ICS package substrate with press-fit binding force enhancing structure and preparation method of ICS package substrate

By setting a rough copper surface and a locking copper ring on the outer surface of the inner copper layer of the packaging substrate, and filling the PP layer with a locking structure during pressing, the problems of insufficient bonding force of the inner copper skin and excessive hole recesses are solved. , improves binding force and heat dissipation efficiency, and achieves higher packaging performance.

CN119008538APending Publication Date: 2024-11-22DONGGUAN KANGYUAN ELECTRONICS CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411127684.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-16
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In power supply and high voltage packaging substrates, the bonding force between the inner large copper skin and PP is insufficient, and the electroplating filling of large holes is difficult to achieve flatness, resulting in excessive recesses of holes and high risk of layering.

Method used

Design an ICS package substrate with enhanced compression bonding force. By setting a rough copper surface and a lock copper ring on the outer surface of the inner copper layer, and filling the PP layer around the lock copper ring during compression process to form a lock buckle structure to improve binding force. The substrate includes a base plate, an inner copper layer, a PP layer and an outer copper layer. The locking copper ring is embedded in the groove, and the outer surface is inclined from top to bottom to form an inverted structure, increasing the copper skin area and heat conduction effect.

Benefits of technology

Effectively improve the bonding force between the PP layer and the inner copper layer, solve the problem of insufficient bonding force caused by the large copper skin of the inner layer, and avoid the risks of excessive recesses and layering by filling the copper ring structure, and improve the heat dissipation efficiency of the packaging substrate. and overall performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008538A_ABST
    Figure CN119008538A_ABST
Patent Text Reader

Abstract

The invention discloses an ICS packaging substrate with a lamination binding force enhancing structure and a preparation method thereof. The ICS packaging substrate comprises a bottom plate, an inner side copper layer, a PP layer and an outer side copper layer, the inner side copper layers are arranged on the upper side face and the lower side face of the bottom plate, the PP layers are arranged on the outer surfaces of the inner side copper layers, and the outer side copper layers are arranged on the outer sides of the PP layers. A rough copper surface and a lock catch copper ring are arranged on the outer surface of the inner side copper layer, the lock catch copper ring protrudes out of the rough copper surface, the lock catch copper ring is arranged in a circular ring shape, and the periphery of the lock catch copper ring is high, and the inner side of the lock catch copper ring is gradually lowered from top to bottom; a rough copper surface is also arranged on the outer surface of the lock catch copper ring; a groove is formed in the bottom face, corresponding to the lock catch copper ring, of the PP layer, and the lock catch copper ring is embedded in the groove. The copper sheet area is effectively increased, and the heat conduction effect is improved; and the binding force between the PP layer and the inner copper layer is greatly improved. And meanwhile, the problem that the hole recess is too large due to the fact that electroplating is difficult to fill and level due to a large hole is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a packaging substrate, and in particular to an IC packaging substrate with a press-fit bonding force enhancement structure and a preparation method thereof. Background Art

[0002] The package substrate is Substrate (SUB for short). The substrate can provide electrical connection, protection, support, heat dissipation, assembly and other functions for the chip to achieve multi-pin, reduce the size of the packaged product, improve electrical performance and heat dissipation, ultra-high density or multi-chip modularization. At present, in the power supply and high voltage package substrate, in order to facilitate heat dissipation, the design of a large inner copper skin often appears. However, due to the large area and flat surface of the inner copper skin, there is a certain risk of delamination after it is combined with PP.

