Flexible heat-conducting material with low oil permeability, high elongation and high resilience and preparation method of flexible heat-conducting material
Thermal conduction materials are solved by using low viscosity vinyl silicone oil, hydrogen-containing silicone oil and end-hydrogen-containing silicone oil with thermal powders in thermal conduction materials, and the use of unsaturated group coupling agent and platinum catalysts. The problem of high is that flexible thermal conductivity materials with low permeability oil, high elongation and high resilience performance are achieved.
Patent Information
- Application Number
- CN202411170431.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing thermally conductive materials are prone to oil leakage after curing, resulting in deterioration of thermal and mechanical properties, excessive hardness, easy breakage of materials, and excessive hardness after filling with thermally conductive powder, resulting in insufficient interfacial adhesion, affecting thermal conductivity.
Low viscosity vinyl silicone oil, hydrogen-containing silicone oil and end hydrogen-containing silicone oil are used to polymerize with thermally conductive powders, and unsaturated group coupling agents are used to modify the thermally conductive powders to reduce viscosity and lock in small molecular substances to form dense crosslinks Structure, reduce exudation, and add platinum catalyst and inhibitor to silica gel to control crosslink density.
A flexible thermally conductive material with low permeability oil, high elongation and high resilience performance is achieved, avoiding the problems of exudation and excessive hardness, and ensuring the balance of thermal conductivity and mechanical properties.
Smart Images

Figure CN118931198A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of heat-conducting materials, and in particular to a flexible heat-conducting material with low oil permeability, high elongation and high resilience, and a preparation method thereof. Background Art
[0002] With the rapid development of semiconductor technology and the continuous progress of electric vehicle technology, the increasing power density also causes heat to accumulate in a limited space, and the problem of heat conduction has received more and more attention. Among them, composite materials prepared by filling thermal conductive powders such as alumina, aluminum hydroxide, aluminum nitride, and boron nitride with silicone gel as the matrix have been favored and widely used because of their softness, high and low temperature resistance, aging resistance, flame retardancy, insulation and low cost. The thermal conductivity of silicone materials themselves is poor, only about 0.2W / (mk), and cannot be used as thermal conductive materials. After filling thermal conductive powder in silica gel, the thermal conductive powder forms a thermal conductive path in the silica gel material, which can achieve a higher thermal conductivity. Therefore, the filling rate of the filler (i.e., the volume ratio or mass ratio of thermal conductive powder to silicone material) is positively correlated with the thermal conductivity of the thermal conductive composition. When filling liquid silicone with thermal conductive powder, the viscosity of the mixture will increase with the increase of the filling amount, which will bring difficulties to subsequent processing. There are usually two ways to improve this problem: one is powder optimization, that is, by selecting thermally conductive powders of specific shapes and particle sizes or modifying the fillers, the compatibility between inorganic powders and organic silica gel can be improved, thereby reducing the viscosity. On the other hand, vinyl silicone oil with lower viscosity can be used; however, low-viscosity vinyl silicone oil has a small molecular weight, and often requires several cross-linkings to form larger molecules or a network molecular structure, resulting in the thermal conductive composition often containing a large number of parts with small molecular weight or insufficient cross-linking after curing. These components have good mobility, causing the thermal management material to leak oil after curing. Oil leakage will not only pollute the application environment, but also cause the thermal conductivity and mechanical properties of the material itself to deteriorate, such as hardening, brittleness, cracking, etc. In order to improve the oil leakage problem, it is usually necessary to increase the amount of hydrogen-containing silicone oil used, reduce the remaining low molecular weight components, increase the cross-linking density, and inhibit the seepage of low molecular weight substances. However, due to the relatively high vinyl content of low-viscosity vinyl silicone oil itself, the spatial network structure after cross-linking has too many cross-linking points, and the large amount of filler added, the hardness of the thermal conductive material after heating and curing is too high, often higher than 80 Shore OO. Excessive hardness will not only make the material too brittle and easy to break, but also lead to insufficient interface adhesion between the thermal conductive material product (such as thermal conductive gasket), the heating element (such as chip) and the heat sink, resulting in excessive interface thermal resistance, affecting the overall thermal conductivity and heat dissipation effect. In order to achieve a higher thermal conductivity coefficient, it is necessary to fill a large amount of thermal conductive powder in the silica gel. In order to achieve low thermal resistance, it is necessary to reduce the cross-linking density of the thermal conductive material, thereby reducing the hardness. This leads to serious deterioration of the mechanical properties of the material, poor elongation and rebound performance, and easy permanent deformation under a slight external force, which is not conducive to subsequent cutting and assembly processes. To this end, we propose a flexible thermal conductive material with low oil permeability, high elongation and high rebound and a preparation method thereof. Summary of the invention
[0003] The object of the present invention is to provide a flexible thermal conductive material with low oil permeability, high elongation and high resilience and a preparation method thereof, so as to solve the problems raised in the above background technology.
