Semiconductor device and manufacturing method thereof
By forming a protective layer on the substrate of the IGBT device and removing it after ion implantation, scratches and contamination problems caused by device contact are solved, and the performance and yield of the device are improved.
Patent Information
- Application Number
- CN202411086928.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-22
AI Technical Summary
In the back process of IGBT devices, the clamp of the equipment contacts the front and causes scratches or contamination, resulting in reduced performance and reduced yield.
A patterned passivation layer is formed on the first surface of the substrate and covered with the first protective layer. After fixed on the carrier device for ion implantation, the protective layer is removed, and the active component is protected by the protective layer to avoid contact with the equipment.
It effectively avoids scratches or contamination on the first surface of the substrate by the equipment, and improves product performance and yield.
Smart Images

Figure CN119008429A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for manufacturing the same. Background Art
[0002] Insulated Gate Bipolar Transistor (IGBT) is a common power device, which is composed of BJT (Bipolar Junction Transistor) and bipolar transistor (Metal Oxide Semiconductor, insulated gate field effect transistor). The ideal IGBT has the advantages of high breakdown voltage, low on-state voltage drop, short turn-off time and long short-circuit resistance time.
[0003] IGBT is a three-terminal device, including: gate, collector and emitter. In the preparation process of IGBT, the back process is usually carried out after the front process is completed. In the back process, multiple processes such as ion implantation, laser annealing and back metallization are generally required.
[0004] However, in the ion implantation and laser annealing processes of the back side process of the IGBT device in the related art, the fixture (or ejector pin) of the corresponding process equipment will directly contact the front side (e.g., active components) of the IGBT device, causing scratches or contamination on the front side of the IGBT device, thereby causing defects and resulting in reduced product performance and yield. Summary of the invention
[0005] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0006] In view of the existing problems, the present invention provides a method for manufacturing a semiconductor device, comprising:
[0007] providing a substrate having a first surface and a second surface opposite to each other, wherein an active component is formed on the first surface of the substrate;
[0008] forming a patterned passivation layer on the first surface of the substrate, the passivation layer exposing a portion of the surface of the active component;
[0009] forming a first protective layer, wherein the first protective layer covers the passivation layer and the exposed surface of the active component;
[0010] Fixing the side of the substrate on which the first protective layer is formed to a carrying device;
[0011] Performing a first ion implantation on the second surface of the substrate to form an implantation region in the second substrate;
[0012] The first protective layer is removed.
[0013] Exemplarily, the method further includes:
[0014] Before forming the implantation region, a second ion implantation is performed on the second surface of the substrate to form a buffer region, wherein the buffer region has a conductivity type different from that of the implantation region.
[0015] Exemplarily, after forming the first protective layer and before placing the side of the substrate on which the first protective layer is formed on the carrier, the method further includes:
[0016] A second protective layer is formed to cover the first protective layer.
[0017] Exemplarily, after forming the second protective layer and before placing the side of the substrate on which the first protective layer is formed on the carrier, the method further includes:
[0018] Performing a thinning process on the second surface of the substrate;
[0019] The second protective layer is removed.
[0020] Exemplarily, after removing the second protective layer and before placing the side of the substrate on which the first protective layer is formed on the carrier, the method further includes:
[0021] An etching process is performed on at least a portion of the second surface of the substrate.
[0022] Exemplarily, when the material of the first protective layer includes titanium, an etching solution is used to remove the first protective layer, the etching solution contains at least hydrogen peroxide, potassium sulfate and potassium ethylenediaminetetraacetate, and the pH value of the etching solution is in the range of 3-4.
[0023] Exemplarily, the method further includes:
[0024] After removing the first protection layer, a collector layer is formed on the second surface of the substrate.
[0025] Exemplarily, the material of the first protective layer includes metal, wherein the metal includes at least one of titanium, tantalum, and nickel.
[0026] Another aspect of an embodiment of the present invention provides a semiconductor device, wherein the semiconductor device is manufactured by using the above method.
[0027] Exemplarily, the semiconductor device includes an IGBT.
