Thermal insulation building material and preparation method thereof

Through the synergistic effect of modified acrylic emulsion and enhanced filler, thermal insulation building materials with excellent thermal insulation, flame retardant and adhesion are prepared, which solves the problems of complex processes and poor performance of traditional materials and achieves efficient thermal insulation effects of building .

CN118994988AInactive Publication Date: 2024-11-22DONGGUAN KAIXIANG DECORATION MATERIAL CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411216945.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-02
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional building thermal insulation materials have complex processes, high cost and poor results. Although existing thermal insulation coatings are simple, they require excellent thermal insulation, flame retardant and adhesion, which is difficult to meet multiple performance requirements.

Method used

Using modified acrylic emulsion as the matrix, combining reinforced fillers (synthesised from elotite, polydopamine and magnesium hydroxide) and nanosilicon dioxide, the insulation building materials are prepared through ultrasonic dispersion and reaction technology to improve their thermal insulation and resistance. Burn and adhesion.

Benefits of technology

The modification of polymer emulsions is achieved, the synergistic effect of fillers is enhanced, the thermal conductivity is significantly reduced, the flame retardant performance and adhesion are improved, and it is suitable for thermal insulation materials in the construction field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

The invention relates to the technical field of building materials, and discloses a thermal insulation building material and a preparation method thereof. The building thermal insulation material is prepared from the following raw materials in parts by weight: 40 to 60 parts of modified acrylic emulsion, 10 to 15 parts of sepiolite fiber, 8 to 15 parts of reinforcing filler, 5 to 7 parts of ceramic particles, 2 to 4 parts of nano silicon dioxide, 2 to 5 parts of calcium silicate and 4 to 8 parts of dispersing agent, a high-molecular polymer emulsion is used as a matrix, and a reinforcing filler and various thermal insulation materials are added, so that the thermal insulation performance, flame retardance and adhesive force of the matrix are improved; wherein the reinforcing filler utilizes the synergistic effect of halloysite, polydopamine and magnesium hydroxide, so that the thermal insulation performance and flame retardant property of the matrix are improved; the high-molecular polymer emulsion is obtained by modifying acrylic emulsion, so that the flame retardant property and adhesive force of a matrix are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of building materials, and in particular to a thermal insulation building material and a preparation method thereof. Background Art

[0002] In the process of actively seeking new technologies for energy saving and consumption reduction, thermal insulation building materials came into being. Traditional building thermal insulation materials, such as EPS boards, XPS boards, PU rigid foams and other organic thermal insulation materials, are limited by the performance of the materials themselves and lack scientific and technological content. The construction projects have complex processes, high overall costs and poor effects. This traditional passive thermal insulation method causes a huge waste of resources and energy.

[0003] Compared with organic thermal insulation materials, thermal insulation coatings have the advantages of simple process and good effect. However, due to the different use environments of thermal insulation coatings, the coatings not only require excellent thermal insulation properties but also certain flame retardancy, high adhesion and other advantages. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides a thermal insulation building material and a preparation method thereof.

[0005] The purpose of the present invention can be achieved through the following technical solutions: A thermal insulation building material, comprising the following raw materials in parts by weight: 40-60 parts of modified acrylic emulsion, 10-15 parts of sepiolite fiber, 8-15 parts of reinforcing filler, 5-7 parts of ceramic particles, 2-4 parts of nano silicon dioxide, 2-5 parts of calcium silicate, and 4-8 parts of dispersant; The reinforcing filler is prepared by the following steps: Step A1, dispersing halloysite in 1 mol / L Tris-HCl buffer solution with a pH of 8.5 and deionized water, ultrasonically dispersing for 30 min, heating to 30° C., then adding dopamine hydrochloride and stirring for 8-12 h, centrifuging, washing, and drying to obtain PDA@haloysite material; Step A2, adding PDA@halloysite material to 8-12wt% magnesium chloride solution and ultrasonically treating for 10 minutes, then slowly adding saturated ammonia solution, reacting at 40-50°C and 3.5-3.8MPa for 2-3 hours, then reacting at 10-15°C and vacuum conditions for 1-2 hours, filtering and drying to obtain a reinforcing filler; Further, in step A1, the usage ratio of halloysite, Tris-HCl buffer solution, deionized water and dopamine hydrochloride is 1-3 g: 2-4 mL: 100 mL: 0.2-0.6 g; Furthermore, in step A2, the dosage ratio of the PDA@halloysite material, the magnesium chloride solution and the saturated ammonia solution is 1-3 g: 20 mL: 40 mL.

