes.

[0040] It can be seen from Comparative Example 1 that when more zeolite (7%) is added to the tail water for adsorption and the adsorption time is longer (120 min), the TN concentration in the tail water is 2.5 mg / L, which still does not meet the standard of Class V water (≤2 mg / L) in the surface water environmental quality standard, and the tail water cannot be discharged directly. However, by changing the addition order of the modified zeolite in Example 1, only 5% of the zeolite addition amount and only 70 min of adsorption time are required to achieve a TN concentration in the tail water as low as 1.1 mg / L.

[0041] In addition, it can be seen from Comparative Example 1 that in order to obtain a mud cake with a moisture content of 35%, dehydration for 75 minutes is required; while in Example 1, due to the order of adding modified zeolite, only 40 minutes of dehydration is required to produce a mud cake with a moisture content of 35%.

[0042] Comparative Example 2

[0043] The difference between Comparative Example 2 and Example 1 is that the zeolite in Comparative Example 2 is not modified, that is, the zeolite in Comparative Example 2 uses original zeolite. The specific steps are as follows:

[0044] (1) Add the acidic admixture ferric chloride and the mud dry matter in a mass ratio of 45:1000 to the mud with a water content higher than the mud liquid limit, set the stirring speed to 600 rpm, and stir for 20 minutes;

[0045] (2) Add zeolite particles with a particle size of 200 mesh to the mud dry matter in a mass ratio of 50:1000 (the amount of zeolite added is equivalent to 5% of the mass of the mud dry matter), set the stirring speed to 500 rpm, and stir for 15 minutes;

[0046] (3) Finally, cationic polyacrylamide and mud dry matter were added to the mud with a water content of 400% at a mass ratio of 2:1000, the stirring speed was set to 500 rpm, stirred for 5 minutes, and then allowed to stand for 10 minutes, and the supernatant was discharged to obtain a sediment;

[0047] (4) The sediment was dehydrated by high-pressure plate and frame filtration. The dehydration time was 85 min and the pressure was set to 1.0 MPa. The mud was quickly dehydrated to obtain a mud cake with a pH of 7.3 and a water content of 35%. The solid mud cake and liquid tail water were effectively separated. The TN concentration in the tail water was 4.4 mg / L.

[0048] Based on the above steps, it can be seen that the total reaction time from the addition of zeolite to the production of tail water is 115 minutes (15+5+10+85=115), and the time for filtration and dehydration is 85 minutes.

[0049] It can be seen from Comparative Example 2 that if the zeolite is not modified and the pre-treated dredged mud is directly dehydrated, on the one hand, the total nitrogen concentration in the tail water is still very high and does not meet the demand for direct discharge. It is better to directly use zeolite to modify the generated tail water; on the other hand, it has little effect on the fluctuation of the mud dehydration rate. The specific resistance of Comparative Example 2 is 6.2×10 10 m / kg, compared with Example 1, it does not have an efficient dehydration rate, and the filtration dehydration time is as high as 85 min.

[0050] Comparative Example 3

[0051] The main difference between Comparative Example 3 and Example 1 is that the zeolite in Comparative Example 3 is Na + Modification, that is, the zeolite of Comparative Example 3 adopts Na + Modified zeolite, the specific steps are as follows:

[0052] (1) Add the acidic admixture ferric chloride and the mud dry matter in a mass ratio of 45:1000 to the mud with a water content higher than the mud liquid limit, set the stirring speed to 600 rpm, and stir for 20 minutes;

[0053] (2) Then, the Na + Modified zeolite particles and mud dry matter were added to the mud at a mass ratio of 80:1000 (the amount of zeolite added was equivalent to 8% of the mud dry matter mass), the stirring speed was set to 500 rpm, and stirring was carried out for 15 min;

[0054] (3) Finally, cationic polyacrylamide and mud dry matter were added to the mud with a water content of 400% at a mass ratio of 2:1000, the stirring speed was set to 500 rpm, stirred for 5 minutes, and then allowed to stand for 10 minutes, and the supernatant was discharged to obtain a sediment;

[0055] (4) The sediment was subjected to high-pressure plate and frame filtration dehydration. The dehydration time was 71 min and the pressure was set to 1.0 MPa. The mud was quickly dehydrated to obtain a mud cake with a pH of 7.3 and a water content of 35%. The solid mud cake and liquid tail water were effectively separated. The TN (total nitrogen) concentration in the tail water was 2.4 mg / L.

