Micron-sized instantaneous laser cutting device and fiber stretching resilience testing method

High-speed and high-precision partial cutting in the fiber tensile rebound test is performed by micron-scale instantaneous laser cutting device, which solves the problem of asymmetric cutting and combustion risks in the prior art, and improves the accuracy and safety of the test results.

CN119000249APending Publication Date: 2024-11-22BEIHANG UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411148876.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the existing fiber tensile rebound test methods, the cutting method has asymmetric cutting, axial friction and combustion risks, which affects the accuracy of the test results.

Method used

Micron-scale instantaneous laser cutting device is used to perform high-speed and high-precision micron-scale cutting using laser emitters. The material itself is destroyed by partial cutting methods to ensure that stress waves are transmitted along the fiber axial direction and avoid mechanical friction and flame ablation.

Benefits of technology

Accurate micron-level cutting is achieved, which reduces test errors, improves the accuracy and safety of the results, and ensures the stability of the cutting process and lossless energy transmission.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119000249A_ABST
    Figure CN119000249A_ABST
Patent Text Reader

Abstract

The invention discloses a micron-sized instantaneous laser cutting device and a fiber stretching resilience test method, and relates to the technical field of fiber strength test.The micron-sized instantaneous laser cutting device comprises a base plate, at least one sliding block is arranged on the base plate, the upper end of each sliding block is connected with a lifting rod, and the lifting rod is connected with a laser source. A laser emitter is installed at the upper end of the lifting rod, a lower clamp is further installed on the base plate and used for clamping the lower end of a to-be-tested sample, and an upper clamp is installed at the upper end of the to-be-tested sample. The fiber tensile resilience testing method comprises the following steps: S1, mounting a to-be-tested sample; s2, laser parameter adjustment; and S3, testing the to-be-tested sample. The high-precision cutting device has high-precision cutting capacity and can be used for partially machining or cutting micron-sized materials. In the fiber stretching springback test method, the fiber is not in contact with a sample to be tested in the cutting process, so that mechanical friction or mechanical vibration is not introduced, and lossless transmission of energy and the accuracy of a test result are ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of fiber strength testing, and in particular to a micron-level instantaneous laser cutting device and a fiber stretching and rebound testing method. Background Art

[0002] The tensile rebound method is often used to test the compressive strength of various materials. The test process requires cutting the preloaded material under the action of external force. There are currently two cutting methods, surgical scissors and electric sparks. The surgical scissors method has serious asymmetric cutting and axial friction, and the cutting time is long; the electric spark cutting causes the material to burn, which affects the propagation of axial stress, and is more dangerous when testing organic materials. There are various problems with the current cutting methods, which have a great impact on the accuracy of the test results.

[0003] Laser cutting uses a focused high-power density laser beam to irradiate the material, causing the affected area to melt or vaporize rapidly, thereby achieving cutting. The laser cutting method has the advantages of high energy, high precision, high speed and non-contact. The laser cutting method improves the cutting speed, increases the cutting accuracy, eliminates the influence of mechanical friction, eliminates the dangers of combustion and the influence of axial asymmetric ablation. In addition, the laser cutting method can achieve partial cutting of micron-level materials, so that the fiber will eventually trigger stretching rebound due to its own destruction, so the coaxiality of the stress wave when it is transmitted in the test sample is better. However, there is no precedent in the prior art for applying laser cutting to the stretching rebound method test.

[0004] Therefore, those skilled in the art are in urgent need of a micron-level instantaneous laser cutting device and a fiber tensile rebound testing method to solve the above problems. Summary of the invention

[0005] The purpose of the present invention is to provide a micron-level instantaneous laser cutting device and a fiber tensile rebound test method to solve the problems existing in the above-mentioned prior art, and to be able to apply laser cutting technology to the tensile rebound test, so as to achieve micron-level precise cutting, small action area, low damage, incomplete cutting, good coaxiality of the rebound stress wave, effectively reduce errors and improve the accuracy of results.

[0006] To achieve the above object, the present invention provides the following solutions:

[0007] The present invention discloses a micron-level instantaneous laser cutting device, comprising a base plate, on which at least one sliding block is arranged, the upper end of each sliding block is connected to a lifting rod, the upper end of the lifting rod is equipped with a laser emitter, a lower clamp is also installed on the base plate, the lower clamp is used to clamp the lower end of a sample to be tested, and an upper clamp is installed on the upper end of the sample to be tested.

[0008] Preferably, a measuring ruler is provided on the substrate.

[0009] Preferably, the upper fixture can be connected to a loading head of a mechanical testing machine.

[0010] Preferably, a laser protection plate is installed on the substrate, and the laser protection plate is an inverted U-shaped plate.

[0011] Preferably, the laser protection plate includes a horizontal plate and two vertical plates parallel to each other, the two vertical plates are respectively fixed to two ends of the horizontal plate, and one of the vertical plates is connected to an extension plate.

