Method for preparing double grooves in semiconductor device
By using a photomask to define and etch the mask layer in a semiconductor device to form a double trench structure, the problems of many process steps and high costs in the prior art are solved, and production efficiency and production capacity are improved.
Patent Information
- Application Number
- CN202411096046.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-19
AI Technical Summary
In the prior art, the preparation of MOSFET devices with dual trench structures requires two photocoats to define the line widths of the two sets of trenches in batches, resulting in the problems of many process steps, long production cycles, high costs and low production capacity.
Using a dual trench preparation method in a semiconductor device, the first mask is patterned by a photomask, the area to be etched by the main trench is defined, and the second mask layer is deposited on its surface to form a recess Structure, the second mask layer is etched to retain the side walls, as the area to be etched by the subtrench, and the remaining mask layer is removed, and the preparation of the main trench and the subtrench is completed.
The process steps are reduced, the preparation cost is reduced, the production efficiency is improved, and the preparation of double trenches is achieved through a photocoat is achieved, avoiding the complexity required to prepare two line width trenches in batches.
Smart Images

Figure CN118983340A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor preparation, and in particular to a method for preparing double trenches in a semiconductor device. Background Art
[0002] Trench MOSFET (trench metal oxide semiconductor field effect transistor) is a vertical structure MOSFET device, which is developed from the optimization of the traditional planar MOSFET structure. Because the trench of Trench MOSFET is deep inside the silicon substrate, more cells can be connected in parallel in design, thereby reducing the on-resistance, achieving greater current conduction and wider switching speed, and has the advantages of high input impedance and low conduction loss.
[0003] Currently, Trench MOSFET includes MOSFET devices with dual trench structures, that is, trenches with smaller line width and depth, and trenches with larger line width and depth. Currently, the preparation of MOSFET devices with dual trench structures generally requires the use of two masks to define the line widths of two groups of trenches in batches to form a dual trench structure. However, this preparation method has many process steps and a long production cycle, resulting in low production capacity and high cost.
[0004] Therefore, how to provide a preparation method that can reduce the production cycle and cost of a dual-trench MOSFET device and improve production efficiency is a technical problem that technical personnel in this field urgently need to solve. Summary of the invention
[0005] In view of this, the purpose of the present invention is to provide a method for preparing double trenches in a semiconductor device, which solves the problem that in the prior art, two masks are generally needed to prepare a MOSFET device with a double trench structure, and the line widths of two groups of trenches are defined in batches to form a double trench structure. However, this preparation method has many process steps and a long production cycle, resulting in low production capacity and high cost.
[0006] In order to solve the above technical problems, the present invention provides a method for preparing double trenches in a semiconductor device, comprising:
[0007] Providing a substrate having a first mask layer on its upper surface, and patterning the first mask layer using a photomask to define a main groove to be etched area;
[0008] Etching the area other than the to-be-etched area of the main trench defined in the first mask layer until the substrate is exposed to obtain a patterned first mask layer;
[0009] Depositing a second mask layer material on the surface of the patterned first mask layer to obtain a second mask layer; the second mask layer corresponds to the area of the substrate exposed by the patterned first mask layer, forming a recessed structure;
[0010] Etching the second mask layer until the second mask layer on the upper side of the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed, so as to obtain a sidewall of the second mask layer retained on the sidewall of the remaining first mask layer as a patterned second mask layer;
[0011] The area of the substrate exposed between the adjacent sidewalls of the second mask layer is used as the sub-groove etching area, and the patterned first mask layer is removed to expose the main groove etching area;
[0012] The substrate is etched along the area to be etched of the main groove and the area to be etched of the sub-groove to complete the preparation of the main groove and the sub-groove.
[0013] Optionally, depositing a second mask layer material on the surface of the patterned first mask layer to obtain the second mask layer includes:
[0014] A second mask layer material is deposited on the surface of the patterned first mask layer by using a chemical vapor deposition process to obtain a second mask layer.
[0015] Optionally, providing a substrate with a first mask layer disposed on its upper surface, and patterning the first mask layer using a photomask to define a main trench etching area, includes:
[0016] Providing a substrate having a first mask layer on its upper surface, and preparing a photoresist on the upper surface of the first mask layer;
[0017] The photoresist is exposed using a photomask to obtain a patterned photoresist to define the main groove to be etched area; the patterned photoresist is formed with a notch exposing the first mask layer corresponding to the main groove to be etched area;
[0018] The etching of the area outside the main trench to be etched area defined in the first mask layer until the substrate is exposed to obtain a patterned first mask layer includes:
[0019] The first mask layer is etched along the notch until the substrate is exposed, and the patterned photoresist is removed to obtain the patterned first mask layer.