[0056] Based on the above steps, it can be seen that the total reaction time from the addition of zeolite to the production of tail water is 101 min (15+5+10+71=101), and the time for filtration and dehydration is 71 min.

[0057] Among them, Na + The modified zeolite is prepared by the following method, specifically:

[0058] (1.1) Add 200 g of zeolite with a particle size of 200 mesh into 1 L of Na + In a 1M sodium ion solution, place the beaker containing zeolite in a constant temperature water bath, set the temperature to 90°C, set the stirrer speed to 120 rpm, and continue stirring evenly for 90 minutes;

[0059] (1.2) After stirring, the zeolite was washed twice with distilled water to remove surface residues, then placed in an oven (temperature set at 50°C) for drying, and sealed for subsequent use.

[0060] Comparative Example 3 shows that if the zeolite is not modified with trivalent metal ions but with Na + The modified zeolite was used to pre-treat the dredged mud for dewatering. On the one hand, the total nitrogen concentration in the tailwater was still very high, which did not meet the demand for direct discharge. It was not as good as the result of adsorption treatment by directly adding zeolite to the tailwater. On the other hand, it had little effect on the fluctuation of the mud dewatering rate. The specific resistance of comparative example 2 was 5.2×1010 m / kg, compared with Example 1, it does not have a high dehydration rate, and the filtration dehydration time is as long as 71 min.

[0061] Comparative Example 4

[0062] The difference between Comparative Example 4 and Example 1 is that the particle size of the zeolite in Comparative Example 4 is 35 mesh, that is, the zeolite in Comparative Example 4 uses a modified zeolite that has passed through a 35 mesh sieve. The specific steps are as follows:

[0063] (1) Add the acidic admixture ferric chloride and the mud dry matter in a mass ratio of 45:1000 to the mud with a water content higher than the mud liquid limit, set the stirring speed to 600 rpm, and stir for 20 minutes;

[0064] (2) Then, Al 3+ Modified zeolite particles and mud dry matter were added to the mud at a mass ratio of 70:1000 (the amount of zeolite added was equivalent to 7% of the mud dry matter mass), the stirring speed was set to 500 rpm, and stirring was carried out for 15 min;

[0065] (3) Finally, cationic polyacrylamide and mud dry matter were added to the mud with a water content of 400% at a mass ratio of 2:1000, the stirring speed was set to 500 rpm, stirred for 5 minutes, and then allowed to stand for 10 minutes, and the supernatant was discharged to obtain a sediment;

[0066] (4) The sediment was subjected to high-pressure plate and frame filtration dehydration. The dehydration time was 58 min and the pressure was set to 1.0 MPa. The mud was quickly dehydrated to obtain a mud cake with a pH of 7.3 and a water content of 35%. The solid mud cake and liquid tail water were effectively separated. The TN (total nitrogen) concentration in the tail water was 5.2 mg / L.

[0067] Based on the above steps, it can be seen that the total reaction time from the addition of zeolite to the production of tail water is 88 minutes (15+5+10+58=88), and the time for filtration and dehydration is 58 minutes.

[0068] Among them, Al 3+ The modified zeolite is prepared by the following method, specifically:

[0069] (1.1) Add 200 g of zeolite with a particle size of 35 mesh into 1 L of Al 3+ In a 1M aluminum ion solution, place the beaker containing zeolite in a constant temperature water bath, set the temperature to 90°C, set the stirrer speed to 120 rpm, and continue stirring evenly for 90 minutes;

[0070] (1.2) After stirring, the zeolite was washed twice with distilled water to remove surface residues, then placed in an oven (temperature set at 50°C) for drying, and sealed for subsequent use.

