Phosphoric acid purification process
By using ionic liquid-loaded resin synthesized by glycine and chloromethylated polystyrene resin, phosphoric acid is adsorbed and desorbed, and combined with water vapor fumigation and infrared laser irradiation, the liquid-liquid extraction in the wet phosphoric acid process is solved. The problems of low efficiency and stability have achieved an efficient and environmentally friendly phosphoric acid purification process.
Patent Information
- Application Number
- CN202411009166.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-22
AI Technical Summary
In the existing wet phosphoric acid process, the liquid-liquid extraction process is complex, the selectivity is poor, the ion separation efficiency is low, and the extractant is prone to volatilization and loss, resulting in low phosphoric acid purification efficiency and difficult to achieve large-scale industrial production.
The ionic liquid-loaded resin synthesized by glycine and chloromethylated polystyrene resin is used to adsorb phosphoric acid, adsorption and desorption are carried out through resin exchange columns, and the activation treatments such as water vapor fumigation and infrared laser radiation are combined to improve the resin Adsorption and desorption properties.
It realizes purification and purification of high-efficiency adsorption amount and low MER value (less than 1), avoids emulsification phenomenon and solvent loss, improves recovery rate and cycle stability, and is suitable for large-scale industrial production.
Smart Images

Figure CN118992996A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of phosphoric acid purification, and in particular to a phosphoric acid purification process. Background Art
[0002] Phosphorus resource processing methods mainly include thermal and wet methods. Among them, the sulfuric acid process in wet phosphoric acid is simple. By acid-leaching phosphate rock powder with sulfuric acid, the product phosphoric acid is a liquid phase, and the byproduct calcium sulfate is a solid phase with very low solubility. Crude phosphoric acid can be obtained by simple solid-liquid separation. It has strong adaptability to ores and is suitable for large-scale industrial production. It is the mainstream technology of the current wet phosphoric acid process. Then, organic matter is used to extract and purify phosphoric acid from crude phosphoric acid. However, the conventional liquid-liquid extraction process is complex, has poor selectivity, and has low ion separation efficiency. In addition, the extraction process is prone to emulsification of the extractant, resulting in difficulty in phase separation. In addition, the organic reagent is easy to volatilize and is lost during the extraction and stripping process, and the circulation performance is poor. The use of ionic liquid-loaded resin to adsorb phosphorus in wet phosphoric acid avoids the above problems in liquid-liquid extraction. According to research, the ionic liquid-loaded resin prepared by chemically grafting glycine with chloromethylated polystyrene resin has good selectivity for phosphate, and the phosphorus adsorption amount exceeds 260 mg / g. After desorption, purified phosphoric acid with a MER value of less than 1 can be obtained. Based on this, the use of ionic liquid-loaded resin to purify wet phosphoric acid is a new process that combines cleanliness and production efficiency.
[0003] Ionic liquid-loaded resins are environmentally friendly and have high cycle stability and excellent selectivity. They can avoid the volatilization of organic solvents and will not cause turbidity and emulsification of the solution phase. The selectivity can be changed by connecting ionic liquids with different functional groups, and ionic liquid-loaded resins with different selectivities can be designed. A stable chemical bond is formed between the ionic liquid and the resin in the ionic liquid-loaded resin, which can prevent the loss of the ionic liquid during the adsorption and desorption process and ensure its cycle stability. Studies have used anionic ionic liquid-loaded resins to adsorb vanadium in the form of anions, with an adsorption amount of more than 300 mg / g. When desorbed with hydrochloric acid, the desorption rate can reach more than 99%, and after 10 cycles of adsorption, there is still more than 96% of the adsorption capacity, with good selectivity, stability and cycle performance. Summary of the invention
[0004] In order to solve the above problems, the present invention provides a phosphoric acid purification process, which uses an ionic liquid loaded resin to adsorb phosphoric acid, comprising the following steps:
[0005] S1. Pre-treatment
[0006] At 20-30°C, add 18-22g of ionic liquid loaded resin into a 1cm×30cm resin exchange column, and insert absorbent cotton into the upper part of the resin exchange column;
[0007] S2. Resin adsorption
[0008] 18 to 22 mL of crude phosphoric acid is pumped into the resin exchange column at a rate of 0.4 to 0.6 mL / min, and the crude phosphoric acid is adsorbed by the ionic liquid loaded resin, and the adsorption is completed when the crude phosphoric acid is completely added;
[0009] S3, sulfuric acid desorption
[0010] Continue to pump 8-12 mL of dilute phosphoric acid at a rate of 1-1.5 mL / min to clean the resin exchange column. After the cleaning is completed, continue to pump 18-22 mL of sulfuric acid with a concentration of 4.8-5.2 mol / L at a flow rate of 0.4-0.6 mL / min to desorb the phosphorus adsorbed on the ionic liquid-loaded resin, and collect the desorbed solution, which is the desorbed phosphoric acid.
