Space strengthening agent for space navigation
Through graphene-encapsulated nanofiber composite materials of tourmaline and titanium dioxide, combined with rare earth oxides and fullerenes, the problems of air pollution and bacterial growth in the space environment are solved, and the release of negative oxygen ions and air purification capacity are significantly improved. Improve the living environment of astronauts.
Patent Information
- Application Number
- CN202411063047.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In the space environment, air pollution and bacterial breeding problems are difficult to solve. The existing tourmaline materials have insufficient negative oxygen ions to effectively purify the air and improve the living environment of astronauts.
The nanofiber composite material that wraps tourmaline and titanium dioxide is prepared by autoclave heating, ultrasonic dispersion and electrospinning technology. The combination of rare earth oxides and fullerenes is used to enhance the release capacity of negative oxygen ions. .
It significantly improves the release of negative oxygen ions and air purification capabilities, improves the living environment of astronauts, improves the quality of life in space, and provides guarantees for long-term manned space missions.
Smart Images

Figure BDA0004978551010000051 
Figure BDA0004978551010000061 
Figure BDA0004978551010000062
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of coatings, in particular to a space aerospace bonding agent. Background Art
[0002] Negative ions (NAI), also known as negative oxygen ions (NOI), are natural components of atmospheric air. They are produced by certain natural phenomena. Negative ions are also called "air vitamins" and are an important factor in assessing air quality. Negative oxygen ions can directly decompose pollutants such as formaldehyde and toluene into non-toxic and odorless carbon dioxide and water, alleviate indoor pollution, and have a significant impact on air purification. In addition, medical research shows that negative oxygen ions increase the oxygen content in the blood, which is beneficial to the transportation, absorption and utilization of blood oxygen, and have the effects of promoting human metabolism, improving human immunity, enhancing human muscle power, and regulating the balance of body functions.
[0003] In space, air quality becomes a key issue due to the closed environment and lack of natural ventilation. The coating designed by the present invention can continuously release negative oxygen ions in the space environment through a special formula, effectively purify the air, remove odors, and inhibit bacterial growth, thereby improving the living environment of astronauts. This coating not only improves the quality of life in space, but also provides important guarantees for future long-term manned space missions.
[0004] Tourmaline is the general term for tourmaline minerals. It has a complex chemical composition and is a ring-structured silicate mineral of aluminum, sodium, iron, magnesium, and lithium characterized by boron. Tourmaline has unique properties such as piezoelectricity, pyroelectricity, conductivity, far-infrared radiation, and release of negative ions. It can be compounded with other materials by physical or chemical methods to produce a variety of functional materials. It is used in environmental protection, electronics, medicine, chemical industry, light industry, building materials and other fields. However, the properties of tourmaline materials are not prominent enough. For example, the release of negative oxygen ions is very low, making it difficult to achieve effective air purification. Summary of the invention
[0005] The object of the present invention is to provide a space aerospace compound to solve the problems raised in the background technology.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] A space aerospace compound comprises the following components in parts by weight: 95-105 parts of deionized water, 35-55 parts of tourmaline nanofiber composite material, 10-25 parts of rare earth oxide, 88-98 parts of polyvinyl alcohol, 0.1-0.5 parts of nano fullerene, 0.5-1 parts of defoaming agent and 0.5-1 parts of surfactant.
[0008] Further: The preparation method of the tourmaline nanofiber composite material is:
[0009] S1. Dispersing a mixture of graphene and tourmaline powder in water, transferring the dispersion into a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heating at 453 K for 10 h, naturally cooling, collecting the precipitate by centrifugation, washing it alternately with deionized water and ethanol several times, and then drying it in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline powder;
[0010] S2, mixing the prepared graphene / tourmaline powder with tetrabutyl titanate and dispersing them in water, transferring the aqueous solution into a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heating at 453 K for 10 h, naturally cooling, collecting the precipitate by centrifugation, washing it alternately with deionized water and ethanol several times, and then drying it in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline / titanium dioxide powder;
[0011] S3. Add graphene / tourmaline / titanium dioxide powder and DMF into a glass bottle and stir vigorously with a magnetic stirrer. Then ultrasonically disperse the mixture for 1 hour. Finally, add polyvinyl butyral powder to the graphene / tourmaline / titanium dioxide powder / DMF dispersion and stir. Use an electrospinning device to suck the polymer solution into a plastic syringe and clamp it on a support frame. Use a metal needle to extrude a uniform solution and apply voltage to the tip of the needle to obtain a tourmaline nanofiber composite material.