[0028] The semiconductor device and manufacturing method of the embodiment of the present invention form a first protective layer covering the passivation layer and the surface of the exposed active components, and remove the first protective layer after the first ion implantation. The first protective layer is used to protect the active components on the first surface of the substrate, which can prevent the equipment from scratching or contaminating the first surface of the substrate during the manufacturing process, thereby improving product performance and device yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] The following drawings of the present invention are used to understand the present invention as part of the present invention. The embodiments of the present invention are shown in the drawings and the description thereof is used to explain the principle of the present invention.
[0030] In the attached figure:
[0031] Figure 1 A flowchart showing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention is shown;
[0032] Figure 2A-2H A cross-sectional schematic diagram of a semiconductor device obtained by sequentially implementing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention is shown. DETAILED DESCRIPTION
[0033] Next, the present invention will be more fully described in conjunction with the accompanying drawings, in which embodiments of the present invention are shown. However, the present invention can be implemented in different forms and should not be construed as being limited to the embodiments set forth herein. On the contrary, providing these embodiments will make the disclosure thorough and complete and fully convey the scope of the present invention to those skilled in the art. In the accompanying drawings, the sizes and relative sizes of layers and regions may be exaggerated for clarity. The same reference numerals throughout represent the same elements.
[0034] It should be understood that when an element or layer is referred to as being "on, adjacent to, connected to or coupled to other elements or layers, it may be directly on, adjacent to, connected to or coupled to other elements or layers, or there may be intervening elements or layers. In contrast, when an element is referred to as being "directly on, directly adjacent to, directly connected to or directly coupled to other elements or layers, there may be no intervening elements or layers. It should be understood that, although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer or part discussed below may be represented as a second element, component, region, layer or part.
[0035] Spatially relative terms such as "under," "below," "below," "under," "above," "above," etc., may be used herein for ease of description to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that in addition to the orientations shown in the figures, the spatially relative terms are intended to include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, then the elements or features described as "under other elements" or "under" or "under" will be oriented as "on" the other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device may be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.
[0036] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present invention. When used herein, the singular forms "a", "an", and "said / the" are also intended to include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0037] Embodiments of the invention are described herein with reference to cross-sectional views that are schematic diagrams of ideal embodiments (and intermediate structures) of the invention. Thus, variations from the shapes shown due to, for example, manufacturing techniques and / or tolerances can be expected. Therefore, embodiments of the invention should not be limited to the specific shapes of the zones shown herein, but include shape deviations due to, for example, manufacturing. For example, an implanted region shown as a rectangle typically has rounded or curved features and / or an implant concentration gradient at its edges, rather than a binary change from an implanted region to a non-implanted region. Similarly, a buried region formed by implantation may result in some implantation in the region between the buried region and the surface through which the implantation is performed. Therefore, the regions shown in the figures are schematic in nature, and their shapes are not intended to show the actual shape of the region of the device and are not intended to limit the scope of the invention.
[0038] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by one of ordinary skill in the art in the field of the present invention. It will also be understood that terms such as those defined in commonly used dictionaries should be understood to have a meaning consistent with their meaning in the context of the relevant art and / or this specification, and should not be interpreted in an ideal or overly formal sense unless expressly defined as such herein.
[0039] In order to fully understand the present invention, detailed steps and structures will be presented in the following description to illustrate the technical solution proposed by the present invention. The preferred embodiments of the present invention are described in detail below, but in addition to these detailed descriptions, the present invention may also have other implementations.
[0040] In the manufacturing process of the IGBT device of the related technology, firstly, active components, such as a gate, an emitter and a conductive wiring layer, are formed on the first surface of the substrate, and then a patterned passivation layer is formed, the passivation layer exposes at least part of the surface of the active components, such as part of the surface of the wiring layer or at least part of the surface of the pad; then the back process is entered, firstly a protective layer is formed to cover the passivation layer and the surface of the exposed active components, and then the second surface of the substrate is thinned, and then after removing the protective layer, ion implantation and laser annealing processes are performed on the second surface of the substrate, and finally a back metallization process is performed to form a collector.