[0011] Description: Using ionic liquid loaded resin to purify phosphoric acid can make the adsorption amount of phosphoric acid reach 260mg / g, the phosphoric acid recovery rate can reach 90%, and the MER value of phosphoric acid after desorption is less than 1
[0012] Furthermore, the ionic liquid loaded resin is synthesized from a glycine solution and a chloromethylated polystyrene resin in a solid-liquid ratio of 1 g: 20-60 mL;
[0013] Note: The ionic liquid loaded resin synthesized under the above ratio has good adsorption capacity for phosphoric acid and also has good desorption effect.
[0014] Furthermore, in step S1, the ionic liquid loaded resin is activated.
[0015] The activation treatment method is as follows: immersing the ionic liquid loaded resin in anhydrous ethanol for ultrasonic treatment for 4 to 6 minutes, taking it out and rinsing it with ultrapure water for 3 to 4 times, then pouring it into a sealable filter chamber, placing the sealable filter chamber horizontally above boiling water at 98 to 100° C., fumigating it with water vapor for 15 to 20 minutes, then turning the sealable filter chamber over and continuing to fumigate for 15 to 20 minutes, finally transferring the sealable filter chamber to a pyridine solution for immersion for 15 to 20 minutes, pouring it out after immersion, washing it with ultrapure water for 2 to 4 times and drying it until the relative humidity of the ionic liquid loaded resin is 30 to 40 RH%, thereby obtaining the activated ionic liquid loaded resin;
[0016] The closable filter chamber is provided with a filter cloth; the water vapor fumigation volume is 120-180 mL / min, and the steam density is 20-28 μg / cm 3; During the ultrasonic treatment, the ultrasonic frequency is 60-80kHz, the temperature is 23-27°C, and the ultrasonic power is 200-300W; the pyridine solution is composed of pyridine and 0.4-1mg / L of tetrahydrofuran derivatives and 94-96% ethanol solution in a volume ratio of 1:1:1-3;
[0017] Description: Ultrasonic treatment of ionic liquid loaded resin with anhydrous ethanol can remove organic impurities and surface pollutants in the resin, thereby enhancing the purity and activity of the resin and further improving the adsorption of phosphoric acid by the resin. Water vapor fumigation can further open the pore structure of the resin, increase the specific surface area and porosity of the resin, and thus enhance its adsorption capacity. At the same time, the heating effect of steam helps the effective loading of the pyridine solution. In the interaction between pyridine, tetrahydrofuran derivatives and ethanol and phosphoric acid, the nitrogen, oxygen and other highly electronegative atoms in these molecules may form hydrogen bonds with the hydrogen atoms in phosphoric acid, further improving the adsorption effect of ionic liquid loaded resin on phosphoric acid. The ionic liquid loaded resin under the above relative humidity has better adsorption performance and a complete structure.
[0018] Furthermore, the fumigation process is coordinated with infrared laser irradiation, and the infrared laser irradiation method is alternating intermittent irradiation, which is divided into three stages:
[0019] The first stage: the wavelength of the infrared laser is 810-850nm, and the infrared laser irradiation is stopped for 1-3 minutes after irradiation for 25-40 seconds;
[0020] The second stage: adjust the wavelength of the infrared laser to 780-800nm, and stop the infrared laser irradiation for 1-3min after irradiation for 5-8s;
[0021] The third stage: adjust the wavelength of the infrared laser to 860-900nm, and stop the infrared laser irradiation for 1-3min after irradiation for 10-15s;
[0022] Description: The first stage of infrared laser can produce a moderate thermal effect, which helps to activate the functional groups on the resin surface and increase the affinity with phosphoric acid. The second stage of infrared laser is used for local rapid heating. The third stage of infrared laser is used to maintain the temperature of the resin surface and maintain adsorption activity. The alternating intermittent irradiation method allows the resin to have recovery time after infrared laser irradiation, which helps to reduce excessive changes or damage to the resin structure that may be caused by continuous irradiation, thereby ensuring the desorption ability of the ionic liquid resin.
