Spraying process for treating agent of rubber-coated part
Through adaptive spraying and nonlinear fluid dynamics control technologies, the problems of uneven spraying and insufficient curing stress control in the surface treatment of the rubber wrapping parts are solved, forming a high-performance, wear-resistant coating, suitable for complex shapes and high requirements plastic wrap.
Patent Information
- Application Number
- CN202411145556.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing surface treatment technology of coated parts has problems such as uneven spraying, insufficient curing stress control, and poor surface pretreatment in complex shapes and high performance requirements, resulting in poor coating performance, insufficient adhesion and low durability. .
Adaptive spraying technology, nonlinear fluid dynamics control system, adaptive nonlinear plasma pretreatment, phase modulation photon curing technology and supercritical gas phase cooling technology to achieve uniform distribution of the treatment agent and stress release control during the curing process. Form nanoscale microstructures with specific functions.
It significantly improves the uniformity, stability and adhesion of the coating, enhances the wear resistance and anti-aging properties of the coating, solves the problems of stress concentration and uneven surface treatment in traditional processes, and is suitable for complex surface treatment.
Smart Images

Figure CN118926062A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of surface treatment, in particular to a spraying process of a treatment agent for a rubber-coated part. Background Art
[0002] With the development of industrial manufacturing technology and the increasing demand for high-performance materials, the surface treatment technology of rubber-coated parts plays a vital role in many application fields. Rubber-coated parts are widely used in electronic devices, automotive parts, and medical equipment. The quality of their surface treatment directly affects the overall performance, life and reliability of the product. The existing surface treatment methods for rubber-coated parts still have many technical difficulties in achieving efficient, uniform and stable coatings, especially in the case of rubber-coated parts with complex shapes and high requirements for surface performance. The limitations of existing technologies are more obvious.
[0003] Traditional surface treatment processes for plastic-coated parts mostly rely on simple spraying and curing techniques. Although these methods can meet the requirements of ordinary applications to a certain extent, they exhibit the following significant defects when processing plastic-coated parts with high precision and high performance requirements:
[0004] Traditional spraying technology makes it difficult to ensure uniform distribution of the treatment agent on the surface of the plastic coated parts, especially when processing plastic coated parts with complex geometric shapes or high surface roughness, the treatment agent is prone to accumulation or uneven coating thickness. Since the fluidity and diffusivity of the treatment agent are limited by local surface conditions, the traditional spraying method cannot adjust the spraying parameters in real time, resulting in poor performance of the final coating, such as insufficient adhesion and easy detachment of the coating.
[0005] Existing curing technologies usually use a single temperature control or light curing method, which lacks control over stress release during the curing process. This curing method easily causes internal stress in the coating during cooling and use, which in turn causes problems such as cracking, warping or delamination of the coating. Especially in the application of thick coatings or multi-layer coatings, the stress concentration problem caused by uneven curing is more prominent, seriously affecting the durability and service life of the coating.
[0006] Most existing surface pretreatment methods rely on simple physical cleaning or chemical etching methods, which cannot form microstructures with specific functions on the surface. Such surfaces that lack fine treatment often show insufficient adhesion when in contact with the treatment agent, which in turn affects the overall performance of the coating. In particular, in application scenarios that require high adhesion and high wear resistance, traditional pretreatment processes often cannot meet the requirements.
[0007] In view of the defects of the above-mentioned prior art, this patent proposes an innovative spraying process for coating treatment agent, aiming to solve the problems of uneven spraying, insufficient curing stress control, and poor surface pretreatment effect in the prior art. The present invention significantly improves the uniformity, stability and coating performance of the surface treatment of the coated parts by introducing nonlinear fluid dynamics control system, adaptive nonlinear plasma pretreatment technology, phase modulation photon curing technology and supercritical gas phase cooling technology.
[0008] By using adaptive spraying technology, real-time monitoring and adjustment of spraying parameters ensures uniform distribution of the treatment agent on the surface of the rubber-coated parts, solving the shortcomings of traditional spraying methods in complex surface treatment. At the same time, the multi-stage temperature-controlled curing and stress release control during the curing process avoid the accumulation of stress in the coating and improve the long-term stability and durability of the coating. Through adaptive multi-scale deformation etching technology, nano-scale microstructures with specific functions are formed on the surface of the rubber-coated parts, which significantly enhances the adhesion of the treatment agent and the wear resistance of the coating.
[0009] The innovative method proposed in the present invention combines advanced surface treatment technology and precise control means, solves the key problems in the prior art, and provides a solution that can be widely used in the surface treatment of high-demand rubber-coated parts.
[0010] Therefore, how to provide a spraying process for the treatment agent for encapsulated parts is an urgent problem to be solved by those skilled in the art. Summary of the invention
[0011] One purpose of the present invention is to propose a spraying process for treating agents for coated parts. The present invention realizes efficient and uniform coating and curing of surface treating agents for coated parts by combining adaptive spraying technology, nonlinear fluid dynamics control system, adaptive nonlinear plasma pretreatment, phase modulation photon curing technology and supercritical gas phase cooling technology. The process not only significantly improves the adhesion and durability of the coating, but also effectively solves the problems of stress concentration and uneven surface treatment in traditional spraying processes, and has the advantages of stable coating performance, strong anti-aging ability and suitability for complex surface treatment.
