Shield synchronous grouting method based on fluid solidified soil
By using a combination technology of fluid solidified soil and fast-condensing slurry in shield grouting, the problems of high shrinkage and high cost of traditional shield grouting fluid are solved, and the effects of low leakage and premature strength are achieved, which improves the effect of Water stop performance and construction efficiency of the tunnel.
Patent Information
- Application Number
- CN202411188693.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-12
AI Technical Summary
The shrinkage rate of traditional shield grouting liquid is high and cannot effectively block water, resulting in serious water leakage in the tunnel and high cost.
The shield structure synchronous grouting method based on fluid solidified soil is adopted to form a cementitious structure by adding curing agents (cement, sodium sulfate and calcium carbonate) to the mud, and secondary supplementation is carried out in combination with quick-set shield structure single or double slurry Grouting delays cement settling time and increases cementation rate, reduces shrinkage, and enhances fluidity to fill gaps.
It achieves low leakage and early strength effects, improves the water stop performance of the tunnel, reduces the risk of leakage, and reduces construction costs.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of shield synchronous grouting, and more specifically to a shield synchronous grouting method based on fluidized solidified soil. Background Art
[0002] Shield construction is a modern technology used for tunnel excavation, which is very common in the development of urban underground space. This method uses a large mechanical equipment called a tunnel boring machine (TBM) to carry out continuous tunnel excavation operations. During shield construction, as the shield machine moves forward, when the segment is separated from the shield tail, a circular gap with a width of about 140 mm will be formed between the soil and the segment. If this gap is not filled in time, the soil around the segment will loosen or even collapse, leading to adverse consequences such as surface settlement. For this reason, grouting must be used to fill the gap in the shield tail building in time. At the same time, backing grouting can also improve the water-stopping performance of the tunnel, so that the external force on the segment can be evenly distributed, ensuring the early stability of the segment lining.
[0003] The biggest disadvantage of the traditional shield grouting used in single shield slurry and double shield slurry is their high shrinkage rate. The shrinkage rate of single shield slurry after hardening is more than 30%, and the shrinkage rate of double shield slurry after hardening is more than 20%. As a result, the shield grouting cannot form hydraulic effect on the surrounding rock and cannot achieve water blocking function, which ultimately causes obvious water leakage in the tunnel and the high cost of shield materials.
[0004] As a new type of filling engineering material, fluidized solidified soil has demonstrated good construction and mechanical properties through the transformation and development of traditional stabilized soil (such as lime soil). This material has strong fluidity before solidification, and has certain strength, low permeability and water stability after solidification. It can maintain long-term stability and has low-carbon and environmentally friendly functions. Summary of the invention
[0005] In order to apply fluidized solidified soil to shield synchronous grouting, the present invention provides a shield synchronous grouting method based on fluidized solidified soil.
[0006] The technical solution of the present invention is as follows:
[0007] A shield synchronous grouting method based on fluidized solidified soil includes synchronous grouting and secondary supplementary grouting. The synchronous grouting injects shield synchronous grouting slurry through the shield grouting system while excavating. The secondary supplementary grouting injects shield supplementary grouting slurry through the grouting holes of the pipe segment behind the shield tail through the supplementary grouting system.
[0008] The shield synchronous grouting slurry is fluidized solidified soil, which consists of mud and curing agent.
[0009] The shield supplementary grouting slurry is shield single slurry or shield double slurry. The shield single slurry is pure cement slurry, and the shield double slurry is a mixed slurry of cement and water glass. The water content of the shield supplementary grouting slurry is greater than 50%.
[0010] Fluidized solidified soil is made by adding a curing agent (a mixture of cement, sodium sulfate and calcium carbonate) to the mud in advance, so that the curing agent and the soil particles in the mud undergo a preliminary hydration reaction, forming a certain degree of bonding and forming a bonding structure centered on the cement hydration product. After the secondary supplementary grouting, the use of quick-setting slurry (shield single slurry or shield double slurry) can further accelerate the curing process, thereby increasing the bonding rate of cement hydration products in the soil, ensuring rapid and stable structure, achieving early strength effect, and quickly forming a supporting force system. (Since cement plays a major role in the curing process of fluidized solidified soil, and the bonding effect of cement in the soil is relatively slow compared to itself or in shield single slurry or shield double slurry, the early strength effect of fluidized solidified soil is poor, so quick-setting slurry is used for supplementation to increase the hydration reaction rate of cement and highlight the early strength effect.)
