Method for preparing synthesis gas by catalytic reforming of sewage sludge in molten salt environment
By performing catalytic reforming of sewage sludge in a molten salt environment, the problems of low quality of gas phase products and high impurity gases during sludge gasification are solved, and more efficient sludge resource conversion and clean production are achieved, reducing harmful gases emission.
Patent Information
- Application Number
- CN202410976008.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-08
AI Technical Summary
During the gasification process of existing sludge, the gas phase products are of low quality and many impurities gases, resulting in unclean production process and complex subsequent gas separation, which is high.
The catalytic reforming of sewage sludge is carried out in a molten salt environment, and the traditional gas phase reaction is replaced by liquid phase reaction. The sludge is treated at the target temperature using molten salt medium and oxidant to generate synthesis gas, and the residual molten salt is recycled.
It improves heat transfer efficiency and reaction kinetics, enhances the selectivity and concentration of gas phase products, significantly reduces the secondary emissions of harmful gases, and promotes clean production.
Smart Images

Figure CN118908526A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of sludge disposal and resource recovery, and in particular to a method for preparing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment. Background Art
[0002] Sewage sludge is the main solid waste generated by municipal sewage treatment systems. Sewage sludge has the dual attributes of pollution and resources. Sludge contains a large amount of organic matter that can be used as biomass resources, but it also contains pollutants such as pathogenic bacteria, refractory organic matter, and heavy metals. The sludge resource process should pay attention to the quality of resource products and control secondary pollution at the same time. Sludge gasification can effectively utilize the resource attributes of sludge by converting organic components in sludge into combustible gases such as synthesis gas through thermochemical methods. At present, conventional sludge gasification processes are mostly carried out under an inert atmosphere, using gases such as oxygen, water vapor, and carbon dioxide as oxidants to achieve partial oxidation of organic components in sludge. Due to the complex sludge components and the difficulty in thermodynamic regulation of thermochemical processes, the gas phase products of conventional gasification reaction processes are of low quality and have many impurity gases, including secondary pollutant gases such as nitrogen oxides and sulfur oxides. This directly leads to unclean production processes and complex and high-cost subsequent gas separation processes. Summary of the invention
[0003] In view of the above-mentioned deficiencies in the prior art, the present invention provides a method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment. The method utilizes a molten salt liquid phase reaction environment to replace the traditional gas phase reaction environment, effectively solving the problems of low quality of gas phase products, high amount of impurity gases, unclean production process and complex subsequent gas separation process in conventional gasification reaction processes.
[0004] To achieve the above object, the technical solution adopted by the present invention to solve the technical problem is: to provide a method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment, comprising the following steps:
[0005] S1. Drying the sewage sludge to obtain sludge powder or lump sludge;
[0006] S2, heating the molten salt medium to the target conversion temperature, then adding the sludge powder or lump sludge obtained in step S1 into the liquid molten salt medium, and simultaneously inputting an oxidant; or heating the molten salt medium and the sludge powder or lump sludge together to the target conversion temperature, and simultaneously inputting an oxidant;
[0007] S3. Keep the temperature at the target conversion temperature, collect the synthesis gas, and then separate the sludge solid residue. The remaining molten salt medium can be recycled.
[0008] Further, in step S1, drying is performed at 60-80°C.
[0009] Further, drying is performed to a moisture content of 10-50%.
[0010] Further, in step S2, the molten salt medium is one of carbonate, chloride, nitrate and sulfate.
[0011] Furthermore, the carbonate is at least one of lithium carbonate, sodium carbonate, potassium carbonate and calcium carbonate.
[0012] Furthermore, the chloride salt is at least one of lithium chloride, sodium chloride, potassium chloride, calcium chloride, zinc chloride, manganese chloride and magnesium chloride.
[0013] Furthermore, the nitrate is at least one of lithium nitrate, sodium nitrate, potassium nitrate and calcium nitrate.
[0014] Furthermore, the sulfate is at least one of lithium sulfate, sodium sulfate, potassium sulfate and calcium sulfate.
[0015] Further, the temperature was raised at 10-20°C / min to the target conversion temperature.
[0016] Furthermore, the temperature was increased at 20°C / min to the target conversion temperature.
[0017] Further, the target conversion temperature is 45-55°C higher than the melting point or eutectic point temperature of the molten salt medium.
[0018] Furthermore, the target conversion temperature is 50° C. or higher than the melting point or eutectic point of the molten salt medium.
[0019] Furthermore, the melting point or eutectic temperature is 400-1000°C.
[0020] Furthermore, the mixture is thoroughly mixed to ensure that the molten salt medium completely immerses the sludge powder or lumpy sludge.
[0021] Furthermore, the oxidant is at least one of oxygen, carbon dioxide and water vapor.
