High-power diode and preparation method thereof
By designing a series PN junction structure in a high-power diode chip, the problems of high-power diodes in the prior art are solved, and the effects of volume reduction and power improvement are achieved.
Patent Information
- Application Number
- CN202410952636.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-05
AI Technical Summary
Existing high-power diodes lead to high cost and large size problems by superimposing multiple diode chips in series and packaging them into a whole.
In the same diode chip structure, the two PN junctions are connected in series, and through the design of the substrate layer, the first epitaxial layer, the second epitaxial layer and the conductive layer, the PN junction is in the on- or off state when the voltage is applied, reducing the Package requirements and increase power by increasing the number of PN junctions.
The volume reduction and power increase of high-power diodes are achieved, while simplifying the processing technology and improving the yield.
Smart Images

Figure CN118899343A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of diodes, and in particular to a high-power diode and a preparation method thereof. Background Art
[0002] A diode is an electronic device made of semiconductor materials. It has unidirectional conductivity and is widely used in various circuits. With the rapid development of science and technology, the complexity of circuits and high-power scenarios are increasing, which makes the demand for high-power diodes increasingly greater.
[0003] At present, high-power diode devices are often obtained by stacking and connecting multiple diode chips in series, leading out pins, and then encapsulating them into an integral device with resin. However, the above method requires multiple diodes to be packaged into an integral device, resulting in high costs and large size. Summary of the invention
[0004] In view of this, the present invention provides a high-power diode and a preparation method thereof to solve the problem that the existing high-power diode stacks a plurality of diode chips in series and then packages them, which leads to high cost and large volume.
[0005] In a first aspect, the present invention provides a high-power diode, comprising:
[0006] substrate layer;
[0007] A first epitaxial layer, located on one side surface of the substrate layer;
[0008] A second epitaxial layer is located on a surface of the first epitaxial layer facing away from the substrate layer, and the second epitaxial layer has a first diffusion region;
[0009] a first conductive layer electrically connected to the first diffusion region;
[0010] A second conductive layer is located on a surface of the substrate layer facing away from the first epitaxial layer and is electrically connected to the substrate layer;
[0011] The substrate layer has an opposite conductivity type to that of the first epitaxial layer, the second epitaxial layer has an opposite conductivity type to that of the first diffusion region, and the first epitaxial layer has an opposite conductivity type to that of the second epitaxial layer.
[0012] Beneficial effect: the first epitaxial layer is located on one side surface of the substrate layer, and the substrate layer and the first epitaxial layer have opposite conductivity types, so that a first PN junction is formed between the substrate layer and the first epitaxial layer; the first diffusion region is located in the second epitaxial layer, and the first diffusion region and the second epitaxial layer have opposite conductivity types, so that a second PN junction is formed between the first diffusion region and the second epitaxial layer; since the first epitaxial layer and the second epitaxial layer have opposite conductivity types, when a voltage is applied to the high-power diode, the first PN junction and the second PN junction are both in an on state or in an off state; the high-power diode of the present application realizes the series connection of two PN junctions in the same diode chip structure, thereby eliminating the need to connect the two diodes in series and then package them into a whole, thereby reducing the volume of the entire high-power diode, and increasing the number of PN junctions to improve the power of the high-power diode.
[0013] In an optional embodiment, it also includes a second diffusion region, which sequentially penetrates the second epitaxial layer and the first epitaxial layer and penetrates into the substrate layer. The second diffusion region is enclosed to form an isolation ring, and the first diffusion region is inside the isolation ring. The conductivity type of the second diffusion region is the same as the conductivity type of the first diffusion region.
[0014] The actual working area of each high-power diode is separated by the second diffusion region, so as to facilitate subsequent division into individual high-power diodes.
[0015] In an optional embodiment, the concentration of conductive impurities doped in the first epitaxial layer, the concentration of conductive impurities doped in the second epitaxial layer, and the concentration of conductive impurities doped in the first diffusion region are all lower than the concentration of conductive impurities doped in the substrate layer.
[0016] In an optional implementation, the concentration of conductive impurities doped in the first diffusion region is greater than the concentration of conductive impurities doped in the second epitaxial layer.
