Electrode body and electric storage element

By placing the resistance portion on the surface of the electrode conductor, the poor connection problem caused by the movement of the electrolyte in the electrochemical battery is solved, the reliability and safety of the battery are improved, the generation of defective products is reduced, and resource and energy saving is achieved.

CN118922964APending Publication Date: 2024-11-08KYOCERA CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280094110.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2022-03-29
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Existing electrochemical batteries are prone to poor connections during the movement of the electrolyte, which affects the reliability and safety of the battery. Especially when the welding strength between the electrode conductor and the connection terminal becomes smaller, it may cause poor connection problems.

Method used

The resistance portion is arranged on the surface of the electrode conductor, and is located on the active material layer and the electrolyte movement path to increase the moving resistance of the electrolyte from the first area to the second area, and reduce the connection defect caused by the electrolyte adhering to the second area. possibility. This resistance portion increases resistance to the electrolyte by reducing the surface roughness and the concave and convex structure, so as to ensure that the electrolyte does not easily move to the second region.

Benefits of technology

Effectively reduces the movement of the electrolyte from the first area to the second area, reduces the possibility of poor connection between the connecting terminal and the electrode conductor, improves the reliability and safety of the battery, reduces the generation of defective products, and saves resources. and energy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118922964A_ABST
    Figure CN118922964A_ABST
Patent Text Reader

Abstract

The electrode body (14) has: an active material layer containing an electrode active material and an electrolyte solution; an electrode conductor (12a) having (i) a first region (121) in which the active material layer is located and (ii) a second region (122) which is a region capable of being electrically connected to the connection terminal, the second region (122) being a region different from the first region; and a resistance part (123) which is positioned closer to the second region than the first region of the electrode conductor and which exhibits a higher resistance than the first region when the electrolyte solution moves along the surface of the electrode conductor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to an electrode body and a power storage device having the electrode body. Background Art

[0002] An example of an electrochemical cell is disclosed in Patent Document 1. The electrochemical cell has: (i) a first current collector coupled to a first portion of a bag; and (ii) a second current collector coupled to a second portion of the bag. A first electrode material is disposed on the first current collector. A second electrode material is disposed on the second current collector. The electrochemical cell also has a separator disposed between the first electrode material and the second electrode material.

[0003] Prior art literature

[0004] Patent Literature

[0005] Patent Document 1: US2019 / 0326562 Summary of the invention

[0006] An electrode body in one embodiment of the present invention comprises: an active material layer including an electrode active material and an electrolyte; an electrode conductor having (i) a first region where the active material layer is located and (ii) a second region where a connection terminal can be electrically connected, the second region being a region different from the first region; and a resistance portion located on a side of the electrode conductor that is closer to the second region than to the first region, and exhibiting a higher resistance than the first region to the movement of the electrolyte along the surface of the electrode conductor on the side where the active material layer is located. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] Figure 1 It is a perspective view showing the appearance of the secondary battery of the present disclosure.

[0008] Figure 2 It is a perspective view showing the appearance of a unit cell of the present disclosure.

[0009] Figure 3 It is decomposed to show Figure 1 Model diagram of the cross section along line III-III.

[0010] Figure 4 It is decomposed to show Figure 1 Model diagram of the cross section of line IV-IV.

[0011] Figure 5 It is a model diagram showing the specific structure of the electrode body.

[0012] Figure 6 It is a plan view showing the structure of the vicinity of the exposed portion of the negative electrode included in the electrode assembly of the present disclosure.

[0013] Figure 7 This is a diagram showing the movement of the electrolyte in the electrode conductor of the negative electrode having no resistance portion.

[0014] Figure 8 This is a diagram showing an example of a cross section of an electrode conductor included in the negative electrode of the present disclosure.

[0015] Fig. 9 It is a schematic cross-sectional view showing a resistance portion according to a first modified example.

[0016] Fig.10 It is a schematic cross-sectional view showing a resistance portion according to a second modification.

[0017] Fig.11 It is a top view showing a modification of a unit cell having the negative electrode of the present disclosure. DETAILED DESCRIPTION

[0018] [Structure of secondary battery]

[0019] Figure 1 1 is a perspective view showing the appearance of a secondary battery 1. The secondary battery 1 is a battery that can be charged or discharged by being electrically connected to an external terminal. For example, at least one secondary battery 1 can be mounted in a power storage device for residential use, base station use, vehicle use, robot use such as an unmanned aerial vehicle, or medical equipment. The secondary battery 1 can include a unit cell 10 (power storage element), connection terminals 21, 22, and a second container 50. The structure of the unit cell 10 will be described later.

