High-consistency MEMS pressure sensor and preparation method thereof

By adopting a dual Wheatstone bridge structure in the MEMS pressure sensor, and using a high-voltage resistance varistor for zero-point drift and thermal stress compensation, the zero-point drift in the mass production of MEMS piezoresistive pressure sensors in the prior art is solved. The problem has improved the stability and reliability of the chip.

CN118936694APending Publication Date: 2024-11-12SOUTHEAST UNIV
View PDF 0 Cites 4 Cited by

Patent Information

Application Number
CN202410989912.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In mass production of existing MEMS piezoresistive pressure sensors, due to process errors, the zero-point drift is inconsistent, affecting the stability and reliability between chips.

Method used

Using a dual Wheatstone bridge structure, one group of Wheatstone bridges are located on the four sides of the sensitive film and the other group is located on the outside of the sensitive film. The output voltage is subtracted to precompensate the zero-point drift deviation and is reduced by a high-voltage resistance coefficient varistor Thermal stress error improves chip consistency.

Benefits of technology

Precompensation for process random errors and thermal stress errors is achieved, the performance consistency of the chip during mass production is improved, the zero-point drift deviation of the sensor is reduced, and the stability and reliability of the product are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118936694A_ABST
    Figure CN118936694A_ABST
Patent Text Reader

Abstract

The invention discloses a high-consistency MEMS pressure sensor and a preparation method thereof, the high-consistency MEMS pressure sensor adopts a double-bridge structure integrating an in-film Wheatstone bridge and an out-film Wheatstone bridge, the in-film Wheatstone bridge is composed of four piezoresistors distributed at the central positions of four sides of a sensitive film; the out-of-film Wheatstone bridge is composed of four piezoresistors on the out-of-film silicon device layer, and the sizes of the corresponding piezoresistors of the inner and outer Wheatstone bridges are consistent; by subtracting the output voltage of the in-film Wheatstone bridge from the output voltage of the out-film Wheatstone bridge, the influence of resistance mismatch of the piezoresistor on zero output can be effectively reduced, so that pre-compensation of zero drift deviation caused by process random errors is realized, and the consistency performance of chips during batch production is improved. Besides, the preparation method of the high-consistency MEMS pressure sensor does not need additional process steps, is beneficial to improving integration of the sensor, and has the advantages of being simple in process, low in cost and easy to produce in batches.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a sensor and a method for preparing the same, and in particular to a MEMS pressure sensor and a method for preparing the same. Background Art

[0002] MEMS pressure sensor is a high-precision device for measuring pressure based on MEMS processing technology. Its core function is to use micromechanical structure to convert pressure signals that are difficult to measure and process into electrical signals that are easy to process and analyze. According to the different measurement mechanisms and structures, mainstream MEMS pressure sensors can be divided into five categories: piezoresistive pressure sensors, capacitive pressure sensors, resonant pressure sensors, piezoelectric pressure sensors and fiber optic pressure sensors. Among them, MEMS piezoresistive pressure sensors are widely used in the fields of automotive electronics, industrial robots, aerospace, medical health, as well as consumer electronics such as e-cigarettes and smart bracelets due to their simple structure, small size, good linearity, low processing difficulty and easy integration.

[0003] The current mainstream MEMS piezoresistive pressure sensor design adopts a single Wheatstone bridge structure, but under actual manufacturing conditions, due to factors such as photolithography process errors and diffusion process errors, there is a resistance mismatch between the four varistors prepared by the ion implantation process. In particular, due to the influence of temperature, time cycle, impurity concentration, mask arrangement and other environmental factors, the doping concentration of the varistor has errors between wafers, that is, inter-wafer errors; due to factors such as temperature gradient, uneven distribution of doping gas in the furnace, and mask errors, the doping concentration of the varistor has errors within the same wafer, that is, intra-wafer errors. And because the inter-wafer error and intra-wafer error are random, the traditional MEMS piezoresistive pressure sensor produces varistor initial resistance mismatch and zero drift. When batch processing is carried out, each sensor may present a different initial resistance mismatch result due to random process errors. This randomness significantly reduces the consistency of the zero drift of the entire batch of sensors.

