Preparation method of brass coated wire
By using pulling and tempering treatment in brass-clad wire to form a permeable bonding layer, the problem of separation between brass and lightweight core wires is solved, reducing costs and improving the use effect of wires, achieving a finer Brass-clad wire with wire diameter.
Patent Information
- Application Number
- CN202410729822.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-06
- Publication Date
- 2024-11-12
AI Technical Summary
The lack of bond between the existing brass-clad wire and the lightweight core wire after annealing, resulting in separation problems and affecting its normal use.
By curling the brass tape onto the lightweight core rod, welding it and pulling and shrinking the diameter to form a permeable bonding layer, combined with tempering treatment to ensure the bonding of the brass and the lightweight core wire. If a thinner wire diameter is required, Re-pull and temper, and clean and wipe to improve surface finish.
It effectively solves the problem of combining brass and lightweight core wires, reduces costs and improves the use effect of brass-clad wires, ensuring the normal use of brass-clad wires and the realization of thinner wire diameters.
Abstract
Description
Technical Field
[0001] The invention relates to a method for preparing a metal-clad wire, in particular to a method for preparing a brass-clad wire. Background Art
[0002] As we all know, traditional bag chains and other accessories are usually made of expensive single metal wires such as brass. In actual production, on the one hand, due to the high density of brass, the weight of the entire bag chain is relatively heavy; on the other hand, the price of non-ferrous metal materials has risen rapidly in recent years, increasing the cost of bag chains and other accessories. Therefore, a small number of brass-coated materials have appeared on the market for bag chains and other accessories. The main reason why they have not been promoted is that the preparation method of brass-coated wire is still immature, and no penetration bonding layer is formed between the copper layer and the lightweight core wire in the brass-coated wire (commonly known as no bonding). After annealing, the brass and the lightweight core wire are separated (commonly known as shelling), which affects the normal use of the brass-coated wire. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a method for preparing a brass-clad wire material in which the brass and the light core wire can still be well combined after annealing.
[0004] In order to solve the above technical problems, the technical solution adopted by the present invention is: a method for preparing a brass coated wire, the steps of which include:
[0005] 1) curling and coating a brass strip on a lightweight core rod, and welding the seams of the brass strip to form a brass coated wire blank;
[0006] 2) The brass coated wire blank is subjected to at least one drawing process to reduce its diameter to between 38.8% and 44.4% of the original diameter, so that a permeation bonding layer is formed between the brass strip and the lightweight core rod, and a finished brass coated wire is obtained after tempering. If a finished brass coated wire with a finer wire diameter is to be obtained, the wire can be further drawn to less than 30% of the wire diameter of the brass coated wire blank, and then tempered again to obtain a finished brass coated wire with a finer wire diameter.
[0007] As a preferred embodiment, in the brass coated wire, the specific process of the tempering treatment is: heating to between 270 and 300°, and then keeping warm for more than 100 minutes; the specific process of the re-tempering treatment is: heating to between 255 and 285°, and then keeping warm for more than 100 minutes.
[0008] As a preferred solution, in the brass clad wire, the heating time of the tempering treatment is between 65 and 90 minutes.
[0009] As a preferred solution, in the brass coated wire, the heating time of the re-tempering treatment is between 60 and 80 minutes.
[0010] As a preferred solution, in the brass clad wire, the obtained brass clad wire product is cleaned and wiped.
[0011] As a preferred embodiment, in the brass sheathed wire, the specific steps of the cleaning and wiping treatment are: first, let the brass sheathed wire pass through the cleaning liquid, then, let the brass sheathed wire pass through two pairs of felts in turn, the two felts in each pair of felts are arranged relative to each other and move intermittently or continuously, and the felts in the two pairs of felts are arranged perpendicular to each other, so that the brass sheathed wire is wiped in two mutually perpendicular directions, and then, it passes through a cotton belt wrapped around the brass sheathed wire and moves intermittently or continuously, and the brass sheathed wire is wiped again to obtain a finished brass sheathed wire with a smooth surface.