[0006] The modified acrylic emulsion is prepared by the following steps: Step B1, dispersing triglycidyl isocyanurate and tetrabutylammonium bromide evenly in N,N-dimethylformamide, adding 4-hydroxyphenylboric acid, and heating to 85-95° C., reacting under nitrogen for 2-3 hours, and after the reaction is completed, an intermediate product is obtained; Step B2, under nitrogen, slowly add allylamine to the intermediate product, and control the temperature at 50-60° C. to stir and react for 5-7 hours. After the reaction is completed, perform vacuum distillation and drying to obtain a terminal double bond functional monomer; Step B3, weigh the raw materials by weight, disperse the emulsifier SE-10N evenly in 1 / 2 of deionized water, then add butyl acrylate, acrylic acid, methyl methacrylate, terminal double-bond functional monomer, vinyl trimethoxy silane and 1-vinyl imidazole and stir for 20-30 minutes to form a pre-emulsion; then stir the initiator ammonium persulfate and the remaining deionized water at 65-75° C. for 10 minutes, and then slowly drop the pre-emulsion for 1-2 hours. After the dropwise addition is completed, the temperature is raised to 80-90° C. and the reaction is continued for 2-3 hours. After the reaction is completed, filter to obtain a modified acrylic emulsion; Further, in step B1, the usage ratio of triglycidyl isocyanurate, tetrabutylammonium bromide, N,N-dimethylformamide and 4-hydroxyphenylboric acid is 0.01-0.02 mol: 0.0005-0.001 mol: 100 mL: 0.02-0.04 mol; Further, the molar ratio of allylamine in step B2 to triglycidyl isocyanurate in step B1 is 1:1; Furthermore, the weight parts of the raw materials in step B3 are: 3-7 parts of emulsifier SE-10N, 40-50 parts of butyl acrylate, 5-8 parts of acrylic acid, 35-45 parts of methyl methacrylate, 5-9 parts of terminal double bond functional monomer, 2-4 parts of vinyltrimethoxysilane, 1-2 parts of 1-vinylimidazole, 0.1-0.3 parts of initiator ammonium persulfate, and 300-400 parts of deionized water.

[0007] A method for preparing a thermal insulation building material comprises the following steps: The raw materials are weighed in parts by weight, and the modified acrylic emulsion is stirred in a stirrer for 10-20 minutes. Then, sepiolite fiber, reinforcing filler, ceramic particles, nano-silicon dioxide, calcium silicate and dispersant are added and stirred for 40-60 minutes to obtain a thermal insulation building material.

[0008] Beneficial effects of the present invention: The building thermal insulation material in the present application is based on a high molecular polymer emulsion, with reinforcing fillers and various thermal insulation materials added to improve the thermal insulation performance, flame retardancy and adhesion of the matrix; wherein the reinforcing filler utilizes the synergistic effect between halloysite, polydopamine and magnesium hydroxide to improve the thermal insulation performance and flame retardancy of the matrix; the high molecular polymer emulsion is obtained by modifying the acrylic emulsion to increase the flame retardancy and adhesion of the matrix.

[0009] In the reinforcing filler, dopamine hydrochloride is firstly condensed on the surface of halloysite to form a polydopamine film to synthesize the PDA@halloysite material; and then magnesium chloride and a saturated ammonia solution are used as raw materials to synthesize magnesium hydroxide, which is loaded on the surface of the PDA@halloysite material to synthesize the reinforcing filler. The reinforcing filler in the matrix improves the thermal insulation performance of the matrix and also has a certain flame retardancy; among them, halloysite has a unique tubular structure, which causes the cavity inside the nanotube to hinder the transmission of heat, forming an isolation effect, reducing the conduction path of the heat, and then effectively reducing the heat transfer in the matrix, thereby reducing the thermal conductivity and improving the thermal insulation performance of the matrix; the formation of the polydopamine film can not only reduce the thermal conductivity of the matrix and play a thermal insulation role, but also use the rich catechol groups on the surface of the polydopamine film to adsorb magnesium ions, and the adsorbed magnesium ions can react with ammonia water to synthesize magnesium hydroxide; and the formation of magnesium hydroxide can not only improve the thermal insulation performance of the matrix, but also play a certain flame retardant role, because magnesium hydroxide itself has good thermal insulation properties, can form a barrier layer in the matrix, and then can effectively prevent the transfer of heat, and at the same time, magnesium hydroxide uses its own structural characteristics to form a fire barrier in the matrix, effectively preventing the occurrence and spread of fire.