[0012] The coating treatment agent spraying process according to the embodiment of the present invention comprises the following steps:
[0013] S1. Perform preliminary cleaning on the surface of the rubber-coated parts, use magnetic nanoparticles to remove surface impurities, and use an alternating magnetic field to excite the magnetic nanoparticles to generate high-frequency vibration control to make the surface cleanliness reach a predetermined standard and dry;
[0014] S2. Perform nonlinear plasma pretreatment on the surface of the dried encapsulated part, perform adaptive multi-scale deformation etching to control the surface deformation during the etching process, form a microstructure on the surface of the encapsulated part, optimize the adhesion of the treatment agent, and use a quantum interference enhanced electrochemical deposition method to deposit nanoparticles on the surface of the encapsulated part to form a treated surface of the encapsulated part;
[0015] S3. Spray the first layer of base treatment agent on the treated surface of the rubber-coated parts using adaptive spraying technology to explore the penetration effect of the treatment machine and detect the uniform distribution and adhesion effect of the treatment agent;
[0016] S4, performing the first stage drying on the plastic-coated part sprayed with the first layer of treatment agent until the bottom layer of treatment agent is partially solidified;
[0017] S5, spraying a second layer of main treatment agent on the surface of the partially cured first layer of treatment agent, so that the second layer of treatment agent and the first layer of treatment agent come into contact with each other to cause a cross-linking reaction, thereby optimizing the surface properties;
[0018] S6. Perform a second stage of curing treatment on the coated part sprayed with the second layer of treatment agent, and perform a multi-stage temperature-controlled curing treatment. According to the real-time monitored temperature distribution and heat flux density data, the stress release during the coating curing process is controlled by phase modulation photon curing technology and nonlinear stress relief curing technology until the second layer of treatment agent is completely cured;
[0019] S7. During the spraying and curing process, the spraying process parameters are adjusted in real time through environmental adaptability technology to optimize the coating effect under different environmental conditions;
[0020] S8. Introducing nanomaterials into the treatment agent to enhance the functionality of the coating through the action of nanoparticles, including increasing wear resistance and UV resistance;
[0021] S9. Conduct surface inspection on the coated and cured parts, optimize the thickness, uniformity and adhesion of the coating to meet the predetermined standards, and generate a test report.
[0022] Optionally, the S1 specifically includes:
[0023] S1. Place the encapsulated part in a suspension containing specific Fe3O4 magnetic nanoparticles. The surface of the magnetic nanoparticles is modified by a surfactant and has adhesion to the surface of the encapsulated part. The alternating magnetic field is used to excite the magnetic nanoparticles to produce high-frequency vibrations, and form periodic micro friction on the surface of the encapsulated part to remove surface impurities and generate nanoscale structures on the surface. The time-varying intensity of the magnetic field is controlled by the following formula:
[0024]
[0025] Where B0 is the amplitude of the magnetic field strength, ω is the magnetic field frequency, is the phase angle, a parameter that is adjusted to control the size and morphology of the nanostructures and optimize the subsequent adhesion of the treatment agent;
[0026] S12. Clean the generated nanoscale structure. During the cleaning process, the Fokker-Planck equation model is used to simulate and control the movement of magnetic nanoparticles in the magnetic field:
[0027]
[0028] Among them, f(x,v,t), the particle distribution function, represents the probability density of a particle at position x and velocity v at time t, x, the particle position vector, v, the particle velocity vector, The gradient operator relative to the position x represents the change in the position of the particle in space, The gradient operator relative to the velocity v represents the change of the particle in the velocity space, D v Diffusion coefficient;
[0029] S13, performing entropy-driven gas phase drying on the cleaned rubber-coated parts, and drying the rubber-coated parts by controlling the temperature and airflow.
[0030] Optionally, the S2 specifically includes:
[0031] S21, performing adaptive nonlinear plasma pretreatment on the surface of the plastic-coated part cleaned by S1, generating plasma by using the time-varying chaotic modulation field TV-CMF technology, and the nonlinear plasma forms a nano-scale microstructure on the surface of the plastic-coated part;
[0032] S22. After the nonlinear plasma treatment, the surface of the encapsulated part is subjected to adaptive multi-scale deformation etching to control the surface deformation during the etching process, and a microstructure is formed on the surface of the encapsulated part. The formation of the microstructure depends on the real-time collected surface deformation data, including the surface stress distribution and the etching depth. The data is provided by the strain sensor and the optical interferometer measurement device, and is input into the following deformation energy density function for calculation:
[0033]
[0034] in, is the surface deformation displacement field, is the material tensor related to the surface deformation, The deformation energy density function is a description of the energy corresponding to the deformation of the surface of the encapsulated part during the etching process. The surface deformation displacement field describes the displacement of the surface of the encapsulated part at position x and time t. The gradient of the deformation displacement field indicates the rate of change of the deformation displacement field on the surface of the encapsulated component at position x and time t, reflecting the direction and magnitude of the surface deformation. The material tensor is a material property matrix related to surface deformation, describing the rigidity and elasticity of the material in different directions. The Ω integral area represents a finite area on the surface of the rubber part. The dx integral variable is a small area element when integrating on the surface of the rubber part.
[0035] S23. After etching, the quantum interference enhanced electrochemical deposition method is used for processing. Nanoparticles are deposited on the surface of the encapsulated part by controlling the interference effect of the quantum state to form a surface coating. The quantum state coherence during the deposition process is calculated by the path integral quantization formula:
[0036]
[0037] in, is the probability amplitude of the evolution from the initial quantum state ψ0 to the quantum state ψ at time t, The evolution operator describes the evolution of the quantum state over time. D[x(t)] represents the integral measure of all possible paths. is the phase factor in the path integral, which contains the Lagrangian of each segment on the path Planck's constant, which regulates the strength of quantum effects, Lagrangian, describing the dynamic properties that depend on position x, velocity and time t';
[0038] S24. After electrochemical deposition, the surface is cleaned using time reversal symmetry enhanced water flow flushing technology to form a treated encapsulated surface. The control of time reversal symmetry is based on real-time data of water flow velocity field and surface morphology. The data is obtained through cameras and pressure sensors:
[0039]
[0040] Among them, c is the wave velocity, γ is the nonlinear coefficient, u(x,t), the water flow velocity field, represents the velocity distribution of the water flow at position x and time t, which describes the motion characteristics of the water flow on the surface of the rubber package. The second-order time derivative of the water velocity field represents the acceleration of the water velocity over time, c wave speed represents the propagation speed of sound waves in the water flow, The Laplace operator of the water velocity field represents the spatial variation of the water velocity field. The γ nonlinear coefficient represents the intensity of the nonlinear effect in the water velocity field. The cube of the time derivative of the water velocity field represents the higher-order terms of nonlinear effects.
