Makeup film pasting processing method

Through the manual splicing film processing method, the side-by-side placement and cutting technology of edge strips and plates is used to solve the problem that vacuum film equipment cannot process small-sized boards, improve the processing capacity and utilization rate of the equipment, simplify the process, and improve the process. Productivity.

CN118984540APending Publication Date: 2024-11-19珠海杰赛科技有限公司 +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411186922.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The existing vacuum film patching equipment cannot effectively process imposition-sized plates with less than 152mm×250mm, resulting in the inability to simplify the wire method gold plating process, shorten the processing cycle, and affect production efficiency and equipment utilization.

Method used

Using manual splicing of the patch film processing method, by selecting the same length as the plate, the sum of the widths of the edge strips and the plate is greater than or equal to 250mm, and place them side by side in the vacuum film equipment for filming, and the film is finished. Cut the rear edge splicing gap to improve the minimum processing size capability and utilization of the equipment.

Benefits of technology

The minimum processing size capability and equipment utilization rate of vacuum film equipment are improved, the process of special process products is simplified, the processing cycle is shortened, and the processing efficiency is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118984540A_ABST
    Figure CN118984540A_ABST
Patent Text Reader

Abstract

The invention discloses a makeup film pasting processing method, and belongs to the technical field of PCB film pasting processing, and the method comprises the steps: selecting the length of an edge strip according to the length of a plate, and enabling the length of the edge strip to be equal to the length of the plate; the width of the edging is selected, and the sum of the width of the edging and the width of the plate is larger than or equal to 250 mm; the edgings and the plate are placed into vacuum film pasting equipment side by side for film pasting; and after film pasting is completed, the edge strips are taken down, and plate film pasting is completed. According to the makeup film pasting processing method, a manual splicing mode is adopted for processing, so that the minimum size capability of equipment processing and the equipment utilization rate are improved. The process and the processing period of special process products are simplified, and the processing efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of PCB film pasting processing, and in particular to a PCB film pasting processing method. Background Art

[0002] PCB conductor gold plating is an electroplating process that is usually used to coat a layer of metal on the conductors (usually copper) on the surface of a PCB or inside a perforation to enhance conductivity and anti-oxidation properties.

[0003] In order to simplify the wire method gold plating process, shorten the processing cycle and improve production efficiency, a vacuum laminating machine is introduced to replace the wet film cover wire process. Affected by the utilization rate and cost of the board material, the design of the wire method gold plating process has a relatively small panel size (the minimum panel size is 152mm×152mm), which exceeds the minimum processing size of the vacuum laminating equipment (152mm×250mm) and accounts for 30% of the wire method gold plating process drawing number. As a result, the panel number with a panel size of less than 152mm×250mm cannot be produced using the vacuum laminating machine, which fails to meet the requirements of simplifying the wire method gold plating process and shortening the processing cycle. Summary of the invention

[0004] The purpose of the present invention is to solve at least one of the technical problems existing in the prior art. To this end, the present invention proposes a plate-making film processing method, which can improve the processing size capacity and equipment utilization rate of vacuum film-making equipment, while increasing the proportion of process and processing cycle reduction of special process products.

[0005] The method for processing a laminated film according to an embodiment of the present invention includes:

[0006] Step 1: Select the length of the edge strip according to the length of the panel so that the length of the edge strip is the same as the length of the panel;

[0007] Step 2: Select the width of the edge strip so that the sum of the width of the edge strip and the panel is greater than or equal to 250mm;

[0008] Step 3: Place the edge strips and panels side by side in the vacuum laminating equipment for laminating;

[0009] Step 4: After the film is applied, remove the edge strips to complete the film application on the panel.

[0010] The method for processing the plate-joining film according to the embodiment of the present invention has at least the following beneficial effects: the method for processing the plate-joining film adopts manual splicing, which improves the minimum size capability and equipment utilization rate of the equipment processing, simplifies the process and processing cycle of special process products, and improves the processing efficiency.

[0011] According to some embodiments of the present invention, the thickness of the edge strip is smaller than the thickness of the panel.

[0012] According to some embodiments of the present invention, the difference between the thickness of the panel and the thickness of the edge strip is less than 0.5 mm.

[0013] According to some embodiments of the present invention, in step 3, when the edge strips and the panels are placed into the vacuum laminating device, the length of the edge strips is consistent with the length of the panels in the conveying direction.

[0014] According to some embodiments of the present invention, in step 3, the side strips and the panel are placed side by side along the width direction, and the side strips and the panel are close to each other but not fixed to each other.

[0015] According to some embodiments of the present invention, in step 4, after the film is applied, the film is cut along the joint gap between the panel and the edge strip.

[0016] According to some embodiments of the present invention, in step 4, the film is cut manually with a blade along the joint gap between the panel and the edge strip.

[0017] According to some embodiments of the present invention, in step 4, the film is cut along the joint gap between the board and the edge strip by an automatic cutting device.

[0018] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention is further described below in conjunction with the accompanying drawings and embodiments:

[0020] Figure 1 It is a flow chart of the method for processing a plate-making film according to an embodiment of the present invention. DETAILED DESCRIPTION

[0021] This section will describe in detail the specific embodiments of the present invention. The preferred embodiments of the present invention are shown in the accompanying drawings. The purpose of the accompanying drawings is to supplement the description of the text part of the specification with graphics, so that people can intuitively and vividly understand each technical feature and the overall technical solution of the present invention, but it cannot be understood as a limitation on the scope of protection of the present invention.