[0023] Furthermore, the drying method is: first centrifuge at a speed of 450 to 550 r / min for 2 to 4 minutes to make the relative humidity of the ionic liquid loaded resin reach 60 to 70 RH%, then naturally dry at room temperature of 20 to 25 ° C for 1 to 1.5 hours to make the relative humidity of the ionic liquid loaded resin reach 45 to 55 RH%, and finally blow dry air at a temperature of 30 to 35 ° C at a flow rate of 6 to 10 m / s on the surface of the ionic liquid loaded resin for 10 to 20 minutes to obtain an ionic liquid loaded resin with a relative humidity of 30 to 40 RH%;
[0024] Note: The centrifugal drying process can remove some moisture at an appropriate speed. At the same time, the step-by-step drying method can avoid excessive damage to the resin structure and help maintain the adsorption capacity of the resin. The natural drying stage at room temperature can allow the resin to gradually adapt to the ambient humidity and reduce internal stress, thereby improving its overall performance. Under the above humidity conditions, the resin's adsorption of phosphoric acid is relatively reversible, thereby improving its desorption performance.
[0025] Furthermore, in step S1, the crude phosphoric acid is crude phosphoric acid with a mass concentration of 40-50% and a MER of <9;
[0026] Note: The initial untreated phosphoric acid is crude phosphoric acid with a mass concentration of 40 to 50%.
[0027] Further, in step S3, the mass concentration of the dilute phosphoric acid is 10-15%;
[0028] Note: The dilute phosphoric acid at the above mass concentration can wash away the crude phosphoric acid and impurity ions adhering to the column, thereby effectively improving the recovery rate of phosphoric acid.
[0029] Furthermore, the ionic liquid loaded resin after the desorption treatment is recovered and returned to step S2 for recycling;
[0030] Description: It can be concluded from the experimental conclusion that the desorption liquid obtained under the phosphoric acid purification process of the present invention is measured, and it is found that the present process can still achieve a good phosphorus recovery effect after multiple adsorptions, indicating that the present process can be recycled and used multiple times, and the adsorption effect is still good.
[0031] Furthermore, after step S3, the phosphoric acid purification effect is measured by using ICP-OES to measure the concentration of each element in the desorption solution;
[0032] Description: ICP-OES refers to an inductively coupled plasma emission spectrometer, which can be used for qualitative and quantitative analysis of metal elements and some non-metal elements in a variety of samples. It has the characteristics of high efficiency, stability, high accuracy, and the ability to continuously and quickly determine multiple elements. It can determine all metal elements and some non-metal elements.
[0033] Compared with the prior art, the present invention has the following beneficial effects:
[0034] (1) The present invention uses glycine solution and ionic liquid loaded resin to purify crude phosphoric acid. Compared with the traditional liquid-liquid extraction process, the present invention has a high recovery rate and a low MER value, can avoid emulsification, reduce solvent loss, is environmentally friendly, and has good recyclability. The traditional liquid-liquid extraction process of phosphoric acid has a low recovery rate and poor selectivity for producing high-value low-MER value phosphoric acid, with a recovery rate of only 60%. The ionic liquid loaded resin prepared by the present invention has an adsorption capacity of 260 mg / g of phosphoric acid, a phosphoric acid recovery rate of up to 90%, and a MER value of phosphoric acid after desorption is less than 1.
[0035] (2) The present invention utilizes water vapor fumigation in conjunction with pyridine solution impregnation to achieve activation treatment of the ionic liquid resin, so that the ionic liquid resin has more active sites that are beneficial to the loading of phosphoric acid. The addition of tetrahydrofuran derivatives and ethanol can cooperate with the pyridine solution to swell the resin. At the same time, the pyridine solution itself also has an adsorption effect on phosphoric acid, which can further improve the purification effect of phosphoric acid. In addition, it is not easy to form ionic bonds between the various components and phosphoric acid under the above environment, so it will not affect the desorption effect of the resin. The synergistic effect between the infrared laser and the fumigation treatment can further improve the activation of the functional groups on the surface of the resin, increase its adsorption activity, and improve the purification effect of phosphoric acid. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 is a process flow chart of Example 1 of the present invention;
[0037] Figure 2 It is a comparison chart of the phosphoric acid adsorption amount of Examples 1 to 11 of the present invention and Comparative Examples 1 to 3;
[0038] Figure 3 It is a comparison chart of phosphorus recovery rates of the primary desorption liquids of Examples 1 to 11 of the present invention and Comparative Examples 1 to 3;
[0039] Figure 4 It is a comparison chart of the MER values of the primary desorption liquids of Examples 1 to 11 of the present invention and Comparative Examples 1 to 3;
[0040] Figure 5 It is a comparison chart of the phosphoric acid adsorption amount of Example 1, Examples 12 to 26, and Comparative Examples 4 to 7 of the present invention;
[0041] Figure 6 It is a comparison chart of phosphorus recovery rates of the primary desorption solutions of Example 1, Examples 12 to 26, and Comparative Examples 4 to 7 of the present invention;
[0042] Figure 7It is a comparison chart of the MER values of the primary desorption liquids of Example 1, Examples 12 to 26, and Comparative Examples 4 to 7 of the present invention. DETAILED DESCRIPTION
[0043] In order to further illustrate the method adopted by the present invention and the effect achieved, the technical solution of the present invention will be clearly and completely described in combination with experiments below.
