A micro LED light-emitting display device and a method for manufacturing the same

By adopting the zirconia protective layer and optimized angle design in the micro LED light emitting display device, combined with ALD and magnetron sputtering processes, the problems of low light output efficiency and easy damage to the metal layer in the prior art are solved, and more efficient Light reflection and protection.

CN118867072BActive Publication Date: 2024-12-06LOHUA CHIP-DISPLAY TECHNOLOGY DEVELOPMENT (JIANGSU) CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411339121.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-25
Publication Date
2024-12-06
Estimated Expiration
2044-09-25

AI Technical Summary

Technical Problem

The preparation process of the existing micro LED light emitting display device has insufficient optimization of the protective layer material and structure, resulting in low light output efficiency and easy damage to the metal layer during the transfer process.

Method used

Zirconia is used as the protective layer of the micro LED unit, and by optimizing the angle between the side surface and the lower surface of the micro LED unit to 50-60 degrees, a first zirconia protective layer with a rough surface and a second zirconia protection with a smooth surface is formed. The layer is formed by combining magnetron sputtering process to increase the interface area to improve the reflective performance.

Benefits of technology

It effectively improves the light output efficiency of the micro LED unit and protects the metal layer during the transfer process to avoid damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118867072B_ABST
    Figure CN118867072B_ABST
Patent Text Reader

Abstract

The present invention relates to a micro-LED light-emitting display device and a preparation method thereof, and to the field of semiconductor display technology. In the preparation method of the micro-LED light-emitting display device of the present invention, zirconium oxide is used as a protective layer of the micro-LED unit. Since zirconium oxide has a high density, the micro-LED unit can be more effectively protected. In the present application, each of the micro-LED units is provided with an upper surface, a lower surface, and an inclined side surface, and the angle between the side surface of the micro-LED unit and the lower surface of the micro-LED unit is 50-60 degrees. By optimizing the angle between the side surface of the micro-LED unit and the lower surface of the micro-LED unit, the preparation of the zirconium oxide protective layer and the first metal layer is facilitated, and the reflection performance of the side of the micro-LED unit is effectively improved, thereby improving the light extraction efficiency of the micro-LED unit.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor light emitting technology, and in particular to a micro LED light emitting display device and a preparation method thereof. Background Art

[0002] The micro-LED light-emitting display device is a new type of display device that uses advanced display technology and has many superior characteristics. The conventional preparation process of the micro-LED light-emitting display device is: first, the LED structure is designed to be micro-sized and arranged in an array; then the micro-LEDs are transferred to the circuit substrate in batches to form a high-density pixel array; then the physical deposition process is used to complete the preparation of the protective layer and the upper electrode, and then the packaging process is performed. The micro-LED light-emitting display device has a wide range of application prospects, including high-end TVs, advertising display screens, conference room screens, smart watch displays, AR / VR glasses, car displays, oversized security screens and other places. How to improve the preparation process of the micro-LED light-emitting display device is a problem of widespread concern in the industry. Summary of the invention

[0003] The object of the present invention is to overcome the above-mentioned deficiencies of the prior art and to provide a micro LED light-emitting display device and a method for preparing the same.

[0004] To achieve the above-mentioned object, the present invention provides a method for preparing a micro LED light-emitting display device, and the method for preparing the micro LED light-emitting display device comprises the following steps:

[0005] A light-emitting wafer is provided. The light-emitting wafer includes a growth substrate and an epitaxial layer located on the growth substrate.

[0006] A carrier substrate is provided, and the light-emitting wafer is disposed on the carrier substrate so that the epitaxial layer faces the carrier substrate.

[0007] Then, the growth substrate is removed, and the epitaxial layer is cut to form micro LED units, each of which has an upper surface, a lower surface and an inclined side surface, and the angle between the side surface of the micro LED unit and the lower surface of the micro LED unit is 50-60 degrees.

[0008] Then, the carrier substrate is placed in an ALD chamber, and a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas are sequentially circulated into the ALD chamber. Then, a reaction gas composed of a second zirconium source precursor and an organic sealing agent, a third cleaning gas, a second oxygen source gas, and a fourth cleaning gas are sequentially circulated into the ALD chamber to form a first zirconium oxide protective layer, so that the surface of the first zirconium oxide protective layer is a rough surface, and the first zirconium oxide protective layer covers the upper surface and the side surface of each of the micro LED units.

[0009] Then, the carrier substrate is transferred to a magnetron sputtering chamber, and a first metal layer is formed on the first zirconium oxide protective layer by a magnetron sputtering process.