[0020] Optionally, the step of exposing the photoresist with a photomask to obtain a patterned photoresist and define the main groove to be etched area includes:
[0021] The photoresist is exposed to yellow light using a photomask to obtain the patterned photoresist, thereby defining the main groove area to be etched.
[0022] Optionally, the first mask layer is an oxide mask layer, and the second mask layer is a silicon nitride mask layer.
[0023] Optionally, etching the first mask layer to obtain the patterned first mask layer, etching the second mask layer to obtain the patterned second mask layer, and etching the substrate to complete the preparation of the main groove and the sub-groove are all performed using a dry etching process.
[0024] Optionally, removing the patterned first mask layer to expose the main trench area to be etched includes:
[0025] The patterned first mask layer is removed by etching using a wet etching process to expose the main trench etching area.
[0026] Optionally, after the preparation of the main groove and the sub-groove is completed, the method further includes:
[0027] The remaining second mask layer is removed.
[0028] Optionally, etching the second mask layer until the second mask layer directly above the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed, obtaining a second mask layer sidewall retained on the sidewall of the remaining first mask layer as a patterned second mask layer; exposing the substrate area between adjacent second mask layer sidewalls as a sub-groove to be etched area, including:
[0029] Etching the second mask layer to obtain the sidewalls of the second mask layer as the patterned second mask layer;
[0030] The area between the adjacent sidewalls of the second mask layer, where the substrate is exposed after etching and adjustment according to the preset sub-groove line width, is used as the sub-groove to-be-etched area; the preset sub-groove line width is the theoretical sub-groove line width to be prepared.
[0031] Optionally, etching the second mask layer to obtain the second mask layer sidewalls as the patterned second mask layer; exposing the area of the substrate between adjacent second mask layer sidewalls after etching and adjusting according to a preset sub-groove line width as the sub-groove to-be-etched area, comprises:
[0032] Etching the second mask layer according to a preset sub-groove line width to obtain the second mask layer sidewall as the patterned second mask layer;
[0033] The area of the substrate exposed between adjacent sidewalls of the second mask layer is used as the etching area of the sub-groove after etching adjustment.
[0034] It can be seen that the method for preparing a double trench in a semiconductor device provided by the present invention comprises providing a substrate having a first mask layer disposed on its upper surface, and patterning the first mask layer using a photomask to define a main trench etching region, etching a region other than the main trench etching region defined in the first mask layer until the substrate is exposed to obtain a patterned first mask layer, and depositing a second mask layer material on the surface of the patterned first mask layer to obtain a second mask layer, the second mask layer corresponding to the region of the substrate exposed by the patterned first mask layer, to form There is a recessed structure, and the second mask layer is etched until the second mask layer on the upper side of the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed, so as to obtain the second mask layer side wall retained on the side wall of the remaining first mask layer, which is used as a patterned second mask layer, and the area of the substrate exposed between adjacent second mask layer side walls is used as the sub-groove to be etched area, and the patterned first mask layer is removed to expose the main groove to be etched area, and the substrate is etched along the main groove to be etched area and the sub-groove to be etched area to complete the preparation of the main groove and the sub-groove. The present invention uses a photomask to prepare a graphic first mask layer, and only retains the first mask layer in the area to be etched corresponding to the main groove, and prepares the second mask layer side wall on the side of the retained first mask layer, and forms a sub-groove to be etched area exposing the substrate between the two main grooves to be etched and the two corresponding second mask layer side walls, and then removes the remaining first mask layer in the area to be etched of the main groove, and etches the substrate based on the area not blocked by the second mask layer side wall, so as to complete the preparation of double grooves by using a photomask, without using two photomasks to prepare grooves of two line widths in batches, thereby reducing the process steps, reducing the preparation cost, and improving the production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.
