Manufacturing method of optical fiber magnetic field sensor composed of Terfenol-D powder and FPI

By applying Terfenol-D powder on the FPI structure and using the principle of primary harmonic cursor effect, the existing fiber optic magnetic field sensors have been solved, and a fiber optic magnetic field sensor with high sensitivity and compact structure is realized, which is suitable for Measurement of magnetic field in narrow spaces.

CN118980976AActive Publication Date: 2024-11-19HUBEI NORMAL UNIV
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202411061525.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-19
Estimated Expiration
2044-08-02

AI Technical Summary

Technical Problem

Existing fiber optic magnetic field sensors have low sensitivity in magnetic field measurement, and improper packaging of ferrofluids will lead to failure. The sensor structure is complex and not compact, making it difficult to be suitable for magnetic field measurement in narrow spaces.

Method used

The optical fiber magnetic field sensor production method is used to uniformly apply Terfenol-D powder on the FPI structure and use the principle of first harmonic cursor effect to form a magnetic field sensor with high sensitivity and compact structure. .

Benefits of technology

It realizes a high sensitivity and suitable for measuring magnetic field in narrow spaces. It has a compact structure and easy to manufacture and is suitable for use in harsh environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure FT_1
    Figure FT_1
  • Figure BDA0004978007320000071
    Figure BDA0004978007320000071
  • Figure BDA0004978007320000072
    Figure BDA0004978007320000072
Patent Text Reader

Abstract

The invention discloses a manufacturing method of an optical fiber magnetic field sensor composed of Terfenol-D powder and an FPI. The method comprises the following steps: step 1, manufacturing a Fabry-Perot interferometer 1, namely an FPI1; 2, uniformly coating Terfenol-D powder on the surface of a large capillary tube of the FPI1 to form the FPI1 sensitive to a magnetic field; a third step, manufacturing a Fabry-Perot interferometer 2, namely an FPI2 (Fabry-Perot Interferometer 2); fourthly, the single-mode optical fiber ends of the FPI1 and the FPI2 are welded together through a welding machine, the distance between the two FPIs ranges from 5 mm to 1 cm, and the two FPIs are cascaded to be manufactured into a primary harmonic vernier effect sensor; according to the method, the advantages of an existing sensor are absorbed, the defects of the existing sensor are overcome, the quartz capillary tube, the single-mode fiber, the Terfenol-D powder, the epoxy resin glue, the ultraviolet glue, the FPI and the first harmonic vernier effect are utilized, and the optical fiber magnetic field sensor which is compact in structure, easy to manufacture and package and high in sensitivity can be well manufactured. The sensor can be suitable for narrow space magnetic field measurement, and has good practical application value.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of high-precision sensor equipment manufacturing process methods, in particular to a method for manufacturing an optical fiber magnetic field sensor composed of Terfenol-D powder and FPI. Background Art

[0002] The accurate measurement of magnetic field is crucial in the fields of nuclear experiments, ocean exploration, geophysics, space exploration, etc. Compared with traditional magnetic field sensors, optical fiber magnetic field sensors are prepared by combining optical fiber and magnetic sensitive materials. They have the advantages of compact structure, easy operation, anti-electromagnetic interference, ability to be used in harsh environments, high sensitivity, etc., and have been widely used in field detection in the field of magnetic field.

[0003] According to the detection principle and magnetic sensitive materials, people have invented a variety of fiber optic magnetic field sensors. For example, fiber grating magnetic field sensor, fiber surface plasmon magnetic field sensor, fiber whispering gallery mode magnetic field sensor, fiber antiresonance optical waveguide mode magnetic field sensor and fiber interferometer magnetic field sensor. These magnetic field sensors have their own characteristics and the sensitivity of the sensors is also different.

