Parallel micro-channel liquid cooling device and manufacturing method thereof
Through wire cutting technology, the inclined microflower heat dissipation teeth are processed and combined with conductive adhesive bonding, the problems of high cost and size limitation of the microflower liquid-cooled plate are solved, and low-cost and efficient heat dissipation effect is achieved.
Patent Information
- Application Number
- CN202410942101.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2024-11-05
AI Technical Summary
The existing microflower liquid-cooled plates are costly to be processed and molded by CNC, and the microflower size is limited, making it impossible to achieve low-cost, high heat dissipation density.
The inclined microflower heat dissipation teeth are processed by wire cutting technology, and a closed cavity is formed with the cold plate core and the cold plate seat. Combined with conductive adhesive bonding, the cooling liquid is fully contacted and heat exchange is achieved, and the device cost is reduced.
Through the closed cavity structure between the cold plate core and the cold plate base and the design of multi-layer heat dissipation teeth, the heat exchange efficiency of the coolant is improved, and the effect of low-cost and high heat dissipation density is achieved.
Smart Images

Figure CN118899280A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of communications, and more specifically, to a parallel microchannel liquid cooling device and a manufacturing method thereof. Background Art
[0002] In the field of communications, a new type of efficient thermal control technology, micro-channel liquid cooling technology, is provided to meet the high heat dissipation requirements of various components. It utilizes the micro-scale effect of flow and heat transfer to greatly improve the convective heat transfer capacity of internal flow, and adopts a group of rectangular micro-fins embedded in the cold plate flow channel to form a micro-channel liquid cooling flow channel structure.
[0003] Currently, most microfluidic liquid cooling plates on the market are CNC machined, which is costly and has restrictions on the size of the microchannel. In order to solve this problem, a beveled microchannel heat dissipation tooth formed by wire cutting technology is proposed, which is then bonded to the cold plate groove with conductive glue to achieve low cost and high heat dissipation density. Summary of the invention
[0004] The present invention aims to overcome at least one defect (shortcoming) of the above-mentioned prior art and provide a parallel microchannel liquid cooling device and a manufacturing method thereof, which are used to solve the problem that the liquid cooling plate is processed at high cost through CNC, the microchannel size is limited, and the heat dissipation effect with low cost and high heat dissipation density cannot be achieved.
[0005] The technical solution adopted by the present invention is a parallel microchannel liquid cooling device, which includes: a cold plate assembly provided with a liquid inlet and a liquid outlet, the cold plate assembly including a cold plate core and a cold plate seat, the cold plate seat is provided with a recess, the cold plate core is placed on the recess of the cold plate seat, and a closed cavity is formed between the cold plate core and the recess; the cold plate core includes heat dissipation teeth, the heat dissipation teeth are connected to the cold plate core and are located in the closed cavity; the cooling liquid flows into the closed cavity from the liquid inlet, exchanges heat with the heat dissipation teeth, and then flows out from the liquid outlet.
[0006] It is beneficial to guide the flow of the coolant through the liquid inlet and the liquid outlet, to form a closed cavity through the cold plate core and the cold plate seat, so that the coolant can fully contact the cold plate assembly and improve the heat exchange efficiency, and to reduce the production cost of the one-piece liquid cooling device through the heat dissipation teeth connected to the cold plate core.
[0007] Furthermore, the cold plate seat includes a plurality of isolation bosses arranged in the recess, the plurality of isolation bosses are arranged in parallel in the long axis direction of the cold plate seat, and form parallel flow channels on the cold plate seat along the long axis direction, and the parallel flow channels are parallel to the flow direction of the coolant.
[0008] It is beneficial to divert the coolant flowing into the closed cavity through the isolation bosses arranged in parallel, so that the flow rate of the coolant in the parallel flow channels is the same; it is beneficial to make the setting direction of the parallel flow channels parallel to the inlet and outlet directions of the coolant, so that the coolant continuously flows in and out of the parallel flow channels to reduce the coolant temperature in the closed cavity, thereby improving the heat dissipation effect of the cold plate assembly.