[0012] As a preferred solution, in the brass coated wire, the two felts in each pair of felts move at equal speeds and in opposite directions; and the cotton belt moves against the moving direction of the brass coated wire.
[0013] As a preferred solution, in the brass coated wire, a cleaning antioxidant is dripped on a cotton tape, wherein the cleaning antioxidant contains no less than 5% of antioxidant and the rest is alcohol.
[0014] As a preferred solution, in the brass coated wire, the cleaning antioxidant contains no more than 10% of antioxidant.
[0015] As a preferred solution, in the brass coated wire, the lightweight core wire is an aluminum core wire.
[0016] The beneficial effects of the present invention are:
[0017] 1. The present invention relates the reduction ratio of drawing to the timing of annealing, so that the annealed brass and the light core wire are more likely to be well combined.
[0018] 2. The present invention further ensures that the brass and the light core wire will not separate by controlling the tempering temperature, heating time and holding time.
[0019] 3. The present invention ensures that the brass and the light core wire in the brass-clad wire with a thinner wire diameter will not separate by controlling the re-tempering temperature, heating time and holding time.
[0020] 4. The present invention further reduces the cost of brass coated wire by coating brass on relatively cheap and readily available aluminum core wire to form brass coated wire, thereby further reducing the cost of finished products such as accessories made therefrom. DETAILED DESCRIPTION
[0021] The specific implementation scheme of the brass clad wire of the present invention is described in detail below with reference to specific embodiments.
[0022] The method for preparing a brass-clad wire according to the present invention comprises the following steps:
[0023] 1) curling and coating a brass strip on a lightweight core rod, and welding the seams of the brass strip to form a brass coated wire blank;
[0024] 2) The brass coated wire blank is subjected to at least one drawing process to reduce its diameter to between 38.8% and 44.4% of the original diameter, so that a permeation bonding layer is formed between the brass strip and the lightweight core rod, and a finished brass coated wire is obtained after tempering. If a finished brass coated wire with a finer wire diameter is to be obtained, the wire can be further drawn to less than 30% of the wire diameter of the brass coated wire blank, and then tempered again to obtain a finished brass coated wire with a finer wire diameter.
[0025] The specific process of the tempering treatment is: heating to between 270 and 300 degrees, and then keeping the temperature for more than 100 minutes; the specific process of the re-tempering treatment is: heating to between 255 and 285 degrees, and then keeping the temperature for more than 100 minutes.
[0026] The heating time of the tempering treatment is between 65 and 90 minutes.
[0027] The heating time of the re-tempering treatment is between 60 and 80 minutes.
[0028] The obtained brass coated wire product is cleaned and wiped.
[0029] The specific steps of the cleaning and wiping treatment are: first, let the brass coated wire pass through the cleaning liquid, then, let the brass coated wire pass through two pairs of felts in turn, the two felts in each pair of felts are arranged relative to each other and move intermittently or continuously, and the felts in the two pairs of felts are arranged perpendicular to each other, so that the brass coated wire is wiped in two mutually perpendicular directions, and then, it passes through a cotton belt wrapped around the brass coated wire and moves intermittently or continuously, and the brass coated wire is wiped again to obtain a finished brass coated wire with a smooth surface.
[0030] The two felts in each pair of felts move at the same speed and in opposite directions; the cotton belt moves against the direction of travel of the brass coated wire.
[0031] A cleaning antioxidant is dripped onto the cotton tape, wherein the cleaning antioxidant contains no less than 5% of antioxidant and the rest is alcohol.
[0032] The cleaning antioxidant contains no more than 10% of antioxidant.
[0033] The light core wire is an aluminum core wire.