[0017] In an optional implementation, the concentration of conductive impurities doped in the second diffusion region is greater than the concentration of conductive impurities doped in the second epitaxial layer.
[0018] The actual operating voltage of the high-power diode is changed by changing the concentration of conductive impurities doped in the first diffusion region, the first epitaxial layer, the second epitaxial layer and the substrate layer, thereby changing the operating power of the high-power diode.
[0019] In an optional embodiment, it also includes an insulating layer, which is located on the side surface of the second epitaxial layer away from the first epitaxial layer, the first conductive layer is located on the side surface of the insulating layer away from the second epitaxial layer, and a portion of the first conductive layer penetrates the insulating layer and is electrically connected to the first diffusion region.
[0020] In a second aspect, the present invention provides a method for preparing a high-power diode, comprising:
[0021] providing a substrate layer;
[0022] forming a first epitaxial layer on a surface of one side of the substrate layer;
[0023] forming a second epitaxial layer on a surface of the first epitaxial layer facing away from the substrate layer;
[0024] forming a first diffusion region in the second epitaxial layer;
[0025] forming a first conductive layer, and electrically connecting the first conductive layer to the first diffusion region;
[0026] forming a second conductive layer on a surface of the substrate layer facing away from the first epitaxial layer, and the second conductive layer is electrically connected to the substrate layer;
[0027] The conductivity type of the substrate layer is opposite to that of the first epitaxial layer, the conductivity type of the second epitaxial layer is opposite to that of the first diffusion region, and the conductivity type of the first epitaxial layer is opposite to that of the second epitaxial layer.
[0028] By realizing the series connection of two PN junctions in the chip structure, not only the operating voltage and operating power of the high-power diode are improved, but also the volume of the high-power diode is reduced, and the processing technology is simple and the yield rate is high.
[0029] In an optional implementation manner, after forming the second epitaxial layer and before forming the first diffusion region, the method further includes:
[0030] forming an insulating layer on a surface of the second epitaxial layer facing away from the first epitaxial layer;
[0031] forming an annular groove penetrating the insulating layer, wherein the annular groove exposes a portion of the second epitaxial layer;
[0032] implanting conductive impurities into the second epitaxial layer in the annular groove to form the second diffusion region;
[0033] Wherein, the second diffusion region sequentially penetrates the second epitaxial layer and the first epitaxial layer and penetrates into the substrate layer;
[0034] The concentration of conductive impurities doped in the second diffusion region is greater than the concentration of conductive impurities doped in the second epitaxial layer.
[0035] In an optional implementation, the step of forming the first diffusion region in the second epitaxial layer includes:
[0036] forming a first through hole in the insulating layer located in the annular groove, wherein the first through hole penetrates the insulating layer and exposes a portion of the second epitaxial layer;
[0037] implanting conductive impurities into the second epitaxial layer in the first through hole to form the first diffusion region;
[0038] Wherein, the first diffusion region is located in the second epitaxial layer; and the concentration of conductive impurities doped in the first diffusion region is greater than the concentration of conductive impurities doped in the second epitaxial layer;
[0039] The concentration of conductive impurities doped in the first epitaxial layer, the concentration of conductive impurities doped in the second epitaxial layer, and the concentration of conductive impurities doped in the first diffusion region are all lower than the concentration of conductive impurities doped in the substrate layer.
[0040] In an optional embodiment,
[0041] Thinning a side of the substrate layer away from the first epitaxial layer;
[0042] The second conductive layer is formed on a surface of the thinned substrate layer that is away from the first epitaxial layer. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0044] Figures 1 to 11 is a schematic diagram of various steps of preparing a high-power diode structure in an embodiment of the present invention;
[0045] Fig.12 It is a schematic diagram of the structure of a high-power diode provided in an embodiment of the present invention.
