Anti-corona manufacturing process for stator bar of high-capacity steam turbine generator
By creating an equipotential layer on the stator bars of a large-capacity steam turbine generator and wrapping it with specific strips, combined with vacuum impregnation, the corona discharge problem was solved, achieving a simple and efficient anti-corona manufacturing process, and improving electrical performance and environmental friendliness.
Patent Information
- Application Number
- CN202411258728.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-09
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-09-09
AI Technical Summary
Large-capacity steam turbine generator stator bars are prone to corona discharge at high voltage levels. Existing manufacturing processes are cumbersome and cause serious environmental pollution, affecting the safe operation of the unit.
The stator bars are pretreated by first creating an equipotential layer, then sequentially wrapping them with main insulation mica tape, low-resistance anti-corona tape, high-resistance anti-corona tape, low-resistance isolation anti-corona tape, and PTFE release tape. The main insulation and anti-corona treatment are completed in one step by vacuum impregnation.
The manufacturing process has been simplified, the electric field balance and anti-corona effect have been improved, the axial slippage of the stator bars has been ensured, it is environmentally friendly and easy to operate, and its electrical performance meets the imported standards.
Smart Images

Figure CN119010496A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of generator stator wire bar manufacturing, and in particular to an anti-corona manufacturing process for large-capacity steam turbine generator stator wire bar. Background Art
[0002] A steam turbine generator is a synchronous generator driven by a steam turbine. In the process of power generation, a steam turbine generator uses different energy sources such as coal, natural gas, nuclear energy, and hydropower to drive the steam turbine to generate electricity. The steam turbine is used as the prime mover to drive the rotor to rotate, and the mechanical energy is converted into electrical energy through the principle of electromagnetic induction. Steam turbine generators are characterized by high efficiency, stability, and large capacity, and are widely used in the fields of power generation, industrial production, and aerospace.
[0003] The most basic components of a steam turbine generator are the rotor, stator, excitation system and cooling system. Among them, the rotor is the power source of the steam turbine generator, and its main function is to convert mechanical energy into electrical energy; the stator is the key component for generating alternating current, and the stator is mainly composed of stator core, stator winding and frame. The stator core is an important component that constitutes the magnetic circuit and fixes the stator winding. It is usually made of cold-rolled silicon steel sheets with good magnetic conductivity. The stator winding is a coil formed by connecting the stator wire rods embedded in the stator core slots at the ends. The stator wire rods of medium and small steam turbine generators are all solid wire rods, while large steam turbine generators use internally cooled wire rods due to the need for heat dissipation, such as a number of solid wire rods and hollow wire rods that can pass water in parallel.
[0004] In recent years, the capacity of steam turbine generators has been continuously improved with the development and improvement of science and technology. However, when the voltage level of large-capacity steam turbine generators is increased to a certain level, corona discharge is prone to occur. The corona discharge phenomenon will cause the gradual corrosion and failure of the stator main insulation material until it breaks down, threatening the safe operation of the unit. At present, the stator wire bars of large-capacity and high-voltage generators will adopt a manufacturing process that combines an internal equipotential layer and an external anti-corona layer to deal with this corona discharge phenomenon. The internal equipotential layer of the stator wire bar is mostly achieved by brushing semi-conductive paint on the side of the stator wire bar before wrapping the main insulation. The semi-conductive paint is easy to fall off during the subsequent handling or wrapping process, and the shielding and balanced electric field effect is not good. The outer anti-corona layer is generally made by painting after the main insulating mica layer is formed and cured, or by wrapping the main insulating mica layer with a conductive tape after being dipped in paint and then hot-pressed and cured. The ends of high-voltage stator bars generally require segmented anti-corona. Most of these external anti-corona manufacturing processes are discontinuous forming processes. On the one hand, the multi-stage anti-corona process is relatively cumbersome. On the other hand, painting or dipping the main insulating mica layer in paint and then wrapping it with a conductive tape can easily cause environmental pollution and harm the health of employees. Summary of the invention
[0005] Aiming at the technical problem that corona discharge is easy to occur in the stator wire rod of a large-capacity steam turbine generator, the present invention provides an anti-corona manufacturing process for the stator wire rod of a large-capacity steam turbine generator, which comprises the following steps: firstly making an equipotential layer, and then wrapping the stator wire rod with a main insulating mica tape, a low-resistance anti-corona tape, a high-resistance anti-corona tape, a low-resistance isolation anti-corona tape and a polytetrafluoroethylene demolding tape in sequence from the inside to the outside, and then placing the pretreated stator wire rod in a mold for vacuum dipping and varnishing treatment. The main insulation and anti-corona treatment of the stator wire rod can be completed by only one dipping and curing. The manufacturing process is simple and environmentally friendly, and the anti-corona effect is stable.
