Production process of shaft sleeve of roll shaft bearing bush
Through centrifugal casting and finishing combined with flame spraying technology, the problems of low production efficiency and unstable quality in traditional processes are solved, the quality and wear resistance of roller bearing bushings are improved, and it is suitable for large-scale industrial production.
Patent Information
- Application Number
- CN202411267786.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-11
- Publication Date
- 2024-11-15
AI Technical Summary
The traditional roller bearing bushing production process has problems such as low production efficiency, unstable quality and poor wear resistance, which is difficult to meet the demand of modern industry for high-performance products.
Centrifugal casting technology is used to form dense blanks, combined with the finishing of CNC lathes and grinders, and flame spraying technology to carry out surface strengthening treatment, and through strict assembly and commissioning, the dimensional accuracy and surface quality of the product are ensured.
It improves the quality and performance of the product, ensures dimensional accuracy and surface quality, enhances wear resistance, is suitable for large-scale industrial production, and extends the service life of the product.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of bearing bushing sleeve production, in particular to a roller bearing bushing sleeve production process. Background Art
[0002] In modern industrial production, roller bearing bushings are key mechanical parts and are widely used in various mechanical equipment, such as papermaking machinery, printing machinery, metallurgical machinery, etc. The quality of their performance directly affects the operating efficiency, stability and service life of the equipment. However, the traditional production process has problems such as low production efficiency, unstable quality, and poor wear resistance, which makes it difficult to meet the needs of modern industry for high-performance roller bearing bushings. Summary of the invention
[0003] In order to overcome the above-mentioned defects in the prior art, the present invention provides a roller bearing bushing production process.
[0004] The technical solution adopted by the present invention to solve the technical problem is: a roller bearing bushing production process, characterized in that it includes the steps of:
[0005] (1) Material preparation stage: According to the product design requirements, calculate the proportion of various alloy materials required, inspect the alloy materials, use a spectrometer to detect their chemical composition to ensure that they meet national standards and design requirements, and test the physical properties of the alloy materials such as hardness and strength;
[0006] (2) Blank forming stage: the alloy material is melted and injected into a high-speed rotating mold by a centrifugal casting process. The rotation speed and casting temperature of the mold are controlled so that the alloy material is evenly distributed on the inner wall of the mold under the action of centrifugal force to form a dense blank. The blank after casting is cooled by a slow cooling method to reduce the stress and deformation inside the blank.
[0007] (3) Machining stage: The blank is rough-turned by a CNC lathe to remove most of the excess, and the inner hole, outer circle and other key parts of the bearing sleeve are fine-machined by a CNC milling machine and a grinder to ensure their dimensional accuracy and surface quality. The cutting parameters for fine machining should be selected to have a smaller cutting depth and feed speed to ensure machining accuracy;
[0008] (4) Surface strengthening treatment stage: flame spraying technology is used to spray the spraying material heated to a molten state onto the surface of the bearing sleeve through a spray gun to form a wear-resistant coating, and then the sprayed surface is polished to improve the surface finish and dimensional accuracy;
[0009] (5) Assembly and debugging stage: the processed bearing sleeve and roller are cleaned and then dried to ensure that their surfaces are dry, the bearing sleeve and roller are assembled, debugged and tested to ensure that the matching accuracy between the bearing sleeve and roller meets the design requirements, and the matching accuracy, running stability, etc. between the bearing sleeve and roller are tested;
[0010] Furthermore, in step (1), the alloy material is a mixture of babbitt alloy and copper alloy in a ratio of 3:1.
[0011] Furthermore, in step (2), the rotation speed of the mold is controlled at 800-1200 revolutions per minute, the casting temperature is controlled at 50-100° C. above the melting point of the alloy material, and the cooling time is controlled at more than 24 hours depending on the size of the blank and the characteristics of the material.
[0012] Furthermore, in step (3), the cutting depth of rough turning is controlled at 2-3 mm, the feed speed is controlled at 100-200 mm per minute, the cutting depth of fine machining is controlled at 0.1-0.2 mm, the feed speed is controlled at 20-50 mm per minute, and during the machining process, a cooling lubricant is used to cool and lubricate the tool and the workpiece to reduce tool wear and machining deformation.
[0013] Furthermore, in step (4), the spraying material is tungsten carbide or aluminum oxide. During the spraying process, the movement speed of the spray gun is controlled at 100-200 mm per minute, the spraying distance is controlled at 100-150 mm, the spraying angle is controlled at 45-90°, and the surface roughness after polishing is controlled at Ra0.2-Ra0.4 μm.