[0041] However, during the ion implantation and laser annealing process on the second surface of the substrate, the protective layer on the first surface of the substrate has been removed, and the fixture (or ejector pin) of the corresponding process equipment will directly contact the front side of the IGBT device (for example, active components), causing scratches or contamination on the front side of the IGBT device, thereby causing defects and reducing product performance and yield.
[0042] In view of the existence of the aforementioned technical problems, an embodiment of the present invention provides a method for manufacturing a semiconductor device, comprising:
[0043] Step S1, providing a substrate, wherein the substrate has a first surface and a second surface opposite to each other, and an active component is formed on the first surface of the substrate;
[0044] Step S2, forming a patterned passivation layer on the first surface of the substrate, wherein the passivation layer exposes a portion of the surface of the active component;
[0045] Step S3, forming a first protective layer, wherein the first protective layer covers the passivation layer and the exposed surface of the active component;
[0046] Step S4, fixing the side of the substrate on which the first protective layer is formed to a carrying device;
[0047] Step S5, performing a first ion implantation on the second surface of the substrate to form an implantation region in the second substrate;
[0048] Step S6, removing the first protective layer.
[0049] The manufacturing method of the semiconductor device in the embodiment of the present invention forms a first protective layer covering the passivation layer and the surface of the exposed active components, and removes the first protective layer after performing the first ion implantation. The active components on the first surface of the substrate are protected by the first protective layer, which can prevent the equipment from scratching or contaminating the first surface of the substrate during the manufacturing process, thereby improving product performance and device yield.
[0050] Embodiment 1
[0051] Below, reference Figures 1 to 2H The method for manufacturing a semiconductor device of the present invention is described in detail, wherein: Figure 1 A flowchart showing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention is shown. Figure 2A-2H A cross-sectional schematic diagram of a semiconductor device obtained by sequentially implementing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention is shown.
[0052] Exemplarily, the semiconductor device of the present application includes an IGBT device, and the semiconductor device may be any suitable device known to those skilled in the art. In this embodiment, the technical solution of the present application is mainly explained and illustrated by taking the case where the semiconductor device is an IGBT device as an example.
[0053] Exemplarily, the method for manufacturing a semiconductor device according to an embodiment of the present invention comprises the following steps:
[0054] First, step S1 is performed to provide a substrate, wherein the substrate has a first surface and a second surface opposite to each other, and an active component is formed on the first surface of the substrate.
[0055] Specifically, Figure 2A As shown, the substrate 200 may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the substrate 200 may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form the substrate 200 are described herein, any material that can be used as the substrate 200 falls within the spirit and scope of the present application.
[0056] Exemplarily, the substrate 200 includes a semiconductor substrate and an epitaxial layer formed on the semiconductor substrate. Optionally, the semiconductor substrate and the epitaxial layer may have the same conductivity type. Exemplarily, the semiconductor substrate and the epitaxial layer may have different doping concentrations, for example, the doping concentration of the epitaxial layer may be lower than the doping concentration of the semiconductor substrate. Exemplarily, the substrate 200 has a first conductivity type, the first conductivity type may be N-type, or the first conductivity type may also be P-type.
[0057] In one example, taking an IGBT device as an example, the active components located on the first surface of the substrate 200 may include structures such as a gate, an emitter, and a conductive wiring layer. Exemplarily, the side of the semiconductor device on which the active components are formed may also be referred to as a functional side, and the side opposite to the functional side is referred to as a back side. The back side of the semiconductor device is also the second surface of the substrate, and the first surface of the substrate 200 in the present application is the functional side.
[0058] Next, step S2 is performed to form a patterned passivation layer on the first surface of the substrate, wherein the passivation layer exposes a portion of the surface of the active component.