[0020] The second container 50 can accommodate the unit cell 10. The second container 50 can be formed of, for example, an aluminum bag film or a laminated film having a metal foil layer such as stainless steel or nickel. The aluminum bag film can be a film formed by evaporating aluminum on a film or a film formed by laminating aluminum foil and a film. The material of the film can be, for example, polypropylene, polyethylene, nylon, or polyethylene terephthalate. The thickness of the second container 50 can be greater than 50 μm and less than 300 μm, for example, 200 μm.

[0021] When the second container 50 is an aluminum bag film, the second container 50 may have a structure in which two sheets of aluminum bag films are located on both sides of the stacking direction (Z-axis direction) of the unit battery 10. In addition, when the second container 50 is an aluminum bag film, the second container 50 may also have a structure in which one sheet of aluminum bag film is folded in half and the unit battery 10 is located therein.

[0022] The connecting terminals 21 and 22 may be terminals connected to external terminals to extract power from the secondary battery 1 or supply power to the secondary battery 1. The connecting terminals 21 and 22 may protrude from the inside of the second container 50 to the outside. The material of the connecting terminals 21 and 22 may be, for example, copper, aluminum, or nickel. The thickness of the connecting terminals 21 and 22 may be greater than 50 μm and less than 500 μm, for example, 200 μm. In addition, the connecting terminals 21 and 22 may be subjected to a surface treatment for improving adhesion to an adhesive member (not shown). In order to determine the position of the connecting terminals 21 and 22 relative to the second container 50, the adhesive member bonds the connecting terminals 21 and 22 to the second container 50 located above and below the connecting terminals 21 and 22.

[0023] Figure 2 1 is a perspective view showing the appearance of the unit cell 10. Figure 2 As shown, the unit cell 10 may include an electrode body 14 and a first container 15 (container). The electrode body 14 may have a sheet-like shape. The sheet-like electrode body 14 may include a positive electrode 11 and a negative electrode 12.

[0024] The first container 15 can accommodate the electrode body 14. The first container 15 can seal the peripheral portion in a state where the electrode body 14 is accommodated. In the case where a plurality of first containers 15 accommodating the electrode body 14 are stacked, the plurality of first containers 15 can be bonded to each other by an adhesive layer not shown. The material of the first container 15 can be, for example, film-like PET (polyethylene terephthalate) or nylon. More specifically, for example, two sheets of the first container 15 can have a structure located on both sides of the stacking direction (Z-axis direction) of the unit cell 10. The thickness of the base material of the first container 15 can be, for example, greater than 10 μm and less than 40 μm, for example, 25 μm. The material of the adhesive layer can be, for example, polypropylene or polyethylene.

[0025] The first receiving body 15 may also be transparent, for example. Figure 2 This is a diagram showing a state where the electrode body 14 can be confirmed through the first housing body 15 by using a transparent first housing body 15 in the unit cell 10 .

[0026] The first container 15 may have a cutout 16. For example, the cutout 16 may be provided in each of the first container 15 on the positive electrode 11 side and the first container 15 on the negative electrode 12 side. By providing the cutout 16 as an unsealed portion in a portion of the unit cell 10, it is possible to release the gas generated by the decomposition reaction of the electrolyte or a trace amount of water inside the unit cell 10 to the outside of the unit cell 10. In addition, by providing the cutout 16, a portion of the positive electrode 11 side and a portion of the negative electrode 12 side may be exposed from the first container 15. Alternatively, a portion of the positive electrode 11 side and a portion of the negative electrode 12 side may not be exposed from the first container 15. In the latter case, a structure may be provided in which the space inside the positive electrode 11 side of the unit cell 10 is connected to the space outside the unit cell 10, and a structure may be provided in which the space inside the negative electrode 12 side of the unit cell 10 is connected to the space outside the unit cell 10. Alternatively, the first container 15 on the negative electrode 12 side may be exposed at the position of the cutout portion 16 on the positive electrode 11 side, and the first container 15 on the positive electrode 11 side may be exposed at the position of the cutout portion 16 on the negative electrode 12 side.