[0006] The technical solution of the present invention is as follows: A large-capacity steam turbine generator stator bar anti-corona manufacturing process comprises the following steps: Step 1: Transpose the stator wire rods and weave them into a shape to obtain a shaped stator wire rod; Step 2: Use a semi-conductive adhesive strip to stick the semiconductor plates to both sides of the slot of the formed stator wire bar, and then heat to 150-170°C for gelation. The gelation time is 10-40 minutes, and the equipotential layer is completed to obtain a gelled stator wire bar; Step 3: Wrap the main insulation mica tape on the outside of the gelled stator bar by overlapping 1 / 2; Step 4: Wrap the low-resistance anti-corona tape on the core slot of the gelled stator wire bar wrapped with the main insulation mica tape, overlapping 1 / 3; Step 5: Wrap the high resistance anti-corona tape between the two side edges of the low resistance anti-corona tape and the end copper blocks at both ends of the gelled stator wire rods with an overlap of 2 / 3; Step 6: Wrap the low-resistance isolation anti-corona tape on the outside of the low-resistance anti-corona tape by overlapping 1 / 3 to obtain the anti-corona stator wire rod. The wrapping direction of the resistance isolation anti-corona tape is opposite to that of the low-resistance anti-corona tape. Step 7: Wrap the polytetrafluoroethylene release tape on the outer side of the anti-corona stator wire rod by 1 / 3 overlap; Step 8: Put the anti-corona stator wire rod wrapped with polytetrafluoroethylene demoulding tape into the mold, and dry it at 100-120° C. for 4-8 hours to obtain a pretreated stator wire rod; Step nine: vacuum dip varnish treatment is performed on the pretreated stator wire rod, and then heat-cured at 100-120° C. for at least 24 hours to obtain a dip varnished stator wire rod; Step 10: Remove the mold of the paint-impregnated stator wire rod, clean the polytetrafluoroethylene demoulding tape and resin chips of the paint-impregnated stator wire rod, obtain the finished stator wire rod, and transfer the finished stator wire rod to the quality inspection for electrical performance test.
[0007] Furthermore, in step 2, the semi-conductive adhesive strip is a semi-cured material with conductivity, and the volume resistivity is less than 5000Ω·m, and the semiconductor plate is a hard plate with conductivity, and the volume resistivity is 2000-20000Ω·cm. In the present invention, the semiconductor plate is first attached to the outer side of the semi-conductive adhesive strip to form an adhesive semiconductor plate, and then the inner side of the semi-conductive adhesive strip to which the semiconductor plate can be attached is attached to both sides of the slot of the formed stator wire bar, and the adhesive semiconductor plate is bonded to both sides of the slot of the formed stator wire bar, which can not only fill the side transposition groove of the formed stator wire bar, but also balance the electric field distribution of the stator wire bar.
[0008] Furthermore, in step 3, the main insulating mica tape is a mica tape with less glue. Before wrapping the main insulating mica tape, first clean the sharp corners of the gelled stator wire rod, and wipe the dust, debris and other debris on the surface of the gelled stator wire rod with a rag dipped in alcohol.
[0009] Furthermore, in step 4, the low-resistance anti-corona tape is a fully cured polyester-glass woven tape with a surface coated with conductive graphite, and the surface resistance of the fully cured polyester-glass woven tape with a small amount of conductive graphite coated on the surface is 1000-3000Ω.
[0010] Further, in step 5, the high resistance anti-corona tape is a fully cured polyester fiber tape coated with silicon carbide on the surface, and the surface resistance of the fully cured polyester fiber tape coated with silicon carbide under a DC voltage of 5000V is 10 9 -10 13 Ω, the overlapping length of the high resistance anti-corona belt and the low resistance anti-corona belt is 20mm to ensure a smooth transition between the high resistance anti-corona belt and the low resistance anti-corona belt. Silicon carbide coating on the surface of the fully cured polyester fiber belt can improve the electric field distribution at the stator slot by utilizing the nonlinear resistance characteristics of silicon carbide.