[0012] Preferably, the laser protection plate can be connected to an unloading protection plate or a loading protection plate, and both the unloading protection plate and the loading protection plate are L-shaped plates.

[0013] Preferably, the laser emitter is a gas laser, a solid laser or a semiconductor laser.

[0014] Preferably, the sample to be tested is a fiber, a film or a metal rod.

[0015] The present invention also discloses a fiber tensile rebound test method, which uses the above-mentioned micron-level instantaneous laser cutting device and includes the following steps:

[0016] S1. Installation of the test sample: Install the laser protection plate and uninstall the protection plate, and fix the test sample with the upper and lower clamps;

[0017] S2, laser parameter adjustment: adjust the laser emission parameters of the laser transmitter to the set value, remove the unloading protection plate, install the loading protection plate, and adjust the laser cutting position to the center of the sample;

[0018] S3. Test the sample to be tested: apply a preload to the sample to be tested through the upper fixture, use the laser transmitter to cut the sample to be tested, and record the test results. The test is completed.

[0019] Preferably, the cutting in step S3 includes complete cutting and partial cutting, wherein the cutting depth of the partial cutting should be 20-80% of the original thickness of the sample to be tested.

[0020] Compared with the prior art, the present invention has achieved the following technical effects:

[0021] The present invention applies laser cutting technology to the tensile rebound method test. The micron-level instantaneous laser cutting device provided by the present invention has high-speed and high-precision cutting capabilities, and can achieve partial processing or cutting of micron-level materials. For materials with a large aspect ratio at the micron level, in the case of incomplete cutting, the material will experience stress concentration due to the reduction of the effective processing area, thereby causing spontaneous tensile failure of the test sample, ensuring that the preloaded stress is transmitted along the fiber axis, effectively avoiding bending and fracture of the fiber, and ensuring stability during the cutting process.

[0022] In the fiber tensile rebound test method, this partial cutting method that relies on the material's own fracture does not contact the test sample during the cutting process, compared to the original complete cutting method, so it does not introduce mechanical friction or mechanical vibration, ensuring lossless energy transmission and the accuracy of the test results. The cutting time of this cutting method can be controlled in milliseconds or less, and the material tends to be gasified rather than ablated during this process, effectively avoiding the asymmetric axial stress caused by the upward ablation of the flame, and ensuring the stability and safety of the cutting process.

[0023] The present invention enables the sample to be tested to be cut quickly, reduces asymmetric cutting and axial friction during the cutting process, and can infinitely approach the assumption that the back impact compression stress is the same as the pre-tension tension, thereby improving the stability and accuracy of the test results. In addition, the laser protection plate effectively avoids the harm of the laser to the human body, ensuring the stability and safety of the cutting process. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0025] Figure 1 It is a schematic diagram of the structure of the micron-level instantaneous laser cutting device of Example 1 when the laser protection plate is not installed, the protection plate is unloaded, and the protection plate is loaded;

[0026] Figure 2 This is a schematic diagram of the structure of installing and removing the laser protection plate in the micron-level instantaneous laser cutting device of Example 1;

[0027] Figure 3 This is a schematic diagram of the structure of installing a laser protection plate and a loading protection plate in a micron-level instantaneous laser cutting device according to Example 1;

[0028] In the figure: 1-substrate; 2-measuring ruler; 3-lifting rod; 4-laser transmitter; 5-upper fixture; 6-sample to be tested; 7-lower fixture; 8-laser protection plate; 801-extension plate; 9-unloading protection plate; 10-loading protection plate. DETAILED DESCRIPTION

[0029] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0030] The purpose of the present invention is to provide a micron-level instantaneous laser cutting device and a fiber tensile rebound test method to solve the problems existing in the above-mentioned prior art, and to be able to apply laser cutting technology to the tensile rebound test, so as to achieve micron-level precise cutting, small action area, low damage, incomplete cutting, good coaxiality of the rebound stress wave, effectively reduce errors and improve the accuracy of results.

[0031] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.

[0032] Embodiment 1

[0033] like Figure 1-Figure 3 As shown, this embodiment provides a micron-level instantaneous laser cutting device, including a substrate 1, which is a rectangular plate structure. The upper surface of the substrate 1 is provided with at least one sliding block (not shown in the figure), and the sliding block can be one, two or more, and each sliding block is placed on the upper surface of the substrate 1 and can slide on the upper surface of the substrate 1. The upper end of each sliding block is connected to a lifting rod 3, and the lifting rod 3 can adopt an existing hydraulic cylinder, a cylinder or an electric telescopic rod, etc. The upper end (i.e., the telescopic end) of the lifting rod 3 is installed with a laser emitter 4, and the number of sliding blocks, lifting rods 3 and laser emitters 4 is the same and one-to-one corresponding. The lifting rod 3 can drive the laser emitter 4 to move up and down, and the sliding block can drive the laser emitter 4 to move in the horizontal direction. It should be noted that when the number of laser emitters 4 is two or more, each laser emitter 4 is evenly spaced in the circumferential direction with the sample to be tested 6 as the center and the laser action distance as the radius. And the size of the substrate 1 can be modified according to the number of laser emitters 4. A lower clamp 7 is also installed on the substrate 1 , and the lower clamp 7 is used to clamp the lower end of the sample 6 to be tested. An upper clamp 5 is installed on the upper end of the sample 6 to be tested.

