Prefabricated ink, lens, lens printing method and electronic equipment
Through the specific ratio and hierarchy of prefabricated ink, the space waste and complex process problems of light filtration design of infrared and post-light sensor devices in the prior art are solved, and the selective transmission of infrared and visible light is realized, and the printing process is simplified. And reduce costs.
Patent Information
- Application Number
- CN202411406359.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the existing design, the light required for infrared and rear-mounted photosensitive devices is filtered on the glass and the screen printing ink respectively, resulting in waste of glass space and complicated processes, and cannot meet the transmission needs of infrared and visible light at the same time.
Provided is a preformed ink, including colored ink, ink defoaming agent, dilution solvent and curing agent. By mixing ink of a specific proportion, it is used for the screen printing process of the glass cover plate to form an outer ring ink layer, a preformed ink layer and a cover bottom ink. layer, realizes selective transmission of infrared and visible light.
Under the limitation of stacking space, an ink is used to meet the needs of infrared light transmittance greater than 90% in the 940nm band and the 550nm band transmittance 0.2%~1.1% in the 550nm band. There is no need for additional holes and multiple printings, saving lens space. Facilitate the miniaturization of lenses.
Smart Images

Figure CN118909485A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the technical field of ink printing, and in particular to a prefabricated ink, a lens, a lens printing method, and an electronic device. Background Art
[0002] In our daily lives, mobile phones have become an essential electronic device. The main plane of the mobile phone lens and the camera hole have transmittance index requirements. The transmittance of light determines the sensitivity of the sensor. Printing IR (Infrared Ray) ink on the sheet can achieve selective transmission of near-infrared light.
[0003] In recent years, mobile phones have been equipped with infrared and rear photosensitive devices. The wavelength of light that can be sensed by the rear photosensitive device is different from that of infrared light. Therefore, in the existing design, IR holes are opened on the glass respectively for the light required by the infrared and rear photosensitive devices, and corresponding inks are screen-printed respectively to filter the light of the corresponding wavelengths. This wastes a lot of glass space and requires multiple printings, and the process is relatively complicated. Summary of the invention
[0004] In order to solve the above technical problems, the present invention provides a prefabricated ink, a lens, a lens printing method, and an electronic device. By preparing a new ink, there is no need to open a separate hole for the rear photosensitive device, while meeting the infrared transmission and light sensing requirements, saving glass space.
[0005] In a first aspect, an embodiment of the present disclosure provides a prefabricated ink, which is applied to a screen printing process of a glass cover plate having a photosensitive hole, wherein the prefabricated ink comprises, by mass percentage: 70%-74% of a colored ink, 2%-4% of an ink defoamer, 8%-10% of a diluent solvent, and 14%-16% of a curing agent; wherein the colored ink comprises isophorone and an acrylic resin; Optionally, the prefabricated ink comprises, by mass percentage: 72% of colored ink, 3% of ink defoamer, 10% of diluent, and 15% of curing agent; In some embodiments, the ink defoamer includes methanol and ethanol; In some embodiments, the diluent solvent comprises isophorone; In some embodiments, the curing agent includes ethyl acetate.
[0006] In a second aspect, an embodiment of the present disclosure provides a lens, comprising: a substrate and an outer ring ink layer, a prefabricated ink layer and a cover bottom ink layer provided on the same surface of the substrate; Wherein, the prefabricated ink layer is formed by curing the prefabricated ink described in the first aspect; The outer ring ink layer and the prefabricated ink layer are located in the same layer; The cover bottom ink layer at least partially covers the outer circle ink layer and the prefabricated ink layer.
[0007] Optionally, the outer circle ink layer, the prefabricated ink layer and the bottom cover ink layer all have the center of the substrate as the center of the circle; The outer ring ink layer is annular, the prefabricated ink layer is circular, the circular shape corresponding to the prefabricated ink layer is located inside the circular shape corresponding to the outer ring ink layer, and there is a gap between the two; The bottom cover ink layer is in a double ring shape, including an inner ring and an outer ring, wherein the inner ring at least partially covers the prefabricated ink layer, and the outer ring at least partially covers the outer ring ink layer.
