Antistatic PC material and preparation method thereof
By using antistatic particles and nanographite powder with three-dimensional network structure in PC materials, the cross-linked structure and conductive network are formed, and the problem of difficult to take into account both the antistatic and mechanical properties of existing PC materials is achieved, and the efficient conductivity of the material is achieved. Improved mechanical properties.
Patent Information
- Application Number
- CN202411282490.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-08
AI Technical Summary
While improving antistatic properties, existing PC materials are difficult to improve their mechanical properties at the same time, especially due to poor compatibility with the conductive components and uneven dispersion of PCs.
The polymer particles are prepared by polymerization of vinyl benzylcinnamate copolymer and styrene by polymerization, and polyaniline fiber and nanographite powder are added during the polymerization process to form intersection Connecting structure and conductive network to enhance the compatibility and conductivity of the material.
The tensile performance, impact resistance and conductivity of PC materials are significantly improved. Through the mechanical performance transmission of the internal network structure and the insertion reaction of nanographite powder, the efficient conductivity and mechanical performance of the material are improved.
Smart Images

Figure BDA0005042092930000081
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of functional materials, and in particular to an antistatic PC material and a preparation method thereof. Background Art
[0002] Polycarbonate (refers to the general term for a class of polymers containing carbonate groups on the main chain of the molecule. According to the different main chain structures, it can be divided into aliphatic, cycloaliphatic and aromatic polycarbonates. As a widely used engineering plastic, polycarbonate has the following advantages: good optical transparency, high glass transition temperature, good toughness at room temperature, good dimensional stability, low water absorption, good flame retardancy and electrical insulation. It is widely used in the fields of electronic appliances, medical equipment, sports equipment, automotive parts and building materials. Although PC has a wide range of applications, research on PC has never stopped both academically and in the field of application. For the antistatic performance of PC, the conventional modification method is to directly add conductive components, but the direct addition of conductive components has poor compatibility with PC. If the added particles are too small, it also has the disadvantage of uneven dispersion. Therefore, further research on it is the focus of the present invention on how to improve its mechanical properties while improving the antistatic effect. Summary of the invention
[0003] Technical problem to be solved: The purpose of the present invention is to provide an antistatic PC material and a preparation method thereof, wherein antistatic microparticles are used as conductive fillers, the antistatic microparticles are particles with a three-dimensional network structure, azobisisobutyronitrile and cocamidopropyl betaine are used as initiators and dispersants, polymer microparticles are prepared by polymerization of vinylbenzyl cinnamate copolymer and styrene, and conductive components polyaniline fibers and nanographite powder are added. During the polymerization process, the microparticles obtain a cross-linked structure through the unsaturated hydrocarbons in the vinylbenzyl cinnamate copolymer. At the same time, the polyaniline fibers can further enhance the density of the cross-linked structure. The high degree of cross-linking structure and good compatibility with PC significantly improve the tensile properties and impact resistance of PC.
[0004] Technical solution: An antistatic PC material, comprising the following components by weight: 100 parts of PC particles, 5-20 parts of antistatic particles, and 1-5 parts of toughening agent. Furthermore, the particle size of the antistatic particles is 0.1-1 mm. Furthermore, the toughening agent includes one or more of Kane Ace M-577, Kane Ace FM-40, Kane Ace M-722 and Kane Ace M-732. The preparation method of the above antistatic PC material is as follows: S1: Take PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: taking out, premixing with antistatic particles and toughening agent, and then extruding and granulating to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine to obtain an antistatic PC material. Furthermore, in S2, the extrusion temperature is 200-250° C., and the screw speed is 300-350 rpm. Furthermore, in S3, the injection temperature is 260-280° C., the injection pressure is 50-70 MPa, and the mold temperature is 80-120° C. Furthermore, the preparation method of the antistatic particles is as follows, in parts by weight: S21: Take 10 parts of a mixture of vinylbenzylcinnamate copolymer and styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 0.5-1.5 parts of polyaniline fibers and 0.2-0.8 parts of nano-graphite powder, and stirring for 10-15 minutes to obtain a mixture; S23: Stir the mixture under N2 atmosphere for 30-40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. Furthermore, in the mixture of vinylbenzylcinnamate copolymer and styrene in S21, the mass ratio of vinylbenzylcinnamate copolymer to styrene is 1:(1-2). Furthermore, the diameter of the polyaniline fiber in S22 is 1-10 μm. Beneficial effects: 1. The present invention adopts antistatic microparticles as conductive fillers, the antistatic microparticles are particles with a three-dimensional network structure, azobisisobutyronitrile