Defect detection scanning program establishing method and defect detection method

By establishing a scan map on the real wafer map and mapping merged defect information, the defect mapping problem caused by merged scanning units is solved, and accurate defect detection of large-scale chips is achieved, and product yield and detection efficiency are improved.

CN118943038APending Publication Date: 2024-11-12GTA SEMICON CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411011796.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-12

Smart Images

  • Figure CN118943038A_ABST
    Figure CN118943038A_ABST
Patent Text Reader

Abstract

The invention provides a defect detection scanning program establishment method and a defect detection method, and the method comprises the steps: establishing a scanning graph of a wafer on the basis of an established real wafer graph, namely, the scanning graph and the real wafer graph are in the same coordinate system; and after a merged defect graph of the scanning graph is obtained, mapping defect information in the merged defect graph back to a real chip defect graph corresponding to the chip in the real wafer graph. Therefore, the defect condition of a real chip in a wafer can be detected under the defect detection scanning program instead of combining the defect condition of a scanning unit, the defect condition of the chip can be directly known, and electronic INK work can be performed on a real wafer graph; in addition, data of the real chip defect graph can be directly compared with data of the wafer electrical property test graph and data of the wafer packaging test graph, the lethality of the real chip defect on the wafer electrical property and the wafer packaging property is calculated, and therefore main problems in engineering are solved in time, and help is provided for rapid improvement of the yield.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology defect detection technology, and in particular to a defect detection scanning program establishment method and a defect detection method. Background Art

[0002] In recent years, with the rapid development of semiconductor integrated circuits and the proportional reduction of key dimensions, their manufacturing processes have become increasingly complex. At present, advanced integrated circuit manufacturing processes generally include hundreds of process steps. If there is a problem in one of the steps, it will cause defects in the entire semiconductor integrated circuit chip on the wafer, and in severe cases, it may even cause the failure of the entire chip. Therefore, in the manufacturing process of semiconductor integrated circuits, it is particularly important to promptly discover problems in the product manufacturing process. Based on the above considerations, the industry generally controls defects in the manufacturing process through defect detection to improve product yield.

[0003] The industry generally uses a scanning machine to scan wafers for defects under a certain scanning program, and compares the number of defects obtained by the scan with the control limit to determine whether the defects on the wafer exceed the control standard and take corresponding measures in a timely manner.

[0004] In the prior art, each semiconductor production line is equipped with a number of defect scanning machines for improving yield, corresponding to different products, different production lines, and even different process links. Each defect scanning machine is equipped with a large number of scanning programs, corresponding to the defect scanning of a certain type of product or a certain layer of structure. The scanning program is the basis for establishing a reasonable and efficient defect detection system, and plays a vital role in investigating, analyzing and feedback on defects that affect product yield on the production line.

[0005] The basic principle of defect detection is to use each chip (gross die) on the wafer as a separate scanning unit (scan die), incident light / electrons on the wafer surface, collect reflected / scattered light / electrons, obtain a grayscale image, compare the image between the scanning unit and its adjacent chips, find the difference and judge according to the set threshold, and when the threshold is exceeded, it is considered a defect. However, when the total number of chips on the wafer is large, for example, more than 2,000, the amount of chip-to-chip defect comparison data of the scanning machine will be very large, exceeding the computer's tolerance, resulting in a longer scanning time and frequent computer jams. Therefore, a merged scanning unit (Merge die Scan) was developed, which merges multiple chips on the wafer into a larger scanning unit (scan die), and then compares the image between the larger scanning unit and its adjacent scanning units to find defects, so as to reduce the computer's data processing and calculation burden and improve scanning efficiency. However, the method of merging scanning defects has defects, that is, the defect map presented is no longer the real map of each individual chip, but a merged map, so it is impossible to directly mark the bad die. Summary of the invention

[0006] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a defect detection scanning program establishment method and a defect detection method, which are used to solve the problem that the defect mapping map obtained by merging scanning units in the establishment of the defect detection scanning program in the prior art is a merged defect mapping map.

