Preparation method of 5000MHz ultra-high frequency communication network cable
By using laser welding of a three-layer insulation structure (skin-foam-skin) and an L-shaped aluminum foil shielding layer, the problems of signal distortion and crosstalk in communication network cables at high frequencies were solved, achieving low-cost and high-efficiency 5000MHz ultra-high frequency transmission.
Patent Information
- Application Number
- CN202410990525.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-08
AI Technical Summary
Existing communication network cables suffer from signal distortion spikes and crosstalk problems when transmitting at high frequencies, and traditional shielding structures are complex and costly, making them unsuitable for civilian use.
It adopts a three-layer insulation structure of skin-foam-skin and an L-shaped aluminum foil shielding layer. The gaps in the aluminum foil are sealed by laser welding. Combined with XY dual-axis laser outer diameter control and twisted tension monitoring, it ensures full signal enclosure and low-cost production.
It achieves high-speed transmission at an ultra-high frequency of 5000MHz, reduces production costs, and improves transmission speed and electromagnetic interference resistance.
Smart Images

Figure CN118919182A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of preparation methods of communication network lines, and in particular to a preparation method of a 5000MHz ultra-high frequency communication network line. Background Art
[0002] Traditional communication network cables, such as Category 7e (transmission frequency 1000MHz) and Category 8 (transmission frequency 2000HMz), generally use a shielding structure, including a serrated sheath and a corrugated shielding cavity (similar to a corrugated tube). The serrated sheath solution is often used in ultra-high frequency network cables, but its frequency is limited. It can only guarantee transmission performance within the 1000Mhz frequency. If it exceeds this frequency, distortion spikes will appear. The corrugated shielding cavity solution consists of 4 pairs of core wires, each pair of core wires is wrapped with a thick aluminum foil corrugated shielding cavity. There is basically no crosstalk signal leakage. Due to the unevenness inside the corrugated cavity, the signal wave cannot penetrate the thick aluminum foil cavity and can only be continuously reflected in the corrugated cavity. The crosstalk signal is consumed inside, and has basically no effect on the other 3 pairs of core wires outside. The high frequency of this solution can reach 3000Mhz, but the process is too complicated, the aluminum foil needs to be very thick and the cost is very high, the production time is very long, and it is not economical. It is only suitable for small-scale military use and not for civilian use.
[0003] Moreover, in the traditional solution, after each pair of core wires is wrapped with aluminum foil, during the cabling process, due to the influence of the wire-winding tension, when the four pairs of core wires are wrapped with aluminum foil and twisted into a cable, the wrapped aluminum foil layer will be loose to a certain extent, and there will be gaps in the aluminum foil. Electromagnetic waves will be reflected in the shielding cavity, causing electromagnetic interference to the core wires, and easily generating distortion spikes to the shielding structure at the frequency of 1200-1700MHz.
[0004] In summary, in order to solve the deficiencies in the prior art, it is necessary to design a method for preparing a 5000 MHz ultra-high frequency communication network line with a simple structure. Summary of the invention
[0005] In order to solve the problems of the prior art, the present invention provides a method for preparing a 5000MHz ultra-high frequency communication network line.
[0006] The purpose of the present invention can be achieved by the following technical solution: A method for preparing a 5000MHz ultra-high frequency communication network line comprises the following steps:
[0007] S1: Wire drawing: The raw copper wire blank is stretched through a wire drawing machine to the required copper core diameter requirement of the communication network line;
[0008] S2: Insulation layer coating: The copper core after stretching is sent into the injection molding machine, the insulating raw material is heated and molten, and then coated on the copper core to form an insulation layer, so that the whole becomes the core wire of the communication network line, and then cooled through a long cooling water tank;
[0009] S3: Detwist and twist: The core wires are twisted and twisted in a combination of orange-white plus orange, blue-white plus blue, brown-white plus brown, and green-white plus green through a detwist and twist machine;
[0010] S4: Shielding layer coating: Wrap the four pairs of back-twisted twisted core wires with aluminum foil respectively, and laser weld the gaps of each group of aluminum foil wrappings and weld the aluminum foils on the outside of adjacent core wires by laser welding;
[0011] S5: Twisting the four pairs of aluminum foil wrapped core wires into a cable according to a certain twist length;
[0012] S6: Sheath coating: Wrap the twisted core wires with a sheath.