[0036] Figure 1 A flow chart of a method for preparing a double trench in a semiconductor device provided by an embodiment of the present invention;
[0037] Figures 2 to 7 An exemplary flow chart of a method for preparing a double trench in a semiconductor device provided by an embodiment of the present invention;
[0038] Figure 8 A flow chart of another method for preparing double trenches in a semiconductor device provided by an embodiment of the present invention;
[0039] Figures 2 to 7 In the figure, the reference numerals are described as follows:
[0040] 10-substrate, 20-first mask layer, 21-patterned first mask layer, 30-patterned photoresist, 40-second mask layer, 41-recess structure, 42-patterned second mask layer, 50-main groove area to be etched, 51-main groove, 60-sub-groove area to be etched, 61-sub-groove. DETAILED DESCRIPTION
[0041] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0042] Embodiment 1:
[0043] Please refer to Figure 1 , Figure 1 A flowchart of a method for preparing a double trench in a semiconductor device provided by an embodiment of the present invention. The method may include:
[0044] S101: providing a substrate 10 having a first mask layer 20 disposed on its upper surface, and patterning the first mask layer 20 using a photomask to define a main trench etching area.
[0045] In this embodiment, step S101 may be specifically referred to Figure 2 . The patterned photoresist 30 is used to define the area to be etched of the main groove and form a shielding protection. In this embodiment, a first mask layer 20 is prepared on the upper surface of the substrate 10, and the first mask layer 20 is patterned using a photomask to define the area corresponding to the first mask layer 20 where the main groove needs to be etched, wherein the first mask layer 20 defining the area to be etched of the main groove needs to be retained at this moment, and the first mask layer 20 in the area outside the area to be etched of the main groove needs to be removed later. In addition, the present invention is explained by taking the surface of the regular substrate 10 where the groove needs to be prepared as an example to be set upward. After the spatial position of the substrate 10 changes, the specifically described orientation should be adaptively changed, for example, it can be outward along the direction of the groove to be etched corresponding to the direction of the upper side in the present invention.
[0046] The present embodiment does not limit the specific method of defining the main groove area to be etched, as long as the first mask layer 20 outside the main groove area to be etched can be removed in the subsequent preparation steps. For example, a protective layer may be prepared only on the upper side of the first mask layer 20 in the main groove area to be etched to prevent the first mask layer 20 in the main groove area to be etched from being removed, or the properties of the first mask layer 20 in the main groove area to be etched may be changed to make the first mask layer 20 in the main groove area to be etched less likely to be etched, or the properties of the first mask layer 20 outside the main groove area to be etched may be changed to make the first mask layer 20 outside the main groove area to be etched easier to be etched. In addition, the present invention does not limit the specific material of the first mask layer 20 and the specific material of the substrate 10, as long as the preparation of the double trench semiconductor device can be completed.
[0047] S102 : etching the area other than the to-be-etched area of the main trench defined in the first mask layer 20 until the substrate 10 is exposed, thereby obtaining a patterned first mask layer 21 .
[0048] In this embodiment, step S102 may be specifically referred to in Figure 3 In this embodiment, the area outside the main groove to be etched area defined in the first mask layer 20 is etched, and the etching is continued until the substrate 10 is exposed, that is, the portion of the first mask layer 20 corresponding to the main groove to be etched area is retained to form a blocking protection for the area of the substrate 10 where the main groove needs to be etched, and the substrate 10 in the area where the main groove does not need to be etched is exposed as the above-mentioned patterned first mask layer 21.
[0049] Further, in order to ensure the preparation efficiency of the patterned first mask layer 21, the above-mentioned substrate 10 is provided with the first mask layer 20 on the upper surface, and the first mask layer 20 is patterned by using a photomask to define the main groove to be etched area, which may include:
[0050] Step S11: providing a substrate 10 having a first mask layer 20 disposed on its upper surface, and preparing a photoresist on the upper surface of the first mask layer 20;
[0051] Step S12: using a photomask to expose the photoresist to obtain a patterned photoresist 30, and completing the definition of the main groove to be etched area; the patterned photoresist 30 forms a gap exposing the first mask layer 20 corresponding to the main groove to be etched area;
[0052] Etching the area outside the main trench to be etched area defined in the first mask layer 20 until the substrate 10 is exposed to obtain the patterned first mask layer 21 may include:
[0053] Step S13 : etching the first mask layer 20 along the notch until the substrate 10 is exposed, and removing the patterned photoresist 30 to obtain a patterned first mask layer 21 .