[0044] Example 1: A phosphoric acid purification process, wherein the purification process is to adsorb phosphoric acid using an ionic liquid loaded resin, comprising the following steps:
[0045] S1. Pre-treatment
[0046] At 25°C, 20 g of ionic liquid loaded resin was added to a 1 cm × 30 cm resin exchange column, and absorbent cotton was plugged into the upper part of the resin exchange column; the ionic liquid loaded resin was synthesized by glycine solution and chloromethylated polystyrene resin at a solid-liquid ratio of 1 g:40 mL;
[0047] The synthesis method is as follows: add chloromethylated polystyrene resin to a glycine solution with a mass concentration of 15%, stir at 90°C for 10 hours, then use quantitative medium-speed filter paper for solid-liquid separation to obtain a pre-ionic liquid-loaded resin, and finally vacuum dry at a temperature of 55°C for 4.5 hours to obtain an ionic liquid-loaded resin.
[0048] S2. Resin adsorption
[0049] 20 mL of crude phosphoric acid is pumped into the resin exchange column at a rate of 0.5 mL / min, and the crude phosphoric acid is adsorbed by the ionic liquid loaded resin, and the adsorption is completed when the crude phosphoric acid is completely added; the crude phosphoric acid is crude phosphoric acid with a mass concentration of 45% and a MER of 8.17;
[0050] S3, sulfuric acid desorption
[0051] Continue to pump 10 mL of dilute phosphoric acid with a mass concentration of 13% at a rate of 1.2 mL / min to clean the resin exchange column. After cleaning, continue to pump 20 mL of sulfuric acid with a concentration of 5.0 mol / L at a flow rate of 0.5 mL / min to desorb the phosphorus adsorbed on the ionic liquid-loaded resin, and collect the desorbed solution, which is the desorbed phosphoric acid; measure the phosphoric acid purification effect by using ICP-OES to measure the concentration of each element in the desorption solution; recover the ionic liquid-loaded resin after desorption and return it to step S2 for recycling.
[0052] Example 2: Different from Example 1, the ionic liquid-loaded resin is synthesized from glycine solution and chloromethylated polystyrene resin at a solid-liquid ratio of 1 g:20 mL; the synthesis method is: adding chloromethylated polystyrene resin to a glycine solution with a mass concentration of 10% according to the above ratio, stirring at 80°C for 12 hours, and then using quantitative medium-speed filter paper for solid-liquid separation to obtain a pre-ionic liquid-loaded resin, and finally vacuum drying at a temperature of 50°C for 5 hours to obtain the ionic liquid-loaded resin.
[0053] Example 3: Different from Example 1, the ionic liquid-loaded resin is synthesized from glycine solution and chloromethylated polystyrene resin at a solid-liquid ratio of 1 g:60 mL; the synthesis method is: adding chloromethylated polystyrene resin to a glycine solution with a mass concentration of 20% according to the above ratio, stirring at 95°C for 8 hours, and then using quantitative medium-speed filter paper for solid-liquid separation to obtain a pre-ionic liquid-loaded resin, and finally vacuum drying at a temperature of 60°C for 4 hours to obtain the ionic liquid-loaded resin.
[0054] Example 4: The difference from Example 1 is that in step S1, 18 g of ionic liquid loaded resin is added to a 1 cm×30 cm resin exchange column at 20° C., and absorbent cotton is plugged into the upper part of the resin exchange column.
[0055] Example 5: Different from Example 1, in step S1, 22 g of ionic liquid loaded resin was added to a 1 cm×30 cm resin exchange column at 30° C., and absorbent cotton was plugged into the upper part of the resin exchange column.
[0056] Example 6: Different from Example 1, 18 mL of crude phosphoric acid was pumped into the resin exchange column at a rate of 0.4 mL / min.
[0057] Example 7: Different from Example 1, 22 mL of crude phosphoric acid was pumped into the resin exchange column at a rate of 0.6 mL / min.