[0059] In one example, if Figure 2A As shown, a patterned passivation layer 201 is formed on the first surface of the substrate 200 to protect the substrate 200, wherein the passivation layer 201 exposes a portion of the surface of the active component. Figure 2A As shown, the passivation layer 201 may include a first sub-passivation layer 2011 and a second sub-passivation layer 2012, wherein the first sub-passivation layer 2011 includes a polyamide layer, and the second sub-passivation layer 2012 includes a polyimide layer. In other embodiments, the passivation layer 201 may also be a single-layer or multi-layer structure, and may also be other materials, such as a silicon nitride layer, a silicon oxide layer, a silicon nitride layer, and a silicon oxide layer, etc., which are not limited in the present application. Exemplarily, the patterned passivation layer 201 may be formed by various deposition methods and etching processes commonly used in the art, which are not limited in the present application.
[0060] Next, step S3 is performed to form a first protection layer, wherein the first protection layer covers the passivation layer and the exposed surface of the active component.
[0061] In one example, if Figure 2B As shown, the first protective layer 202 may be formed by various deposition methods commonly used in the art, for example, the first protective layer 202 may be formed by a plasma enhanced chemical vapor deposition (PECVD) method, a low pressure chemical vapor deposition (LPCVD) method, a physical vapor deposition method, or an atomic layer deposition (ALD) method. The formed first protective layer 202 covers the surface of the exposed active component, thereby protecting the first surface of the substrate 200, that is, protecting the active component on the first surface of the substrate 200.
[0062] In one example, the material of the first protective layer 202 includes metal, wherein the metal includes at least one of titanium, tantalum, and nickel, and the wear resistance and hardness of the metal can be used to better protect the first surface of the device. In other examples, the material of the first protective layer 202 can also be any other suitable material.
[0063] In one example, if Figure 2C As shown, after forming the first protective layer 202 in step S3, and before placing the side of the substrate 200 formed with the first protective layer 202 on a carrier device, the method of the present application further includes: forming a second protective layer 203 covering the first protective layer 202. Exemplarily, the second protective layer 203 may also be referred to as a protective tape, which is mainly used to protect the active components and the passivation layer 201 on the first surface of the substrate 200 from contamination by impurities during the subsequent thinning process. Exemplarily, the material of the second protective layer 203 includes at least one of polyurethane, polyimide and the like, or the material of the second protective layer 203 is not particularly limited, and those skilled in the art may flexibly select it as needed, as long as it can play a protective role. Illustratively, after forming the second protective layer 203, the second protective layer 203 may be cured and planarized, for example, by irradiating the second protective layer 203 with ultraviolet light to cure the second protective layer 203, thereby facilitating the subsequent removal of the second protective layer 203; and the second protective layer 203 may be planarized by methods such as but not limited to mechanical planarization methods and chemical mechanical polishing planarization methods, so that more uniform and accurate thickness control can be achieved when the second surface of the substrate 200 is subsequently thinned.
[0064] In one example, if Figure 2D and Figure 2EAs shown, after forming the second protective layer 203, and before placing the side of the substrate 200 formed with the first protective layer 202 on the carrier device, the method of the present application further includes: thinning the second surface of the substrate 200; removing the second protective layer 203. Exemplarily, the purpose of thinning the second surface of the substrate 200 is to thin the thickness of the substrate 200 to reduce internal stress, package height and package volume, and to improve heat dissipation efficiency. The thickness of the thinned substrate 200 is generally 50-300 microns, but it should be understood that the thickness of the thinned semiconductor substrate should be adjusted accordingly according to different products. Exemplarily, the method for thinning the second surface of the substrate 200 can include but is not limited to chemical mechanical grinding or etching processes. Exemplarily, when removing the second protective layer 203, the stickiness of its surface can be removed by light, thereby facilitating the removal of the second protective layer 203.
[0065] In one example, after removing the second protective layer 203 and before placing the side of the substrate 200 formed with the first protective layer 202 on a carrier device, the method of the present application further includes: performing an etching process on at least a portion of the second surface of the substrate 200. Exemplarily, the etching process can be used to eliminate residual stress and defects generated after the thinning process of the substrate 200 and can improve the surface properties of the second surface of the substrate 200 to facilitate the subsequent ion implantation process. Exemplarily, before performing the etching process, the step of cleaning the second surface of the substrate 200 can also be included, and cleaning the second surface of the substrate 200 can remove impurities such as abrasive liquid and particles remaining from the thinning process.