[0009] Furthermore, the recess and the isolation boss are both step-shaped with a lower convex edge, a cold plate hole corresponding to the isolation boss is provided in the middle of the cold plate core, the outer edge of the cold plate core abuts the lower convex edge of the recess, and the cold plate hole abuts the lower convex edge of the isolation boss.
[0010] It is beneficial to realize the fitting installation of the cold plate core and the cold plate seat through the step-shaped recess and the isolation boss. At the same time, the fitted cold plate core and the cold plate seat form a closed cavity to protect the coolant from leakage.
[0011] Furthermore, the upper surface of the isolation boss is flush with the upper surface of the cold plate seat, and the distance between the upper surface of the lower convex edge and the upper surface of the cold plate seat is equal to the thickness of the cold plate core.
[0012] It is beneficial to make the upper surface of the isolation boss flush with the upper surface of the cold plate seat, and the thickness of the cold plate core is embedded in the lower convex edge of the cold plate seat and the lower convex edge of the isolation boss, thereby forming a cold plate assembly with a flat upper surface, increasing the application flexibility of the cold plate assembly.
[0013] Furthermore, the heat dissipation teeth are perpendicular to the parallel flow channels, abutting between the inner wall of the recess and the side wall of the isolation boss, and abutting against the side wall gap between two adjacent isolation bosses, and the flow direction of the heat dissipation teeth is parallel to the flow direction of the coolant.
[0014] The heat dissipation teeth are arranged perpendicular to the parallel flow channels, thereby increasing the contact area between the coolant and the heat dissipation teeth, so that the coolant is in full contact with the heat dissipation teeth in the parallel flow channels, thereby improving the heat dissipation efficiency.
[0015] Furthermore, the heat dissipation teeth include upper heat dissipation teeth, lower heat dissipation teeth and an intermediate layer, the upper heat dissipation teeth are fixedly connected to the cold plate core, and the lower heat dissipation teeth are fixedly connected to the upper heat dissipation teeth through the intermediate layer.
[0016] It is beneficial to isolate the upper and lower sides of the liquid cooling device through the double-layer heat dissipation teeth to achieve heat dissipation on both sides of the liquid cooling device, and to achieve a constant contact area between the coolant and the heat dissipation teeth through the fixed connection between the upper heat dissipation teeth and the cold plate core and the fixed connection between the lower heat dissipation teeth and the middle layer.
[0017] Furthermore, the lower heat dissipation teeth are arranged in the direction in which the upper heat dissipation teeth extend downward, the cross section of the upper heat dissipation teeth is inclined at an angle α to the cross section of the cold plate core, and the cross section of the lower heat dissipation teeth is inclined at an angle α to the cross section of the middle layer.
[0018] It is beneficial to make the extension direction of the lower heat dissipation teeth consistent with that of the upper heat dissipation teeth, avoiding too much flow resistance affecting the flow direction when the coolant passes through the upper heat dissipation teeth and the lower heat dissipation teeth at the same time. It is beneficial to increase the contact area between the coolant and the heat dissipation teeth through the inclined upper heat dissipation teeth and the lower heat dissipation teeth, so as to improve the heat dissipation efficiency.
[0019] Furthermore, the upper heat dissipation teeth and the lower heat dissipation teeth each include a plurality of wave-shaped protrusions.
[0020] It is beneficial to increase the disturbance effect of the coolant on the heat dissipation teeth through the wave-like protrusions, thereby increasing the turbulence effect of the coolant in the parallel channel and improving the heat dissipation efficiency.
[0021] Furthermore, a gap between two adjacent wave-shaped protrusions on the upper heat dissipation teeth, and / or a gap between two adjacent wave-shaped protrusions on the lower heat dissipation teeth, is less than or equal to 0.5 mm.
[0022] It is beneficial to form a microchannel through a gap within a specific numerical range, thereby utilizing the microscale effect and boundary layer effect of the flow to improve the convective heat transfer coefficient between the coolant and the liquid cooling device and improve the heat dissipation efficiency.
