Fragrant Chinese fir beautiful core board not prone to deformation and production method of fragrant Chinese fir beautiful core board
Through the multi-layer structure of the fragrant fir wood core board and the reverse pin rod card table design, the problems of deformation and angle of conventional ecological boards are solved, the structural strength and flatness are improved, internal defects are hidden, and log utilization is improved.
Patent Information
- Application Number
- CN202411157514.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-22
AI Technical Summary
Conventional ecological boards on the existing market are prone to deformation and corners, and cannot be used to make cabinet doors. In addition, internal defects and deformation problems under PET finishes are obvious, and the utilization rate of log scraps is low.
The multi-layer structure of the scented fir wood core board is used to achieve hot pressing and bonding through the interlocking design of the lower, middle and upper boards, and the reverse pin rod and the casing structure are used to fill the gap with adhesive to improve structural strength and adhesive. and reduce deformation by multiple stress removal treatments.
It effectively solves the deformation and angle problems, hides and beautifies internal defects, improves the flatness and finish of the board surface, enhances structural strength, and improves log utilization.
Smart Images

Figure CN118990706A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of wooden laminates, and in particular to a non-deformable fragrant fir wood core board and a production method thereof. Background Art
[0002] At present, the core of conventional ecological boards on the market mostly uses a layer of standard planks of the same thickness, width and length, which are made into a whole core through the process of splicing and gluing them together head to tail. The biggest disadvantage of conventional ecological boards made by this process is that they are easy to deform and warp, and thus cannot be used to make doors of cupboards and cabinets. Moreover, when the conventional ecological board core on the market is used to make PET veneer (especially high-gloss PET veneer) veneer, it is particularly easy to expose or even magnify the flaws, defects, deformation and other problems existing in the internal conventional board core under the (high-gloss) PET veneer. In addition, conventional ecological boards on the market are easily affected by external forces, air humidity, sunlight, etc., and problems such as shingle-like and rib-like deformation may occur. At the same time, because conventional ecological boards on the market need to use standard planks of the same thickness, width and length, when the thickness, width and length of the log scraps are lower than the size of the standard planks, or if they are thinning materials, they cannot be used, resulting in low log utilization. Summary of the invention
[0003] The purpose of the present invention is to solve any one of the problems in the above-mentioned technologies, thereby providing a non-deformable fragrant fir wood core board and a production method thereof.
[0004] In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme: a kind of non-deformable fragrant fir wood core board and its production method, including a bottom layer board and a middle layer board arranged above it, and an upper layer board arranged on the top of the middle layer board, wherein a middle layer card platform is arranged on the middle layer board, and a reverse pin rod is passed through the middle layer card platform. The reverse pin rod tightens the middle layer card platform so that the lower layer board, the middle layer board and the upper layer board are pressed together to achieve structural interlocking.
[0005] Furthermore, the upper surface of the lower plate is provided with lower plate snap-ons distributed in an array, and the lower plate snap-ons are in the shape of trapezoidal cylindrical grooves closing upward.
[0006] Furthermore, the lower surface of the middle plate is provided with an array-distributed middle layer card platform corresponding to the lower plate card position of the lower plate, the middle layer card platform is in the shape of a circular ring with an inner wall closing downward, the center of the middle layer card platform is a through hole penetrating into the middle layer plate, a plurality of middle layer expansion joints distributed in a circular array are provided on the circular ring of the middle layer card platform, and an annular notch-shaped middle layer release groove is provided above the outer wall of the circular ring of the middle layer card platform.
[0007] Furthermore, the bottom of the reverse lock pin rod is a cylindrical pin shaft rod, the top of the reverse lock pin rod is a reverse lock platform with a circular inner wall that closes upward, the circular ring of the reverse lock platform is provided with multiple upper expansion joints distributed in a circular array, and an upper release groove in the form of an annular notch is provided below the circular outer wall of the reverse lock platform.
[0008] Furthermore, an array of upper plate bayonet holes are provided on the lower surface of the upper plate. The upper plate bayonet holes are in the shape of trapezoidal cylindrical notches closing downwards. A cylindrical tensioning column with a chamfered bottom is provided at the center of the upper plate bayonet holes.