[0012] It should be noted that: graphene wraps tourmaline and is attached to the fiber structure formed by the polymer together with titanium dioxide. Graphene can improve the dispersibility of tourmaline in the fiber structure and improve the ability of tourmaline to release negative oxygen ions. The high conductivity and high electron mobility of graphene itself can also improve the negative oxygen ion release performance of tourmaline. In addition, the presence of a large number of hydroxyl structures in the polyvinyl butyral fiber matrix can promote the release of negative oxygen ions. The interaction between it and titanium dioxide makes the spatial position of titanium dioxide and the graphene and tourmaline on the fiber structure close. Titanium dioxide can increase the potential difference between tourmaline crystals and further promote the release of negative oxygen ions. The interaction between graphene and titanium dioxide can increase the valence band height of TiO2, narrow its bandgap width, increase the visible light absorption efficiency, improve the electron conduction efficiency, and further increase the release of negative oxygen ions.
[0013] Furthermore: in step S1, the usage ratio of graphene, tourmaline and water is 30-50 mg: 300-500 mg: 25-50 mL.
[0014] Furthermore, in step S2, the usage ratio of graphene / tourmaline powder, tetrabutyl titanate and water is 300-500 mg: 1-2 mL: 25-50 mL.
[0015] Further: in step S3, the usage ratio of graphene / tourmaline / titanium dioxide powder, DMF and polyvinyl butyral powder is 100-200 mg: 10-15 mL: 200-400 mg.
[0016] Furthermore: in step S3, the injection speed of the metal needle to squeeze the uniform solution is 0.5-1 mL / h, and the DC voltage applied to the tip of the needle is 30-35 kV.
[0017] Further: the rare earth oxide is lanthanum oxide, cerium oxide or praseodymium oxide.
[0018] Furthermore: the defoaming agent is a silicone oil defoaming agent.
[0019] Further: the surfactant is sodium dodecylbenzene sulfonate or sodium laurate sulfonate.
[0020] Compared with the prior art, the present invention has the following beneficial effects:
[0021] (1) Graphene has a strong electron migration ability. When the surface of tourmaline crystal releases charges, graphene will cause these charges to move within a certain range, so that more electrons and holes are generated on the surface of tourmaline crystal, which is equivalent to increasing the amount of charge on the surface of tourmaline crystal, increasing the strength of the electrostatic field, and promoting the electrolysis of more neutral molecules, thereby increasing the number of negative ions;
[0022] (2) Titanium dioxide interacts with the hydroxyl structure in the polymer fiber matrix, which promotes the dispersion of titanium dioxide in the fiber structure and makes it very close to tourmaline and graphene in space. The unbonded π electrons on the surface of carbon atoms in graphene will bond with the free electrons on the surface of titanium dioxide to form Ti-OC bonds, thereby increasing the valence band height of TiO2, reducing its bandgap width, increasing visible light absorption efficiency, improving electron conduction efficiency, and further increasing the release of negative oxygen ions;
[0023] (3) The combination of fullerene and tourmaline can release small-particle negative oxygen ions with high concentration and strong activity. Rare earth oxides and titanium dioxide can activate electrons in the electric field on the surface of tourmaline, promote electron migration, and improve the ionization efficiency of water molecules.
[0024] (4) The fiber structure can increase the potential difference on the surface of tourmaline crystals, thereby enhancing the performance of tourmaline in releasing negative oxygen ions. The synergistic effect between tourmaline, graphene and titanium dioxide in the fiber structure greatly improves the ability of the composite material to release negative oxygen ions, which is reflected in the corresponding improvement of the air purification ability of the composite material, thereby improving the living environment of astronauts. DETAILED DESCRIPTION
[0025] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0026] The present invention provides a technical solution: a space aerospace health compound.
