Preparation method of high-dispersity silicon dioxide used in cosmetics

By using a specific mixing method of long-chain alkyl amine with silicon-containing compounds and surfactants in cosmetics, highly dispersible silica was prepared, which solved the problem of preparing highly dispersible silica in the prior art, and achieved the Significantly improves oil control performance and skin improvement effects, and reduces preparation costs.

CN118993089APending Publication Date: 2024-11-22SHANGHAI NAT ENG RES CENT FORNANOTECH +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411100085.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The prior art is difficult to prepare silica powders with high dispersion and good oil control properties, which limits their application in cosmetics.

Method used

Prepare by dissolving long-chain alkylamine in an alcohol solution, mixing with silicon-containing compounds, acids and surfactants in a specific molar ratio, adding slowly dropwise and stirring at room temperature, followed by centrifugation, washing and oven drying, Highly dispersible silica.

Benefits of technology

It significantly increases the specific surface area of ​​the material, improves oil control and skin quality improvement performance, and has simple process and low cost, which has important application value.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides a preparation method of high-dispersity silicon dioxide used in cosmetics, which comprises the following steps: dissolving long-chain alkylamine in an alcoholic solution until the concentration is 5-100g / L, and marking as a solution A; respectively taking a silicon-containing compound, an acid and a surfactant according to a molar ratio of 1: 0.5: 0.01-1: 3: 1, and marking as a solution B; and slowly dropwise adding the solution B into the solution A, stirring at room temperature for 2-30 hours, centrifuging the product, washing with ethanol and deionized water for 3-5 times, and drying in a drying oven at 60-80 DEG C to obtain the final product. Compared with the prior art, the SiO2 nano-material has the advantages that the specific surface area of the surface of the material can be increased, the oil control and skin improvement performance of the material can be greatly improved, the dispersity is very good, the preparation process is simple, the preparation cost is low, and the important value is achieved for further promoting the application of the SiO2 material in cosmetics.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of daily chemical industry, and specifically refers to a method for preparing highly dispersible silicon dioxide used in cosmetics. Background Art

[0002] Silica is widely used in cosmetics, mainly as a lubricant, adsorbent, anti-caking agent and thickener. Silicon dioxide has a strong adsorption capacity and can absorb an appropriate amount of oil. It has an oil-control effect, can make the skin smooth and tender, visually improve skin wrinkles, cover fine lines without clogging pores, and can be used in sunscreen products to increase the sun protection value and improve the spreadability. Silicon dioxide's spherical shape, small particle size, and porous properties make it an anti-caking agent and thickener in the cosmetics field. It can improve storage stability and dispersibility of powdered products and is widely used, such as distributing pigments in lipsticks and cosmetics to help improve the free flow properties of hair bleach and the coating properties of nail polish. Silicon dioxide has different particle sizes, particle size distributions, and pore volumes, and its oil absorption value and skin feel are also different, so it can be used in different cosmetics. Therefore, as an important raw material for cosmetics, its market demand has increased with the development of the cosmetics industry. The present invention provides a simple method for preparing highly dispersible silica, which can increase the specific surface area of ​​the material surface, greatly improve the oil control and skin quality improvement performance of the material, and has very good dispersibility, and the preparation process is simple and the preparation cost is low, which is of great value for further promoting the application of SiO2 materials in cosmetics. Summary of the invention

[0003] The present invention aims to provide a method for preparing highly dispersible silicon dioxide for use in cosmetics.

[0004] The object of the present invention is achieved by the following scheme: A method for preparing highly dispersible silicon dioxide for use in cosmetics, characterized in that the specific steps of the method are: (1) Dissolve a long-chain alkylamine in an alcohol solution to a concentration of 5-100 g / L, labeled solution A.

[0005] (2) Take the silicon-containing compound, acid and surfactant respectively so that their molar ratio is 1:0.5:0.01-1:3:1 and mark it as solution B.

[0006] (3) Solution B was slowly added dropwise to solution A and stirred at room temperature for 2 to 30 h. The product was centrifuged, washed with ethanol and deionized water for 3 to 5 times, and dried in an oven at 60 to 80 °C to obtain the final product.

[0007] The long-chain alkylamine described in the above preparation method is one of decaamine, dodecylamine, hexadecyl ammonium bromide or a combination thereof.

[0008] The alcohol described in the above preparation method is one or a combination of methanol, ethanol or propanol.

[0009] The silicon-containing compound described in the above preparation method is one of monomethyltriethoxysilane, dimethyldiethoxysilane and tetraethyl orthosilicate or a combination thereof.

[0010] The acid described in the above preparation method is one of sulfuric acid, hydrochloric acid, acetic acid, ethylenediaminetetraacetic acid or a combination thereof.

[0011] The surfactant described in the above preparation method is one of Tween 20, polyethylene glycol ether, sodium polyacrylate, hydroxyethyl phenethyl ether, sodium benzoate or a combination thereof.

[0012] The present invention can increase the specific surface area of ​​the material surface, greatly improve the oil control and skin quality improvement performance of the material, and has very good dispersibility, and the preparation process is simple and the preparation cost is low. It is of great value to further promote the application of SiO2 materials in cosmetics. DETAILED DESCRIPTION

[0013] The embodiments are implemented on the premise of the technical solution of the present invention, and detailed implementation methods and specific operation processes are given, but the protection scope of the present invention is not limited to the following embodiments.