[0011] Furthermore, in step 6, the low resistance isolation anti-corona tape is a fully cured polyester glass woven tape with a large amount of conductive graphite coated on the surface, and the surface resistance of the fully cured polyester glass woven tape with a large amount of conductive graphite coated on the surface is 200-2000Ω. Coating a large amount of conductive graphite on the surface of the fully cured polyester glass woven tape can reduce friction, improve the conductivity of the fully cured polyester glass woven tape, and reduce resistance.
[0012] Furthermore, the distance between the side edge of the low-resistance isolation anti-corona belt and the side edge of the proximal high-resistance anti-corona belt is 1-3 mm. During the wrapping process, the low-resistance isolation anti-corona belt should avoid being pressed on top of the high-resistance anti-corona belt to ensure a smooth transition of the resistance values of the low-resistance anti-corona belt and the high-resistance anti-corona belt. The setting of the low-resistance isolation anti-corona belt makes it possible for the stator wire bar to expand and contract during operation after being embedded in the core slot and the axial movement of the stator wire bar.
[0013] Furthermore, in step 7, the tetrafluoroethylene demoulding tape has a porous structure with uniform pore distribution, and the pore diameter of the tetrafluoroethylene demoulding tape is 0.7-0.8 mm; the number of pores per unit area of the tetrafluoroethylene demoulding tape is about 300 / dm 2 The use of a porous tetrafluoroethylene demoulding tape with uniform pore distribution is conducive to the separation of the varnished stator wire rod from the mold, and prevents the anti-corona layer of the varnished stator wire rod from being damaged during the removal of the mold.
[0014] Furthermore, in step nine, the vacuum dipping treatment includes vacuum drying treatment and pressure dipping treatment. During vacuum drying: the vacuum degree reaches below 0.2 mbar and the vacuum is maintained for at least 10 hours; during pressure dipping: the pressure is 2.7-3.0 bar and the pressure is maintained for 10-20 hours. The surface resistance of the core slot of the painted stator bar is 1000-8000Ω.
[0015] The beneficial effects of the present invention are: The present invention provides a large-capacity steam turbine generator stator wire bar anti-corona manufacturing process. First, equipotential layers are made on both sides of the groove portion of the formed stator wire bar, and the equipotential layers are used to fill the transposition grooves on the sides of the stator wire bar, thereby ensuring the fastening effect of the stator wire bar and the balanced electric field effect is stable and good; low-resistance anti-corona tape, high-resistance anti-corona tape and low-resistance isolation anti-corona tape are superimposed, and the wrapping positions and overlapping multiples of the main insulating mica tape, low-resistance anti-corona tape, high-resistance anti-corona tape and low-resistance isolation anti-corona tape are adjusted. Under the premise of ensuring the resistance value of the anti-corona tape, the axial slippage of the stator wire bar is improved, the anti-corona paint is formed in one step, the operation is simple, the process is environmentally friendly, and the anti-corona effect is good. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0017] Figure 1 It is a schematic diagram of the stator bar structure of Example 1.
[0018] In the figure, ①-formed stator bar, ②-equipotential layer, ③-main insulation mica tape, ④-low resistance anti-corona tape, ⑤-high resistance anti-corona tape, ⑥-low resistance isolation anti-corona tape. DETAILED DESCRIPTION
[0019] In order to enable those skilled in the art to better understand the technical solutions in the present invention, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0020] Example 1 A 220MW generator stator bar anti-corona manufacturing process comprises the following steps: Step 1: On the automatic blanking machine platform, the stator wire rod strands are cut, pressed, transposed and bent, and transposed and braided to obtain a formed stator wire rod.
[0021] Step 2: Attach the semiconductor board to the outside of the semi-conductive rubber strip to make an adhesive semiconductor board, and attach the inner sides of the two semi-conductive rubber strips of the adhesive semiconductor board to the two sides of the slot of the molded stator wire rod respectively, and then heat it to 155°C in a curing mold for gelation. The gelation time is 35 minutes, and the equipotential layer is completed to obtain a gelled stator wire rod.