[0007] To achieve the above-mentioned and other related purposes, the present invention provides a defect detection scanning program establishment method, the defect detection scanning program establishment method comprising:

[0008] Loading a wafer into a defect scanning machine, and aligning the wafer with the defect scanning machine;

[0009] creating a wafer map of the wafer;

[0010] Establishing a scan map of the wafer based on the wafer map, wherein a scan unit of the scan map is formed by merging at least two chips;

[0011] Determining scanning parameters for scanning the scanned image;

[0012] Performing a test scan and threshold adjustment on the wafer to obtain a merged defect map corresponding to the scanned image;

[0013] The defect information in the merged defect map is mapped back into a real chip defect map corresponding to the wafer map.

[0014] Optionally, the method of establishing the scan image of the wafer includes:

[0015] Selecting a starting chip to be merged on the wafer map;

[0016] Input the number of chips to be merged along the first direction X and the second direction Y in the plane rectangular coordinate system;

[0017] A merging direction of the defect scanning machine is determined, and the defect scanning machine tiles the largest scanning image of the wafer based on the merging direction.

[0018] Furthermore, a chip located at the outermost edge of the wafer is selected as a starting chip to be merged on the wafer.

[0019] Optionally, the number of chips that need to be merged along the first direction is not less than 2, and the number of chips that need to be merged along the second direction is zero; or the number of chips that need to be merged along the second direction is not less than 2, and the number of chips that need to be merged along the first direction is zero; or the number of chips that need to be merged along the first direction is M, and the number of chips that need to be merged along the second direction is N, M≥1, N≥1.

[0020] Optionally, the defect information of the merged defect map includes the vector coordinates (A, B) of the defect in the scanning unit where the defect is located and the size DieX of the chip in the wafer along the first direction and the size DieY along the second direction.

[0021] Furthermore, a scribe line is arranged between each of the chips in the wafer, and the defect information of the merged defect map further includes a size ScribeX of the scribe line along the first direction and a size ScribeY of the scribe line along the second direction.

[0022] Furthermore, when the defect information in the merged defect map is mapped back to the real chip defect map corresponding to the wafer map, the vector coordinates of the defect in the chip where it is located are (a, b), where a=A-(DieX+ScribeX)*n1, b=B-(DieY+ScribeY)*n2, n1 is the integer of A / (DieX+ScribeX), and n2 is the integer of B / (DieY+ScribeY).

[0023] The present invention also provides a defect detection method, the defect detection method comprising:

[0024] Loading a wafer to be inspected into a defect scanning machine, and aligning the wafer to be inspected with the defect scanning machine;

[0025] The defect scanning machine uses a defect detection scanning program to perform defect scanning on the wafer to be inspected to obtain a real chip defect map of the wafer to be inspected, wherein the defect detection scanning program is obtained using the defect detection scanning program establishment method described in any one of the above items.

[0026] Optionally, after obtaining the real chip defect map of the wafer to be inspected, the method further includes exporting the real chip defect map.

[0027] Optionally, the number of chips on the wafer to be inspected is greater than 2000.

[0028] As described above, the defect detection scanning program establishment method and defect detection method of the present invention establish a wafer scan map based on the established real wafer map, that is, the two are in the same coordinate system, and after obtaining the merged defect map of the scan map, the defect information in the merged defect map is mapped back to the real chip defect map corresponding to the chip in the real wafer map. Therefore, under the defect detection scanning program, the defect conditions on the real chip in the wafer can be detected, rather than the defect conditions of the merged scanning unit, and the defect conditions of the chip can be directly known, and electronic INK work can be realized on the real wafer map; it can also realize the direct comparison of the real chip defect map with the data of the wafer electrical test map and the wafer packaging test map, and calculate the lethality of the real chip defects to the wafer electrical performance and wafer packaging performance, so as to solve the main problems in the project in time and provide help for the rapid improvement of yield. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 A schematic diagram of a wafer using a single chip as a scanning unit in an example of wafer defect inspection is shown.

[0030] Figure 2 A schematic diagram of a wafer using multiple merged chips as scanning units in an example of wafer defect inspection is shown.

[0031] Figure 3 Shown is a schematic diagram of a wafer in the defect detection scanning program establishment method of the present invention.

[0032] Figure 4 Shown is a wafer map of a wafer created in the defect detection scan program creation method of the present invention.