and cocamidopropyl betaine are used as initiators and dispersants, and polymer microparticles are prepared by polymerization of vinylbenzyl cinnamate copolymer and styrene, and conductive components polyaniline fiber and nanographite powder are added. The microparticles obtain a cross-linked structure through the unsaturated hydrocarbons in the vinylbenzyl cinnamate copolymer during the polymerization process, and the polyaniline fiber can further enhance the density of the cross-linked structure. The highly cross-linked structure and good compatibility with PC significantly improve the tensile properties and impact resistance of PC. 2. When the material of the present invention is subjected to stress, the stress is first transferred from the PC substrate to the antistatic microparticles, and then the antistatic microparticles transfer the stress to the nanographite powder particles through the internal network structure, dispersing the stress step by step, thereby improving the mechanical properties. 3. In the present invention, polyaniline fibers and nanographite powder are added to the antistatic particles, polyaniline forms a conductive network, and nanographite powder and polyaniline macromolecules can undergo insertion reaction to form graphite insertion compounds. The synergistic effect of the two can further improve the conductivity of the antistatic particles. DETAILED DESCRIPTION Example 1 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 5 parts of vinylbenzylcinnamate copolymer and 5 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 1 part of polyaniline fiber having a diameter of 1-10 μm and 0.6 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Example 2 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 1 part of polyaniline fiber having a diameter of 1-10 μm and 0.6 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Example 3 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 3.33 parts of vinylbenzylcinnamate copolymer and 6.66 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 1 part of polyaniline fiber having a diameter of 1-10 μm and 0.6 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Example 4 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 0.5 parts of polyaniline fibers having a diameter of 1-10 μm and 0.6 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Example 5 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 1.5 parts of polyaniline fibers having a diameter of 1-10 μm and 0.6 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Example 6 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 1 part of polyaniline fiber having a diameter of 1-10 μm and 0.2 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Example 7 A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 1 part of polyaniline fiber having a diameter of 1-10 μm and 0.8 parts of nano-graphite powder, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Comparative Example 1 The difference between this embodiment and embodiment 2 is that polyaniline fiber is used instead of nano graphite powder, as follows: A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.% and 1.6 parts of polyaniline fibers having a diameter of 1-10 μm, and stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Comparative Example 2 The difference between this embodiment and embodiment 2 is that nano graphite powder is used instead of polyaniline fiber, specifically as follows: A method for preparing antistatic particles is as follows, in parts by weight: S21: Take 4 parts of vinylbenzylcinnamate copolymer and 6 parts of styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine with a concentration of 1 wt.% and 1.6 parts of nano-graphite powder, stirring for 15 minutes to obtain a mixture; S23: The mixture was stirred under N2 atmosphere for 40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles. The particle size of the antistatic particles is 0.1-1 mm. Table 1 Conductivity (S / cm) <![CDATA[Impact strength (kJ / m 2 )]]> Example 1 <![CDATA[4.28×10 -3 ]]> 13.6 Example 2 <![CDATA[4.42×10 -3 ]]> 14.2 Example 3 <![CDATA[4.66×10 -3 ]]> 14.0 Example 4 <![CDATA[4.01×10 -3 ]]> 13.9 Example 5 <![CDATA[4.88×10 -3 ]]> 14.3 Example 6 <![CDATA[3.24×10 -3 ]]> 14.0 Example 7 <![CDATA[4.98×10 -3 ]]> 14.1 Comparative Example 1 <![CDATA[8.77×10 -10 ]]> 13.9 Comparative Example 2 <![CDATA[5.17×10 2 ]]> 7.8 After comprehensive consideration of the conductivity and mechanical properties of the antistatic particles, the antistatic particles prepared in Example 5 were selected for subsequent tests. Example 8 A method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with 5 parts of antistatic particles and 4 parts of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 250°C and a screw speed of 350 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 280° C., the injection molding pressure is 70 MPa, and the mold temperature is 120° C. to obtain an antistatic PC material. Example 9 A method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with 10 parts of antistatic particles and 4 parts of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 250°C and a screw speed of 350 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 280° C., the injection molding pressure is 70 MPa, and the mold temperature is 120° C. to obtain an antistatic PC material. Example 10 A method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with 15 parts of antistatic particles and 4 parts of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 250°C and a screw speed of 350 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 280° C., the injection molding pressure is 70 MPa, and the mold temperature is 120° C. to obtain an antistatic PC material. Embodiment 11 A method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with 20 parts of