[0004] The first category, the most common fiber optic magnetic field sensor, is based on the combined structure of fiber optic interferometer and ferrofluid, which has been rapidly developed due to its compact structure and easy integration. For example, a high-sensitivity magnetic field sensor formed by filling magnetic fluid into the FP cavity of a Fabry-Perot interferometer (FPI); a magnetic field sensor in which magnetic fluid is wrapped on the surface of a Mach-Zehnder interferometer (MZI); a vector magnetic field sensor based on U-shaped bent optical fiber and magnetic fluid wrapping, etc. In the above-mentioned magnetic field sensors based on magnetic fluid, the change in the refractive index of the magnetic fluid caused by the external magnetic field is small, resulting in a small drift in the sensor's spectral resonance wavelength, and the resulting magnetic field sensitivity is usually low. In addition, ferrofluid is a water-soluble liquid. If it is not wrapped well, the magnetic fluid will fail to work, so it is also a tricky problem to effectively package it with the fiber optic interferometer.

[0005] The second type, a common magnetic field sensor structure, is to use Terfenol-D magnetostrictive material combined with fiber Bragg grating or fiber interferometer. For example, a magnetic field sensor combining FPI with Terfenol-D; a magnetic field sensor based on the whispering gallery mode of a hollow microbubble resonator and Terfenol-D; a magnetic field sensor based on Terfenol-D and fiber Bragg grating, etc. The magnetostrictive material Terfenol-D can be used to effectively measure the magnetic field, but the Terfenol-D rod is usually large in size, and the size of the prepared sensor is also large, which is not suitable for magnetic field measurement in a small space.

[0006] In recent years, in order to improve the sensitivity of magnetic field sensors, people have also applied optical vernier effect and harmonic vernier effect to the field of fiber optic magnetic field sensors. For example, a high-sensitivity vernier magnetic field sensor based on two MZI cascades and a magnetic fluid combination; a high-sensitivity vernier effect magnetic field sensor based on two FPIs in parallel and a magnetic fluid combination; a high-sensitivity vernier magnetic field sensor based on a cantilever beam FPI combined with Terfenol-D material; an ultra-sensitive magnetic field sensor based on three-reflection surface interference and harmonic vernier effect combined with Terfenol-D material, etc. These sensors have achieved extremely high sensitivity, but they also have defects such as complex structure, difficulty in manufacturing, and non-compact structure. Summary of the invention

[0007] The purpose of the present invention is to provide a method for producing an optical fiber magnetic field sensor composed of Terfenol-D powder and FPI in view of the above situation. The method can produce a magnetic field sensor with high sensitivity, large measurement range, small size and suitable for magnetic field measurement in a small space.

[0008] The specific scheme of the present invention is: a method for manufacturing an optical fiber magnetic field sensor composed of Terfenol-D powder and FPI, the method comprising the following steps:

[0009] The first step is to make a Fabry-Perot interferometer 1, or FPI1: take a large quartz capillary and burn off the protective layer on its surface with fire. Its inner diameter is 150 microns and its outer diameter is 360 microns. Then, insert two sections of single-mode optical fibers with their coatings stripped and their end faces cut flat into the large capillary from both ends, adjust the distance between the two single-mode optical fibers, and when the spectrum meets the requirements, use ultraviolet glue to glue the single-mode optical fiber and the large capillary together at both ends of the large capillary. Irradiate with an ultraviolet lamp for 1 minute, and glue the large capillary and the single-mode optical fiber together to form an FPI1. FPI1 is formed by the interference of reflected light from two reflection surfaces M1 and M2. The FP cavity of FPI1 is an air cavity with a length of L1. In the FPI1 structure, the length between the bonding points of the capillaries on both sides is L, and the single-mode optical fibers inserted from both sides of the capillary form a cantilever beam structure in the capillary.