[0004] At present, in order to achieve zero point compensation for a large number of pressure sensors, the usual practice is to first measure and calibrate a batch of sensors to obtain the average value of their zero drift, and then apply the zero drift constant to the zero point compensation of the entire batch of sensors. However, due to the existence of mismatch random errors, this direct compensation method will significantly affect the consistency between chips, resulting in a large error after compensation. Therefore, there is an urgent need for a method to pre-compensate chip consistency to ensure the stability and reliability of the final product. Summary of the invention

[0005] Purpose of the invention: In view of the above-mentioned prior art, a high-consistency MEMS pressure sensor and a preparation method thereof are proposed, which can improve the performance consistency of chips between wafers and chips within a wafer during mass production.

[0006] Technical solution: A high-consistency MEMS pressure sensor, comprising a silicon substrate layer, a cavity is arranged at the central position of the upper surface of the silicon substrate layer, an oxide layer is arranged on the silicon substrate layer, a silicon device layer is arranged on the oxide layer, wherein the silicon device layer portion located directly above the cavity forms a sensitive film; eight varistors are arranged on the upper surface of the silicon device layer, wherein four varistors are respectively located at the center positions of the four sides of the sensitive film, and the other four varistors are respectively located outside the sensitive film area, and both ends of each varistor are respectively provided with a plurality of electrodes for forming an ohmic contact and an electrical A heavily doped region connected to the silicon device layer; an intermediate layer is arranged on the silicon device layer, and a metal lead is arranged on the intermediate layer, and the four varistors relatively located on the inner side are connected to the metal lead through the heavily doped region to form a first Wheatstone bridge; the four varistors relatively located on the outer side are connected to the metal lead through the heavily doped region to form a second Wheatstone bridge; a protective layer is arranged on the intermediate layer and the metal lead; wherein the varistors constituting the first Wheatstone bridge have a high voltage resistance coefficient, and the output voltage of the first Wheatstone bridge is subtracted from the output voltage of the second Wheatstone bridge as the output of the pressure sensor.

[0007] Furthermore, the first Wheatstone bridge uses four varistors with a

[110] crystal orientation, and the second Wheatstone bridge uses four varistors with a

[100] crystal orientation, and the sizes of the varistors are the same.

[0008] Furthermore, the first Wheatstone bridge uses four

[110] varistor crystal orientations, and the second Wheatstone bridge uses four The varistors have the same crystal orientation and the sizes of the varistors are the same.

[0009] Furthermore, the first Wheatstone bridge uses four

[110] varistors, the second Wheatstone bridge uses four

[110] varistors, and the sizes of the varistors are consistent.

[0010] Furthermore, a through hole connecting the cavity with the outside of the sensor is provided on the silicon substrate layer to form a differential pressure MEMS pressure sensor.

[0011] A method for preparing the high-consistency MEMS pressure sensor comprises:

[0012] S1: Select two single crystal silicon wafers as silicon substrate layer and silicon device layer respectively;

[0013] S2: forming an oxide layer on the surface of the silicon substrate layer by a thermal oxidation process, and then forming a cavity of a desired size on the front side of the silicon substrate layer by a bulk silicon etching process;

[0014] S3: bonding the silicon substrate layer with the cavity etched therein to the silicon device layer under vacuum conditions to form a sealed cavity, and then thinning the bonded silicon device layer to the thickness of the sensitive film;

[0015] S4: implanting boron ions into a local area of ​​the silicon device layer to produce various varistors and heavily doped areas;

[0016] S5: depositing a layer of silicon oxide on the upper surface of the silicon device layer by using an LPCVD process to form the intermediate layer;

[0017] S6: performing photolithography on the interposer to form contact holes connected to the heavily doped regions; and then performing photolithography and magnetron sputtering on the interposer to form the metal leads;

[0018] S7: Depositing a protective layer on the upper surface of the interposer by using an LPCVD process;

[0019] S8: performing photolithography on the surface of the protective layer to expose the metal pad.

