Small-size oxide semiconductor etching method

By preparing polycrystalline silicon on oxide semiconductor materials and forming a silicon nanowire mask, and etching of small-sized oxide semiconductor devices is achieved in combination with different etching methods, the problem of preparing small-sized devices in the prior art is solved, the integration density is improved and the integration density is reduced. Equipment requirements.

CN118919414APending Publication Date: 2024-11-08BEIJING SUPERSTRING ACAD OF MEMORY TECH +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411000344.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The prior art is difficult to achieve high yield and large-area preparation of small-sized oxide semiconductor devices, and has high requirements for lithography and etching equipment, which limits the improvement of integrated circuit density.

Method used

By preparing an amorphous silicon layer on an oxide semiconductor material, lateral crystallization is carried out by metal induced to form polycrystalline silicon, and silicon nanowires are formed as self-aligned hard masks through thermal oxidation and dry etching, combined with wet or dry etching Etching achieves small-size etching of oxide semiconductor materials, and finally uses ion beam etching to remove the mask.

Benefits of technology

Reduces the demand for exposure equipment, increases the integrated density of oxide semiconductor transistors, and significantly reduces the impact of etching on the oxide semiconductor layer. It is not limited to etching equipment and gases, achieving high efficiency of small-size etching. preparation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919414A_ABST
    Figure CN118919414A_ABST
Patent Text Reader

Abstract

The invention discloses a small-size oxide semiconductor etching method, and belongs to the technical field of information materials and devices. According to the method, a nanowire material is obtained through a low-temperature process, the diameter of the nanowire is further reduced through a method of combining self-oxidation and self-limiting etching, and self-alignment and high-precision etching of an oxide semiconductor on the small size is achieved. Compared with traditional other mask etching depending on the exposure precision of equipment such as DUV and EUV, the method solves the problem that an existing oxide semiconductor device is miniature in size, the density of an integrated circuit can be improved, the requirement for photoetching equipment is greatly reduced, and the process cost is effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The patent of this invention relates to a method for realizing small-size oxide semiconductor etching, which belongs to the field of information materials and device technology. Background Art

[0002] Oxide semiconductor materials have shown great advantages in the field of flat display thin-film transistors due to their unique characteristics of high mobility, high transmittance and large-area uniformity. The characteristic of this application is that the device size is at the micron level. In recent years, with the in-depth study of oxide semiconductor materials and devices, it has been found that the ultra-low off-state current brought by the wide bandgap, the low mechanical stress caused by the amorphous characteristics and the back-end compatibility achieved by the low process thermal budget make oxide semiconductors one of the most promising materials for realizing high-density, high-energy-efficiency three-dimensional integrated circuits.

[0003] Currently, by optimizing the exposure and etching processes, oxide semiconductor devices with a groove length and width of less than 100 nanometers can be realized, and good device performance can be achieved, demonstrating the application potential of oxide semiconductors in the field of integrated circuits. However, the realization of small-sized devices requires extremely high requirements for lithography and etching equipment, making it difficult to achieve high-yield large-area preparation. Summary of the invention

[0004] In order to solve the size miniaturization problem of existing oxide semiconductor devices and improve the density of integrated circuits, the present invention proposes a small-size oxide semiconductor etching method.

[0005] The technical solution provided by the present invention is as follows:

[0006] A small-sized oxide semiconductor etching method, the steps comprising:

[0007] Step 1) preparing an amorphous silicon layer on the oxide semiconductor material to be etched;

[0008] Step 2) annealing at a low temperature, using the metal in the oxide semiconductor material to induce lateral crystallization of the amorphous silicon layer to form polycrystalline silicon;

[0009] Step 3) thermal oxidation and oxygen plasma treatment are used to oxidize the surface layer of polysilicon into SiO2, and then a high selectivity dry etching method is used to remove the surface SiO2, which is repeated several times to reduce the diameter to the required diameter, thereby forming silicon nanowires;

[0010] Step 4) using the silicon nanowires obtained in step 3) as a hard mask, and etching the oxide semiconductor material by a wet or dry etching method;

[0011] Step 5) using ion beam etching with shaping function to remove the silicon nanowire hard mask without damaging the oxide semiconductor material.

[0012] Furthermore, in step 1), the amorphous silicon layer is prepared by plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, pulsed vapor deposition or atomic layer deposition.

[0013] Furthermore, in step 1), the thickness of the amorphous silicon layer is in the range of 20 nanometers to 200 nanometers.

[0014] Furthermore, the temperature in step 2) ranges from 150°C to 400°C.

[0015] Furthermore, the dry etching method in step 3) is specifically reactive ion etching, reactive coupled plasma etching or atomic layer etching.

[0016] Furthermore, in step 3), the diameter of the silicon nanowires ranges from 10 nanometers to 200 nanometers, and the length ranges from about 50 nanometers to 2000 nanometers.

[0017] Furthermore, the oxide semiconductor is In2O3, SnO2, Ga2O3, ZnO, ITO, IGO, IZO, IGZO, IAZO, ITZO, IWO, ITWO, etc., as well as all oxide semiconductor single-layer films and composite films stacked with multiple oxide films of various doping components and proportions, with a thickness ranging from about 0.5 nanometers to 50 nanometers.