[0022] Furthermore, the oxidant was input at a flow rate of 150-250 mL / min.
[0023] Furthermore, an oxidant is introduced by bubbling.
[0024] Furthermore, a mixed gas of an oxidant and nitrogen may be input.
[0025] The beneficial effect of adopting the above further scheme is: by controlling the ratio of the oxidant to nitrogen, the concentration of the oxidant participating in the reaction is adjusted, thereby adjusting the reaction kinetics.
[0026] Further, in step S3, the temperature is maintained at the target conversion temperature until no carbon monoxide or hydrogen is generated.
[0027] In summary, the present invention has the following beneficial effects:
[0028] 1. Compared with the conventional gasification reaction of sewage sludge, the present invention utilizes a molten salt liquid phase reaction environment to replace the traditional gas phase reaction environment, thereby enhancing the heat transfer efficiency, being able to enhance the conversion kinetics of organic components in the sludge, and being conducive to the generation of gas phase products.
[0029] 2. The method provided by the present invention utilizes the characteristics of enhanced heat transfer and catalytic activity of molten salt to achieve the improvement of the selectivity of synthesis gas in gas phase products and increase the concentration and yield of target products.
[0030] 3. The present invention, by means of the strong solubility of molten salt, can significantly reduce the secondary emission of harmful gases, such as nitrogen oxides, sulfur oxides, hydrogen sulfide, polycyclic aromatic hydrocarbons, etc., and promote clean production. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 Generate a curve comparison chart for carbon monoxide;
[0032] Figure 2 This is a comparison chart of hydrogen generation curves;
[0033] Figure 3 This is a comparison chart of sulfur dioxide emissions;
[0034] Figure 4 Comparison chart of nitrogen oxide emissions. DETAILED DESCRIPTION
[0035] The principles and features of the present invention are described below, and the examples are only used to explain the present invention and are not used to limit the scope of the present invention. If no specific conditions are specified in the embodiments, they are carried out according to normal conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments is not specified, they are all conventional products that can be purchased commercially.
[0036] Example 1
[0037] A method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment comprises the following steps:
[0038] S1. Dry the sewage sludge in an oven at 80°C until the moisture content is 15% to obtain sludge powder or lumpy sludge;
[0039] S2, selecting 200g of Li-Na-K ternary carbonate molten salt as the molten salt medium, wherein the molar ratio of lithium carbonate, sodium carbonate and potassium carbonate is 43.5:31.5:25, heating the molten salt medium to 650°C at a rate of 10°C / min, and then adding 20g of the sludge powder or lump sludge obtained in step S1 and mixing them thoroughly to ensure that the molten salt medium completely immerses the sludge powder or lump sludge, and at the same time, inputting a mixed gas of carbon dioxide and nitrogen at a flow rate of 200mL / min and in a bubbling manner, wherein the concentration of carbon dioxide is 15%;
[0040] S3. Keep the temperature at 650°C until no new nitrogen monoxide or hydrogen is generated, collect the synthesis gas, and then separate the sludge solid residue. The remaining molten salt medium can be recycled.
[0041] Example 2
[0042] A method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment comprises the following steps:
[0043] S1. Dry the sewage sludge in an oven at 60°C until the moisture content is 30% to obtain sludge powder or lumpy sludge;
[0044] S2, selecting 300g of Li-Na-K ternary chloride molten salt as the molten salt medium, wherein the molar ratio of lithium chloride, sodium chloride and potassium chloride is 47.5:15:37.5, and then adding 20g of the sludge powder or lump sludge obtained in step S1 and mixing them thoroughly to ensure that the molten salt medium completely immerses the sludge powder or lump sludge, and then heating the molten salt medium to 750°C at a rate of 20°C / min, and using the water contained in the sludge itself to generate water vapor at high temperature as an oxidant;
[0045] S3. Keep the temperature at 750°C until no new nitrogen monoxide or hydrogen is generated, collect the synthesis gas, and then separate the sludge solid residue. The remaining molten salt medium can be recycled.
[0046] Example 3
[0047] A method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment comprises the following steps:
[0048] S1. Dry the sewage sludge in an oven at 70°C until the moisture content is 50% to obtain sludge powder or lumpy sludge;
[0049] S2, selecting 200g of Li-Na-K ternary nitrate molten salt as the molten salt medium, wherein the molar ratio of lithium nitrate, sodium nitrate and potassium nitrate is 45:32.5:22.5, heating the molten salt medium to 450°C at a rate of 15°C / min, and then adding 20g of the sludge powder or lump sludge obtained in step S1 and mixing them thoroughly to ensure that the molten salt medium completely immerses the sludge powder or lump sludge, and then inputting oxygen at a flow rate of 250mL / min and in a bubbling manner;
[0050] S3. Keep the temperature at 400°C until no new nitrogen monoxide or hydrogen is generated, collect the synthesis gas, and then separate the sludge solid residue. The remaining molten salt medium can be recycled.
