Microbial remediation method for hexavalent chromium contaminated soil
By mixing chromium-contaminated soil with biochar fixed uria for in situ accumulation, the structural characteristics of extracellular polymers and nanocomposite biochar are used to synergistically reduce the toxicity of hexavalent chromium, and hexavalent chromium pollution in the prior art is solved The problem of poor soil repair results has achieved efficient and low-cost repair results.
Patent Information
- Application Number
- CN202411245014.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-06
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing technologies are difficult to repair hexavalent chromium contaminated soil efficiently, with low energy consumption and low investment, especially due to the difficulty of separation of hexavalent chromium and the difficulty of separation of impurities in the soil, which leads to poor results in traditional repair methods.
The mixture of chromium-contaminated soil and biochar is used to fix uria in situ. Through the synergistic action of extracellular polymers and biochar, the biological activity and toxicity of hexavalent chromium are reduced, and the pore structure of nanocomposite biochar is used and Functional groups improve the adsorption and reduction effects of pollutants.
Effectively reduce the concentration and toxicity of hexavalent chromium in the soil, improve the repair effect, meet the national standards of hexavalent chromium concentration and leaching concentration requirements, and have good application potential.
Smart Images

Figure CN118926298A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of soil heavy metal pollution remediation, and specifically relates to a hexavalent chromium contaminated soil microbial remediation method. Background Art
[0002] The soil environment is an open system, and its quality is affected by multiple factors. The stacking and dumping of solid waste on the soil surface, the infiltration of hazardous wastewater into the soil, the landing of harmful substances in the atmosphere into the soil, the spillage of pollutants or the leakage of pipes / tanks during industrial production, etc., are all ways to cause soil pollution. Chromium is also one of the main soil pollutants. When the soil is contaminated by chromium, it will lead to soil degradation, crop yield reduction, and in severe cases, no grass will grow and lose its ecological function. Therefore, the soil contaminated by chromium must be repaired.
[0003] Chromium-contaminated soil contains a large amount of toxic hexavalent chromium, which is easily soluble in water and has strong permeability. In addition, the soil contains a large amount of weeds, dead wood, sand, and domestic garbage, which are difficult to separate and have high processing costs. It is difficult to achieve high-efficiency, low-energy, and low-investment repair effects using traditional repair methods. Therefore, a microbial repair method for hexavalent chromium-contaminated soil is needed to improve the repair effect. Summary of the invention
[0004] The purpose of the present invention is to provide a method for microbial remediation of hexavalent chromium contaminated soil, so as to solve the existing technical problems.
[0005] In order to achieve the above object, the present invention adopts the following technical solutions: The present invention provides a method for microbial remediation of hexavalent chromium contaminated soil, comprising the following steps: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the materials at 50-65%; Step (2) stacking and treating the material mixed uniformly in step (1) in situ, during which the moisture content of the material is maintained between 50% and 65%; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
[0006] Preferably, in step (1), the mass ratio of chromium-contaminated soil to biochar-fixed urolytic bacteria is 100:0.5-5.
[0007] Preferably, in step (1), the hexavalent chromium content in the chromium-contaminated soil is 300-600 mg / kg.
[0008] Preferably, in step (2), the in-situ stacking depth is 0.5-1 m; and the processing time is 20-30 days.
[0009] Preferably, in step (1), the method for preparing biochar-immobilized urolytic bacteria comprises the following steps: S1: 10-20 g of nanocomposite biochar was added to 200-400 mL of Arthrobacter creatinolyticus culture solution, and the mixture was shaken at 100-200 r / min for 1.5-2.5 h at 29-31° C., and then 500-1000 mL of 2% w / v sodium alginate solution was added to obtain a mixture; S2: The mixture was dropped into 500-1000 mL of 2% w / v CaCl2 solution, cross-linked at 3-5°C for 20-28 h, washed with sterile saline for 3-5 times, and dried to obtain biochar-fixed urolytic bacteria.
[0010] Preferably, the number of the Arthrobacter creatinolyticus Microbial Resource Center is 5604MTCC.
[0011] Preferably, the OD600 of the urolytic bacteria in the urolytic bacteria culture solution is 1.0.
[0012] Preferably, the method for preparing the nanocomposite biochar comprises the following steps: P1: Cut the discarded apples into small pieces, wash them with deionized water to remove impurities, and then dry them at 75-85 °C for 15-21 h to constant weight, and then crush them with a high-speed crusher to obtain apple pomace particles of 0.4-0.6 mm. Pyrolyze the apple pomace particles at 450-550 °C for 1.5-2.5 h, and grind them to obtain apple pomace biochar of 0.1-0.24 mm; P2: apple pomace biochar was added into 50wt% H3PO4 solution at a mass ratio of 1:1, soaked at room temperature for 20-28h, washed with deionized water for 3-5 times, and then dried at 75-85°C to constant weight to obtain phosphoric acid-modified apple pomace biochar; P3: In a nitrogen atmosphere, 20-40 g of phosphoric acid-modified apple pomace biochar, 840-1680 g of FeSO4·H2O, and 42-84 g of ZIF-8 were added to 20-40 L of water, stirred at 200-400 rpm at 25 °C for 0.5-1.5 h, then 10-20 L of 72.4 g / L NaBH4 aqueous solution was added, filtered, and the filter residue was washed with water 3-5 times, and dried at 70-80 °C in a N2 atmosphere to constant weight to obtain nanocomposite biochar.