[0014] Furthermore, in step (5), the gap between the bearing sleeve and the roller shaft is controlled to be 0.05-0.1 mm.
[0015] The beneficial effects of the present invention are:
[0016] 1. The alloy material can be evenly and densely distributed on the inner wall of the mold under the promotion of centrifugal force, thus forming a high-quality blank, effectively avoiding the common internal defects and uneven organization problems in traditional casting processes, and improving the quality and performance of the product.
[0017] 2. The product has high dimensional accuracy and surface quality, high degree of automation in the production process, high production efficiency, and is suitable for large-scale industrial production.
[0018] 3. Improve product quality, performance and service life, and ensure product quality stability and reliability. DETAILED DESCRIPTION
[0019] In order to more clearly illustrate the technical solution of the present invention, the present invention is further described below. Obviously, what is described below is only one embodiment of the present invention. For ordinary technicians in this field, other embodiments can be obtained based on this embodiment without paying creative work, and they all belong to the protection scope of the present invention.
[0020] A roller bearing bushing production process, material preparation stage:
[0021] According to the product design requirements, the required proportions of various alloy materials are calculated. The alloy material can be made by mixing Babbitt alloy and copper alloy in a ratio of 3:1.
[0022] The alloy material is inspected and its chemical composition is detected by using a spectrometer to ensure that it meets national standards and design requirements. At the same time, the physical properties of the alloy material, such as hardness and strength, are tested.
[0023] Blank forming stage:
[0024] The centrifugal casting process is adopted to inject the molten alloy material into a high-speed rotating mold. By controlling the rotation speed and casting temperature of the mold, the alloy material is evenly distributed on the inner wall of the mold under the action of centrifugal force to form a dense blank. The rotation speed of the mold is controlled at about 1000 revolutions per minute, and the casting temperature is controlled at 50-100°C above the melting point of the alloy material.
[0025] The casting blank is cooled by slow cooling to reduce the stress and deformation inside the blank. The cooling time is reasonably adjusted according to the size of the blank and the characteristics of the material and is controlled within 24 hours.
[0026] Machining stage:
[0027] First, rough processing is carried out, and the blank is turned using a CNC lathe to remove most of the excess to improve processing efficiency. The cutting depth is controlled at 2-3mm and the feed speed is controlled at 100-200mm per minute.
[0028] Then, semi-finishing and finishing are carried out, and CNC milling machines and grinders are used to process the inner hole, outer circle and other key parts of the bearing sleeve to ensure its dimensional accuracy and surface quality, to ensure processing accuracy, the cutting depth is controlled at 0.1-0.2mm, and the feed speed is controlled at 20-50mm per minute. During the processing, cooling lubricants are used to cool and lubricate the tool and workpiece to reduce tool wear and processing deformation.
[0029] Surface strengthening treatment stage:
[0030] A flame spraying technique is used to spray a wear-resistant coating on the surface of the bearing sleeve. Suitable spraying materials, such as tungsten carbide, aluminum oxide, etc., are selected. After the spraying material is heated to a molten state, it is sprayed at high speed onto the surface of the bearing sleeve through a spray gun. During the spraying process, the moving speed, spraying distance and spraying angle of the spray gun are controlled to ensure the uniformity and thickness of the coating. The moving speed of the spray gun is controlled at 100-200 mm per minute, the spraying distance is controlled at 100-150 mm, and the spraying angle is controlled at 45-90°.
[0031] The surface after spraying is polished, and high-precision polishing equipment and polishing materials are used to finely polish the coating surface to improve the surface finish and dimensional accuracy. The surface roughness after polishing is controlled within Ra0.2-Ra0.4μm.
[0032] Assembly and commissioning phase:
[0033] The processed bearing bushings, sleeves and rollers are cleaned with detergent and ultrasonic cleaning equipment to remove oil, impurities and other dirt from their surfaces. Then they are dried to ensure that their surfaces are dry.
[0034] Special assembly tools and equipment are used to assemble the bearing sleeve and the roller shaft. During the assembly process, it is ensured that the matching accuracy between the bearing sleeve and the roller shaft meets the design requirements, and the gap between the bearing sleeve and the roller shaft is controlled at 0.05-0.1mm.
[0035] Carry out debugging and testing after assembly, and test the matching accuracy, running stability, etc. between the bearing sleeve and the roller shaft.