[0008] Optionally, the outer diameter of the outer ring ink layer is 13.5 mm, and the inner diameter is 10.2 mm; the diameter of the prefabricated ink layer is 7.7 mm; the outer diameter of the inner ring in the bottom cover ink layer is 7.7 mm, the inner diameter of the inner ring is 5.1 mm, the outer diameter of the outer ring is 13.5 mm, and the inner diameter of the outer ring is 10.2 mm.
[0009] Optionally, the ink in the outer circle ink layer includes epichlorohydrin copolymer, and the ink in the bottom cover ink layer is high-godarin black oil.
[0010] In a third aspect, the present disclosure provides a lens printing method for preparing the lens according to the second aspect, comprising: Take a glass middle sheet, use a printing machine to print an outer circle ink layer on a plurality of single lens lenses on the glass middle sheet, and then perform a first baking; After the outer circle ink layer is solidified, a prefabricated ink layer is printed on the same layer of the outer circle ink layer and then baked for the second time; After the prefabricated ink layer is cured, a cover ink layer is printed on a plurality of single lens elements in the glass middle sheet and then baked for the third time.
[0011] Optionally, when printing the pre-made ink layer, when a new glass sheet is printed and the printing machine has been running for a cycle of 40-60 minutes, the remaining pre-made ink on the screen printing screen is collected and weighed; Add an appropriate amount of diluent according to the weight of the remaining pre-made ink and the diluent at a ratio of 1: (3-5), stir thoroughly, and then pour into the screen printing screen to continue printing.
[0012] Optionally, when printing the outer ring ink layer, the preformed ink layer and the cover bottom ink layer: The parameters of the printing machine are set to a scraper angle of 80°, a scraper glue hardness of 70-80 degrees, and a printing speed of 150-200 mm / s.
[0013] Optionally, the baking temperatures of the first baking and the second baking are both 155° C.-165° C., and the baking time is both 10 minutes; the baking temperature of the third baking is 155° C.-165° C., and the baking time is 60 minutes.
[0014] In a fourth aspect, an embodiment of the present disclosure provides an electronic device, comprising a lens as described in the second aspect.
[0015] Compared with the prior art, the technical solution provided by the embodiments of the present disclosure has the following advantages: 1. Under the limitation of stacking space, one ink is used to meet the requirements of infrared light transmittance greater than 90% in the 940nm band and light-sensitive light transmittance of 0.2%~1.1% in the 550nm band.
[0016] 2. There is no need to open additional holes on the lens for the rear light sensor, and there is no need to print another type of ink to allow visible light to pass through, which saves lens space and facilitates the miniaturization of the lens. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments consistent with the present disclosure and, together with the description, serve to explain the principles of the present disclosure.
[0018] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0019] Figure 1 This is a schematic diagram of the shapes and relative positions of the ink layers of the lens according to the embodiment of the present disclosure; Figure 2 This is a schematic diagram of the arrangement of single lens particles in the glass sheet according to the embodiment of the present disclosure; Figure 3 This is a lens printing flow chart according to an embodiment of the present disclosure. DETAILED DESCRIPTION
[0020] In order to more clearly understand the above-mentioned objectives, features and advantages of the present disclosure, the scheme of the present disclosure will be further described below. It should be noted that the embodiments of the present disclosure and the features in the embodiments can be combined with each other without conflict.
[0021] In the following description, many specific details are set forth to facilitate a full understanding of the present disclosure, but the present disclosure may also be implemented in other ways different from those described herein; it is obvious that the embodiments in the specification are only part of the embodiments of the present disclosure, rather than all of the embodiments.
[0022] In a first aspect, the present disclosure provides a prefabricated ink for use in a silk-screen printing process of a glass cover plate having photosensitive holes. The prefabricated ink is formed by mixing a colored ink, an ink defoamer, a diluent solvent, and a curing agent. The prefabricated ink comprises, by mass percentage: 70%-74% of a colored ink, 2%-4% of an ink defoamer, 8%-10% of a diluent solvent, and 14%-16% of a curing agent.
[0023] In some embodiments, illustratively, the colored ink accounts for 70%-74% of the overall mass of the prefabricated ink. Optionally, the colored ink accounts for 70%-72%, 71%-73%, 72%-74%... and so on, which are not listed here one by one, and it is only necessary to satisfy that the colored ink accounts for 70%-74% of the overall mass of the prefabricated ink; the colored ink includes isophorone and acrylic resin. In some embodiments, illustratively, the composition of the colored ink is shown in Table 1 below.