[0013] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are: 1. The urolytic bacteria of the present invention can tolerate up to 100 ppm of Cr(VI) and can be effectively used for the restoration of chromium in soil; Cr(VI) is reduced outside the cell instead of being bioaccumulated or biosorbed, and the reduction of hexavalent chromium occurs outside the cell, which is because the urolytic bacteria produce extracellular polymeric substances (EPS), and functional groups such as hydroxyl, carboxyl and amine in the extracellular polymeric substances can serve as electron donors to provide electrons for the reduction of hexavalent chromium to trivalent chromium; the extracellular polymeric substances secreted by the urolytic bacteria serve as effective sites for heterogeneous nucleation, and when all functional groups on the extracellular polymeric substances are saturated with bound cations, the presence of free calcium ions under alkaline conditions promotes the nucleation of calcium carbonate on the extracellular polymeric substance matrix, and the proteins and acidic amino acids present in the EPS carry negative charges in an alkaline environment, and are easy to adsorb metal ions in the solution, providing a large number of nucleation sites for calcium carbonate precipitation, and can complex and chelate trivalent chromium, thereby reducing the biological activity and toxicity of chromium in the soil.
[0014] 2. In the present invention, due to the oxidative corrosion of phosphoric acid, the formation of pore structure is promoted, and surface dirt and impurities are cleaned and removed, thereby improving the smoothness and overall appearance of the biochar surface, and having a pore expansion effect, the apple pomace biochar has developed pores, which is beneficial to the dispersion of nanoparticles and the enrichment of pollutants; ZIF-8 is successfully deposited in the pores of biochar, and zero-valent iron rice particles are deposited in the pores of ZIF-8 and biochar. ZIF-8 can effectively disperse the nanoparticles, prevent the aggregation of zero-valent iron rice particles, and provide a large number of adsorption sites for the accumulation of Cr(VI), thereby promoting the subsequent reduction process.
[0015] 3. In the present invention, both pectin and hemicellulose in apples can prevent the formation of crystalline graphite and promote the generation of non-graphite carbon. The apple pomace biochar mainly presents an amorphous structure. The prepared biochar has a highly porous structure and contains abundant oxygen-containing functional groups (-OH, -COOH and C-O-C). The strong carboxyl and phenol functional groups with negative charges on the surface of biochar can increase the cation exchange capacity of the soil, thereby improving soil fertility and the adsorption capacity of inorganic and organic compounds. The present invention synergistically improves the effect of chromium-contaminated soil remediation by combining nanocomposite biochar and microorganisms, and has good application potential. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1The present invention is a preparation process flow chart of the method for microbial remediation of hexavalent chromium contaminated soil. DETAILED DESCRIPTION
[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0019] Example 1 This embodiment discloses a method for preparing nanocomposite biochar, comprising the following steps: P1: The discarded apples were cut into small pieces, washed with deionized water to remove impurities, and then dried at 80 °C for 18 h to constant weight, and then crushed with a high-speed crusher to obtain 0.5 mm apple pomace particles. The apple pomace particles were pyrolyzed at 500 °C for 2 h and ground to obtain 0.1-0.24 mm apple pomace biochar; P2: Apple pomace biochar was added into 50wt% H3PO4 solution at a mass ratio of 1:1, soaked at room temperature for 24h, washed with deionized water 4 times, and then dried at 80°C to constant weight to obtain phosphoric acid-modified apple pomace biochar; P3: In a nitrogen atmosphere, 30 g of phosphoric acid-modified apple pomace biochar, 1260 g of FeSO4·H2O, and 63 g of ZIF-8 were added to 30 L of water and stirred at 300 rpm at 25 °C for 1 h. Then, 15 L of 72.4 g / L NaBH4 aqueous solution was added, filtered, and the residue was washed with water for 4 times and dried at 75 °C in a N2 atmosphere to constant weight to obtain nanocomposite biochar.
[0020] Example 2 This embodiment discloses a method for preparing biochar-immobilized urolytic bacteria, comprising the following steps: S1: 15 g of nanocomposite biochar was added to 300 mL of Arthrobacter creatinolyticus culture solution, and the mixture was shaken at 150 r / min for 2 h at 30 °C, and then 750 mL of 2% w / v sodium alginate solution was added to obtain a mixture; S2: The mixture was dropped into 750 mL of 2% w / v CaCl2 solution, cross-linked at 4 °C for 24 h, washed four times with sterile saline, and dried to obtain biochar-immobilized urolytic bacteria.