[0033] Figure 5 Shown is a process diagram of establishing a wafer scan image based on a wafer image in the defect detection scan program establishment method of the present invention.

[0034] Figure 6 Shown is a scanning image of a wafer established based on a wafer image in the defect detection scanning program establishment method of the present invention.

[0035] Figure 7 and Figure 8 Display as Figure 6 Merged defect map of a scan unit in .

[0036] Component number description

[0037] 10 Wafer

[0038] 11 Chip

[0039] 12 Scan Units

[0040] 13 Cutting Road

[0041] 14 Defects

[0042] 15 Wafer coordinate origin

[0043] 16 Starter Chip

[0044] 20 Wafer

[0045] 21 Chip

[0046] 22 Scan Units DETAILED DESCRIPTION

[0047] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0048] See also Figures 1 to 8 It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0049] As described in the background technology, the basic principle of wafer defect detection is to use each chip (gross die) on the wafer as a separate scanning unit (scan die), incident light / electrons on the wafer surface, collect reflected / scattered light / electrons, obtain a grayscale image, compare the image between the scanning unit and its adjacent chips, find the difference and make a judgment based on the set threshold. When the threshold is exceeded, it is considered a defect. Figure 1When the wafer 20 shown in the figure has 16 chips 21 arranged in a 4×4 array, the wafer 20 is subjected to defect scanning to obtain a scanned image, and each chip 21 in the wafer 20 is used as a scan unit 22 to compare the scanned image with the adjacent chip 21, for example. Figure 1 In the example, when chip B is used as the scanning unit 22, the scanned image of chip B is compared with the scanned images of the two A chips on the left and right of chip B. By finding the difference and judging according to the set threshold, the defect situation of chip B is obtained, and the defect situation of all chips 21 on the entire wafer 20 is obtained by analogy. However, when the total number of chips on the wafer is large, for example, more than 2,000, the amount of chip-to-chip defect comparison data of the scanning machine will be very large, exceeding the computer's ability to bear, resulting in a longer scanning time and frequent computer jams. Therefore, a merged scanning unit (Merge die Scan) was developed, such as Figure 2 As shown, multiple chips 21 on a wafer 20 are combined into a larger scanning unit 22, for example Figure 2 In the example, 16 chips 21 arranged in 4×4 are combined into a scanning unit 22, and the image of the larger scanning unit 22 is compared with the image of the adjacent scanning unit. Figure 2 In the example, the scanned image of the B scanning unit is compared with the scanned images of the two adjacent A scanning units to obtain the defect situation of the B scanning unit, and the defect situation of all scanning units 22 on the entire wafer 20 is obtained by analogy. This combined chip scanning method can reduce the data processing volume and calculation burden of the computer and improve the scanning efficiency. However, the combined scanning defect method has a defect, that is, the defect map presented is no longer the real map of each individual chip, but the combined map, so the bad die cannot be directly marked.

[0050] Based on this, this embodiment provides a defect detection scanning program establishment method, which uses the defect detection scanning program to scan wafer defects using a method of merging scanning units to obtain a real chip defect map. The defect detection scanning program establishment method includes:

[0051] S1, loading a wafer into a defect scanning machine, and aligning the wafer with the defect scanning machine;

[0052] S2, establishing a wafer map of the wafer;

[0053] S3, establishing a scan map of the wafer based on the wafer map, wherein a scan unit of the scan map is formed by merging at least two chips;

[0054] S4, determining scanning parameters for scanning the scanned image;

[0055] S5, performing a test scan and threshold adjustment on the wafer to obtain a merged defect map corresponding to the scanned image;

[0056] S6, mapping the defect information in the combined defect map back to the real chip defect map corresponding to the wafer map.

[0057] The defect detection scanning program establishment method of this embodiment establishes a wafer scan map based on the established real wafer map, that is, the two are in the same coordinate system, and after obtaining the merged defect map of the scan map, the defect information in the merged defect map is mapped back to the real chip defect map corresponding to the chip in the real wafer map. Therefore, under this defect detection scanning program, the defect conditions on the real chip in the wafer can be detected, rather than the defect conditions of the merged scanning unit, and the defect conditions of the chip can be directly known, and electronic INK work can be realized on the real wafer map; it can also realize the direct comparison of the real chip defect map with the data of the wafer electrical test map and the wafer packaging test map, and calculate the lethality of the real chip defects to the wafer electrical performance and wafer packaging performance, so as to solve the main problems in the project in time and provide help for the rapid improvement of yield.