[0010] The second step is to evenly coat the Terfenol-D powder on the surface of the large capillary of FPI1 to form FPI1 that is sensitive to the magnetic field. Specifically, Terfenol-D powder and epoxy resin glue are first configured according to a powder-to-glue mass ratio of 95:5, that is, 95% Terfenol-D powder and 5% epoxy resin glue are mixed and stirred to form a uniform mixed colloid for standby use; then the configured Terfenol-D mixed glue is evenly coated on the outer surface of the large capillary in FPI1 to cover the entire outer surface of the large capillary; the prepared structure is first placed at room temperature for two hours, then placed in a drying oven at 40°C for 8 hours, and finally placed at room temperature for half a month to allow the coated material to dry completely;

[0011] The third step is to make Fabry-Perot interferometer 2, or FPI2: take a small quartz capillary and burn off the protective layer on its surface with fire. Its inner diameter is 75 microns and its outer diameter is 125 microns. Then, use a fiber fusion splicer to fuse a section of single-mode optical fiber with its coating stripped and end face cut flat to the small quartz capillary. Use a fiber cleaver to cut the capillary to the designed length L2. Then, fuse another section of single-mode optical fiber with its coating stripped and end face flat to the other end of the small capillary. Finally, use a fiber cleaver to cut the end of the single-mode optical fiber into an inclined surface. In this way, the production of FPI2 is completed. FPI2 is formed by the interference of reflected light from the two reflection surfaces M3 and M4. The FP cavity of FPI2 is also an air cavity with a length of L2.

[0012] In the fourth step, the single-mode optical fiber ends of FPI1 and FPI2 are welded together using a welding machine. The two FPIs are 5 mm to 1 cm apart. The two FPIs are cascaded to produce a first harmonic vernier effect sensor.

[0013] Furthermore, the FPI1 and FPI2 described in the present invention are both non-intrinsic low-fineness FPIs.

[0014] Furthermore, the diameter of the Terfenol-D powder in the second step of the present invention is 100 microns to 150 microns.

[0015] Furthermore, in the present invention, the thickness of the Terfenol-D mixed solution coating on the outer wall of the large capillary in the second step is maintained at 0.8 to 1.2 mm.

[0016] Furthermore, the FP cavity length in FPI1 and FPI2 of the present invention is L I and L2, L2 is approximately twice that of L1, and the reflectance spectra of the two FPIs have similar extinction ratios, and their free spectral ranges are approximately twice the relationship.

[0017] The method of the present invention absorbs the advantages of existing sensors and overcomes their disadvantages. It utilizes quartz capillaries, single-mode optical fibers, Terfenol-D powder, epoxy resin glue, ultraviolet glue, FPI and the first harmonic cursor effect to produce an optical fiber magnetic field sensor with a particularly compact structure, easy production, easy packaging and high sensitivity. The sensor can be applied to magnetic field measurement in a narrow space and has good practical application value. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the structure of the sensor produced by the method of the present invention.

[0019] In the figure: 1, 5 and 7 - single-mode optical fibers, 2 - large capillary, 3 - Terfenol-D mixed liquid coating, 4 - UV glue, 6 - small capillary. DETAILED DESCRIPTION

[0020] The technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings of the present invention. It is obvious that the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the protection scope of the present invention. In the description of the present invention, it should be noted that the terms "upper", "lower", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, or the orientations or positional relationships in which the invented product is usually placed when used, which are only for the convenience of describing the present invention or simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed or operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0021] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "setting", "installation" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0022] See also Figure 1 The present invention is a method for manufacturing an optical fiber magnetic field sensor composed of Terfenol-D powder and FPI, and the method comprises the following steps:

[0023] The first step is to make a Fabry-Perot interferometer 1, namely FPI1: take a large quartz capillary, namely large capillary 2, and burn off the protective layer on its surface with fire. Its inner diameter is 150 microns and its outer diameter is 360 microns; then, insert two sections of single-mode optical fibers 1 and 5 with their coatings stripped and their end faces cut flat into the large capillary from both ends, adjust the distance between the two single-mode optical fibers, and when the spectrum meets the requirements, use ultraviolet glue 4 at both ends of the large capillary to stick the single-mode optical fiber and the large capillary together, irradiate with an ultraviolet lamp for 1 minute, and stick the large capillary and the single-mode optical fiber together to form an FPI1. FPI1 is formed by the interference of reflected light from two reflection surfaces M1 and M2. The FP cavity of FPI1 is an air cavity with a length of L1. In the FPI1 structure, the length between the sticking points of the capillaries on both sides is L, and the single-mode optical fibers inserted from both sides of the capillary form a cantilever beam structure in the capillary;

