High-ink-absorption synthetic paper and preparation method thereof

By adopting a three-layer composite structure, the combination of cellulose/SiO2 micro-nanospheres and PVC is used to solve the problems of complex and high cost in the existing synthetic paper production process, achieving efficient ink absorption and reducing filler use improves productivity and cost-effectiveness.

CN118895690AActive Publication Date: 2024-11-05SUZHOU HUIERSI ELECTRONIC NEW MATERIAL TECH CO LTD
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
CN202411136503.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-05
Estimated Expiration
2044-08-19

AI Technical Summary

Technical Problem

The existing synthetic paper production process is complex and costly, which restricts the widespread application of products, especially the two-way stretching process, which leads to expensive equipment and increases production costs.

Method used

High-inspired synthetic paper with three-layer composite structure, including PVC/cellulose/SiO2 composite layer, porous cellulose electrospinning layer and PVC layer. The ink absorption effect is improved through the cooperation of cellulose/SiO2 micro-nanospheres and PVC. , reduce the amount of filler used.

Benefits of technology

It achieves efficient ink absorption effect, while reducing the use of filler, improving production efficiency and cost-effectiveness, and is suitable for a wide range of applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides high-ink-absorption synthetic paper which is of a three-layer composite structure and comprises a PVC / cellulose / SiO2 composite layer, a porous cellulose electrostatic spinning layer and a PVC layer, the PVC / cellulose / SiO2 composite layer is composed of cellulose / SiO2 micro-nanospheres and PVC, and the mass ratio of the cellulose / SiO2 micro-nanospheres to the PVC is (1-2): 10. The composite synthetic paper is prepared by adopting wet phase inversion and inorganic / organic filling modification technologies, and cellulose / SiO2 micro-nano and the cellulose electrostatic spinning layer are added into PVC, so that the adsorption effect of the synthetic paper on ink can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of papermaking, and in particular to a highly ink-absorbent synthetic paper and a preparation method thereof. Background Art

[0002] Synthetic paper, also known as plastic paper, chemical film paper, and stone paper, is a multifunctional material with the characteristics of plastic and paper made of calcium carbonate and polymer materials as the main raw materials, various additives are added, and the polymer interface chemistry principle and filling modification technology are used. Through special processing technology, it is made. Synthetic paper has fundamentally changed the traditional papermaking process and can completely solve the environmental damage and water pollution problems caused by traditional papermaking. The emergence of synthetic paper has its fundamental reasons, which is the inevitable result of social development. First, the rapid economic development has sharply increased the demand for paper, resulting in soaring pulp prices, reducing people's purchasing power, and prompting people to look for substitutes for traditional fiber paper; secondly, the characteristics of ordinary paper cannot meet special requirements, such as water resistance, oil resistance, acid and alkali resistance, etc., and synthetic paper can make up for these defects to a certain extent; finally, the plant fibers such as wood used as papermaking raw materials are decreasing day by day, and the papermaking production process is extremely damaging to the environment. The emergence of synthetic paper, especially the emergence of highly filled synthetic paper-stone paper, can slow down the consumption of the earth's vegetation and the damage to the environment by the paper industry. Therefore, the emergence of synthetic paper meets the current requirements of economic development, environmental protection and low carbon. Although there is a lot of room for the development of synthetic paper in China, the production process mostly uses biaxial stretching. This process is not only complex in formula and technology, but also very expensive in equipment. The cost of producing synthetic paper will increase accordingly, and the sales price will also increase accordingly, which seriously restricts the wide application of the product. Summary of the invention

[0003] Technical problem to be solved: The purpose of the present invention is to provide a highly ink-absorbing synthetic paper, which has a three-layer composite structure and can achieve a good ink-absorbing effect through the coordination between the layers.