[0009] Furthermore, the method for producing the non-deformable fragrant fir wood core board comprises the following steps: S1: Lay the lower board on the hot pressing platform, which is not started at present, apply adhesive on the upper surface of the lower board, place the middle board on the lower board, and the middle card of the middle board is correspondingly inserted into the lower board card opening of the lower board; S2: insert the reverse buckle pin into the middle card platform of the middle board, apply adhesive on the reverse buckle pin and the upper surface of the middle board, place the upper board on the middle board, and at the same time, the upper board card slot of the upper board is set on the reverse buckle platform of the reverse buckle pin; S3: The hot pressing platform is started, hot pressing and gluing is performed at 130-200℃, and the hot pressing pressure is 7-13MPa. The hot pressing begins, and the middle card platform of the middle board is tightened outward when the reverse buckle pin is pressed down, and the middle card platform of the middle board is tightly fitted with the lower board opening of the lower board. When the tensioning column of the upper board is pressed down, the reverse buckle platform of the reverse buckle pin is tightened outward, and the upper board opening of the upper board is tightly fitted with the reverse buckle platform of the reverse buckle pin; S4: After hot pressing, the board surface is placed at room temperature for more than 7 days for stress relief treatment, and the hot pressed board surface is re-cut into long strips of 1.25cm*3.6cm*2.48m, and laid vertically into a board core of 1.25cm*2.48m*1.245m for hot pressing. After pressing, it is placed again for more than 7 days for stress relief treatment; S5: After hot pressing, the 1.25cm*2.48m*1.245m board core is sanded to a thickness of 1.22cm, inspected, and unqualified strips are replaced to make the board surface flat, and the first assembly is carried out. After the board core is glued, 1.7mm eucalyptus is pasted, and then cold pressed, repaired, and hot pressed in sequence. The thickness range after hot pressing is 1.53-1.56cm. Manual plastering is carried out to fill the eucalyptus knots and gaps and make them flat. Place it for more than 7 days for stress relief treatment, and then sand it to 1.48cm, inspect it again, fill the knots and gaps that have not been filled in place, and proceed The second assembly is carried out, and a layer of 1.5mm eucalyptus is pasted on both sides. Then it is cold pressed, repaired and hot pressed in sequence. The thickness range is 1.76-1.78cm after hot pressing. The edge is cleaned and machine scraped. The specification is 1.235cm*2.46m. It is placed for more than 7 days for stress relief treatment, and polished and sanded to 1.71cm. It is inspected again. The boards with insufficient thickness are taken off the line for rework and sanding, and various colored high-tech wood papers are pasted. It is placed for more than 7 days for stress relief treatment, and the finished product is cleaned. The finished product board is cleaned to a width * length of 1.22m*2.4m, and then inspected, packaged and shipped.
[0010] The beneficial effects of the present invention are: When the reverse lock pin is pressed down, the middle-layer clamping platform of the middle-layer board is stretched outward, and the middle-layer clamping platform of the middle-layer board is stretched and fitted tightly with the lower board clamping opening of the lower board. When the tensioning column of the upper board is pressed down, the reverse lock platform of the reverse lock pin is stretched outward, and the upper board clamping opening of the upper board is stretched and fitted tightly with the reverse lock platform of the reverse lock pin. The middle-layer clamping platform and the reverse lock platform respectively pull the lower board and the upper board inward and interlock them, which effectively improves the structural strength of the lower board, the middle board and the lower board after three-in-one hot pressing.
[0011] The lower plate snap-in of the lower plate and the upper plate snap-in of the upper plate not only perform reverse-button positioning but also have a good glue storage effect. When pressed, the adhesive in the lower plate snap-in and the upper plate snap-in effectively fills the fitting gap between the lower plate snap-in, the middle plate platform, the reverse-button platform, the upper plate snap-in and the tensioning column platform. There is no need to open additional glue storage grooves when hot-pressing the lower plate, the middle plate and the lower plate, and the bonding between the lower plate, the middle plate and the lower plate is better.