[0071] It can be seen from Comparative Example 4 that if the modified zeolite particle size is not appropriate, such as using 35-mesh modified zeolite for pre-treatment of dredged mud dewatering, on the one hand, the total nitrogen concentration in the tail water is still very high, which does not meet the demand for direct discharge, and it is not as good as directly adding zeolite into the tail water for adsorption treatment; on the other hand, it has little effect on the fluctuation of the mud dewatering rate. The specific resistance of Comparative Example 2 is 3.7×10 10 m / kg, compared with Example 1, it does not have a high dehydration rate, and the filtration and dehydration time is 58 min.

[0072] Table 1 shows the TN concentration and specific resistance results in the tail water of Example 1 and Comparative Examples 1 to 2

[0073] Physical and chemical properties Example 1 Comparative Example 1 Comparative Example 2 Comparative Example 3 Comparative Example 4 Tail water TN (mg / L) 1.1 2.5 4.4 2.7 5.2 Specific resistance (m / kg) <![CDATA[1.11×10 10 ]]> <![CDATA[5.6×10 10 ]]> <![CDATA[6.2×10 10 ]]> <![CDATA[5.2×10 10 ]]> <![CDATA[3.7×10 10 ]]>

[0074] It can be seen from Table 1 that the TN concentration of the tail water of Example 1 is 1.1 mg / L, which meets the standard of Class V water in the surface water environmental quality standard (≤2 mg / L) and can be discharged directly. Compared with Example 1, which adds modified zeolite to the mud before dehydration and Comparative Example 1, which adds modified zeolite to the tail water after dehydration, the former can more effectively reduce the TN content in the tail water, that is, it has a more efficient nitrogen removal efficiency. In addition, the specific resistance of Example 1 is 1.11×10 10 m / kg, while the specific resistance of comparative example 1 is higher, indicating that adding modified zeolite to the mud before dehydration can greatly improve the dehydration rate of dredged mud.

[0075] Comparative Examples 2 to 4 use the same zeolite addition order as Example 1, i.e., zeolite is added before mud dehydration. It can be seen that if suitable zeolite is not used, the TN index of the tail water not only cannot meet the requirements for direct discharge, but the TN index is even worse than that of Comparative Example 1. It is better to directly add zeolite to the tail water for adsorption.

[0076] Table 2 shows the TN content of the mud cakes obtained in Example 1 and Comparative Examples 1 to 4 as planting soil

[0077] Mud cake physical and chemical properties Example 1 Comparative Example 1 Comparative Example 2 Comparative Example 3 Comparative Example 4 TN (mg / kg) 1662.21 512.27 1021.57 1257.58 722.53

[0078] It can be seen from Table 2 that the TN content of the mud cake of Example 1 is significantly higher than that of Comparative Example 1. This is because the addition of modified zeolite in advance adsorbs most of the TN in a particle state, which remains in the mud cake after filtration and dehydration, making the TN content in the mud cake higher and easy to use as planting soil. However, the TN in the mud of Comparative Example 1 is retained in the tail water after dehydration, which not only brings difficulties to the treatment of the tail water, but also makes the TN content in the mud cake lower, which is not conducive to the subsequent soil resource utilization. By comparing Example 1 with Comparative Examples 2-4, it can be seen that the use of suitable zeolite to treat the mud can obtain a mud cake with a higher TN content, which is more conducive to the resource utilization of the mud cake planting soil.