[0020] Beneficial effects: 1. The high-consistency MEMS pressure sensor of the present invention adopts a dual Wheatstone bridge structure. The two groups of Wheatstone bridges are located on the upper surface of the silicon device layer, one group is located at the center of the four sides of the sensitive film, and the other group is located outside the sensitive film area. By subtracting the output voltage of the first Wheatstone bridge sensitive to pressure on the sensitive film and the second Wheatstone bridge used for compensation outside the sensitive film, pre-compensation for the zero drift deviation caused by random process errors is achieved, which helps to improve the consistency performance of the chip during mass production.

[0021] 2. When a varistor with a high resistivity is used to form a second Wheatstone bridge outside the sensitive film for compensation, the second Wheatstone bridge outside the film can output the thermal stress error caused by the mismatch of the thermal expansion coefficient. The output voltage of the first Wheatstone bridge is subtracted from the output voltage of the second Wheatstone bridge to reduce the influence of the thermal stress error and play a role in temperature compensation.

[0022] 3. The high-consistency MEMS pressure sensor and its preparation method of the present invention do not require additional process steps, which is conducive to improving the integration of the sensor and has the advantages of simple process, low cost and easy mass production. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a schematic diagram of a double Wheatstone bridge arrangement of a high consistency MEMS pressure sensor according to Example 1 of the present invention;

[0024] Figure 2 A schematic diagram of the connection of a double Wheatstone bridge structure of a high consistency MEMS pressure sensor of the present invention;

[0025] Figure 3 This is a schematic diagram of a double Wheatstone bridge arrangement of a high consistency MEMS pressure sensor according to Example 2 of the present invention;

[0026] Figure 4 This is a schematic diagram of a double Wheatstone bridge arrangement of a high consistency MEMS pressure sensor according to Example 3 of the present invention;

[0027] Figure 5 It is a schematic diagram of the cross-sectional structure along the A-A' direction of the high consistency MEMS pressure sensor of Example 3 of the present invention;

[0028] Figure 6 It is a structural schematic diagram corresponding to step 1 of preparing a high-consistency MEMS pressure sensor of the present invention;

[0029] Figure 7 It is a structural schematic diagram corresponding to step 2 of preparing the high consistency MEMS pressure sensor of the present invention;

[0030] Figure 8 It is a structural schematic diagram corresponding to step 3 of preparing the high-consistency MEMS pressure sensor of the present invention;

[0031] Fig. 9 It is a structural schematic diagram corresponding to step 4 of preparing the high-consistency MEMS pressure sensor of the present invention;

[0032] Fig.10 It is a structural schematic diagram corresponding to step 5 of preparing the high-consistency MEMS pressure sensor of the present invention;

[0033] Fig.11 It is a structural schematic diagram corresponding to step 6 of preparing the high-consistency MEMS pressure sensor of the present invention. DETAILED DESCRIPTION

[0034] The present invention will be further explained below in conjunction with the accompanying drawings.

[0035] Embodiment 1:

[0036] A high consistency MEMS pressure sensor includes a silicon substrate layer 1, a cavity 4 is arranged at the central position of the upper surface of the silicon substrate layer 1, an oxide layer 3 is arranged on the silicon substrate layer 1, and a silicon device layer 2 is arranged on the oxide layer 3, wherein the portion of the silicon device layer 2 located directly above the cavity 4 forms a sensitive film 5. Eight varistors 6 are arranged on the upper surface of the silicon device layer 2, wherein four varistors 6 are respectively located at the central positions of the four sides of the sensitive film 5, and the other four varistors 6 are respectively located in the outer area of ​​the sensitive film 5, and the two ends of each varistor 6 are respectively provided with a heavily doped region 7 for forming an ohmic contact and an electrical connection. An intermediate layer 8 and a metal lead 9 are arranged on the silicon device layer 2. The four varistors 6 located relatively on the inner side are connected to the metal lead 9 through the heavily doped region 7 to form a first Wheatstone bridge 11; the four varistors 6 located relatively on the outer side are connected to the metal lead 9 through the heavily doped region 7 to form a second Wheatstone bridge 12. The power input and ground terminals of the first Wheatstone bridge 11 and the second Wheatstone bridge 12 are respectively connected in parallel through the metal lead 9. A protective layer 10 and a metal pad connected to the Wheatstone bridge are arranged on the intermediate layer 8 and the metal lead 9. Among them, the varistor 6 constituting the first Wheatstone bridge 11 has a high voltage resistance coefficient, and the output voltage of the first Wheatstone bridge 11 and the second Wheatstone bridge 12 is subtracted as the output of the pressure sensor, such as Figure 2 shown.