[0046] Description of reference numerals:
[0047] 1. Substrate layer;
[0048] 2. The first epitaxial layer;
[0049] 3. The second epitaxial layer;
[0050] 41. a first conductive layer; 42. a second conductive layer;
[0051] 5 first diffusion area;
[0052] 6. Insulating layer; 61. Annular groove; 62. First through hole;
[0053] 7. The second diffusion region. DETAILED DESCRIPTION
[0054] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It is understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only some structures related to the present invention are shown in the accompanying drawings, rather than all structures. In the following description, the description of known structures and technologies is omitted to avoid unnecessary confusion of the concept of the present invention. Various structural schematic diagrams according to embodiments of the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified for the purpose of clear expression, and some details may be omitted. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships between them are only exemplary, and may be deviated due to manufacturing tolerances or technical limitations in practice, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs. In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element, or there may be an intermediate layer / element between them. In addition, if one layer / element is "on" another layer / element in one orientation, then when the orientation is reversed, the layer / element may be "below" the other layer / element.
[0055] In the related art, a high-power diode device is often obtained by stacking and connecting multiple diode chips in series, leading out pins, and then encapsulating them into an integral device with resin. However, the above method requires multiple diodes to be packaged into an integral device, resulting in high costs and large size.
[0056] Therefore, an embodiment of the present invention provides a high-power diode, which realizes the series connection of two PN junctions in the same chip structure, thereby reducing the volume of the entire high-power diode and improving the power of the high-power diode by increasing the number of PN junctions.
[0057] The present invention provides a high-power diode, such as Fig.12As shown, it includes a substrate layer 1, a first epitaxial layer 2, a second epitaxial layer 3, a first conductive layer 41 and a second conductive layer 42, the first epitaxial layer 2 is located on one side surface of the substrate layer 1, the second epitaxial layer 3 is located on the side surface of the first epitaxial layer 2 away from the substrate layer 1, and the second epitaxial layer 3 has a first diffusion region 5, the first conductive layer 41 is electrically connected to the first diffusion region 5, the second conductive layer 42 is located on the side surface of the substrate layer 1 away from the first epitaxial layer 2, and is electrically connected to the substrate layer 1; the substrate layer 1 and the first epitaxial layer 2 have opposite conductivity types, the second epitaxial layer 3 and the first diffusion region 5 have opposite conductivity types, and the first epitaxial layer 2 and the second epitaxial layer 3 have opposite conductivity types.
[0058] Specifically, Fig.12 As shown, the first conductive layer 41 and the second conductive layer 42 are two electrodes of the high-power diode, and the materials of the first conductive layer 41 and the second conductive layer 42 can be gold, silver, iron, copper or other conductive materials; the substrate layer 1 can be an N-type semiconductor material or a P-type semiconductor material. When the substrate layer 1 is an N-type semiconductor material, the first epitaxial layer 2 is a P-type semiconductor material, the second epitaxial layer 3 is an N-type semiconductor material, and the first diffusion region 5 is a P-type semiconductor material. The first conductive layer 41 is the anode of the power diode, and the second conductive layer 42 is the cathode of the power diode; when the substrate layer 1 is a P-type semiconductor material, the first epitaxial layer 2 is an N-type semiconductor material, and the second epitaxial layer 3 is an N-type semiconductor material. 3 is a P-type semiconductor material, the first diffusion region 5 is an N-type semiconductor material, the first conductive layer 41 is the cathode of the power diode, and the second conductive layer 42 is the anode of the power diode; the substrate layer 1 and the first epitaxial layer 2 form a first PN junction, and the first diffusion region 5 and the second epitaxial layer 3 form a second PN junction. When a forward voltage (greater than the dead zone voltage of the power diode) is applied to the first conductive layer 41 and the second conductive layer 42, the first PN junction and the second PN junction are both in a conducting state; when a reverse voltage (less than the breakdown voltage of the power diode) is applied to the first conductive layer 41 and the second conductive layer 42, the first PN junction and the second PN junction are both in a cut-off state. The material of the substrate layer 1 can be silicon or germanium, and the first epitaxial layer 2 and the second epitaxial layer 3 can both be silicon or germanium.