[0058] The defect detection scanning program establishment method of this embodiment is described in detail below with reference to specific drawings.

[0059] like Figure 3 As shown, firstly, step S1 is performed to provide a wafer 10, and the wafer 10 is loaded into a defect scanning machine (not shown in the figure), and the wafer 10 is aligned with the defect scanning machine.

[0060] like Figure 3 and Figure 7 As shown, the wafer 10 for wafer defect detection generally has a plurality of identical chips 11, and all the chips 11 are arranged in an array, with a cutting path 13 provided between two adjacent chips 11. The wafer will be cut along the cutting path 13 to obtain independent chips. The number of chips 11 on the wafer 10 of this embodiment is preferably greater than 2000.

[0061] The conventional alignment method can be used to achieve the alignment between the wafer 10 and the defect scanning machine. For example, generally, an alignment mark is provided on the wafer 10, and a sensor is provided at a corresponding position of the defect scanning machine for alignment.

[0062] like Figure 4 As shown, step S2 is then performed to create a wafer map of the wafer 10 .

[0063] like Figure 4 In the figure, the center of the wafer 10 is used as the wafer coordinate origin 15 of the wafer map.

[0064] like Figure 6 As shown, step S3 is then performed to establish a scan map of the wafer 10 based on the wafer map, wherein a scan unit 12 of the scan map is formed by combining at least two chips 11 .

[0065] Here, the number of chips 11 synthesized in the scanning unit 12 is not excessively limited, and they are merged according to actual needs. In principle, the fewer the number of chips 11 synthesized in the scanning unit 12, the more chips 11 in the wafer 10 can be merged into the scanning image, but the improvement in the computer's scanning efficiency is not significant; the more the number of chips 11 synthesized in the scanning unit 12, the more chips 11 cannot be merged into the scanning image, but the improvement in the computer's scanning efficiency is significant. The specific choice can be made according to actual needs. Generally, the merging rule of the chips 11 in the scanning unit 12 is array merging, that is, merging in an M×N array.

[0066] like Figures 4 to 6 As shown, as an example, the method of establishing the scanning image of the wafer includes:

[0067] like Figure 4 As shown, first select the starting chip 16 to be merged on the wafer map. It should be noted that the selection of the starting chip 16 is based on the actual situation. In order to merge more chips on the wafer and simplify the merging method, the chip at the outermost edge of the wafer is generally selected as the starting chip 16. For example, Figure 4 Select the chip in the upper left corner of the wafer map as the starting chip 16;

[0068] like Figure 5 As shown, the number of chips 11 to be merged along the first direction X and the second direction Y in the plane rectangular coordinate system is input; that is, the merging rule of the chips in the scanning unit 12 is set. As an example, the number of chips to be merged along the first direction X is not less than 2, and the number of chips to be merged along the second direction is zero; or the number of chips to be merged along the second direction Y is not less than 2, and the number of chips to be merged along the first direction is zero; or the number of chips to be merged along the first direction X is M, and the number of chips to be merged along the second direction Y is N, M≥1, N≥1, as shown in FIG. Figure 4 The merging rule of the chips in the scanning unit 12 is a 2×2 array merging rule;

[0069] like Figure 5 and Figure 6 As shown, the merging direction of the defect scanning machine is finally determined, and the defect scanning machine tiles the largest scanning image of the wafer based on the merging direction; that is, the merging direction of the scanning unit 12 is set, such as Figure 4The merging direction is to tile from the starting chip 16 in the X+ and Y- directions, so as to obtain the maximum scan image of the wafer 10.

[0070] Then, step S4 is performed to determine the scanning parameters for scanning the scanned image.

[0071] As an example, the scanning parameters generally include the light intensity used during scanning, the minimum pixel of the scan, the scanning method, the polarization direction of the light, and the like.

[0072] like Figure 7 As shown, step S5 is then performed to perform a trial scan and threshold adjustment on the wafer 10 to obtain a merged defect map corresponding to the scan image.