[0024] Table 1:
[0025] In some embodiments, the ink defoamer accounts for 2%-4% of the total mass of the prefabricated ink, and optionally, the ink defoamer accounts for 2.5%-3.5%, 2%-3%, 3%-3.5%, 3%-4%... and so on. They are not listed here one by one. It is only necessary to satisfy that the ink defoamer accounts for 2%-4% of the total mass of the prefabricated ink. In some embodiments, the ink defoamer includes methanol and ethanol. For example, the composition of the colored ink is shown in Table 2 below. When the ink defoamer accounts for more than 4% of the total mass of the prefabricated ink, excessive ink defoamer may cause problems such as reduced fluidity, color change or uneven coating of the prefabricated ink. When the ink defoamer accounts for less than 2% of the total mass of the prefabricated ink, the foam in the ink cannot be effectively eliminated, thereby affecting the quality of the printed product. When the ink defoamer accounts for 2%-4% of the total mass of the prefabricated ink, the foam in the prefabricated ink can be eliminated without causing problems such as uneven coating or reduced fluidity, which is beneficial to the subsequent printing of the prefabricated ink and improves product quality.
[0026] Table 2:
[0027] In some embodiments, illustratively, the dilution solvent accounts for 8%-10% of the total mass of the prefabricated ink. Optionally, the dilution solvent accounts for 8%-8.5%, 8.5%-9%, 10%-10.5%, 9.5%-10% of the total mass of the prefabricated ink, etc., which are not listed here one by one, and it is only necessary to satisfy that the dilution solvent accounts for 8%-10% of the total mass of the prefabricated ink; in some embodiments, the dilution solvent includes isophorone, and illustratively, the composition of the dilution solvent is shown in Table 3; when the dilution solvent accounts for more than 10% of the total mass percentage of the prefabricated ink, excessive addition of the dilution solvent will cause changes in the color and pH value of the ink, reduce the viscosity of the prefabricated ink, increase the fluidity, and lose the covering power due to being too thin. When the dilution solvent accounts for less than 8% of the total mass percentage of the prefabricated ink, the prepared prefabricated ink has a high viscosity and is too thick, resulting in uneven printing. When the dilution solvent accounts for 8%-10% of the total mass of the prefabricated ink, the prefabricated ink can be at a suitable viscosity and good fluidity, which is conducive to the subsequent printing of the prefabricated ink and improves product quality.
[0028] Table 3:
[0029] In some embodiments, the curing agent exemplarily accounts for 14%-16% of the total mass of the prefabricated ink. Optionally, the curing agent accounts for 14%-15%, 14.5%-15.5%, 15%-16%, 15.5%-16%... and so on. They are not listed here one by one. It is only necessary to satisfy that the curing agent accounts for 14%-16% of the total mass of the prefabricated ink. In some embodiments, the curing agent includes ethyl acetate. Exemplarily, the composition of the curing agent is shown in Table 4. When the curing agent accounts for 100% of the total mass of the prefabricated ink, When the fraction is greater than 16%, excess curing agent will harden the surface of the prefabricated ink, while the interior of the prefabricated ink is not fully dried and cured, and cracking is likely to occur. When the curing agent accounts for less than 14% of the overall mass of the prefabricated ink, too little curing agent will reduce the elasticity and flexibility of the prefabricated ink and increase the risk of cracking after the prefabricated ink hardens. When the curing agent accounts for 14%-16% of the overall mass of the prefabricated ink, the prefabricated ink can be in a suitable elasticity and flexibility, and cured evenly, which is conducive to the subsequent printing of the prefabricated ink and improves product quality.
[0030] Table 4:
[0031] In some embodiments, for example, the prefabricated ink includes, by mass percentage, 72% colored ink, 3% ink defoamer, 10% diluent, and 15% curing agent; in some embodiments, for example, the colored ink is Seiko HF GV3 series and model 2302-2014C; the ink defoamer is Seiko CARE 73N defoamer; the diluent is Seiko T-980 series diluent, and the curing agent is Seiko A hardener. The prefabricated ink prepared in this proportion can achieve an infrared transmittance of greater than 90% at a wavelength of 940nm and a visible light transmittance of 0.2% to 1.1% at a wavelength of 550nm accepted by the post-photosensitive device.