[0023] Another technical solution adopted by the present invention is a method for manufacturing a parallel microchannel liquid cooling device, which includes the following steps:
[0024] S1. Forming a cooling seat and a cooling core in the liquid cooling device respectively;
[0025] S2. Use wire cutting to make heat dissipation teeth suitable for the cooling core, and perform surface conductive oxidation treatment;
[0026] S3. The heat dissipation teeth processed in S2 are bonded to the cold plate core by H20E two-component conductive adhesive. The two-component conductive adhesive includes component A and component B. The two components are stirred and mixed at a ratio of 1:1 under room temperature. The uniformly mixed conductive adhesive is evenly brushed on the bottom surface of the heat dissipation teeth. The thickness of the adhesive is 0.2-0.4mm. The heat dissipation teeth are then pressed on the bonding reserved position of the cold plate core. After pressing, the conductive adhesive will be squeezed and overflow from the bonding reserved position surface to ensure that the surface thickness of the overflowed conductive adhesive does not exceed 0.2mm. The top surface of the heat dissipation teeth is pressed with external force. The cold plate core bonded with the heat dissipation teeth is placed in a constant temperature box; the temperature of the constant temperature box is set to 115-125°, and high-temperature baking is performed for 1.5-2.5 hours of curing;
[0027] S4. After the cooling core is cooled after step S3 is completed, it is taken out and subjected to a vibration test on a vibration platform;
[0028] S5. The cold plate core is sealed by laser welding or friction stir welding. After welding, the surface is milled flat and finished by a milling cutter to complete the production of the cooling core;
[0029] S6. Install the cooling core and cooling seat manufactured in S5 to form a cold plate assembly, introduce coolant through the liquid inlet and the liquid outlet, and start heat exchange on the cold plate assembly.
[0030] The above-mentioned manufacturing method is beneficial for realizing the processing of a microchannel heat dissipation with a maximum flow area in a limited space, and the processing and molding of the microchannel cooling device is realized by high-temperature bonding with conductive glue, thereby achieving the optimization effect of low processing cost and increased heat dissipation area.
[0031] Compared with the prior art, the beneficial effects of the present invention are: through the closed cavity formed by the cold plate core and the cold plate seat, the coolant is fully in contact with the cold plate assembly and the heat exchange efficiency is improved, and the heat dissipation teeth connected to the cold plate core reduce the production cost of the one-piece liquid cooling device, thereby achieving a heat dissipation effect with low cost and high heat dissipation density. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is an exploded bottom view of the structure of the present invention.
[0033] Figure 2 It is a schematic diagram of the structural explosion of the present invention.
[0034] Figure 3 It is a partially enlarged schematic diagram of the heat dissipation teeth of the present invention.
[0035] Figure 4 It is a top view of the coolant flow direction of the present invention.
[0036] Figure 5 It is a schematic cross-sectional view of the heat dissipation teeth of the present invention.
[0037] Figure 6 It is an enlarged cross-sectional view of the heat dissipation teeth of the present invention.
[0038] Figure 7 It is an enlarged schematic diagram of a preferred embodiment of the connection method of the heat dissipation teeth of the present invention.
[0039] Figure 8 It is an enlarged schematic diagram of a preferred embodiment of the connection method of the heat dissipation teeth of the present invention.
[0040] Fig. 9 It is an enlarged schematic diagram of a preferred embodiment of the connection method of the heat dissipation teeth of the present invention.