[0010] Then, the carrier substrate is placed in the ALD chamber again, and a third zirconium source precursor, a fifth cleaning gas, a third oxygen source gas and a sixth cleaning gas are circulated into the ALD chamber in sequence to form a second zirconium oxide protective layer, so that the surface of the second zirconium oxide protective layer is a smooth surface, and the second zirconium oxide protective layer covers the first metal layer.

[0011] Then, a first electrode is formed on the upper surface of each of the micro LED units, wherein the first electrode is electrically connected to the epitaxial layer of each of the corresponding micro LED units.

[0012] A driving substrate is provided, and then a plurality of the micro LED units are transferred to the driving substrate.

[0013] As a preferred technical solution, the growth substrate is a sapphire substrate or a gallium nitride substrate, and the epitaxial layer includes a first semiconductor layer, a light-emitting quantum well layer and a second semiconductor layer.

[0014] As a preferred technical solution, the angle between the side surface of the micro LED unit and the lower surface of the micro LED unit is 53-58 degrees.

[0015] As a preferred technical solution, the roughness of the rough surface of the first zirconium oxide protective layer is 0.4-0.8 microns.

[0016] As a preferred technical solution, the first zirconium source precursor, the second zirconium source precursor and the third zirconium source precursor are one of zirconium tetra-tert-butoxide, zirconium chloride and zirconium iodide.

[0017] As a preferred technical solution, the organic sealing agent is one of methoxytrimethylsilane, trimethylchlorosilane and monochlorosilane.

[0018] As a preferred technical solution, the first oxygen source gas, the second oxygen source gas and the third oxygen source gas are one of water vapor, oxygen, ozone and hydrogen peroxide.

[0019] As a preferred technical solution, the thickness of the first zirconia protective layer is greater than the thickness of the second zirconia protective layer, and the thickness of the second zirconia protective layer is greater than the thickness of the first metal layer.

[0020] As a preferred technical solution, the roughness of the smooth surface of the second zirconium oxide protective layer is less than 50 nanometers.

[0021] The present invention also provides a micro LED light-emitting display device, which is manufactured using the above-mentioned method for manufacturing the micro LED light-emitting display device.

[0022] The beneficial effects of the present invention are:

[0023] In existing micro-LED light-emitting display devices, materials such as aluminum oxide and silicon nitride are usually used as protective layers of micro-LED units. In the preparation method of the micro-LED light-emitting display device of the present invention, zirconium oxide is used as the protective layer of the micro-LED unit. Due to the high density of zirconium oxide, the micro-LED unit can be more effectively protected. In the present application, each of the micro-LED units is provided with an upper surface, a lower surface and an inclined side surface, and the angle between the side surface of the micro-LED unit and the lower surface of the micro-LED unit is 50-60 degrees. By optimizing the angle between the side surface of the micro-LED unit and the lower surface of the micro-LED unit, the preparation of the zirconium oxide protective layer and the first metal layer is facilitated, and the reflective performance of the side of the micro-LED unit is effectively improved, thereby improving the light output efficiency of the micro-LED unit. In the present application, a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas are sequentially circulated into the ALD chamber, and then a reaction gas composed of a second zirconium source precursor and an organic sealing agent, a third cleaning gas, a second oxygen source gas, and a fourth cleaning gas are sequentially circulated into the ALD chamber to form a first zirconium oxide protective layer, so that the surface of the first zirconium oxide protective layer is a rough surface, and the roughness of the rough surface of the first zirconium oxide protective layer is 0.4-0.8 microns. The above process can directly form a surface with an uneven surface. The rough structure of the first zirconium oxide protective layer can effectively improve the bonding performance of the two when the first metal layer is subsequently formed, and due to the existence of the uneven rough structure, the interface area between the first metal layer and the first zirconium oxide protective layer is greatly increased, and when the micro LED unit emits light, the light irradiated to the interface can be reflected multiple times and then emitted from the light emitting surface of the micro LED unit, thereby greatly improving the light emitting efficiency of the micro LED unit; and the setting of the second zirconium oxide protective layer can effectively protect the first metal layer, thereby avoiding damage to the metal layer during the transfer of the micro LED unit. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic diagram showing the structure of disposing a light-emitting wafer on a carrier substrate in an embodiment of the present invention.

[0025] Figure 2 It is a schematic diagram showing the structure of forming a micro LED unit in an embodiment of the present invention.