[0027] Preparation of tourmaline nanofiber composites:
[0028] S1. A mixture of 50 mg of graphene and 500 mg of tourmaline powder was dispersed in water, and the dispersion was transferred to a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heated at 453 K for 10 h, and after natural cooling, the precipitate was collected by centrifugation, washed alternately with deionized water and ethanol several times, and then dried in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline powder;
[0029] S2, 300 mg of the prepared graphene / tourmaline powder was mixed with 1.28 mL of tetrabutyl titanate and dispersed in water, and the aqueous solution was transferred to a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heated at 453 K for 10 h, and after natural cooling, the precipitate was collected by centrifugation, washed alternately with deionized water and ethanol several times, and then dried in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline / titanium dioxide powder;
[0030] S3. Add 200 mg of graphene / tourmaline / titanium dioxide powder and 10 mL of DMF into a glass bottle and stir vigorously with a magnetic stirrer. Then, ultrasonically disperse the mixture for 1 h. Finally, add 400 mg of polyvinyl butyral powder into the graphene / tourmaline / titanium dioxide powder / DMF dispersion and stir. Use an electrospinning device to suck the polymer solution into a plastic syringe and clamp it on a support frame. Use a metal needle to extrude a uniform solution at an injection rate of 0.5 mL / h. At the same time, apply a DC voltage of 30-5 kV to the tip of the needle to obtain a tourmaline nanofiber composite material.
[0031] Preparation of tourmaline nanocomposites:
[0032] S1. A mixture of 50 mg of graphene and 500 mg of tourmaline powder was dispersed in water, and the dispersion was transferred to a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heated at 453 K for 10 h, and after natural cooling, the precipitate was collected by centrifugation, washed alternately with deionized water and ethanol several times, and then dried in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline powder;
[0033] S2, 300 mg of the prepared graphene / tourmaline powder was mixed with 1.28 mL of tetrabutyl titanate and dispersed in water, the aqueous solution was transferred to a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heated at 453 K for 10 h, and after natural cooling, the precipitate was collected by centrifugation, washed alternately with deionized water and ethanol several times, and then dried in a vacuum oven at 343 K for 4 h to obtain a tourmaline nanocomposite material;
[0034] Preparation of graphene / tourmaline composites:
[0035] A mixture of 50 mg of graphene and 500 mg of tourmaline powder was dispersed in water, and the dispersion was transferred to a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heated at 453 K for 10 h, and after natural cooling, the precipitate was collected by centrifugation, washed alternately with deionized water and ethanol several times, and then dried in a vacuum oven at 343 K for 4 h to obtain a graphene / tourmaline composite material;
[0036] Preparation of titanium dioxide / tourmaline composites:
[0037] 300 mg of tourmaline powder was mixed with 1.28 mL of tetrabutyl titanate and dispersed in water. The aqueous solution was transferred to a 50 mL polytetrafluoroethylene-lined stainless steel autoclave and heated at 453 K for 10 h. After natural cooling, the precipitate was collected by centrifugation, washed alternately with deionized water and ethanol several times, and then dried in a vacuum oven at 343 K for 4 h to obtain a titanium dioxide / tourmaline composite material.
[0038] Example 1
[0039] A space aerospace compound comprises the following components in parts by weight:
[0040]
[0041]
[0042] Example 2
[0043] A space aerospace compound comprises the following components in parts by weight:
[0044] Components Weight parts Deionized water 100 Tourmaline nanofiber composites 40 Cerium Oxide 12 Polyvinyl alcohol 90 Sodium laurate sulfonate 1 Defoaming agent 0.5 Nanofullerene 0.2
[0045] Example 3
[0046] A space aerospace compound comprises the following components in parts by weight:
[0047]
[0048]
[0049] Example 4
[0050] A space aerospace compound comprises the following components in parts by weight:
[0051] Components Weight parts Deionized water 105 Tourmaline nanofiber composites 38 Praseodymium oxide 14 Polyvinyl alcohol 91 Sodium laurate sulfonate 0.5 Defoaming agent 1 Nanofullerene 0.5
[0052] Comparative Example 1
[0053] A space aerospace compound comprises the following components in parts by weight:
[0054] Components Weight parts Deionized water 105 Graphene / Tourmaline Composites 38 Praseodymium oxide 14 Polyvinyl alcohol 91 Sodium laurate sulfonate 0.5 Defoaming agent 1 Nanofullerene 0.5
[0055] Comparative Example 2
[0056] A space aerospace compound comprises the following components in parts by weight:
[0057] Components Weight parts Deionized water 105 Titanium dioxide / tourmaline composites 38 Praseodymium oxide 14 Polyvinyl alcohol 91 Sodium laurate sulfonate 0.5 Defoaming agent 1 Nanofullerene 0.5
[0058] Comparative Example 3
[0059] A space aerospace compound comprises the following components in parts by weight:
[0060] Components Weight parts Deionized water 105 Tourmaline Nanocomposite Materials 38 Praseodymium oxide 14 Polyvinyl alcohol 91 Sodium laurate sulfonate 0.5 Defoaming agent 1 Nanofullerene 0.5
[0061] Comparative Example 4
[0062] A space aerospace compound comprises the following components in parts by weight:
[0063]
[0064]
[0065] Test experiments were carried out on each embodiment and comparative example: using a WST-05A negative ion air detector, the effective measurement range of negative ions is 0-5 million / cm. In order to minimize the impact of environmental factors on the experimental results, a sealed glass container with a volume of 15 liters was used in the experiment. The specific experimental method is as follows: 1 gram of the prepared material is weighed and flattened in a glass container. After that, the amount of negative oxygen ions released is observed, and the data is recorded every 5 minutes.