[0037] like Figure 1 As shown, in this embodiment, the first Wheatstone bridge 11 uses four

[110] piezoresistors 6, which are R11, R12, R13, and R14, respectively, and are located at the center of the four sides of the sensitive film 5, respectively, to form an intra-film Wheatstone bridge that is sensitive to pressure. The second Wheatstone bridge 12 uses four

[100] piezoresistors 6, which are R21, R22, R23, and R24, respectively, and are located on the upper surface of the silicon device layer 2 outside the sensitive film 5, respectively, to form an extra-film Wheatstone bridge used for compensation. Among them, the sizes of the eight piezoresistors 6 are all the same. Since the first Wheatstone bridge 11 and the second Wheatstone bridge 12 use two types of piezoresistors 6, which are

[110] and

[100] piezoresistors 6, respectively, a 45° angle is formed between the two types of piezoresistors 6.

[0038] The working principle of the high consistency MEMS pressure sensor of this embodiment is as follows:

[0039] The

[110] crystal orientation varistor 6 constituting the first Wheatstone bridge 11 has a high voltage resistivity and is used to sense changes in pressure on the sensitive film 5; the

[100] crystal orientation varistor 6 constituting the second Wheatstone bridge 12 has a low voltage resistivity and is insensitive to stress fields; the eight varistors 6 of the two Wheatstone bridges have the same size, so the resistance mismatch and zero-point drift of the varistors 6 of the first Wheatstone bridge 11 and the second Wheatstone bridge 12 caused by random process errors are basically the same. By subtracting the output voltages of the first Wheatstone bridge 11 from the second Wheatstone bridge 12, the zero-point output of the chip is pre-compensated, which reduces the impact of process errors on the zero-point drift deviation of the device and improves the consistency performance of mass production.

[0040] Embodiment 2:

[0041] The only difference from Example 1 is that the first Wheatstone bridge 11 uses four

[110] varistor 6, and the second Wheatstone bridge 12 uses four Crystal orientation of the varistor 6.

[0042] Since the first Wheatstone bridge 11 and the second Wheatstone bridge 12 respectively adopt the

[110] crystal orientation and The two crystal orientations of the varistors 6 form a 90° angle between the two crystal orientations of the varistors 6. Figure 3 shown.

[0043] The working principle of the high consistency MEMS pressure sensor of this embodiment is as follows:

[0044] The

[110] oriented varistor 6 constituting the first Wheatstone bridge 11 and the second Wheatstone bridge 12 The crystal varistors 6 all have a high resistance coefficient, and when affected by temperature changes, thermal stress output deviation caused by thermal expansion coefficient mismatch will be generated. By subtracting the output voltage of the first Wheatstone bridge 11 from the output voltage of the second Wheatstone bridge 12, not only can the zero drift deviation caused by the process random error be pre-compensated, but also a certain temperature compensation effect can be achieved to compensate for the thermal stress error caused by temperature changes.

[0045] Embodiment 3:

[0046] like Figure 4 , Figure 5 As shown, the only difference from Embodiment 1 is that the first Wheatstone bridge 11 uses four varistors 6 with a

[110] crystal orientation, and the second Wheatstone bridge 12 uses four varistors 6 with a

[110] crystal orientation.

[0047] Since both the first Wheatstone bridge 11 and the second Wheatstone bridge 12 use the varistors 6 with a

[110] crystal orientation, the varistors 6 inside and outside the film are parallel to each other.