[0032] Figure 1 This is a schematic diagram of the shapes and relative positions of the ink layers of the lens according to the embodiment of the present disclosure. Figure 2 This is a schematic diagram of the arrangement of single lens elements in the glass sheet according to the embodiment of the present disclosure. Figure 3 Please refer to the lens printing process diagram of the embodiment of the present disclosure. Figures 1 to 3 The light transmittance of the lens 50 printed with the prefabricated ink provided in the embodiment of the present disclosure is shown in Table 5: Table 5:
[0033]
[0034] Please refer to Table 5 and Figures 1 to 3 Table 5 shows 6 sheets of glass middle sheets 60 printed with the prefabricated ink provided by the present disclosure. Figure 2 The 10 determined areas shown are tested. It can be seen from Table 5 that the present disclosure provides 6 groups of verification data on the light transmittance of lenses 50 at wavelengths of 550nm and 940nm, which are made of prefabricated inks with different component contents. From the experimental data, it can be seen that only by opening a hole once and printing the 6 groups of different prefabricated inks in Table 5 provided by the present disclosure, the requirements of a transmittance of infrared light at 940nm band greater than 90% and a transmittance of light at 550nm band of 0.2%~1.1% can be achieved on a piece of lens 50. The number of hole openings and the number of ink printings are reduced while achieving selective transmission of infrared light and visible light, which is beneficial to reducing costs and realizing mass production of lenses 50.
[0035] It should be noted that Figure 2 The arrangement and number of the single lens elements 61 in the glass middle sheet 60 do not represent the arrangement and number of the single lens elements 61 in actual production. They are for illustration only and the specific situation shall be subject to actual production.
[0036] The present disclosure also provides a comparative example 1. In the comparative example 1, when the colored ink does not include isophorone and acrylic resin, a comparative colored ink (such as melamine-based ink) is used to replace the colored ink in the present disclosure, and the contents of other components remain unchanged to prepare the comparative ink. The full inspection data of the printed glass sheet 60 is shown in Table 6: Table 6:
[0037] As can be seen from Table 6, the present disclosure provides a set of comparative inks, which include 71% comparative colored ink, 4% ink defoamer, 9% diluent, and 16% curing agent, wherein the comparative colored ink is a melamine-based ink, that is, the comparative colored ink does not include isophorone and acrylic resin. In the glass middle sheet 60 provided in Comparative Example 1, 10 samples of lenses 50 printed by single-grain lenses 61 are taken, and the 10 sample lenses are tested. It is detected that the transmittance of the 10 sample lenses at a wavelength of 940nm is all less than 90%, and the transmittance of the light at a wavelength of 550nm is all between 5-8%. By comparing the experimental data measured in Table 5 and Table 6, it is found that When the colored ink does not include isophorone and acrylic resin, it cannot meet the requirements that the transmittance of all sample lenses 50 in the 940nm infrared light band is greater than 90% and the transmittance of light in the 550nm band is 0.2%~1.1%. However, it can be seen from Table 5 that the lenses 50 printed with the prefabricated ink containing isophorone and acrylic resin all meet the requirements that the transmittance of the infrared light in the 940nm band is greater than 90% and the transmittance of light in the 550nm band is 0.2%~1.1%. This shows that the prefabricated ink provided in the present disclosure that contains isophorone and acrylic resin components and has a specific ratio can meet the needs of solving the above problems.