[0034] In the production process of the brass coated wire of the present invention, the brass coated wire of the present invention can be formed by coating a brass strip on an aluminum alloy rod, and then the wire diameter is reduced to a required wire diameter by drawing and tempering. The components of the aluminum alloy rod include: trace amounts of manganese (0.0043%), trace amounts of magnesium (0.0025%), trace amounts of copper (0.1934%), trace amounts of zinc (0.0052%), trace amounts of silicon (0.0435%), iron (1.032%), trace amounts of nickel (0.0042%), trace amounts of chromium (0.001%) and trace amounts of titanium (0.0126%), and the balance is aluminum.
[0035] In summary, the above is only a preferred embodiment of the present invention and is not intended to limit the scope of the present invention. All equivalent changes and modifications made to the shape, structure, characteristics and spirit described in the claims of the present invention should be included in the scope of the claims of the present invention.
Claims
1. A method for preparing a brass coated wire, comprising the steps of: 1) curling and coating a brass strip on a lightweight core rod, and welding the seams of the brass strip to form a brass coated wire blank; 2) Drawing the brass coated wire blank at least once to reduce its diameter to between 38.8% and 44.4% of the original diameter, so that a permeation bonding layer is formed between the brass strip and the lightweight core rod, and tempering is performed to obtain a finished brass coated wire; If a finished brass clad wire with a finer wire diameter is to be obtained, the wire may be further drawn to less than 30% of the wire diameter of the brass clad wire blank, and then tempered again to obtain a finished brass clad wire with a finer wire diameter.
2. The method for preparing the brass coated wire according to claim 1, characterized in that: The specific process of the tempering treatment is: heating to between 270 and 300 degrees, and then keeping the temperature for more than 100 minutes; the specific process of the re-tempering treatment is: heating to between 255 and 285 degrees, and then keeping the temperature for more than 100 minutes.
3. The method for preparing the brass coated wire according to claim 2, characterized in that: The heating time of the tempering treatment is between 65 and 90 minutes.
4. The method for preparing the brass coated wire according to claim 2, characterized in that: The heating time of the re-tempering treatment is between 60 and 80 minutes.
5. The method for preparing the brass coated wire according to claim 1, characterized in that: The obtained brass coated wire product is cleaned and wiped.
6. The method for preparing the brass coated wire according to claim 5, characterized in that: The specific steps of the cleaning and wiping treatment are: first, let the brass coated wire pass through the cleaning liquid, then, let the brass coated wire pass through two pairs of felts in turn, the two felts in each pair of felts are arranged relative to each other and move intermittently or continuously, and the felts in the two pairs of felts are arranged perpendicular to each other, so that the brass coated wire is wiped in two mutually perpendicular directions, and then, it passes through a cotton belt wrapped around the brass coated wire and moves intermittently or continuously, and the brass coated wire is wiped again to obtain a finished brass coated wire with a smooth surface.
7. The method for preparing the brass coated wire according to claim 6, characterized in that: The two felts in each pair of felts move at the same speed and in opposite directions; the cotton belt moves against the direction of travel of the brass coated wire.
8. The method for preparing the brass coated wire according to claim 6, characterized in that: A cleaning antioxidant is dripped onto the cotton tape, wherein the cleaning antioxidant contains no less than 5% of antioxidant and the rest is alcohol.
9. The method for preparing the brass coated wire according to claim 8, characterized in that: The cleaning antioxidant contains no more than 10% of antioxidant.
10. The method for preparing a brass coated wire according to any one of claims 1 to 9, characterized in that: The light core wire is an aluminum core wire.
Citation Information
Patent Citations
Manufacturing method for copper covered flat aluminum wire
CN101131892A
Copper / aluminum composite wire material and anneal manufacturing method thereof
CN101148693A
Production process for flexible copper-clad aluminum wire with diameter of below 0.4 millimeter
CN105097131A
On-line cleaning device for conducting wire
CN107617601A
Method of and apparatus for producing copper cald aluminum wire
GB1410928A