[0004] Technical solution: A highly ink-absorbent synthetic paper, which has a three-layer composite structure, including a PVC / cellulose / SiO2 composite layer, a porous cellulose electrospinning layer and a PVC layer. The PVC / cellulose / calcium carbonate composite layer is composed of cellulose / SiO2 micro-nano balls and PVC, wherein the mass ratio of cellulose / SiO2 micro-nano balls to PVC is 1-2:10. Preferably, the method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 60-80°C, stirring and dissolving to obtain a cellulose solution having a concentration of 1.5-3wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1 to obtain a cellulose / calcium carbonate composite solution; S13. electrospinning the cellulose / calcium carbonate composite solution to obtain a cellulose electrospinning membrane; S14. Add the fiber bundle electrospun membrane into a dilute acid solution, soak to remove calcium carbonate, wash and dry to obtain a porous electrospun membrane. Preferably, in step S12, the content of nano-calcium carbonate in the cellulose solution is 2-4 wt %. Preferably, in step S13, the electrospinning distance is 12-18 cm, the flow rate is 0.05-0.1 mL / min, and the voltage is 15-18 kV. Preferably, the preparation method of cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.2-3wt%; S22. Add nanoporous SiO2 particles to the cellulose solution prepared in step S21, stir and mix evenly to obtain a cellulose / SiO2 mixed solution; S23. The mixed solution prepared in step S23 is sprayed with high-voltage electrostatic spray to prepare cellulose / SiO2 micro-nanospheres. Preferably, in step S22, the content of the nano-SiO2 particles in the mixed solution is 5-30wt%. Preferably, in the step S23, the inner diameter of the needle used in the high-voltage electrostatic spray is 1.2-1.5 mm, the spray distance is 12-18 cm, the flow rate is 0.01-0.03 mL / min, and the voltage is 12-15 kV. The method for preparing the above-mentioned highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, and obtain a PVC synthetic pulp; S3. pouring the remaining PVC pulp prepared in step S1 into a mold, evaporating the solvent to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper. Beneficial effects: The high ink absorption of the present invention has the following advantages: The present invention adopts wet phase transfer and inorganic / organic filling modification technology to prepare composite synthetic paper. Adding cellulose / SiO2 micro-nano to PVC can improve the adsorption effect of synthetic paper on ink. At the same time, a cellulose electrospinning layer is added to two layers of PVC. The cellulose / SiO2 micro-nano has a loose and porous structure. The pores formed by it in PVC are equivalent to capillaries, and the electrospinning layer also has a loose and porous structure. Under the action of the capillaries and the electrospinning layer, it can quickly absorb ink. In the present invention, the amount of cellulose / SiO2 micro-nano added is much lower than the current content of 40-60% of fillers that needs to be added, and a good ink absorption effect can also be achieved. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 60°C, stirring and dissolving to obtain a cellulose solution having a concentration of 1.5 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 4 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 12 cm, a flow rate of 0.1 mL / min, and a voltage of 15 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.2 wt %; S22. Nanoporous SiO2 particles are added to the cellulose solution prepared in step S21, and stirred to mix evenly to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution is 5wt%; S23. The mixed solution prepared in step S23 is used for preparing cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.2 mm, the spraying distance is 12 cm, the flow rate is 0.01 mL / min, and the voltage is 12 kV. Example 2 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1:5, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 80°C, stirring and dissolving to obtain a cellulose solution having a concentration of 3 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 2 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 18 cm, a flow rate of 0.05 mL / min, and a voltage of 18 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 3 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 30wt%; S23. The mixed solution prepared in step S23 is used for preparing cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.5 mm, the spraying distance is 18 cm, the flow rate is 0.03 mL / min, and the voltage is 15 kV. Example 3 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1.2:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 65°C, stirring and dissolving to obtain a cellulose solution having a concentration of 1.8 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 2.5wt%, to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 14 cm, a flow rate of 0.05 mL / min, and a voltage of 15 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.4 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 15wt%; S23. The mixed solution prepared in step S23 is used to prepare cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.2 mm, the spraying distance is 16 cm, the flow rate is 0.01 mL / min, and the voltage is 12 kV. Example 4 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1.6:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 75°C, stirring and dissolving to obtain a cellulose solution having a concentration of 2.5 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 3.5wt%, to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 16 cm, a flow rate of 0.1 mL / min, and a voltage of 18 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.8 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 25wt%; S23. The mixed solution prepared in step S23 is used to prepare cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.5 mm, the spraying distance is 16 cm, the flow rate is 0.03 mL / min, and the voltage is 15 kV. Example 5 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1.5:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 70°C, stirring and dissolving to obtain a cellulose solution with a concentration of 2.2 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 3 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 15 cm, a flow rate of 0.08 mL / min, and a voltage of 16 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.6 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 20wt%; S23. The mixed solution prepared in step