[0010] In the modified acrylic emulsion, the epoxy group in triglycidyl isocyanurate is firstly reacted with the hydroxyl group in 4-hydroxyphenylboronic acid to generate an intermediate product; then the remaining epoxy group in the intermediate product is reacted with the amino group in allylamine to generate a terminal double-bond functional monomer; finally, butyl acrylate, acrylic acid, methyl methacrylate, a terminal double-bond functional monomer, vinyltrimethoxysilane and 1-vinylimidazole are used as raw materials and the modified acrylic emulsion is synthesized under the action of an emulsifier. Functional groups such as triazine ring, boric acid group and imidazole structure are introduced into the modified acrylic emulsion to improve the flame retardant properties of the acrylic emulsion. This is because the N, B and C elements contained in the functional groups cooperate with each other to promote the formation of a carbon layer by the polymer. The formation of the carbonized layer helps to isolate oxygen and heat, thereby preventing or slowing down the further degradation and combustion of the polymer material. At the same time, the N element can also generate non-flammable gas, which not only dilutes the concentration of oxygen and combustible gas on the combustion interface, but also consumes oxygen in the air. In addition, the boric acid group and imidazole group in the modified acrylic emulsion can also work synergistically to improve the adhesion between the substrate and the building wall. This is because both the boric acid group and the imidazole group can chelate with the metal cations on the wall surface to form a stable complex, thereby improving the adhesion of the substrate and reducing the occurrence of shedding, cracking, peeling and other phenomena caused by insufficient adhesion. DETAILED DESCRIPTION

[0011] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example

[0012] The reinforcing filler is prepared by the following steps: Step A1, dispersing 1 g of halloysite in 2 mL of 1 mol / L Tris-HCl buffer solution with a pH of 8.5 and 100 mL of deionized water, ultrasonically dispersing for 30 min, and heating to 30° C., then adding 0.2 g of dopamine hydrochloride and stirring for 8 h, centrifuging, washing, and drying to obtain PDA@haloysite material; Step A2, add 1g of PDA@halloysite material to 20mL of 8wt% magnesium chloride solution and ultrasonically treat for 10min, then slowly add 40mL of saturated ammonia solution, and react at 40°C and 3.5MPa for 2h, then react at 10°C and vacuum conditions for 1h, filter and dry to obtain a reinforced filler.

[0013] The modified acrylic emulsion is prepared by the following steps: Step B1, 0.01 mol of triglycidyl isocyanurate and 0.0005 mol of tetrabutylammonium bromide are evenly dispersed in 100 mL of N,N-dimethylformamide, and then 0.02 mol of 4-hydroxyphenylboric acid is added, and the temperature is raised to 85° C., and the reaction is carried out under nitrogen for 2 hours. After the reaction is completed, an intermediate product is obtained; Step B2, under nitrogen conditions, slowly add allylamine to the intermediate product, and control the temperature at 50°C to stir and react for 5 hours. After the reaction is completed, vacuum distillation and drying are performed to obtain a terminal double bond functional monomer, wherein the molar ratio of allylamine to triglycidyl isocyanurate in step B1 is 1:1; Step B3, weigh the raw materials by weight, evenly disperse 3 parts of emulsifier SE-10N in 150-200 parts of deionized water, then add 40 parts of butyl acrylate, 5 parts of acrylic acid, 35 parts of methyl methacrylate, 5 parts of terminal double bond functional monomer, 2 parts of vinyltrimethoxysilane and 1 part of 1-vinyl imidazole and stir for 20 minutes to form a pre-emulsion; then stir 0.1 parts of initiator ammonium persulfate and 150 parts of deionized water at 65° C. for 10 minutes, and then slowly drop the pre-emulsion, the dropping time is 1 hour, after the dropwise addition is completed, the temperature is raised to 80° C. and the reaction is continued for 2 hours. After the reaction is completed, filter to obtain a modified acrylic emulsion. Example

