Slurry temperature control by mixing under dosing

By injecting steam into the polishing liquid during the CMP process to increase the temperature and performing temperature control on the polishing pad, the polishing uniformity and life problems caused by the surface temperature change of the polishing pad are solved, achieving a more uniform polishing effect and lower Defect rate.

CN118927155APending Publication Date: 2024-11-12APPLIED MATERIALS INC
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410966129.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2020-03-26
Filing Date
2020-08-11
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

During the chemical mechanical polishing (CMP), temperature control is difficult to achieve, resulting in temperature changes on the surface of the polishing pad affecting polishing uniformity, erosion and depression, which in turn leads to wafer defects and shortening of the polishing pad life.

Method used

The temperature uniformity of the polishing pad and the polishing liquid is ensured by injecting a heating fluid such as steam into the polishing liquid after the polishing liquid leaves the storage room, and temperature control is performed before dispensing on the polishing pad.

Benefits of technology

Effectively reduces temperature-related process effects, such as depression, erosion and corrosion, improves polishing uniformity, extends the life of the polishing pad, and reduces corrosion of CMP device components, and reduces wafer defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118927155A_ABST
    Figure CN118927155A_ABST
Patent Text Reader

Abstract

The invention discloses slurry temperature control by mixing under dosing. A chemical mechanical polishing system includes a platform for supporting a polishing pad having a polishing surface; a source of heating fluid; a storage chamber for holding a polishing liquid; and a dispenser having one or more apertures suspended above the platform to direct a polishing liquid onto the polishing surface, where a source of heating fluid is coupled to the dispenser, and configured to transfer the heating fluid into the polishing liquid to heat the polishing liquid after the polishing liquid exits the storage chamber and before the polishing liquid is dispensed onto the polishing surface.
Need to check novelty before this filing date? Find Prior Art

Description

This application is a divisional application of the invention patent application with the application date of August 11, 2020, application number "202080056668.1", and invention name "Slurry temperature control by mixing under dosing". Technical Field

[0001] The present disclosure relates to chemical mechanical polishing (CMP), and more particularly, to temperature control during CMP. Background Art

[0002] Integrated circuits are typically formed by sequentially depositing conductive, semiconductive, or insulating layers on a semiconductor wafer. Various manufacturing processes require planarization of the layers on the substrate. For example, one manufacturing step involves depositing a filler layer on a non-planar surface and planarizing the filler layer. For some applications, the filler layer is planarized until the top surface of the patterned layer is exposed. For example, a metal layer may be deposited on a patterned insulating layer to fill trenches and holes in the insulating layer. After planarization, the remaining portions of the metal in the trenches and holes of the patterned layer form vias, plugs, and lines to provide conductive paths between thin film circuits on the substrate. As another example, a dielectric layer may be deposited on top of the patterned conductive layer and then planarized to enable subsequent photolithography steps.

[0003] Chemical mechanical polishing (CMP) is an acceptable planarization method. This planarization method generally requires mounting the substrate on a carrier head. The exposed surface of the substrate is generally placed against a rotating polishing pad. The carrier head provides a controllable load on the substrate to push the substrate against the polishing pad. A polishing slurry having abrasive particles is generally supplied to the surface of the polishing pad. Summary of the invention

[0004] In one aspect, a chemical mechanical polishing system includes: a platform for supporting a polishing pad having a polishing surface; a source of a heating fluid; a reservoir for holding the polishing liquid; and a dispenser having one or more holes suspended above the platform to direct the polishing liquid onto the polishing surface, wherein the source of the heating fluid is coupled to the dispenser and configured to transfer the heating fluid into the polishing liquid to heat the polishing liquid after the polishing liquid leaves the reservoir and before the polishing liquid is dispensed onto the polishing surface.

[0005] Implementations of any of the above aspects may include one or more of the following features.

[0006] The heating fluid may include one or more of: water, deionized water, or water including additives or chemicals.

[0007] The source of the heating fluid may include a steam generator, and the heating fluid may contain steam. The steam generator may heat the steam to 40-120°C.

[0008] A source of heating fluid may be coupled to the dispenser in a dispenser arm extending above the platform so as to deliver the heating fluid to the polishing liquid in the dispenser arm. A source of heating fluid may be coupled to the dispenser in a mixing chamber located in the dispenser arm so as to deliver the heating fluid to the polishing liquid in the mixing chamber.

[0009] A source of heating fluid may be coupled to the fluid supply line between the reservoir and a slurry delivery arm extending above the platform to deliver the heating fluid to the polishing liquid in the fluid supply line.

[0010] One or more valves may control relative flow rates of the heating fluid and the polishing liquid. The source of the heating fluid may include a steam generator, and the heating fluid may include steam, and the controller may be configured to control a steam valve located between the steam generator and the dispenser to cause the steam to flow through the steam valve into the dispenser at a first rate, and to control a polishing liquid valve located between the polishing liquid reservoir and the dispenser to cause the polishing liquid to flow into the dispenser at a second rate.

[0011] In another aspect, a chemical mechanical polishing system may include: a platform for supporting a polishing pad having a polishing surface; a dispenser assembly including a reservoir for holding a polishing liquid, and a dispenser having one or more holes suspended above the platform for directing the polishing liquid onto the polishing surface; and a steam generator coupled to the dispenser assembly and configured to transmit steam into the polishing liquid to heat the polishing liquid before the polishing liquid is dispensed onto the polishing surface.

[0012] Implementations of any of the above aspects may include one or more of the following features.

[0013] A steam generator may be coupled to the dispenser and configured to deliver steam into the polishing liquid after the polishing liquid exits the reservoir.

[0014] In another aspect, a method for temperature control of a chemical mechanical polishing system includes heating the polishing liquid using a heating fluid after the polishing liquid leaves a reservoir and before dispensing the polishing liquid onto a polishing pad; and dispensing the heated polishing liquid onto the polishing pad.

[0015] Implementations of any of the above aspects may include one or more of the following features.

[0016] The source of heating fluid may include a steam generator, and the heating fluid contains steam.

[0017] The heating fluid may include steam. The steam may be heated to 40-120° C. before being injected into the polishing liquid. The heating fluid may include one or more of the following: water, deionized water, or water including additives or chemicals. The heating fluid and the polishing liquid may be mixed at a flow rate ratio of 10:1 to 1:10.

[0018] Possible advantages may include, but are not limited to, one or more of the following.

[0019] Controlling the temperature of various components can reduce the effects of temperature-related processes, such as dishing, erosion, and corrosion. Controlling temperature can also create a more uniform pad roughness, thus enhancing polishing uniformity, for example, for cleaning metal residues and extending pad life.

[0020] In one example, the temperature of the polishing process is elevated. Specifically, steam (i.e., gaseous H2O produced by boiling) can be injected into the slurry to deliver energy at low liquid content (i.e., low dilution) to quickly and efficiently raise the temperature of the slurry. This can increase the polishing rate (e.g., during batch polishing).

[0021] In another example, the temperature of the polishing pad surface may be reduced during one or more of the metal cleaning, over-polishing, or conditioning steps of a polishing operation. This may reduce dishing and corrosion, and / or enhance the uniformity of the pad roughness, thereby enhancing polishing uniformity and extending the life of the pad.

[0022] In addition, the temperature of various components of the CMP apparatus can be reduced, which can reduce electrical reaction rates and reduce corrosion of various components. This can reduce defects in the polished wafer.

[0023] This can enhance the predictability of polishing during the CMP process, reduce polishing variation from one polishing run to another, and enhance wafer-to-wafer uniformity.