S23 is used to prepare cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.5 mm, the spraying distance is 16 cm, the flow rate is 0.02 mL / min, and the voltage is 14 kV. Comparative Example 1 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1.5:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. Pour PVC synthetic paper slurry on the surface of the PVC layer, evaporate the solvent, and obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.6 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 20wt%; S23. The mixed solution prepared in step S23 is used to prepare cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.5 mm, the spraying distance is 16 cm, the flow rate is 0.02 mL / min, and the voltage is 14 kV. Comparative Example 2 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. placing the porous cellulose electrospun layer in a mold, pouring the PVC pulp prepared in step S1 into the mold, evaporating the solvent, and obtaining a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 70°C, stirring and dissolving to obtain a cellulose solution with a concentration of 2.2 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 3 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 15 cm, a flow rate of 0.08 mL / min, and a voltage of 16 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; Comparative Example 3 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add calcium carbonate to the PVC pulp, stir evenly, the mass ratio of calcium carbonate to PVC is 4:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 70°C, stirring and dissolving to obtain a cellulose solution with a concentration of 2.2 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 3 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 15 cm, a flow rate of 0.08 mL / min, and a voltage of 16 kV to obtain a cellulose electrospinning membrane; S14. Add the fiber bundle electrospun membrane into a dilute acid solution, soak to remove calcium carbonate, wash and dry to obtain a porous electrospun membrane. Comparative Example 4 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of SiO2 micro-nanospheres to PVC is 2.5:10, and obtain PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 70°C, stirring and dissolving to obtain a cellulose solution with a concentration of 2.2 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 3 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 15 cm, a flow rate of 0.08 mL / min, and a voltage of 16 kV to obtain a cellulose electrospinning membrane; S14. Add the fiber bundle electrospun membrane into a dilute acid solution, soak to remove calcium carbonate, wash and dry to obtain a porous electrospun membrane. Comparative Example 5 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 1.5:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. Placing a multi-cellulose electrospinning membrane on the surface of the PVC layer, then pouring a PVC synthetic paper slurry, evaporating the solvent, and obtaining a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 70°C, stirring and dissolving to obtain a cellulose solution with a concentration of 2.2 wt%; S12. The cellulose solution was electrospun at an electrospinning distance of 15 cm, a flow rate of 0.08 mL / min, and a voltage of 16 kV to obtain a cellulose electrospinning membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.6 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 20wt%; S23. The mixed solution prepared in step S23 is used to prepare cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.5 mm, the spraying distance is 16 cm, the flow rate is 0.02 mL / min, and the voltage is 14 kV. Comparative Example 6 A method for preparing highly ink-absorbent synthetic paper comprises the following steps: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1, add the cellulose / SiO2 micro-nanospheres to the PVC pulp, stir evenly, the mass ratio of cellulose / SiO2 micro-nanospheres to PVC is 3:10, and obtain a PVC synthetic pulp; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper; The method for preparing the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 70°C, stirring and dissolving to obtain a cellulose solution with a concentration of 2.2 wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1, wherein the content of the nano-calcium carbonate in the cellulose solution is 3 wt % to obtain a cellulose / calcium carbonate composite solution; S13. The cellulose / calcium carbonate composite solution was electrospun at an electrospinning distance of 15 cm, a flow rate of 0.08 mL / min, and a voltage of 16 kV to obtain a cellulose electrospinning membrane; S14. adding the fiber bundle electrospun membrane to a dilute acid solution, soaking to remove calcium carbonate, washing and drying to obtain a porous electrospun membrane; The method for preparing the cellulose / SiO2 micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.6 wt %; S22. Nanoporous SiO2 particles were added to the cellulose solution prepared in step S21, and the mixture was stirred to obtain a cellulose / SiO2 mixed solution, wherein the content of nano-SiO2 particles in the mixed solution was 20wt%; S23. The mixed solution prepared in step S23 is used to prepare cellulose / SiO2 micro-nanospheres by high-voltage electrostatic spraying. The inner diameter of the needle used in the high-voltage electrostatic spraying is 1.5 mm, the spraying distance is 16 cm, the flow rate is 0.02 mL / min, and the voltage is 14 kV. Performance Test: Water absorption and ink absorption test: Cut the synthetic paper into 30mm*30mm size, dry it at 40℃ to constant weight, weigh it, record it as m0, and then soak it in water or carbon ink for 24 hours, then use filter paper to absorb the water / ink on the surface of the sample, weigh it, record it as m1. Calculate the water / ink absorption of the sample: water / ink absorption = (m1-m0) / m0*100%; Mechanical properties test: The synthetic paper is sampled using a mold (dumbbell type) and its thickness is measured. The mechanical properties of the synthetic paper are then measured using a universal testing machine at a test speed of 50 mm / min. Water absorption % Ink absorption rate% Tensile strength MPa Example 1 24.2 17.2 8.8 Example 2 28.6 20.6 8.6 Example 3 25.9 18.1 9.2 Example 4 26.8 18.5 8.5 Example 5 26.7 18.5 9.0 Comparative Example 1 15.6 11.2 6.7 Comparative Example 2 14.2 8.6 9.6 Comparative Example 3 18.9 15.2 8.6 Comparative Example 4 16.5 11.1 9.1 Comparative Example 5 21.6 16.0 9.5 Comparative Example 6 29.9 22.3 3.5 Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.