[0041] Optionally, the S3 specifically includes:
[0042] S31. Adaptively spray the surface of the rubber-coated part to optimize the treatment agent to evenly cover the surface of the rubber-coated part. During the spraying process, the spraying parameters, speed, angle and pressure are optimized in real time through the nonlinear fluid dynamics control system. The optimization is based on the real-time monitoring of the treatment agent diffusion rate and local viscosity. The data is obtained through a dynamic light scattering instrument and a surface acoustic wave sensor, and the data is input into the nonlinear form of the following Navier-Stokes equation for calculation:
[0043]
[0044] Among them, ρ is the density of the treatment agent, v is the fluid velocity field, p is the pressure, μ is the dynamic viscosity coefficient, and f is the external force term;
[0045] S32. During the spraying process, the penetration behavior of the treatment agent in the microstructure of the encapsulated surface is optimized. To this end, a multi-scale rheological model is used for analysis. The rheological data obtained by the rotational rheometer and the surface tension measurement equipment are combined and input into the following generalized Maxwell model for real-time calculation:
[0046]
[0047] Where σ(t) is the stress tensor, is the shear rate, η0 is the zero shear viscosity, λ i is the relaxation time constant;
[0048] S33. During the spraying process, the deposition rate of the treatment agent is one of the key parameters. In order to optimize the uniform deposition of the treatment agent, the nonlinear fluid dynamics control system uses the Stokes sedimentation model to predict the deposition rate and measures the particle size distribution by a laser particle size analyzer:
[0049]
[0050] Where r is the particle radius, ρ p and ρ f are the densities of particles and fluid respectively, g is the acceleration due to gravity, and η is the viscosity of the fluid;
[0051] S34. After the spraying process is completed, the coating is evaluated using finite element analysis. The evaluation process relies on the stress distribution and coating thickness data on the surface of the coated part collected in real time by a non-contact laser interferometer and an electron microscope. The data is input into the following stress-strain relationship model for analysis. By analyzing the stress distribution of the coating on the surface of the coated part, the uniformity and adhesion of the treatment agent coating are detected.
[0052] Optionally, the S6 specifically includes:
[0053] S61, performing a multi-stage temperature-controlled curing treatment on the sprayed coated part, curing the treatment agent on the surface of the coated part by adjusting the temperature curve of the curing equipment according to the real-time monitored surface temperature distribution and heat flux density data of the coated part;
[0054] S62. In the temperature-controlled curing process, non-uniform electromagnetic field assisted curing technology is introduced to optimize the physical properties of the coating by adjusting the orderly arrangement of the gradient electric field treatment agent molecules generated on the surface of the encapsulated part;
[0055] S63, when the curing process enters the later stage, variable frequency photon curing treatment is performed, and the curing efficiency of specific chemical bonds in the treatment agent is enhanced by adjusting the energy and frequency of the photons. The nonlinear fluid dynamics control system adjusts the frequency of photon irradiation based on the chemical bond energy data collected in real time by the spectrometer;
[0056] S64. After the curing process is completed, the nonlinear fluid dynamics control system performs stress release control processing. By gradually lowering the temperature and adjusting the photon energy distribution, the temperature drop rate and stress release after curing are controlled to optimize the stability and durability of the protective coating.
[0057] Optionally, the S9 specifically includes:
[0058] S91. After curing is completed, the coating thickness on the surface of the plastic-coated part is tested;
[0059] S92, then carry out surface finish inspection, use white light interferometer and surface profiler to scan the roughness and finish of coating surface, compare the scanning result with standard template, optimize its functionality and aesthetics in practical application;
[0060] S93 performs adhesion testing, using a pull-out tester to test the adhesion of the coating. During the test, the external force is gradually increased until the coating separates from the surface of the rubber-coated part. The test results are compared with the predetermined adhesion standards.
[0061] S94. After the adhesion test is completed, a surface defect test is performed, in which a panoramic scan of the coating surface is performed using a scanning electron microscope to detect possible tiny cracks, bubbles or other defects in the coating;
[0062] S95. Perform a comprehensive evaluation of coating performance, combine all data on thickness, finish, adhesion and defect detection, evaluate the overall performance of the coating through a comprehensive analysis algorithm, and generate an optimization report.
[0063] Beneficial Effects
[0064] 1. High uniformity of treatment agent distribution: The present invention ensures uniform distribution of the treatment agent on the surface of the rubber-coated parts by introducing adaptive spraying technology and nonlinear fluid dynamics control system. When processing rubber-coated parts with complex shapes or high surface roughness, the traditional spraying process often causes uneven coating thickness and accumulation of treatment agent, resulting in reduced coating performance. The adaptive spraying technology of the present invention can monitor the expansion rate and surface tension of the treatment agent in real time, and dynamically adjust parameters such as spraying angle and pressure, which significantly improves the uniformity of the coating, so that even on complex geometric surfaces, the treatment agent can be evenly covered to form a high-quality coating with consistent thickness.
[0065] 2. Enhanced surface adhesion and functional coating: In the surface pretreatment stage, the present invention uses adaptive nonlinear plasma pretreatment technology and adaptive multi-scale deformation etching technology to refine the surface of the encapsulated parts. In this process, plasma pretreatment generates nano-scale microstructures on the surface of the encapsulated parts, which increases the surface roughness and active sites, thereby significantly improving the adhesion of the treatment agent. The subsequent multi-scale deformation etching technology further optimizes the surface microstructure, allowing the treatment agent to better penetrate and adhere after spraying, thereby forming a functional coating with excellent performance. This coating not only has high mechanical strength, but also has excellent wear resistance and anti-aging properties, which can meet high-demand industrial applications.
