Compound master batch for polyethylene device and preparation method of compound master batch

By using a compound masterbatch of specific ratios in a polyethylene device, the problem of insufficient acid and alkali resistance of existing masterbatches is solved, which significantly improves the acid resistance and alkali resistance of plastic products and extends the service life of the product.

CN118956066APending Publication Date: 2024-11-15JIANGSU HANGUANG IND CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411179497.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The existing masterbatch has weak acid-base resistance, resulting in a short service life of plastic products after forming.

Method used

The compound masterbatch is used for polyethylene devices, and the composition includes composite permeability enhancers, dispersants, light stabilizers, linear low-density polyethylene, matrix resin and polystyrene. Through specific proportions and processing techniques, it has excellent resistance. Complex masterbatch with acid and alkali resistance.

Benefits of technology

It significantly improves the acid-resistant and alkali-resistant properties of compound masterbatch molding products and extends the service life of plastic products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118956066A_ABST
    Figure CN118956066A_ABST
Patent Text Reader

Abstract

The invention discloses a compound master batch for a polyethylene device and a preparation method of the compound master batch, relates to the technical field of compound master batches, and solves the problem that the service life of a plastic product produced and molded by using the master batch is relatively short due to relatively weak acid and alkali resistance of the existing master batch. The invention relates to a compound master batch for a polyethylene device. The compound master batch comprises the following components in percentage by weight: 3-8% of a composite anti-reflection agent, 4-7% of a dispersing agent, 6-8% of a light stabilizer, 15-25% of linear low-density polyethylene, 25-30% of matrix resin and 15-30% of polystyrene. The compound master batch disclosed by the invention has good acid resistance and alkali resistance, the quality of a product produced by molding the compound master batch is improved, and the service life of a plastic product is effectively prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of compound masterbatches, in particular to a compound masterbatch for polyethylene devices. Background Art

[0002] Masterbatch refers to the granular material obtained by mixing and kneading various additives, fillers and a small amount of carrier resin in the process of plastic processing and molding for the convenience of operation, and then measuring, mixing, melting, extruding, pelletizing and other processing processes such as extruders and other equipment. Masterbatch can usually be divided into ordinary filling masterbatch (referred to as filling masterbatch) and functional masterbatch, such as color masterbatch, anti-drip masterbatch, etc. Masterbatch is composed of carrier resin, various fillers and various additives. The limit of additives or filler content in masterbatch is several to dozens of times higher than the required amount in actual plastic products. During the molding process, the ratio of masterbatch to matrix resin must be adjusted according to the content of relevant components in the masterbatch and the amount required to be added in the actual product.

[0003] The existing masterbatches have weak acid and alkali resistance, resulting in a short service life of plastic products produced using these masterbatches; therefore, they do not meet existing needs. In this regard, we have proposed a compound masterbatch for polyethylene devices. Summary of the invention

[0004] The object of the present invention is to provide a compound masterbatch for polyethylene devices to solve the problems mentioned in the above background technology that the existing masterbatch has weak acid and alkali resistance, resulting in a short service life of plastic products produced using these masterbatches.

[0005] To achieve the above object, the present invention provides the following technical solution: a composite masterbatch for polyethylene device, wherein the proportions of the components are: Composite permeability enhancer 3-8% Dispersant 4-7% Light stabilizer 6-8% Linear low density polyethylene 15-25% Base resin 25-30% Polystyrene 15-30%.

[0006] Preferably, the surfactant composite permeability enhancer is composed of sodium stearate, sodium dodecylbenzene sulfonate, a nucleating agent and hydrated magnesium silicate powder.

[0007] Preferably, the ratio of the sodium stearate, sodium dodecylbenzene sulfonate, nucleating agent and hydrated magnesium silicate powder is 3:1:3:2.

[0008] Preferably, the base resin is a blend of propylene, ethylene and octene copolymer.

[0009] Preferably, the composition ratio of the propylene, ethylene and octene copolymer is 3:3:4.

[0010] Preferably, the dispersant is composed of methylpentanol, cellulose derivatives, and fatty acid polyethylene glycol esters.

[0011] Preferably, the respective component ratios of the methyl pentanol, the cellulose derivative, and the fatty acid polyethylene glycol ester are 1:1:2.

[0012] A method for preparing a composite masterbatch for a polyethylene device comprises the following steps: S1: First, the components of the compound masterbatch: composite transmittance enhancer, dispersant, light stabilizer, linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene are weighed according to the processing ratio; S2: adding the weighed linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene into the reaction mixture; S3: adding solvent to the reactor and closing the reactor; S4: starting the reactor to stir the added linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene at a stirring speed of 1800-2000 rpm for 2-3 hours, and controlling the stirring temperature at 800-1000 degrees Celsius; S5: After the linear low-density polyethylene, the base resin, the oleic acid diethanolamide and the polystyrene are fully mixed with the solvent, a dispersant, a light stabilizer and a composite transmittance enhancer are successively added to the mixed solution; S6: After adding the dispersant, light stabilizer and composite transmittance enhancer, the temperature of the reactor is controlled at 400-600 degrees Celsius, and the reaction is continued under stirring for 1-1.5 hours; S7: After the reaction is completed, the finished product is taken out and cooled to set; S8: Put the cooled and shaped product into a granulator for granulation, and weigh and package the granulated product.