[0027] The positive electrode 11 may have an exposed portion 11e exposed from the first container 15. The negative electrode 12 may have an exposed portion 12e exposed from the first container 15. Specifically, the exposed portions 11e and 12e protrude from the first container 15. The connection terminals 21 and 22 may be electrically connected to the exposed portions 11e and 12e, respectively, by, for example, ultrasonic welding, laser welding, or resistance welding. The details of the positive electrode 11 and the negative electrode 12 will be described later.

[0028] The secondary battery 1 may have a structure in which the unit cell 10 is further contained in the second container 50, and the unit cell 10 contains the positive electrode 11 and the negative electrode 12 in the first container 15. With this structure, the electrode body 14 is doubly contained, which can improve the safety of the secondary battery 1. In addition, the second container 50 may be further contained in the container. However, the secondary battery 1 only needs to have the positive electrode 11 and the negative electrode 12, and only needs to be contained in at least one container.

[0029] In the first embodiment, the secondary battery 1 has a structure in which a plurality of unit cells 10 are stacked, for example, a structure in which 10 layers of unit cells 10 are stacked. However, the secondary battery 1 of the present disclosure may have a plurality of layers of unit cells 10 other than 10 layers, or may have only one layer. In the case where the secondary battery 1 has a plurality of layers of unit cells 10, these unit cells 10 may be stacked. Figure 1 In the case of the secondary battery 1 shown in the figure, the portion other than the connection terminals 21 and 22 may be substantially rectangular or may be of a different shape. Figure 2 In the case of the unit cell 10 shown, the portion other than the exposed portions 11 e and 12 e may be substantially rectangular or may have a different shape.

[0030] Figure 3 is shown in exploded form Figure 1 Model diagram of the cross section along line III-III. Figure 4 is shown in exploded form Figure 1 Model diagram of the cross section of line IV-IV. For simplicity, Figure 3 and Figure 4 In the embodiment, the second container 50 is omitted. Figure 3 and Figure 4 The main figure shows the positional relationship of each component. Therefore, the size relationship of the thickness of each component is not necessarily the same as Figure 3 and Figure 4 shown.

[0031] like Figure 3 and Figure 4 As shown, the secondary battery 1 may further include a first protective member 30 .

[0032] The first protective member 30 can protect the first connection portion electrically connecting the exposed portions 11e exposed from the first housing 15 of each unit battery 10 and the second connection portion electrically connecting the exposed portions 12e exposed from the first housing 15 of each unit battery 10. The exposed portions 11e and the exposed portions 12e can be connected to each other by, for example, ultrasonic welding, laser welding, or resistance welding. Figure 3 and Figure 4 In the embodiment, the exposed portions 11e of the positive electrode 11 and the exposed portions 12e of the negative electrode 12 are not connected to each other as described above, but are actually connected.

[0033] The material of the first protective member 30 may be, for example, a film-like polyolefin or polyimide. The first protective member 30 may be bonded to the exposed portions 11e and 12e by an adhesive layer (not shown). In addition, the material of the adhesive layer in the first protective member 30 may be a material that is difficult to dissolve into the electrolyte (electrolyte). The material of the adhesive layer may be, for example, an acrylic adhesive.

[0034] In this embodiment, the first protective member 30 can cover a portion of the first container 15 from the first connection portion and the second connection portion. As a result, when stress is generated in the exposed portion 11e or 12e, stress concentration is not easily generated, so the possibility of damage or breakage of the exposed portion 11e or 12e near the first connection portion and the second connection portion can be reduced. However, the first protective member 30 only needs to protect at least the first connection portion and the second connection portion, and does not necessarily have to cover the first container 15 from the first connection portion and the second connection portion.

[0035] In addition, if Figure 3 and Figure 4 As shown, the positive electrode 11 may include an electrode conductor 11 a and a positive electrode active material layer 11 b , and the negative electrode 12 may include an electrode conductor 12 a and a negative electrode active material layer 12 b .

[0036] The electrode conductor 11a may be, for example, aluminum foil. The thickness of the electrode conductor 11a may be 5 μm to 25 μm, for example, 10 μm. The electrode conductor 12a may be, for example, copper foil. The thickness of the electrode conductor 12a may be 5 μm to 25 μm, for example, 10 μm.