[0024] The details of one or more implementations are set forth in the accompanying drawings and the description that follows.Other aspects, features, and advantages will be apparent from the description and drawings, and from the claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic plan view of an example of a polishing apparatus.

[0026] Figure 2A is a schematic cross-sectional view of an example carrier head vapor handling assembly.

[0027] Figure 2B A schematic cross-sectional view of an example adjustment head vapor handling assembly.

[0028] Figure 3A A schematic cross-sectional view of an example of a polishing station of a polishing apparatus.

[0029] Figure 3B A schematic top view of an exemplary polishing station of a chemical mechanical polishing apparatus is shown.

[0030] Figure 4A is a schematic cross-sectional view of an example steam generator.

[0031] Figure 4B is a schematic cross-sectional top view of an example steam generator. DETAILED DESCRIPTION

[0032] Chemical mechanical polishing operates by combining mechanical grinding and chemical etching at the interface between the substrate, polishing liquid, and polishing pad. During the polishing process, a large amount of heat is generated due to the friction between the surface of the substrate and the polishing pad. In addition, some processes also include an in-situ pad conditioning step, in which a conditioning disk (e.g., a disk coated with abrasive diamond particles) is pressed against the rotating polishing pad to condition and texture the polishing pad surface. The grinding of the conditioning process can also generate heat. For example, at a nominal press pressure of 2 psi and The surface temperature of the polyurethane polishing pad can rise by about 30°C during a typical one-minute copper CMP process at a removal rate of 1.38°C.

[0033] On the other hand, the slurry dispensed onto the polishing pad can act as a heat sink. Overall, these effects lead to temperature variations of the polishing pad both spatially and over time.

[0034] Both chemically related variables (e.g., the initiation and rate of the reactions involved) and mechanically related variables (e.g., the surface coefficient of friction, storage modulus, and viscoelasticity of the polishing pad) in the CMP process are strongly temperature dependent. Thus, variations in the surface temperature of the polishing pad can result in variations in removal rate, polishing uniformity, erosion, dishing, and residue. By more tightly controlling the temperature of the surface of the polishing pad during one or more of the metal cleaning, overpolishing, or conditioning steps, temperature variations can be reduced and polishing performance, for example, as measured by intra-wafer non-uniformity or inter-wafer non-uniformity, can be enhanced.

[0035] In general, as the temperature of the polishing liquid 38 increases, the polishing rate of the polishing liquid 38 increases. Conversely, as the temperature of the polishing liquid 38 decreases, the polishing rate of the polishing liquid 38 decreases. An increased polishing rate may be desirable during some stages of the polishing operation (e.g., during batch polishing), and a decreased polishing rate may be desirable during other stages of the polishing operation (e.g., during metal cleaning, over-polishing, and conditioning steps).

[0036] In addition, during CMP, debris and slurry can accumulate on various components of the CMP apparatus. Mechanical and chemical etching by the debris and slurry can cause dishing and erosion of the polishing pad, and can corrode various components of the CMP apparatus.

[0037] A technique that may address one or more of these issues is to preheat the polishing pad and / or slurry during portions of the polishing process (e.g., during batch polishing). For example, various components of the CMP apparatus (e.g., polishing liquid 38 from polishing liquid reservoir 37) may be heated using steam (i.e., gaseous H2O) to increase the polishing rate during the polishing process. Additionally, the temperature of the polishing pad and various components may be reduced (e.g., using vortex tube cooling and / or by dosing coolant) to reduce the polishing rate of the slurry chemistry during one or more of the metal cleaning, overpolishing, or conditioning steps.

[0038] Figure 1 FIG. 2 is a plan view of a chemical mechanical polishing apparatus 2 for processing one or more substrates. The polishing apparatus 2 includes a polishing platform 4, which at least partially supports and accommodates a plurality of polishing stations 20. For example, the polishing apparatus may include four polishing stations 20a, 20b, 20c, and 20d. Each polishing station 20 is adapted to polish a substrate held in a carrier head 70. Figure 1 Not all components of each station are shown.

[0039] The polishing apparatus 2 also includes a plurality of carrier heads 70, each of which is configured to carry a substrate. The polishing apparatus 2 also includes a transfer station 6 for loading and unloading substrates from the carrier heads. The transfer station 6 may include a plurality of load cups 8 (e.g., two load cups 8a, 8b) adapted to facilitate transfer of substrates between the carrier heads 70 and a factory interface (not shown) or other equipment (not shown) via a transfer robot 9. The load cups 8 typically facilitate transfer between the robot 9 and each of the carrier heads 70 by loading and unloading the carrier heads 70.

[0040] The stations of the polishing apparatus 2, including the transfer station 6 and the polishing station 20, may be positioned at substantially equal angular intervals around the center of the platform 4. This is not required, but may provide a good footprint for the polishing apparatus.

[0041] For polishing operations, one carrier head 70 is positioned at each polishing station. Two additional carrier heads may be positioned in the loading and unloading station 6 to exchange polished substrates with unpolished substrates while other substrates are being polished at the polishing station 20.

[0042] The carrier heads 70 are held by a support structure that allows each carrier head to move along a path that sequentially passes through the first polishing station 20a, the second polishing station 20b, the third polishing station 20c, and the fourth polishing station 20d. This allows each carrier head to be selectively positioned above the polishing station 20 and the load cup 8.

[0043] In some implementations, each carrier head 70 is coupled to a carriage 78 mounted to a support structure 72. By moving the carriage 78 along the support structure 72 (e.g., a track), the carrier heads 70 can be positioned on a selected polishing station 20 or load cup 8. Alternatively, the carrier heads 70 can be suspended from a turntable, and rotation of the turntable moves all of the carrier heads simultaneously along a circular path.

[0044] Each polishing station 20 of the polishing apparatus 2 may include a port (eg, at the end of a slurry dispenser 39 (eg, a dispenser arm)) to dispense a polishing liquid 38 (eg, abrasive slurry) such as a polishing slurry. Figure 3A ) is dispensed onto the polishing pad 30. Each polishing station 20 of the polishing apparatus 2 may further include a pad conditioner 93 to grind the polishing pad 30 to maintain the polishing pad 30 in a consistent grinding state.

[0045] Figure 3A and Figure 3B An example of a polishing station 20 of a chemical mechanical polishing system is shown. The polishing station 20 includes a rotatable disk-shaped platform 24 on which a polishing pad 30 is placed. The platform 24 is operable to rotate about an axis 25 (see Figure 3B 2. For example, the motor 22 may rotate the drive shaft 28 to rotate the platform 24. The polishing pad 30 may be a dual-layer polishing pad having an outer polishing layer 34 and a softer backing layer 32.

[0046] Reference Figure 1 , Figure 3A and Figure 3B The polishing station 20 may include a supply port (eg, at an end of a slurry delivery arm 39 ) to dispense a polishing liquid 38 , such as an abrasive slurry, onto the polishing pad 30 .

[0047] The polishing station 20 may include a pad conditioner 90 having a conditioning disk 92 (see Figure 2B ) to maintain the surface roughness of the polishing pad 30. The conditioning disk 92 can be positioned in the conditioning head 93 at the end of the arm 94. The arm 94 and the conditioning head 93 are supported by the base 96. The arm 94 can swing so as to sweep the conditioning head 93 and the conditioning disk 92 laterally across the polishing pad 30. The cleaning cup 250 can be positioned adjacent to the platform 24 at the position where the arm 94 can move the conditioning head 93.