[0013] Further improvement, in step S2: the insulating layer is coated in the insulating layer, and the insulating layer includes an inner skin layer, a foaming layer and an outer skin layer. The insulating raw materials include high-density polyethylene masterbatch particles and foaming powder. The high-density polyethylene masterbatch particles are first heated to become a molten state, and are extruded by an injection molding machine and coated on the copper core to form an inner skin layer, and then sent to the injection molding machine again after cooling. The high-density polyethylene masterbatch particles and the foaming powder are again molten by an injection molding machine and are extruded by an injection molding machine and coated on the copper core to form a foaming layer, and then sent to the injection molding machine again after cooling. Finally, the high-density polyethylene masterbatch particles are heated to become a molten state, and are extruded by an injection molding machine and coated on the copper core to form an outer skin layer, and then sent out after cooling. The thickness and diameter of the inner skin layer, the foaming layer and the outer skin layer are not more than 1.5 mm.
[0014] As a further improvement, in step S2: the core wire in the insulation coating is monitored by an XY dual-axis laser outer diameter controller to control the core wire diameter tolerance within 3um, and to monitor the concentricity of the copper core and the insulation layer in the core wire.
[0015] As a further improvement, in the step S3: in the detwisting twisting, the detwisting twisting machine controls the lay length of each pair of twisted core wires to be uniform, and controls the double twist lay lengths between the four pairs of twisted core wires to be unequal.
[0016] As a further improvement, in the step S3: untwisting the twisting, a real-time monitoring system for the twisting tension is used, and feedback adjustment is made through the PLC to ensure that the tension during the twisting process is constant.
[0017] As a further improvement, the aluminum foil is of L-shaped structure, the thickness of the aluminum foil is not less than 0.012 mm, the wrapping overlap rate is not less than 25%, and a tinned round copper wire with a diameter of 0.5 mm is arranged inside the aluminum foil.
[0018] As a further improvement, the sheath material is a highly flame retardant, low smoke, halogen-free polyolefin material.
[0019] As a further improvement, an annealing process is performed on the copper core that has been stretched in step S1.
[0020] Compared with the prior art, the preparation method of the 5000MHz ultra-high frequency communication network line of the present invention is:
[0021] In the one-time cabling production process of four pairs of core wires in the present invention, while the four pairs of core wires are wrapped with aluminum foil at the same time, laser welding is adopted at the aluminum foil wrapping gap, so that the entire shielding cavity is round and smooth, the shielding cavity is fully closed, and there is no signal leakage. The signal wave cannot penetrate the thick aluminum foil cavity, and can only be continuously reflected in the cavity. The crosstalk signal is consumed inside, and has basically no effect on the other three pairs of core wires outside, so that the entire distortion peak is shifted to after 5000MHz, ensuring high-speed transmission within 5000MHz. Using thinner aluminum foil for laser welding can achieve a sealing effect, low cost and high economic benefit. The skin-foam-skin three-layer physical foaming technology is adopted, and the foaming degree reaches 60%. After the foaming insulation is adopted, the dielectric constant of the insulation can be greatly reduced, thereby achieving the effect of improving the propagation delay and increasing the transmission speed. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 The structural diagram of the network cable of the present invention is
[0023] In the figure, 1-copper core, 2-insulating layer, 21-inner skin layer, 22-foaming layer, 23-outer skin layer, 3-core wire, 4-aluminum foil, 5-sheath. DETAILED DESCRIPTION
[0024] In the description of the present invention, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they cannot be understood as limitations on the present invention.
[0025] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected" and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0026] The following is combined with the embodiments and attached Figure 1 , the technical solution of the present invention is further elaborated.
[0027] Example 1
[0028] A method for preparing a 5000 MHz ultra-high frequency communication network line comprises the following steps:
[0029] S1: Wire drawing: The raw copper wire blank is stretched through a wire drawing machine to the required diameter requirement of the copper core 1 of the communication network line;
[0030] S2: Insulation layer 2 coating: The copper core 1 after stretching is sent into the injection molding machine, the insulating raw material is heated and molten, and then coated on the copper core 1 to form an insulation layer 2, so that the whole becomes the core wire 3 of the communication network line, and then cooled through a long cooling water tank;
[0031] S3: Detwist and twist: The core wire 3 is detwist and twisted in a combination of orange-white plus orange, blue-white plus blue, brown-white plus brown, and green-white plus green through a detwist and twist machine;
[0032] S4: shielding layer coating: the four pairs of back-twisted twisted core wires 3 are respectively wrapped with aluminum foil 4, the gaps of the aluminum foil 4 are laser welded, and the aluminum foil 4 outside the adjacent core wires 3 is laser welded;
[0033] S5: Overall twisting into cable: the four pairs of core wires 3 wrapped with aluminum foil 4 are overall twisted according to a certain twist length;
[0034] S6: Sheath 5 coating: Wrap the core wire 3 after the total twisting with the sheath 5.