[0026] Figure 3 It is a schematic diagram showing the structure of forming a first zirconium oxide protective layer in an embodiment of the present invention.

[0027] Figure 4 It is a schematic diagram showing the structure of forming a first metal layer and a second zirconium oxide protective layer in an embodiment of the present invention.

[0028] Figure 5 It is a schematic diagram showing the structure of forming a first electrode in an embodiment of the present invention.

[0029] Figure 6 It is a schematic diagram showing the structure of transferring a plurality of micro LED units to a driving substrate in an embodiment of the present invention. DETAILED DESCRIPTION

[0030] In order to facilitate the understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are given in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thoroughly and comprehensively understood.

[0031] like Figure 1 to Figure 6 As shown, this embodiment provides a method for preparing a micro LED light-emitting display device, and the method for preparing the micro LED light-emitting display device includes the following steps:

[0032] like Figure 1 As shown, a light-emitting wafer is provided. The light-emitting wafer includes a growth substrate 100 and an epitaxial layer located on the growth substrate 100 .

[0033] In a specific embodiment, the growth substrate 100 is a sapphire substrate or a gallium nitride substrate, and the epitaxial layer includes a first semiconductor layer 101 , a light-emitting quantum well layer 102 , and a second semiconductor layer 103 .

[0034] In a specific embodiment, the first semiconductor layer 101, the light-emitting quantum well layer 102 and the second semiconductor layer 103 are formed by an MOCVD process, wherein the first semiconductor layer 101 and the second semiconductor layer 103 are gallium nitride layers with different doping types, specifically, the first semiconductor layer 101 is a silicon-doped n-type gallium nitride layer or a magnesium-doped p-type gallium nitride layer, and correspondingly, the second semiconductor layer 103 is a magnesium-doped p-type gallium nitride layer or a silicon-doped n-type gallium nitride layer; the quantum well layer 102 can be an InGaN quantum well layer and a GaN quantum barrier layer grown alternately.

[0035] like Figure 1 As shown, a carrier substrate 200 is provided, and the light-emitting wafer is disposed on the carrier substrate so that the epitaxial layer faces the carrier substrate 200 .

[0036] In a specific embodiment, the second semiconductor layer 103 of the epitaxial layer faces the carrier substrate 200 .

[0037] like Figure 2As shown, the growth substrate 100 is then removed, and the epitaxial layer is cut to form micro LED units 201, each of which has an upper surface, a lower surface and an inclined side surface, and the angle between the side surface of the micro LED unit 201 and the lower surface of the micro LED unit 201 is 50-60 degrees.

[0038] In a specific embodiment, the epitaxial layer is cut by a laser cutting process to form a micro LED unit 201. In a more preferred embodiment, the angle between the side surface of the micro LED unit 201 and the lower surface of the micro LED unit 201 is 53-58 degrees. By optimizing and adjusting the specific angle of the angle, it is convenient to attach the zirconium oxide protective layer and the metal layer in the subsequent process. The setting of this angle is more convenient for reflecting the light emitted by the micro LED unit, thereby greatly improving the light output efficiency of the micro LED unit.

[0039] like Figure 3 As shown, the carrier substrate 200 is then placed in an ALD chamber, and a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas are sequentially circulated into the ALD chamber, and then a reaction gas composed of a second zirconium source precursor and an organic sealant, a third cleaning gas, a second oxygen source gas, and a fourth cleaning gas are sequentially circulated into the ALD chamber to form a first zirconium oxide protective layer 301, so that the surface of the first zirconium oxide protective layer 301 is a rough surface, and the first zirconium oxide protective layer 301 covers the upper surface and the side surface of each of the micro LED units 201.

[0040] In a specific embodiment, the roughness of the rough surface of the first zirconium oxide protective layer 301 is 0.4-0.8 microns.

[0041] In a specific embodiment, the first zirconium source precursor and the second zirconium source precursor are one of zirconium tetra-tert-butoxide, zirconium chloride, and zirconium iodide.

[0042] In a specific embodiment, the organic blocking agent is one of methoxytrimethylsilane, trimethylchlorosilane and monochlorosilane.

[0043] In a specific embodiment, the first oxygen source gas and the second oxygen source gas are one of water vapor, oxygen, ozone and hydrogen peroxide.

[0044] In a specific embodiment, the temperature of the ALD chamber is maintained at 250-400°C, and the gas pressure of the ALD chamber is set to 0.5-5 torr. More specifically, the temperature of the ALD chamber can be set to 250°C, 280°C, 320°C, 350°C or 400°C, and the gas pressure of the ALD chamber can be set to 0.5 torr, 1 torr, 1.5 torr, 2 torr, 2.5 torr, 3 torr, 3.5torr, 4 torr, 4.5 torr or 5 torr.