[0003] In addition, in order to improve the heat dissipation efficiency, some power supplies and high-voltage packaging substrates will also be provided with large holes. Due to the requirements of heat dissipation, resin plugging is usually not allowed, and copper plating is used. However, because the holes are large, it is difficult to fill them during electroplating, resulting in the problem of excessive hole depression. The conventional processing method is to grind the holes flat, however, this method will increase the deformation of the substrate, and the flat surface after grinding is not conducive to the combination of the large copper surface and PP, and the risk of delamination is high. Therefore, how to fill the holes and ensure the bonding strength between the large copper skin and PP without delamination during the processing process has become the main difficulty in the processing of such products. Summary of the invention

[0004] Based on this, it is necessary to provide an ICS packaging substrate with a press-fit bonding force enhancement structure and a preparation method thereof to address the deficiencies in the prior art, so as to solve at least one technical problem in the above-mentioned background technology.

[0005] An ICS packaging substrate with a press-fit bonding force enhancement structure comprises a bottom plate, an inner copper layer, a PP layer and an outer copper layer; the inner copper layer is arranged on the upper and lower side surfaces of the bottom plate, the PP layer is arranged on the outer surface of the inner copper layer, and the outer copper layer is arranged on the outer side of the PP layer; the outer surface of the inner copper layer is provided with a rough copper surface and a locking copper ring, the locking copper ring protrudes from the rough copper surface, the locking copper ring is arranged in a circular ring shape, and has a high periphery and a gradually lower inner side from top to bottom; a rough copper surface is also arranged on the outer surface of the locking copper ring; the PP layer is formed with a groove on the bottom surface corresponding to the locking copper ring, and the locking copper ring is embedded in the groove.

[0006] Furthermore, a heat dissipation hole is arranged on the bottom plate, and the locking copper ring is arranged on the outside of the heat dissipation hole. The heat dissipation hole is filled with copper and is integrally connected with the inner copper layer.

[0007] Furthermore, the aperture of the groove is larger than the outermost aperture of the heat dissipation hole.

[0008] Furthermore, the height of the locking copper ring is less than or equal to one third of the thickness of the PP layer.

[0009] Furthermore, the outer surface of the lock copper ring is extended inwardly from top to bottom to form an inverted structure.

[0010] A method for preparing an IC packaging substrate with a press-fit bonding strength enhancement structure comprises the following steps:

[0011] Step 1: electroplating: electroplating the outer surface of the base plate to form an inner copper layer;

[0012] Step 2, pressing the dry film; pressing the dry film on the outer surface of the inner copper layer, and exposing the hole at the set position to form a boss hole;

[0013] Step 3, electroplating to fill the hole; forming a concave ring in the boss hole, the outer surface of the concave ring forms an outer groove with a concave middle, the lowest position of the bottom end of the outer groove is higher than the outer surface of the inner copper layer and lower than the outer surface of the dry film;

[0014] Step 4, removing the dry film; removing the dry film on the outside, micro-etching the inner copper layer, and then roughening the copper surface with potassium acid solution to obtain a rough copper surface and a lock copper ring;

[0015] Step six, pressing; laminating the PP layer on the outside, the resin of the PP layer is filled around the locking copper ring and the inner and outer side walls, and the locking copper ring and the PP layer form a locking structure.

[0016] Furthermore, in step three and step four, a copper reduction step is also included, and when the copper thickness exceeds the requirement, the concave ring is subjected to copper reduction treatment.

[0017] Furthermore, in step three, the current used for electroplating is gradually increased from a relatively small current.

[0018] Furthermore, the diameter of the boss hole needs to be greater than or equal to 100 um.

[0019] Furthermore, the bottom plate is also provided with heat dissipation holes. In step three, the heat dissipation holes and boss holes are filled with electroplating.