[0054] It should be noted that, in this embodiment, a photoresist is prepared on the upper surface of the first mask layer 20, and the photoresist is exposed to obtain a patterned photoresist 30, and the first mask layer 20 is etched based on the first mask layer 20 exposed by the patterned photoresist 30 to obtain a patterned first mask layer 21, which can reduce the complexity of preparing the patterned first mask layer 21. In this embodiment, the photoresist can be exposed to obtain the patterned photoresist 30 by using a self-alignment process through a photomask.
[0055] Further, in order to improve the efficiency of preparing the patterned photoresist 30 using one photomask, the above-mentioned exposure process of the photoresist using one photomask to obtain the patterned photoresist 30 and complete the definition of the main groove to be etched area may include:
[0056] A photomask is used to expose the photoresist with yellow light to obtain a patterned photoresist 30, thereby completing the definition of the main groove to be etched area.
[0057] In this embodiment, yellow light exposure is used to define the patterned photoresist 30, which facilitates the patterning preparation of the photoresist.
[0058] S103 : depositing a second mask layer material on the surface of the patterned first mask layer 21 to obtain a second mask layer 40 ; the second mask layer 40 corresponds to the region of the substrate 10 exposed by the patterned first mask layer 21 , forming a recessed structure 41 .
[0059] In this embodiment, step S103 can be specifically referred to Figure 4In this embodiment, the second mask layer material is directly deposited on the surface of the patterned first mask layer 21, and the second mask layer 40 is prepared by deposition. Since the patterned first mask layer 21 has a gap exposing the substrate 10 in the area other than the area to be etched corresponding to the main groove, when the second mask layer material is deposited, the second mask layer 40 has a recessed structure 41 in the area corresponding to the patterned first mask layer 21 where the substrate 10 is exposed. Naturally, the height of the second mask layer 40 deposited on the surface of the remaining first mask layer in the patterned first mask layer 21 is higher than the height of the second mask layer 40 at the recessed structure 41, and a second mask layer sidewall is formed between the remaining first mask layer in the patterned first mask layer 21 and the recessed structure 41, which is upward from the substrate 10 and flush with the second mask layer 40 deposited on the surface of the remaining first mask layer, that is, the second mask layer 40 deposited in the area where the substrate 10 is exposed in the patterned first mask layer 21 is a concave mask layer structure. It should be noted that, since deposition is generally performed on the entire surface, the corners of the concave structure of the concave mask layer structure are mostly rounded corners. This embodiment also does not limit the specific material of the second mask layer 40, as long as the etching resistance is different from that of the first mask layer 20, the first mask layer 20 and the second mask layer 40 can be etched separately.
[0060] Further, in order to ensure the convenience of preparing the second mask layer 40, the above-mentioned depositing the second mask layer material on the surface of the patterned first mask layer 21 to obtain the second mask layer 40 may include:
[0061] The second mask layer material is deposited on the surface of the patterned first mask layer 21 by using a chemical vapor deposition process to obtain the second mask layer 40 .
[0062] It should be noted that in this embodiment, a chemical vapor deposition process is used to deposit and prepare the second mask layer 40 on the surface of the patterned first mask layer 21, so as to form a concave-shaped second mask layer structure in the exposed area corresponding to the substrate 10, and it is more convenient to control the preparation amount, thereby improving the convenience of preparation.
[0063] S104: Etching the second mask layer 40 until the second mask layer directly above the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed, to obtain the second mask layer sidewalls retained on the sidewalls of the remaining first mask layer as a patterned second mask layer 42.
[0064] In this embodiment, step S104 may be specifically referred to Figure 5. In the present embodiment, the second mask layer 40 is etched, and the second mask layer on the upper side of the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed during etching. At this time, since the thickness of the bottom surface of the recessed structure 41 is relatively thin, the second mask layer of a partial width removed in the recessed structure 41 should appear in the bottom surface of the recessed structure 41. In the present embodiment, the width of the second mask layer of a partial width removed in the recessed structure 41 is the width along the lateral direction, that is, the second mask layer located beside the remaining first mask layer and located within the above-mentioned partial width range are all removed to expose the substrate 10 of a partial width. For example, in the present embodiment, anisotropic etching can be used to etch the second mask layer 40 only in the direction from top to bottom to obtain the above-mentioned patterned second mask layer 42.
[0065] S105 : using the area of the substrate 10 exposed between the adjacent second mask layer sidewalls as the sub-trench to-be-etched area 60 , removing the patterned first mask layer 21 , and exposing the main trench to-be-etched area 50 .
