Low-roughness optical module processing technology

By controlling the surface roughness of die-cast parts, and employing methods such as spark drilling with fine copper mesh, longitudinal light brushing with sponge sand, step-by-step sandblasting, and ordinary electroplating, the problem of achieving a surface roughness of less than Ra0.6 for optical modules was solved, resulting in cost reduction and improved production efficiency.

CN118990355AInactive Publication Date: 2024-11-22DONGGUAN XINGHE PRECISION DIECASTING MOLD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411121977.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing optical module processing technology makes it difficult to achieve a surface roughness of Ra0.6 or less without increasing electroplating costs and complexity. Traditional methods are costly and unstable.

Method used

By controlling the surface roughness of die-cast parts, the following methods are employed: sparking with fine copper mesh, longitudinal brushing with sponge sand, step-by-step sandblasting, and ordinary electroplating. Combined with the turnover of blister trays, the surface roughness is controlled to be below Ra0.6.

Benefits of technology

It reduced production costs, shortened electroplating time, and improved production efficiency and product quality stability.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a low-roughness optical module machining process, which comprises the following process steps of: A, preparing a material and a mold, sparking the mold by using a finest copper male screen plate, and controlling the surface roughness of a die casting to be Ra 0.4-0.7; b, the die casting is stamped, it is guaranteed that die casting blanking does not fall off, and water gap slag ladle blanking is conducted; c, the local surface of the die casting is longitudinally and slightly brushed with sponge sand, and the roughness of the local surface of the die casting is controlled to be Ra 0.4-0.5; d, the inner cavity and the outer surface of the die casting are subjected to two-step sand blasting treatment, the roughness of the inner cavity after sand blasting is controlled to be Ra1.6-3.2, and the roughness of the outer surface after sand blasting is controlled to be Ra0.8 or below; e, common electroplating treatment is conducted on the die casting, and the roughness of the outer surface of the die casting is controlled to be Ra0.6 or below; and F, carrying out spot check on roughness, flatness, width and thickness dimensions of a specified area of the die casting to obtain a qualified product. According to the invention, the surface roughness after final electroplating is less than Ra0.6 by adopting a process method for controlling the surface roughness of the die casting, so that the production cost is greatly reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of optical module processing, and in particular to a low-roughness optical module processing technology. Background Art

[0002] In 2024, the capital expenditure of global telecom operators in the optical communication industry will be approximately US$334 billion. The global optical communication industry will enter a new investment cycle. According to the forecast of market research organization Lightcounting, the global optical communication industry will maintain an annual growth rate of 15% in the next five years. Due to the active promotion of domestic national policies, it is expected that domestic optical communications will continue to show a rapid growth momentum at an average annual rate of at least 20% in the next five years, becoming the world's largest optical communication market. Affected by this environment, the domestic optical module market will usher in a booming development opportunity.

[0003] Although the requirements for the photoelectric transmission speed of optical modules are getting faster and faster, 400G and 800G have become the mainstream, and 1.2T and 1.5T have become the development direction. The rapid development of transmission speed has brought high process requirements to traditional die-cast optical modules, because the faster the transmission speed, the more serious the heat generation of the optical module products. If the heat is quickly dissipated, it is a difficult problem that needs to be solved in the optical module processing industry. The optical module shell contacts the surrounding cage. The finer the roughness of the contact surface between the optical mold block and the surrounding cage, the better the heat dissipation effect. However, how to make the surface of the optical module below Ra0.6 is a technical bottleneck in all optical module processing industries.