[0034] In actual work, it is only necessary to use the upper clamp 5 and the lower clamp 7 to clamp and fix the test sample 6, and the upper clamp 5 and the lower clamp 7 can give a certain pulling force to both ends of the test sample 6, and adjust the position of the laser emitter 4. Finally, start the laser emitter 4 to cut the test sample 6.

[0035] In this embodiment, a measuring ruler 2 is provided on the substrate 1, and the measuring ruler 2 is fixedly arranged along a long side of the substrate 1. The distance between the laser emitter 4 and the sample to be tested 6 can be more intuitively seen through the measuring ruler 2, ensuring that the distance between the laser emitter 4 and the sample to be tested 6 is set to the focal length of the laser.

[0036] In this embodiment, in order to apply pressure to both ends of the test sample 6, the upper fixture 5 can be connected to the upper loading head of the mechanical testing machine, and the substrate 1 can be installed on the supporting component of the mechanical testing machine. The loading head of the mechanical testing machine can give a pulling force to the upper fixture 5, so that the test sample 6 always remains vertical. As for the mechanical testing machine, an existing material mechanical testing machine or fatigue testing machine can be used, as long as it can provide pulling force.

[0037] As for the upper clamp 5 and the lower clamp 7, both use a connecting block and an existing mechanical, pneumatic or electric clamp. The connecting block is fixed to the end of the clamp away from the sample to be tested 6, and the clamp is connected to other structures through the connecting block.

[0038] Furthermore, a tension sensor may be provided on the upper clamp 5 to measure the tension applied to the upper clamp 5 by the mechanical testing machine.

[0039] In this embodiment, if Figure 2-Figure 3 As shown, a laser protection plate 8 is also installed on the substrate 1, and the number of laser protection plates 8 and laser emitters 4 is the same and corresponds one to one. The laser protection plate 8 is an inverted U-shaped plate, which is made of three flat plates welded, bonded or sheet metal. In actual use, the laser emitter 4 after adjusting the position is just located in the laser protection plate 8, and the laser protection plate 8 can effectively cover the emission part of the laser emitter 4, thereby preventing the laser from causing damage to people.

[0040] In this embodiment, if Figure 2 As shown, the laser protection plate 8 includes a horizontal plate and two vertical plates parallel to each other, the upper ends of the two vertical plates are respectively fixed to the two ends of the horizontal plate, and the lower ends of the two vertical plates are fixed to the two sides of the base plate 1. It should be noted that one of the vertical plates is connected to an extension plate 801, and the extension plate 801 is arranged perpendicular to the base plate 1.

[0041] In this embodiment, the laser protection plate 8 can be connected to the unloading protection plate 9 or the loading protection plate 10, and the unloading protection plate 9 and the loading protection plate 10 are both L-shaped plates. When the laser emitter 4 does not need to be started, in order to avoid the accidental start of the laser emitter 4 causing harm to the staff, the unloading protection plate 9 can be installed at this time to block the laser at the emission point of the laser emitter 4, such as Figure 2 As shown, when the unloading protection plate 9 is installed, both sides of the unloading protection plate 9 are perpendicular to the substrate 1, one side is used to block the hole on the side of the laser protection plate 8 away from the laser emitter 4, and the other side is set on the outer side of the vertical plate that is not connected to the extension plate 801. When conducting a test, a loading protection plate 10 can be installed to surround the test sample 6 and prevent the laser from being emitted to the outside, as shown in the figure. Figure 3 As shown, one end of the loading protection plate 10 is perpendicular to and abuts against the extension plate 801 , and the other end of the loading protection plate 10 is connected to the vertical plate that is not connected to the extension plate 801 , so as to surround the test sample 6 .

[0042] In this embodiment, the laser emitter 4 can be any existing gas laser, solid laser or semiconductor laser.

[0043] In this embodiment, the test sample 6 may be a fiber, a film, or a metal rod of various existing materials suitable for the stretch-rebound method.

[0044] Embodiment 2

[0045] This embodiment provides a fiber tensile rebound test method, which uses the micron-level instantaneous laser cutting device disclosed in the first embodiment, and includes the following steps:

[0046] S1. Installation of the test sample 6: Install the laser protection plate 8 and the unloading protection plate 9, and fix the test sample 6 with the upper clamp 5 and the lower clamp 7.