[0038] The present disclosure also provides a comparative example 2. In the comparative example 2, when the amount of diluent added is greater than 10%, the full inspection data of the printed glass middle sheet 60 is shown in Table 7: Table 7:
[0039]
[0040] Comparative Example 2 is a glass middle sheet 60 printed with an excessive amount of prefabricated ink added to a dilute solvent. Each lens 50 printed from a single lens 61 in the glass middle sheet 60 is tested. As shown in Table 7, 44 samples of lenses 50 printed from the single lens 61 are taken from the glass middle sheet 60 provided in Comparative Example 2. After testing these 44 sample lenses, it is found that 15 of the sample lenses have a transmittance of less than 90% at a wavelength of 940 nm. That is, the yield of the lens 50 printed with an excessive amount of prefabricated ink added to a dilute solvent having a transmittance of more than 90% at a wavelength of 940 nm is about 66%. The experimental results measured in Tables 5 and 7 show that the transmittance of the lens 50 printed from the single lens 61 is less than 90%. Comparison of the data shows that when the amount of diluent added is greater than 10% of the mass percentage of the prefabricated ink, the requirements that the transmittance of all sample lenses 50 in the 940nm infrared band is greater than 90% and the transmittance of light in the 550nm band is 0.2%~1.1% cannot be met. However, in the present invention, the lenses 50 printed by prefabricated ink with an added amount of diluent of 8%-10%, all the sample lenses 50 experimentally measured meet the requirements that the transmittance of infrared light in the 940nm band is greater than 90% and the transmittance of light in the 550nm band is 0.2%~1.1%, which indicates that the ratio of the prefabricated ink in the present invention is precisely controlled and the amount of diluent added is appropriate.
[0041] The prefabricated ink provided by the present disclosure is in a liquid form with a certain fluidity at room temperature, and can form a stable solid form after screen printing and heating and curing.
[0042] It should be noted that the order of adding various raw materials can be, but is not limited to, the process of first adding the colored ink, then adding the ink defoamer, the diluent solvent, and the curing agent. Alternatively, the order of adding various raw materials is the process of first adding the colored ink, the ink defoamer, the diluent solvent, and then adding the curing agent.
[0043] The prefabricated ink provided by the present invention has a simple preparation process and can be used for large-scale industrial production. The prefabricated ink prepared by the above-mentioned ratio has suitable viscosity, good fluidity and stable properties. The prefabricated ink layer formed after the prefabricated ink is cured has the characteristics of uniform film layer, strong adhesion and not easy to crack. The prefabricated ink layer can meet the light transmittance of 940nm infrared light of more than 90%, and can also achieve a transmittance of 0.2%~1.1% of 550nm visible light with acceptable post-photosensitivity.
[0044] Please continue to refer to Figures 1 to 3 In a second aspect, an embodiment of the present disclosure provides a lens 50, which includes a substrate 10, and the substrate 10 includes but is not limited to a circular shape. The lens 50 also includes an outer ring ink layer 20, a prefabricated ink layer 30 and a bottom cover ink layer 40 located on the same surface of the substrate 10; wherein the prefabricated ink layer 30 is formed by curing the prefabricated ink as described above.
[0045] In some embodiments, illustratively, the outer circle ink layer 20 and the prefabricated ink layer 30 are located in the same layer on the same surface of the substrate 10, and the cover bottom ink layer 40, the outer circle ink layer 20 and the prefabricated ink layer 30 are located in different layers on the same surface of the substrate 10; in a direction perpendicular to the plane of the substrate 10, the outer circle ink layer 20 and the prefabricated ink layer 30 do not overlap, the cover bottom ink layer 40 at least partially overlaps with the outer circle ink layer 20, and the cover bottom ink layer 40 at least partially overlaps with the prefabricated ink layer 30; after the outer circle ink layer 20 and the prefabricated ink layer 30 are cured, when the cover bottom ink layer 40 is printed, the cover bottom ink layer 40 at least partially covers the outer circle ink layer 20, and the cover bottom ink layer 40 at least partially covers the prefabricated ink layer 30.
[0046] It should be noted that the prefabricated ink layer 30 is formed by curing the prefabricated ink mentioned above on the surface of the substrate 10 through screen printing.