[0048] The carrier head 70 is operable to hold the substrate 10 against the polishing pad 30. The carrier head 70 is suspended from a support structure 72 (e.g., a turntable or track) and is connected to a carrier head rotation motor 76 by a drive rod 74 so that the carrier head can rotate about an axis 71. Alternatively, the carrier head 70 can oscillate laterally by moving along a track or by rotational oscillation of the turntable itself (e.g., on a slide on the turntable).

[0049] The carrier head 70 may include a flexible membrane 80 having a substrate mounting surface to contact the back side of the substrate 10, and a plurality of pressurizable chambers 82 to apply different pressures to different regions (e.g., different radial regions) on the substrate 10. The carrier head 70 may include a retaining ring 84 to hold the substrate. In some implementations, the retaining ring 84 may include a lower plastic portion 86 that contacts the polishing pad and an upper portion 88 of a harder material (e.g., metal).

[0050] In operation, the platform rotates about its central axis 25, and the carrier head rotates about its central axis 71 (see Figure 3B B) and laterally translates across the top surface of the polishing pad 30 (see Figure 3B Arrow C in the figure).

[0051] Reference Figure 3A and Figure 3B As the carrier head 70 is swept across the polishing pad 30, any exposed surface of the carrier head 70 tends to become covered with slurry. For example, the slurry may adhere to the outer or inner diameter surface of the retaining ring 84. In general, the slurry will tend to coagulate and / or dry out for any surface that is not maintained in a wet condition. As a result, particles may form on the carrier head 70. If these particles become dislodged, the particles may scratch the substrate, resulting in polishing defects.

[0052] Additionally, the slurry may flake onto carrier head 70, or sodium hydroxide in the slurry may crystallize on one of the surfaces of carrier head 70 and / or substrate 10 and cause surface corrosion of carrier head 70. Flaked slurry is difficult to remove and crystallized sodium hydroxide is difficult to return to solution.

[0053] Similar problems occur with the conditioning head 92 , for example, particles may form on the conditioning head 92 , the slurry may flake onto the conditioning head 92 , or sodium hydroxide in the slurry may crystallize on one of the surfaces of the conditioning head 92 .

[0054] One solution is to clean the components (e.g., carrier head 70 and conditioning head 92) with a jet of liquid water. However, it may be difficult to clean the components with a jet of water alone, and a large amount of water may be required. In addition, the components in contact with the polishing pad 30 (e.g., carrier head 70, substrate 10, and conditioning disk 92) may act as a heat sink that hinders the temperature uniformity of the polishing pad.

[0055] To solve these problems, Figure 2A As shown, the polishing apparatus 2 includes one or more carrier head vapor treatment assemblies 200. Each vapor treatment assembly 200 can be used to clean and / or preheat the carrier head 70 and the substrate 10.

[0056] The steam handling assembly 200 may be part of the load cup 8 (eg, part of the load cup 8a or 8b). Alternatively or additionally, the steam handling assembly 200 may be disposed at one or more inter-platform stations 9 located between adjacent polishing stations 20.

[0057] The load cup 8 includes a base 204 to hold the substrate 10 during the loading / unloading process. The load cup 8 also includes a housing 206 that surrounds or substantially surrounds the base 204. A plurality of nozzles 225 are supported by the housing 206 or a separate support to transmit steam 245 to a carrier head and / or a substrate positioned in a cavity 208 defined by the housing 206. For example, the nozzles 225 may be positioned on one or more interior surfaces of the housing 206 (e.g., the floor 206a and / or the sidewalls 206b and / or the ceiling of the cavity). The nozzles 225 may be configured (e.g., using the controller 12) to start and stop the flow of fluid through the nozzles 225. The nozzles 225 may be oriented to direct steam inwardly into the cavity 206. The steam 245 may be generated using a steam generator 410 (e.g., a steam generator discussed further below). The drain pipe 235 may allow excess water, cleaning solution, and cleaning byproducts to pass through to avoid accumulation in the load cup 8.

[0058] The actuator provides relative vertical movement between the housing 206 and the carrier head 70. For example, the rod 210 can support the housing 206 and be vertically actuatable to raise and lower the housing 206. Alternatively, the carrier head 70 can be vertically movable. The base 205 can be on the axis of the rod 210. The base 204 can be vertically movable relative to the housing 206.

[0059] In operation, the carrier head 70 may be positioned over the load cup 8, and the housing 206 may be raised (or the carrier head 70 lowered) so that the carrier head 70 is partially within the cavity 208. The substrate 10 may start on the pedestal 204 and be chucked onto the carrier head 70, and / or start on the carrier head 70 and be unclamped onto the pedestal 204.

[0060] Steam is directed through the nozzles 225 to clean and / or preheat one or more surfaces of the substrate 10 and / or the carrier head 70. For example, one or more of the nozzles may be positioned to direct steam to an exterior surface of the carrier head 70, an exterior surface 84a of the retaining ring 84, and / or a bottom surface 84b of the retaining ring 84. One or more of the nozzles may be positioned to direct steam to a front surface (i.e., a surface to be polished) of the substrate 10 held by the carrier head 70, or to a bottom surface of the film 80 if no substrate 10 is supported on the carrier head 70. One or more of the nozzles may be positioned below the pedestal 204 to direct steam upward to a front surface of the substrate 10 positioned on the pedestal 204. One or more of the nozzles may be positioned above the pedestal 204 to direct steam downward to a back surface of the substrate 10 positioned on the pedestal 204. The carrier head 70 may be rotated within the load cup 8 and / or moved vertically relative to the load cup 8 to allow the nozzles 225 to treat different areas of the carrier head 70 and / or the substrate 10. The substrate 10 may be placed on a pedestal 205 to allow an interior surface of the carrier head 70 (eg, a bottom surface of the membrane 82, or an interior surface of the retaining ring 84) to be vapor treated.

[0061] Steam is circulated from a steam source through a supply line 230 through the housing 206 to the nozzle 225. The nozzle 225 may spray steam 245 to remove organic residues, byproducts, debris, and slurry particles remaining on the carrier head 70 and the substrate 10 after each polishing operation. The nozzle 225 may spray steam 245 to heat the substrate 10 and / or the carrier head 70.

[0062] The inter-platform station 9 may be similarly constructed and operated, but need not have a substrate support pedestal.

[0063] The vapor 245 delivered through the nozzles 225 can have adjustable temperature, pressure, and flow rate to vary the cleaning and preheating of the carrier head 70 and substrate 10. In some implementations, the temperature, pressure, and / or flow rate can be independently adjustable for each nozzle or between groups of nozzles.

[0064] For example, when (for example, in Figure 4A When the steam 245 is generated in the steam generator 410 in the nozzle 225, the temperature of the steam 245 may be 90° C. to 200° C. When the steam 245 is distributed through the nozzle 225, the temperature of the steam 245 may be between 90° C. and 150° C., for example, due to heat losses in transmission. In some implementations, the steam is transmitted through the nozzle 225 at a temperature of 70-100° C. (e.g., 80-90° C.). In some implementations, the steam transmitted through the nozzle is superheated (i.e., at a temperature above the boiling point).

[0065] When steam 245 is transmitted through nozzle 225, the flow rate of steam 245 may be 1-1000cc / minute, depending on the heater power and pressure. In some implementations, the steam is mixed with other gases, such as with normal atmosphere or with N2. Alternatively, the fluid transmitted through nozzle 225 is substantially pure water. In some implementations, steam 245 transmitted through nozzle 225 is mixed with liquid water (e.g., atomized water). For example, liquid water and steam can be combined at a relative flow ratio (e.g., flow rate in sccm) of 1:1 to 1:10. However, if the amount of liquid water is low (e.g., less than 5wt%, such as less than 3wt%, such as less than 1wt%), the steam will have excellent heat transfer quality. Therefore, in some implementations, the steam is dry steam, i.e., substantially free of water droplets.