[0014] The reinforcing filler is prepared by the following steps: Step A1, dispersing 2 g of halloysite in 3 mL of 1 mol / L Tris-HCl buffer solution with a pH of 8.5 and 100 mL of deionized water, ultrasonically dispersing for 30 min, and heating to 30° C., then adding 0.4 g of dopamine hydrochloride and stirring for 10 h, centrifuging, washing, and drying to obtain PDA@haloysite material; Step A2, add 2 g of PDA@halloysite material to 20 mL of 10 wt% magnesium chloride solution and ultrasonically treat for 10 min, then slowly add 40 mL of saturated ammonia solution, and react at 45 ° C and 3.7 MPa for 2.5 h, then react at 15 ° C and vacuum conditions for 1.5 h, filter and dry to obtain a reinforced filler.

[0015] The modified acrylic emulsion is prepared by the following steps: Step B1, 0.015 mol of triglycidyl isocyanurate and 0.00075 mol of tetrabutylammonium bromide are evenly dispersed in 100 mL of N,N-dimethylformamide, and then 0.03 mol of 4-hydroxyphenylboric acid is added, and the temperature is raised to 90° C., and the reaction is carried out under nitrogen for 2.5 hours. After the reaction is completed, an intermediate product is obtained; Step B2, under nitrogen conditions, slowly add allylamine to the intermediate product, and control the temperature at 55°C to stir and react for 6 hours. After the reaction is completed, vacuum distillation and drying are performed to obtain a terminal double bond functional monomer, wherein the molar ratio of allylamine to triglycidyl isocyanurate in step B1 is 1:1; Step B3, weigh the raw materials by weight, evenly disperse 5 parts of emulsifier SE-10N in 170 parts of deionized water, then add 45 parts of butyl acrylate, 7 parts of acrylic acid, 40 parts of methyl methacrylate, 7 parts of terminal double bond functional monomer, 3 parts of vinyltrimethoxysilane and 1.5 parts of 1-vinyl imidazole and stir for 20-30 minutes to form a pre-emulsion; then stir 0.2 parts of initiator ammonium persulfate and 170 parts of deionized water at 70°C for 10 minutes, and then slowly drop the pre-emulsion, the dropping time is 1.5 hours, after the dropwise addition is completed, the temperature is raised to 85°C and the reaction is continued for 2.5 hours, after the reaction is completed, filter to obtain a modified acrylic emulsion. Example

[0016] The reinforcing filler is prepared by the following steps: Step A1, 3 g of halloysite is dispersed in 4 mL of 1 mol / L Tris-HCl buffer solution with a pH of 8.5 and 100 mL of deionized water, ultrasonically dispersed for 30 min, and heated to 30° C., then 0.6 g of dopamine hydrochloride is added and stirred for 12 h, centrifuged, washed, and dried to obtain PDA@haloysite material; Step A2, add 3g of PDA@halloysite material to 20mL of 12wt% magnesium chloride solution and ultrasonically treat for 10min, then slowly add 40mL of saturated ammonia solution, and react at 50°C and 3.8MPa for 3h, then react at 15°C and vacuum conditions for 2h, filter and dry to obtain a reinforced filler.

[0017] The modified acrylic emulsion is prepared by the following steps: Step B1, 0.02 mol of triglycidyl isocyanurate and 0.001 mol of tetrabutylammonium bromide are evenly dispersed in 100 mL of N,N-dimethylformamide, and then 0.04 mol of 4-hydroxyphenylboric acid is added, and the temperature is raised to 95° C., and the reaction is carried out under nitrogen for 3 hours. After the reaction is completed, an intermediate product is obtained; Step B2, under nitrogen conditions, slowly add allylamine to the intermediate product, and control the temperature at 60°C to stir and react for 7 hours. After the reaction is completed, vacuum distillation and drying are performed to obtain a terminal double bond functional monomer, wherein the molar ratio of allylamine to triglycidyl isocyanurate in step B1 is 1:1; Step B3, weigh the raw materials by weight, disperse 7 parts of emulsifier SE-10N evenly in 200 deionized water, then add 50 parts of butyl acrylate, 8 parts of acrylic acid, 45 parts of methyl methacrylate, 9 parts of terminal double bond functional monomer, 4 parts of vinyltrimethoxysilane and 2 parts of 1-vinylimidazole and stir for 30 minutes to form a pre-emulsion; then stir 0.3 parts of initiator ammonium persulfate and 200 deionized water at 75°C for 10 minutes, and then slowly add the pre-emulsion dropwise for 2 hours. After the addition is completed, the temperature is raised to 90°C and the reaction is continued for 3 hours. After the reaction is completed, filter to obtain a modified acrylic emulsion. Example