[0073] like Figure 8 As shown, as an example, the defect information of the merged defect map includes the vector coordinates (A, B) of the defect in the scanning unit 12 where the defect is located and the size DieX of the chip 11 in the wafer along the first direction X and the size DieY of the chip 11 along the second direction Y. Figure 8 The defect map of a scanning unit 12 in the entire merged defect map is shown in the figure, where O is a defect, Q is the coordinate origin in the scanning unit 12, and P is the coordinate origin of the chip where the defect O is located, so the vector coordinates of the defect O relative to the coordinate origin Q of the scanning unit 12 where it is located are (A, B). As mentioned above, a cutting path 13 is generally set between two adjacent chips 11 of the wafer 10, so the defect information of the merged defect map also includes the size ScribeX of the cutting path 13 along the first direction X and the size ScribeY along the second direction Y. The size ScribeX of the cutting path 13 along the X direction and the size ScribeY along the Y direction can be the same or different, and are set according to actual conditions.

[0074] like Figure 8 As shown, step S6 is finally performed to map the defect information in the combined defect map back to the real chip defect map corresponding to the wafer map.

[0075] Since the merged defect map, the scanning map and the wafer map are all established in the same coordinate system, the defect scanning machine knows the coordinate position of each scanning unit in its coordinate system. Therefore, when mapping the defect information in the merged defect map back to the real chip defect map, it is only necessary to calculate the specific position of the defect in each scanning unit in the scanning unit relative to the chip where it is located. The calculation is simple and fast, and easy to implement.

[0076] like Figure 8The vector coordinates of the known defect O relative to the coordinate origin Q of the scanning unit 12 where it is located are (A, B), the size of the chip 11 along the first direction X is DieX and the size along the second direction Y is DieY, and the size of the cutting path 13 along the first direction X is ScribeX and the size along the second direction Y is ScribeY; when mapping the defect O back to the real chip defect map, it is necessary to calculate the specific position of the defect O in the chip where it is located, that is, it is necessary to calculate the vector coordinates (a, b) of the defect O in the chip. The calculation method of the vector coordinates (a, b) is: a = A-(DieX+ScribeX)*n1, b = B-(DieY+ScribeY)*n2, n1 is the integer of A / (DieX+ScribeX), and n2 is the integer of B / (DieY+ScribeY), for example Figure 8 The scanning unit 12 in the figure is formed by merging four chips 11 of 2×2. The defect O is located in the chip 11 at the upper right corner of the scanning unit 12. Relative to the coordinate origin Q of the scanning unit, the rounded value of n1 should be 1, and the rounded value of n2 should also be 1.

[0077] This embodiment also provides a defect detection method, the defect detection method comprising:

[0078] S1, loading a wafer to be inspected into a defect scanning machine, and aligning the wafer to be inspected with the defect scanning machine;

[0079] S2, performing defect scanning on the wafer to be inspected by using a defect detection scanning program on the defect scanning machine to obtain a real chip defect map of the wafer to be inspected, wherein the defect detection scanning program is obtained by using the defect detection scanning program establishment method described in this embodiment.

[0080] As an example, the conventional alignment method can be used to achieve the alignment between the wafer to be inspected and the defect scanning machine. For example, an alignment mark is generally provided on the wafer to be inspected, and a sensor is provided at a corresponding position of the defect scanning machine for alignment.

[0081] As an example, the wafer to be inspected for wafer defect detection generally has a number of identical chips, and all chips are arranged in an array, with a cutting path between two adjacent chips. The wafer will be cut along the cutting path to obtain independent chips. The number of chips on the wafer to be inspected in this embodiment is preferably greater than 2000.

[0082] As an example, after obtaining the real chip defect map of the wafer to be tested, the process also includes exporting the real chip defect map. This is to facilitate electronic INK work on the real wafer map. In addition, the real chip defect map can be directly compared with the data of the wafer electrical test map and the wafer packaging test map to calculate the damage of the real chip defect to the wafer electrical performance and wafer packaging performance, so as to promptly solve the main problems in the project and provide help for rapid improvement of yield.