[0045] In a specific embodiment, in the process of cyclically introducing a first zirconium source precursor, a first cleaning gas, a first oxygen source gas and a second cleaning gas into the ALD chamber in sequence, the flow rate of the first zirconium source precursor is 20-60 sccm, the time for each introduction of the first zirconium source precursor is 2-6 seconds, and before the introduction of the first cleaning gas and after the introduction of the first zirconium source precursor is stopped, it is maintained for 0.5-4 seconds, and then the first cleaning gas is introduced, the flow rate of the first cleaning gas is 800-5000 sccm, and the time for introducing the first cleaning gas is 10-20 seconds, then the first oxygen source gas is introduced, the flow rate of the first oxygen source gas is 20-60 sccm, the time for each introduction of the first oxygen source gas is 2-6 seconds, and before the introduction of the second cleaning gas and after the introduction of the first oxygen source gas is stopped, it is maintained for 0.5-4 seconds, and then the second cleaning gas is introduced, the flow rate of the second cleaning gas is 800-5000 sccm, and the time for introducing the second cleaning gas is 10-20 seconds.

[0046] Then, in the process of sequentially circulating the reaction gas composed of the second zirconium source precursor and the organic sealing agent, the third cleaning gas, the second oxygen source gas and the fourth cleaning gas into the ALD chamber, the flow rate of the reaction gas composed of the second zirconium source precursor and the organic sealing agent is 50-150 sccm, and the time for each introduction of the reaction gas composed of the second zirconium source precursor and the organic sealing agent is 3-7 seconds, wherein the flow rate of the organic sealing agent accounts for 6-15% of the reaction gas composed of the second zirconium source precursor and the organic sealing agent, and it is ensured that the flow rate of the second zirconium source precursor is greater than the flow rate of the first zirconium source precursor, and before the introduction of the third cleaning gas and after the introduction of the reaction gas composed of the second zirconium source precursor and the organic sealing agent is stopped, it is maintained for 0.5-4 seconds, and then the third cleaning gas is introduced, and the flow rate of the third cleaning gas is 2000-8000. sccm, the time for introducing the third cleaning gas is 10-20 seconds, and then the second oxygen source gas is introduced, the flow rate of the second oxygen source gas is 50-100sccm, the time for each introduction of the second oxygen source gas is 3-7 seconds, and before the fourth cleaning gas is introduced and after the second oxygen source gas is stopped, it is kept for 0.5-4 seconds, and then the fourth cleaning gas is introduced, the flow rate of the fourth cleaning gas is 2000-8000 sccm, and the time for introducing the fourth cleaning gas is 10-20 seconds, so as to form a first zirconia protective layer 301, and the thickness of the first zirconia protective layer 301 is 2-5 microns by cycling a suitable number of times, and the roughness of the rough surface of the first zirconia protective layer 301 is 0.4-0.8 microns by adjusting various process parameters, and more preferably, the roughness is 0.5-0.6 microns.