[0024] The second step is to evenly coat the Terfenol-D powder on the surface of the large capillary of FPI1 to form FPI1 that is sensitive to the magnetic field, specifically: first, Terfenol-D powder and epoxy resin glue are configured according to a powder-to-glue mass ratio of 95:5, that is, 95% Terfenol-D powder and 5% epoxy resin glue are mixed and stirred to form a uniform mixed colloid for standby use; then the configured Terfenol-D mixed glue is evenly coated on the outer surface of the large capillary in FPI1, and the entire outer surface of the large capillary is coated to form a Terfenol-D mixed glue coating 3; the prepared structure is first placed at room temperature for two hours, then placed in a drying oven at 40°C for 8 hours, and finally placed at room temperature for half a month to allow the coated material to dry completely; further, the diameter of the above-mentioned Terfenol-D powder is 100 microns to 150 microns; further, the thickness of the Terfenol-D mixed glue coating on the outer wall of the above-mentioned large capillary is maintained at 0.8 to 1.2 mm;

[0025] The third step is to make a Fabry-Perot interferometer 2, namely FPI2: take a small quartz capillary, namely the small capillary 6, and burn off the protective layer on its surface with fire. Its inner diameter is 75 microns and its outer diameter is 125 microns. Then, use a fiber fusion splicer to fuse a section of single-mode optical fiber 7 with its coating stripped and end face cut flat to the small quartz capillary. Use a fiber cleaver to cut the capillary to the designed length L2, and then fuse another section of single-mode optical fiber with its coating stripped and end face flat to the other end of the small capillary. Finally, use a fiber cleaver to cut the end of the single-mode optical fiber into an inclined surface. In this way, the production of FPI2 is completed. FPI2 is formed by the interference of reflected light from the two reflection surfaces M3 and M4. The FP cavity of FPI2 is also an air cavity, and the FP cavity length is L2.

[0026] In the fourth step, the single-mode optical fiber ends of FPI1 and FPI2 are welded together using a welding machine. The two FPIs are 5 mm to 1 cm apart. The two FPIs are cascaded to produce a first harmonic vernier effect sensor.

[0027] Furthermore, the FPI1 and FPI2 described in this embodiment are both extrinsic low-fineness FPIs. Furthermore, the FP cavity length in the FPI1 and FPI2 described in the present invention is L I and L2, L2 is approximately twice that of L1, and the reflectance spectra of the two FPIs have similar extinction ratios, and their free spectral ranges are approximately twice the relationship.

[0028] exist Figure 1 In the structure, based on the FPI theory, it can be deduced that the trough wavelengths in the reflection spectra of FPI1 and FPI2 are:

[0029]

[0030] Here, λ FPI1 and λ FPI2 They represent the trough wavelengths of the reflection spectra of FPI1 and FPI2 respectively, m is a positive integer, n1 and n2 are the refractive indices of the air in the FP cavities of FPI1 and FPI2 respectively, and L1 and L2 are the cavity lengths of the FP cavities of FPI1 and FPI2 respectively.