[0048] The working principle of the high consistency MEMS pressure sensor of this embodiment is as follows:

[0049] The parallel structures of the varistors 6 of the first Wheatstone bridge 11 and the second Wheatstone bridge 12 are highly symmetrical. At this time, the consistency of the errors introduced by processes such as lithography and diffusion in the first Wheatstone bridge 11 and the second Wheatstone bridge 12 is higher, and the matching of the two varistors 6 inside and outside the membrane corresponding to the same side is better. Therefore, the scheme of subtracting the output voltage of the first Wheatstone bridge 11 from the output voltage of the second Wheatstone bridge 12 can more accurately pre-compensate the zero drift deviation caused by the random process error, thereby better improving the consistency performance of mass production. In addition, the first Wheatstone bridge 11 and the second Wheatstone bridge 12 are both composed of

[110] crystal orientation varistors 6, which have the same high voltage resistance coefficient, and the varistors 6 are parallel to each other, so the thermal stress directions output by the first Wheatstone bridge 11 and the second Wheatstone bridge 12 are also the same, which can achieve a better thermal stress error compensation effect.

[0050] Furthermore, the double Wheatstone bridge structure design scheme of the above-mentioned embodiments 1, 2 and 3 can be extended to be applied in differential pressure MEMS pressure sensors, specifically by providing a through hole connecting the cavity 4 with the outside of the sensor on the silicon substrate layer 1. The differential pressure MEMS pressure sensor can also reduce the sensor zero drift deviation caused by random process errors, thereby achieving corresponding beneficial effects such as improving the performance consistency of chips between wafers and chips within a wafer during mass production.

[0051] The difference between the above-mentioned embodiment 1, embodiment 2 and embodiment 3 is that the second Wheatstone bridge 12 is different, but the process steps required for preparation are the same. A method for preparing the above-mentioned high consistency MEMS pressure sensor comprises:

[0052] S1: Select two N-type

[100] single crystal silicon wafers with a thickness of 300 to 700 μm, one of which is used as the silicon substrate layer 1 and the other is used as the silicon device layer 2.

[0053] S2: Form an oxide layer 3 on the surface of the silicon substrate layer 1 by a thermal oxidation process, and then form a cavity 4 of a desired size on the front side of the silicon substrate layer 1 by a bulk silicon etching process, such as Figure 6 shown.

[0054] S3: Bonding the silicon substrate layer 1 with the cavity 4 etched therein to the silicon device layer 2 under vacuum conditions to form a sealed cavity 4, and then thinning the bonded silicon device layer 2 to the required thickness of the sensitive film 5, such as Figure 7 shown.

[0055] S4: Boron ion implantation is performed on a local area of ​​the silicon device layer 2 to form each varistor 6 and a heavily doped region 7, such as Figure 8 shown.

[0056] S5: Using LPCVD process to deposit a layer of silicon oxide on the upper surface of the silicon device layer 2 to form an intermediate layer 8, such as Fig. 9 shown.

[0057] S6: Perform photolithography on the intermediary layer 8 to make contact holes connected to the heavily doped region 7; then perform magnetron sputtering and photolithography on the surface of the intermediary layer 8 to form metal leads 9, such as Fig.10 shown.

[0058] S7: Depositing a protective layer 10 of silicon oxide, silicon nitride or other materials on the upper surface of the interposer 8 by using LPCVD (Low Pressure Chemical Vapor Deposition) process.

[0059] S8: Photolithography is performed on the surface of the protective layer 10 to expose the metal pad, such as Fig.11 shown.

[0060] Furthermore, the above-mentioned MEMS pressure sensor may also use a substrate layer such as glass, organic matter, etc.