[0066] To avoid thermal degradation of the membrane, water may be mixed with the steam 245 to reduce the temperature, for example to about 40-50° C. The temperature of the steam 245 may be reduced by mixing cooled water into the steam 245, or by mixing water into the steam 245 at the same or substantially the same temperature (because liquid water transfers less energy than gaseous water).

[0067] In some implementations, a temperature sensor 214 may be mounted in or adjacent to the steam treatment assembly 200 to detect the temperature of the carrier head 70 and / or the substrate 10. Signals from the sensor 214 may be received by the controller 12 to monitor the temperature of the carrier head 70 and / or the substrate 10. The controller 12 may control the steam transmitted through the assembly 100 based on the temperature measurement from the temperature sensor 214. For example, the controller may receive a target temperature value. If the controller 12 detects that the temperature measurement exceeds the target value, the controller 12 terminates the flow of steam. As another example, the controller 12 may reduce the steam transmission flow rate and / or reduce the steam temperature, for example to avoid overheating of the components during cleaning and / or preheating.

[0068] In some implementations, the controller 12 includes a timer. In this case, the controller 12 can start when the steam delivery begins and can terminate the steam delivery when the timer expires. The timer can be set based on experimental testing to obtain the desired temperature of the carrier head 70 and substrate 10 during cleaning and / or preheating.

[0069] Figure 2BA conditioning steam treatment assembly 250 is shown that includes a housing 255. The housing 255 may form a "cup" to house the conditioning disc 92 and the conditioning head 93. Steam is circulated to one or more nozzles 275 through a supply line 280 in the housing 255. The nozzles 275 may spray steam 295 to remove polishing byproducts (e.g., debris or abrasive particles) left on the conditioning disc 92 and / or the conditioning head 93 after each conditioning operation. The nozzles 275 may be positioned in the housing 255 (e.g., on the floor, sidewalls, or ceiling of the interior of the housing 255). The nozzles 275 may be configured (e.g., using the controller 12) to start and stop the flow of fluid through the nozzles 275. One or more nozzles may be positioned to clean the bottom surface of the pad conditioning disc and / or the bottom surface, sidewalls, and / or top surface of the conditioning head 93. The steam 295 may be generated using a steam generator 410. The drain pipe 285 may allow excess water, cleaning solution, and cleaning byproducts to pass through to avoid accumulation in the housing 255.

[0070] The conditioning head 93 and conditioning disk 92 can be at least partially lowered into the housing 255 to be steam disposed. When the conditioning disk 92 is to be returned to operation, the conditioning head 93 and conditioning disk 92 are lifted out of the housing 255 and positioned on the polishing pad 30 to condition the polishing pad 30. When the conditioning operation is completed, the conditioning head 93 and conditioning disk 92 are lifted off the polishing pad and swept back to the housing cup 255 for removal of polishing byproducts on the conditioning head 93 and conditioning disk 92. In some implementations, the housing 255 is vertically actuatable (e.g., mounted to a vertical drive rod 260).

[0071] The housing 255 is positioned to house the adjustment disk 92 and the adjustment head 93. The adjustment disk 92 and the adjustment head 93 can rotate within the housing 255 and / or move vertically in the housing 255 to allow the nozzle 275 to steam treat various surfaces of the adjustment disk 92 and the adjustment head 93.

[0072] The steam 295 delivered by the nozzle 275 may have an adjustable temperature, pressure, and / or flow rate. In some implementations, the temperature, pressure, and / or flow rate may be independently adjustable for each nozzle or between groups of nozzles. This allows for varying and therefore more efficient cleaning of the adjustment disk 92 or adjustment head 93.

[0073] For example, when (for example, in Figure 4A When the steam 295 is generated by the steam generator 410 in the nozzle 275, the temperature of the steam 295 may be 90° C. to 200° C. When the steam 295 is distributed through the nozzle 275, the temperature of the steam 295 may be between 90° C. and 150° C., for example, due to heat losses in transmission. In some implementations, the steam may be transmitted through the nozzle 275 at a temperature of 70-100° C. (e.g., 80-90° C.). In some implementations, the steam transmitted through the nozzle is superheated (i.e., at a temperature above the boiling point).

[0074] When steam 295 is transmitted through nozzle 275, the flow rate of steam 2945 may be 1-1000cc / minute. In some implementations, the steam is mixed with other gases, such as with normal atmosphere or with N2. Alternatively, the fluid transmitted through nozzle 275 is substantially pure water. In some implementations, steam 295 transmitted through nozzle 275 is mixed with liquid water (e.g., atomized water). For example, liquid water and steam can be combined at a relative flow ratio (e.g., flow rate in sccm) of 1:1 to 1:10. However, if the amount of liquid water is low (e.g., less than 5wt%, such as less than 3wt%, such as less than 1wt%), the steam will have excellent heat transfer quality. Therefore, in some implementations, the steam is dry steam, that is, does not include water droplets.

[0075] In some implementations, a temperature sensor 264 may be mounted in or adjacent to the housing 255 to detect the temperature of the adjustment head 93 and / or the adjustment disk 92. The controller 12 may receive a signal from the temperature sensor 264 to monitor the temperature of the adjustment head 93 or the adjustment disk 92 (e.g., to detect the temperature of the pad adjustment disk 92). The controller 12 may control the transmission of steam through the component 250 based on the temperature measurement from the temperature sensor 264. For example, the controller may receive a target temperature value. If the controller 12 detects that the temperature measurement exceeds the target value, the controller 12 terminates the flow of steam. As another example, the controller 12 may reduce the steam transmission flow rate and / or reduce the steam temperature, for example, to avoid overheating of the components during cleaning and / or preheating.

[0076] In some implementations, the controller 12 uses a timer. In this case, the controller 12 may start a timer when steam delivery begins, and may terminate steam delivery when the timer expires. The timer may be set based on experimental testing to obtain a desired temperature of the conditioning disc 92 during cleaning and / or preheating, for example, to avoid overheating.

[0077] Reference Figure 3A In some implementations, the polishing station 20 includes a temperature sensor 64 to monitor the temperature of components in or of the polishing station, such as the temperature of the polishing pad 30 and / or the polishing liquid 38 on the polishing pad. For example, the temperature sensor 64 can be an infrared (IR) sensor (e.g., an IR camera) positioned above the polishing pad 30 and configured to measure the temperature of the polishing pad 30 and / or the polishing liquid 38 on the polishing pad. Specifically, the temperature sensor 64 can be configured to measure at multiple points along the radius of the polishing pad 30 in order to generate a radial temperature profile. For example, the IR camera can have a field of view that spans the radius of the polishing pad 30.

[0078] In some implementations, the temperature sensor is a contact sensor rather than a non-contact sensor. For example, the temperature sensor 64 can be a thermocouple or an IR thermocouple positioned on or in the platform 24. In addition, the temperature sensor 64 can be in direct contact with the polishing pad.

[0079] In some implementations, multiple temperature sensors may be spaced across the polishing pad 30 at different radial locations to provide temperature at multiple points along the radius of the polishing pad 30. This technique may be used instead of or in addition to an IR camera.