[0031] Since the reflection spectra of FPI1 and FPI2 are both periodic waveforms similar to sine waves, the difference between the wavelengths of two adjacent troughs in their spectra is defined as their free spectral range (FSR). Therefore, the approximate calculation formulas for the FSR of FPI1 and FPI2 are:

[0032]

[0033] In FPI1, due to the existence of the cantilever beam structure, it increases the effective action length of the strain acting on FPI1 from L1 to L, so the strain sensitivity of FPI1 is increased by L / L1 times. If L is designed to be much larger than L1, FPI1 will have a high sensitivity to axial strain. In addition, since Terfenol-D powder is a material that can produce linear expansion and contraction under the action of a magnetic field, it is now coated on the surface of FPI1. When an increased magnetic field is applied to both ends of FPI1, the Terfenol-D material will stretch along the direction of the magnetic field, which is equivalent to applying an axial strain to FPI1. Since FPI1 is very sensitive to axial strain, FPI1 is also very sensitive to the applied magnetic field. By demodulating the trough wavelength drift of FPI1, the measurement of the external magnetic field can be achieved. The magnetic field sensitivity of FPI1 can be simply expressed as follows:

[0034]

[0035] FPI2 is an interferometer formed by two reflecting surfaces between a single-mode optical fiber and air. There is no magnetostrictive material Terfenol-D attached to its surface. Therefore, under the action of an external magnetic field, its refractive index n2 and cavity length L2 will not change, so it is insensitive to the external magnetic field.

[0036] Finally, when FPI1 and FPI2 are cascaded together, since the FSR of FPI1 is designed to be nearly twice the FSR of FPI2, according to the principle of optical harmonic vernier effect, their spectra will be superimposed to form large periodic inner and outer envelope spectra. If the wavelength of the intersection of the inner envelope of the spectrum is used for measurement, it will have a greater amplification effect on the sensitivity of the sensor unit FPI1. This is the so-called optical harmonic vernier effect. In the harmonic vernier effect sensor formed by the cascade of FPI1 and FPI2, FPI1, which is sensitive to magnetic fields, serves as a sensing element, and FPI2, which is insensitive to magnetic fields, serves as a reference element. Based on the principle of optical harmonic vernier effect, it can be deduced that the inner envelope of the first harmonic vernier effect spectrum as follows:

[0037]

[0038] Therefore, using the principle of optical harmonic vernier effect amplification, when we examine the change of the wavelength of the envelope crossover point in the spectrum with the magnetic field, we find that the magnetic field causes a small drift in the wavelength of the trough of the FPI1 spectrum, which will cause the wavelength drift of the envelope crossover point in the spectrum to be amplified by M times. M is the amplification factor of the wavelength drift, which is also the amplification factor of the magnetic field sensitivity, and it can be defined as:

[0039]

[0040] in, is the magnetic field sensitivity of the first harmonic vernier effect sensor.

[0041] In summary, a FPI1 that is sensitive to magnetic fields was designed using magnetic Terfenol-D powder material and FPI. Then, using the principle of optical harmonic vernier effect, a cascade structure of FPI1 and FPI2 was constructed to produce a harmonic vernier effect, forming a harmonic vernier effect magnetic field sensor, which can further amplify the magnetic field sensitivity and obtain a fiber optic magnetic field sensor that is extremely sensitive to magnetic field intensity.

[0042] The method of the present invention absorbs the advantages of existing sensors and overcomes their disadvantages. It utilizes quartz capillaries, single-mode optical fibers, Terfenol-D powder, epoxy resin glue, ultraviolet glue, FPI and the first harmonic cursor effect to produce an optical fiber magnetic field sensor with a particularly compact structure, easy production, easy packaging and high sensitivity. The sensor can be applied to magnetic field measurement in a narrow space and has good practical application value.