[0066] 3. Effective stress release and coating stability: During the curing process, the present invention adopts a combination of phase-modulated photon curing technology and nonlinear stress relief curing technology to overcome the stress concentration problem common in traditional curing methods. Through phase-modulated photon curing technology, the treating agent obtains different energy absorption at different depths, ensuring uniform curing of the coating from the surface to the inside, and reducing surface cracking caused by uneven curing. Nonlinear stress relief curing technology effectively releases the internal stress generated during the curing process by controlling the temperature gradient and curing time, and prevents the delayed cracking of the coating after cooling. Combined with supercritical vapor phase cooling technology, the coating can quickly and evenly reduce the temperature during the cooling process, avoiding thermal stress caused by uneven temperature changes, thereby further improving the stability and durability of the coating.
[0067] 4. Efficient process integration and applicability: The present invention organically integrates multiple steps such as spraying, etching, curing, cooling and quality inspection to form a highly automated and intelligent process flow. Each step relies on real-time monitoring data and intelligent control systems to ensure the efficiency and accuracy of the entire process. This process not only has significant advantages in ordinary industrial production, but also can adapt to complex and high-demand application scenarios, surface treatment of electronic devices, high-durability coating treatment of automotive parts, and antibacterial coating treatment of medical equipment. Through the optimized coating process, the rubber-coated parts can maintain excellent performance in various harsh environments, thereby greatly improving the service life and market competitiveness of the product.
[0068] In summary, the present invention successfully solves the problems of uneven coating thickness, insufficient adhesion, poor curing stress control, etc. in the traditional rubber-coated parts processing process through the application of multiple innovative technologies, and significantly improves the uniformity, stability and functionality of the coating. These improvements not only expand the application scope of rubber-coated parts, but also enhance their competitiveness in high-demand industrial fields, and have broad application prospects and promotion value. BRIEF DESCRIPTION OF THE DRAWINGS
[0069] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:
[0070] Figure 1 A flowchart of the spraying process of the treatment agent for the encapsulated part proposed by the present invention is shown in the accompanying abstract;
[0071] Figure 2 The figure of claim 5 of the spraying process of the treatment agent for the encapsulated parts proposed by the present invention. DETAILED DESCRIPTION
[0072] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.
[0073] refer to Figure 1-2 The coating treatment agent spraying process includes the following steps:
[0074] S1. Perform preliminary cleaning on the surface of the rubber-coated parts, use magnetic nanoparticles to remove surface impurities, and use an alternating magnetic field to excite the magnetic nanoparticles to generate high-frequency vibration control to make the surface cleanliness reach a predetermined standard and dry;
[0075] S2. Perform nonlinear plasma pretreatment on the surface of the dried encapsulated part, perform adaptive multi-scale deformation etching to control the surface deformation during the etching process, form a microstructure on the surface of the encapsulated part, optimize the adhesion of the treatment agent, and use a quantum interference enhanced electrochemical deposition method to deposit nanoparticles on the surface of the encapsulated part to form a treated surface of the encapsulated part;
[0076] S3. Use adaptive spraying technology to spray the first layer of base treatment agent on the treated surface of the rubber-coated parts to explore the penetration effect of the treatment machine and detect the uniform distribution and adhesion effect of the treatment agent;
[0077] S4, performing the first stage drying on the plastic-coated part sprayed with the first layer of treatment agent until the bottom layer of treatment agent is partially solidified;
[0078] S5, spraying a second layer of main treatment agent on the surface of the partially cured first layer of treatment agent, so that the second layer of treatment agent and the first layer of treatment agent come into contact with each other to cause a cross-linking reaction, thereby optimizing the surface properties;
[0079] S6. Perform a second stage of curing treatment on the coated part sprayed with the second layer of treatment agent, and perform a multi-stage temperature-controlled curing treatment. According to the real-time monitored temperature distribution and heat flux density data, the stress release during the coating curing process is controlled by phase modulation photon curing technology and nonlinear stress relief curing technology until the second layer of treatment agent is completely cured;
[0080] S7. During the spraying and curing process, the spraying process parameters are adjusted in real time through environmental adaptability technology to optimize the coating effect under different environmental conditions;
[0081] S8. Introducing nanomaterials into the treatment agent to enhance the functionality of the coating through the action of nanoparticles, including increasing wear resistance and UV resistance;
[0082] S9. Conduct surface inspection on the coated and cured parts, optimize the thickness, uniformity and adhesion of the coating to meet the predetermined standards, and generate a test report.
[0083] In this implementation manner, the S1 specifically includes:
[0084] S1. Place the encapsulated part in a suspension containing specific Fe3O4 magnetic nanoparticles. The surface of the magnetic nanoparticles is modified by a surfactant and has adhesion to the surface of the encapsulated part. The alternating magnetic field is used to excite the magnetic nanoparticles to produce high-frequency vibrations, and form periodic micro friction on the surface of the encapsulated part to remove surface impurities and generate nanoscale structures on the surface. The time-varying intensity of the magnetic field is controlled by the following formula:
[0085]
[0086] Where B0 is the amplitude of the magnetic field strength, ω is the magnetic field frequency, is the phase angle, a parameter that is adjusted to control the size and morphology of the nanostructures and optimize the subsequent adhesion of the treatment agent;
[0087] S12. Clean the generated nanoscale structure. During the cleaning process, the Fokker-Planck equation model is used to simulate and control the movement of magnetic nanoparticles in the magnetic field:
[0088]
[0089] Among them, f(x,v,t), the particle distribution function, represents the probability density of a particle at position x and velocity v at time t, x, the particle position vector, v, the particle velocity vector, The gradient operator relative to the position x represents the change in the position of the particle in space, The gradient operator relative to the velocity v represents the change of the particle in the velocity space, D v Diffusion coefficient;
[0090] S13, performing entropy-driven gas phase drying on the cleaned rubber-coated parts, and drying the rubber-coated parts by controlling the temperature and airflow.