[0066] In one example, the etching process for at least a portion of the second surface of the substrate 200 includes a single wafer spinning wet etching method, and the single wafer spinning wet etching method can better control the uniformity of the etching on the back side of the wafer. Exemplarily, the etching solution used in the single wafer spinning wet etching method includes a combination of hydrofluoric acid, sulfuric acid, nitric acid and phosphoric acid.
[0067] Next, step S4 is performed to place the side of the substrate formed with the first protective layer on a carrier. For example, in a subsequent step, the second surface of the substrate 200 needs to be implanted with the first ion, so the side of the substrate 200 formed with the first protective layer 202 needs to be disposed toward the carrier, so that the second surface of the substrate 200 is disposed upward. For example, the carrier includes an ion implantation machine, and a pin or a fixture may be disposed on the carrier.
[0068] Next, step S5 is performed to perform a first ion implantation on the second surface of the substrate to form an implantation region in the second substrate.
[0069] In one example, if Figure 2F As shown, a first ion implantation can be performed by an ion implantation machine to form an implantation region 205. The implanted ions of the first ion implantation can be N-type ions or P-type ions. It should be understood that the implanted ions and the dosage range should be adjusted accordingly according to different products.
[0070] In one example, if Figure 2F As shown, the method of the present application also includes: before performing the first ion implantation, performing a second ion implantation on the second surface of the substrate 200 to form a buffer zone 204, wherein the buffer zone 204 has a conductivity type different from that of the implantation zone 205. Exemplarily, taking the implantation zone 205 having a P-type conductivity type as an example, the implanted ions of the second ion implantation are N-type ions, and the buffer zone 204 has an N-type conductivity type. The N-type ions may be ions such as phosphorus, arsenic, or antimony, and the P-type ions may be ions such as boron, aluminum, or gallium. In some examples, the buffer zone 204 may be an N-type heavily doped region, while the implantation zone 205 is a P-type heavily doped region.
[0071] In one example, after the second ion implantation and the first ion implantation, an annealing process should be performed to activate the implanted ions and diffuse the ions to form the desired doping region, and at the same time repair the lattice structure damaged in the ion implantation process, thereby obtaining the activated buffer region 204 and the implantation region 205. Exemplarily, the annealing process of the present application includes a laser annealing process, which has a faster heating speed and a higher control sensitivity than the traditional annealing process, thereby making the production efficiency and reliability of the final product higher.
[0072] In one example, when performing ion implantation and annealing processes, the side of the substrate 200 formed with the first protective layer 202 is placed on a carrier device, and the first protective layer 202 can cover the passivation layer and the surface of the exposed active components, thereby protecting the active components on the first surface of the substrate 200 to prevent the first surface of the substrate from being scratched or contaminated by equipment (for example, ejector pins or fixtures on the carrier device) during the manufacturing process, thereby improving product performance and device yield.
[0073] Finally, execute step S6, such as Figure 2G As shown, the first protective layer 202 is removed. By way of example, various etching processes commonly used in the art may be used to remove the first protective layer 202, for example, a wet etching process may be used to remove the first protective layer 202.
[0074] In one example, any suitable etching method may be used to remove the first protection layer 202 , and the etching method only etches the first protection layer 202 and hardly corrodes other metals (eg, pads, etc.) in the semiconductor device.
[0075] Specifically, when the material of the first protective layer 202 includes titanium, an etching solution can be used to etch and remove the first protective layer 202, and the etching solution contains at least hydrogen peroxide, potassium sulfate and potassium ethylenediaminetetraacetate, and the pH value of the etching solution is in the range of 3-4, so that other metals (for example, copper, aluminum, etc.) will not be corroded when the first protective layer 202 is removed. Among them, the pH value of the etching solution can be controlled within the range of 3-4 using hydrofluoric acid. Exemplarily, the content of hydrogen peroxide can be 160g / L-180g / L, the content of potassium sulfate can be 150g / L-210g / L, and the content of potassium ethylenediaminetetraacetate can be 0.08g / L-0.12g / L. For these reagents, other suitable contents can also be used under the premise of meeting the requirements.