[0037] Figure 5 1 is a cross-sectional view showing a specific structure of the electrode body 14. Figure 5 As shown, the positive electrode active material layer 11b (active material layer) can be a mixture of the positive electrode active material 11c (electrode active material) and the conductive aid 11d, that is, a positive electrode material layer. In addition, the negative electrode active material layer 12b (active material layer) can be a mixture of the negative electrode active material 12c (electrode active material) and the conductive aid 12d, that is, a layer of the negative electrode material. The positive electrode active material 11c can be, for example, lithium cobalt oxide, lithium nickel oxide, lithium iron phosphate or lithium manganese oxide. The negative electrode active material 12c can be, for example, graphite or lithium titanate. The conductive aids 11d and 12d can be, for example, carbon black or acetylene black. However, the positive electrode active material 11c, the negative electrode active material 12c, and the conductive aids 11d and 12d are not limited to this.

[0038] The positive electrode material may have a so-called clay-like property in which an electrolyte is mixed into a mixture consisting of a positive electrode active material 11c and a conductive auxiliary agent 11d. The negative electrode material may have a so-called clay-like property in which an electrolyte is mixed into a mixture consisting of a negative electrode active material 12c and a conductive auxiliary agent 12d. The positive electrode 11 may be an electrode in which a positive electrode material is coated on an electrode conductor 11a. The negative electrode 12 may be an electrode in which a negative electrode material is coated on an electrode conductor 12a.

[0039] The electrolyte is formed by dissolving a lithium salt as an electrolyte in a non-aqueous solvent. As a non-aqueous solvent, a carbonate-based solvent may be used. As a carbonate-based solvent, γ-butyrolactone may be used, ethylene carbonate may be used, or both γ-butyrolactone and ethylene carbonate may be used. In addition, as a carbonate-based solvent, as long as at least any one of γ-butyrolactone and ethylene carbonate is included, other solvents may also be included. As other solvents, for example, propylene carbonate, dimethyl carbonate, dimethoxyethane, diethyl carbonate, tetrahydrofuran, and triethylene glycol dimethyl ether may be mentioned. As an electrolyte, lithium hexafluorophosphate or lithium bis(fluorosulfonyl)imide (LiFSI) may be used.

[0040] In addition, the electrode body 14 may further include a separator 13. The positive electrode 11, the negative electrode 12, and the separator 13 may have a positional relationship in which the positive electrode active material layer 11b and the negative electrode active material layer 12b are in contact with the separator 13. That is, the unit cell 10 may have a structure in which the positive electrode 11 and the negative electrode 12 are stacked with the separator 13 interposed therebetween. The separator 13 may function as an insulating member that insulates the positive electrode 11 and the negative electrode 12. For example, a sheet-like nonwoven fabric or a porous material may be used for the separator 13.

[0041] When a porous material is used as the separator 13 , specifically, a porous film made of a thermoplastic resin having a melting point of about 80° C. to 140° C. As the thermoplastic resin, for example, a polyolefin polymer such as polypropylene or polyethylene, or polyethylene terephthalate can be used.

[0042] (Structure of Negative Electrode 12)

[0043] Figure 6 1 is a top view showing the structure of the exposed portion 12e of the negative electrode 12 of the electrode body 14. Figure 6 In the embodiment, the negative electrode active material layer 12b is omitted. Figure 6 As shown, in the negative electrode 12, the electrode conductor 12a has a first region 121 and a second region 122. The first region 121 is a region where the negative electrode active material layer 12b is located. The first region 121 may be substantially the entire surface of the electrode conductor 12a on the side where the negative electrode active material layer 12b is located, except for the exposed portion 12e. The second region 122 is a region where the connection terminal 22 can be electrically connected. The second region 122 is a region on a portion of the exposed portion 12e on the surface on the side where the negative electrode active material layer 12b is located.

[0044] In the following description, the surface of the electrode conductor 12a on the side where the negative electrode active material layer 12b is located is simply referred to as the surface of the electrode conductor 12a. Figure 6 As shown, a resistance portion 123 is arranged between the first region 121 and the second region 122 on the surface of the electrode conductor 12a. That is, the electrode body 14 has a resistance portion 123. The resistance portion 123 has a linear shape when the electrode conductor 12a is viewed from above. The linear shape is a shape having a length and a width that can be substantially regarded as a line. The resistance portion 123 shows a higher resistance than the first region 121 to the movement of the electrolyte contained in the negative electrode active material layer 12b along the surface of the electrode conductor 12a. The resistance portion 123 is located on the side of the electrode conductor 12a that is closer to the second region 122 than the first region 121. The width of the resistance portion 123 having a linear shape can be greater than 20μm, for example, can be 50μm.