Claims

1. A highly ink-absorbent synthetic paper, Features: The synthetic paper is a three-layer composite structure, including PVC / cellulose / SiO 2 Composite layer, porous cellulose electrospinning layer and PVC layer, the PVC / cellulose / calcium carbonate composite layer is composed of cellulose / SiO 2 Micro-nanospheres and PVC, cellulose / SiO 2 The mass ratio of micro-nanospheres to PVC is 1-2:

10.

2. The highly ink-absorbent synthetic paper according to claim 1, Features: The preparation method of the cellulose electrospinning layer comprises the following steps: S11. Dissolving cellulose in a DMAc / LiCl mixed solvent, maintaining the reaction temperature of the solution at 60-80°C, stirring and dissolving to obtain a cellulose solution having a concentration of 1.5-3wt%; S12. The nano-calcium carbonate is added to DMAc, mixed and stirred, and then added to the cellulose solution prepared in step S1 to obtain a cellulose / calcium carbonate composite solution; S13. electrospinning the cellulose / calcium carbonate composite solution to obtain a cellulose electrospinning membrane; S14. Add the fiber bundle electrospun membrane into a dilute acid solution, soak to remove calcium carbonate, wash and dry to obtain a porous electrospun membrane.

3. The highly ink-absorbent synthetic paper according to claim 2, Features: In step S12, the content of nano calcium carbonate in the cellulose solution is 2-4 wt%.

4. The highly ink-absorbent synthetic paper according to claim 2, Features: In the step S13, the electrospinning distance is 12-18 cm, the flow rate is 0.05-0.1 mL / min, and the voltage is 15-18 kV.

5. The highly ink-absorbent synthetic paper according to claim 1, Features: The cellulose / SiO 2 The preparation method of micro-nanospheres comprises the following steps: S21. Dissolving cellulose in an alkaline urea solution to prepare a cellulose solution having a concentration of 2.2-3wt%; S22. Add nanoporous SiO 2 The particles are stirred and mixed evenly to obtain cellulose / SiO 2 Mixing solutions; S23. The mixed solution prepared in step S23 is sprayed with high-voltage electrostatic spray to prepare cellulose / SiO 2 Micro-nano spheres.

6. The highly ink-absorbent synthetic paper according to claim 5, Features: In step S22, the nano-SiO 2 The content of the particles in the mixed solution is 5-30wt%.

7. The highly ink-absorbent synthetic paper according to claim 5, Features: In the step S23, the inner diameter of the needle used in the high-voltage electrostatic spray is 1.2-1.5 mm, the spray distance is 12-18 cm, the flow rate is 0.01-0.03 mL / min, and the voltage is 12-15 kV.

8. The method for preparing the highly ink-absorbent synthetic paper according to claim 1, It is characterized in that The following steps are involved: S1. Dissolve PVC in DMF, mix and stir, and after dissolution, obtain PVC pulp liquid; S2. Take part of the PVC pulp prepared in step S1 and mix the cellulose / SiO 2 The micro-nano balls are added into the PVC pulp liquid and stirred evenly to obtain the PVC synthetic pulp liquid; S3. The PVC pulp prepared in step S1 is poured into a mold, and the solvent is evaporated to obtain a PVC layer; S4. A porous cellulose electrospinning layer is placed on the surface of the PVC layer, and then a PVC synthetic paper slurry is poured, and the solvent is evaporated to obtain a highly ink-absorbent synthetic paper.

Citation Information

Patent Citations

  • Stone water-free paper-making method and flow

    CN101701433A

  • Ink jet recording medium

    CN102632737A

  • Method for manufacturing synthetic paper with high ink receptivity

    CN102837473A

  • Preparation method and application of electrostatic spinning modified membrane adsorption material

    CN103161064A

  • Thermal sublimation and transfer digital paper with high ink suction amount

    CN103397576A