[0018] A method for preparing a thermal insulation building material comprises the following steps: 40 parts of the modified acrylic emulsion prepared in Example 1, 10 parts of sepiolite fibers, 8 parts of the reinforcing filler prepared in Example 1, 5 parts of ceramic particles, 2 parts of nano-silicon dioxide, 2 parts of calcium silicate, and 4 parts of a dispersant (polyethylene glycol); The raw materials were weighed by weight, and the modified acrylic emulsion prepared in Example 1 was stirred in a stirrer for 10 minutes. Then, sepiolite fibers, the reinforcing filler prepared in Example 1, ceramic particles, nano-silicon dioxide, calcium silicate and dispersant (polyethylene glycol) were added and stirred for 40 minutes to obtain a thermal insulation building material. Example

[0019] A method for preparing a thermal insulation building material comprises the following steps: 50 parts of the modified acrylic emulsion prepared in Example 2, 13 parts of sepiolite fibers, 12 parts of the reinforcing filler prepared in Example 2, 6 parts of ceramic particles, 3 parts of nano-silicon dioxide, 4 parts of calcium silicate, and 6 parts of a dispersant (polyethylene glycol); The raw materials were weighed by weight, and the modified acrylic emulsion prepared in Example 2 was stirred in a stirrer for 15 minutes. Then, sepiolite fibers, reinforcing fillers prepared in Example 2, ceramic particles, nano-silicon dioxide, calcium silicate and dispersant (polyethylene glycol) were added and stirred for 50 minutes to obtain a thermal insulation building material. Example

[0020] A method for preparing a thermal insulation building material comprises the following steps: 60 parts of the modified acrylic emulsion prepared in Example 3, 15 parts of sepiolite fibers, 15 parts of the reinforcing filler prepared in Example 3, 7 parts of ceramic particles, 4 parts of nano-silicon dioxide, 5 parts of calcium silicate, and 8 parts of a dispersant (polyethylene glycol); The raw materials were weighed by weight, and the modified acrylic emulsion prepared in Example 3 was stirred in a stirrer for 20 minutes. Then, sepiolite fibers, the reinforcing filler prepared in Example 3, ceramic particles, nano-silicon dioxide, calcium silicate and dispersant (polyethylene glycol) were added and stirred for 60 minutes to obtain a thermal insulation building material.

[0021] Comparative Example 1 This comparative example is a thermal insulation material, which differs from Example 6 in that commercially available acrylic emulsion is used instead of the modified acrylic emulsion prepared in Example 3, and the rest are the same.

[0022] Comparative Example 2 This comparative example is a thermal insulation material, which differs from Example 6 in that calcium carbonate is used instead of the reinforcing filler prepared in Example 3, and the rest is the same.

[0023] The thermal insulation materials prepared in Examples 4-6 and Comparative Examples 1-3 were subjected to performance tests: Thermal conductivity test: According to ASTM E1530 coating thermal conductivity test standard test; Adhesion test: Tested according to GB9286-98 100-grid test standard; Flame retardant performance test: Test the flame retardant time according to GB12441-2005; The test results are shown in the following table:

[0024] It can be seen from the above table that the building thermal insulation material prepared by the present invention has a thermal conductivity of 0.014W / m·K-0.019W / m·K, indicating that it has a low thermal conductivity and excellent thermal insulation performance; the adhesion grade is 5B, the surface has excellent adhesion, good bonding performance, and is not easy to fall off; the flame retardant time is ≥15min, indicating that it has excellent flame retardant properties; therefore, the thermal insulation material can be widely used in the field of construction.

[0025] The above contents are merely examples and explanations of the concept of the present invention. The technicians in this technical field may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the scope defined by the concept of the invention, they should all fall within the protection scope of the present invention.