[0004] To achieve the above object, the present invention provides the following technical solutions:
[0005] A flexible thermal conductive material with low oil permeability, high elongation and high resilience, comprising the following raw materials:
[0006] Vinyl silicone oil;
[0007] Hydrogenated silicone oil;
[0008] Hydrogen terminated silicone oil;
[0009] Thermally conductive powder;
[0010] Coupling agent;
[0011] The ratio R of the sum of the amount of Si-H in the side hydrogen-containing silicone oil and the end hydrogen-containing silicone oil to the amount of CH2=CH- in the low-viscosity vinyl silicone oil is 1:0.9-1:2;
[0012] The ratio r of the amount of Si-H in the terminal hydrogen-containing silicone oil to the amount of Si-H in the multi-hydrogen-containing silicone oil is 0.8-1.3;
[0013] The low-viscosity vinyl silicone oil is a vinyl silicone oil with a viscosity of 50-200000 mPa·S.
[0014] Furthermore: the mass of the vinyl silicone oil is 100 parts, the mass of the thermally conductive powder is 800-1400 parts, the thermally conductive material also includes an inhibitor and a platinum catalyst, the mass of the inhibitor is 0.01-0.1 parts, and the mass of the platinum element in the platinum catalyst accounts for 3-20ppm of the total mass of the thermally conductive material.
[0015] Furthermore: the vinyl silicone oil is one or more of the compounds having the structure shown in A-1, A-2 or A-3.
[0016] Furthermore: the total hydrogen content of the terminal hydrogen-containing silicone oil and the hydrogen-containing silicone oil is 0.1%-1.0%, preferably 0.5%-1.0.
[0017] Furthermore: the thermally conductive powder is one or more of alumina, aluminum hydroxide, silicon powder, aluminum nitride, silicon nitride, silicon carbide, metal aluminum powder, and asphalt-based carbon fiber.
[0018] Furthermore: the shape of the thermally conductive powder is one of spherical, quasi-spherical and non-spherical, and the median particle size of the thermally conductive powder is 0.1-120 um.
[0019] Further: the coupling agent is one or more of a silane coupling agent, a titanate coupling agent, and an aluminate coupling agent.
[0020] Furthermore: the platinum catalyst is one or more of a Karstedt catalyst, a Speier catalyst, an Ashby catalyst, a Lamoreaux catalyst or a capsule-type platinum catalyst.
[0021] Further: the inhibitor is one or more of alkynol inhibitors, fumarate and maleate inhibitors, butynedioic acid ester inhibitors, carbene inhibitors, polyvinyl inhibitors or phosphite inhibitors.
[0022] A method for preparing a flexible thermally conductive material with low oil permeability, high elongation and high resilience comprises the following steps: firstly, wet-treating a thermally conductive powder with a silane coupling agent; uniformly mixing vinyl silicone oil, terminal hydrogenated silicone oil and the thermally conductive powder treated with the silane coupling agent, adding an optional inhibitor, an optional platinum catalyst and hydrogenated silicone oil, and performing a mixing and degassing process to obtain a flexible thermally conductive material with low oil permeability, high elongation and high resilience. The thermally conductive material can be used to prepare a thermally conductive gasket and a thermally conductive gel.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] The low-oil permeability, high-elongation, high-rebound flexible thermally conductive material and its preparation method, the thermally conductive material proposed in the present invention is composited with vinyl silicone oil, end-hydrogenated silicone oil, multi-hydrogenated silicone oil and thermally conductive powder, the three silicone oils undergo polymerization reaction to form a soft rubber body, and the thermally conductive powder coated therein forms a thermally conductive path. In the present invention, a coupling agent with an unsaturated group is used to modify the thermally conductive powder, so that the surface of the thermally conductive powder is provided with an unsaturated group, the compatibility between the powder and the silica gel is improved, and the viscosity is reduced. The unsaturated groups on the surface of the thermally conductive powder can undergo polymerization reaction with the end-hydrogenated silicone oil and the multi-hydrogenated silicone oil, thereby connecting the thermally conductive powder and the silica gel into one, reducing the damage to the mechanical properties of the silica gel caused by a large amount of filling of the thermally conductive powder, and the dense cross-linked structure can also lock small molecules to avoid seepage. Therefore, high elongation and high resilience can be guaranteed while achieving high thermal conductivity. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 This is a molecular diagram of the vinyl silicone oil of the present invention;