[0079] The present invention adds modified zeolite to the waste mud for pretreatment before dehydration of the dredged mud, thereby achieving a low nitrogen content in the tail water, and the tail water can be discharged directly without treatment; compared with the conventional addition of zeolite to the dehydrated tail water to adsorb nitrogen, the present invention pre-adds modified zeolite before mud dehydration, which has a better effect of removing nitrogen. In addition, the modified zeolite also improves the dehydration efficiency of the mud, and makes the mud cake contain a higher content of nitrogen, which is easier to be used as a planting soil resource. Through reasonable zeolite modification and appropriate addition order, the triple advantages of "no need for tail water treatment", "fast dehydration rate" and "mud cake soil resource" are achieved.

Claims

1. A method for dewatering dredged mud without tailwater treatment, characterized in that: The steps include: (1) Pre-treating the mud: adding an acidic admixture or an alkaline admixture to the mud, stirring it fully, then adding a modified zeolite thereto, stirring it fully, then adding a flocculant thereto, stirring it fully, then letting it stand, and then discharging the supernatant to obtain a sediment; (2) The sediment is filtered and dehydrated to obtain a solid mud cake and liquid tail water.

2. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (1), the acidic admixture is any one of acetic acid, citric acid, oxalic acid, lactic acid, formic acid, ferric chloride, aluminum sulfate, aluminum chloride, calcium chloride, magnesium chloride, manganese chloride, ammonium sulfate, calcium hydrogen phosphate or sodium citrate; the alkaline admixture is any one of sodium hydroxide, potassium hydroxide, calcium hydroxide, magnesium hydroxide, sodium carbonate, sodium bicarbonate, potassium carbonate, calcium oxide or magnesium oxide.

3. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (1), the modified zeolite is a trivalent metal ion modified zeolite, and the metal ion is Fe 3+ or Al 3+ ; The particle size of the modified zeolite is 200-400 mesh.

4. The method for dewatering dredged mud without tailwater treatment according to claim 3, characterized in that: The modified zeolite is prepared by the following method: adding zeolite to a salt solution containing trivalent metal ions, placing the solution containing zeolite in a constant temperature water bath, stirring while reacting, and after the reaction is completed, washing and drying the obtained solid product to obtain the trivalent metal ion modified zeolite.

5. The method for dewatering dredged mud without tailwater treatment according to claim 4, characterized in that: The water bath temperature is 80-90°C; the stirring time is 90-100 min, and the rotation speed is 110-130 rpm.

6. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (1), the flocculant is any one of ferric chloride, polyacrylamide, polyaluminum sulfate, polyaluminum chloride, polyaluminum silicate, polyaluminum sulfate, polyaluminum passivated polymer, polyiron passivated polymer, polyaluminum passivated silicate, polyferric sulfate, polyferric chloride, polyammonium ferric chloride, polyammonium aluminum silicate, aluminum sulfate, ferrous sulfate, chitosan or guar gum.

7. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (1), the water content of the mud is higher than the mud liquid limit; the mass ratio of the acidic admixture or the alkaline admixture to the mud dry matter is 45:1000-1200; the stirring speed is 600-650 rpm, and the stirring time is 20-25 min.

8. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (1), the mass ratio of modified zeolite to mud dry matter is 50:1000-1200; the stirring speed is 500-550 rpm, and the stirring time is 15-20 min.

9. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (1), the mass ratio of flocculant to mud dry matter is 2:1000-1200; the stirring speed is 500-550 rpm, the stirring time is 5-10 min; and the standing time is 10-15 min.

10. The method for dewatering dredged mud without tailwater treatment according to claim 1, characterized in that: In step (2), the sediment is filtered and dehydrated by using a high-pressure plate frame, the pressure is not less than 1.0 MPa, and the moisture content of the obtained mud cake is not higher than 35%.

Citation Information

Patent Citations

  • Inorganic ion modified zeolite composite material and application thereof

    CN104941574A

  • Preparation method of efficient modified adsorbent for treating high-ammonia-nitrogen refuse leachate

    CN106268628A

  • Method for efficient in-situ control of sludge endogenous pollution

    CN107759040A

  • Bottom mud conditioning and pollutant blocking and controlling coupling treatment method

    CN114716119A