[0022] In the description of the present invention, it should be understood that descriptions involving orientations, such as up, down, front, back, left, right, etc., and orientations or positional relationships indicated are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0023] In the description of the present invention, "several" means one or more, "more" means more than two, "greater than", "less than", "exceed" etc. are understood as not including the number itself, and "above", "below", "within" etc. are understood as including the number itself. If there is a description of "first" or "second", it is only used for the purpose of distinguishing the technical features, and cannot be understood as indicating or implying the relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.

[0024] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.

[0025] refer to Figure 1 A method for processing a laminated film according to an embodiment of the present invention is described.

[0026] like Figure 1 As shown, the method for processing a laminated film according to an embodiment of the present invention includes:

[0027] Step 1: Select the length of the edge strip according to the length of the panel so that the length of the edge strip is the same as the length of the panel;

[0028] Step 2: Select the width of the edge strip so that the sum of the width of the edge strip and the panel is greater than or equal to 250mm;

[0029] Step 3: Place the edge strips and panels side by side in the vacuum laminating equipment for laminating;

[0030] Step 4: After the film is applied, remove the edge strips to complete the film application on the panel.

[0031] When selecting the edge strips in step 1 and step 2, it is also necessary to note that the thickness of the edge strip is less than the thickness of the radius, and the difference between the thickness of the panel and the edge strip is less than 0.5mm. If the edge strip is thicker than the panel, the panel will be less stressed during film application, resulting in an unstable film application. At the same time, the height difference between the panel and the edge strip should not be too large, so the thickness of the edge strip is 0 to 0.5mm less than the thickness of the panel.

[0032] In step 3, when the edge strips and the panels are placed in the vacuum laminating equipment, the length of the edge strips is consistent with the length of the panels in the conveying direction. The edge strips and the panels are placed side by side in the width direction, and the edge strips and the panels are close to each other but not fixed to each other.

[0033] In step 4, after the film is applied, the film is cut along the joint gap between the panel and the edge strip. Depending on the processing conditions, it is cut manually with a blade or automatically with a cutting device.

[0034] The following is a specific processing example to illustrate the present method of processing a laminated film:

[0035] The minimum width of the center baffle of the vacuum laminating equipment is 250mm, but the width of the board is less than 250mm, so it cannot be centered. The laminating process cannot leave copper on the edge of the board, which affects the vacuum quality of the vacuum laminating stage and causes the laminating to be loose. Therefore, the existing laminating processing method cannot meet the processing requirements of the minimum board size of 152mm×250mm.

[0036] Select the edge strips according to the length and width of the board. The length of the edge strips is the same as the length of the board. The sum of the width of the edge strips and the board is greater than or equal to 250mm. Use manual splicing, use the edge strips to make a plate and pass the film pasting machine. Put the edge strips and the board side by side in the vacuum film pasting equipment for film pasting. The length of the edge strips is consistent with the length of the board in the conveying direction. The edge strips and the board are placed side by side in the width direction. The edge strips and the board are close to each other but not fixed together. The thickness of the edge strips is 0 to 0.5mm less than the thickness of the board. After film pasting in the vacuum film pasting equipment, the film is cut along the splicing gap between the board and the edge strips by equipment or manually, and the edge strips are removed to complete the film pasting of small-sized boards.

[0037] Therefore, the present method for processing plate-making and film lamination adopts manual splicing, which improves the minimum size capability and equipment utilization rate of equipment processing, simplifies the process and processing cycle of special process products, and improves processing efficiency.

[0038] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the technical field without departing from the purpose of the present invention.

Claims

1. A method for processing a collage film, characterized in that: include: Step 1: Select the length of the edge strip according to the length of the panel so that the length of the edge strip is the same as the length of the panel; Step 2: Select the width of the edge strip so that the sum of the width of the edge strip and the panel is greater than or equal to 250mm; Step 3: Place the edge strips and panels side by side in the vacuum laminating equipment for laminating; Step 4: After the film is applied, remove the edge strips to complete the film application on the panel.

2. The method for processing the collage film according to claim 1, characterized in that: The thickness of the edge strip is less than the thickness of the plate.

3. The method for processing the collage film according to claim 2, characterized in that: The difference between the plate thickness and the edge strip thickness is less than 0.5 mm.

4. The method for processing the collage film according to claim 1, characterized in that: In step 3, when the edge strips and panels are placed in the vacuum laminating equipment, the length of the edge strips is consistent with the length of the panels in the conveying direction.

5. The method for processing the collage film according to claim 4, characterized in that: In step 3, the edge strips and the panels are placed side by side in the width direction, and the edge strips and the panels are close to each other but not fixed to each other.

6. The method for processing the collage film according to claim 5, characterized in that: In step 4, after the film is applied, the film is cut along the joint gap between the panel and the edge strip.

7. The method for processing the collage film according to claim 6, characterized in that: In step 4, the membrane is cut manually with a blade along the joint gap between the panel and the edge strip.

8. The method for processing the collage film according to claim 6, characterized in that: In step 4, the membrane is cut along the joint gap between the panel and the edge strip by an automatic cutting device.