[0051] Comparative Example
[0052] A method for gasifying wet sludge in nitrogen comprises the following steps:
[0053] S1. Dry the sewage sludge in an oven at 80°C until the moisture content is 15% to obtain sludge powder or lumpy sludge;
[0054] S2, the sludge powder or block sludge obtained in step S1 is placed under nitrogen atmosphere, the temperature of the molten salt medium is raised to 650°C at a rate of 10°C / min, and a mixed gas of carbon dioxide and nitrogen is introduced at a flow rate of 200 mL / min in a bubbling manner, wherein the concentration of carbon dioxide is 15%;
[0055] S3. Keep the temperature at 650°C until no new nitrogen monoxide or hydrogen is generated, collect the synthesis gas, and recover the sludge solid residue.
[0056] Test example
[0057] In the process of preparing synthesis gas in Example 1, the concentrations of carbon monoxide (CO), hydrogen (H2), sulfur dioxide (SO2), and nitrogen oxides (NOx) in the gas phase products were monitored by an online gas analyzer throughout the process, and compared with the comparative example. The results are as follows: Figure 1-Figure 4 As shown. Among them, Figure 1 is the concentration of carbon monoxide, Figure 2 is the concentration of hydrogen, Figure 3 is the concentration of sulfur dioxide, Figure 4 is the concentration of nitrogen oxides.
[0058] Depend on Figure 1-Figure 4 It can be seen that the concentrations of carbon monoxide and hydrogen in the gas phase products of sludge thermal conversion under molten salt environment are significantly higher than the concentrations of gas phase products gasified in sludge nitrogen. This shows that the molten salt liquid phase reaction environment has advantages in enhancing sludge gasification kinetics and improving conversion rate. Correspondingly, the emission intensity of sulfur dioxide and nitrogen oxides in the molten salt environment is significantly reduced, indicating that molten salt has the ability to control secondary gas pollution emissions.
[0059] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment, characterized in that: The following steps are involved: S1. Drying the sewage sludge to obtain sludge powder or lump sludge; S2, heating the molten salt medium to the target conversion temperature, then adding the sludge powder or lump sludge obtained in step S1 into the liquid molten salt medium, and simultaneously inputting an oxidant; or heating the molten salt medium and the sludge powder or lump sludge together to the target conversion temperature, and simultaneously inputting an oxidant; S3. Keep the temperature at the target conversion temperature, collect the synthesis gas, and then separate the sludge solid residue. The remaining molten salt medium can be recycled.
2. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1, characterized in that: In step S1, drying is performed until the moisture content is 10-50%.
3. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1, characterized in that: In step S2, the molten salt medium is one of carbonate, chloride, nitrate and sulfate.
4. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment as claimed in claim 3, characterized in that: The carbonate is at least one of lithium carbonate, sodium carbonate, potassium carbonate and calcium carbonate; the chloride salt is at least one of lithium chloride, sodium chloride, potassium chloride, calcium chloride, zinc chloride, manganese chloride and magnesium chloride; the nitrate is at least one of lithium nitrate, sodium nitrate, potassium nitrate and calcium nitrate; the sulfate is at least one of lithium sulfate, sodium sulfate, potassium sulfate and calcium sulfate.
5. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1, characterized in that: In step S2, the temperature is raised to the target conversion temperature at 10-20°C / min.
6. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1 or 5, characterized in that: The target conversion temperature is 45-55°C higher than the melting point or eutectic point of the molten salt medium.
7. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 6, characterized in that: The melting point or eutectic point temperature is 400-1000°C.
8. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1, characterized in that: In step S2, the oxidant is at least one of oxygen, carbon dioxide and water vapor.
9. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1, characterized in that: In step S2, an oxidant is introduced by bubbling.
10. The method for producing synthesis gas by catalytic reforming of sewage sludge in a molten salt environment according to claim 1, characterized in that: In step S3, the temperature is maintained at the target conversion temperature until no carbon monoxide or hydrogen is generated.
Citation Information
Patent Citations
Process for co-producing bio-oil and biological carbon by utilizing crop straws and special device
CN101875845A
Method for preparing hydrogen through fused salt
CN102838084A
System and method for catalytic purification treatment on coal chemical industry crude synthesis gas
CN105838449A
Urban solid waste and carbon dioxide co-recycling method
CN113025388A
Method and device for preparing carbon-based material and co-producing fuel gas from organic waste and molten salt
CN114717015A