[0047] In some embodiments, illustratively, the outer circle ink layer 20 and the prefabricated ink layer 30 are located in the same layer of the same surface of the substrate 10, and the cover bottom ink layer 40 and the outer circle ink layer 20 and the prefabricated ink layer 30 are located in different layers of the same surface of the substrate 10; the outer circle ink layer 20 is annular, the prefabricated ink layer 30 is circular, and the cover bottom ink layer 40 is double annular, wherein the ring corresponding to the outer circle ink layer 20, the circle corresponding to the prefabricated ink layer 30, and the double annular shape corresponding to the cover bottom ink layer 40 all take the center of the substrate 10 as the center; the circle corresponding to the prefabricated ink layer 30 and the ring corresponding to the outer circle ink layer 20 are located in the same layer of the same surface of the substrate 10, and the circle corresponding to the prefabricated ink layer 30 is located inside the ring corresponding to the outer circle ink layer 20, and in the direction perpendicular to the plane where the substrate 10 is located, the prefabricated ink layer 30 and the outer circle ink layer 20 do not overlap, that is, in the direction parallel to the plane where the substrate 10 is located, there is a gap between the prefabricated ink layer 30 and the outer circle ink layer 20.
[0048] Please continue to refer to Figures 1 to 3 The double ring shape of the bottom ink layer 40 includes an inner ring 41 and an outer ring 42. In a direction perpendicular to the plane where the substrate 10 is located, the bottom ink layer 40 at least partially overlaps with the prefabricated ink layer 30 and the outer ring ink layer 20. That is, in a direction perpendicular to the plane where the substrate 10 is located, the inner ring 41 of the bottom ink layer 40 at least partially covers the prefabricated ink layer 30, and the outer ring 42 of the bottom ink layer 40 at least partially covers the outer ring ink layer 20. In this way, by printing the prefabricated ink layer 30 only once, the lens 50 that allows light to pass through the 940nm band and the 550nm band can be satisfied. Compared with the conventional technology of printing one ink for infrared light transmission and another ink for visible light transmission, the printing process of the lens 50 provided by the embodiment of the present disclosure is simple, no multiple printings are required, and there is no positioning problem in subsequent assembly.
[0049] In some embodiments, for example, the outer diameter of the ring corresponding to the outer circle ink layer 20 is 13.5 mm, and the inner diameter is 10.2 mm; the diameter of the circle corresponding to the prefabricated ink layer 30 is 7.7 mm; the outer diameter of the inner ring 41 in the double ring corresponding to the bottom ink layer 40 is 7.7 mm, and the inner diameter of the inner ring 41 is 5.1 mm; the outer diameter of the outer ring 42 in the double ring corresponding to the bottom ink layer 40 is 13.5 mm, and the inner diameter of the outer ring 42 is 10.2 mm.
[0050] In some embodiments, for example, the ink in the outer circle ink layer 20 includes epichlorohydrin copolymer, and optionally, the ink in the outer circle ink layer 20 is Seiko CE 501T series ink; the ink in the bottom cover ink layer 40 is high-value black oil, which can enhance adhesion, block light, and reduce cross-talk.
[0051] Please continue to refer to Figures 1 to 3 In a third aspect, the present disclosure provides a lens 50 printing method for preparing the lens 50 as described above; in some embodiments, illustratively, the lens 50 printing method is as follows: Step S1 specifically comprises taking a glass middle piece 60, the glass middle piece 60 comprising a plurality of single-grain lenses 61 arranged in an array, and printing an outer ring ink layer 20 on the plurality of single-grain lenses 61 on the glass middle piece 60 through a printing machine, and performing a first baking after printing is completed, the first baking temperature is 155°C-165°C, and the baking time is 10 minutes.
[0052] Step S2 specifically includes, after the outer ring ink layer 20 printed on the single-particle lens 61 is cured, printing a prefabricated ink layer 30 on the same layer of the same surface as the outer ring ink layer 20 on the single-particle lens 61, the ink of the prefabricated ink layer 30 is prepared by the prefabricated ink described in the first aspect, and a second baking is performed after the prefabricated ink layer 30 is printed, the temperature of the second baking is 155°C-165°C, and the baking time is 10 minutes.
[0053] Step S3 specifically includes, after the prefabricated ink layer 30 printed on the substrate 10 is cured, printing the cover ink layer 40 on the surface of the outer circle ink layer 20 and the prefabricated ink layer 30 on the substrate 10, and performing a third baking after the printing of the cover ink layer 40 is completed. The baking temperature of the third baking is 155°C-165°C, and the baking time is 60 minutes.