[0026] Figure 2 This is a molecular diagram of the end-containing hydrogen silicone oil of the present invention;
[0027] Figure 3 This is a molecular diagram of the hydrogen-containing silicone oil of the present invention. DETAILED DESCRIPTION
[0028] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0029] Example
[0030] See also Figure 1-3 The present invention provides a technical solution: a flexible thermal conductive material with low oil permeability, high elongation and high resilience, comprising the following raw materials:
[0031] Vinyl silicone oil;
[0032] Hydrogenated silicone oil;
[0033] Hydrogen terminated silicone oil;
[0034] Thermally conductive powder;
[0035] Coupling agent;
[0036] The ratio R of the sum of the amount of Si-H in the side hydrogen-containing silicone oil and the end hydrogen-containing silicone oil to the amount of CH2=CH- in the low-viscosity vinyl silicone oil is 1:0.9-1:2. Figure 3 The compound of the structure shown in B-2 and / or B-3, the terminal hydrogen-containing silicone oil is Figure 2 A compound having the structure shown in B-1;
[0037] The ratio r of the amount of Si-H in the terminal hydrogen-containing silicone oil to the amount of Si-H in the multi-hydrogen-containing silicone oil is 0.8-1.3;
[0038] The low-viscosity vinyl silicone oil is a vinyl silicone oil with a viscosity of 50-200000 mPa·S.
[0039] Among them, preferably, the mass of the vinyl silicone oil is 100 parts, the mass of the thermally conductive powder is 800-1400 parts, the thermally conductive material also includes an inhibitor and a platinum catalyst, and the mass of the inhibitor is 0.01-0.1 parts based on the mass of the vinyl silicone oil as 100 parts, and the mass of the platinum element in the platinum catalyst accounts for 3-20ppm of the total mass of the thermally conductive material.
[0040] Preferably, the vinyl silicone oil is one or more of the compounds having the structure shown in A-1, A-2 or A-3.
[0041] Preferably, the total hydrogen content of the terminal hydrogen-containing silicone oil and the hydrogen-containing silicone oil is 0.1%-1.0%, preferably 0.5%-1.0.
[0042] Preferably, the thermally conductive powder is one or more of alumina, aluminum hydroxide, silicon powder, aluminum nitride, silicon nitride, silicon carbide, metal aluminum powder, and asphalt-based carbon fiber.
[0043] Preferably, the shape of the thermally conductive powder is spherical, quasi-spherical, and non-spherical, preferably spherical, and the thermally conductive powder has a median particle size of 0.1-120 um, preferably 0.1-40 um.
[0044] Preferably, the coupling agent is one or more of a silane coupling agent, a titanate coupling agent, and an aluminate coupling agent. If the amount of the coupling agent is too little, the thermally conductive powder will not be sufficiently coated; if the amount is too much, the excess coupling agent will cause isolation between the powder and the silica gel, reducing the thermal conductivity and mechanical properties of the material. Therefore, preferably, the amount of the silane coupling agent is 0.05-5% of the mass of the thermally conductive powder, preferably 0.5-1%.
[0045] Preferably, the platinum catalyst is one or more of a Karstedt catalyst, a Speier catalyst, an Ashby catalyst, a Lamoreaux catalyst or a capsule-type platinum catalyst, preferably a Karstedt catalyst.
[0046] Preferably, the inhibitor is one or more of an acetylenic alcohol inhibitor, a fumarate ester, a maleate ester inhibitor, a butynedioate inhibitor, a carbene inhibitor, a polyvinyl inhibitor or a phosphite inhibitor, preferably a polyvinyl inhibitor, and more preferably tetramethyltetravinylcyclotetrasiloxane.