[0012] By dynamically utilizing slats of different thicknesses, widths and lengths, and efficiently gluing and splicing multi-layer fir slats, the biggest drawback of conventional ecological boards on the market, that is, they are easily deformed and warped and cannot be used to make doors of cupboards and cabinets, can be effectively solved, while matching the overall width, thickness and length of general ecological boards on the market. Moreover, the ecological boards with PET veneer on the multi-layer fir core can also hide, cover up and even beautify and optimize the internal core flaws, defects, deformation and other problems. In addition, the structure of the multi-layer fir solid wood core of the multi-layer fir core board with efficient gluing and splicing has been subjected to stress relief treatment for many times and is not affected by external forces, air humidity, sunlight and other external factors, thereby greatly reducing the problems of shingle-like and rib-like deformation, and the board surface is smoother, smoother and more beautiful. The gluing and splicing structure simultaneously solves the problem of low utilization rate of logs. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 A cross-sectional view of the present invention as a whole; Figure 2 An exploded view of the present invention as a whole; Figure 3 It is a structural schematic diagram of the lower plate of the present invention; Figure 4 is a cross-sectional view of the lower plate of the present invention; Figure 5 It is a schematic diagram of the structure of the middle layer board of the present invention; Figure 6 is a cross-sectional view of the middle layer board of the present invention; Figure 7 It is a structural schematic diagram of the reverse buckle pin rod of the present invention; Figure 8 is a cross-sectional view of the buckle pin rod of the present invention; Fig. 9 It is a schematic diagram of the structure of the upper plate of the present invention; Fig.10 It is a cross-sectional view of the upper plate of the present invention.
[0014] exist Figures 1 to 10 , the correspondence between the component names or lines and the figure numbers is: lower plate 1, lower plate bayonet 11, middle plate 2, middle plate platform 21, middle layer expansion joint 22, middle layer release groove 23, reverse buckle pin rod 3, pin shaft rod 31, reverse buckle platform 32, upper layer expansion joint 33, upper layer release groove 34, upper plate 4, upper plate bayonet 41, tensioning column platform 42. DETAILED DESCRIPTION
[0015] Please refer to Figures 1 to 10 ; The present embodiment provides a non-deformable fragrant fir wood core board and a production method thereof, comprising a bottom layer board 1 and a middle layer board 2 arranged above it, and an upper layer board 4 arranged on the top of the middle layer board 2. A middle layer card platform 21 is arranged on the middle layer board 2, and a reverse pin rod 3 is passed through the middle layer card platform 21. The reverse pin rod 3 tightens the middle layer card platform 21 so that the lower layer board 1, the middle layer board 2 and the upper layer board 4 are pressed together to achieve structural interlocking.
[0016] Preferably, the upper surface of the lower plate 1 is provided with lower plate snap-in openings 11 distributed in an array, and the lower plate snap-in openings 11 are in the shape of trapezoidal cylindrical notches closing upward.
[0017] In a specific embodiment, the lower plate snap-in 11 of the lower plate 1 and the upper plate snap-in 41 of the upper plate 4 have a good glue storage effect in addition to reverse-button positioning. When pressed, the adhesive in the lower plate snap-in 11 and the upper plate snap-in 41 effectively fills the fitting gap between the lower plate snap-in 11, the middle layer card platform 21, the reverse-button platform 32, the upper plate snap-in 41 and the tensioning column platform 42. There is no need to open an additional glue storage groove when hot pressing the lower plate 1, the middle plate 2 and the lower plate 1, and the bonding between the lower plate 1, the middle plate 2 and the lower plate 1 is better.
[0018] Preferably, the lower surface of the middle plate 2 is provided with an array-distributed middle layer platform 21 corresponding to the position of the lower plate clamping port 11 of the lower plate 1. The middle layer platform 21 is in the shape of a circular ring with an inner wall closing downward. The center of the middle layer platform 21 is a through hole penetrating through the middle plate 2. A plurality of middle layer expansion joints 22 distributed in a circular array are provided on the circular ring of the middle layer platform 21. A middle layer release groove 23 in the shape of an annular notch is provided above the outer wall of the circular ring of the middle layer platform 21.
[0019] In a specific embodiment, when the reverse latch pin 3 is pressed down, the middle layer card platform 21 of the middle layer board 2 is stretched outward, and the middle layer card platform 21 of the middle layer board 2 is stretched and fitted tightly with the lower plate clamping opening 11 of the lower layer board 1. When the tensioning column 42 of the upper layer board 4 is pressed down, the reverse latch platform 32 of the reverse latch pin 3 is stretched outward, and the upper plate clamping opening 41 of the upper layer board 4 is stretched and fitted tightly with the reverse latch platform 32 of the reverse latch pin 3. The middle layer card platform 21 and the reverse latch platform 32 respectively pull the lower layer board 1 and the upper layer board 4 inward to interlock.