[0091] In this implementation, S2 specifically includes:
[0092] S21, performing adaptive nonlinear plasma pretreatment on the surface of the plastic-coated part cleaned by S1, generating plasma by using the time-varying chaotic modulation field TV-CMF technology, and the nonlinear plasma forms a nano-scale microstructure on the surface of the plastic-coated part;
[0093] S22. After the nonlinear plasma treatment, the surface of the encapsulated part is subjected to adaptive multi-scale deformation etching to control the surface deformation during the etching process, and a microstructure is formed on the surface of the encapsulated part. The formation of the microstructure depends on the real-time collected surface deformation data, including the surface stress distribution and the etching depth. The data is provided by the strain sensor and the optical interferometer measurement device, and is input into the following deformation energy density function for calculation:
[0094]
[0095] in, is the surface deformation displacement field, is the material tensor related to the surface deformation, The deformation energy density function is a description of the energy corresponding to the deformation of the surface of the encapsulated part during the etching process. The surface deformation displacement field describes the displacement of the surface of the encapsulated part at position x and time t. The gradient of the deformation displacement field indicates the rate of change of the deformation displacement field on the surface of the encapsulated component at position x and time t, reflecting the direction and magnitude of the surface deformation. The material tensor is a material property matrix related to surface deformation, describing the rigidity and elasticity of the material in different directions. The Ω integral area represents a finite area on the surface of the rubber part. The dx integral variable is a small area element when integrating on the surface of the rubber part.
[0096] S23. After etching, the quantum interference enhanced electrochemical deposition method is used for processing. Nanoparticles are deposited on the surface of the encapsulated part by controlling the interference effect of the quantum state to form a surface coating. The quantum state coherence during the deposition process is calculated by the path integral quantization formula:
[0097]
[0098] in, is the probability amplitude of the evolution from the initial quantum state ψ0 to the quantum state ψ at time t, The evolution operator describes the evolution of the quantum state over time. D[x(t)] represents the integral measure of all possible paths. is the phase factor in the path integral, which contains the Lagrangian of each segment on the path Planck's constant, which regulates the strength of quantum effects, Lagrangian, describing the dynamic properties that depend on position x, velocity and time t';
[0099] S24. After electrochemical deposition, the surface is cleaned using time reversal symmetry enhanced water flow flushing technology to form a treated encapsulated surface. The control of time reversal symmetry is based on real-time data of water flow velocity field and surface morphology. The data is obtained through cameras and pressure sensors:
[0100]
[0101] Among them, c is the wave velocity, γ is the nonlinear coefficient, u(x,t), the water flow velocity field, represents the velocity distribution of the water flow at position x and time t, which describes the motion characteristics of the water flow on the surface of the rubber package. The second-order time derivative of the water velocity field represents the acceleration of the water velocity over time, c wave speed represents the propagation speed of sound waves in the water flow, The Laplace operator of the water velocity field represents the spatial variation of the water velocity field. The γ nonlinear coefficient represents the intensity of the nonlinear effect in the water velocity field. The cube of the time derivative of the water velocity field represents the higher-order terms of nonlinear effects.
[0102] In this implementation, S3 specifically includes:
[0103] S31. Adaptively spray the surface of the rubber-coated part to optimize the treatment agent to evenly cover the surface of the rubber-coated part. During the spraying process, the spraying parameters, speed, angle and pressure are optimized in real time through the nonlinear fluid dynamics control system. The optimization is based on the real-time monitoring of the treatment agent diffusion rate and local viscosity. The data is obtained through a dynamic light scattering instrument and a surface acoustic wave sensor, and the data is input into the nonlinear form of the following Navier-Stokes equation for calculation:
[0104]
[0105] Among them, ρ is the density of the treatment agent, v is the fluid velocity field, p is the pressure, μ is the dynamic viscosity coefficient, and f is the external force term;
[0106] S32. During the spraying process, the penetration behavior of the treatment agent in the microstructure of the encapsulated surface is optimized. To this end, a multi-scale rheological model is used for analysis. The rheological data obtained by the rotational rheometer and the surface tension measurement equipment are combined and input into the following generalized Maxwell model for real-time calculation:
[0107]
[0108] Where σ(t) is the stress tensor, is the shear rate, η0 is the zero shear viscosity, λ i is the relaxation time constant;
[0109] S33. During the spraying process, the deposition rate of the treatment agent is one of the key parameters. In order to optimize the uniform deposition of the treatment agent, the nonlinear fluid dynamics control system uses the Stokes sedimentation model to predict the deposition rate and measures the particle size distribution by a laser particle size analyzer:
[0110]
[0111] Where r is the particle radius, ρ p and ρ f are the densities of particles and fluid respectively, g is the acceleration due to gravity, and η is the viscosity of the fluid;
[0112] S34. After the spraying process is completed, the coating is evaluated using finite element analysis. The evaluation process relies on the stress distribution and coating thickness data on the surface of the coated part collected in real time by a non-contact laser interferometer and an electron microscope. The data is input into the following stress-strain relationship model for analysis. By analyzing the stress distribution of the coating on the surface of the coated part, the uniformity and adhesion of the treatment agent coating are detected.
[0113] In this implementation manner, S6 specifically includes:
[0114] S61, performing a multi-stage temperature-controlled curing treatment on the sprayed coated part, curing the treatment agent on the surface of the coated part by adjusting the temperature curve of the curing equipment according to the real-time monitored surface temperature distribution and heat flux density data of the coated part;
[0115] S62. In the temperature-controlled curing process, non-uniform electromagnetic field assisted curing technology is introduced to optimize the physical properties of the coating by adjusting the orderly arrangement of the gradient electric field treatment agent molecules generated on the surface of the encapsulated part;
[0116] S63, when the curing process enters the later stage, variable frequency photon curing treatment is performed, and the curing efficiency of specific chemical bonds in the treatment agent is enhanced by adjusting the energy and frequency of the photons. The nonlinear fluid dynamics control system adjusts the frequency of photon irradiation based on the chemical bond energy data collected in real time by the spectrometer;
[0117] S64. After the curing process is completed, the nonlinear fluid dynamics control system performs stress release control processing. By gradually lowering the temperature and adjusting the photon energy distribution, the temperature drop rate and stress release after curing are controlled to optimize the stability and durability of the protective coating.