[0058] Example 8: Different from Example 1, 8 mL of dilute phosphoric acid with a mass concentration of 10% was continuously pumped in at a rate of 1 mL / min to clean the resin exchange column.
[0059] Example 9: Different from Example 1, 12 mL of dilute phosphoric acid with a mass concentration of 15% was continuously pumped in at a rate of 1.5 mL / min to clean the resin exchange column.
[0060] Example 10: Different from Example 1, after cleaning, 18 mL of sulfuric acid with a concentration of 4.8 mol / L is continuously pumped in at a flow rate of 0.4 mL / min.
[0061] Example 11: Different from Example 1, after cleaning, 22 mL of sulfuric acid with a concentration of 5.2 mol / L is continuously pumped in at a flow rate of 0.6 mL / min.
[0062] Example 12: Different from Example 1, in step S1, the ionic liquid loaded resin is activated.
[0063] The activation treatment method is as follows: immerse the ionic liquid loaded resin in anhydrous ethanol and perform ultrasonic treatment for 5 minutes, take it out and rinse it with ultrapure water for 3 times, then pour it into a sealable filter chamber, place the sealable filter chamber horizontally above boiling water at 99°C, fumigate it with water vapor for 18 minutes, then turn the sealable filter chamber over and continue to fumigate it for 18 minutes, finally transfer the sealable filter chamber to a pyridine solution and immerse it for 18 minutes, pour it out after immersion, wash it with ultrapure water for 3 times and dry it until the relative humidity of the ionic liquid loaded resin is 35RH%, thus obtaining the activated ionic liquid loaded resin;
[0064] The filter cloth is installed in the sealable filter chamber; the water vapor fumigation volume is 150mL / min, and the vapor density is 24μg / cm 3 ; During the ultrasonic treatment, the ultrasonic frequency is 70kHz, the temperature is 25°C, and the ultrasonic power is 250W; the pyridine solution is composed of pyridine, 0.6mg / L tetrahydrofuran derivative, and 95% ethanol solution in a volume ratio of 1:1:2; in this embodiment, the tetrahydrofuran derivative is α-pyrrolidone solution;
[0065] The fumigation process is coordinated with infrared laser irradiation. The infrared laser irradiation method is alternating intermittent irradiation, which is divided into three stages:
[0066] The first stage: the wavelength of the infrared laser is 830nm, and the infrared laser irradiation is stopped for 2min after irradiation for 30s;
[0067] The second stage: adjust the wavelength of the infrared laser to 790nm, and stop the infrared laser irradiation for 2min after irradiation for 6s;
[0068] The third stage: adjust the wavelength of the infrared laser to 880nm, and stop the infrared laser irradiation for 2min after irradiation for 13s;
[0069] The drying method is as follows: first use a centrifuge to centrifuge and dry for 3 minutes at a rotation speed of 500r / min to make the relative humidity of the ionic liquid-loaded resin reach 65RH%, then naturally dry for 1.3 hours at room temperature of 22°C to make the relative humidity of the ionic liquid-loaded resin reach 50RH%, and finally blow dry air at a temperature of 33°C on the surface of the ionic liquid-loaded resin at a flow rate of 8m / s for 15 minutes to obtain an ionic liquid-loaded resin with a relative humidity of 35RH%.
[0070] Example 13: Different from Example 12, the ionic liquid loaded resin was immersed in anhydrous ethanol and ultrasonically treated for 4 minutes, and then taken out and rinsed with ultrapure water for 3 times.
[0071] Example 14: Different from Example 12, the ionic liquid loaded resin was immersed in anhydrous ethanol and ultrasonically treated for 6 minutes, and then taken out and rinsed with ultrapure water for 4 times.
[0072] Example 15: Different from Example 12, the sealable filter chamber is placed horizontally above boiling water at 98°C, fumigated with water vapor for 15 minutes, and then the sealable filter chamber is turned over and fumigated for another 15 minutes.
[0073] Example 16: Different from Example 12, the sealable filter chamber is placed horizontally above boiling water at 100°C, fumigated with water vapor for 20 minutes, and then the sealable filter chamber is turned over and fumigated for another 20 minutes.
[0074] Example 17: Different from Example 12, the sealable filter cavity is finally transferred to the pyridine solution and immersed for 15 minutes.
[0075] Example 18: Different from Example 12, the sealable filter cavity is finally transferred to the pyridine solution and immersed for 20 minutes.