[0004] At present, large enterprises require the roughness of the local surface of high-end 400G optical modules to be below Ra0.6. Currently, only three optical module die-casting structural parts processing plants can meet this requirement. However, in order to meet the requirements, these two optical module die-casting structural parts processing plants use expensive electroplating pre-treatment solutions for reducing roughness, and the electroplated nickel layer is thickened. The total thickness of the copper layer is 10-20μm, and the total thickness of the nickel layer (including the nickel-phosphorus layer) is 8-18μm, of which the nickel-phosphorus layer is 2-4μm thick. According to this process, the electroplating cost is extremely high, which is three times the cost of traditional optical module electroplating. In addition, the process is complicated and difficult to control, and the quality is also unstable. Summary of the invention

[0005] The present invention provides a low-roughness optical module processing technology, which adopts a process method of controlling the surface roughness of a die-casting part to achieve a final surface roughness below Ra0.6 after electroplating, thereby greatly reducing the production cost.

[0006] To achieve the above object, the present invention adopts the following technical solutions:

[0007] A low-roughness optical module processing process includes the following process steps:

[0008] A. Prepare the materials and molds. The mold uses the finest copper mesh plate to spark and control the surface roughness of the die casting to Ra0.4-0.7;

[0009] B. Stamping die castings, ensure that the die castings do not fall and the slag bag at the nozzle does not fall;

[0010] C. Use sponge sand to lightly brush the local surface of the die casting longitudinally to control the local surface roughness of the die casting to Ra0.4-0.5;

[0011] D. The inner cavity and outer surface of the die casting are sandblasted in two steps. The roughness of the inner cavity after sandblasting is controlled within Ra1.6-3.2, and the roughness of the outer surface after sandblasting is controlled below Ra0.8;

[0012] E. Perform ordinary electroplating treatment on the die casting to control the outer surface roughness of the die casting to below Ra0.6;

[0013] F. Randomly inspect the roughness, flatness, width and thickness of designated areas of die castings to obtain qualified products.

[0014] Preferably, from step B to step F, a blister tray is used throughout the entire process to prevent collision and friction.

[0015] Preferably, in step C, 1000 mesh sponge sand is used to lightly brush longitudinally until the local surface of the die casting is brushed to a shine.

[0016] Preferably, in step D, 100# steel sand is used for sandblasting the inner cavity of the die casting at an air pressure of 2.0KG, and 240# steel sand is used for sandblasting the outer surface at an air pressure of 1.0KG.

[0017] Preferably, after the sandblasting treatment in step D, the outer surface of the die-casting is fully inspected. If there are scratches, it needs to be re-polished with 1000 mesh sponge sand and then re-sandblasted. After ensuring that the outer surface is qualified, it is circulated with a blister tray padded with copy paper to prevent collision and friction throughout the process.

[0018] Preferably, in step E, a commonly used ordinary electroplating chemical nickel process is adopted, Ni: 2.5-7um, Cu: 12-25um.

[0019] Compared with the prior art, the beneficial effects of the present invention are that there is no need to use expensive designated pre-treatment solutions and there is no need to increase the thickness of the electroplated nickel to ensure roughness, which greatly saves the electroplating cost and reduces the electroplating time by about 2 / 3, greatly improving the electroplating capacity and product production efficiency. DETAILED DESCRIPTION

[0020] The technical solutions in the embodiments of the present invention will be described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0021] It should be noted that when a component / part is referred to as being "set on" another component / part, it may be directly set on the other component / part or there may also be an intermediate component / part. When a component / part is referred to as being "connected / coupled" to another component / part, it may be directly connected / coupled to the other component / part or there may be an intermediate component / part at the same time. The term "connection / coupling" as used herein may include electrical and / or mechanical physical connections / couplings. The term "includes / comprising" as used herein refers to the presence of a feature, step or component / part, but does not exclude the presence or addition of one or more other features, steps or components / parts. The term "and / or" as used herein includes any and all combinations of one or more relevant listed items.

[0022] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein are only for the purpose of describing specific embodiments and are not intended to limit this application.

[0023] A low-roughness optical module processing process includes the following process steps:

[0024] A. Prepare the materials and molds. The mold uses the finest copper mesh plate to spark (No. 18 pattern) and the surface roughness of the die casting is controlled at Ra0.4-0.7;

[0025] B. Stamping die castings, ensure that the die castings do not fall and the slag at the nozzle does not fall; to the greatest extent possible, ensure that the die castings will not be damaged due to collision.