[0045] The resistance portion 123 may be arranged to be located on any path along which the electrolyte moves from the first region 121 to the second region 122 on the surface of the electrode conductor 12a. Figure 6 As shown, the resistance portion 123 can be arranged at a position closer to the first area 121 than the second area 122, between the two ends of the exposed portion 12e in the left-right direction when the direction from the first area 121 to the second area 122 is regarded as the front. In this case, no matter which path the electrolyte moves from the first area 121 to the second area 122, the resistance portion 123 is located on the path. By configuring the resistance portion 123 in this way, it is possible to increase the resistance to the movement of the electrolyte from the first area 121 to the second area 122 regardless of the movement path of the electrolyte. The position of the resistance portion 123 can be separated by more than 3 mm from the end of the first area 121 opposite to the second area 122.

[0046] However, the resistance portion 123 may not be arranged to be located on all paths where the electrolyte can move from the first region 121 to the second region 122. In other words, the resistance portion 123 only needs to be arranged to be located on at least a portion of the path where the electrolyte moves from the first region 121 to the second region 122. By arranging the resistance portion 123 in this way, the resistance to the movement of the electrolyte is increased on the path where the resistance portion 123 is located.

[0047] The resistance portion 123 does not necessarily need to be a region different from the second region 122, and may be included in the second region 122. In this case, the resistance portion 123 may exhibit higher resistance than the second region 122 to the electrolyte contained in the negative electrode active material layer 12b moving along the surface of the electrode conductor 12a.

[0048] Figure 7 1 is a diagram showing the movement of the electrolyte in the electrode conductor 12a of the negative electrode 12 which does not have the resistance portion 123. Figure 7 , the movement of the electrolyte from the first region 121 side to the second region 122 side is shown over time for the four examples of the negative electrode 12. The four examples of the negative electrode 12 do not differ in manufacturing conditions and the like. Figure 7 Reference numeral 701 is an image showing a state immediately after the negative electrode active material layer 12 b is formed. Figure 7 Reference numeral 702 is an image showing a state where one hour has passed from the state of reference numeral 701 . Figure 7 Reference numeral 703 is an image showing a state where four hours have passed from the state of reference numeral 701 . Figure 7 Reference numeral 704 is an image showing a state in which 12 hours have passed from the state of reference numeral 701 .

[0049] In each image, the darker areas are where the electrolyte is moving. Figure 7 As shown in the figure numeral 701, the electrolyte solution moves immediately after the negative electrode active material layer 12b is formed. Figure 7 As shown in the reference numerals 702 to 704, when the negative electrode 12 does not include the resistance portion 123, in any example, the movement of the electrolyte proceeds with the passage of time. Figure 7 In the figure mark 704, in all four examples, the electrolyte reaches the second area 122. When the electrolyte moves to the second area 122 where the connection terminal 22 is welded to the electrode conductor 12a, the strength of the welding of the connection terminal 22 to the second area 122 decreases, which may cause poor connection.

[0050] Figure 8 1 is a diagram showing an example of a cross section of the electrode conductor 12a. Figure 8 In FIG. 8 , reference numeral 801 is a large-scale photograph of a cross section of the electrode conductor 12 a including the resistance portion 123 and a portion of the first region 121 and a portion of the second region 122 located on both sides thereof. Figure 8 , reference numeral 802 is an enlarged view of region R1 of reference numeral 801. Figure 8 , reference numeral 803 is an enlarged view of region R2 of reference numeral 801. Figure 8 , reference numeral 804 is an enlarged view of region R3 of reference numeral 801. Region R1 is a region of the first region 121 separated from the resistance portion 123. Region R2 is a region between the first region 121 and the resistance portion 123. Region R3 is a region including the resistance portion 123.

[0051] like Figure 8 As shown in the figure mark 802, in order to facilitate the coating of the negative electrode active material 12c and the like, the surface of the electrode conductor 12a in the first region 121 is processed (roughened) in a manner that the surface roughness becomes coarser. For example, the thickness of the electrode conductor 12a can be 5 μm to 25 μm. The arithmetic mean roughness Ra of the surface of the electrode conductor 12a can be 0.15 μm to 0.6 μm. The maximum height Rz of the surface of the electrode conductor 12a can be 1.2 μm to 5 μm. Figure 8 As shown in the figure 803, the surface of the electrode conductor 12a is processed so that the surface roughness is also increased in the region R2. On such a surface, due to the capillary phenomenon caused by the surface irregularities, the resistance to the movement of the electrolyte contained in the negative electrode active material layer 12b becomes low. Therefore, on such a surface, the electrolyte contained in the negative electrode active material layer 12b easily moves to the second region 122 side.