[0061] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A high consistency MEMS pressure sensor, characterized in that: The invention comprises a silicon substrate layer (1), a cavity (4) is arranged at the central position of the upper surface of the silicon substrate layer (1), an oxide layer (3) is arranged on the silicon substrate layer (1), a silicon device layer (2) is arranged on the oxide layer (3), wherein the portion of the silicon device layer (2) located directly above the cavity (4) forms a sensitive film (5); eight varistors (6) are arranged on the upper surface of the silicon device layer (2), wherein four varistors (6) are respectively located at the central positions of the four sides of the sensitive film (5), and the other four varistors (6) are respectively located outside the sensitive film (5) region, and heavily doped regions (7) for forming ohmic contacts and electrical connections are respectively arranged at both ends of each varistor (6); 2) is provided with an intermediate layer (8), and a metal lead (9) is provided on the intermediate layer (8); four varistors (6) located relatively on the inner side are connected to the metal lead (9) through a heavily doped region (7) to form a first Wheatstone bridge (11); four varistors (6) located relatively on the outer side are connected to the metal lead (9) through a heavily doped region (7) to form a second Wheatstone bridge (12); a protective layer (10) is provided on the intermediate layer (8) and the metal lead (9); wherein the varistors (6) constituting the first Wheatstone bridge (11) have a high voltage resistance coefficient, and the output voltage of the first Wheatstone bridge (11) and the second Wheatstone bridge (12) is subtracted to serve as the output of the pressure sensor.

2. The high consistency MEMS pressure sensor according to claim 1, characterized in that: The first Wheatstone bridge (11) uses four varistors (6) with a [110] crystal orientation, and the second Wheatstone bridge (12) uses four varistors (6) with a [100] crystal orientation, and the sizes of the varistors (6) are all the same.

3. The high consistency MEMS pressure sensor according to claim 1, characterized in that: The first Wheatstone bridge (11) uses four varistors (6) with a [110] crystal orientation, and the second Wheatstone bridge (12) uses four The varistor (6) has a uniform crystal orientation, and the sizes of the varistor (6) are all the same.

4. The high consistency MEMS pressure sensor according to claim 1, characterized in that: The first Wheatstone bridge (11) uses four varistors (6) with a [110] crystal orientation, and the second Wheatstone bridge (12) uses four varistors (6) with a [110] crystal orientation, and the sizes of the varistors (6) are all the same.

5. The high consistency MEMS pressure sensor according to any one of claims 1 to 4, characterized in that: The silicon substrate layer (1) is also provided with a through hole connecting the cavity (4) with the outside of the sensor, thereby forming a differential pressure MEMS pressure sensor.

6. A method for preparing a high consistency MEMS pressure sensor as claimed in any one of claims 1 to 4, characterized in that: include: S1: Select two single crystal silicon wafers to be used as a silicon substrate layer (1) and a silicon device layer (2) respectively; S2: forming an oxide layer (3) on the surface of the silicon substrate layer (1) by a thermal oxidation process, and then forming a cavity (4) of a desired size on the front side of the silicon substrate layer (1) by a bulk silicon etching process; S3: bonding the silicon substrate layer (1) with the cavity (4) etched therein to the silicon device layer (2) under vacuum conditions to form a sealed cavity (4), and then thinning the bonded silicon device layer (2) to the thickness of the sensitive film (5); S4: implanting boron ions into a local area of ​​the silicon device layer (2) to form various varistors (6) and heavily doped areas (7); S5: using an LPCVD process to deposit a layer of silicon oxide on the upper surface of the silicon device layer (2) to form the intermediate layer (8); S6: performing photolithography on the intermediate layer (8) to form a contact hole connected to the heavily doped region (7); and then performing photolithography and magnetron sputtering on the intermediate layer (8) to form the metal lead (9); S7: Depositing a protective layer (10) on the upper surface of the intermediate layer (8) using an LPCVD process; S8: Photolithography is performed on the surface of the protective layer (10) to expose the metal pad.

Citation Information

Cited By

  • Pressure sensor chip capable of reducing output drift in situ and preparation method thereof

    CN119573927A

  • Silicon piezoresistive pressure chip and sensor

    CN121430898A

  • High-consistency MEMS (Micro Electro Mechanical System) array device and preparation process

    CN122079063A

  • Sensing module and method of manufacturing the same

    US20250137857A1