[0035] In the one-time cabling production process of the four pairs of core wires of the present invention, the four pairs of core wires are simultaneously wrapped with aluminum foil, and laser welding is adopted at the aluminum foil wrapping gap, so that the entire shielding cavity is round and smooth, the shielding cavity is fully closed, and there is no signal leakage. The signal wave cannot penetrate the thick aluminum foil cavity and can only be continuously reflected in the cavity. The crosstalk signal is consumed inside and has basically no effect on the other three pairs of core wires outside, so that the entire distortion peak is shifted to after 5000MHz, ensuring high-speed transmission within 5000MHz. Using thinner aluminum foil for laser welding can achieve a closed effect, with low cost and high economic benefit.
[0036] As a further preferred embodiment, in step S2: the insulating layer 2 is coated in batches, and the insulating layer 2 includes an inner skin layer 21, a foaming layer 22 and an outer skin layer 23. The insulating raw materials include high-density polyethylene masterbatch particles and foaming powder. First, the high-density polyethylene masterbatch particles are heated to become a molten state, and are extruded by an injection molding machine and coated on the copper core 1 to form the inner skin layer 21, and then sent to the injection molding machine again after cooling. The high-density polyethylene masterbatch particles and the foaming powder are molten again, and are extruded by an injection molding machine and coated on the copper core 1 to form the foaming layer 22, and then sent to the injection molding machine again after cooling. Finally, the high-density polyethylene masterbatch particles are heated to become a molten state, and are extruded by an injection molding machine and coated on the copper core 1 to form the outer skin layer 23, and then sent out after cooling. The thickness and diameter of the inner skin layer 21, the foaming layer 22 and the outer skin layer 23 are not more than 1.5 mm.
[0037] Skin-foam-skin three-layer physical foaming technology, with a foaming degree of 60%. The use of foamed insulation can greatly reduce the dielectric constant of insulation, thereby improving the propagation delay and increasing the transmission speed;
[0038] The outer diameter of the insulation layer 2 of the network cable is not greater than 1.5 mm, so that the high-voltage spark test is carried out synchronously with a DC voltage of 2kv-6kv, and the test result shows no breakdown.
[0039] As a further preferred embodiment, in step S2: the core wire 3 in the insulation layer 2 coating is monitored by an XY dual-axis laser outer diameter controller to control the wire diameter tolerance of the core wire 3 within 3um, and monitor the concentricity of the copper core 1 and the insulation layer 2 in the core wire 3. The concentricity is made above 99%, the impedance and attenuation performance are improved, and the return loss in the network cable is reduced.
[0040] As a further preferred embodiment, in the step S3: the untwisting twisting machine controls the twisting length of each pair of twisted core wires 3 to be uniform, and controls the twisting lengths of the four pairs of twisted core wires 3 to be unequal.
[0041] The twisted pair of network cables has a uniform lay length, which reduces line interference, matches the characteristic impedance of the cables, and reduces the return loss caused by the signal being partially reflected back to the signal transmitter. The same lay length will directly couple the interfering electromagnetic waves between the pairs to the signal, increasing the interference. This will directly cause one pair of network cables to be interfered by the other three pairs of cables, that is, the near-end crosstalk attenuation power will increase, and the unequal twisted pair lay length will stabilize the crosstalk.
[0042] As a further preferred embodiment, in step S3: untwisting the twisting, a real-time monitoring system for the twisting tension is used, and feedback adjustment is made through PLC to ensure that the tension in the twisting process is constant, thereby reducing crosstalk and making the crosstalk more stable.