[0020] In summary, the present invention effectively increases the copper skin area and improves the heat conduction effect by providing a straight rough copper surface and a lock copper ring on the outer surface of the inner copper layer; during pressing, the PP layer will fill the periphery and inner and outer side walls of the lock copper ring, so that the PP layer and the lock copper ring form a lock-like structure, greatly improving the bonding force between the PP layer and the inner copper layer. The bonding force problem caused by the inner layer being designed as a large copper skin is solved, and at the same time, the problem of the hole being too large due to the difficulty of electroplating to fill the large hole is solved. The present invention has strong practicality and strong promotion significance. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 It is a structural schematic diagram of a first embodiment of an ICS packaging substrate with a press-fit bonding force enhancement structure of the present invention;

[0022] Figure 2 for Figure 1 Schematic diagram of the outer surface structure of the inner copper layer;

[0023] Figure 3 for Figure 1 A schematic flow chart of a method for preparing a packaging substrate;

[0024] Figure 4 It is a structural schematic diagram of a second embodiment of an ICS packaging substrate with a press-fit bonding force enhancement structure of the present invention;

[0025] Figure 5 for Figure 4 Schematic diagram of the process flow of the method for preparing a packaging substrate. DETAILED DESCRIPTION

[0026] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0027] like Figure 1 and Figure 2 As shown, it is an IC CS packaging substrate provided by the present invention, and the IC CS packaging substrate includes a base plate 10, an inner copper layer 20, a PP layer 30 and an outer copper layer 40. The inner copper layer 20 is arranged on the upper and lower sides of the base plate 10, and a heat dissipation hole 11 is arranged on the base plate 10. The heat dissipation hole 11 is filled with copper and is integrally connected with the inner copper layer 20. The PP layer 30 is arranged on the outer surface of the inner copper layer 20. The outer copper layer 40 is arranged on the outer side of the PP layer 30.

[0028] In this embodiment, the heat dissipation hole 11 is in a structure that is small in the middle and gradually becomes larger on both sides. The outer surface of the inner copper layer 20 is provided with a rough copper surface 21 and a lock copper ring 22, and the rough copper surface 21 has a plurality of grooves and protrusions to increase the bonding area with the PP layer 30. The lock copper ring 22 protrudes from the rough copper surface 21. The lock copper ring 22 is arranged in a circular ring shape, and has a high periphery and a gradually lower structure from top to bottom on the inside. A rough copper surface is also provided on the outer surface of the lock copper ring 22, and the rough copper surface is provided with protrusions and recessed portions to increase the bonding area between the inner copper layer 20 and the PP and improve the bonding force. Furthermore, the outer surface of the lock copper ring 22 is arranged to extend inwardly from top to bottom in an inclined manner, thereby forming an inverted structure.

[0029] The PP layer 30 is formed with a groove on the bottom surface corresponding to the locking copper ring 22, and the locking copper ring 22 is embedded in the groove. In this embodiment, the aperture of the groove is larger than the outermost aperture of the heat dissipation hole 11. The thickness of the locking copper ring 22 is less than or equal to 1 / 3 of the thickness of the PP layer 30.

[0030] like Figure 3 As shown, it is a method for preparing an IC packaging substrate with a press-fit bonding strength enhancement structure provided by the present invention, which is used to prepare Figure 1 The method for preparing the I CS packaging substrate with a press-fit bonding strength enhancement structure specifically comprises the following steps:

[0031] Step 1: drilling and electroplating: drilling the heat dissipation hole 11 on the bottom plate 10, and performing bottom electroplating on the outer surface of the bottom plate 10 to form the inner copper layer 20, wherein the inner copper layer 20 covers the outer surface of the bottom plate 10 and the heat dissipation hole 11;

[0032] Step 2, pressing the dry film 50; pressing the dry film 50 on the outer surface of the inner copper layer 20, and then making an exposure hole opening at the position corresponding to the heat dissipation hole 11 to form a boss hole 51.

[0033] Since there will be a certain position deviation when the pattern is transferred, the aperture of the boss hole 51 should be larger than the aperture of the heat dissipation hole 11 to prevent the dry film 50 from entering the hole and causing bubbles and cavities during subsequent electroplating. In this embodiment, the dry film 50 is vacuum pressed to prevent bubbles.