[0059] In the high-power diode provided in this embodiment, the first epitaxial layer 2 is located on one side surface of the substrate layer 1, and the conductivity types of the substrate layer 1 and the first epitaxial layer 2 are opposite, so that a first PN junction is formed between the substrate layer 1 and the first epitaxial layer 2, and the first diffusion region 5 is located in the second epitaxial layer 3, and the conductivity types of the first diffusion region 5 and the second epitaxial layer 3 are opposite, so that a second PN junction is formed between the first diffusion region 5 and the second epitaxial layer 3. Since the conductivity types of the first epitaxial layer 2 and the second epitaxial layer 3 are opposite, when voltage is applied to the high-power diode, the first PN junction and the second PN junction are both in the on state or in the off state. The high-power diode of the present application realizes the series connection of two PN junctions in the same diode chip structure, so there is no need to connect the two diodes in series and then package them into a whole, thereby reducing the volume of the entire high-power diode, and by increasing the number of PN junctions, the power of the high-power diode is improved.
[0060] In this embodiment, as an optional implementation, Fig.12 As shown, it also includes a second diffusion region 7, which sequentially penetrates the second epitaxial layer 3 and the first epitaxial layer 2 and penetrates into the substrate layer 1. The second diffusion region 7 encloses an isolation ring. The cross-sectional shape of the isolation ring can be a circular ring, a square ring or other hollow shapes. The second diffusion region 7 surrounds the outer periphery of the first diffusion region 5, that is, the first diffusion region 5 is included in the second diffusion region 7. The conductivity type of the second diffusion region 7 is the same as the conductivity type of the first diffusion region 5. When the first diffusion region 5 is a P-type semiconductor material, the second diffusion region 7 is also a P-type semiconductor material. When the first diffusion region 5 is an N-type semiconductor material, the second diffusion region 7 is also an N-type semiconductor material. The actual working area of each high-power diode is separated by the second diffusion region 7 to facilitate subsequent segmentation into each high-power diode, and the second diffusion region 7 can protect the actual working area of the high-power diode to prevent impurities from entering the actual working area.
[0061] In this embodiment, as an optional implementation, the conductive impurities doped in the N-type semiconductor are one or more of phosphorus, antimony, and other pentavalent elements, and the conductive impurities doped in the P-type semiconductor are also one or more of pentavalent elements. Personnel in the art can adjust the doping concentrations of the substrate layer 1, the first epitaxial layer 2, the second epitaxial layer 3, the first diffusion region 5, and the second diffusion region 7 as needed. Preferably, the concentration of the conductive impurities doped in the first epitaxial layer 2, the concentration of the conductive impurities doped in the second epitaxial layer 3, the concentration of the conductive impurities doped in the first diffusion region 5, and the concentration of the conductive impurities doped in the second diffusion region 7 are all less than the concentration of the conductive impurities doped in the substrate layer 1. The concentration of the conductive impurities doped in the first diffusion region 5 is greater than the concentration of the conductive impurities doped in the second epitaxial layer 3, and the concentration of the conductive impurities doped in the second diffusion region 7 is greater than the concentration of the conductive impurities doped in the second epitaxial layer 3, that is, the substrate layer 1 can be heavily doped, the first epitaxial layer 2 is lightly doped, the second epitaxial layer 3 is also lightly doped, the first diffusion region 5 is medium doped, and the second diffusion region 7 is also medium doped. By changing the concentration of the conductive impurities doped in the first diffusion region 5, the first epitaxial layer 2, the second epitaxial layer 3 and the substrate layer 1, the actual operating voltage of the high-power diode is changed, thereby changing the operating power of the high-power diode.
[0062] In this embodiment, as an optional implementation, the thickness of the substrate layer 1 is greater than or equal to the thickness of the first epitaxial layer 2 , and the thickness of the first epitaxial layer 2 is the same as or different from the thickness of the second epitaxial layer 3 .
[0063] In this embodiment, as an optional implementation, Fig.12 As shown, it also includes an insulating layer 6, the material of the insulating layer 6 can be silicon dioxide or other insulating materials, the insulating layer 6 is located on the side surface of the second epitaxial layer 3 away from the first epitaxial layer 2, the first conductive layer 41 is located on the side surface of the insulating layer 6 away from the second epitaxial layer 3, and a portion of the first conductive layer 41 penetrates the insulating layer 6 and is electrically connected to the first diffusion region 5, the first diffusion region 5 is flush with the second epitaxial layer 3, and the first conductive layer 41 is separated from the second epitaxial layer 3 by the insulating layer 6, thereby avoiding a short circuit between the first diffusion region 5 and the second epitaxial layer 3.