[0054] In some embodiments, for example, when printing the outer ring ink layer 20, the prefabricated ink layer 30 and the bottom cover ink layer 40, the parameters of the printing machine are a scraper angle of 80°, a scraper glue hardness of 70-80 degrees, and a printing speed of 150-200 mm / s. In this way, the lens 50 obtained by the lens printing method described in the third aspect can meet the requirements of infrared and post-light sensing functions at the same time without the need for additional separate openings and separate printing of different types of inks.
[0055] In some embodiments, for example, when printing a pre-made ink layer, when a new glass sheet is printed and the printing machine has been running for a cycle of 40-60 minutes, the remaining pre-made ink on the screen printing screen is collected and weighed; an appropriate amount of diluent is added according to the weight of the remaining pre-made ink and the diluent at a ratio of 1: (3-5), and after being fully stirred, it is poured into the screen printing screen to continue printing. It is understandable that in actual production, after a certain amount of prefabricated ink is added to the printing machine, the certain amount of prefabricated ink is used to print multiple glass sheets. When the printing number of the printing machine reaches a certain range, the prefabricated ink in the printing machine will become thick. At this time, the prefabricated ink will block the screen holes. It is necessary to add an appropriate amount of diluent to reduce the viscosity of the prefabricated ink at this time to ensure smooth printing. That is to say, when printing the prefabricated ink layer, when printing to a new glass sheet and the working time of the printing machine for printing the prefabricated ink layer has reached 40-60 minutes per cycle, it is necessary to collect the remaining prefabricated ink on the silk screen, weigh it, and add an appropriate amount of diluent. It is understandable that the time for collecting the remaining prefabricated ink is after each printing cycle of 40 minutes, 45 minutes, 50 minutes, 55 minutes or 60 minutes. They are not listed here one by one, and the present disclosure does not limit the collection time. Optionally, the amount of diluent added is required to be: the diluent is added at a ratio of 1:3 or 1:3.5 or 1:4 or 1:4.5 or 1:5 to the weight of the remaining pre-made ink and the added diluent. The specific amount of diluent added can be added according to actual conditions and is not listed here one by one. In some embodiments, for example, an anti-fouling layer is coated on one side of the single-lens lens 61 that is not printed with ink. For example, the material of the anti-fouling layer can be a material with low surface energy such as silicone and organic fluorine material, which can play an anti-fingerprint and anti-fouling role.
[0056] It should be noted that after the printing process is completed and the coating is performed, the single lens 61 can be split from the glass middle piece 60 to obtain the lens 50 described in the second aspect.
[0057] It should be noted that the substrate 10 herein includes but is not limited to a single lens 61 .
[0058] In a fourth aspect, the present disclosure provides an electronic device, comprising the lens 50 as described above.
[0059] In some embodiments, exemplarily, the lens 50 described in the second aspect is installed on an electronic device, and the electronic device includes but is not limited to a mobile phone, a tablet, smart glasses, a smart watch, a car central control screen, etc., wherein the side of the lens 50 printed with the prefabricated ink layer 30 faces the inside of the electronic device, and the side of the lens 50 coated with the anti-fouling layer faces the outside of the electronic device.
[0060] In summary, the embodiments of the present disclosure provide a prefabricated ink, a lens, a lens printing method, and an electronic device, wherein the prefabricated ink comprises: 70%-74% of colored ink, 2%-4% of ink defoaming agent, 8%-10% of diluting solvent, and 14%-16% of curing agent; the colored ink comprises isophorone and acrylic resin; the ink defoaming agent comprises methanol and ethanol; the diluting solvent comprises isophorone; the curing agent comprises ethyl acetate; experimental data verify that the prefabricated ink prepared in this way can simultaneously meet the requirements of infrared light transmittance of 940nm band being greater than 90% and light sensitivity of 550nm band transmittance of 0.2%~1.1%; the lens printed with the prefabricated ink provided by the present disclosure only needs to print the prefabricated ink once to simultaneously meet the transmittance of light in the 940nm and 550nm bands, the manufacturing process is simple, and the number of printing times is reduced; the electronic device obtained by using the lens provided by the present disclosure does not need to open a separate hole for the rear photosensitive device of the electronic device, thereby reducing the manufacturing process and reducing the production cost.