[0034] Step 3, electroplating and filling the holes; electroplating and filling the heat dissipation holes 11 and the boss holes 51, and forming a concave ring 52 in the boss hole 51, the outer surface of the concave ring 52 forms an outer groove 53, the bottom surface of the outer groove 53 is a spherical shape with a concave middle part, and the lowest position of the bottom end of the outer groove 53 is higher than the outer surface of the inner copper layer 20 and lower than the outer surface height of the dry film 50.

[0035] The dry film 50 can make the heat dissipation hole 11 become a deep hole, and the larger the aspect ratio, the more difficult it is to fill, so that when the hole is filled by electroplating, the electroplated hole can be concave to avoid the problem of forming a bulge outward, which leads to the problem of concave copper surface after copper reduction.

[0036] During electroplating, the electroplating parameters need to use smaller current parameters and continuously strengthen them so that the heat dissipation holes form a continuous current and eventually form a concave ring.

[0037] Step 4: Reduce copper (not shown in the figure); Since there is still circuit pattern processing in the later process, the final height of the concave ring 52 needs to be controlled. Since it is covered by the dry film 50, the thickness of the concave ring can be measured based on the thickness of the dry film 50. If the copper thickness exceeds the requirement, the concave ring 52 can be reduced to the corresponding height by reducing copper because the dry film 50 protects the copper surface.

[0038] Step 5, remove the dry film 50; remove the outer dry film 50. At this time, the concave ring 52 produced is flat and regular, and the height is relatively high, which will puncture the subsequent circuit dry film 50 and fail to meet the requirements of effectively increasing the bonding force. Therefore, the inner copper layer 20 is micro-etched with hydrogen peroxide solution to etch it into a circular ring shape and reduce its height to maximize the cross-sectional area and meet the thickness requirements of the dry film 50. Then the copper surface is roughened with potassium acid solution to form coarse grains of varying roughness on the concave ring 52 and its surface; further increase the contact area between copper and PP. In this process, the copper surface of the inner copper layer 20 will also be roughened to form a rough copper surface 21. Since the greater the degree of micro-etching, the higher the degree of coarsening, the micro-etching amount here needs to be greater than 3um, so the circuit pattern needs to be compensated in advance, and finally the required rough copper surface 21 and lock copper ring 22 are obtained.

[0039] Step 6: Lamination: During lamination, the resin of the PP layer 30 not only combines with the rough copper surface 21, but also fills the rough surface around and on the outer surface of the lock copper ring 22, and finally forms a mortise and tenon structure on the inner and outer walls of the lock copper ring 22, so that the PP layer 30 and the lock copper ring 22 are firmly combined and cannot be separated. After that, the product is subjected to thermal stress and reflow soldering, and the substrate still has no delamination phenomenon.

[0040] like Figure 4 As shown, it is a schematic diagram of the structure of a second embodiment of an I CS packaging substrate of the present invention, and its structure is basically the same as that of the first embodiment, except that the I CS packaging substrate in this embodiment does not have a heat dissipation hole 11.

[0041] like Figure 5 As shown, it is a second embodiment of a method for preparing an IC packaging substrate with a press-fit bonding strength enhancement structure of the present invention. This embodiment is used to prepare Figure 4 The method of this embodiment is basically the same as that of the first embodiment, except that there is no hole. Therefore, the bottom plating does not need to be plated into the hole, and the window of the dry film 50 is opened to a preset position, not a corresponding through hole. In addition, in this embodiment, the large aperture of the boss hole 51 formed by the window of the dry film 50 needs to be greater than or equal to 100um, so as to ensure that the concave ring 52 has a certain depression after plating.

[0042] In summary, the present invention effectively increases the copper skin area and improves the heat conduction effect by providing a straight rough copper surface 21 and a lock copper ring 22 on the outer surface of the inner copper layer; during pressing, the PP layer 30 will fill the periphery and inner and outer side walls of the lock copper ring 22, so that the PP layer 30 and the lock copper ring 22 form a lock-like structure, greatly improving the bonding force between the PP layer 30 and the inner copper layer 20. The bonding force problem caused by the inner layer being designed as a large copper skin is solved, and the problem of excessive hole depression caused by the difficulty of electroplating to fill the large hole is solved. The present invention has strong practicality and strong promotion significance.