Claims

1. A method for manufacturing an optical fiber magnetic field sensor composed of Terfenol-D powder and FPI, characterized in that: The method comprises the following steps: The first step is to make a Fabry-Perot interferometer 1, or FPI1: take a large quartz capillary and burn off the protective layer on its surface with fire. Its inner diameter is 150 microns and its outer diameter is 360 microns. Then, insert two sections of single-mode optical fibers with their coatings stripped and their end faces cut flat into the large capillary from both ends, adjust the distance between the two single-mode optical fibers, and when the spectrum meets the requirements, use ultraviolet glue to glue the single-mode optical fiber and the large capillary together at both ends of the large capillary. Irradiate with an ultraviolet lamp for 1 minute, and glue the large capillary and the single-mode optical fiber together to form an FPI1. FPI1 is formed by the interference of reflected light from two reflection surfaces M1 and M2. The FP cavity of FPI1 is an air cavity with a length of L1. In the FPI1 structure, the length between the bonding points of the capillaries on both sides is L, and the single-mode optical fibers inserted from both sides of the capillary form a cantilever beam structure in the capillary. The second step is to evenly coat the Terfenol-D powder on the surface of the large capillary of FPI1 to form FPI1 that is sensitive to the magnetic field. Specifically, Terfenol-D powder and epoxy resin glue are first configured according to a powder-to-glue mass ratio of 95:5, that is, 95% Terfenol-D powder and 5% epoxy resin glue are mixed and stirred to form a uniform mixed colloid for standby use; then the configured Terfenol-D mixed glue is evenly coated on the outer surface of the large capillary in FPI1 to cover the entire outer surface of the large capillary; the prepared structure is first placed at room temperature for two hours, then placed in a drying oven at 40°C for 8 hours, and finally placed at room temperature for half a month to allow the coated material to dry completely; The third step is to make Fabry-Perot interferometer 2, or FPI2: take a small quartz capillary and burn off the protective layer on its surface with fire. Its inner diameter is 75 microns and its outer diameter is 125 microns. Then, use a fiber fusion splicer to fuse a section of single-mode optical fiber with its coating stripped and end face cut flat to the small quartz capillary. Use a fiber cleaver to cut the capillary to the designed length L2. Then, fuse another section of single-mode optical fiber with its coating stripped and end face flat to the other end of the small capillary. Finally, use a fiber cleaver to cut the end of the single-mode optical fiber into an inclined surface. In this way, the production of FPI2 is completed. FPI2 is formed by the interference of reflected light from the two reflection surfaces M3 and M4. The FP cavity of FPI2 is also an air cavity with a length of L2. In the fourth step, the single-mode optical fiber ends of FPI1 and FPI2 are welded together using a welding machine. The two FPIs are 5 mm to 1 cm apart. The two FPIs are cascaded to produce a first harmonic vernier effect sensor.

2. The method for manufacturing a fiber optic magnetic field sensor composed of Terfenol-D powder and FPI according to claim 1, characterized in that: The FPI1 and FPI2 are both extrinsic low-fineness FPIs.

3. The method for manufacturing a fiber optic magnetic field sensor composed of Terfenol-D powder and FPI according to claim 1, characterized in that: The diameter of the Terfenol-D powder in the second step is 100 microns to 150 microns.

4. The method for manufacturing a fiber optic magnetic field sensor composed of Terfenol-D powder and FPI according to claim 1, characterized in that: The thickness of the Terfenol-D mixed glue coating on the outer wall of the large capillary in the second step is maintained at 0.8 to 1.2 mm.

5. The method for manufacturing a fiber optic magnetic field sensor composed of Terfenol-D powder and FPI according to claim 1, characterized in that: The FP cavity length in FPI1 and FPI2 is L I and L2, L2 is approximately twice that of L1, and the reflectance spectra of the two FPIs have similar extinction ratios, and their free spectral ranges are approximately twice the relationship.

Citation Information

Patent Citations

  • Quartz capillary tube embedded all-silica fiber Fabry-Perot interferometric sensor and manufacturing method thereof

    CN102374874A

  • Temperature-insensitive magnetic field sensor based on magnetic fluid filling optical fiber microcavity

    CN106338702A

  • Double-magnetosensitive optical fiber magnetic field sensing probe with magnetofluid and magnetostrictive sleeve

    CN109932667A

  • High-sensitivity optical fiber magnetic field sensor based on optical vernier effect

    CN113805125A

  • Semi-fixed high-sensitivity optical fiber magnetic field sensor

    CN114397609A