[0066] Table 1 Negative oxygen ion release amount of the embodiment and the comparative example
[0067] sample <![CDATA[NAI(ions / cm 3 )]]> Example 1 6500 Example 2 6700 Example 3 6400 Example 4 6800 Comparative Example 1 5000 Comparative Example 2 5200 Comparative Example 3 5400 Comparative Example 4 2500
[0068] From the data in the analysis table, it can be seen that the synergistic effect between titanium dioxide, graphene and tourmaline in the polymer fiber matrix of the embodiment can greatly enhance the ability of tourmaline to release negative oxygen ions and improve the performance of the composite material in purifying the air. In the comparative example, there is only one or two promoting effects, and there is no polymer fiber matrix. Tourmaline, graphene and titanium dioxide do not have good dispersibility, and have little promoting effect on the release of negative oxygen ions by tourmaline.
[0069] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A space aerospace compound, characterized in that: The invention comprises the following components in parts by weight: 95-105 parts of deionized water, 35-55 parts of tourmaline nanofiber composite material, 10-25 parts of rare earth oxide, 88-98 parts of polyvinyl alcohol, 0.1-0.5 parts of nano fullerene, 0.5-1 parts of defoaming agent and 0.5-1 parts of surfactant.
2. A space aerospace compound according to claim 1, characterized in that: The preparation method of the tourmaline nanofiber composite material is: S1. Dispersing a mixture of graphene and tourmaline powder in water, transferring the dispersion into a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heating at 453 K for 10 h, naturally cooling, collecting the precipitate by centrifugation, washing it alternately with deionized water and ethanol several times, and then drying it in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline powder; S2, mixing the prepared graphene / tourmaline powder with tetrabutyl titanate and dispersing them in water, transferring the aqueous solution into a 50 mL polytetrafluoroethylene-lined stainless steel autoclave, heating at 453 K for 10 h, naturally cooling, collecting the precipitate by centrifugation, washing it alternately with deionized water and ethanol several times, and then drying it in a vacuum oven at 343 K for 4 h to obtain graphene / tourmaline / titanium dioxide powder; S3. Add graphene / tourmaline / titanium dioxide powder and DMF into a glass bottle and stir vigorously with a magnetic stirrer. Then ultrasonically disperse the mixture for 1 hour. Finally, add polyvinyl butyral powder to the graphene / tourmaline / titanium dioxide powder / DMF dispersion and stir. Use an electrospinning device to suck the polymer solution into a plastic syringe and clamp it on a support frame. Use a metal needle to extrude a uniform solution and apply voltage to the tip of the needle to obtain a tourmaline nanofiber composite material.
3. A space aerospace compound according to claim 2, characterized in that: In the step S1, the usage ratio of graphene, tourmaline and water is 30-50 mg: 300-500 mg: 25-50 mL.
4. The space aerospace compound according to claim 2, characterized in that: In the step S2, the usage ratio of graphene / tourmaline powder, tetrabutyl titanate and water is 300-500 mg: 1-2 mL: 25-50 mL.
5. The space aerospace compound according to claim 2, characterized in that: In the step S3, the usage ratio of graphene / tourmaline / titanium dioxide powder, DMF and polyvinyl butyral powder is 100-200 mg: 10-15 mL: 200-400 mg.
6. The space aerospace compound according to claim 2, characterized in that: In step S3, the injection speed of the metal needle squeezing the uniform solution is 0.5-1 mL / h, and the DC voltage applied to the tip of the needle is 30-35 kV.
7. The space aerospace compound according to claim 1, characterized in that: The rare earth oxide is lanthanum oxide, cerium oxide or praseodymium oxide.
8. The space aerospace compound according to claim 1, characterized in that: The defoaming agent is a silicone oil defoaming agent.
9. The space aerospace compound according to claim 1, characterized in that: The surfactant is sodium dodecylbenzene sulfonate or sodium laurate sulfonate.