[0052] like Figure 8As shown in the figure mark 804, the resistance part 123 may include a region on the surface of the electrode conductor 12a having a surface roughness smaller than that of the first region 121. By including such a region, the resistance part 123 has a smaller influence of the capillary phenomenon in the resistance part 123. Therefore, the resistance part 123 shows a higher resistance than the first region 121 to the movement of the electrolyte along the surface of the electrode conductor 12a. That is, in the region where the surface roughness of the resistance part 123 is smaller than that of the first region 121, it is difficult for the electrolyte contained in the negative electrode active material layer 12b to move to the second region 122 side.

[0053] In the following description, the area of ​​the resistance portion 123 having a surface roughness smaller than that of the first area 121 is referred to as a roughness reduction area. The entire resistance portion 123 may be a roughness reduction area, or only a portion of the resistance portion 123 may be a roughness reduction area. In the case where only a portion of the resistance portion 123 is a roughness reduction area, there may be another structure in which the portion other than the roughness reduction area of ​​the resistance portion 123 shows a higher resistance to the movement of the electrolyte than the first area 121. The portion other than the roughness reduction area of ​​the resistance portion 123 may have a structure described in the modified example described later, for example.

[0054] The arithmetic mean roughness Ra in the roughness reduction region may be, for example, 0.05 μm to 0.1 μm. In addition, the maximum height Rz in the roughness reduction region may be 0.3 μm to 1.0 μm. By having such a roughness in the roughness reduction region, the resistance of the resistance portion 123 to the movement of the electrolyte along the surface of the electrode conductor 12a becomes sufficiently high.

[0055] In the process of providing the roughness reduction region on the surface of the electrode conductor 12a, the thickness of the electrode conductor 12a may vary. Specifically, the thickness of the electrode conductor 12a in the roughness reduction region may become smaller. When the thickness of the electrode conductor 12a becomes smaller, the strength of the electrode conductor 12a decreases.

[0056] When the thickness of the electrode conductor 12a in the roughness reduction region varies, a difference is generated between the thickness of the electrode conductor 12a in the first region 121 and the thickness of the electrode conductor 12a in the roughness reduction region. The difference between the thickness of the electrode conductor 12a in the first region 121 and the thickness of the electrode conductor 12a in the roughness reduction region may be 20% or less of the thickness of the electrode conductor 12a in the first region 121. In addition, the thickness of the electrode conductor 12a in the roughness reduction region may not vary. In this case, the difference between the thickness of the electrode conductor 12a in the first region 121 and the thickness of the electrode conductor 12a in the roughness reduction region is 0% of the thickness of the electrode conductor 12a in the first region 121. That is, the variation in thickness in the process of setting the roughness reduction region on the surface of the electrode conductor 12a may be 20% or less of the thickness of the electrode conductor 12a in the first region 121. Thus, the reduction in the strength of the electrode conductor 12a in the roughness reduction region can be reduced. Such a roughness-reduced region can be provided by, for example, pressing the surface of the electrode conductor 12 a using a roller or the like.

[0057] In addition, if Figure 8 As shown in FIG. 1 , the electrode conductor 12a may be bent into a convex shape in the resistance portion 123 toward the side opposite to the surface of the electrode conductor 12a. The electrode conductor 12a has such a shape, and the resistance portion 123 functions as a liquid reservoir for the electrolyte. That is, it is difficult for the electrolyte to move from the resistance portion 123 to the outside. Therefore, the resistance of the resistance portion 123 to the movement of the electrolyte can be further increased.

[0058] As described above, in the electrode body 14, the negative electrode 12 has the resistance portion 123, which can reduce the movement of the electrolyte from the first region 121 to the second region 122 on the surface of the electrode conductor 12a. Therefore, according to the electrode body 14, the possibility of poor connection between the connection terminal 22 welded to the second region 122 and the electrode conductor 12a due to the adhesion of the electrolyte to the second region 122 can be reduced.