[0011] The curing agent of fluidized solidified soil contains sodium sulfate, which can play a retarding role in the cement system. Sodium sulfate can react with certain hydration products in cement, such as calcium hydroxide (Ca(OH)2) to generate calcium sulfate (CaSO4·2H2O). This process is relatively slow, so it can delay the setting time of cement. The sodium sulfate in the curing agent delays the setting time of cement in the curing agent, ensuring that the shield synchronous grouting slurry can still flow when injected behind the segment. The injection of shield supplementary grouting slurry, due to its high water content, improves the fluidity of the slurry behind the shield segment, further prolonging the flow time of the slurry. The calcium sulfate generated in advance by the fluidized solidified soil can also delay the hydration reaction of cement in the shield supplementary grouting slurry, ensuring that the slurry has enough time to fully flow and fill all the gaps behind the segment, including filling complex or narrow gaps.
[0012] Due to its own high fluidity, the shield supplementary grouting slurry brings its own cement hydration products into the fluidized solidified soil. From a microscopic perspective, although the fluidized solidified soil has a low shrinkage rate, the subsequent cement hydration products can well fill the pores in the cementing structure formed by the fluidized solidified soil (the filling uniformity is relatively good under the action of the calcium carbonate of the curing agent), reducing the porosity and pore size of the fluidized solidified soil after solidification. In addition, the high water content of the shield supplementary grouting slurry can reduce the shrinkage of the slurry behind the shield segment during the hardening process, thereby reducing the shrinkage rate, which is beneficial to reduce the occurrence of water leakage in the shield segment.
[0013] The above-mentioned shield synchronous grouting method based on fluidized solidified soil, the shield grouting system includes
[0014] The conveying pipeline is made from the slurry station, passes through the shaft where the shield construction is located, and ends below the shield construction shaft. Through the conveying pipeline, the shield grouting slurry in the slurry station is transported to the shield construction site.
[0015] The transport equipment receives the shield grouting slurry transported by the conveying pipeline below the shield construction shaft, and transports the shield grouting slurry to the vicinity of the shield machine.
[0016] The slurry storage tank is set up near the location of the shield machine. It is used to receive and store the shield grouting slurry transported to the shield construction site by the self-made slurry station. The shield grouting slurry is transported to the vicinity of the slurry storage tank by the transportation equipment, and the slurry pump is used to transport the shield grouting slurry in the transportation equipment to the slurry storage tank.
[0017] The grouting machine is connected to the slurry storage tank and injects the shield grouting slurry into the gap behind the shield segments through the grouting pipe.
[0018] Furthermore, several transport equipments are arranged to receive the shield grouting slurry under the conveying pipeline in turn, and after the slurry pump transports the shield grouting slurry to the slurry storage tank, the shield slag is loaded and transported to the bottom of the vertical shaft where the shield construction is located.
[0019] The above-mentioned shield synchronous grouting method based on fluidized solidified soil is characterized in that N+T grouting holes are set on the shield segment. During the synchronous grouting process, the shield grouting system uses N+T grouting holes to inject shield synchronous grouting slurry into the gap behind the shield segment. During the secondary supplementary grouting process, the shield grouting system uses N grouting holes to inject supplementary grouting slurry into the gap behind the shield segment.
[0020] Compared with the supplementary grouting slurry with increased fluidity, the shield synchronous grouting slurry has a high specific gravity and high viscosity, which may cause the shield synchronous grouting to be not smooth, affecting the efficiency of the shield synchronous grouting. But in fact, since the shield synchronous grouting slurry of the present invention has an obvious retarding effect, the fluidity has a greater impact on the shield synchronous grouting relative to its high specific gravity, and the grouting machine of the shield synchronous grouting can, in principle, pump and grout any slurry that can flow. Therefore, the shield synchronous grouting slurry of the present invention does not have as much impact on the efficiency of the shield synchronous grouting as imagined. In order to maintain the speed of synchronous grouting, one or more grouting holes (N and T are both positive integers) can be added when necessary to improve the efficiency of the shield synchronous grouting.
[0021] In the above-mentioned shield synchronous grouting method based on fluidized solidified soil, the synchronous grouting speed should be equal to the shield machine excavation speed.