[0014] Example 1 A highly dispersible silicon dioxide for use in cosmetics, prepared according to the following method: (1) Dissolve 0.5 g of long-chain alkylamine decaamine in 30 ml of methanol solution, labeled as solution A; (2) Take 4.91 g of silicon-containing compound monomethyltriethoxysilane, 5.73 g of acid and 1.4 g of surfactant Tween 20, slowly add them dropwise to solution A, and stir at room temperature for 30 h to obtain the initial product; (3) The product was centrifuged, washed three times with ethanol and deionized water, and dried in an oven at 60°C to obtain the final product.

[0015] The final product can increase the specific surface area of ​​the material, greatly improve the oil control and skin quality improvement performance of the material, and has very good dispersibility, and the preparation process is simple and the preparation cost is low. Example 2 A highly dispersible silicon dioxide for use in cosmetics, prepared according to the following method: (1) Dissolve 1 g of dodecylamine in 50 ml of ethanol solution, labeled as solution A; (2) Slowly add 3.85 g of dimethyldiethoxysilane, 5.98 g of ethylenediaminetetraacetic acid and 0.85 g of polyethylene glycol ether to solution A respectively, and stir to react for 20 h to obtain a preliminary product; (3) The product was centrifuged, washed four times alternately with ethanol and aqueous solution, and dried in an oven at 80°C to obtain the final product.

[0016] Example 3 A highly dispersible silicon dioxide for use in cosmetics, prepared according to the following method: (1) Dissolve 0.8 g of hexadecyl ammonium bromide in 50 ml of ethanol solution, labeled as solution A; (2) Slowly add 4.463 g of tetraethyl orthosilicate, 2.54 g of acetic acid and 0.56 g of sodium polyacrylate to solution A respectively, and stir to react for 24 h to obtain a preliminary product; The product was centrifuged, washed alternately with ethanol and aqueous solution for three times, and dried in an oven at 80°C to obtain the final product.

Claims

1. A method for preparing highly dispersible silicon dioxide for use in cosmetics, characterized in that: The specific steps of this method are: (1) Dissolve the long-chain alkylamine in an alcohol solution to a concentration of 5-100 g / L, labeled as solution A; (2) Take the silicon-containing compound, acid and surfactant respectively at a molar ratio of 1:0.5:0.01-1:3:1, slowly add them dropwise to solution A, and stir at room temperature for 2-30 h to obtain a preliminary product; (3) The product is centrifuged, washed with ethanol and deionized water for 3 to 5 times, and dried in an oven at 60 to 80 °C to obtain the final product.

2. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to claim 1, characterized in that: The long-chain alkylamine is one of decaamine, dodecylamine, hexadecyl ammonium bromide or a combination thereof.

3. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to claim 1, characterized in that: The alcohol is one of methanol, ethanol or propanol or a combination thereof.

4. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to claim 1, characterized in that: The silicon-containing compound is one of monomethyltriethoxysilane, dimethyldiethoxysilane and tetraethyl orthosilicate or a combination thereof.

5. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to claim 1, characterized in that: The acid is one of sulfuric acid, hydrochloric acid, acetic acid, and ethylenediaminetetraacetic acid, or a combination thereof.

6. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to claim 1, characterized in that: The surfactant is one of Tween 20, polyethylene glycol ether, sodium polyacrylate, hydroxyethyl phenethyl ether, sodium benzoate or a combination thereof.

7. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to any one of claims 1 to 6, characterized in that: Prepared as follows: (1) Dissolve 0.5 g of long-chain alkylamine decaamine in 30 ml of methanol solution, labeled as solution A; (2) Take 4.91 g of silicon-containing compound monomethyltriethoxysilane, 5.73 g of acid and 1.4 g of surfactant Tween 20, slowly add them dropwise to solution A, and stir at room temperature for 30 h to obtain the initial product; (3) The product was centrifuged, washed three times with ethanol and deionized water, and dried in an oven at 60°C to obtain the final product.

8. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to any one of claims 1 to 6, characterized in that: Prepared as follows: (1) Dissolve 1 g of dodecylamine in 50 ml of ethanol solution, labeled as solution A; (2) Slowly add 3.85 g of dimethyldiethoxysilane, 5.98 g of ethylenediaminetetraacetic acid and 0.85 g of polyethylene glycol ether to solution A respectively, and stir to react for 20 h to obtain a preliminary product; (3) The product was centrifuged, washed four times alternately with ethanol and aqueous solution, and dried in an oven at 80°C to obtain the final product.

9. The method for preparing highly dispersible silicon dioxide for use in cosmetics according to any one of claims 1 to 6, characterized in that: Prepared as follows: (1) Dissolve 0.8 g of hexadecyl ammonium bromide in 50 ml of ethanol solution, labeled as solution A; (2) Slowly add 4.463 g of tetraethyl orthosilicate, 2.54 g of acetic acid and 0.56 g of sodium polyacrylate to solution A respectively, and stir to react for 24 h to obtain a preliminary product; (3) The product was centrifuged, washed three times alternately with ethanol and aqueous solution, and dried in an oven at 80°C to obtain the final product.

Citation Information

Patent Citations

  • Preparation method of mesoporous silica microsphere

    CN102050454A

  • Preparation method of hollow mesoporous silica material

    CN103449450A

  • Method for synthesizing highly ordered super-microporous silicon dioxide

    CN107188186A

  • Prepn process of monodisperse microporous silica microballoon with great specific surface area

    CN1608985A