[0066] In this embodiment, step S105 can be specifically referred to Figure 6 . It should be noted that, in this embodiment, the area where the substrate 10 is exposed between the adjacent second mask layer side walls can be used as the sub-groove to-be-etched area 60, and the adjacent second mask layer side walls are located in a continuous area between two adjacent remaining first mask layers, and are relatively arranged on the side of the remaining first mask layer. In this embodiment, after obtaining the sub-groove to-be-etched area 60, the patterned first mask layer 21 can be removed, that is, the remaining first mask layer can be removed to expose the main groove to-be-etched area 50 covered by the remaining first mask layer. At this time, the definition of the to-be-etched areas of the main groove and the sub-groove of two different line widths is completed simultaneously through one photomask, and the second mask layer side walls are used to shield and protect the areas that do not need to be etched.
[0067] Furthermore, in order to ensure the cleanliness of the exposed main trench area 50 to be etched and improve the preparation efficiency, the above-mentioned removal of the patterned first mask layer 21 to expose the main trench area 50 to be etched may include:
[0068] The patterned first mask layer 21 is removed by etching using a wet etching process to expose the main trench etching area 50 .
[0069] It should be noted that, in this embodiment, the patterned first mask layer 21 is removed by etching using a wet etching process, which can ensure the removal rate, avoid the existence of residual impurities, and improve the removal efficiency.
[0070] S106 : etching the substrate 10 along the main trench to-be-etched region 50 and the sub-trench to-be-etched region 60 , and completing the preparation of the main trench 51 and the sub-trench 61 .
[0071] In this embodiment, step S106 may be specifically referred to Figure 7 In this embodiment, after the main groove area to be etched 50 and the sub-groove area to be etched 60 are defined, the substrate 10 can be directly etched along the defined main groove area to be etched 50 and the sub-groove area to be etched 60 to complete the preparation of the main groove 51 and the sub-groove 61. Since the line width of the main groove area to be etched 50 and the line width of the sub-groove area to be etched 60 in this embodiment are different, the etching rate of the main groove 51 with a larger line width is faster, so direct etching can achieve the preparation of the main groove 51 and the sub-groove 61 of different depths.
[0072] Furthermore, in order to ensure the smooth preparation of the double trench semiconductor device, the first mask layer 20 may be set as an oxide mask layer, and the second mask layer 40 may be set as a silicon nitride mask layer.
[0073] It should be noted that in this embodiment, the first mask layer 20 is set as an oxide mask layer, and the second mask layer 40 is set as a silicon nitride mask layer, which can ensure the graphical preparation of the first mask layer 20 and the second mask layer 40 respectively, and can serve as etching stop layers between each other to improve the preparation efficiency.
[0074] Furthermore, in order to ensure the completion of the specified graphical preparation, the above-mentioned etching of the first mask layer 20 to obtain the patterned first mask layer 21, etching of the second mask layer 40 to obtain the patterned second mask layer 42, and etching of the substrate 10 to complete the preparation of the main groove 51 and the sub-groove 61 can be set, all of which are etched using a dry etching process.
[0075] In this embodiment, dry etching is used to ensure the accuracy of pattern etching, thereby ensuring that the line widths of different grooves can be defined.
[0076] Furthermore, in order to facilitate subsequent preparation, after the preparation of the main groove 51 and the sub-groove 61 is completed, the following steps may be further included:
[0077] The remaining second mask layer is removed.
[0078] It should be noted that in order to facilitate the subsequent preparation of other components and avoid obstruction caused by the remaining second mask layer, the remaining second mask layer can be directly removed after the preparation of the main groove 51 and the sub-groove 61 is completed.