[0036] The present invention ensures that the chemical composition of the raw materials is highly accurate and meets strict quality standards by proportioning alloy materials, uses advanced casting technology to accurately control the design and manufacturing accuracy of the mold, and controls the casting temperature to ensure that the alloy material can be evenly and densely distributed on the inner wall of the mold under the promotion of centrifugal force, thereby forming a high-quality blank, effectively avoiding common internal defects and uneven structure problems in traditional casting processes, with high processing accuracy, good surface strengthening treatment and assembly effects, improving product quality, performance and service life, and having the characteristics of high efficiency, precision and reliability.
[0037] The above embodiments are only exemplary embodiments of the present invention and are not intended to limit the present invention. The protection scope of the present invention is defined by the claims. Those skilled in the art may make various modifications or equivalent substitutions to the present invention within the essence and protection scope of the present invention, and such modifications or equivalent substitutions shall also be deemed to fall within the protection scope of the present invention.
Claims
1. A roller bearing bushing production process, characterized in that: The following steps are involved: (1) Material preparation stage: According to the product design requirements, calculate the proportion of various alloy materials required, inspect the alloy materials, use a spectrometer to detect their chemical composition to ensure that they meet national standards and design requirements, and test the physical properties of the alloy materials such as hardness and strength; (2) Blank forming stage: the alloy material is melted and injected into a high-speed rotating mold by a centrifugal casting process. The rotation speed and casting temperature of the mold are controlled so that the alloy material is evenly distributed on the inner wall of the mold under the action of centrifugal force to form a dense blank. The blank after casting is cooled by a slow cooling method to reduce the stress and deformation inside the blank. (3) Machining stage: The blank is rough-turned by a CNC lathe to remove most of the excess, and the inner hole, outer circle and other key parts of the bearing sleeve are fine-machined by a CNC milling machine and a grinder to ensure their dimensional accuracy and surface quality. The cutting parameters for fine machining should be selected to have a smaller cutting depth and feed speed to ensure machining accuracy; (4) Surface strengthening treatment stage: flame spraying technology is used to spray the spraying material heated to a molten state onto the surface of the bearing sleeve through a spray gun to form a wear-resistant coating, and then the sprayed surface is polished to improve the surface finish and dimensional accuracy; (5) Assembly and debugging stage: The processed bearing sleeves and rollers are cleaned and then dried to ensure that their surfaces are dry. The bearing sleeves and rollers are assembled, debugged and tested to ensure that the fitting accuracy between the bearing sleeves and rollers meets the design requirements. The fitting accuracy, operating stability, etc. between the bearing sleeves and rollers are tested.
2. A roller bearing bushing production process according to claim 1, characterized in that: In step (1), the alloy material is a mixture of babbitt alloy and copper alloy in a ratio of 3:
1.
3. A roller bearing bushing production process according to claim 1, characterized in that: In step (2), the rotation speed of the mold is controlled at 800-1200 revolutions per minute, the casting temperature is controlled at 50-100° C. above the melting point of the alloy material, and the cooling time is controlled at more than 24 hours depending on the size of the blank and the characteristics of the material.
4. A roller bearing bushing production process according to claim 1, characterized in that: In step (3), the cutting depth of rough turning is controlled at 2-3 mm, the feed speed is controlled at 100-200 mm per minute, the cutting depth of fine machining is controlled at 0.1-0.2 mm, and the feed speed is controlled at 20-50 mm per minute. During the machining process, a cooling lubricant is used to cool and lubricate the tool and the workpiece to reduce tool wear and machining deformation.
5. The roller bearing bushing production process according to claim 1, characterized in that: In step (4), the spraying material is tungsten carbide or aluminum oxide. During the spraying process, the moving speed of the spray gun is controlled at 100-200 mm per minute, the spraying distance is controlled at 100-150 mm, the spraying angle is controlled at 45-90°, and the surface roughness after polishing is controlled at Ra0.2-Ra0.4 μm.
6. A roller bearing bushing production process according to claim 1, characterized in that: In step (5), the gap between the bearing sleeve and the roller shaft is controlled to be 0.05-0.1 mm.
Citation Information
Patent Citations
Manufacturing process of high-power low-speed diesel shaft bushing
CN101275606A
Compound centrifugal manufacturing method for axial sleeve of bushing
CN101596583A
Shaft sleeve machining method
CN105441858A
Axle sleeve machining method
CN109483158A
Manufacturing method for copper-steel composite wear-resistant bearing bushing with high-stress self-tightening force
WO2023142397A1
Cited By
Simplified machining process for bearing sleeve
CN120080117A
Machining method of eccentric bearing bush
CN120095511A