[0047] S2. Adjustment of laser parameters: adjust the laser emission parameters of the laser emitter 4 to the set values, remove the unloading protection plate 9, and install the loading protection plate 10. The adjustment means include adjusting the sliding block, adjusting the lifting and retracting rod, controlling the laser emission position, and adjusting the laser cutting position to the center of the sample to be tested 6.

[0048] S3. Testing of the test sample 6: Place the entire device on the mechanical testing machine, connect the upper clamp 5 to the loading head of the mechanical testing machine, and apply a preload to the test sample 6 through the upper clamp 5 to ensure that the test sample 6 is in a vertically taut state. At this time, use the laser transmitter 4 to cut the test sample 6, and record the test results. The test is completed.

[0049] In this embodiment, the cutting in step S3 includes full cutting and partial cutting, and full cutting means cutting off the test sample 6. This embodiment mainly emphasizes the partial cutting, wherein the cutting depth of the partial cutting should be 20-80% of the original thickness (or diameter if it is a cylindrical structure) of the test sample 6.

[0050] Embodiment 3

[0051] This embodiment provides a specific example of a fiber tensile rebound test method, comprising the following steps:

[0052] S1. Install the laser protection plate 8 and the unloading protection plate 9, fix the carbon fiber sample to be tested with the upper clamp 5 and the lower clamp 7, and connect the upper clamp 5 to the loading head of the mechanical testing machine.

[0053] S2. Adjust the laser emission parameters of the laser emitter 4 to completely cut the fiber or to cut a thickness of 50% of the fiber diameter. Remove the unloading protection plate 9 and replace it with the loading protection plate 10. Adjust the positions of the sliding block, the lifting rod and the laser emitter 4 to adjust the laser cutting position to the center of the carbon fiber sample.

[0054] S3. Apply preload to the carbon fiber sample, cut it using laser cutting method, and record the test results. After calculation, under the cutting conditions of complete fiber cutting or cutting thickness of 50% of fiber diameter, the compressive strength test values ​​of the carbon fiber sample are 1670MPa and 1700MPa respectively.

[0055] The present invention uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only used to help understand the method and core ideas of the present invention. At the same time, for those skilled in the art, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A micron-level instantaneous laser cutting device, characterized in that: It includes a base plate, on which at least one sliding block is arranged, the upper end of each sliding block is connected to a lifting rod, the upper end of the lifting rod is equipped with a laser emitter, a lower clamp is also installed on the base plate, the lower clamp is used to clamp the lower end of the sample to be tested, and the upper end of the sample to be tested is equipped with an upper clamp.

2. The micron-level instantaneous laser cutting device according to claim 1, characterized in that: A measuring ruler is arranged on the substrate.

3. The micron-level instantaneous laser cutting device according to claim 1, characterized in that: The upper fixture can be connected to the loading head of the mechanical testing machine.

4. The micron-level instantaneous laser cutting device according to claim 1, characterized in that: A laser protection plate is installed on the base plate, and the laser protection plate is an inverted U-shaped plate.

5. The micron-level instantaneous laser cutting device according to claim 4, characterized in that: The laser protection plate includes a horizontal plate and two vertical plates parallel to each other. The two vertical plates are respectively fixed at two ends of the horizontal plate, and one of the vertical plates is connected to an extension plate.

6. The micron-level instantaneous laser cutting device according to claim 4, characterized in that: The laser protection plate can be connected to an unloading protection plate or a loading protection plate, and both the unloading protection plate and the loading protection plate are L-shaped plates.

7. The micron-level instantaneous laser cutting device according to claim 1, characterized in that: The laser emitter is a gas laser, a solid laser or a semiconductor laser.

8. The micron-level instantaneous laser cutting device according to claim 1, characterized in that: The sample to be tested is fiber, film or metal rod.

9. A fiber tensile rebound test method, characterized in that: The micron-level instantaneous laser cutting device according to any one of claims 1 to 8 is used, comprising the following steps: S1. Installation of the test sample: Install the laser protection plate and uninstall the protection plate, and fix the test sample with the upper and lower clamps; S2, laser parameter adjustment: adjust the laser emission parameters of the laser transmitter to the set value, remove the unloading protection plate, install the loading protection plate, and adjust the laser cutting position to the center of the sample; S3. Test the sample to be tested: apply a preload to the sample to be tested through the upper fixture, use the laser transmitter to cut the sample to be tested, and record the test results. The test is completed.

10. The fiber tensile rebound test method according to claim 9, characterized in that: The cutting in step S3 includes full cutting and partial cutting, wherein the cutting depth of the partial cutting should be 20-80% of the original thickness of the sample to be tested.