[0021] The number of the Arthrobacter creatinolyticus Microbial Resource Center is 5604MTCC.
[0022] The optical density measurement value OD600 of the urolytic bacteria in the urolytic bacteria culture solution is 1.0.
[0023] Example 3 See also Figure 1 As shown, this embodiment discloses a method for microbial remediation of hexavalent chromium contaminated soil, comprising the following steps: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the materials at 58%; The hexavalent chromium content in the chromium-contaminated soil is 450 mg / kg; Step (2) stacking the uniformly mixed material in step (1) in situ for 25 days, during which the moisture content of the material is maintained between 50% and 65%; the in situ stacking depth is 0.75m; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
[0024] In the step (1), the mass ratio of the chromium-contaminated soil to the biochar-fixed urolytic bacteria is 2:100.
[0025] Example 4 See also Figure 1 As shown, this embodiment discloses a method for microbial remediation of hexavalent chromium contaminated soil, comprising the following steps: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the materials at 50%; The hexavalent chromium content in the chromium-contaminated soil is 600 mg / kg; Step (2) stacking the uniformly mixed material in step (1) in situ for 20 days, during which the moisture content of the material is maintained between 50% and 65%; the in situ stacking depth is 1m; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
[0026] In the step (1), the mass ratio of the chromium-contaminated soil to the biochar-fixed urolytic bacteria is 0.5:100.
[0027] Example 5 See also Figure 1 As shown, this embodiment discloses a method for microbial remediation of hexavalent chromium contaminated soil, comprising the following steps: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the materials at 65%; The hexavalent chromium content in the chromium-contaminated soil is 300 mg / kg; Step (2) stacking the uniformly mixed materials in step (1) in situ and treating them for 30 days, during which the moisture content of the materials is maintained between 50% and 65%; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
[0028] In the step (1), the mass ratio of the chromium-contaminated soil to the biochar-fixed urolytic bacteria is 5:100.
[0029] Example 6 See also Figure 1 As shown, this embodiment discloses a method for microbial remediation of hexavalent chromium contaminated soil, comprising the following steps: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the material at 52%; The hexavalent chromium content in the chromium-contaminated soil is 500 mg / kg; Step (2) the material mixed evenly in step (1) is piled in situ for 22 days, during which the moisture content of the material is maintained between 50% and 65%; the in situ pile depth is 0.8 m; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
[0030] In the step (1), the mass ratio of the chromium-contaminated soil to the biochar-fixed urolytic bacteria is 1:100.
[0031] Example 7 See also Figure 1 As shown, this embodiment discloses a method for microbial remediation of hexavalent chromium contaminated soil, comprising the following steps: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the materials at 60%; The hexavalent chromium content in the chromium-contaminated soil is 400 mg / kg; the in-situ accumulation depth is 0.6 m; Step (2) stacking the uniformly mixed materials in step (1) in situ and treating them for 28 days, during which the moisture content of the materials is maintained between 50% and 65%; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
[0032] In the step (1), the mass ratio of the chromium-contaminated soil to the biochar-fixed urolytic bacteria is 4:100.
[0033] Comparative Example 1 Comparative Example 1 Compared with Example 3, in the process of microbial remediation of hexavalent chromium contaminated soil in Comparative Example 1, urolytic bacteria were used instead of biochar to fix urolytic bacteria, and other conditions remained unchanged.
[0034] Comparative Example 2 Comparative Example 2 Compared with Example 3, in the process of microbial remediation of hexavalent chromium contaminated soil in Comparative Example 2, nano-composite biochar was used instead of biochar to fix urea-soluble bacteria, and other conditions remained unchanged.
[0035] Performance testing Hexavalent chromium concentration detection: The repaired soil obtained in Examples 3-7 and Comparative Examples 1-2 was taken, and the concentration of hexavalent chromium in the soil was detected according to HJ908-2017 "Determination of Hexavalent Chromium in Water Quality - Flow Injection-Diphenylcarbazide Spectrophotometry". The test results are shown in Table 1.
[0036] Hexavalent chromium leaching concentration detection: The repaired soil obtained in Examples 3-7 and Comparative Examples 1-2 was taken, and the hexavalent chromium leaching amount in the soil was detected according to HJ / T299 "Solid Waste Leaching Toxicity Leaching Method Sulfuric Acid and Nitric Acid Method". The test results are shown in Table 1.