[0076] In one example, if Figure 2H As shown, the method of the present application also includes: after removing the first protective layer 202, forming a collector layer 206 on the second surface of the substrate. Exemplarily, the method of forming the collector layer 206 is not particularly limited, and those skilled in the art can flexibly select as needed. For example, the collector layer 206 can be formed on the second surface of the substrate by an evaporation process, and the evaporation process can make the collector layer 206 form an ohmic contact with the injection region 205, and can reduce the contact resistance. Exemplarily, the material of the collector layer 206 is not particularly limited, including but not limited to at least one of a metal layer formed by superimposing titanium, nickel and silver, a metal layer formed by superimposing nickel and silver, and a metal layer formed by superimposing aluminum, titanium, nickel and silver, that is, TiNiAg, NiAg, AlTiNiAg, etc.
[0077] So far, the description of the key steps of the method for manufacturing the semiconductor device of the present invention has been completed. The manufacture of a complete semiconductor device may also include other steps, which will not be described one by one here. It is worth mentioning that the order of the above steps can be adjusted without conflict.
[0078] In summary, the method for manufacturing a semiconductor device according to an embodiment of the present invention forms a first protective layer covering the surface of the passivation layer and the exposed active components, and removes the first protective layer after performing the first ion implantation. The first protective layer protects the active components on the first surface of the substrate, which can prevent the equipment from scratching or contaminating the first surface of the substrate during the manufacturing process, thereby improving product performance and device yield. More specifically, the first protective layer is removed after performing the first ion implantation and annealing process, which can prevent the equipment from scratching or contaminating the first surface of the substrate during the ion implantation and annealing process.
[0079] Embodiment 2
[0080] The present invention also provides a semiconductor device, which is prepared by the method in the above-mentioned embodiment 1. Specifically, Figure 2G As shown, the semiconductor device includes a substrate 200, a passivation layer 201, a buffer area 204 and an injection area 205, wherein an active component is formed on the first surface of the substrate 200, the passivation layer 201 is located on the first surface of the substrate 200 and exposes a portion of the surface of the active component, and the buffer area 204 and the injection area 205 are located on the second surface of the substrate 200.
[0081] Exemplarily, the semiconductor device of the present application includes an IGBT device, and the semiconductor device may be any suitable device known to those skilled in the art. In this embodiment, the technical solution of the application is mainly explained and illustrated by taking the case where the semiconductor device is an IGBT device as an example.
[0082] In one example, if Figure 2G As shown, the substrate 200 may include at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP, InGaAs or other III / V compound semiconductors, or the substrate 200 may also include silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) or germanium on insulator (GeOI), etc. Although several examples of materials that can form the substrate 200 are described herein, any material that can be used as the substrate 200 falls within the spirit and scope of the present application.
[0083] In one example, taking an IGBT device as an example, the active components located on the first surface of the substrate 200 may include structures such as a gate, an emitter, and a conductive wiring layer. Exemplarily, the side of the semiconductor device on which the active components are formed may also be referred to as a functional side, and the side opposite to the functional side is referred to as a back side. The back side of the semiconductor device is also the second surface of the substrate, and the first surface of the substrate 200 in the present application is the functional side.
[0084] In one example, if Figure 2G As shown, the passivation layer 201 may include a first sub-passivation layer 2011 and a second sub-passivation layer 2012, wherein the first sub-passivation layer 2011 includes a polyamide layer, and the second sub-passivation layer 2012 includes a polyimide layer. In other embodiments, the passivation layer 201 may also be a single-layer or multi-layer structure, and may also be other materials, such as a silicon nitride layer, a silicon oxide layer, a silicon nitride layer, and a silicon oxide layer, etc., which is not limited in the present application.
[0085] In one example, the buffer region 204 has a different conductivity type from the implantation region 205. For example, taking the implantation region 205 as having a P-type conductivity type, the implanted ions of the second ion implantation are N-type ions, and the buffer region 204 has an N-type conductivity type. The N-type ions may be ions such as phosphorus, arsenic, or antimony, and the P-type ions may be ions such as boron, aluminum, or gallium. In some examples, the buffer region 204 may be an N-type heavily doped region, while the implantation region 205 is a P-type heavily doped region.