[0059] The above description has been given of an example in which the electrode body 14 includes the resistance portion 123 on the surface of the electrode conductor 12a. However, the electrode body 14 may include the resistance portion 123 on the surface of the electrode conductor 11a.

[0060] In particular, when the surface of the electrode conductor 11a is roughened, the capillary phenomenon has a greater effect on the movement of the electrolyte on the surface of the electrode conductor 11a. That is, the electrolyte can reach the second region 122 on the surface of the electrode conductor 11a. When the electrode body 14 has the resistance portion 123 on the surface of the electrode conductor 11a, the movement of the electrolyte can be reduced even on the electrode conductor 11a with a roughened surface.

[0061] (Variant 1)

[0062] Fig. 9 FIG. 1 is a schematic cross-sectional view showing a resistance portion 123A according to a first modified example of the resistance portion 123. Fig. 9 As shown, the resistance portion 123A may be a recessed portion on the surface of the electrode conductor 12a. The resistance portion 123A functions as a liquid reservoir of the electrolyte. Therefore, such a resistance portion 123A also shows a higher resistance than the first region 121 to the movement of the electrolyte along the surface of the electrode conductor 12a. The resistance portion 123A may be provided, for example, by excavating the surface of the electrode conductor 12a using a laser. The depth of the resistance portion 123A may be 0.5 μm or more. The difference between the thickness of the electrode conductor 12a in the first region 121 and the thickness of the electrode conductor 12a in the resistance portion 123A may be less than 20% of the thickness of the electrode conductor 12a in the first region 121. In addition, the vicinity of the resistance portion 123A may also be raised more than other regions of the electrode conductor 12a. That is, the thickness of the first region 121 and the second region 122 in the vicinity of the resistance portion 123A may be thicker than the thickness of the electrode conductor 12a in the first region 121 away from the resistance portion 123A.

[0063] In addition, the surface roughness of the bottom or at least one side of the resistance portion 123A may be smaller than that of the first region 121. By having such a surface roughness at the bottom or side of the resistance portion 123A, the resistance portion 123A shows a higher resistance to the electrolyte moving along the surface of the electrode conductor 12a. Therefore, the possibility of poor connection between the connection terminal 22 and the electrode conductor 12a can be further reduced. When the surface roughness of the bottom or side of the resistance portion 123A is smaller than that of the first region 121, the specific surface roughness of the bottom or side of the resistance portion 123A may be the same as the surface roughness of the above-mentioned roughness reduction region. Furthermore, the bottom or at least one side of the resistance portion 123A may also include a gap portion on the inner side of the surface. The gap portion is formed by, for example, taking in the surrounding air of the portion heated by the laser in the process of cooling after the resistance portion 123A is formed by laser, or by deformation caused by expansion and contraction of the electrode conductor 12a. Alternatively, a recessed portion may be further formed on the surface of the electrode conductor 12 a at the bottom portion or at least one side portion of the resistance portion 123A.

[0064] (Variant 2)

[0065] Fig.10 FIG. 1 is a schematic cross-sectional view showing a resistance portion 123B of a second modified example of the resistance portion 123. Fig.10As shown, the resistance portion 123B may be a member having a thickness different from that of the electrode conductor 12a and located on the surface of the electrode conductor 12a. In this case, the resistance portion 123B blocks the movement of the electrolyte along the surface of the electrode conductor 12a, and exhibits a higher resistance to the movement than the first region 121.

[0066] The material constituting the resistance portion 123B in this modification example may be any material as long as it can be liquid-tightly bonded to the surface of the electrode conductor 12a and is impermeable to the electrolyte. A specific example of the material constituting the resistance portion 123B is styrene-butadiene rubber.

[0067] (Variant 3)

[0068] Fig.11 1 is a plan view showing a modification of the unit cell 10 having the negative electrode 12. In this modification, the resistance portion 123 includes a region having a smaller surface roughness than the first region 121 (roughness reduced region).

[0069] As described above, in the unit cell 10, the first container 15 can contain the electrode body 14. At this time, the exposed portion 12e of the electrode conductor 12a protrudes from the first container 15. In addition, as described above, the first container 15 can be sealed at the peripheral portion in a state where the electrode body 14 is contained. In the following description, the portion of the first container 15 where the edge of the first container 15 protruding along the exposed portion 12e is sealed is referred to as a sealing portion 151.