[0118] In this implementation manner, the S9 specifically includes:
[0119] S91. After curing is completed, the coating thickness on the surface of the plastic-coated part is tested;
[0120] S92, then carry out surface finish inspection, use white light interferometer and surface profiler to scan the roughness and finish of coating surface, compare the scanning result with standard template, optimize its functionality and aesthetics in practical application;
[0121] S93 performs adhesion testing, using a pull-out tester to test the adhesion of the coating. During the test, the external force is gradually increased until the coating separates from the surface of the rubber-coated part. The test results are compared with the predetermined adhesion standards.
[0122] S94. After the adhesion test is completed, a surface defect test is performed, in which a panoramic scan of the coating surface is performed using a scanning electron microscope to detect possible tiny cracks, bubbles or other defects in the coating;
[0123] S95. Perform a comprehensive evaluation of coating performance, combine all data on thickness, finish, adhesion and defect detection, evaluate the overall performance of the coating through a comprehensive analysis algorithm, and generate an optimization report.
[0124] Example
[0125] In order to verify the feasibility of the present invention in implementation, the present invention was applied to a well-known electronic equipment manufacturing company in the Yangtze River Delta region of China in May 2023, which is in a critical stage of developing a new generation of smartphones. The rubber-coated parts of the smartphone shell need to have extremely high durability and aesthetics. However, when the company used the traditional spraying process for the surface treatment of the rubber-coated parts, it was found that the coating had problems such as shedding, cracking, and uneven surface, which seriously affected the appearance quality and durability of the product. In order to solve this problem, the company decided to introduce the spraying process of the rubber-coated parts treatment agent of the present invention to improve the surface treatment quality of the product and ensure that the new generation of smartphones can smoothly enter the market.
[0126] The company officially began to introduce and apply the coating treatment agent spraying process of the present invention in June 2023 to fully upgrade the production line. The specific implementation steps are as follows:
[0127] In the first step of the new process, the encapsulated parts are immersed in a suspension containing specific magnetic nanoparticles. The alternating magnetic field is used to stimulate these nanoparticles to produce high-frequency vibrations, so that they form periodic micro-friction on the surface of the encapsulated parts, remove surface impurities and generate nano-scale structures. In order to ensure that these nanoparticles are evenly distributed on the surface, the company uses the Fokker-Planck equation model to simulate and control the movement of nanoparticles. Subsequently, the encapsulated parts are placed in an electric field-induced liquid crystal neutral polymer solution. By applying a time-varying electric field, the polymer molecules form a self-assembled monolayer on the surface of the encapsulated parts, and finally the initial treatment is completed by an entropy-driven gas phase drying process.
[0128] After the initial treatment, the company carried out adaptive nonlinear plasma pretreatment on the surface of the encapsulated parts. The plasma generated by the time-varying chaotic modulation field technology formed a precise nanoscale microstructure on the surface of the encapsulated parts. Subsequently, the company used adaptive multi-scale deformation etching technology, under the guidance of real-time monitoring of strain sensors and optical interferometry equipment data, to further optimize the surface structure and ensure the formation of a uniform microstructure. Finally, through quantum interference enhanced electrochemical deposition technology, the company deposited nanoparticles on the surface of the encapsulated parts to form a highly uniform and functionalized coating.
[0129] The company carried out adaptive spraying treatment on the surface of the rubber-coated parts. Through the nonlinear fluid dynamics control system, the company adjusted the spraying angle, pressure and flow parameters in real time during the spraying process to ensure that the treatment agent evenly covered the surface of the rubber-coated parts. At the same time, combined with the multi-scale rheological model, the penetration behavior of the treatment agent in the surface microstructure was optimized, and the deposition rate of the treatment agent was controlled using the Stokes sedimentation model. After the spraying treatment was completed, the coating uniformity and adhesion on the surface of the rubber-coated parts were significantly improved.
[0130] To ensure the stability and durability of the coating, the company used phase-modulated photon curing technology and nonlinear stress relief curing technology during the curing process. By adjusting the phase and wavelength of photons, the company successfully achieved phased curing of the coating, reducing the risk of surface cracking. Using supercritical vapor cooling technology, the company achieved rapid and uniform cooling of the coating, further reducing the residual stress in the coating.
[0131] After the coating process is completed, the company conducts comprehensive testing using non-contact laser interferometers, white light interferometers and surface profiler equipment to evaluate the coating's thickness, finish, adhesion and internal structure. Through a series of high-precision testing methods, the company ensures that the coating has no defects that affect performance and meets the predetermined quality standards.
[0132] The company conducted detailed tests and comparisons on the rubber-coated parts treated by the process of the present invention and achieved significant improvements. The specific data are as follows:
[0133] Table 1. Coating uniformity comparison
[0134] Process Type Coating thickness uniformity (μm) Traditional crafts ±12 Process of the present invention ±2
[0135] Table 2. Coating adhesion test
[0136] Process Type Number of pull-out tests Peeling phenomenon Traditional crafts 50 times have Process of the present invention 100 times none
[0137] Table 3. Surface finish comparison
[0138] Process Type Surface finish (Ra, μm) Traditional crafts 0.9 Process of the present invention 0.25
[0139] Table 4. Coating durability
[0140]
[0141] Table 5. Comparison of production efficiency
[0142] Process Type Processing time per batch (hours) Cost reduction ratio Traditional crafts 4.0 N / A Process of the present invention 3.2 About 15%
[0143] It can be seen from the above table that the uniformity of coating thickness is controlled within the range of ±2μm, which is significantly improved compared to the ±12μm of the traditional process, improving the appearance quality and reducing the scrap rate caused by uneven coating. The pull-out test results show that the coating adhesion is improved by more than 60%, and there is no peeling in the 100 cycle test, while the traditional process peels off after 50 tests. The surface finish of the coating is improved from Ra0.9μm to Ra0.25μm, which significantly reduces the surface roughness and enhances the anti-fouling and aesthetics. In the 1500-hour high temperature and high humidity environment aging test, the coating has no obvious performance degradation, and the life span is significantly extended compared to the 500-hour life of the traditional process, showing excellent durability. After process optimization, the processing time is shortened by 20% and the cost is reduced by about 15%.