[0083] In summary, the present invention provides a defect detection scanning program establishment method and a defect detection method, which establishes a wafer scan map based on the established real wafer map, that is, the two are in the same coordinate system, and after obtaining the merged defect map of the scan map, the defect information in the merged defect map is mapped back to the real chip defect map corresponding to the chip in the real wafer map. Therefore, under the defect detection scanning program, the defect conditions on the real chip in the wafer can be detected, rather than the defect conditions of the merged scanning unit, and the defect conditions of the chip can be directly known, and electronic INK work can be realized on the real wafer map; it can also realize the direct comparison of the real chip defect map with the data of the wafer electrical test map and the wafer packaging test map, and calculate the lethality of the real chip defects to the wafer electrical performance and wafer packaging performance, so as to promptly solve the main problems in the project and provide help for the rapid improvement of the yield. Therefore, the present invention effectively overcomes the various shortcomings in the prior art and has a high industrial utilization value.

[0084] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for establishing a defect detection scanning program, characterized in that: The defect detection scanning program establishment method comprises: Loading a wafer into a defect scanning machine, and aligning the wafer with the defect scanning machine; creating a wafer map of the wafer; Establishing a scan map of the wafer based on the wafer map, wherein a scan unit of the scan map is formed by merging at least two chips; Determining scanning parameters for scanning the scanned image; Performing a test scan and threshold adjustment on the wafer to obtain a merged defect map corresponding to the scanned image; The defect information in the merged defect map is mapped back into a real chip defect map corresponding to the wafer map.

2. The defect detection scanning program establishment method according to claim 1, characterized in that: The method of establishing the scan image of the wafer includes: Selecting a starting chip to be merged on the wafer map; Input the number of chips to be merged along the first direction X and the second direction Y in the plane rectangular coordinate system; A merging direction of the defect scanning machine is determined, and the defect scanning machine tiles the largest scanning image of the wafer based on the merging direction.

3. The defect detection scanning program establishment method according to claim 2, characterized in that: The chip located at the outermost edge of the wafer is selected as the starting chip to be merged on the wafer.

4. The defect detection scanning program establishment method according to claim 2, characterized in that: The number of chips that need to be merged along the first direction is not less than 2, and the number of chips that need to be merged along the second direction is zero; or the number of chips that need to be merged along the second direction is not less than 2, and the number of chips that need to be merged along the first direction is zero; or the number of chips that need to be merged along the first direction is M, and the number of chips that need to be merged along the second direction is N, M≥1, N≥1.

5. The defect detection scanning program establishment method according to claim 2, characterized in that: The defect information of the merged defect map includes the vector coordinates (A, B) of the defect in the scanning unit where the defect is located and the size DieX of the chip in the wafer along the first direction and the size DieY of the chip along the second direction.

6. The defect detection scanning program establishment method according to claim 5, characterized in that: A dicing road is arranged between each of the chips in the wafer, and the defect information of the merged defect map further includes a size ScribeX of the dicing road along the first direction and a size ScribeY of the dicing road along the second direction.

7. The defect detection scanning program establishment method according to claim 6, characterized in that: When the defect information in the merged defect map is mapped back to the real chip defect map corresponding to the wafer map, the vector coordinates of the defect in the chip where it is located are (a, b), where a=A-(DieX+ScribeX)*n1, b=B-(DieY+ScribeY)*n2, n1 is the integer of A / (DieX+ScribeX), and n2 is the integer of B / (DieY+ScribeY).

8. A defect detection method, characterized in that: The defect detection method comprises: Loading a wafer to be inspected into a defect scanning machine, and aligning the wafer to be inspected with the defect scanning machine; The defect scanning machine uses a defect detection scanning program to perform defect scanning on the wafer to be inspected to obtain a real chip defect map of the wafer to be inspected, wherein the defect detection scanning program is obtained using the defect detection scanning program establishment method as described in any one of claims 1 to 7.

9. The defect detection method according to claim 8, characterized in that: After obtaining the real chip defect map of the wafer to be inspected, the method further includes exporting the real chip defect map.

10. The defect detection method according to claim 8, characterized in that: The number of chips on the wafer to be inspected is greater than 2000.

Citation Information

Cited By

  • Wafer surface defect scanning arrangement method and system

    CN120637260A