[0022] In the above-mentioned shield synchronous grouting method based on fluidized solidified soil, the amount of curing agent added to the fluidized solidified soil is: 150-200 kg of curing agent per ton of mud.
[0023] In the above-mentioned shield synchronous grouting method based on fluidized solidified soil, the components of the curing agent include cement, sodium sulfate and calcium carbonate, and the mass mix ratio of cement, sodium sulfate and calcium carbonate is: cement: sodium sulfate: calcium carbonate = 8:1:1.
[0024] The above-mentioned shield synchronous grouting method based on fluidized solidified soil has a retarding time standard of 18-24h for the shield synchronous grouting slurry, a strength standard of 0.1-0.3MPa 1d after final setting, and a strength standard of greater than or equal to 2.0MPa at 28d.
[0025] The above-mentioned shield synchronous grouting method based on fluidized solidified soil has a shrinkage rate standard of less than 1%, a permeability standard of less than 8-10cm / s, a viscosity standard of greater than 50s, and a specific gravity standard of greater than or equal to 1.5g / cm 3 .
[0026] In the above-mentioned shield synchronous grouting method based on fluidized solidified soil, the water-cement ratio of the shield single slurry is 1:1-1.5:1.
[0027] The present invention according to the above scheme has the beneficial effect that:
[0028] The shield grouting of the present invention is divided into two injections, one is the synchronous grouting using fluidized solidified soil, and the second is the supplementary grouting using shield single slurry or shield double slurry with high water content. On the one hand, the early strength property of shield single slurry or shield double slurry is used to improve the hydration reaction rate of the fluidized solidified soil of synchronous grouting, reflecting the early strength effect, and on the other hand, the fluidity is supplemented and the setting time of cement is delayed, so that the shield grouting slurry can fill and have sufficient time to fill the gap behind the shield segment, thereby improving the density, helping to improve the water-stopping performance of the tunnel, and reducing the infiltration of groundwater, thereby reducing the risk of tunnel leakage.
[0029] The fluidized solidified soil has extremely low shrinkage and water permeability, perfectly realizing the low leakage function of the shield section, and its strength also meets the requirements for optimizing the stress of the shield segment. At the same time, the fluidized solidified soil uses the slag at the construction site as the main building material, which enables the reduction of slag at the construction site. DETAILED DESCRIPTION
[0030] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0031] A shield synchronous grouting method based on fluidized solidified soil comprises synchronous grouting and secondary supplementary grouting, wherein the synchronous grouting injects shield synchronous grouting slurry as the tunneling progresses through a shield grouting system, and the secondary supplementary grouting injects shield supplementary grouting slurry through a segment grouting hole behind the shield tail through a supplementary grouting system, wherein the shield synchronous grouting slurry is fluidized solidified soil, the fluidized solidified soil comprises mud and a curing agent, the shield supplementary grouting slurry is shield single slurry or shield double slurry, the shield single slurry is pure cement slurry, and the shield double slurry is a mixed slurry of cement and water glass, and the water content of the shield supplementary grouting slurry is greater than 50%.
[0032] The shield synchronous grouting slurry is fluidized solidified soil. The components of the fluidized solidified soil include mud and solidifying agent. The amount of solidifying agent added to the fluidized solidified soil is: 150-200 kg of solidifying agent per ton of mud. The components of the solidifying agent include cement, sodium sulfate and calcium carbonate. The mass mix ratio of cement, sodium sulfate and calcium carbonate is: cement: sodium sulfate: calcium carbonate = 8:1:1.
[0033] Performance standard conditions for shield synchronous grouting slurry: The shrinkage standard of shield synchronous grouting slurry is less than 1%, the permeability standard is less than 8-10cm / s, the viscosity standard is greater than 50s, the specific gravity standard is greater than or equal to 1.5g / cm3, the retarding time standard is 18-24h, the strength standard of shield synchronous grouting slurry 1d after final setting is 0.1-0.3MPa, and the 28d strength standard is greater than or equal to 2.0MPa.
[0034] The shield grouting system of the present invention comprises a conveying pipeline, a transportation device, a slurry storage tank and a grouting machine.
[0035] The conveying pipeline is made from the slurry station, passes through the vertical shaft where the shield construction is located, and ends below the shield construction shaft. Through the conveying pipeline, the shield grouting slurry in the slurry station is transported along the conveying pipeline to the shield construction site.