[0080] although Figure 3A As shown in FIG. 1 , positioned to monitor the temperature of the polishing pad 30 and / or the polishing liquid 38 on the pad 30, a temperature sensor 64 can be positioned inside the carrier head 70 to measure the temperature of the substrate 10. The temperature sensor 64 can be in direct contact (i.e., a contact sensor) with the semiconductor wafer of the substrate 10. In some implementations, multiple temperature sensors are included in the polishing station 22, for example, to measure the temperature of different components of / in the polishing station.

[0081] The polishing system 20 also includes a temperature control system 100 to control the temperature of the polishing pad 30 and / or the polishing liquid 38 on the polishing pad. The temperature control system 100 may include a cooling system 102 and / or a heating system 104. At least one of the cooling system 102 and the heating system 104, and in some implementations both, controls the temperature of the polishing pad 30 by delivering a temperature-controlled medium (e.g., liquid, vapor, or spray) to the polishing surface 36 of the polishing pad 30 (or to the polishing liquid already present on the polishing pad).

[0082] For the cooling system 102, the cooling medium may be a gas (e.g., air) or a liquid (e.g., water). The medium may be at room temperature or cooled to below room temperature (e.g., at 5-15°C). In some implementations, the cooling system 102 uses a spray of air and liquid (e.g., an atomized spray of a liquid (e.g., water)). Specifically, the cooling system may have a nozzle that produces an atomized spray of water cooled to below room temperature. In some implementations, a solid material may be mixed with the gas and / or liquid. The solid material may be a cooled material (e.g., ice), or a material that absorbs heat when dissolved in water (e.g., through a chemical reaction).

[0083] The cooling medium may be delivered by flowing through one or more apertures (eg, holes or slots) in the coolant delivery arm (optionally formed in the nozzle). The apertures may be provided by a manifold connected to a coolant source.

[0084] like Figure 3A and Figure 3BAs shown, the exemplary cooling system 102 includes an arm 110 extending above the platform 24 and the polishing pad 30 from the edge of the polishing pad to or at least close to (e.g., within 5% of the total radius of the polishing pad) the center of the polishing pad 30. The arm 110 can be supported by a base 112, and the base 112 can be supported on the same frame 40 as the platform 24. The base 112 can include one or more actuators, such as linear actuators to raise or lower the arm 110, and / or rotary actuators to swing the arm 110 laterally above the platform 24. The arm 110 is positioned to avoid collision with other hardware components, such as the polishing head 70, the pad conditioning disk 92, and the slurry dispenser 39.

[0085] The example cooling system 102 includes a plurality of nozzles 120 suspended from an arm 110. Each nozzle 120 is configured to spray a liquid coolant medium (e.g., water) onto the polishing pad 30. The arm 110 can be supported by a base 112 such that the nozzles 120 are separated from the polishing pad 30 by a gap 126. Each nozzle 120 can be configured (e.g., using a controller 12) to start and stop the flow of fluid through each nozzle 120. Each nozzle 120 can be configured to direct atomized water in a spray 122 toward the polishing pad 30.

[0086] The cooling system 102 may include a source 130 of a liquid coolant medium and a source 132 of a gaseous coolant medium (see Figure 3B ). Liquid from source 130 and gas from source 132 may be mixed in mixing chamber 134 (see Figure 3A ) (eg, in or on arm 110) to form spray 122. When dispensed, this coolant may be below room temperature, such as from -100 to 20°C, such as below 0°C.

[0087] The coolant used in the cooling system 102 may include, for example, liquid nitrogen, or a gas formed from liquid nitrogen and / or dry ice. In some implementations, water droplets may be added to the gas stream. The water may be cooled to form ice droplets, which efficiently cool the polishing pad due to the latent heat of melting of the ice droplets. In addition, the ice or water droplets may prevent the polishing pad 30 from drying out due to cooling by the cooled gas. Instead of water, ethanol or isopropanol may be injected into the gas stream to form frozen particles.

[0088] Gas (e.g., compressed gas) from a gas source 132 can be connected to a vortex tube 50, which can separate the compressed gas into a cold flow and a hot flow, and direct the cold flow to the nozzle 120 onto the polishing pad 30. In some implementations, the nozzle 120 is the lower end of the vortex tube, which directs the cold flow of compressed gas onto the polishing pad 30.

[0089] In some implementations, process parameters such as flow rate, pressure, temperature, and / or liquid to gas mixture ratio may be independently controlled for each nozzle (e.g., by controller 12). For example, the coolant for each nozzle 120 may flow through an independently controllable chiller to independently control the temperature of the spray. As another example, a separate pair of pumps (one for gas and one for liquid) may be connected to each nozzle so that the flow rate, pressure, and gas to liquid mixture ratio may be independently controlled for each nozzle.

[0090] Various nozzles can spray on different radial zones 124 on the polishing pad 30. Adjacent radial zones 124 can overlap. In some implementations, the nozzles 120 produce a spray that impinges on the polishing pad 30 along an elongated region 128. For example, the nozzles can be configured to produce a spray in a substantially planar triangular space.

[0091] One or more of the elongated regions 128 (eg, all of the elongated regions 128) may have a longitudinal axis (see region 128a) that is parallel to a radius extending through the region 128. Alternatively, the nozzle 120 produces a cone-shaped spray.

[0092] although Figure 1 While the sprays themselves are shown overlapping, the nozzles 120 may be oriented so that the elongated regions do not overlap. For example, at least some of the nozzles 120 (eg, all of the nozzles 120) may be oriented so that the elongated regions 128 are at an oblique angle relative to a radius through the elongated regions (see region 128b).

[0093] At least some of the nozzles 120 can be oriented so that the central axis of the spray from the nozzle (see arrow A) is at an oblique angle relative to the polishing surface 36. Specifically, the spray 122 can be directed from the nozzle 120 to have a horizontal component (see arrow A) in a direction opposite to the direction of movement of the polishing pad 30 in the impact area caused by the rotation of the platform 24.

[0094] although Figure 3A and Figure 3B The nozzles 120 are shown as being spaced at uniform intervals, which is not required. The nozzles 120 may be distributed non-uniformly in the radial direction or in the angle, or both. For example, the nozzles 120 may be more densely clustered along the radial direction toward the edge of the polishing pad 30. In addition, although Figure 3A and Figure 3B While nine nozzles are shown, a greater or lesser number of nozzles may be present, such as three to twenty nozzles.

[0095] The cooling system 102 may be used to reduce the temperature of the polishing surface 36. For example, the temperature of the polishing surface 36 may be reduced using liquid from the liquid coolant 130 via the spray 122, gas from the gas coolant 132 via the spray 122, the cold stream 52 from the vortex tube 50, or a combination thereof. In some embodiments, the temperature of the polishing surface 36 may be reduced to or below 20° C. Reducing the temperature during one or more of the metal cleaning, overpolishing, or conditioning steps may reduce dishing and erosion of soft metals during CMP by reducing the selectivity of the polishing liquid 38.

[0096] In some implementations, a temperature sensor measures the temperature of the polishing pad or the temperature of the polishing liquid on the polishing pad, and a controller executes a closed-loop control algorithm to control the flow rate of the coolant relative to the flow rate of the polishing liquid so as to maintain the polishing pad or the polishing liquid on the polishing pad at a desired temperature.

[0097] Reducing the temperature during CMP can be used to reduce corrosion. For example, reducing the temperature during one or more of the metal cleaning, overpolishing, or conditioning steps can reduce galvanic corrosion in various components, as galvanic corrosion can be temperature dependent. In addition, during CMP, the vortex tube 50 can use a gas that is inert in the polishing process. Specifically, a gas lacking oxygen (or having less oxygen than normal atmosphere) can be used to establish a local inert environment to reduce oxygen in the local inert environment, which can result in reduced corrosion. Examples of such gases include nitrogen and carbon dioxide (e.g., evaporated from liquid nitrogen or dry ice).