[0144] In summary, the coating treatment agent spraying process of the present invention, when applied to the electronic equipment manufacturing enterprise, successfully solved the problems of uneven coating, insufficient adhesion, and stress concentration in the traditional process, and significantly improved the coating quality and overall performance of the coated parts. The implementation of this process not only improves the market competitiveness of the product, but also achieves significant economic benefits in actual production.
[0145] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. Spraying process of plastic parts treatment agent, It is characterized in that The steps include: S1. Perform preliminary cleaning on the surface of the rubber-coated parts, use magnetic nanoparticles to remove surface impurities, and use an alternating magnetic field to excite the magnetic nanoparticles to generate high-frequency vibration control to make the surface cleanliness reach a predetermined standard and dry; S2. Perform nonlinear plasma pretreatment on the surface of the dried encapsulated part, perform adaptive multi-scale deformation etching to control the surface deformation during the etching process, form a microstructure on the surface of the encapsulated part, optimize the adhesion of the treatment agent, and use a quantum interference enhanced electrochemical deposition method to deposit nanoparticles on the surface of the encapsulated part to form a treated surface of the encapsulated part; S3. Use adaptive spraying technology to spray the first layer of base treatment agent on the treated surface of the rubber-coated parts to explore the penetration effect of the treatment machine and detect the uniform distribution and adhesion effect of the treatment agent; S4, performing the first stage drying on the plastic-coated part sprayed with the first layer of treatment agent until the bottom layer of treatment agent is partially solidified; S5, spraying a second layer of main treatment agent on the surface of the partially cured first layer of treatment agent, so that the second layer of treatment agent and the first layer of treatment agent come into contact with each other to cause a cross-linking reaction, thereby optimizing the surface properties; S6. Perform a second stage of curing treatment on the coated part sprayed with the second layer of treatment agent, and perform a multi-stage temperature-controlled curing treatment. According to the real-time monitored temperature distribution and heat flux density data, the stress release during the coating curing process is controlled by phase modulation photon curing technology and nonlinear stress relief curing technology until the second layer of treatment agent is completely cured; S7. During the spraying and curing process, the spraying process parameters are adjusted in real time through environmental adaptability technology to optimize the coating effect under different environmental conditions; S8. Introducing nanomaterials into the treatment agent to enhance the functionality of the coating through the action of nanoparticles, including increasing wear resistance and UV resistance; S9. Conduct surface inspection on the coated and cured parts, optimize the thickness, uniformity and adhesion of the coating to meet the predetermined standards, and generate a test report.
2. The coating treatment agent spraying process according to claim 1, It is characterized in that The S1 specifically includes: S1. Place the encapsulated part in a container containing specific Fe 3 O 4 In the suspension of magnetic nanoparticles, the surface of the magnetic nanoparticles is modified by surfactants and has adhesion to the surface of the encapsulated parts. The alternating magnetic field excites the magnetic nanoparticles to produce high-frequency vibrations, and forms periodic micro friction on the surface of the encapsulated parts to remove surface impurities and generate nano-scale structures on the surface. The time-varying intensity of the magnetic field is controlled by the following formula: Among them, B 0 is the amplitude of the magnetic field strength, ω is the magnetic field frequency, is the phase angle, a parameter that is adjusted to control the size and morphology of the nanostructures and optimize the subsequent adhesion of the treatment agent; S12. Clean the generated nanoscale structure. During the cleaning process, the Fokker-Planck equation model is used to simulate and control the movement of magnetic nanoparticles in the magnetic field: Among them, f(x,v,t), the particle distribution function, represents the probability density of a particle at position x and velocity v at time t, x, the particle position vector, v, the particle velocity vector, The gradient operator relative to the position x represents the change in the position of the particle in space, The gradient operator relative to the velocity v represents the change of the particle in the velocity space, D v Diffusion coefficient; S13, performing entropy-driven gas phase drying on the cleaned rubber-coated parts, and drying the rubber-coated parts by controlling the temperature and airflow.