[0036] The transport equipment receives the shield grouting slurry (including shield synchronous grouting slurry and supplementary grouting slurry) transported by the conveying pipeline below the shield construction shaft, and transports the shield grouting slurry to the vicinity of the shield machine. There are multiple transport equipments, which take turns to receive the shield grouting slurry below the conveying pipeline, and after the slurry pump transports the shield grouting slurry to the slurry storage tank, load the shield slag, and transport the shield slag to the bottom of the shield construction shaft.
[0037] The slurry storage tank is installed near the location of the shield machine. It is used to receive and store the shield grouting slurry transported to the shield construction site by the self-made slurry station. The shield grouting slurry is transported to the vicinity of the slurry storage tank by the transportation equipment, and the shield grouting slurry in the transportation equipment is transported to the slurry storage tank by the mud pump.
[0038] Grouting machine, which is connected to the slurry storage tank, injects the shield grouting slurry into the gap behind the shield segment through the grouting pipeline. The shield segment is provided with N+T grouting holes. During the synchronous grouting process, the shield grouting system uses N+T grouting holes to inject the shield synchronous grouting slurry into the gap behind the shield segment. During the secondary supplementary grouting process, the shield grouting system uses N grouting holes to inject supplementary grouting slurry into the gap behind the shield segment.
[0039] In this embodiment, the shield synchronous grouting slurry is slurried by the mortar mixing station (i.e., slurry making station) on the east side of the entrance of the site. After the mortar mixing station is slurried, it is connected to the bottom of the wellhead (the vertical shaft where the shield construction is located) through a conveying pipeline and injected into the battery car (i.e., transportation equipment). The loading capacity of a battery car is 15 cubic meters. After the battery car is full, it is transported to the shield machine, and the shield synchronous grouting slurry is pumped into the horizontal mud tank (i.e., slurry storage tank) by a mud pump. A grouting machine is equipped under the horizontal mud tank. During grouting, the slurry is injected into the upper edge of the shield segment through four pipes (i.e., grouting pipes). Start the grouting machine to inject the shield synchronous grouting slurry into the rear of the shield segment. The single grouting time is about two hours, the initial grouting pressure is 0.6bar-0.8bar, the synchronous grouting pressure is 2-3bar, and the pressure range during grouting basically fluctuates in the range of 2.0-2.8.
[0040] After the grouting is completed, the battery car needs to wait for the shield slag from the shield to be filled before it can go out to transport the shield synchronous grouting slurry again. The shield slag pulled out with the battery car is transported to the slag pool. The shield slag in the slag pool is excavated by the excavator and poured into the screening equipment for screening. The screened mud falls directly into the mud pool below the screening equipment. The mud pool is connected to two pipes to transport it to the mud cake filter press inside the site and the mud cake filter press outside the site for filtering the mud cake. The clean water after filtering has been extracted and stored in the clean water pool, and the mud cake is transported to the mortar mixing station to prepare the shield synchronous grouting slurry.
[0041] The mud cake is crushed by a pulverizer and falls into the mixing tank. Water is added to prepare mud with a specific gravity of 1.5, and the mud in the mixing tank is continuously stirred. The mud in the mixing tank is pumped to the mixing device by a mud pump. According to the amount of mud pumped to the mixing device, the curing agent is added in proportion and continuously stirred. The amount of curing agent per ton of mud is 150 kg. The components of the curing agent include cement, sodium sulfate and calcium carbonate. The mass ratio of cement, sodium sulfate and calcium carbonate is: cement: sodium sulfate: calcium carbonate = 8:1:1.
[0042] Embodiment 1: The total amount of fluidized solidified soil is 8888.89 kg, the total amount of curing agent is 1333 kg, the amount of cement (curing agent) is 1067 kg, the amount of sodium sulfate (curing agent) is 133 kg, and the amount of calcium carbonate (curing agent) is 133 kg.
[0043] Example 2: The total amount of fluidized solidified soil is 8947 kg, the total amount of curing agent is 1566 kg, the amount of cement (curing agent) is 1253 kg, the amount of sodium sulfate (curing agent) is 157 kg, and the amount of calcium carbonate (curing agent) is 157 kg.
[0044] Example 3: The total amount of fluidized solidified soil is 8333 kg, the total amount of curing agent is 1667 kg, the amount of cement (curing agent) is 1333 kg, the amount of sodium sulfate (curing agent) is 167 kg, and the amount of calcium carbonate (curing agent) is 167 kg.