[0079] The method for preparing a double trench in a semiconductor device provided by an embodiment of the present invention comprises providing a substrate 10 having a first mask layer 20 disposed on its upper surface, and patterning the first mask layer 20 using a photomask to define a main trench etching region 50, etching an area other than the main trench etching region 50 defined in the first mask layer 20 until the substrate 10 is exposed to obtain a patterned first mask layer 21, and depositing a second mask layer material on the surface of the patterned first mask layer 21 to obtain a second mask layer 40, wherein the second mask layer 40 corresponds to an area of the substrate 10 exposed by the patterned first mask layer 21, and forming a A recessed structure 41 is formed, and the second mask layer 40 is etched until the second mask layer on the upper side of the remaining first mask layer and the second mask layer of a partial width in the recessed structure 41 are removed, so as to obtain the second mask layer sidewalls retained on the sidewalls of the remaining first mask layer as the patterned second mask layer 42, and the area of the substrate 10 exposed between adjacent second mask layer sidewalls is used as the sub-groove etching area 60, and the patterned first mask layer 21 is removed to expose the main groove etching area 50, and the substrate 10 is etched along the main groove etching area 50 and the sub-groove etching area 60 to complete the preparation of the main groove 51 and the sub-groove 61. The present invention uses a photomask to prepare a patterned first mask layer 21, and only retains the first mask layer 20 in the corresponding main groove to-be-etched area 50, and prepares the second mask layer side wall on the side of the retained first mask layer 20, and between the two main groove to-be-etched areas 50 and the corresponding two second mask layer side walls, a sub-groove to-be-etched area 60 exposing the substrate 10 is formed, and then the remaining first mask layer 20 at the main groove to-be-etched area 50 is removed, and the substrate 10 is etched based on the area not blocked by the second mask layer side wall, so as to complete the preparation of the double grooves by using a photomask, without using two photomasks to prepare grooves of two line widths in batches, thereby reducing the process steps, reducing the preparation cost, and improving the production efficiency.
[0080] In addition, the embodiment of the present invention prepares a photoresist on the upper surface of the first mask layer 20, and exposes the photoresist to obtain a patterned photoresist 30, and etches the first mask layer 20 based on the first mask layer 20 exposed by the patterned photoresist 30 to obtain a patterned first mask layer 21, which can reduce the complexity of preparing the patterned first mask layer 21; the patterned photoresist 30 is defined by yellow light exposure, which is convenient for patterning the photoresist; the second mask layer 40 is deposited on the surface of the patterned first mask layer 21 by a chemical vapor deposition process, so as to form a concave-shaped second mask layer structure in the exposed area of the corresponding substrate 10, and it is more convenient to control the preparation amount. The convenience of preparation is improved; the wet etching process is used to etch and remove the patterned first mask layer 21, which can ensure the removal rate, avoid the existence of residual impurities, and improve the removal efficiency; the first mask layer 20 is set as an oxide mask layer, and the second mask layer 40 is set as a silicon nitride mask layer, which can ensure the patterned preparation of the first mask layer 20 and the second mask layer 40 respectively, and can serve as etching stop layers to improve the preparation efficiency; dry etching is used to ensure the accuracy of patterned etching, and then ensure that the line width of different grooves can be defined; after completing the preparation of the main groove 51 and the sub-groove 61, the remaining second mask layer 40 is directly removed to facilitate subsequent preparation.
[0081] Embodiment 2:
[0082] Please refer to Figure 8 , Figure 8 A flow chart of another method for preparing a double trench in a semiconductor device provided by an embodiment of the present invention. The method may include:
[0083] S201: providing a substrate with a first mask layer disposed on its upper surface, and patterning the first mask layer using a photomask to define a main trench etching area.
[0084] S202: etching the area outside the main trench to-be-etched area defined in the first mask layer until the substrate is exposed to obtain a patterned first mask layer.
[0085] S203: depositing a second mask layer material on the surface of the patterned first mask layer to obtain a second mask layer; the second mask layer corresponds to the region of the substrate exposed by the patterned first mask layer, forming a recessed structure.
[0086] S204: etching the second mask layer to obtain a second mask layer sidewall as a patterned second mask layer.
[0087] It should be noted that in this embodiment, the second mask layer is etched until the second mask layer directly above the remaining first mask layer and the second mask layer of partial width in the recessed structure are removed, so as to obtain the second mask layer sidewalls retained on the sidewalls of the remaining first mask layer as a patterned second mask layer.
[0088] S205: Exposing the area of the substrate between the adjacent second mask layer sidewalls after etching and adjusting according to the preset sub-trench line width as the sub-trench to-be-etched area; the preset sub-trench line width is the theoretical sub-trench line width to be prepared.
[0089] In this embodiment, the spacing between adjacent second mask layer sidewalls is etched and adjusted according to the preset sub-trench line width, for example, etching adjacent second mask layer sidewalls can achieve custom setting of the sub-trench line width, thereby improving the flexible control of the sub-trench line width.
[0090] S206: removing the patterned first mask layer to expose the main trench area to be etched.