[0047] In a specific embodiment, the temperature of the ALD chamber is maintained at 320° C., and the gas pressure of the ALD chamber is set to 2 torr. In the process of cyclically introducing a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas into the ALD chamber in sequence, the first zirconium source precursor is zirconium chloride, and the flow rate of the first zirconium source precursor is 35 sccm. The time for each introduction of the first zirconium source precursor is 5 seconds, and before the introduction of the first cleaning gas and after the introduction of the first zirconium source precursor is stopped, it is maintained for 2 seconds, and then the first cleaning gas is introduced. The first cleaning gas is nitrogen, and the flow rate of the first cleaning gas is 3000 sccm. The time for introducing the first cleaning gas is 15 seconds, and then the first oxygen source gas is introduced, and the flow rate of the first oxygen source gas is 35 sccm, each time the first oxygen source gas is introduced, the first oxygen source gas is water vapor, the first oxygen source gas is introduced for 4 seconds, and before the second cleaning gas is introduced and after the first oxygen source gas is stopped, it is kept for 2 seconds, and then the second cleaning gas is introduced, the second cleaning gas is nitrogen, and the flow rate of the second cleaning gas is 3000 sccm, the time for introducing the second cleaning gas is 15 seconds; then the temperature of the ALD chamber is maintained at 320° C., and the gas pressure of the ALD chamber is set to 2 torr. In the process of cyclically introducing a reaction gas composed of a second zirconium source precursor and an organic sealing agent, a third cleaning gas, a second oxygen source gas and a fourth cleaning gas into the ALD chamber in sequence, the flow rate of the reaction gas composed of the second zirconium source precursor and the organic sealing agent is 100 sccm, and the time for each introduction of the reaction gas composed of the second zirconium source precursor and the organic sealing agent is 6 seconds, wherein the second zirconium source precursor is zirconium chloride, and the organic sealing agent is methoxytrimethylsilane, and the flow rate of the organic sealing agent accounts for 10% of the reaction gas composed of the second zirconium source precursor and the organic sealing agent, and before the introduction of the third cleaning gas and after the introduction of the reaction gas composed of the second zirconium source precursor and the organic sealing agent is stopped, it is maintained for 2 seconds, and then the third cleaning gas is introduced, and the flow rate of the third cleaning gas is 6000 sccm, the time for introducing the third cleaning gas is 15 seconds, and then the second oxygen source gas is introduced, the second oxygen source gas is water vapor, the flow rate of the second oxygen source gas is 90sccm, the time for each introduction of the second oxygen source gas is 6 seconds, and before the fourth cleaning gas is introduced and after the second oxygen source gas is stopped, it is kept for 2 seconds, and then the fourth cleaning gas is introduced, the fourth cleaning gas is nitrogen, the flow rate of the fourth cleaning gas is 6000 sccm, and the time for introducing the fourth cleaning gas is 15 seconds to form a first zirconia protective layer 301, and by cycling a suitable number of times, the thickness of the first zirconia protective layer 301 is 3 microns, and the roughness of the rough surface of the first zirconia protective layer 301 is 0.5-0.6 microns.

[0048] like Figure 4As shown, the carrier substrate 200 is then transferred to a magnetron sputtering chamber, and a first metal layer 302 is formed on the first zirconium oxide protective layer 301 by a magnetron sputtering process.

[0049] In a specific embodiment, the material of the first metal layer 302 is copper or aluminum, and the thickness of the first metal layer 302 is 100-500 nanometers. Since the thickness of the first metal layer 302 is much smaller than the thickness of the first zirconia protective layer 301, the first metal layer 302 is conformally formed on the rough surface of the first zirconia protective layer 301, thereby greatly increasing the interface area between the first metal layer 302 and the first zirconia protective layer 301, thereby greatly increasing the reflection effect of light, and by using an organic sealant in the process of depositing the first zirconia protective layer 301, there is no need for an etching process, and the first zirconia protective layer 301 with a rough surface structure can be directly formed.

[0050] like Figure 4 As shown, the carrier substrate 200 is then placed in the ALD chamber again, and a third zirconium source precursor, a fifth cleaning gas, a third oxygen source gas and a sixth cleaning gas are sequentially circulated into the ALD chamber to form a second zirconium oxide protective layer 303, so that the surface of the second zirconium oxide protective layer 303 is a smooth surface, and the second zirconium oxide protective layer 303 covers the first metal layer.

[0051] In a specific embodiment, the third zirconium source precursor is one of zirconium tetra-tert-butoxide, zirconium chloride, and zirconium iodide.

[0052] In a specific embodiment, the third oxygen source gas is one of water vapor, oxygen, ozone and hydrogen peroxide.

[0053] In a specific embodiment, the roughness of the smooth surface of the second zirconium oxide protective layer 303 is less than 50 nanometers.

[0054] In a specific embodiment, the thickness of the first zirconia protective layer 301 is greater than the thickness of the second zirconia protective layer 303 , and the thickness of the second zirconia protective layer 303 is greater than the thickness of the first metal layer 302 .

[0055] In a specific embodiment, the temperature of the ALD chamber is maintained at 250-400°C, and the gas pressure of the ALD chamber is set to 0.5-5 torr. More specifically, the temperature of the ALD chamber can be set to 250°C, 280°C, 320°C, 350°C or 400°C, and the gas pressure of the ALD chamber can be set to 0.5 torr, 1 torr, 1.5 torr, 2 torr, 2.5 torr, 3 torr, 3.5torr, 4 torr, 4.5 torr or 5 torr.