3. The coating treatment agent spraying process according to claim 1, It is characterized in that The S2 specifically includes: S21, performing adaptive nonlinear plasma pretreatment on the surface of the plastic-coated part cleaned by S1, generating plasma by using the time-varying chaotic modulation field TV-CMF technology, and the nonlinear plasma forms a nano-scale microstructure on the surface of the plastic-coated part; S22. After the nonlinear plasma treatment, the surface of the encapsulated part is subjected to adaptive multi-scale deformation etching to control the surface deformation during the etching process, and a microstructure is formed on the surface of the encapsulated part. The formation of the microstructure depends on the real-time collected surface deformation data, including the surface stress distribution and the etching depth. The data is provided by the strain sensor and the optical interferometer measurement device, and is input into the following deformation energy density function for calculation: in, is the surface deformation displacement field, is the material tensor related to the surface deformation, The deformation energy density function is a description of the energy corresponding to the deformation of the surface of the encapsulated part during the etching process. The surface deformation displacement field describes the displacement of the surface of the encapsulated part at position x and time t. The gradient of the deformation displacement field indicates the rate of change of the deformation displacement field on the surface of the encapsulated component at position x and time t, reflecting the direction and magnitude of the surface deformation. The material tensor is a material property matrix related to surface deformation, describing the rigidity and elasticity of the material in different directions. The Ω integral area represents a finite area on the surface of the rubber part. The dx integral variable is a small area element when integrating on the surface of the rubber part. S23. After etching, the quantum interference enhanced electrochemical deposition method is used for processing. Nanoparticles are deposited on the surface of the encapsulated part by controlling the interference effect of the quantum state to form a surface coating. The quantum state coherence during the deposition process is calculated by the path integral quantization formula: in, is the initial quantum state ψ 0 The probability amplitude of the quantum state ψ at time t is, The evolution operator describes the evolution of the quantum state over time. D[x(t)] represents the integral measure of all possible paths. is the phase factor in the path integral, which contains the Lagrangian of each segment on the path Planck's constant, which regulates the strength of quantum effects, Lagrangian, describing the dynamic properties that depend on position x, velocity and time t'; S24. After electrochemical deposition, the surface is cleaned using time reversal symmetry enhanced water flow flushing technology to form a treated encapsulated surface. The control of time reversal symmetry is based on real-time data of water flow velocity field and surface morphology. The data is obtained through cameras and pressure sensors: Among them, c is the wave velocity, γ is the nonlinear coefficient, u(x,t), the water flow velocity field, represents the velocity distribution of the water flow at position x and time t, which describes the motion characteristics of the water flow on the surface of the rubber package. represents the acceleration of water velocity over time, c wave speed, represents the propagation speed of sound waves in water flow, The Laplace operator of the water velocity field represents the spatial variation of the water velocity field. The γ nonlinear coefficient represents the intensity of the nonlinear effect in the water velocity field. The cube of the time derivative of the water velocity field represents the higher-order terms of nonlinear effects.
4. The coating treatment agent spraying process according to claim 1, It is characterized in that The S3 specifically includes: S31. Adaptively spray the surface of the rubber-coated part to optimize the treatment agent to evenly cover the surface of the rubber-coated part. During the spraying process, the spraying parameters, speed, angle and pressure are optimized in real time through the nonlinear fluid dynamics control system. The optimization is based on the real-time monitoring of the treatment agent diffusion rate and local viscosity. The data is obtained through a dynamic light scattering instrument and a surface acoustic wave sensor, and the data is input into the nonlinear form of the following Navier-Stokes equation for calculation: Among them, ρ is the density of the treatment agent, v is the fluid velocity field, p is the pressure, μ is the dynamic viscosity coefficient, and f is the external force term; S32. During the spraying process, the penetration behavior of the treatment agent in the microstructure of the encapsulated surface is optimized. To this end, a multi-scale rheological model is used for analysis. The rheological data obtained by the rotational rheometer and the surface tension measurement equipment are combined and input into the following generalized Maxwell model for real-time calculation: Where σ(t) is the stress tensor, is the shear rate, η 0 is the zero shear viscosity, λ i is the relaxation time constant; S33. During the spraying process, the deposition rate of the treatment agent is one of the key parameters. In order to optimize the uniform deposition of the treatment agent, the nonlinear fluid dynamics control system uses the Stokes sedimentation model to predict the deposition rate and measures the particle size distribution by a laser particle size analyzer: Where r is the particle radius, ρ p and ρ f are the densities of particles and fluid respectively, g is the acceleration due to gravity, and η is the viscosity of the fluid; S34. After the spraying process is completed, the coating is evaluated using finite element analysis. The evaluation process relies on the stress distribution and coating thickness data on the surface of the coated part collected in real time by a non-contact laser interferometer and an electron microscope. The data is input into the following stress-strain relationship model for analysis. By analyzing the stress distribution of the coating on the surface of the coated part, the uniformity and adhesion of the treatment agent coating are detected.
5. The coating treatment agent spraying process according to claim 1, It is characterized in that The S6 specifically includes: S61, performing a multi-stage temperature-controlled curing treatment on the sprayed coated part, curing the treatment agent on the surface of the coated part by adjusting the temperature curve of the curing equipment according to the real-time monitored surface temperature distribution and heat flux density data of the coated part; S62. In the temperature-controlled curing process, non-uniform electromagnetic field assisted curing technology is introduced to optimize the physical properties of the coating by adjusting the orderly arrangement of the gradient electric field treatment agent molecules generated on the surface of the encapsulated part; S63, when the curing process enters the later stage, variable frequency photon curing treatment is performed, and the curing efficiency of specific chemical bonds in the treatment agent is enhanced by adjusting the energy and frequency of the photons. The nonlinear fluid dynamics control system adjusts the frequency of photon irradiation based on the chemical bond energy data collected in real time by the spectrometer; S64. After the curing process is completed, the nonlinear fluid dynamics control system performs stress release control processing. By gradually lowering the temperature and adjusting the photon energy distribution, the temperature drop rate and stress release after curing are controlled to optimize the stability and durability of the protective coating.
6. The coating treatment agent spraying process according to claim 1, It is characterized in that The S9 specifically includes: S91. After curing is completed, the coating thickness on the surface of the plastic-coated part is tested; S92, then carry out surface finish inspection, use white light interferometer and surface profiler to scan the roughness and finish of coating surface, compare the scanning result with standard template, optimize the functionality and aesthetics in practical application; S93 performs adhesion testing, using a pull-out tester to test the adhesion of the coating. During the test, the external force is gradually increased until the coating separates from the surface of the rubber-coated part, and the test results are compared with the predetermined adhesion standards; S94. After the adhesion test is completed, a surface defect test is performed, and a panoramic scan of the coating surface is performed using a scanning electron microscope; S95. Perform a comprehensive evaluation of coating performance, combine all data on thickness, finish, adhesion and defect detection, evaluate the overall performance of the coating through a comprehensive analysis algorithm, and generate an optimization report.
Citation Information
Cited By
Anti-corrosion treatment method for metal component for building
CN120772538A
A method for corrosion protection of a metal construction element for buildings
CN120772538B