[0076] Example 19: Different from Example 12, the pyridine solution is composed of pyridine, 0.4 mg / L of a tetrahydrofuran derivative, and an ethanol solution with a mass concentration of 94% in a volume ratio of 1:1:1.
[0077] Example 20: Different from Example 12, the pyridine solution is composed of pyridine, 1 mg / L tetrahydrofuran derivative and 96% ethanol solution in a volume ratio of 1:1:3.
[0078] Example 21: Different from Example 12, the water vapor fumigation rate is 120 mL / min and the vapor density is 20 μg / cm 3 .
[0079] Example 22: Different from Example 12, the water vapor fumigation rate is 180 mL / min and the vapor density is 28 μg / cm 3 .
[0080] Example 23: Different from Example 12, during the ultrasonic treatment, the ultrasonic frequency is 60kHz, the temperature is 23°C, and the ultrasonic power is 200W.
[0081] Example 24: Different from Example 12, during the ultrasonic treatment, the ultrasonic frequency is 80kHz, the temperature is 27°C, and the ultrasonic power is 300W.
[0082] Example 25: Different from Example 12, the drying method is: first use a centrifuge to centrifuge and dry at a rotation speed of 450r / min for 2 minutes to make the relative humidity of the ionic liquid-loaded resin reach 60RH%, then naturally dry at room temperature of 20°C for 1 hour to make the relative humidity of the ionic liquid-loaded resin reach 45RH%, and finally blow dry air at a temperature of 30°C on the surface of the ionic liquid-loaded resin at a flow rate of 6m / s for 10 minutes to obtain an ionic liquid-loaded resin with a relative humidity of 30RH%.
[0083] Example 26: Different from Example 12, the drying method is: first use a centrifuge to centrifuge and dry at a rotation speed of 550r / min for 4 minutes to make the relative humidity of the ionic liquid-loaded resin reach 70RH%, then naturally dry at room temperature of 25°C for 1.5h to make the relative humidity of the ionic liquid-loaded resin reach 55RH%, and finally blow dry air at a temperature of 35°C on the surface of the ionic liquid-loaded resin at a flow rate of 10m / s for 20min to obtain an ionic liquid-loaded resin with a relative humidity of 40RH%.
[0084] Experimental Example: The description of this experimental example is based on the scheme described in Example 1, and is intended to illustrate the practical application effect of the present invention.
[0085] The method for determining the concentration of each element in the desorption solution by ICP-OES is as follows: the desorption solution is sent to the Materials Research and Testing Center of Wuhan University of Technology for testing. The results are as follows:
[0086] Table 1 Concentration of each element in the primary desorption liquid and the secondary desorption liquid obtained by the phosphoric acid purification process in Example 1
[0087] element P Fe Al Mg MER Crude Phosphoric Acid 138.17g / L 1.82g / L 6.19g / L 6.89g / L 8.17 Primary desorption liquid 127.87g / L 0.24g / L 0.26g / L 0.29g / L 0.45 Secondary desorption liquid 127.32g / L 0.25g / L 0.25g / L 0.31g / L 0.46
[0088] From the data in Table 1, it can be seen that the phosphorus recovery rate in the primary desorption liquid is 92.55%, and the MER value is reduced from 8.17 to 0.45, indicating that the process used to purify crude phosphoric acid has a high recovery rate and a low MER value compared to the traditional liquid-liquid extraction process, and can also avoid emulsification, reduce solvent loss and be environmentally friendly; and from the data of the secondary desorption liquid, it can be seen that the adsorption of the ionic liquid-loaded resin can still reach 99.56% of the original adsorption amount, and the recovery rate is also 92.14%, the cycle performance is good, and the MER value is still small, and it can be recycled for many times.
[0089] 1. Explore the effects of resin and desorbent on the purification of phosphoric acid in the purification process
[0090] Comparative Example 1: The difference from Example 1 is that phosphoric acid is replaced by dilute hydrochloric acid.
[0091] Comparative Example 2: Different from Example 1, phosphoric acid was replaced by water.
[0092] Comparative Example 3: Different from Example 1, the glycine ionic liquid loaded resin is replaced by an ionic liquid loaded resin prepared by pyridine and N,N-dimethylformamide.
[0093] Conclusion: Figure 2 to Figure 4 From the data comparison of Examples 1 to 11, it can be seen that the change of parameters in the phosphoric acid purification process within the scope of this application has little effect on the effect of phosphoric acid purification. Considering the adsorption and desorption, MER value and economy, Example 1 is selected as the optimal solution, while Comparative Examples 1 and 2 use dilute hydrochloric acid or water for desorption, and the desorption effect is not as good as sulfuric acid in Example 1. Moreover, the industrial phosphoric acid process itself is carried out in a sulfuric acid system, and sulfuric acid will not introduce too many other impurities; the ionic liquid-loaded resin prepared in Comparative Example 3 has a higher adsorption capacity for phosphorus, which can reach 420 mg / g, and has better adsorption performance, but poor desorption effect, and a higher MER value (about 3).