[0056] In a specific embodiment, in the process of cyclically introducing a third zirconium source precursor, a fifth cleaning gas, a third oxygen source gas and a sixth cleaning gas into the ALD chamber in sequence, the flow rate of the third zirconium source precursor is 20-60 sccm, the time for each introduction of the third zirconium source precursor is 2-6 seconds, and before the introduction of the fifth cleaning gas and after the third zirconium source precursor is stopped, it is maintained for 0.5-4 seconds, and then the fifth cleaning gas is introduced, the flow rate of the fifth cleaning gas is 800-5000 sccm, and the time for the fifth cleaning gas is 10-20 seconds, then the third oxygen source gas is introduced, the flow rate of the third oxygen source gas is 20-60 sccm, the time for each introduction of the third oxygen source gas is 2-6 seconds, and before the introduction of the sixth cleaning gas and after the third oxygen source gas is stopped, it is maintained for 0.5-4 seconds, and then the sixth cleaning gas is introduced, and the flow rate of the sixth cleaning gas is 800-5000 sccm. sccm, the time for introducing the second cleaning gas is 10-20 seconds, and the thickness of the second zirconia protective layer 303 is made to be 0.8-2 microns by circulating an appropriate number of times, and the roughness of the smooth surface of the second zirconia protective layer 303 is made to be less than 50 nanometers by adjusting various process parameters.

[0057] In a specific embodiment, the temperature of the ALD chamber is maintained at 320° C., and the gas pressure of the ALD chamber is set to 2 torr. In the process of cyclically introducing a third zirconium source precursor, a fifth cleaning gas, a third oxygen source gas, and a sixth cleaning gas into the ALD chamber in sequence, the third zirconium source precursor is zirconium chloride, and the flow rate of the third zirconium source precursor is 35 sccm. The time for each introduction of the third zirconium source precursor is 5 seconds, and before the introduction of the fifth cleaning gas and after the introduction of the third zirconium source precursor is stopped, it is maintained for 2 seconds, and then the fifth cleaning gas is introduced. The fifth cleaning gas is nitrogen, and the flow rate of the fifth cleaning gas is 3000 sccm. The time for introducing the fifth cleaning gas is 15 seconds, and then the third oxygen source gas is introduced, and the flow rate of the third oxygen source gas is 35 sccm, each time a third oxygen source gas is introduced, the third oxygen source gas is water vapor, the time for introducing the third oxygen source gas is 4 seconds, and before the sixth cleaning gas is introduced and after the third oxygen source gas is stopped, it is kept for 2 seconds, and then the sixth cleaning gas is introduced, the sixth cleaning gas is nitrogen, the flow rate of the sixth cleaning gas is 3000 sccm, and the time for introducing the sixth cleaning gas is 15 seconds, so as to form a second zirconia protective layer 303, by cycling a suitable number of times, the thickness of the second zirconia protective layer 303 is 1.5 microns, and the roughness of the smooth surface of the second zirconia protective layer 303 is less than 50 nanometers.

[0058] like Figure 5 As shown, a first electrode 401 is then formed on the upper surface of each of the micro LED units 201 , and the first electrode 401 is electrically connected to the epitaxial layer of each of the corresponding micro LED units 201 .

[0059] In a specific embodiment, a mask is used to form a through hole exposing the epitaxial layer of each micro LED unit 201, and then metal copper is formed as the first electrode 401 through a PVD process, and the through hole is passivated (not shown) to electrically insulate the first electrode 401 from the first metal layer 302.

[0060] like Figure 6 As shown, a driving substrate 500 is provided, and then the plurality of micro LED units 201 are transferred to the driving substrate 500 .

[0061] In a specific embodiment, a plurality of the micro LED units 201 are transferred to the driving substrate 500 by using a transfer device, so that each of the first electrodes 401 is electrically connected to a pixel circuit of the driving substrate 500 .

[0062] In a specific embodiment, a packaging layer 600 is formed to package the plurality of micro LED units 201 , and then a common electrode 700 is formed on the packaging layer. The common electrode 700 is electrically connected to the plurality of micro LED units 201 .

[0063] like Figure 6 As shown, the present invention also provides a micro LED light-emitting display device, which is manufactured using the above-mentioned method for preparing the micro LED light-emitting display device.

[0064] In other preferred technical solutions, the present invention provides a method for preparing a micro LED light-emitting display device, and the method for preparing the micro LED light-emitting display device comprises the following steps:

[0065] A light-emitting wafer is provided. The light-emitting wafer includes a growth substrate and an epitaxial layer located on the growth substrate.

[0066] A carrier substrate is provided, and the light-emitting wafer is disposed on the carrier substrate so that the epitaxial layer faces the carrier substrate.