[0098] Lowering the temperature of the polishing surface 36 (e.g., for a conditioning step) can increase the storage modulus of the polishing pad 30 and reduce the viscoelasticity of the polishing pad 30. The increased storage modulus and reduced viscoelasticity combined with reduced down force on the pad conditioning disk 92 and / or less aggressive conditioning by the pad conditioning disk 92 can result in a more uniform pad roughness. Advantages of a uniform pad roughness are reduced scratching on the substrate 10 during subsequent polishing operations and increased life of the polishing pad 30.

[0099] In some implementations, instead of or in addition to using a coolant to reduce the temperature of the polishing liquid, a heated fluid (e.g., steam) can be injected into the polishing liquid 38 (e.g., a slurry) to raise the temperature of the polishing liquid 38 before the polishing liquid 38 is dispensed. Alternatively, the heated fluid (e.g., steam) can be directed onto the polishing pad, i.e., such that the temperature of the polishing liquid is adjusted after the polishing liquid is dispensed.

[0100] For the heating system 104, the heating fluid may be a gas (e.g., steam (e.g., from a steam generator 410, see Figure 4A) or heated air), or a liquid (e.g., heated water), or a combination of gas and liquid. The heated fluid is above room temperature, for example at 40-120° C., for example at 90-110° C. The fluid can be water, such as substantially pure deionized water, or water including additives or chemicals. In some implementations, the heating system 104 uses a spray of steam. The steam can include additives or chemicals.

[0101] The heated fluid may be delivered by flowing through apertures (eg holes or slots) in the heated delivery arm (eg provided by one or more nozzles). The apertures may be provided by a manifold connected to a source of the heated fluid.

[0102] The example heating system 104 includes an arm 140 that extends over the platform 24 and the polishing pad 30, from the edge of the polishing pad to or at least close to (e.g., within 5% of the total radius of the polishing pad) the center of the polishing pad 30. The arm 140 can be supported by a base 142, and the base 142 can be supported on the same frame 40 as the platform 24. The base 142 can include one or more actuators, such as linear actuators to raise or lower the arm 140, and / or rotary actuators to swing the arm 140 laterally over the platform 24. The arm 140 is positioned to avoid collision with other hardware components, such as the polishing head 70, the pad conditioning disk 92, and the slurry dispenser 39.

[0103] Along the rotation direction of the platform 24, the arm 140 of the heating system 104 may be positioned between the arm 110 of the cooling system 110 and the carrier head 70. Along the rotation direction of the platform 24, the arm 140 of the heating system 104 may be positioned between the arm 110 of the cooling system 110 and the slurry dispenser 39. For example, the arm 110 of the cooling system 110, the arm 140 of the heating system 104, the slurry dispenser 39, and the carrier head 70 may be positioned in this order along the rotation direction of the platform 24.

[0104] A plurality of openings 144 are formed in the bottom surface of the arm 140. Each opening 144 is configured to direct a gas or vapor (e.g., steam) onto the polishing pad 30. The arm 140 can be supported by the base 142 so that the opening 144 is separated from the polishing pad 30 by a gap. The gap can be 0.5 mm to 5 mm. Specifically, the gap can be selected so that the heat of the heating fluid does not significantly dissipate before the fluid reaches the polishing pad. For example, the gap can be selected so that the steam emitted from the opening does not condense before reaching the polishing pad.

[0105] The heating system 104 may include a source 148 of steam (e.g., a steam generator 410 (see Figure 4A )), a source 148 of steam can be connected to the arm 140 via a pipe. Each opening 144 can be configured to direct steam toward the polishing pad 30.

[0106] In some implementations, process parameters such as flow rate, pressure, temperature, and / or liquid to gas mixture ratio can be independently controlled for each nozzle. For example, the fluid of each opening 144 can flow through an independently controllable heater to independently control the temperature of the heated fluid (e.g., the temperature of the steam).

[0107] The various openings 144 can direct the steam onto different radial zones on the polishing pad 30. Adjacent radial zones can overlap. Optionally, some of the openings 144 can be oriented so that the central axis of the spray from such openings is at an oblique angle relative to the polishing surface 36. The steam can be directed from one or more of the openings 144 to have a horizontal component in a direction opposite to the direction of motion of the polishing pad 30 in the impact area caused by the rotation of the platform 24.

[0108] although Figure 3B The openings 144 are shown as being spaced at uniform intervals, which is not required. The nozzles 120 may be distributed non-uniformly in the radial direction or in the angle, or both. For example, the openings 144 may be more densely clustered toward the center of the polishing pad 30. As another example, the openings 144 may be more densely clustered at a radius corresponding to the radius at which the polishing liquid 38 is delivered to the polishing pad 30 by the slurry dispenser 39. In addition, although Figure 3B While nine openings are shown, a greater or lesser number of openings may be provided.

[0109] Reference Figure 3A and Figure 3B , from steam generator 410 (see Figure 4A ) can be injected into the polishing liquid 38 (e.g., slurry) before the polishing liquid 38 is dispensed and raises the temperature of the polishing liquid 38. The advantage of using steam 245 rather than liquid water to heat the polishing liquid 38 is that a smaller amount of steam 245 will need to be injected into the polishing liquid 38 because the latent heat of vaporization allows for greater energy to be transferred from the steam than from liquid water. Moreover, because less steam 245 is required to raise the temperature of the polishing pad 38 than liquid water, the polishing liquid 38 does not become too diluted. Steam can be injected into the polishing liquid at a flow ratio of 1:100 to 1:5. For example, a small amount of steam 245 (e.g., 1 cc of steam 245 (at 1 atm) for every 50 cc of polishing liquid 38) can be used to heat the polishing liquid 38.

[0110] The vapor 245 and the polishing liquid 38 may be mixed in a mixing chamber 35 positioned within an arm of the polishing dispenser 39. A heating fluid (e.g., vapor 245) may also be used to heat the slurry dispenser 39 and / or the polishing liquid reservoir 37, which in turn may heat the polishing liquid 38 prior to being dispensed onto the polishing pad 30.

[0111] Steam 245 can similarly be used to heat other liquids used in CMP, such as deionized water and other chemicals (e.g., cleaning chemicals). In some embodiments, these liquids can be mixed with polishing liquid 38 before being dispensed by slurry dispenser 39. The increased temperature can increase the chemical etch rate of polishing liquid 38, thereby enhancing its efficiency during the polishing operation and reducing the amount of polishing liquid 38 required.

[0112] In some implementations, a temperature sensor measures the temperature of the mixture, and a controller executes a closed-loop control algorithm to control the flow rate of the steam relative to the flow rate of the polishing liquid in order to maintain the mixture at a desired temperature.

[0113] In some implementations, a temperature sensor measures the temperature of the polishing pad or slurry on the polishing pad, and a controller executes a closed-loop control algorithm to control the flow rate of the steam relative to the flow rate of the polishing liquid to maintain the polishing pad or slurry on the polishing pad at a desired temperature.

[0114] The controller 12 can control the flow of steam 245 by positioning a nozzle or valve (e.g., a steam valve) (not shown) between the steam generator 410 and the slurry dispenser 39, and the controller 12 can control the flow of polishing liquid 38 by positioning a nozzle or valve (e.g., a polishing liquid valve) (not shown) between the polishing liquid storage chamber 37 and the slurry dispenser 39.