[0041] Description of the symbols in the accompanying drawings: cold plate assembly 10 , liquid inlet 11 , liquid outlet 12 , cold plate core 100 , cold plate hole 110 , heat dissipation teeth 300 , cold plate seat 200 , recess 210 , isolation boss 220 , parallel flow channel 230 . DETAILED DESCRIPTION
[0042] The drawings of the present invention are only for illustrative purposes and should not be construed as limiting the present invention. In order to better illustrate the following embodiments, some parts of the drawings may be omitted, enlarged or reduced, and do not represent the size of the actual product; it is understandable to those skilled in the art that some well-known structures and their descriptions in the drawings may be omitted. Example 1
[0043] like Figure 1-6 As shown, this embodiment provides a parallel microchannel liquid cooling device, which includes: a cold plate assembly 10 provided with a liquid inlet 11 and a liquid outlet 12, the cold plate assembly 10 includes a cold plate core 100 and a cold plate seat 200, the cold plate seat 200 is provided with a recess 210, the cold plate core 100 is placed on the recess 210 of the cold plate seat 200, and a closed cavity is formed between the cold plate core 100 and the recess 210; the cold plate core 100 includes heat dissipation teeth, the heat dissipation teeth 300 are connected to the cold plate core 100 and are located in the closed cavity; the coolant flows into the closed cavity from the liquid inlet 11, and after heat exchange with the heat dissipation teeth, it flows out from the liquid outlet 12.
[0044] In this embodiment, the liquid inlet 11 and the liquid outlet 12 are both protrusions formed below the cold plate seat 200, so that the coolant does not need to be punched in and out, thereby avoiding leakage of the coolant. The cold plate core 100 is embedded in the cold plate seat 200, so that the recess 210 in the cold plate seat 200 becomes a closed cavity, and the heat dissipation teeth connected to the cold plate core 100, the coolant flows in the closed cavity and exchanges heat with the heat dissipation teeth.
[0045] The cold plate seat 200 includes a plurality of isolation bosses 220 disposed in the recess 210. The plurality of isolation bosses 220 are arranged in parallel in the long axis direction of the cold plate seat 200 and form parallel flow channels on the cold plate seat 200 along the long axis direction. The parallel flow channels are parallel to the flow direction of the coolant.
[0046] In this embodiment, the isolation boss 220 is used to separate the space of the closed cavity, thereby guiding the coolant to flow along the parallel flow channel formed by the separation, so that each isolation boss 220 is in full contact with the coolant. Heat-generating components can be placed in the isolation boss 220, so that the heat-generating components can dissipate heat to the upper cold plate core 100 and the lower cold plate seat 200 in the closed cavity at the same time. The isolation boss 220 is in the shape of a rectangular block with a waist depression 210, so that the width of the parallel flow channel at the waist depression 210 is the largest, which is convenient for the placement of the heat dissipation teeth, and also convenient for controlling the coolant to flow into the heat dissipation teeth to reduce the flow rate, and then increase the flow rate of the coolant flowing out of the heat dissipation teeth.
[0047] The recess 210 and the isolation boss 220 are both stepped with a lower convex edge. A cold plate hole 110 corresponding to the isolation boss 220 is provided in the middle of the cold plate core 100. The outer edge of the cold plate core 100 abuts against the lower convex edge of the recess 210, and the cold plate hole 110 abuts against the lower convex edge of the isolation boss 220.
[0048] In this embodiment, the lower convex edge of the recess 210 and the lower convex edge of the isolation boss 220 are used to support the placement of the cold plate core 100, the outer edge of the cold plate core 100 is placed on the step of the recess 210, and the cold plate hole 110 is placed on the step of the isolation boss 220. In this embodiment, the step height of the isolation boss 220 is inconsistent with the step height of the recess 210.
[0049] The upper surface of the isolation boss 220 is flush with the upper surface of the cold plate seat 200 , and the distance between the upper surface of the lower convex edge and the upper surface of the cold plate seat 200 is equal to the thickness of the cold plate core 100 .
[0050] In this embodiment, the height of the lower convex edge of the recess 210 is the same as the height of the lower convex edge of the isolation boss 220, both of which are the thickness of the cold plate core 100, so that when the cold plate core 100 is embedded on the lower convex edge, it can achieve complete fit and avoid leakage of coolant.
[0051] The heat dissipation teeth 300 are perpendicular to the parallel flow channels, and abut between the inner wall of the recess 210 and the side wall of the isolation boss 220 , and abut against the gap between the side walls of two adjacent isolation bosses 220 .