[0067] Then, the growth substrate is removed, and the epitaxial layer is cut to form micro LED units, each of which has an upper surface, a lower surface and an inclined side surface, and the angle between the side surface of the micro LED unit and the lower surface of the micro LED unit is 50-60 degrees.

[0068] Then, the carrier substrate is placed in an ALD chamber, and a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas are sequentially circulated into the ALD chamber. Then, a reaction gas composed of a second zirconium source precursor and an organic sealing agent, a third cleaning gas, a second oxygen source gas, and a fourth cleaning gas are sequentially circulated into the ALD chamber to form a first zirconium oxide protective layer, so that the surface of the first zirconium oxide protective layer is a rough surface, and the first zirconium oxide protective layer covers the upper surface and the side surface of each of the micro LED units.

[0069] Then, the carrier substrate is transferred to a magnetron sputtering chamber, and a first metal layer is formed on the first zirconium oxide protective layer by a magnetron sputtering process.

[0070] Then, the carrier substrate is placed in the ALD chamber again, and a third zirconium source precursor, a fifth cleaning gas, a third oxygen source gas and a sixth cleaning gas are circulated into the ALD chamber in sequence to form a second zirconium oxide protective layer, so that the surface of the second zirconium oxide protective layer is a smooth surface, and the second zirconium oxide protective layer covers the first metal layer.

[0071] Then, a first electrode is formed on the upper surface of each of the micro LED units, wherein the first electrode is electrically connected to the epitaxial layer of each of the corresponding micro LED units.

[0072] A driving substrate is provided, and then a plurality of the micro LED units are transferred to the driving substrate.

[0073] In a more preferred technical solution, the growth substrate is a sapphire substrate or a gallium nitride substrate, and the epitaxial layer includes a first semiconductor layer, a light-emitting quantum well layer and a second semiconductor layer.

[0074] In a more preferred technical solution, the angle between the side surface of the micro LED unit and the lower surface of the micro LED unit is 53-58 degrees.

[0075] In a more preferred technical solution, the roughness of the rough surface of the first zirconium oxide protective layer is 0.4-0.8 microns.

[0076] In a more preferred technical solution, the first zirconium source precursor, the second zirconium source precursor and the third zirconium source precursor are one of zirconium tetra-tert-butoxide, zirconium chloride and zirconium iodide.

[0077] In a more preferred technical solution, the organic sealing agent is one of methoxytrimethylsilane, trimethylchlorosilane and monochlorosilane.

[0078] In a more preferred technical solution, the first oxygen source gas, the second oxygen source gas and the third oxygen source gas are one of water vapor, oxygen, ozone and hydrogen peroxide.

[0079] In a more preferred technical solution, the thickness of the first zirconia protective layer is greater than the thickness of the second zirconia protective layer, and the thickness of the second zirconia protective layer is greater than the thickness of the first metal layer.

[0080] In a more preferred technical solution, the roughness of the smooth surface of the second zirconium oxide protective layer is less than 50 nanometers.

[0081] In a more optimal technical solution, the present invention further proposes a micro LED light-emitting display device, which is manufactured using the above-mentioned method for preparing the micro LED light-emitting display device.

[0082] In existing micro-LED light-emitting display devices, materials such as aluminum oxide and silicon nitride are usually used as protective layers of micro-LED units. In the preparation method of the micro-LED light-emitting display device of the present invention, zirconium oxide is used as the protective layer of the micro-LED unit. Due to the high density of zirconium oxide, the micro-LED unit can be more effectively protected. In the present application, each of the micro-LED units is provided with an upper surface, a lower surface and an inclined side surface, and the angle between the side surface of the micro-LED unit and the lower surface of the micro-LED unit is 50-60 degrees. By optimizing the angle between the side surface of the micro-LED unit and the lower surface of the micro-LED unit, the preparation of the zirconium oxide protective layer and the first metal layer is facilitated, and the reflective performance of the side of the micro-LED unit is effectively improved, thereby improving the light output efficiency of the micro-LED unit. In the present application, a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas are sequentially circulated into the ALD chamber, and then a reaction gas composed of a second zirconium source precursor and an organic sealing agent, a third cleaning gas, a second oxygen source gas, and a fourth cleaning gas are sequentially circulated into the ALD chamber to form a first zirconium oxide protective layer, so that the surface of the first zirconium oxide protective layer is a rough surface, and the roughness of the rough surface of the first zirconium oxide protective layer is 0.4-0.8 microns. The above process can directly form a surface with an uneven surface. The rough structure of the first zirconium oxide protective layer can effectively improve the bonding performance of the two when the first metal layer is subsequently formed, and due to the existence of the uneven rough structure, the interface area between the first metal layer and the first zirconium oxide protective layer is greatly increased, and when the micro LED unit emits light, the light irradiated to the interface can be reflected multiple times and then emitted from the light emitting surface of the micro LED unit, thereby greatly improving the light emitting efficiency of the micro LED unit; and the setting of the second zirconium oxide protective layer can effectively protect the first metal layer, thereby avoiding damage to the metal layer during the transfer of the micro LED unit.