[0094] 2. Explore the effect of activation treatment on the purification effect of phosphoric acid
[0095] Comparative Example 4: Different from Example 12, the ionic liquid loaded resin after being rinsed with ultrapure water is directly placed in a heating furnace at a temperature of 99°C for heating treatment.
[0096] Comparative Example 5: Different from Example 12, the pyridine solution lacks the addition of tetrahydrofuran derivative.
[0097] Control Example 6: Different from Example 12, no infrared laser irradiation treatment is performed during the fumigation treatment.
[0098] Comparative Example 7: Different from Example 12, the drying method is to directly dry at room temperature to a relative humidity of 35 RH%.
[0099] Conclusion: Figure 5 to Figure 7It can be seen that the activation treatment methods in Examples 12 to 26 do not perform activation treatment compared to Example 1, and do improve the adsorption and desorption capabilities of phosphoric acid by the ionic liquid-loaded resin to a certain extent, and the adjustment within the above parameter range has little effect on the adsorption and desorption effects of phosphoric acid by the ionic liquid-loaded resin. Considering the comprehensive economic efficiency, Example 12 is selected as a further optimized scheme; and from the comparison of Example 12 and Control Example 4, it can be seen that the fumigation activation of the ionic liquid-loaded resin by water vapor is better than directly heating in a heating furnace, mainly because water vapor can penetrate and heat the resin more evenly, because the diffusion capacity of steam is generally better than that of dry hot air, and this uniform heating helps to avoid changes in resin properties caused by local overheating or rapid heating. Steam heating can generally provide a milder heating rate, which helps to control the polymerization and cross-linking process of the resin, thereby obtaining a resin with a better activation effect, and further improving the phosphoric acid purification effect;
[0100] From the comparison between Example 12 and Control Example 5, it can be seen that α-pyrrolidone may serve as a hydrophilic additive to help improve the hydrophilicity of the resin, making the resin more easily contacted with water vapor, thereby promoting the penetration and adsorption of water vapor. The addition of α-pyrrolidone will also change the internal structure of the resin, increase its swelling capacity, and make the resin more easily swell under the action of water vapor, which helps to increase the resin's loading capacity for phosphoric acid; and the weakened swelling capacity of the resin may directly affect its loading capacity for glycine ionic liquid, because insufficient swelling will lead to a weakened ability of the resin's internal space to accommodate phosphoric acid; at the same time, the lack of α-pyrrolidone as a stabilizer will make the resin more susceptible to chemical changes during the swelling process, thereby reducing the overall stability. In the control example 6, the resin activation effect is weakened due to the lack of infrared laser irradiation during the fumigation process, thereby reducing the purification efficiency of phosphoric acid; in the control example 7, direct drying at room temperature to a relative humidity of 35RH% also weakens the phosphoric acid adsorption and desorption performance of the resin. In this scheme, the pore structure of the resin can be optimized by precisely controlling the humidity, thereby increasing its adsorption capacity for phosphoric acid; the staged drying process can reduce the damage to the resin caused by rapid changes in temperature or humidity, extend the service life of the resin, and help maintain the structural stability of the resin, thereby improving its reusability.
Claims
1. A phosphoric acid purification process, characterized in that: The method of adsorbing phosphoric acid with an ionic liquid loaded resin comprises the following steps: S1. Pre-treatment At 20-30°C, add 18-22g of ionic liquid loaded resin into a 1cm×30cm resin exchange column, and insert absorbent cotton into the upper part of the resin exchange column; S2. Resin adsorption 18 to 22 mL of crude phosphoric acid is pumped into the resin exchange column at a rate of 0.4 to 0.6 mL / min, and the crude phosphoric acid is adsorbed by the ionic liquid loaded resin, and the adsorption is completed when the crude phosphoric acid is completely added; S3, sulfuric acid desorption Continue to pump 8-12 mL of dilute phosphoric acid at a rate of 1-1.5 mL / min to clean the resin exchange column. After the cleaning is completed, continue to pump 18-22 mL of sulfuric acid with a concentration of 4.8-5.2 mol / L at a flow rate of 0.4-0.6 mL / min to desorb the phosphorus adsorbed on the ionic liquid-loaded resin, and collect the desorbed solution, which is the desorbed phosphoric acid.