[0091] S207: etching the substrate along the area to be etched in the main groove and the area to be etched in the sub-groove, completing the preparation of the main groove and the sub-groove.
[0092] Further, in order to improve the adjustment efficiency of the sub-groove line width, the second mask layer is etched to obtain the second mask layer sidewall as a patterned second mask layer; the area between the adjacent second mask layer sidewalls, which is exposed after etching and adjusting according to the preset sub-groove line width, is used as the sub-groove to-be-etched area, which may include:
[0093] Step S21: etching the second mask layer according to a preset sub-trench line width to obtain a second mask layer sidewall as a patterned second mask layer;
[0094] Step S22: using the area of the substrate exposed between the adjacent sidewalls of the second mask layer as the sub-trench etching area after etching adjustment.
[0095] It should be noted that in this embodiment, when etching the second mask layer, the etching time can be controlled according to the preset sub-groove line width to obtain a substrate exposed area with a composite preset sub-groove line width, and then obtain an etched sub-groove area to be etched after the etching adjustment.
[0096] By using the method for preparing a double trench in a semiconductor device provided by an embodiment of the present invention, the spacing between adjacent sidewalls of the second mask layer is adjusted by etching according to a preset sub-trench line width, so that the sub-trench line width can be customized, thereby improving the flexible control of the sub-trench line width. In addition, according to the preset sub-trench line width, the embodiment of the present invention controls the etching time to obtain a substrate exposed area with a composite preset sub-trench line width, and then obtains an etching-adjusted sub-trench to-be-etched area, thereby improving the adjustment efficiency of the sub-trench line width.
[0097] In an application scenario embodiment, the method for preparing the double trenches in the semiconductor device may specifically include the following steps:
[0098] Step 1: deposit an oxide mask layer on the upper surface of the silicon epitaxial wafer, and spin-coat photoresist, use a photomask, expose the photoresist with yellow light to obtain a patterned photoresist, and complete the definition of the main groove to be etched area; the patterned photoresist forms a gap exposing the first mask layer corresponding to the main groove to be etched area.
[0099] Step 2: Etching the first mask layer along the notch until the substrate is exposed, and removing the patterned photoresist to obtain a patterned first mask layer.
[0100] Step three: using a chemical vapor deposition process to deposit a second mask layer material on the surface of the patterned first mask layer to obtain a second mask layer; the second mask layer corresponds to the region of the substrate exposed by the patterned first mask layer to form a recessed structure.
[0101] Step 4: Use a dry etching process to etch the second mask layer according to the preset sub-groove line width until the second mask layer directly above the remaining first mask layer and the second mask layer with the preset sub-groove line width in the recessed structure are removed, thereby obtaining the second mask layer sidewalls retained on the sidewalls of the remaining first mask layer as a patterned second mask layer.
[0102] Step 5: Exposing the area of the substrate between the adjacent second mask layer sidewalls after etching and adjusting according to the preset sub-groove line width as the sub-groove to be etched area; the preset sub-groove line width is the theoretical sub-groove line width to be prepared.
[0103] Step six: using a wet etching process to remove the patterned first mask layer to expose the main trench area to be etched.
[0104] Step seven: etching the substrate along the main trench to be etched area and the sub-trench to be etched area, completing the preparation of the main trench and the sub-trench, and removing the remaining second mask layer.
[0105] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0106] Professionals may further appreciate that the units and algorithm steps of each example described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, computer software, or a combination of the two. In order to clearly illustrate the interchangeability of hardware and software, the composition and steps of each example have been generally described in the above description according to function. Whether these functions are performed in hardware or software depends on the specific application and design constraints of the technical solution. Professionals and technicians may use different methods to implement the described functions for each specific application, but such implementation should not be considered to be beyond the scope of the present invention.
[0107] Finally, it should be noted that, in this article, relationships such as first and second, etc. are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprises" or any other variations are intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0108] The above is a detailed introduction to the method for preparing a double trench in a semiconductor device provided by the present invention. Specific examples are used in this article to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for those skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.