[0043] As a further preferred embodiment, the aluminum foil 4 is an L-shaped structure, the thickness of the aluminum foil 4 is not less than 0.012 mm, the wrapping overlap rate is not less than 25%, and a tinned round copper wire with a diameter of 0.5 mm is arranged inside the aluminum foil 4. The tinned round copper wire is used for grounding, draining away the induced current on the surface of the aluminum foil, and also preventing the cable from being struck by indirect or direct lightning in thunderstorms.
[0044] As a further preferred embodiment, the sheath 5 is made of highly flame-retardant low-smoke halogen-free polyolefin material to improve the flame retardancy of the cable. Low-smoke halogen-free polyolefin material is mainly obtained by adding magnesium hydroxide and aluminum hydroxide to polyolefin materials such as polyethylene and polypropylene to achieve flame retardancy requirements.
[0045] As a further preferred embodiment, the copper core 1 that has been stretched in step S1 is subjected to an annealing process to improve the toughness and strength of the copper core 1 .
[0046] The preferred specific embodiments of the present invention are described in detail above. It should be understood that a person skilled in the art can make many modifications and changes based on the concept of the present invention without creative work. Therefore, any technical solution that can be obtained by a person skilled in the art through logical analysis, reasoning or limited experiments based on the concept of the present invention on the basis of the prior art should be within the scope of protection determined by the claims.
Claims
1. A method for preparing a 5000MHz ultra-high frequency communication network line, characterized in that: The following steps are involved: S1: Wire drawing: The raw copper wire blank is stretched through a wire drawing machine to the required copper core diameter requirement of the communication network line; S2: Insulation layer coating: The copper core after stretching is sent into the injection molding machine, the insulating raw material is heated and molten, and then coated on the copper core to form an insulation layer, so that the whole becomes the core wire of the communication network line, and then cooled through a long cooling water tank; S3: Detwist and twist: The core wires are twisted and twisted in a combination of orange-white plus orange, blue-white plus blue, brown-white plus brown, and green-white plus green through a detwist and twist machine; S4: Shielding layer coating: Wrap the four pairs of back-twisted twisted core wires with aluminum foil respectively, and laser weld the gaps of each group of aluminum foil wrappings and weld the aluminum foils on the outside of adjacent core wires by laser welding; S5: Twisting the four pairs of aluminum foil wrapped core wires into a cable according to a certain twist length; S6: Sheath coating: Wrap the twisted core wires with a sheath.
2. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that: In step S2: the insulating layer is formed in the insulating layer coating, including an inner skin layer, a foaming layer and an outer skin layer, and the insulating raw materials include high-density polyethylene masterbatch particles and foaming powder. First, the high-density polyethylene masterbatch particles are heated to become a molten state, and are extruded by an injection molding machine to be coated on the copper core to form an inner skin layer, and then are sent to the injection molding machine again after cooling. The high-density polyethylene masterbatch particles and the foaming powder are molten again, and are extruded by an injection molding machine to be coated on the copper core to form a foaming layer, and then are sent to the injection molding machine again after cooling. Finally, the high-density polyethylene masterbatch particles are heated to become a molten state, and are extruded by an injection molding machine to be coated on the copper core to form an outer skin layer, and then are cooled and sent out. The thickness and diameter of the inner skin layer, the foaming layer and the outer skin layer are not more than 1.5 mm.
3. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that: In step S2: the core wire in the insulation layer coating is monitored by an XY dual-axis laser outer diameter controller to control the core wire diameter tolerance within 3um, and monitor the concentricity of the copper core and the insulation layer in the core wire.
4. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that: In the step S3: in the back-twisting twisting, the back-twisting twisting machine controls the twisting length of each pair of twisted core wires to be uniform, and controls the twisting lengths of the four pairs of twisted core wires to be unequal.
5. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that In the step S3: the real-time monitoring system of the twisting tension is used in the back-twisting twisting, and feedback adjustment is made through the PLC to ensure that the tension of the twisting process is constant.
6. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that: The aluminum foil is of L-shaped structure, the thickness of the aluminum foil is not less than 0.012 mm, the wrapping overlap rate is not less than 25%, and a tinned round copper wire with a diameter of 0.5 mm is arranged inside the aluminum foil.
7. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that: The sheath material is a highly flame-retardant, low-smoke, halogen-free polyolefin material.
8. The method for preparing a 5000MHz ultra-high frequency communication network line according to claim 1, characterized in that: The copper core that has been stretched in step S1 is subjected to an annealing process.