[0064] In a second aspect, the present invention provides a method for preparing a high-power diode, comprising the following steps:
[0065] S1, such as Figure 1 As shown, a substrate layer 1 is provided;
[0066] The substrate layer 1 may be heavily doped single crystal silicon or polycrystalline silicon, or heavily doped germanium crystal, and the resistance of the substrate layer 1 is 0.001-0.004Ω, which reduces the resistance of the substrate layer 1;
[0067] S2, such as Figure 2As shown, a first epitaxial layer 2 is formed on one side surface of the substrate layer 1;
[0068] A first epitaxial layer 2 can be formed on one surface of the substrate layer 1 by using one of the vapor phase epitaxy process, liquid phase epitaxy process, vapor deposition process, and molecular beam epitaxy process. The thickness of the first epitaxial layer 2 is 5-6um. Of course, those skilled in the art can adjust the thickness of the first epitaxial layer 2 as needed. The resistance of the first epitaxial layer 2 is 0.03-0.035Ω.
[0069] S3, such as Figure 3 As shown, a second epitaxial layer 3 is formed on a surface of the first epitaxial layer 2 facing away from the substrate layer 1;
[0070] The second epitaxial layer 3 can be formed on the surface of the first epitaxial layer 2 facing away from the substrate layer 1 by one of vapor phase epitaxy, liquid phase epitaxy, vapor deposition and molecular beam epitaxy processes. The thickness of the second epitaxial layer 3 is 5-6um, and the resistance of the second epitaxial layer 3 is 0.018-0.02Ω.
[0071] S4, forming a second diffusion region 7;
[0072] S41, using a first cleaning solution to clean the structure prepared in step 3, the first cleaning solution includes sulfuric acid and hydrogen peroxide, the cleaning temperature is 120-150°C, the first cleaning solution is used to remove heavy organic contamination and part of the metal on the surface of the structure prepared in step 3, after cleaning with the first cleaning solution, the above structure is rinsed with deionized water, and then the structure prepared in step 3 is cleaned with a second cleaning solution, the second cleaning solution includes ammonia water, hydrogen peroxide and water, the cleaning temperature is 25°C, the second cleaning solution is used to remove particulate impurities and polymers on the surface of the structure prepared in step 3, after cleaning with the second cleaning solution, the structure prepared in step 3 is rinsed with deionized water, and then the structure prepared in step 3 is cleaned with a third cleaning solution, the third cleaning solution includes hydrochloric acid, hydrogen peroxide and water, the third cleaning solution is used to remove metal ions on the surface of the structure prepared in step 3, after cleaning is completed, deionized water is used for rinsing, and then the structure prepared in step 3 is cleaned with a fourth cleaning solution, the fourth cleaning solution includes hydrofluoric acid, the fourth cleaning solution is used to remove particles on the surface of the structure prepared in step 3, after cleaning is completed, deionized water is used for rinsing.
[0073] S42, subjecting the structure obtained in step 41 to high temperature treatment in an atmosphere of oxygen and chlorine to repair lattice defects;
[0074] S43, such as Figure 4 As shown, an insulating layer 6 is formed on the surface of the second epitaxial layer 3 facing away from the first epitaxial layer 2 by using one of vapor deposition process, sol-gel method and liquid deposition method. The insulating layer 6 is made of silicon dioxide with a thickness of 1-1.2 um.
[0075] S45, such as Figure 5 As shown, a ring-shaped groove 61 is formed in the insulating layer 6 by using a photolithography process and an etching process. The ring-shaped groove 61 penetrates the second epitaxial layer 3 to expose a portion of the second epitaxial layer 3 .
[0076] S46, such as Figure 6 As shown, an ion implantation process is used to implant doped conductive impurities into the second epitaxial layer 3 in the annular groove 61. The conductive impurities may be one of the trivalent elements, and high-temperature diffusion is performed to form a second diffusion region 7. The diffusion depth is 14-18um, wherein the second diffusion region 7 sequentially penetrates the second epitaxial layer 3 and the first epitaxial layer 2, and penetrates into the substrate layer 1. The concentration of doped conductive impurities in the second diffusion region 7 is greater than the concentration of doped conductive impurities in the second epitaxial layer 3.