Claims
1. A method for preparing a double trench in a semiconductor device, characterized in that: include: Providing a substrate having a first mask layer on its upper surface, and patterning the first mask layer using a photomask to define a main groove to be etched area; Etching the area other than the to-be-etched area of the main trench defined in the first mask layer until the substrate is exposed to obtain a patterned first mask layer; Depositing a second mask layer material on the surface of the patterned first mask layer to obtain a second mask layer; The second mask layer corresponds to the area of the substrate exposed by the patterned first mask layer, forming a recessed structure; Etching the second mask layer until the second mask layer on the upper side of the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed, so as to obtain a sidewall of the second mask layer retained on the sidewall of the remaining first mask layer as a patterned second mask layer; The area of the substrate exposed between the adjacent sidewalls of the second mask layer is used as the sub-groove etching area, and the patterned first mask layer is removed to expose the main groove etching area; The substrate is etched along the area to be etched of the main groove and the area to be etched of the sub-groove to complete the preparation of the main groove and the sub-groove.
2. The method for preparing a double trench in a semiconductor device according to claim 1, characterized in that: The step of depositing a second mask layer material on the surface of the patterned first mask layer to obtain a second mask layer comprises: A second mask layer material is deposited on the surface of the patterned first mask layer by using a chemical vapor deposition process to obtain a second mask layer.
3. The method for preparing a double trench in a semiconductor device according to claim 1, characterized in that: The method of providing a substrate with a first mask layer on its upper surface and patterning the first mask layer using a photomask to define a main groove etching area includes: Providing a substrate having a first mask layer on its upper surface, and preparing a photoresist on the upper surface of the first mask layer; The photoresist is exposed using a photomask to obtain a patterned photoresist to define the main groove to be etched area; the patterned photoresist is formed with a notch exposing the first mask layer corresponding to the main groove to be etched area; The etching of the area outside the main trench to be etched area defined in the first mask layer until the substrate is exposed to obtain a patterned first mask layer includes: The first mask layer is etched along the notch until the substrate is exposed, and the patterned photoresist is removed to obtain the patterned first mask layer.
4. The method for preparing double trenches in a semiconductor device according to claim 3, characterized in that: The method of using a photomask to expose the photoresist to obtain a patterned photoresist and define the main groove to be etched area includes: The photoresist is exposed to yellow light using a photomask to obtain the patterned photoresist, thereby defining the main groove area to be etched.
5. The method for preparing double trenches in a semiconductor device according to claim 1, characterized in that: The first mask layer is an oxide mask layer, and the second mask layer is a silicon nitride mask layer.
6. The method for preparing double trenches in a semiconductor device according to claim 1, characterized in that: The etching of the first mask layer to obtain the patterned first mask layer, the etching of the second mask layer to obtain the patterned second mask layer, and the etching of the substrate to complete the preparation of the main groove and the sub-groove are all performed by dry etching process.
7. The method for preparing double trenches in a semiconductor device according to claim 1, characterized in that: Removing the patterned first mask layer to expose the main trench area to be etched, comprising: The patterned first mask layer is removed by etching using a wet etching process to expose the main trench etching area.
8. The method for preparing double trenches in a semiconductor device according to claim 1, characterized in that: After the preparation of the main groove and the sub-groove is completed, it also includes: The remaining second mask layer is removed.
9. The method for preparing a double trench in a semiconductor device according to any one of claims 1 to 8, characterized in that: Etching the second mask layer until the second mask layer on the upper side of the remaining first mask layer and the second mask layer of a partial width in the recessed structure are removed, so as to obtain a sidewall of the second mask layer retained on the sidewall of the remaining first mask layer as a patterned second mask layer; The method further comprises: exposing the substrate area between adjacent sidewalls of the second mask layer as a sub-groove to be etched area, comprising: Etching the second mask layer to obtain the sidewalls of the second mask layer as the patterned second mask layer; The area between the adjacent sidewalls of the second mask layer, where the substrate is exposed after etching and adjustment according to the preset sub-groove line width, is used as the sub-groove to-be-etched area; the preset sub-groove line width is the theoretical sub-groove line width to be prepared.
10. The method for preparing double trenches in a semiconductor device according to claim 9, characterized in that: The etching of the second mask layer to obtain the sidewalls of the second mask layer as the patterned second mask layer; The area between the adjacent sidewalls of the second mask layer, where the area of the substrate is exposed after etching and adjustment according to the preset sub-groove line width, is used as the sub-groove to-be-etched area, including: Etching the second mask layer according to a preset sub-groove line width to obtain the second mask layer sidewall as the patterned second mask layer; The area of the substrate exposed between adjacent sidewalls of the second mask layer is used as the etching area of the sub-groove after etching adjustment.