antistatic particles and 4 parts of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 250°C and a screw speed of 350 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 280° C., the injection molding pressure is 70 MPa, and the mold temperature is 120° C. to obtain an antistatic PC material. Example 12 A method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with 15 parts of antistatic particles and 1 part of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 200°C and a screw speed of 300 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 260° C., the injection molding pressure is 50 MPa, and the mold temperature is 80° C. to obtain an antistatic PC material. Example 13 A method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with 15 parts of antistatic particles and 5 parts of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 200°C and a screw speed of 300 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 260° C., the injection molding pressure is 50 MPa, and the mold temperature is 80° C. to obtain an antistatic PC material. Comparative Example 3 The difference between this embodiment and embodiment 10 is that the same amount of polyaniline fiber and nano graphite powder as in embodiment 10 are added. Specifically: a method for preparing an antistatic PC material, the preparation method is as follows: S1: Take 100 parts of PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: Take out, premix with polyaniline fiber, nano graphite powder and 4 parts of Kane Ace M-577 toughening agent, and then extrude and granulate at an extrusion temperature of 250°C and a screw speed of 350 rpm to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine. The injection molding temperature is 280° C., the injection molding pressure is 70 MPa, and the mold temperature is 120° C. to obtain an antistatic PC material. With reference to national standards, various properties of the antistatic PC materials prepared in various embodiments were tested. With reference to GB / T1410-2006, the volume resistance of the material was determined by a three-electrode method and converted into a corresponding resistivity value; with reference to GB / T 1843-2008, the notched impact strength of the cantilever beam of the test sample was tested, and a notch sample making machine was used to make a "V"-shaped notch with a notch depth of 2 mm, and the test was performed at room temperature; the test results are shown in Table 2 below: Table 2 The above embodiments are intended to provide a clear and complete description of the technical solution, and are partial implementations of the present invention, rather than all implementations. However, the implementations of the present invention are not limited to the above embodiments, and any other changes, modifications, substitutions, combinations or simplifications that do not deviate from the spirit and principle of the present invention shall be equivalent replacement methods and are included in the protection scope of the present invention.
Claims
1. An antistatic PC material, characterized in that: The composition comprises the following components in parts by weight: 100 parts of PC particles, 5-20 parts of antistatic particles and 1-5 parts of toughening agent.
2. The antistatic PC material according to claim 1, characterized in that: The particle size of the antistatic particles is 0.1-1 mm.
3. The antistatic PC material according to claim 1, characterized in that: The toughening agent includes one or more of Kane Ace M-577, Kane Ace FM-40, Kane Ace M-722 and Kane Ace M-732.
4. A method for preparing an antistatic PC material according to any one of claims 1 to 3, characterized in that: The preparation method is as follows: S1: Take PC particles, place them in an oven, and dry them at 110°C for 4 hours; S2: taking out, premixing with antistatic particles and toughening agent, and then extruding and granulating to obtain pellets; S3: Dry the pellets and perform injection molding using an injection molding machine to obtain an antistatic PC material.
5. The method for preparing an antistatic PC material according to claim 3, characterized in that: In the S2, the extrusion temperature is 200-250°C, and the screw speed is 300-350rpm.
6. The method for preparing an antistatic PC material according to claim 3, characterized in that: In the S3, the injection temperature is 260-280°C, the injection pressure is 50-70MPa, and the mold temperature is 80-120°C.
7. The method for preparing an antistatic PC material according to claim 3, characterized in that: The preparation method of the antistatic particles is as follows, in parts by weight: S21: Take 10 parts of a mixture of vinylbenzylcinnamate copolymer and styrene, add 0.5 parts of azobisisobutyronitrile, and dissolve in 20 parts of dichloromethane; S22: adding 500 parts of an aqueous solution of cocamidopropyl betaine having a concentration of 1 wt.%, 0.5-1.5 parts of polyaniline fibers and 0.2-0.8 parts of nano-graphite powder, and stirring for 10-15 minutes to obtain a mixture; S23: Stir the mixture under N2 atmosphere for 30-40 min; S24: After degassing for 30 min, polymerization was carried out by stirring for 18 h at 70 °C and 300 rpm in a N2 atmosphere; S25: centrifugation to remove excess azobisisobutyronitrile and cocamidopropyl betaine, and washing with deionized water; S26: Freeze-drying to obtain antistatic microparticles.
8. The method for preparing an antistatic PC material according to claim 7, characterized in that: The mass ratio of the vinylbenzylcinnamate copolymer to styrene in the mixture of the vinylbenzylcinnamate copolymer and styrene in S21 is 1:(1-2).
9. The method for preparing an antistatic PC material according to claim 7, characterized in that: The diameter of the polyaniline fiber in S22 is 1-10 μm.