2. A phosphoric acid purification process according to claim 1, characterized in that: The ionic liquid loaded resin is synthesized from a glycine solution and a chloromethylated polystyrene resin in a solid-liquid ratio of 1 g: 20-60 mL.
3. A phosphoric acid purification process as claimed in claim 2, characterized in that: The synthesis method comprises the following steps: adding chloromethylated polystyrene resin to a glycine solution with a mass concentration of 10 to 20% according to the above ratio, stirring at 80 to 95° C. for 8 to 12 hours, then using quantitative medium-speed filter paper for solid-liquid separation to obtain a pre-ionic liquid loaded resin, and finally vacuum drying at a temperature of 50 to 60° C. for 4 to 5 hours to obtain an ionic liquid loaded resin.
4. A phosphoric acid purification process according to claim 1, characterized in that: In step S1, the ionic liquid loaded resin is activated. The activation treatment method is as follows: immersing the ionic liquid loaded resin in anhydrous ethanol for ultrasonic treatment for 4 to 6 minutes, taking it out and rinsing it with ultrapure water for 3 to 4 times, then pouring it into a sealable filter chamber, placing the sealable filter chamber horizontally above boiling water at 98 to 100° C., fumigating it with water vapor for 15 to 20 minutes, then turning the sealable filter chamber over and continuing to fumigate for 15 to 20 minutes, finally transferring the sealable filter chamber to a pyridine solution for immersion for 15 to 20 minutes, pouring it out after immersion, washing it with ultrapure water for 2 to 4 times and drying it until the relative humidity of the ionic liquid loaded resin is 30 to 40 RH%, thereby obtaining the activated ionic liquid loaded resin; The closable filter chamber is provided with a filter cloth; the water vapor fumigation volume is 120-180 mL / min, and the steam density is 20-28 μg / cm 3 ; During the ultrasonic treatment process, the ultrasonic frequency is 60-80kHz, the temperature is 23-27°C, and the ultrasonic power is 200-300W; the pyridine solution is composed of pyridine and 0.4-1mg / L of a tetrahydrofuran derivative and an ethanol solution with a mass concentration of 94-96% in a volume ratio of 1:1:1-3.
5. A phosphoric acid purification process as claimed in claim 4, characterized in that: The fumigation process is coordinated with infrared laser irradiation. The infrared laser irradiation method is alternating intermittent irradiation, which is divided into three stages: The first stage: the wavelength of the infrared laser is 810-850nm, and the infrared laser irradiation is stopped for 1-3 minutes after irradiation for 25-40 seconds; The second stage: adjust the wavelength of the infrared laser to 780-800nm, and stop the infrared laser irradiation for 1-3min after irradiation for 5-8s; The third stage: adjust the wavelength of the infrared laser to 860-900 nm, and stop the infrared laser irradiation for 1-3 minutes after irradiation for 10-15 seconds.
6. A phosphoric acid purification process as claimed in claim 4, characterized in that: The drying method comprises the following steps: firstly, centrifugally drying the resin at a rotation speed of 450 to 550 r / min for 2 to 4 minutes to make the relative humidity of the ionic liquid loaded resin reach 60 to 70 RH%, then naturally drying the resin at a room temperature of 20 to 25° C. for 1 to 1.5 hours to make the relative humidity of the ionic liquid loaded resin reach 45 to 55 RH%, and finally, blowing dry air at a temperature of 30 to 35° C. at a flow rate of 6 to 10 m / s on the surface of the ionic liquid loaded resin for 10 to 20 minutes to obtain the ionic liquid loaded resin with a relative humidity of 30 to 40 RH%.
7. A phosphoric acid purification process according to claim 1, characterized in that: In step S1, the crude phosphoric acid is crude phosphoric acid with a mass concentration of 40-50% and a MER of less than 9.
8. A phosphoric acid purification process according to claim 1, characterized in that: In step S3, the mass concentration of the dilute phosphoric acid is 10-15%.
9. A phosphoric acid purification process according to claim 1, characterized in that: The ionic liquid loaded resin after the desorption treatment is recovered and returned to step S2 for recycling.
Citation Information
Patent Citations
Method for preparing high-purity sodium hypophosphite
CN101555002A
Method for preparing novel epoxidation catalyst of cyclohexene
CN102527436A
Method for extraction and oxidative desulfurization of fuel oil by solid acid coupled ionic liquid
CN110229693A
Cited By
Resin pretreatment method
CN119608253A
A resin pretreatment method
CN119608253B