[0115] The steam 245 and the polishing liquid 38 may be mixed in a mixing chamber 35 positioned within an arm of the slurry dispenser 39. A heating fluid (e.g., steam 245) may also be used to heat the slurry dispenser 39 and / or the polishing liquid reservoir 37, which in turn may heat the polishing liquid 38 before dispensing the polishing liquid 38 onto the polishing pad 30.

[0116] Steam 245 can similarly be used to heat other liquids used in CMP, such as deionized water and other chemicals (e.g., cleaning chemicals). In some embodiments, these liquids can be mixed with polishing liquid 38 before being dispensed by slurry dispenser 39. The increased temperature can increase the chemical etch rate of polishing liquid 38, thereby enhancing its efficiency during the polishing operation and reducing the amount of polishing liquid 38 required.

[0117] The polishing system 20 may also include a high pressure rinse system 106. The high pressure rinse system 106 includes a plurality of nozzles 154 (e.g., three to twenty nozzles) that direct a cleaning fluid (e.g., water) at high intensity onto the polishing pad 30 to clean the pad 30 and remove used slurry, polishing debris, and the like.

[0118] like Figure 3BAs shown, the example rinsing system 106 includes an arm 150 extending above the platform 24 and the polishing pad 30 from the edge of the polishing pad to or at least close to (e.g., within 5% of the total radius of the polishing pad) the center of the polishing pad 30. The arm 150 can be supported by a base 152, and the base 152 can be supported on the same frame 40 as the platform 24. The base 152 can include one or more actuators, such as a linear actuator to raise or lower the arm 150, and / or a rotary actuator to swing the arm 150 laterally above the platform 24. The arm 150 is positioned to avoid collision with other hardware components, such as the polishing head 70, the pad conditioning disk 92, and the slurry dispenser 39.

[0119] The arm 150 of the rinsing system 106 may be positioned between the arm 110 of the cooling system 110 and the arm 140 of the heating system 140 along the rotation direction of the platform 24. For example, the arm 110 of the cooling system 110, the arm 150 of the rinsing system 106, the arm 140 of the heating system 104, the slurry dispenser 39, and the carrier head 70 may be positioned in this order along the rotation direction of the platform 24. Alternatively, the arm 140 of the cooling system 104 may be between the arm 150 of the rinsing system 106 and the arm 140 of the heating system 140 along the rotation direction of the platform 24. For example, the arm 150 of the rinsing system 106, the arm 110 of the cooling system 110, the arm 140 of the heating system 104, the slurry dispenser 39, and the carrier head 70 may be positioned in this order along the rotation direction of the platform 24.

[0120] although Figure 3B The nozzles 154 are shown as being spaced at even intervals, which is not required. Figure 3A and Figure 3B While nine nozzles are shown, a greater or lesser number of nozzles may be present, such as three to twenty nozzles.

[0121] The polishing system 2 may also include a controller 12 to control the operation of various components (e.g., the temperature control system 100). The controller 12 is configured to receive temperature measurements from the temperature sensors 64 for each radial zone of the polishing pad. The controller 12 may compare the measured temperature profile to the desired temperature profile and generate feedback signals to the control mechanism (e.g., actuators, power supplies, pumps, valves, etc.) for each nozzle or opening. The feedback signals are calculated by the controller 12 (e.g., based on an internal feedback algorithm) to cause the control mechanism to adjust the amount of cooling and heating so that the polishing pad and / or slurry reaches (or at least moves closer to) the desired temperature profile.

[0122] In some implementations, the polishing system 20 includes a wiper blade or body 170 to evenly distribute the polishing liquid 38 across the polishing pad 30. The wiper blade 170 can be between the slurry dispenser 39 and the carrier head 70 along the direction of rotation of the platen 24.

[0123] Figure 3B Separate arms are shown for each subsystem (e.g., heating system 102, cooling system 104, and cleaning system 106), and the various subsystems may be included in a single assembly supported by a common arm. For example, an assembly may include a cooling module, a cleaning module, a heating module, a slurry transfer module, and an optional arc brush module. Each module may include a body (e.g., an arcuate body) that can be fastened to a common mounting plate, and the common mounting plate can be fastened at the end of the arm so that the assembly is positioned above the polishing pad 30. Various fluid transfer components (e.g., pipes, passages, etc.) may extend within each body. In some implementations, the modules are individually removable from the mounting plate. Each module may have similar components to perform the functions of the arms of the associated system described above.

[0124] Reference Figure 4A Steam for the processes described herein or for other uses in a chemical mechanical polishing system can be generated using a steam generator 410. An example steam generator 410 may include a tank 420 enclosing an interior space 425. The walls of the tank 420 may be made of a thermally insulating material (e.g., quartz) having very low levels of mineral contaminants. Alternatively, the walls of the tank may be formed of another material, for example, and the interior surface of the tank may be coated with polytetrafluoroethylene (PTFE) or another plastic. In some implementations, the tank 420 may be 10-20 inches long and 1-5 inches wide.

[0125] Reference Figure 4A and Figure 4BIn some embodiments, the interior space 425 of the tank 420 is divided into a lower chamber 422 and an upper chamber 424 by a barrier layer 426. The barrier layer 426 may be made of the same material as the tank wall (e.g., quartz, stainless steel, aluminum, or a ceramic such as alumina). Quartz may be superior in reducing the risk of contamination. The barrier layer 426 may include one or more holes 428. The holes 428 may be located at the edge of the barrier layer 426 where the barrier layer 426 meets the interior wall of the tank 420 (e.g., only at the edge). The holes 428 may be located near the edge of the barrier layer 426, such as between the edge of the barrier layer 426 and the center of the barrier layer 426. In some implementations, the holes are also located away from the edge, such as across the width of the barrier layer 426, such as evenly spaced across the area of ​​the barrier layer 425. The barrier layer 426 may substantially prevent liquid water 440 from entering the upper chamber 424 by blocking water droplets splashed by boiling water. This allows dry steam to accumulate in the upper chamber 424. The holes 428 allow steam to pass from the lower chamber 422 into the upper chamber 424. The holes 428, and particularly the holes 428 near the edge of the barrier layer 426, can allow condensation on the walls of the upper chamber 424 to drip down into the lower chamber 422 to reduce the liquid content in the upper chamber 426 and allow the liquid to reheat with the water 440.

[0126] Reference Figure 4A The water inlet 432 may connect the water storage chamber 434 to the lower chamber 422 of the tank body 420. The water inlet 432 may be positioned at or near the bottom of the tank body 420 to provide water 440 to the lower chamber 422.

[0127] One or more heating elements 430 may surround a portion of the lower chamber 422 of the tank 420. For example, the heating element 430 may be a heating coil (e.g., a resistive heater) wrapped around the outside of the tank 420. The heating element may also be provided by a thin film coating on the material of the tank sidewall; if an electric current is applied, this thin film coating may act as a heating element.

[0128] The heating element 430 may also be positioned within the lower chamber 422 of the tank 420. For example, the heating element may be coated with a material that prevents contaminants (eg, metal contaminants) from migrating from the heating element into the steam.

[0129] The heating element 430 may apply heat to the bottom portion of the tank body 420 up to the minimum water level 443a. That is, the heating element 430 may cover the portion of the tank body 420 below the minimum water level 443a to avoid overheating and reduce unnecessary energy expenditure.

[0130] The steam outlet 436 can connect the upper chamber 424 to a steam delivery passage 438. The steam delivery passage 438 can be located at or near the top of the tank 420 (e.g., in a ceiling of the tank 420) to allow steam to pass from the tank 420 into the steam delivery passage 438 and to various components of the CMP apparatus. The steam delivery passage 438 can be used to deliver steam toward various areas of the chemical mechanical polishing apparatus, such as for steam cleaning and preheating of the carrier head 70, substrate 10, and pad conditioning plate 92.