[0047] A method for preparing a flexible thermally conductive material with low oil permeability, high elongation and high resilience, method 1: comprising the following steps: firstly, wet-treating a thermally conductive powder with a silane coupling agent; uniformly mixing vinyl silicone oil, terminal hydrogenated silicone oil and the thermally conductive powder treated with the silane coupling agent, adding an optional inhibitor, an optional platinum catalyst and hydrogenated silicone oil, and performing a mixing and degassing process to obtain a flexible thermally conductive material with low oil permeability, high elongation and high resilience, wherein the thermally conductive material can be used to prepare a thermally conductive gasket and a thermally conductive gel;
[0048] Method 2: Vinyl silicone oil, terminal hydrogenated silicone oil, thermally conductive powder, hydrogenated silicone oil, optional inhibitor and optional platinum catalyst are mixed and degassed to obtain a low-permeability oil, high-elongation and high-rebound flexible thermally conductive material; The third object of the present invention is to provide a use of a thermally conductive material, which can be used to prepare thermally conductive gaskets and thermally conductive gels.
[0049] The electrical appliances mentioned in this article are all connected to an external power source through wires.
[0050] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A flexible thermal conductive material with low oil permeability, high elongation and high resilience, characterized by: The raw materials include the following components: Vinyl silicone oil; Hydrogenated silicone oil; Hydrogen terminated silicone oil; Thermally conductive powder; Coupling agent; The ratio R of the sum of the amount of Si-H in the side hydrogen-containing silicone oil and the end hydrogen-containing silicone oil to the amount of CH2=CH- in the low-viscosity vinyl silicone oil is 1:0.9-1:2; The ratio r of the amount of Si-H in the terminal hydrogen-containing silicone oil to the amount of Si-H in the multi-hydrogen-containing silicone oil is 0.8-1.3; The low-viscosity vinyl silicone oil is a vinyl silicone oil with a viscosity of 50-200000 mPa·S.
2. The flexible thermal conductive material with low oil permeability, high elongation and high resilience according to claim 1, characterized in that: The mass of the vinyl silicone oil is 100 parts, the mass of the thermal conductive powder is 800-1400 parts, and the thermal conductive material also includes an inhibitor and a platinum catalyst. The mass of the inhibitor is 0.01-0.1 parts, and the mass of the platinum element in the platinum catalyst accounts for 3-20ppm of the total mass of the thermal conductive material.
3. The flexible thermal conductive material with low oil permeability, high elongation and high resilience according to claim 1, characterized in that: The vinyl silicone oil is one or more of the compounds having the structure shown in A-1, A-2 or A-3.
4. The low oil permeability, high elongation and high resilience flexible thermal conductive material according to claim 1, characterized in that: The total hydrogen content of the terminal hydrogen-containing silicone oil and the hydrogen-containing silicone oil is 0.1%-1.0%, preferably 0.5%-1.
0.
5. The low oil permeability, high elongation and high resilience flexible thermal conductive material according to claim 1, characterized in that: The thermally conductive powder is one or more of aluminum oxide, aluminum hydroxide, silicon powder, aluminum nitride, silicon nitride, silicon carbide, metal aluminum powder, and asphalt-based carbon fiber.
6. The low oil permeability, high elongation and high resilience flexible thermal conductive material according to claim 1, characterized in that: The shape of the thermally conductive powder is one of spherical, quasi-spherical and non-spherical, and the median particle size of the thermally conductive powder is 0.1-120 um.
7. The low oil permeability, high elongation and high resilience flexible thermal conductive material according to claim 1, characterized in that: The coupling agent is one or more of a silane coupling agent, a titanate coupling agent, and an aluminate coupling agent.
8. The low oil permeability, high elongation and high resilience flexible thermal conductive material according to claim 2, characterized in that: The platinum catalyst is one or more of a Karstedt catalyst, a Speier catalyst, an Ashby catalyst, a Lamoreaux catalyst or a capsule-type platinum catalyst.
9. The low oil permeability, high elongation and high resilience flexible thermal conductive material according to claim 2, characterized in that: The inhibitor is one or more of alkynol inhibitors, fumarate and maleate inhibitors, butynedioic acid ester inhibitors, carbene inhibitors, polyvinyl inhibitors or phosphite inhibitors.
10. A method for preparing a flexible thermally conductive material with low oil permeability, high elongation and high resilience according to any one of claims 1 to 9, characterized in that: The method comprises the following steps: firstly, wet-treating the thermal conductive powder with a silane coupling agent; uniformly mixing vinyl silicone oil, terminal hydrogenated silicone oil and the thermal conductive powder treated with the silane coupling agent, adding an optional inhibitor, an optional platinum catalyst and hydrogenated silicone oil, and obtaining a low-oil permeability, high-elongation and high-rebound flexible thermal conductive material after uniform mixing and degassing. The thermal conductive material can be used to prepare thermal conductive gaskets and thermal conductive gels.