Claims

1. A thermal insulation building material, characterized in that: The raw materials include the following parts by weight: 40-60 parts of modified acrylic emulsion, 10-15 parts of sepiolite fiber, 8-15 parts of reinforcing filler, 5-7 parts of ceramic particles, 2-4 parts of nano silicon dioxide, 2-5 parts of calcium silicate, and 4-8 parts of dispersant; The reinforcing filler is prepared by the following steps: Step A1, dispersing halloysite in 1 mol / L Tris-HCl buffer solution with a pH of 8.5 and deionized water, ultrasonically dispersing for 30 min, heating to 30° C., then adding dopamine hydrochloride and stirring for 8-12 h, centrifuging, washing, and drying to obtain PDA@haloysite material; Step A2, adding the PDA@halloysite material to an 8-12wt% magnesium chloride solution and ultrasonically treating it for 10 minutes, then slowly adding a saturated ammonia solution, and reacting it at 40-50°C and 3.5-3.8MPa for 2-3 hours, and then reacting it at 10-15°C and vacuum conditions for 1-2 hours, filtering and drying to obtain a reinforced filler.

2. A thermal insulation building material according to claim 1, characterized in that: In step A1, the usage ratio of halloysite, Tris-HCl buffer solution, deionized water and dopamine hydrochloride is 1-3 g: 2-4 mL: 100 mL: 0.2-0.6 g.

3. A thermal insulation building material according to claim 1, characterized in that: In step A2, the dosage ratio of the PDA@halloysite material, the magnesium chloride solution and the saturated ammonia solution is 1-3 g: 20 mL: 40 mL.

4. A thermal insulation building material according to claim 1, characterized in that: The modified acrylic emulsion is prepared by the following steps: Step B1, dispersing triglycidyl isocyanurate and tetrabutylammonium bromide evenly in N,N-dimethylformamide, adding 4-hydroxyphenylboric acid, and heating to 85-95° C., reacting under nitrogen for 2-3 hours, and after the reaction is completed, an intermediate product is obtained; Step B2, under nitrogen, slowly add allylamine to the intermediate product, and control the temperature at 50-60° C. to stir and react for 5-7 hours. After the reaction is completed, perform vacuum distillation and drying to obtain a terminal double bond functional monomer; Step B3, weigh the raw materials by weight, disperse the emulsifier SE-10N evenly in 1 / 2 of deionized water, then add butyl acrylate, acrylic acid, methyl methacrylate, terminal double bond functional monomer, vinyl trimethoxy silane and 1-vinyl imidazole and stir for 20-30 minutes to form a pre-emulsion; then stir the initiator ammonium persulfate and the remaining deionized water at 65-75°C for 10 minutes, and then slowly drop the pre-emulsion for 1-2 hours. After the dropwise addition is completed, the temperature is raised to 80-90°C and the reaction is continued for 2-3 hours. After the reaction is completed, filter to obtain a modified acrylic emulsion.

5. A thermal insulation building material according to claim 1, characterized in that: In step B1, the usage ratio of triglycidyl isocyanurate, tetrabutylammonium bromide, N,N-dimethylformamide and 4-hydroxyphenylboric acid is 0.01-0.02 mol: 0.0005-0.001 mol: 100 mL: 0.02-0.04 mol.

6. A thermal insulation building material according to claim 1, characterized in that: The molar ratio of allylamine in step B2 to triglycidyl isocyanurate in step B1 is 1:

1.

7. The thermal insulation building material according to claim 1, characterized in that: The weight proportions of the raw materials in step B3 are: 3-7 parts of emulsifier SE-10N, 40-50 parts of butyl acrylate, 5-8 parts of acrylic acid, 35-45 parts of methyl methacrylate, 5-9 parts of terminal double bond functional monomer, 2-4 parts of vinyltrimethoxysilane, 1-2 parts of 1-vinylimidazole, 0.1-0.3 parts of initiator ammonium persulfate, and 300-400 parts of deionized water.

8. The method for preparing a thermal insulation building material according to claim 1, characterized in that: The following steps are involved: The raw materials are weighed in parts by weight, and the modified acrylic emulsion is stirred in a stirrer for 10-20 minutes. Then, sepiolite fiber, reinforcing filler, ceramic particles, nano-silicon dioxide, calcium silicate and dispersant are added and stirred for 40-60 minutes to obtain a thermal insulation building material.

Citation Information

Cited By

  • Lightweight foam concrete, preparation method thereof and application of lightweight foam concrete in thermal insulation and sound insulation walls

    CN120136502A