[0077] S5, forming a first diffusion region 5 in the second epitaxial layer 3;
[0078] S51, such as Figure 7 As shown, a first through hole 62 is formed in the insulating layer 6 located in the annular groove 61 by photolithography and etching processes. The shape of the first through hole 62 can be rectangular or other shapes. The shape of the first through hole 62 can be adjusted as needed. The first through hole 62 exposes a portion of the second epitaxial layer 3.
[0079] S52, such as Figure 8 As shown, an ion implantation process is used to implant doped conductive impurities into the second epitaxial layer 3 in the first through hole 62. The conductive impurities may be one of the trivalent elements, and high-temperature diffusion is performed to form a first diffusion region 5. The depth of the first diffusion region 5 is 2um. The first diffusion region 5 is flush with the first epitaxial layer 2, and the first diffusion region 5 does not penetrate the first diffusion region. The concentration of doped conductive impurities in the first diffusion region 5 is greater than the concentration of doped conductive impurities in the second epitaxial layer 3. The concentration of doped conductive impurities in the first epitaxial layer 2, the concentration of doped conductive impurities in the second epitaxial layer 3, and the concentration of doped conductive impurities in the first diffusion region 5 are all less than the concentration of doped conductive impurities in the substrate layer 1.
[0080] S6, such as Fig. 9 As shown, a first conductive layer 41 is formed on the surface of the insulating layer 6 facing away from the second epitaxial layer 3 by an evaporation process. The material of the first conductive layer 41 can be one or more of titanium, nickel, silver, aluminum or other conductive materials, and the first conductive layer 41 fills the first through hole 62 so that the first conductive layer 41 is electrically connected to the first diffusion region 5. Fig.10 As shown, the photolithography process and the etching process are used to remove the redundant first conductive layer 41 , and a portion of the first conductive layer 41 in and above the first through hole 62 is retained.
[0081] S7, such as Fig.11 As shown, a thinning process is adopted to thin the side of the substrate layer 1 away from the first epitaxial layer 2 , thereby reducing the thickness of the substrate layer 1 .
[0082] S8, such as Fig.12 As shown, after thinning is completed, a second conductive layer 42 is formed on the surface of the substrate layer 1 facing away from the first epitaxial layer 2 by an evaporation process. The material of the second electrode layer can be one or more of titanium, nickel, silver, aluminum or other conductive materials.
[0083] By realizing the series connection of two PN junctions in the chip structure, not only the operating voltage and operating power of the high-power diode are improved, but also the volume of the high-power diode is reduced. In addition, the first PN junction does not need to be prepared in the epitaxial layer, which simplifies the processing technology and improves the yield.
[0084] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.
[0085] Although the embodiments of the present invention have been described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present invention, and such modifications and variations are all within the scope defined by the appended claims.
Claims
1. A high power diode, characterized in that: include: A substrate layer (1); A first epitaxial layer (2) is located on a surface of one side of the substrate layer (1); A second epitaxial layer (3) is located on a surface of the first epitaxial layer (2) that is away from the substrate layer (1), and the second epitaxial layer (3) has a first diffusion region (5); A first conductive layer (41) electrically connected to the first diffusion region (5); A second conductive layer (42) is located on a surface of the substrate layer (1) that is away from the first epitaxial layer (2) and is electrically connected to the substrate layer (1); The conductivity type of the substrate layer (1) is opposite to that of the first epitaxial layer (2), the conductivity type of the second epitaxial layer (3) is opposite to that of the first diffusion region (5), and the conductivity type of the first epitaxial layer (2) is opposite to that of the second epitaxial layer (3).
2. The high power diode according to claim 1, characterized in that: It also includes a second diffusion region (7), which sequentially penetrates the second epitaxial layer (3), the first epitaxial layer (2), and penetrates into the substrate layer (1); the second diffusion region (7) encloses an isolation ring, the isolation ring has the first diffusion region (5), and the conductivity type of the second diffusion region (7) is the same as the conductivity type of the first diffusion region (5).