[0043] The above-mentioned embodiments only express two implementation modes of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. An ICS packaging substrate with a press-fit bonding strength enhancement structure, characterized in that: It comprises a bottom plate, an inner copper layer, a PP layer and an outer copper layer; the inner copper layer is arranged on the upper and lower side surfaces of the bottom plate, the PP layer is arranged on the outer surface of the inner copper layer, and the outer copper layer is arranged on the outer side of the PP layer; the outer surface of the inner copper layer is provided with a rough copper surface and a lock copper ring, the lock copper ring protrudes from the rough copper surface, the lock copper ring is arranged in a circular ring shape, and has a high periphery and a gradually lower inner side from top to bottom; a rough copper surface is also provided on the outer surface of the lock copper ring; the PP layer is formed with a groove on the bottom surface corresponding to the lock copper ring, and the lock copper ring is embedded in the groove.

2. The ICS packaging substrate with a press-fit bonding strength enhancement structure according to claim 1, characterized in that: The bottom plate is provided with a heat dissipation hole, the locking copper ring is arranged outside the heat dissipation hole, the heat dissipation hole is filled with copper and is integrally connected with the inner copper layer.

3. The ICS packaging substrate with a press-fit bonding strength enhancement structure according to claim 2, characterized in that: The aperture of the groove is larger than the outermost aperture of the heat dissipation hole.

4. The ICS packaging substrate with a press-fit bonding strength enhancement structure according to claim 1, characterized in that: The height of the locking copper ring is less than or equal to one third of the thickness of the PP layer.

5. The ICS packaging substrate with a press-fit bonding strength enhancement structure according to claim 1, characterized in that: The outer surface of the lock copper ring is extended inwardly from top to bottom to form an inverted structure.

6. A method for preparing an ICS packaging substrate having a press-fit bonding strength enhancement structure, characterized in that: The steps include: Step 1: electroplating: electroplating the outer surface of the base plate to form an inner copper layer; Step 2, pressing the dry film; pressing the dry film on the outer surface of the inner copper layer, and exposing the hole at the set position to form a boss hole; Step 3, electroplating to fill the hole; forming a concave ring in the boss hole, the outer surface of the concave ring forms an outer groove with a concave middle, the lowest position of the bottom end of the outer groove is higher than the outer surface of the inner copper layer and lower than the outer surface of the dry film; Step 4, removing the dry film; removing the dry film on the outside, micro-etching the inner copper layer, and then roughening the copper surface with potassium acid solution to obtain a rough copper surface and a lock copper ring; Step six, pressing; laminating the PP layer on the outside, the resin of the PP layer is filled around the locking copper ring and the inner and outer side walls, and the locking copper ring and the PP layer form a locking structure.

7. The method for preparing an ICS packaging substrate having a press-fit bonding strength enhancement structure according to claim 6, characterized in that: In step three and step four, a copper reduction step is also included. When the copper thickness exceeds the requirement, the concave ring is subjected to copper reduction treatment.

8. The method for preparing an ICS packaging substrate having a press-fit bonding strength enhancement structure according to claim 6, wherein: In step three, the current used for electroplating is gradually increased from a relatively small current.

9. The method for preparing an ICS packaging substrate having a press-fit bonding strength enhancement structure according to claim 6, wherein: The diameter of the boss hole must be greater than or equal to 100um.

10. The method for preparing an ICS packaging substrate having a press-fit bonding strength enhancement structure according to claim 6, characterized in that: The bottom plate is also provided with heat dissipation holes. In step three, the heat dissipation holes and boss holes are filled by electroplating.