[0026] C. Use sponge sand to brush the local surface of the die casting lightly several times vertically to control the local surface roughness of the die casting to Ra0.4-0.5;

[0027] D. The inner cavity and outer surface of the die casting are sandblasted in two steps. The roughness of the inner cavity after sandblasting is controlled within Ra1.6-3.2, and the roughness of the outer surface after sandblasting is controlled below Ra0.8;

[0028] E. Perform ordinary electroplating treatment on the die casting to control the outer surface roughness of the die casting to below Ra0.6;

[0029] F. Randomly inspect the roughness, flatness, width and thickness of designated areas of die castings to obtain qualified products.

[0030] From step B to step F, the blister tray is used throughout the process to prevent collision and friction. In step C, 1000 mesh sponge sand is used to lightly brush the die casting surface longitudinally until the local surface is brushed to light. In step D, 100# steel sand is used for sandblasting the inner cavity of the die casting at an air pressure of 2.0KG, and 240# steel sand is used for sandblasting the outer surface at an air pressure of 1.0KG.

[0031] After the sandblasting treatment in step D, the outer surface of the die casting is fully inspected. If there are scratches, it needs to be re-polished with 1000 mesh sponge sand and re-sandblasted. After ensuring that the outer surface is qualified, it is turned over with a blister tray padded with copy paper to prevent collision and friction throughout the process. In step E, the commonly used ordinary electroplating chemical nickel process is adopted, Ni: 2.5-7um, Cu: 12~25um.

[0032] The present invention does not need to use expensive designated pre-treatment solutions and does not need to increase the thickness of the electroplated nickel to ensure roughness, which greatly saves the electroplating cost and reduces the electroplating time by about 2 / 3, greatly improving the electroplating capacity and product production efficiency.

[0033] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A low-roughness optical module processing technology, It is characterized in that The process steps include: A. Prepare the materials and molds. The mold uses the finest copper mesh plate to spark and control the surface roughness of the die casting to Ra0.4-0.7; B. Stamping die castings, ensure that the die castings do not fall and the slag bag at the nozzle does not fall; C. Use sponge sand to lightly brush the local surface of the die casting longitudinally to control the local surface roughness of the die casting to Ra0.4-0.5; D. The inner cavity and outer surface of the die casting are sandblasted in two steps. The roughness of the inner cavity after sandblasting is controlled within Ra1.6-3.2, and the roughness of the outer surface after sandblasting is controlled below Ra0.8; E. Perform ordinary electroplating treatment on the die casting to control the outer surface roughness of the die casting to below Ra0.6; F. Randomly inspect the roughness, flatness, width and thickness of designated areas of die castings to obtain qualified products.

2. The low-roughness optical module processing technology according to claim 1, It is characterized in that From step B to step F, the blister tray is used throughout the entire process to prevent collision and friction.

3. The low-roughness optical module processing technology according to claim 1, It is characterized in that In step C, 1000 mesh sponge sand is used to lightly brush longitudinally to make the local surface of the die casting shiny.

4. The low-roughness optical module processing technology according to claim 1, It is characterized in that In the step D, 100# steel sand is used for sandblasting the inner cavity of the die casting at an air pressure of 2.0KG, and 240# steel sand is used for sandblasting the outer surface at an air pressure of 1.0KG.

5. The low-roughness optical module processing technology according to claim 4, It is characterized in that After the sandblasting treatment in step D, the outer surface of the die-casting is fully inspected. If there are scratches, it needs to be re-polished with 1000 mesh sponge sand and then re-sandblasted. After the outer surface is fully inspected and qualified, it can be circulated on a blister tray padded with copy paper to prevent collision and friction throughout the process.

6. The low-roughness optical module processing process according to claim 1, It is characterized in that In the step E, a common electroplating process of chemical nickel is used, with Ni: 2.5-7um, Cu: 12-25um.