3. The high power diode according to claim 2, characterized in that: The concentration of conductive impurities doped in the first epitaxial layer (2), the concentration of conductive impurities doped in the second epitaxial layer (3), and the concentration of conductive impurities doped in the first diffusion region (5) are all lower than the concentration of conductive impurities doped in the substrate layer (1).
4. The high power diode according to claim 3, characterized in that: The concentration of conductive impurities doped in the first diffusion region (5) is greater than the concentration of conductive impurities doped in the second epitaxial layer (3).
5. The high power diode according to claim 4, characterized in that: The concentration of conductive impurities doped in the second diffusion region (7) is greater than the concentration of conductive impurities doped in the second epitaxial layer (3).
6. The high power diode according to any one of claims 1 to 5, characterized in that: The present invention also comprises an insulating layer (6), wherein the insulating layer (6) is located on a side surface of the second epitaxial layer (3) away from the first epitaxial layer (2), and the first conductive layer (41) is located on a side surface of the insulating layer (6) away from the second epitaxial layer (3), and a portion of the first conductive layer (41) penetrates the insulating layer (6) and is electrically connected to the first diffusion region (5).
7. A method for preparing a high-power diode, characterized in that: include: Providing a substrate layer (1); Forming a first epitaxial layer (2) on one side surface of the substrate layer (1); forming a second epitaxial layer (3) on a surface of the first epitaxial layer (2) facing away from the substrate layer (1); forming a first diffusion region (5) in the second epitaxial layer (3); forming a first conductive layer (41), and electrically connecting the first conductive layer (41) to the first diffusion region (5); A second conductive layer (42) is formed on a surface of the substrate layer (1) that is away from the first epitaxial layer (2), and the second conductive layer (42) is electrically connected to the substrate layer (1); The conductivity type of the substrate layer (1) is opposite to that of the first epitaxial layer (2), the conductivity type of the second epitaxial layer (3) is opposite to that of the first diffusion region (5), and the conductivity type of the first epitaxial layer (2) is opposite to that of the second epitaxial layer (3).
8. The method for preparing a high-power diode according to claim 7, characterized in that: After forming the second epitaxial layer (3) and before forming the first diffusion region (5), the method further includes: forming an insulating layer (6) on a surface of the second epitaxial layer (3) that is away from the first epitaxial layer (2); forming an annular groove (61) penetrating the insulating layer (6), wherein the annular groove (61) exposes a portion of the second epitaxial layer (3); Implanting conductive impurities into the second epitaxial layer (3) in the annular groove (61) to form the second diffusion region (7); The second diffusion region (7) ring sequentially penetrates the second epitaxial layer (3), the first epitaxial layer (2), and penetrates into the substrate layer (1); The concentration of conductive impurities doped in the second diffusion region (7) is greater than the concentration of conductive impurities doped in the second epitaxial layer (3).
9. The method for preparing a high-power diode according to claim 8, characterized in that: The step of forming the first diffusion region (5) in the second epitaxial layer (3) comprises: A first through hole (62) is formed in the insulating layer (6) located in the annular groove (61), wherein the first through hole (62) penetrates the insulating layer (6) and exposes a portion of the second epitaxial layer (3); Injecting conductive impurities into the second epitaxial layer (3) in the first through hole (62) to form the first diffusion region (5); The first diffusion region (5) is located in the second epitaxial layer (3), and the concentration of conductive impurities doped in the first diffusion region (5) is greater than the concentration of conductive impurities doped in the second epitaxial layer (3); The concentration of conductive impurities doped in the first epitaxial layer (2), the concentration of conductive impurities doped in the second epitaxial layer (3), and the concentration of conductive impurities doped in the first diffusion region (5) are all lower than the concentration of conductive impurities doped in the substrate layer (1).
10. The method for preparing a high power diode according to claim 9, characterized in that: Thinning the side of the substrate layer (1) facing away from the first epitaxial layer (2); The second conductive layer (42) is formed on a surface of the thinned substrate layer (1) that is away from the first epitaxial layer (2).