[0052] In this embodiment, the heat dissipation teeth 300 are bonded to the bottom of the cold plate core 100 by conductive adhesive. When the cold plate core 100 is placed on the lower convex edge of the recess 210 and the lower convex edge of the isolation boss 220, the ends of the heat dissipation teeth 300 are in contact with both sides in the parallel channel 230.
[0053] The heat dissipation teeth 300 include an upper heat dissipation tooth, a lower heat dissipation tooth and an intermediate layer. The upper heat dissipation tooth is fixedly connected to the cold plate core 100 , and the lower heat dissipation tooth is fixedly connected to the upper heat dissipation tooth through the intermediate layer.
[0054] In the present embodiment, the upper heat dissipation teeth, the lower heat dissipation teeth and the middle layer are made of aviation aluminum alloy, and are specially designed as oblique wavy teeth by slow wire cutting technology. The fixed connection between the upper heat dissipation teeth and the lower heat dissipation teeth cannot be disassembled, so that the flow area of the heat dissipation teeth 300 in the closed cavity remains constant, and the heat dissipation efficiency under different heat-generating components is achieved by adjusting the inlet and outlet flow rates of the coolant.
[0055] The lower heat dissipation teeth are arranged in the direction in which the upper heat dissipation teeth extend downward, the cross section of the upper heat dissipation teeth is inclined at an angle α to the cross section of the cold plate core 100, and the cross section of the lower heat dissipation teeth is inclined at an angle α to the cross section of the middle layer.
[0056] In this embodiment, the inclination angle α=60°, the lower heat dissipation teeth are arranged in the downward extending direction of the upper heat dissipation teeth and the two have the same inclination angle, so that the flow area of the upper heat dissipation teeth is extended and expanded through the setting position of the lower heat dissipation teeth, thereby improving the heat dissipation efficiency.
[0057] The upper heat dissipation teeth and the lower heat dissipation teeth each include a plurality of wave-shaped protrusions.
[0058] In this embodiment, the middle layer is in the shape of a long strip, and the upper heat dissipation teeth and the lower heat dissipation teeth are provided with wave-shaped protrusions protruding outwards, which are used to disturb the flow and increase the contact time between the coolant and the heat dissipation teeth, thereby improving the heat dissipation efficiency. Each upper heat dissipation tooth and the lower heat dissipation tooth include 4-5 wave-shaped protrusions.
[0059] The gap between two adjacent wave-shaped protrusions on the upper heat dissipation teeth and / or the gap between two adjacent wave-shaped protrusions on the lower heat dissipation teeth are both less than or equal to 0.5 mm.
[0060] In this embodiment, the gap between two adjacent wave-shaped protrusions on the heat dissipation teeth 300 can be 0.5 mm or less. Example 2
[0061] Another technical solution adopted by the present invention is a method for manufacturing a parallel microchannel liquid cooling device, which includes the following steps:
[0062] S1. Forming a cooling seat and a cooling core in the liquid cooling device respectively;
[0063] S2. Use wire cutting to make heat dissipation teeth suitable for the cooling core, and perform surface conductive oxidation treatment;
[0064] S3. The heat dissipation tooth 300 processed in S2 is bonded to the cold plate core 100 by H20E two-component conductive adhesive. The two-component conductive adhesive includes component A and component B. The two components are stirred and mixed at a ratio of 1:1 under room temperature. The uniformly mixed conductive adhesive is evenly brushed on the bottom surface of the heat dissipation tooth 300. The thickness of the adhesive is 0.2-0.4mm. The heat dissipation tooth 300 is then pressed on the bonding reserved position of the cold plate core 100. After pressing, the conductive adhesive will be squeezed and overflowed from the bonding reserved position surface to ensure that the surface thickness of the overflowed conductive adhesive does not exceed 0.2mm. The top surface of the heat dissipation tooth is pressed with external force. The cold plate core 100 bonded with the heat dissipation tooth is placed in a constant temperature box; the temperature of the constant temperature box is set to 115-125°, and high-temperature baking is performed for 1.5-2.5 hours of curing;
[0065] S4. After the cooling core is cooled after step S3 is completed, it is taken out and subjected to a vibration test on a vibration platform;
[0066] S5. The cold plate core 100 is sealed by laser welding or friction stir welding. After welding, the surface is milled and finished by a milling cutter to complete the production of the cooling core;
[0067] S6. Install the cooling core and cooling seat manufactured in S5 to form a cold plate assembly 10, introduce cooling liquid through the liquid inlet 11 and the liquid outlet 12, and start heat exchange for the cold plate assembly 10. Example 3
[0068] Different from the first embodiment, in the present embodiment, the upper heat dissipation teeth are movably connected to the cold plate core 100, and the lower heat dissipation teeth are movably connected to the middle layer.