[0061] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0062] The above description is only a specific embodiment of the present disclosure, so that those skilled in the art can understand or implement the present disclosure. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present disclosure. Therefore, the present disclosure will not be limited to the embodiments described herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A prefabricated ink, characterized in that: Applied to the silk-screen printing process of the glass cover plate with photosensitive holes, the prefabricated ink includes, by mass percentage: 70%-74% of colored ink, 2%-4% of ink defoamer, 8%-10% of diluent solvent, and 14%-16% of curing agent; wherein the colored ink includes isophorone and acrylic resin.
2. The prefabricated ink according to claim 1, characterized in that: The prefabricated ink comprises, by mass percentage, 72% of colored ink, 3% of ink defoamer, 10% of diluent, and 15% of curing agent; wherein: the ink defoamer comprises methanol and ethanol; the diluent comprises isophorone; and the curing agent comprises ethyl acetate.
3. A lens, characterized in that: include: A substrate and an outer ring ink layer, a prefabricated ink layer and a cover bottom ink layer arranged on the same surface of the substrate; Wherein, the prefabricated ink layer is formed by curing the prefabricated ink according to claim 1 or 2; The outer ring ink layer and the prefabricated ink layer are located in the same layer; The cover bottom ink layer at least partially covers the outer circle ink layer and the prefabricated ink layer.
4. The lens according to claim 3, characterized in that: The outer circle ink layer, the prefabricated ink layer and the bottom cover ink layer all have the center of the substrate as the center of the circle; The outer ring ink layer is annular, the prefabricated ink layer is circular, the circular shape corresponding to the prefabricated ink layer is located inside the circular shape corresponding to the outer ring ink layer, and there is a gap between the two; The bottom cover ink layer is in a double ring shape, including an inner ring and an outer ring, wherein the inner ring at least partially covers the prefabricated ink layer, and the outer ring at least partially covers the outer ring ink layer.
5. The lens according to claim 4, characterized in that: The outer diameter of the outer ring ink layer is 13.5mm, and the inner diameter is 10.2mm; the diameter of the prefabricated ink layer is 7.7mm; the outer diameter of the inner ring in the bottom cover ink layer is 7.7mm, and the inner diameter of the inner ring is 5.1mm; the outer diameter of the outer ring is 13.5mm, and the inner diameter of the outer ring is 10.2mm.
6. The lens according to claim 3, characterized in that: The ink in the outer circle ink layer includes epichlorohydrin copolymer, and the ink in the bottom cover ink layer is high-end black oil.
7. A lens printing method, characterized in that: Used to prepare the lens according to any one of claims 3 to 6, comprising: Take a glass middle sheet, use a printing machine to print an outer circle ink layer on a plurality of single lens lenses on the glass middle sheet, and then perform a first baking; After the outer circle ink layer is solidified, a prefabricated ink layer is printed on the same layer of the outer circle ink layer and then baked for the second time; After the prefabricated ink layer is cured, a cover ink layer is printed on a plurality of single lens elements in the glass middle sheet and then baked for the third time.
8. The lens printing method according to claim 7, characterized in that: When printing the pre-made ink layer, when printing a new glass middle sheet and the printing machine has been running for a cycle of 40-60 minutes, collect and weigh the remaining pre-made ink on the screen printing screen; Add an appropriate amount of diluent according to the weight of the remaining pre-made ink and the diluent at a ratio of 1: (3-5), stir thoroughly, and then pour into the screen printing screen to continue printing.
9. The lens printing method according to claim 7, characterized in that: When printing the outer ring ink layer, the prefabricated ink layer and the bottom cover ink layer: set the parameters of the printing machine to 80° scraper angle, 70-80° scraper hardness and 150-200 mm / s printing speed; The baking temperatures of the first baking and the second baking are both 155° C.-165° C., and the baking time is both 10 minutes; the baking temperature of the third baking is 155° C.-165° C., and the baking time is 60 minutes.
10. An electronic device, characterized in that: Comprising the lens as described in any one of claims 3-6.
Citation Information
Patent Citations
Infrared light sensitive transparent ink and preparation method thereof
CN103450741A
IR baking type light guiding and brightening optical emulsion and preparation method thereof
CN113308145A
Infrared glass
CN215678831U
decorative sheet
JP3205986U
Ink composition for screen printing and method of manufacturing pattern using the same
KR1020110057309A