[0070] In the first embodiment, the position of the sealing portion 151 is not particularly limited, and may be located, for example, between the first region 121 and the resistance portion 123. Fig.11 As shown, in this variation, the sealing portion 151 can be located in the resistance portion 123. The degree of close contact of the sealing portion 151 with respect to the roughness reduction area included in the resistance portion 123 is higher than the degree of close contact of the sealing portion 151 with respect to the area outside the roughness reduction area. In the roughness reduction area, the sealing portion 151 is in close contact, so that the resistance to the movement of the electrolyte along the surface of the electrode conductor 12a becomes higher than the case where the sealing portion 151 is not in close contact with the roughness reduction area. Therefore, in the resistance portion 123 including the roughness reduction area, the resistance of the resistance portion 123 to the movement of the electrolyte along the surface of the electrode conductor 12a can be further increased compared with the case where the sealing portion 151 is not located in the resistance portion 123.

[0071] As described above, according to the electrode body 14 and the unit cell 10 of the present disclosure, the possibility of poor connection between the connection terminal 22 welded to the second region 122 and the electrode conductor 12a due to the adhesion of the electrolyte to the second region 122 can be reduced. Therefore, the possibility of defective secondary batteries 1 can be reduced. Therefore, the energy and resources consumed in the manufacture of defective secondary batteries 1 can be saved, and thus, it can contribute to the achievement of sustainable development goals (SDGs).

[0072] [Additional Notes]

[0073] The invention of the present disclosure is described above based on the drawings and embodiments. However, the invention of the present disclosure is not limited to the above-mentioned embodiments. That is, the invention of the present disclosure can be variously modified within the scope shown in the present disclosure, and the embodiments obtained by appropriately combining the technical means respectively disclosed in different embodiments are also included in the technical scope of the invention of the present disclosure. In other words, it should be noted that it is easy for those skilled in the art to make various deformations or modifications according to the present disclosure. In addition, it should be noted that these deformations or modifications are included in the scope of the present disclosure.

[0074] Description of Reference Numerals

[0075] 10-cell battery (storage element)

[0076] 11a Electrode conductor

[0077] 11b Positive electrode active material layer (electrode active material layer)

[0078] 11c Positive electrode active material (electrode active material)

[0079] 12a Electrode conductor

[0080] 12b Negative electrode active material layer (electrode active material layer)

[0081] 12c Negative active material (electrode active material)

[0082] 121 First Area

[0083] 122 Second Area

[0084] 123 resistance part

[0085] 14 Electrode body

[0086] 15 first container (container)

[0087] 151 Sealing part

Claims

1. An electrode body, in, have: An active material layer, including an electrode active material and an electrolyte; an electrode conductor having (i) a first region where the active material layer is located and (ii) a second region that is electrically connectable to a connection terminal, the second region being a region different from the first region; as well as The resistance portion is located closer to the second region than the first region of the electrode conductor, and exhibits higher resistance than the first region to movement of the electrolyte along the surface of the electrode conductor on the side where the active material layer is located.

2. The electrode body according to claim 1, in, The resistance portion includes a region on the surface of the electrode conductor having a surface roughness smaller than that of the first region.

3. The electrode body according to claim 2, in, A difference between the thickness of the electrode conductor in the first region and the thickness of the electrode conductor in a region of the resistance portion having a surface roughness smaller than that of the first region is 20% or less of the thickness of the electrode conductor in the first region.

4. The electrode body according to any one of claims 1 to 3, in, The resistance portion is a part of the electrode conductor, The electrode conductor is bent in a convex shape toward the side opposite to the surface at the resistance portion.

5. The electrode body according to claim 1 or 2, in, The resistance portion is a recessed portion on the surface of the electrode conductor.

6. The electrode body according to claim 1 or 2, in, The resistance portion is a member that is located on the surface of the electrode conductor and has a thickness different from that of the electrode conductor.

7. The electrode body according to any one of claims 1 to 6, in, The resistance portion is arranged so as to be located on an arbitrary path along which the electrolyte solution moves from the first region to the second region on the surface of the electrode conductor.

8. An electric storage element, in, An electrode body according to any one of claims 1 to 7.

9. The electric storage element according to claim 8, in, The resistance portion includes a region having a surface roughness smaller than that of the first region on the surface of the electrode conductor, The power storage element includes a housing that houses the electrode body. A portion of the electrode conductor protrudes from the housing, A sealing portion of the housing body which is sealed in a state where the electrode body is housed is located at the resistance portion.