[0069] In this embodiment, there are turning connections between the cold plate core 100 and the upper heat dissipation teeth, and between the middle layer and the lower heat dissipation teeth, so that the inclination angle between the upper heat dissipation teeth and the cold plate core 100, and the inclination angle between the lower heat dissipation teeth and the middle layer are not fixed. The adjustable inclination angle can change the flow direction of the coolant and also allow impurities in the coolant to fall off during the process of adjusting the inclination angle.
[0070] like Figure 7 As shown, in this embodiment, the steering connection is a spherical hinge, and other steering connection methods can also be used. Example 4
[0071] Different from the first embodiment, in the present embodiment, the upper heat dissipation teeth are movably connected to the cold plate core 100, and the lower heat dissipation teeth are movably connected to the middle layer.
[0072] like Figure 8As shown, in this embodiment, the cold plate core 100 and the upper heat dissipation teeth are spherically hinged, the middle layer includes an annular track, when the root of the upper heat dissipation teeth rotates around the spherical hinge, the tip of the upper heat dissipation teeth is in contact with the annular track, the lower heat dissipation teeth and the middle layer are spherically hinged, and the root of the lower heat dissipation teeth rotates around the spherical hinge. The inclination angle between the upper heat dissipation teeth and the cold plate core 100 changes around the annular track, and the inclination angle between the lower heat dissipation teeth and the middle layer is not fixed. The adjustable inclination angle can change the flow direction of the coolant and also allow impurities in the coolant to fall off during the adjustment of the inclination angle. Example 5
[0073] Different from the first embodiment, in the present embodiment, the upper heat dissipation teeth are movably connected to the cold plate core 100, and the lower heat dissipation teeth are movably connected to the middle layer.
[0074] like Fig. 9 As shown, in this embodiment, the middle layer and the isolation boss 220 are movably connected via a pull-out bracket, and the bracket is provided with limiting thorns. When the middle layer is pulled out, the limiting thorns drive the upper heat dissipation teeth and the lower heat dissipation teeth to turn at the same time, and the initial directions of the upper heat dissipation teeth and the lower heat dissipation teeth can be manually adjusted. The adjustable inclination angle can change the flow direction of the coolant, and can also allow impurities in the coolant to fall off during the process of adjusting the inclination angle.
[0075] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the technical solution of the present invention, and are not intended to limit the specific implementation methods of the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the claims of the present invention shall be included in the protection scope of the claims of the present invention.
Claims
1. A parallel microchannel liquid cooling device, characterized in that: include: A cold plate assembly is provided with a liquid inlet and a liquid outlet, the cold plate assembly comprises a cold plate core and a cold plate seat, the cold plate seat is provided with a recess, the cold plate core is placed on the recess of the cold plate seat, and a closed cavity is formed between the cold plate core and the recess; the cold plate core comprises a heat dissipation tooth, the heat dissipation tooth is connected to the cold plate core and is located in the closed cavity; The coolant flows into the closed cavity from the liquid inlet, exchanges heat with the heat dissipation teeth, and then flows out from the liquid outlet.