[0045] After the shield synchronous grouting slurry for the last synchronous grouting is transported out of the mortar mixing station, the mortar mixing station prepares the shield supplementary grouting slurry. The shield supplementary grouting slurry is a shield single slurry or a shield double slurry. If the shield supplementary grouting slurry is a shield single slurry, the water-cement ratio of the shield single slurry is 1:1-1.5:1. In this embodiment, the water-cement ratio of the shield single slurry is 1.2:1; if the shield supplementary grouting slurry is a shield double slurry, in this embodiment, the proportion of the shield double slurry is cement: water: 10% water glass slurry = 1:0.6:1. After the shield supplementary grouting slurry is stirred evenly, it is also connected to the bottom of the wellhead through a pipeline, injected into the battery car, transported to the shield machine by the battery car, and finally injected into the rear of the shield segment through the grouting machine.
[0046] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A shield synchronous grouting method based on fluidized solidified soil, characterized in that: It includes synchronous grouting and secondary supplementary grouting. Synchronous grouting injects shield synchronous grouting slurry through the shield grouting system as the tunnel is advancing. Secondary supplementary grouting injects shield supplementary grouting slurry through the grouting holes of the pipe segment behind the shield tail through the supplementary grouting system. The shield synchronous grouting slurry is fluidized solidified soil, which consists of mud and curing agent. The shield supplementary grouting slurry is shield single slurry or shield double slurry. The shield single slurry is pure cement slurry, and the shield double slurry is a mixed slurry of cement and water glass. The water content of the shield supplementary grouting slurry is greater than 50%.
2. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The shield grouting system includes The conveying pipeline is made from the slurry station, passes through the shaft where the shield construction is located, and ends below the shield construction shaft. Through the conveying pipeline, the shield grouting slurry in the slurry station is transported to the shield construction site. The transport equipment receives the shield grouting slurry transported by the conveying pipeline below the shield construction shaft, and transports the shield grouting slurry to the vicinity of the shield machine. The slurry storage tank is set up near the location of the shield machine. It is used to receive and store the shield grouting slurry transported to the shield construction site by the self-made slurry station. The shield grouting slurry is transported to the vicinity of the slurry storage tank by the transportation equipment, and the slurry pump is used to transport the shield grouting slurry in the transportation equipment to the slurry storage tank. The grouting machine is connected to the slurry storage tank and injects the shield grouting slurry into the gap behind the shield segments through the grouting pipe.
3. A shield synchronous grouting method based on fluidized solidified soil according to claim 2, characterized in that: Several transport equipments are set up to receive the shield grouting slurry under the conveying pipeline in turn, and after the slurry pump transports the shield grouting slurry to the slurry storage tank, the shield slag is loaded and transported to the bottom of the vertical shaft where the shield construction is located.
4. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The shield segments are provided with N+T grouting holes. During the synchronous grouting process, the shield grouting system uses N+T grouting holes to inject shield synchronous grouting slurry into the gap behind the shield segments. During the secondary supplementary grouting process, the shield grouting system uses N grouting holes to inject supplementary grouting slurry into the gap behind the shield segments.
5. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The synchronous grouting speed should be equal to the shield machine excavation speed.
6. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The amount of curing agent added to the fluidized solidified soil is: 150-200 kg of curing agent per ton of mud.
7. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The components of the curing agent include cement, sodium sulfate and calcium carbonate. The mass ratio of cement, sodium sulfate and calcium carbonate is: cement: sodium sulfate: calcium carbonate = 8:1:
1.
8. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The retarding time standard of shield synchronous grouting slurry is 18-24h, the strength standard of shield synchronous grouting slurry 1d after final setting is 0.1-0.3MPa, and the strength standard of 28d is greater than or equal to 2.0MPa.
9. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The shrinkage standard of shield synchronous grouting slurry is less than 1%, the permeability standard is less than 8-10cm / s, the viscosity standard is greater than 50s, and the specific gravity standard is greater than or equal to 1.5g / cm 3 .
10. A shield synchronous grouting method based on fluidized solidified soil according to claim 1, characterized in that: The water-cement ratio of shield single slurry is 1:1-1.5:1.
Citation Information
Cited By
Novel grouting method applied to shield wall back grouting
CN119754783A