[0020] Preferably, the bottom of the reverse lock pin rod 3 is a cylindrical pin shaft rod 31, and the top of the reverse lock pin rod 3 is a reverse lock platform 32 with a circular inner wall that closes upward. The circular ring of the reverse lock platform 32 is provided with multiple upper expansion joints 33 distributed in a circular array, and an upper release groove 34 in the form of an annular notch is provided below the circular outer wall of the reverse lock platform 32.
[0021] In a specific embodiment, the upper expansion joint 33 and the upper release groove 34 of the reverse buckle table 32 and the middle expansion joint 22 and the middle release groove 23 of the middle clamping table 21 reserve sufficient release space for the expansion and deformation of the reverse buckle table 32 and the middle clamping table 21, which has a good glue storage effect and avoids the occurrence of bulging in the expansion and deformation area of the plate during hot pressing.
[0022] Preferably, the lower surface of the upper plate 4 is provided with an array of upper plate snap-in sockets 41 , which are in the shape of a downwardly constricted trapezoidal cylindrical notch, and a cylindrical tensioning column 42 with a chamfered bottom is provided at the center of the upper plate snap-in socket 41 .
[0023] When the present invention is used, the lower plate 1 is laid on the hot pressing platform, and the hot pressing platform is not started at present. The adhesive is applied on the upper surface of the lower plate 1, and the middle plate 2 is placed on the lower plate 1. At the same time, the middle plate 21 of the middle plate 2 corresponds to the lower plate slot 11 of the lower plate 1, and the reverse buckle pin rod 3 is inserted into the middle plate 21 of the middle plate 2. The adhesive is applied on the reverse buckle pin rod 3 and the upper surface of the middle plate 2, and the upper plate 4 is placed on the middle plate 2. At the same time, the upper plate slot 41 of the upper plate 4 is sleeved on the reverse buckle platform 32 of the reverse buckle pin rod 3, and the hot pressing platform is started, 130~2 00℃ hot pressing bonding, hot pressing pressure of 7~13MPa, lower plate 1, middle plate 2, buckle pin 3 and upper plate 4 are hot pressed and buckled, the plate surface after hot pressing is placed at room temperature for more than 7 days for stress relief treatment, the hot pressed plate surface is re-cut into 1.25cm*3.6cm*2.48m long strips, and laid vertically into 1.25cm*2.48m*1.245m plate core for hot pressing, and the pressing is placed again for more than 7 days for stress relief treatment, and the 1.25cm*2.48m*1.245m plate after hot pressing is completed. The core is polished and sanded to a thickness of 1.22cm, and then inspected. Unqualified slats are replaced to make the board surface flat, and the first assembly is carried out. After the board core is coated with glue, 1.7mm eucalyptus is pasted, and then cold pressed, repaired, and hot pressed in sequence. The thickness range after hot pressing is 1.53-1.56cm. Manual plastering is carried out to fill the eucalyptus knots and gaps and make them flat. It is placed for more than 7 days for stress relief treatment, and then polished and sanded to 1.48cm. It is inspected again, and the knots and gaps that have not been filled in place are filled in place. The second assembly is carried out, and a layer of 1.5 is pasted on both sides. mm eucalyptus wood, and then cold pressed, repaired and hot pressed in turn. The thickness range is 1.76-1.78cm after hot pressing. It is cleaned and machine scraped. The specification is 1.235cm*2.46m. It is placed for more than 7 days for stress relief treatment, polished and sanded to 1.71cm, inspected again, and the boards with insufficient thickness are taken off the line for rework and sanding, and various colored technological wood papers are pasted. It is placed for more than 7 days for stress relief treatment, and the finished product is cleaned. The finished product board is cleaned to a width * length of 1.22m*2.4m, and then inspected, packaged and shipped.
[0024] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A non-deformable fir wood core board, comprising a bottom layer board and a middle layer board arranged above the bottom layer board, and an upper layer board arranged on the top of the middle layer board, characterized in that: The middle layer plate is provided with a middle layer card platform, and the reverse buckle pin rod is penetrated in the middle layer card platform. The reverse buckle pin rod tightens the middle layer card platform so that the lower layer plate, the middle layer plate and the upper layer plate are pressed together to achieve structural interlocking.