2. The parallel microchannel liquid cooling device according to claim 1, characterized in that: The cold plate seat comprises a plurality of isolation bosses arranged in the depression, the plurality of isolation bosses are arranged in parallel in the long axis direction of the cold plate seat, and form parallel flow channels on the cold plate seat along the long axis direction, and the parallel flow channels are parallel to the flow direction of the coolant.
3. The parallel microchannel liquid cooling device according to claim 2, characterized in that: The recess and the isolation boss are both step-shaped with a lower convex edge, a cold plate hole corresponding to the isolation boss is provided in the middle of the cold plate core, the outer edge of the cold plate core abuts the lower convex edge of the recess, and the cold plate hole abuts the lower convex edge of the isolation boss.
4. The parallel microchannel liquid cooling device according to claim 3, characterized in that: The upper surface of the isolation boss is flush with the upper surface of the cold plate seat, and the distance between the upper surface of the lower convex edge and the upper surface of the cold plate seat is equal to the thickness of the cold plate core.
5. The parallel microchannel liquid cooling device according to claim 2, characterized in that: The heat dissipation teeth are perpendicular to the parallel flow channels, abut between the inner wall of the recess and the side wall of the isolation boss, and abut against the gap between the side walls of two adjacent isolation bosses.
6. The parallel microchannel liquid cooling device according to claim 1, characterized in that: The heat dissipation teeth include upper heat dissipation teeth, lower heat dissipation teeth and an intermediate layer. The upper heat dissipation teeth are fixedly connected to the cold plate core, and the lower heat dissipation teeth are fixedly connected to the upper heat dissipation teeth through the intermediate layer.
7. The parallel microchannel liquid cooling device according to claim 6, characterized in that: The lower heat dissipation teeth are arranged in the direction in which the upper heat dissipation teeth extend downward, the cross section of the upper heat dissipation teeth is inclined at an angle α to the cross section of the cold plate core, and the cross section of the lower heat dissipation teeth is inclined at an angle α to the cross section of the middle layer.
8. The parallel microchannel liquid cooling device according to claim 6, characterized in that: The upper heat dissipation teeth and the lower heat dissipation teeth each include a plurality of wave-shaped protrusions.
9. The parallel microchannel liquid cooling device according to claim 8, characterized in that: The gap between two adjacent wave-shaped protrusions on the upper heat dissipation teeth and / or the gap between two adjacent wave-shaped protrusions on the lower heat dissipation teeth are both less than or equal to 0.5 mm.
10. A method for manufacturing a parallel microchannel liquid cooling device, characterized in that: The following steps are involved: S1. Forming a cooling seat and a cooling core in the liquid cooling device respectively; S2. Use wire cutting to make heat dissipation teeth suitable for the cooling core, and perform surface conductive oxidation treatment; S3. The heat dissipation teeth processed in S2 are bonded to the cold plate core by H20E two-component conductive adhesive. The two-component conductive adhesive includes component A and component B. The two components are stirred and mixed at a ratio of 1:1 under room temperature. The uniformly mixed conductive adhesive is evenly brushed on the bottom surface of the heat dissipation teeth. The thickness of the adhesive is 0.2-0.4mm. The heat dissipation teeth are then pressed on the bonding reserved position of the cold plate core. After pressing, the conductive adhesive will be squeezed and overflow from the bonding reserved position surface to ensure that the surface thickness of the overflowed conductive adhesive does not exceed 0.2mm. The top surface of the heat dissipation teeth is pressed with external force. The cold plate core bonded with the heat dissipation teeth is placed in a constant temperature box; the temperature of the constant temperature box is set to 115-125°, and high-temperature baking is performed for 1.5-2.5 hours of curing; S4. After the cooling core is cooled after step S3 is completed, it is taken out and subjected to a vibration test on a vibration platform; S5. The cold plate core is sealed by laser welding or friction stir welding. After welding, the surface is milled flat and finished by a milling cutter to complete the production of the cooling core; S6. Install the cooling core and cooling seat manufactured in S5 to form a cold plate assembly, introduce coolant through the liquid inlet and the liquid outlet, and start heat exchange on the cold plate assembly.