[0037] Table 1 Detection of hexavalent chromium concentration in soil after restoration in Examples 3-7 and Comparative Examples 1-2 In the soil treated with reference to Example 3-7, the hexavalent chromium concentration is reduced to 0.96-2.51mg / kg, and the hexavalent chromium concentration after repair is lower than the second class land standard of "Soil Environmental Quality Construction Land Soil Pollution Risk Control Standard (Trial)" (GB36600-2018), and the hexavalent chromium leaching concentration after repair is lower than the pollution control index limit when chromium slag is used as roadbed material and concrete aggregate in "Technical Specification for Environmental Protection of Chromium Slag Pollution Control" (Provisional). The hexavalent chromium concentration in the soil repaired according to this detoxification process and the hexavalent chromium leaching concentration meet the requirements of current national standards. It can be seen from the comparison of Comparative Example 1, Comparative Example 2 and Example 3 that the present invention, in the process of carrying out hexavalent chromium contaminated soil microbial remediation, adds biochar to fix urea-soluble bacteria, which is more effective than single use of urea-soluble bacteria or nano-composite biochar, and can improve the remediation effect of hexavalent chromium contaminated soil.
[0038] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
[0039] The preferred embodiments of the present invention disclosed above are only used to help explain the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to only specific implementation methods. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A method for microbial remediation of hexavalent chromium contaminated soil, characterized in that: The following steps are involved: Step (1) mixing the chromium-contaminated soil and the biochar-fixed urea-dissolving bacteria evenly, and adding water during the mixing process to keep the moisture content of the materials at 50-65%; Step (2) stacking and treating the material mixed uniformly in step (1) in situ, during which the moisture content of the material is maintained between 50% and 65%; Step (3) detects the hexavalent chromium content in the soil to obtain the repaired soil.
2. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 1, characterized in that: In the step (1), the mass ratio of chromium-contaminated soil to biochar-fixed urolytic bacteria is 100:0.5-5.
3. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 1, characterized in that: In the step (1), the hexavalent chromium content in the chromium-contaminated soil is 300-600 mg / kg.
4. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 1, characterized in that: In the step (2), the in-situ stacking depth is 0.5-1m; and the processing time is 20-30 days.
5. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 1, characterized in that: In step (1), the method for preparing biochar-fixed urolytic bacteria comprises the following steps: S1: 10-20 g of nanocomposite biochar was added to 200-400 mL of Arthrobacter creatinolyticus culture solution, and the mixture was shaken at 100-200 r / min for 1.5-2.5 h at 29-31° C., and then 500-1000 mL of 2% w / v sodium alginate solution was added to obtain a mixture; S2: The mixture was dropped into 500-1000 mL of 2% w / v CaCl2 solution, cross-linked at 3-5°C for 20-28 h, washed with sterile saline for 3-5 times, and dried to obtain biochar-fixed urolytic bacteria.
6. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 5, characterized in that: The number of the Urolytic Bacteria Microbial Resource Center is 5604MTCC.
7. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 5, characterized in that: The OD600 of the urolytic bacteria in the urolytic bacteria culture solution is 1.
0.
8. The method for microbial remediation of hexavalent chromium contaminated soil according to claim 5, characterized in that: The method for preparing the nanocomposite biochar comprises the following steps: P1: Cut the discarded apples into small pieces, wash them with deionized water to remove impurities, and then dry them at 75-85 °C for 15-21 h to constant weight, and then crush them with a high-speed crusher to obtain apple pomace particles of 0.4-0.6 mm. Pyrolyze the apple pomace particles at 450-550 °C for 1.5-2.5 h, and grind them to obtain apple pomace biochar of 0.1-0.24 mm; P2: apple pomace biochar was added into 50wt% H3PO4 solution at a mass ratio of 1:1, soaked at room temperature for 20-28h, washed with deionized water for 3-5 times, and then dried at 75-85°C to constant weight to obtain phosphoric acid-modified apple pomace biochar; P3: In a nitrogen atmosphere, 20-40 g of phosphoric acid-modified apple pomace biochar, 840-1680 g of FeSO4·H2O, and 42-84 g of ZIF-8 were added to 20-40 L of water, stirred at 200-400 rpm at 25 °C for 0.5-1.5 h, and then 10-20 L of 72.4 g / L NaBH4 aqueous solution was added, filtered, and the filter residue was washed with water 3-5 times, and dried at 70-80 °C in a N2 atmosphere to constant weight to obtain nanocomposite biochar.
Citation Information
Patent Citations
Biological processing method of ammonia-containing wastewater
CN105712487A
Method for reducing bio-availability of agricultural land heavy metal composite contaminated soil
CN111330970A
Method for preparing magnetic biochar by pyrolyzing apple residues
CN111921497A
Carbon-based biological agent for efficiently converting heavy metal chromium in soil
CN114231520A
Method for restoring soil polluted by fluoroquinolone antibiotics
CN115368911A
Cited By
Biomimetic reduction repair method for stable hexavalent chromium in chromium-contaminated soil
CN121017243A