[0131] Reference Figure 4A In some embodiments, a filter 470 is coupled to the steam outlet 438, and the steam outlet 438 is configured to reduce contaminants in the steam 446. The filter 470 can be an ion exchange filter.

[0132] Water 440 may flow from the water reservoir 434 through the water inlet 432 and into the lower chamber 422. The water 440 may fill the tank 420 at least until a water level 442 above the heating element 430 and below the barrier 426. As the water 440 is heated, a gaseous medium 446 is generated and rises through the holes 428 of the barrier 426. The holes 428 allow the steam to rise and simultaneously allow condensation to fall, resulting in a gaseous medium 446 in which the water is a vapor that is substantially free of liquid (e.g., without liquid water droplets suspended in the vapor).

[0133] In some embodiments, the water level is determined using a water level sensor 460 that measures the water level 442 in a bypass tube 444. The bypass tube connects the water reservoir 434 to a vapor transmission passage 438 that is parallel to the tank 420. The water level sensor 460 can indicate what the water level 442 is within the bypass tube 444, and therefore what the water level 442 is within the tank 420. For example, the water level sensor 444 and the tank 420 are equally pressurized (e.g., both receive water from the same water reservoir 434 and both have the same pressure at the top, e.g., both are connected to the vapor transmission passage 438), so that the water level 442 is the same between the water level sensor and the tank 420. In some embodiments, the water level 442 in the water level sensor 444 can indicate the water level 442 in the tank 420 in other ways, for example, the water level 442 in the water level sensor 444 is scaled to indicate the water level 442 in the tank 420.

[0134] In operation, the water level 442 in the tank is above the minimum water level 443a and below the maximum water level 443b. The minimum water level 443a is at least above the heating element 430, and the maximum water level 443b is significantly below the steam outlet 436 and the barrier layer 426, so that sufficient space is provided to allow the gaseous medium 446 (e.g., steam) to accumulate at the top of the tank 420 and still be substantially free of liquid water.

[0135] In some embodiments, the controller 12 is coupled to a valve 480 that controls fluid flow through the water inlet 432, a valve 482 that controls fluid flow through the steam outlet 436, and / or a water level sensor 460. Using the water level sensor 460, the controller 90 is configured to modulate the flow of water 440 into the tank 420 and the flow of gas 446 out of the tank 420 to maintain a water level 442 above a minimum water level 443a (and above the heating element 430) and below a maximum water level 443b (and below the barrier 426, if present). The controller 12 may also be coupled to a power source 484 for the heating element 430 in order to control the amount of heat transferred to the water 440 in the tank 420.

[0136] Reference Figure 1 , Figure 2A , Figure 2B , Figure 3A , Figure 3B and Figure 4A , the controller 12 can monitor the temperature measurements received via the sensors 64, 214, and 264 and control the temperature control system 100, the water inlet 432, and the steam outlet 436. The controller 12 can continuously monitor the temperature measurements and control the temperatures in a feedback loop to tune the temperatures of the polishing pad 30, the carrier head 70, and the conditioning plate 92. For example, the controller 12 can receive the temperature of the polishing pad 30 from the sensor 64 and control the water inlet 432 and the steam outlet 436 to control the delivery of steam to the carrier head 70 and / or the conditioning head 92 to raise the temperature of the carrier head 70 and / or the conditioning head 92 to match the temperature of the polishing pad 30. Reducing the temperature differential can help prevent the carrier head 70 and / or the conditioning head 92 from acting as a heat sink on the relatively higher temperature polishing pad 30 and can enhance intra-wafer uniformity.

[0137] In some embodiments, the controller 12 stores desired temperatures for the polishing pad 30, the carrier head 70, and the conditioning plate 92. The controller 12 can monitor the temperature measurements from the sensors 64, 214, and 264, and control the temperature control system 100, the water inlet 432, and the steam outlet 436 to achieve the desired temperatures for the polishing pad 30, the carrier head 70, and / or the conditioning plate 92. By causing the temperatures to reach the desired temperatures, the controller 12 can enhance intra-wafer uniformity and inter-wafer uniformity.

[0138] Alternatively, the controller 12 may raise the temperature of the carrier head 70 and / or the conditioning head 92 to be slightly higher than the temperature of the polishing pad 30 to allow the carrier head 70 and / or the conditioning head 92 to cool to the same or substantially the same temperature as the polishing pad 30 when moving from their respective cleaning and preheating stations to the polishing pad 30.

[0139] In another process, the temperature of the polishing liquid 38 is raised for batch polishing operations. After the batch polishing operation, the temperature of various components of the carrier head 70 (eg, polishing surface 36, conditioning disk 92) may be cooled for metal cleaning, over-polishing, and / or conditioning operations.

[0140] Several embodiments of the present invention have been described. However, it should be understood that various modifications can be made without departing from the invention and its scope. Therefore, other embodiments are within the scope of the following claims.

Claims

1. A chemical mechanical polishing system, comprising: A platform for supporting a polishing pad having a polishing surface; a steam source, the steam source comprising a steam generator; a storage chamber for holding a polishing liquid; as well as Sources of cleaning chemicals; The vapor source is coupled to the cleaning chemistry and is configured to deliver the vapor into the cleaning chemistry to heat the cleaning chemistry before the cleaning chemistry is used in chemical mechanical polishing.

2. The system of claim 1, wherein the steam generator causes the steam to be heated to 90-200°C.

3. The system of claim 1, wherein the steam source is coupled to a dispenser arm extending above the platform so as to deliver steam to the cleaning chemical in the dispenser arm.

4. The system of claim 3, wherein the steam source is coupled to a mixing chamber located in the dispenser arm so as to deliver steam to the cleaning chemical in the mixing chamber.

5. The system of claim 1, comprising one or more valves for controlling the relative flow rates of steam and cleaning chemicals.

6. The system of claim 5, comprising a controller configured to control the one or more valves so that the steam and the cleaning chemical are mixed at a flow rate ratio of 10:1 to 1:

10.

7. A chemical mechanical polishing system comprising: A platform for supporting a polishing pad having a polishing surface; a steam source, the steam source comprising a steam generator; a storage chamber for holding a polishing liquid; and a source of deionized water; The steam source is coupled to the deionized water and is configured to deliver the steam into the deionized water to heat the deionized water before the deionized water is used for chemical mechanical polishing.

8. The system of claim 7, wherein the steam generator causes the steam to be heated to 90-200°C.

9. The system of claim 7, wherein the steam source is coupled to a dispenser arm extending above the platform so as to deliver steam into the deionized water in the dispenser arm.

10. The system of claim 9, wherein the steam source is coupled to a mixing chamber located in the dispenser arm so as to deliver steam into the deionized water in the mixing chamber.

11. The system of claim 7, comprising one or more valves for controlling the relative flow rates of steam and deionized water.

12. The system of claim 11, comprising a controller configured to control the one or more valves such that the steam and the deionized water are mixed at a flow rate ratio of 10:1 to 1:10.

Citation Information

Patent Citations

  • Chemical mechanical polishing apparatus

    CN109397071A

  • Semiconductor manufacturing method and polishing equipment

    JP2007035973A

  • Polishing device and substrate processing device

    JP2018187724A

  • System and Method of Delivering Slurry for Chemical Mechanical Polishing

    US20170361419A1

  • Apparatus and process for high temperature wafer edge polishing

    US6257954B1