[0083] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for preparing a micro LED light-emitting display device, characterized in that: The method for preparing the micro LED light-emitting display device comprises the following steps: Providing a light-emitting wafer, the light-emitting wafer comprising a growth substrate and an epitaxial layer located on the growth substrate; Providing a carrier substrate, and disposing the light-emitting wafer on the carrier substrate so that the epitaxial layer faces the carrier substrate; Then, the growth substrate is removed, and the epitaxial layer is cut to form micro LED units, each of which has an upper surface, a lower surface, and an inclined side surface, and the angle between the side surface of the micro LED unit and the lower surface of the micro LED unit is 50-60 degrees; Then, the carrier substrate is placed in an ALD chamber, a first zirconium source precursor, a first cleaning gas, a first oxygen source gas, and a second cleaning gas are sequentially introduced into the ALD chamber in a cycle, and then a reaction gas consisting of a second zirconium source precursor and an organic sealing agent, a third cleaning gas, a second oxygen source gas, and a fourth cleaning gas are sequentially introduced into the ALD chamber in a cycle to form a first zirconium oxide protective layer, so that the surface of the first zirconium oxide protective layer is a rough surface, and the first zirconium oxide protective layer covers the upper surface and the side surface of each of the micro LED units; Then, the carrier substrate is transferred to a magnetron sputtering chamber, and a first metal layer is formed on the first zirconium oxide protective layer by a magnetron sputtering process; Then, the carrier substrate is placed in the ALD chamber again, and a third zirconium source precursor, a fifth cleaning gas, a third oxygen source gas, and a sixth cleaning gas are sequentially introduced into the ALD chamber in a circular manner to form a second zirconium oxide protective layer, so that the surface of the second zirconium oxide protective layer is a smooth surface, and the second zirconium oxide protective layer covers the first metal layer; Then, forming a first electrode on the upper surface of each micro LED unit, wherein the first electrode is electrically connected to the epitaxial layer of each corresponding micro LED unit; A driving substrate is provided, and then a plurality of the micro LED units are transferred to the driving substrate.

2. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: The growth substrate is a sapphire substrate or a gallium nitride substrate, and the epitaxial layer includes a first semiconductor layer, a light-emitting quantum well layer and a second semiconductor layer.

3. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: An included angle between the side surface of the micro LED unit and the lower surface of the micro LED unit is 53-58 degrees.

4. The method for preparing a micro LED light-emitting display device according to claim 3, characterized in that: The roughness of the rough surface of the first zirconium oxide protective layer is 0.4-0.8 microns.

5. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: The first zirconium source precursor, the second zirconium source precursor and the third zirconium source precursor are one of zirconium tetra-tert-butoxide, zirconium chloride and zirconium iodide.

6. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: The organic sealing agent is one of methoxytrimethylsilane, trimethylchlorosilane and monochlorosilane.

7. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: The first oxygen source gas, the second oxygen source gas, and the third oxygen source gas are one of water vapor, oxygen, ozone, and hydrogen peroxide.

8. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: The thickness of the first zirconia protective layer is greater than the thickness of the second zirconia protective layer, and the thickness of the second zirconia protective layer is greater than the thickness of the first metal layer.

9. The method for preparing a micro LED light-emitting display device according to claim 1, characterized in that: The roughness of the smooth surface of the second zirconium oxide protective layer is less than 50 nanometers.

10. A micro LED light-emitting display device, characterized in that: The micro LED light-emitting display device is manufactured using the preparation method of any one of claims 1 to 9.

Citation Information

Patent Citations

  • Semiconductor light emitting device

    CN102881811A

  • Micro-LED display device and manufacturing method thereof

    CN115312637A

  • Flip chip optical semiconductor element

    JP2004080050A

  • Optical semiconductor device, and composition for forming optical semiconductor device protective layer

    JP2011146674A

  • Method of manufacturing light emitting element

    US20150364643A1