2. The non-deformable fir wood core board according to claim 1, characterized in that: The upper surface of the lower plate is provided with lower plate snap-ons distributed in an array, and the lower plate snap-ons are in the shape of trapezoidal cylindrical notches closing upward.
3. The non-deformable fir wood core board according to claim 1, characterized in that: The lower surface of the middle layer plate is provided with an array-distributed middle layer card platform corresponding to the lower plate card position of the lower layer plate. The middle layer card platform is in the shape of a circular ring with an inner wall closing downward. The center of the middle layer card platform is a through hole penetrating into the middle layer plate. A plurality of middle layer expansion joints distributed in a circular array are provided on the circular ring of the middle layer card platform. A middle layer release groove in the shape of an annular notch is provided above the outer wall of the circular ring of the middle layer card platform.
4. The non-deformable fir wood core board according to claim 1, characterized in that: The bottom of the reverse lock pin rod is a cylindrical pin shaft rod, and the top of the reverse lock pin rod is a reverse lock platform with a circular inner wall that closes upward. The circular ring of the reverse lock platform is provided with multiple upper expansion joints distributed in a circular array, and an upper release groove in the form of an annular notch is provided below the circular outer wall of the reverse lock platform.
5. The non-deformable fir wood core board according to claim 1, characterized in that: The lower surface of the upper plate is provided with upper plate snap-ons distributed in an array, the upper plate snap-ons are in the shape of trapezoidal cylindrical notches closing downward, and a cylindrical tensioning column with a chamfered bottom is provided in the center of the upper plate snap-ons.
6. A method for producing a non-deformable fragrant cedar core board, providing the non-deformable fragrant cedar core board according to any one of claims 1 to 5, the non-deformable fragrant cedar core board, the non-deformable fragrant cedar core board production method comprising the following steps: S1: Lay the lower board on the hot pressing platform, which is not started at present, apply adhesive on the upper surface of the lower board, place the middle board on the lower board, and the middle card of the middle board is correspondingly inserted into the lower board card opening of the lower board; S2: insert the reverse buckle pin into the middle card platform of the middle board, apply adhesive on the reverse buckle pin and the upper surface of the middle board, place the upper board on the middle board, and at the same time, the upper board card slot of the upper board is set on the reverse buckle platform of the reverse buckle pin; S3: The hot pressing platform is started, hot pressing and gluing is performed at 130-200℃, and the hot pressing pressure is 7-13MPa. The hot pressing begins, and the middle card platform of the middle board is tightened outward when the reverse buckle pin is pressed down, and the middle card platform of the middle board is tightly fitted with the lower board opening of the lower board. When the tensioning column of the upper board is pressed down, the reverse buckle platform of the reverse buckle pin is tightened outward, and the upper board opening of the upper board is tightly fitted with the reverse buckle platform of the reverse buckle pin; S4: After hot pressing, the board surface is placed at room temperature for more than 7 days for stress relief treatment, and the hot pressed board surface is re-cut into long strips of 1.25cm*3.6cm*2.48m, and laid vertically into a board core of 1.25cm*2.48m*1.245m for hot pressing. After pressing, it is placed again for more than 7 days for stress relief treatment; S5: After hot pressing, the 1.25cm*2.48m*1.245m board core is sanded to a thickness of 1.22cm, inspected, and unqualified strips are replaced to make the board surface flat, and the first assembly is carried out. After the board core is glued, 1.7mm eucalyptus is pasted, and then cold pressed, repaired, and hot pressed in sequence. The thickness range after hot pressing is 1.53-1.56cm. Manual plastering is carried out to fill the eucalyptus knots and gaps and make them flat. Place it for more than 7 days for stress relief treatment, and then sand it to 1.48cm, inspect it again, fill the knots and gaps that have not been filled in place, and proceed The second assembly is carried out, and a layer of 1.5mm eucalyptus is pasted on both sides. Then it is cold pressed, repaired and hot pressed in sequence. The thickness range is 1.76-1.78cm after hot pressing. The edge is cleaned and machine scraped. The specification is 1.235cm*2.46m. It is placed for more than 7 days for stress relief treatment, and polished and sanded to 1.71cm. It is inspected again. The boards with insufficient thickness are taken off the line for rework and sanding, and various colored high-tech wood papers are pasted. It is placed for more than 1 day for stress relief treatment, and the finished product is cleaned. The finished product board is cleaned to a width * length of 1.22m*2.4m, and then inspected, packaged and shipped.