[0013] Compared with the prior art, the manufacturing method of the present invention has the following beneficial effects: The compound masterbatch of the invention has excellent acid resistance and alkali resistance, improves the quality of products produced by using the compound masterbatch, and effectively prolongs the service life of plastic products. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 It is a schematic diagram of the overall process of the present invention. DETAILED DESCRIPTION

[0015] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0016] like Figure 1 As shown, a composite masterbatch for polyethylene device, in parts by weight, the proportions of the components are: Composite permeability enhancer 3-8% Dispersant 4-7% Light stabilizer 6-8% Linear low density polyethylene 15-25% Base resin 25-30% Polystyrene 15-30%.

[0017] As a preferred embodiment of this embodiment, the components of the surfactant composite permeability enhancer are sodium stearate, sodium dodecylbenzene sulfonate, a nucleating agent and hydrated magnesium silicate powder, and the ratio of sodium stearate, sodium dodecylbenzene sulfonate, a nucleating agent and hydrated magnesium silicate powder is 3:1:3:2, which improves the plasticity and transparency of the compound masterbatch.

[0018] The base resin is a blend of propylene, ethylene and octene copolymer, and the composition ratio of the propylene, ethylene and octene copolymer is 3:3:4, which improves the overall structural strength of the compound masterbatch and has better acid and alkali resistance.

[0019] The dispersant comprises methyl amyl alcohol, cellulose derivatives and fatty acid polyethylene glycol esters, and the proportion of the methyl amyl alcohol, cellulose derivatives and fatty acid polyethylene glycol esters is 1:1:2.

[0020] A method for preparing a composite masterbatch for a polyethylene device comprises the following steps: S1: First, the components of the compound masterbatch: composite transmittance enhancer, dispersant, light stabilizer, linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene are weighed according to the processing ratio; S2: adding the weighed linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene into the reaction mixture; S3: adding solvent to the reactor and closing the reactor; S4: starting the reactor to stir the added linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene at a stirring speed of 1800-2000 rpm for 2-3 hours, and controlling the stirring temperature at 800-1000 degrees Celsius; S5: After the linear low-density polyethylene, the base resin, the oleic acid diethanolamide and the polystyrene are fully mixed with the solvent, a dispersant, a light stabilizer and a composite transmittance enhancer are successively added to the mixed solution; S6: After adding the dispersant, light stabilizer and composite transmittance enhancer, the temperature of the reactor is controlled at 400-600 degrees Celsius, and the reaction is continued under stirring for 1-1.5 hours; S7: After the reaction is completed, the finished product is taken out and cooled to set; S8: Put the cooled and shaped product into a granulator for granulation, and weigh and package the granulated product.

[0021] It will be apparent to those skilled in the art that the invention is not limited to the details of the exemplary embodiments described above and that the invention can be implemented in other specific forms without departing from the spirit or essential features of the invention. Therefore, the embodiments should be considered exemplary and non-limiting in all respects, and the scope of the invention is defined by the appended claims rather than the foregoing description, and it is intended that all variations falling within the meaning and scope of the equivalent elements of the claims be included in the invention. Any reference numeral in a claim should not be considered as limiting the claim to which it relates.

Claims

1. A compound masterbatch for polyethylene device, characterized in that: The ratio of each component is: Composite permeability enhancer 3-8% Dispersant 4-7% Light stabilizer 6-8% Linear low density polyethylene 15-25% Base resin 25-30% Polystyrene 15-30%.

2. The composite masterbatch for polyethylene device according to claim 1, characterized in that: The surfactant composite permeability enhancer comprises sodium stearate, sodium dodecylbenzene sulfonate, a nucleating agent and hydrated magnesium silicate powder.

3. The composite masterbatch for polyethylene device according to claim 2, characterized in that: The mixing ratio of the sodium stearate, sodium dodecylbenzene sulfonate, nucleating agent and hydrated magnesium silicate powder is 3:1:3:

2.

4. The composite masterbatch for polyethylene device according to claim 1, characterized in that: The base resin is a blend of propylene, ethylene and octene copolymer.

5. The composite masterbatch for polyethylene device according to claim 4, characterized in that: The composition ratio of the propylene, ethylene and octene copolymer is 3:3:

4.

6. The compound masterbatch for polyethylene device according to claim 1, characterized in that: The dispersant comprises methyl amyl alcohol, cellulose derivatives and fatty acid polyethylene glycol ester.

7. The composite masterbatch for polyethylene device according to claim 6, characterized in that: The respective component ratios of the methyl amyl alcohol, the cellulose derivative and the fatty acid polyethylene glycol ester are 1:1:

2.

8. A method for preparing a compound masterbatch for a polyethylene device, characterized in that: The following steps are involved: S1: First, the components of the compound masterbatch: composite transmittance enhancer, dispersant, light stabilizer, linear low-density polyethylene, base resin and polystyrene are weighed according to the processing ratio; S2: adding the weighed linear low-density polyethylene, base resin and polystyrene into the reaction vessel; S3: adding solvent to the reactor and closing the reactor; S4: starting the reactor to stir the added linear low-density polyethylene, base resin, oleic acid diethanolamide and polystyrene at a stirring speed of 1800-2000 rpm for 2-3 hours, and controlling the stirring temperature at 800-1000 degrees Celsius; S5: After the linear low-density polyethylene, the base resin, the oleic acid diethanolamide and the polystyrene are fully mixed with the solvent, a dispersant, a light stabilizer and a composite transmittance enhancer are successively added to the mixed solution; S6: After adding the dispersant, light stabilizer and composite transmittance enhancer, the temperature of the reactor is controlled at 400-600 degrees Celsius, and the reaction is continued under stirring for 1-1.5 hours; S7: After the reaction is completed, the finished product is taken out and cooled to set; S8: Put the cooled and shaped product into a granulator for granulation, and weigh and package the granulated product.