[0018] The beneficial effects of the present invention are as follows:

[0019] The present invention proposes to use nanowire materials as a self-aligned hard mask for etching, and realizes small-size etching by combining self-oxidation of nanowires with self-limiting etching while reducing the demand for exposure equipment. The present invention has great potential in improving the integration density of oxide semiconductor transistors. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1-8 is a process flow chart of a specific embodiment of the present invention;

[0021] Fig. 9 for Figure 1-8 Example description. Specific implementation methods

[0023] The embodiments of the present invention are described in detail below by means of implementation cases, which are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be interpreted as limiting the present invention.

[0024] The implementation case is to use the etching of indium oxide film as an example. The specific steps include:

[0025] S001, preparing an indium oxide thin film on a substrate, the thickness of which ranges from about 0.5 nanometers to 50 nanometers, such as Figure 1 shown.

[0026] S002, preparing an amorphous silicon layer by plasma enhanced chemical vapor deposition, such as Figure 2 shown.

[0027] S003, heating the sample in an annealing furnace, the amorphous silicon on the surface of the indium oxide is crystallized into polycrystalline silicon under the induction of the indium metal. In this example, the temperature is 350°C and the atmosphere is nitrogen. Figure 3 shown.

[0028] S004, thermal oxidation is used to oxidize the surface of polycrystalline silicon and residual amorphous silicon, such as Figure 4 shown.

[0029] S005, using dry etching based on CHF3 gas and oxygen, removes the surface SiO2 without affecting the internal polysilicon, such as Figure 5 shown.

[0030] S006, repeating steps S004 and S005 until the polysilicon is reduced to a desired size to form a silicon nanowire, such as Figure 6 shown.

[0031] S007 uses silicon nanowires as a self-aligned mask and removes the uncovered indium oxide material through atomic layer etching based on methane gas. In this case, the temperature is 120°C. Each cycle of atomic layer etching is divided into two steps: reaction and etching. During the reaction, 100 sccm argon and 10 sccm methane are introduced, the ICP power is 400W, and the duration is 5s. During etching, 100 sccm Ar is introduced, the RF power is 15W, the ICP power is 250W, and the duration is 8s. Figure 7 Shown

[0032] S008, using ion beam shaping dry etching to remove the silicon nanowire mask, ion beam shaping IBS can remove the protrusions by etching angles, such as Figure 8 shown.

[0033] Compared with the prior art, the present invention adopts the above technical solution, which significantly reduces the requirements for exposure accuracy while achieving a small size, reduces the impact of etching on the oxide semiconductor layer, and is not limited by etching equipment and gases.

[0034] The present invention can be used to prepare planar transistors and vertical transistors of oxide semiconductors, as well as logic and storage devices based on the above transistors. All technical solutions formed by equivalent transformation or equivalent transformation fall within the protection scope of the present invention.

[0035] It should be noted that the above-mentioned embodiments illustrate rather than limit the invention and that those skilled in the art will be able to design alternative embodiments without departing from the scope of the appended claims.

Claims

1. A small-sized oxide semiconductor etching method, characterized in that: The steps include: Step 1) preparing an amorphous silicon layer on the oxide semiconductor material to be etched; Step 2) annealing at a low temperature, using the metal in the oxide semiconductor material to induce lateral crystallization of the amorphous silicon layer to form polycrystalline silicon; Step 3) thermal oxidation and oxygen plasma treatment are used to oxidize the surface layer of polysilicon into SiO2, and then a high selectivity dry etching method is used to remove the surface SiO2, which is repeated several times to reduce the diameter to the required diameter, thereby forming silicon nanowires; Step 4) using the silicon nanowires obtained in step 3) as a hard mask, and etching the oxide semiconductor material by a wet or dry etching method; Step 5) using ion beam etching with shaping function to remove the silicon nanowire hard mask without damaging the oxide semiconductor material.

2. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: Step 1) preparing an amorphous silicon layer by plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, pulsed vapor deposition or atomic layer deposition.

3. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: The thickness of the amorphous silicon layer in step 1) ranges from 20 nanometers to 200 nanometers.

4. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: The temperature in step 2) ranges from 150°C to 400°C.

5. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: The dry etching method in step 3) is specifically reactive ion etching, reactive coupled plasma etching or atomic layer etching.

6. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: In step 3), the diameter of the silicon nanowires ranges from 10 nanometers to 200 nanometers.

7. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: In step 3), the length of the silicon nanowires ranges from 50 nanometers to 2000 nanometers.

8. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: The oxide semiconductor material is selected from one or more of In2O3, SnO2, Ga2O3, ZnO, ITO, IGO, IZO, IGZO, IAZO, ITZO, IWO or ITWO.

9. The small-sized oxide semiconductor etching method according to claim 8, characterized in that: The oxide semiconductor material is a single-layer film or a composite film of stacked multiple films.

10. The small-sized oxide semiconductor etching method according to claim 1, characterized in that: The thickness of the oxide semiconductor material ranges from 0.5 nanometers to 50 nanometers.

Citation Information

Cited By

  • Small-sized oxide semiconductor etching method

    WO2026020668A1