[0086] In one example, if Figure 2H As shown, a collector layer 206 is also included on the second surface of the substrate 200. Exemplarily, the material of the collector layer 206 is not particularly limited, including but not limited to at least one of a metal layer formed by superposition of titanium, nickel and silver, a metal layer formed by superposition of nickel and silver, and a metal layer formed by superposition of aluminum, titanium, nickel and silver, i.e., TiNiAg, NiAg, AlTiNiAg, etc.
[0087] The structure of the semiconductor device of the present invention has been introduced so far. The complete device may also include other component structures, which will not be described in detail here.
[0088] The semiconductor device of the embodiment of the present invention is prepared by the method in the aforementioned embodiment 1, and a first protective layer covering the surface of the passivation layer and the exposed active components is formed, and the first protective layer is removed after the first ion implantation. The active components on the first surface of the substrate are protected by the first protective layer, which can prevent the equipment from scratching or contaminating the first surface of the substrate during the manufacturing process, thereby improving product performance and device yield. More specifically, the first protective layer is removed after the first ion implantation and annealing process, which can prevent the equipment from scratching or contaminating the first surface of the substrate during the ion implantation and annealing process.
[0089] Although multiple embodiments are described herein, it should be understood that a variety of other modifications and embodiments may be conceived by those skilled in the art, all of which will fall within the spirit and scope of the concepts disclosed in the present invention. More particularly, various modifications and changes may be made to the arrangements and / or components of the combined arrangements of the subject matter within the scope of the present disclosure, the drawings, and the appended claims. In addition to modifications and changes to the components and / or arrangements, the use of alternatives is also an obvious option for those skilled in the art.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: The method comprises: providing a substrate having a first surface and a second surface opposite to each other, wherein an active component is formed on the first surface of the substrate; forming a patterned passivation layer on the first surface of the substrate, the passivation layer exposing a portion of the surface of the active component; forming a first protective layer, wherein the first protective layer covers the passivation layer and the exposed surface of the active component; Placing the side of the substrate on which the first protective layer is formed on a carrying device; Performing a first ion implantation on the second surface of the substrate to form an implantation region in the second substrate; The first protective layer is removed.
2. The manufacturing method according to claim 1, characterized in that: The method further comprises: Before forming the implantation region, a second ion implantation is performed on the second surface of the substrate to form a buffer region, wherein the buffer region has a conductivity type different from that of the implantation region.
3. The manufacturing method according to claim 1, characterized in that: After forming the first protective layer and before placing the side of the substrate on which the first protective layer is formed on the carrier, the method further includes: A second protective layer is formed to cover the first protective layer.
4. The manufacturing method according to claim 3, characterized in that: After forming the second protective layer and before placing the side of the substrate on which the first protective layer is formed on the carrier, the method further includes: Performing a thinning process on the second surface of the substrate; The second protective layer is removed.
5. The manufacturing method according to claim 4, characterized in that: After removing the second protective layer and before placing the side of the substrate on which the first protective layer is formed on the carrier, the method further includes: An etching process is performed on at least a portion of the second surface of the substrate.
6. The manufacturing method according to claim 1, characterized in that: When the material of the first protective layer includes titanium, an etching solution is used to remove the first protective layer. The etching solution at least contains hydrogen peroxide, potassium sulfate and potassium ethylenediaminetetraacetate, and the pH value of the etching solution is in the range of 3-4.
7. The manufacturing method according to claim 1, characterized in that: The method further comprises: After removing the first protection layer, a collector layer is formed on the second surface of the substrate.
8. The manufacturing method according to claim 1, characterized in that: The material of the first protective layer includes metal, wherein the metal includes at least one of titanium, tantalum and nickel.
9. A semiconductor device, characterized in that: The semiconductor device is manufactured by the method according to any one of claims 1 to 8.
10. The semiconductor device according to claim 9, characterized in that The semiconductor device includes an IGBT.