[0022] Step 3: Clean the sharp corners of the gelled stator wire rods, and wipe the dust, debris and other debris on the surface of the gelled stator wire rods with a rag dipped in alcohol. Use an automatic tape wrapping machine to wrap the main insulation mica tape on the outside of the gelled stator wire rods with an overlap of 1 / 2.
[0023] Step 4: Wrap a low-resistance anti-corona tape on the core slot of the gelled stator wire rod wrapped with the main insulating mica tape, overlapping 1 / 3. The low-resistance anti-corona tape is a fully cured polyester-glass braided tape coated with conductive graphite on the surface. The surface resistance of the low-resistance anti-corona tape is 1000-3000Ω.
[0024] Step 5: Wrap the high resistance anti-corona tape between the two sides of the low resistance anti-corona tape and the end copper blocks at both ends of the gelled stator wire rod by overlapping 2 / 3. The high resistance anti-corona tape is a fully cured polyester fiber tape coated with silicon carbide. The surface resistance of the high resistance anti-corona tape at a DC voltage of 5000V is 10 9 -10 13 Ω, the overlapping length of the high resistance anti-corona tape and the low resistance anti-corona tape is 20mm.
[0025] Step 6: Wrap the low resistance isolation anti-corona tape on the outside of the low resistance anti-corona tape in the opposite direction of the wrapping direction of the low resistance anti-corona tape by overlapping 1 / 3 to obtain the anti-corona stator wire rod. During the wrapping process, the low resistance isolation anti-corona tape should avoid being pressed on the top of the high resistance anti-corona tape. The distance between the side edges of the low resistance isolation anti-corona tape and the side edges of the near high resistance anti-corona tape is 2mm. The low resistance isolation anti-corona tape is a fully cured polyester glass braided tape with a large amount of conductive graphite coated on the surface. The surface resistance of the low resistance isolation anti-corona tape is 200-2000Ω.
[0026] Step 7: Wrap the outer side of the anti-corona stator wire rod with a porous polytetrafluoroethylene release tape with a pore diameter of 0.7-0.8mm by overlapping 1 / 3. The number of pores per unit area of the porous polytetrafluoroethylene release tape is about 300 / dm 2 .
[0027] Step 8: Place the anti-corona stator wire rod wrapped with polytetrafluoroethylene release tape into a mold, and dry it in a drying kiln at 110° C. for 8 hours to obtain a pretreated stator wire rod.
[0028] Step 9: Vacuum dip varnish treatment is performed on the pre-treated stator wire rod in the VPI dipping tank. The vacuum dip varnish treatment includes vacuum drying treatment and pressure dip varnish treatment. During vacuum drying, the vacuum degree reaches below 0.2 mbar and the vacuum is maintained for 12 hours. During pressure dip varnish treatment, the pressure is 2.8 bar and the pressure is maintained for 20 hours. After vacuum dip varnishing, the stator wire rod is transferred to the drying kiln and heated and cured at 110°C for 30 hours to obtain the dip varnished stator wire rod. After vacuum dip varnishing treatment, the surface resistance of the core slot of the dip varnished stator wire rod at multiple points is 1000-8000Ω.
[0029] Step 10: Remove the mold of the varnished stator wire rod, clean the polytetrafluoroethylene demoulding tape and resin chips of the varnished stator wire rod, obtain the finished stator wire rod, and transfer the finished stator wire rod to the quality inspection for the equipotential layer resistance value and the electrical performance test of the whole wire rod. The test results are as follows: (1) The resistance value of the equipotential layer of the finished stator wire rod meets the standard requirement of less than 100kΩ, mainly concentrated in 15-80kΩ; (2) The surface anti-corona resistance of the finished stator wire rod in the low-resistance anti-corona area meets the requirement of 1000-8000Ω, mainly concentrated in 1500-7000Ω; ( 3) AC power frequency withstand voltage corona test, 1.5 times the corona condition was observed, far exceeding the requirement of 1.5Un (Un=18kV) without corona, and generally reached above 40kV; (4) AC power frequency withstand voltage test: without protective resistor, test voltage 48.6kV, 1 minute, passed; (5) AC power frequency withstand voltage test: with protective resistor, test voltage 64.8kV, 1 minute, passed; (6) Dielectric loss test: tgδ0.2Un=9.08‰ (required ≤30‰); (Δtgδ / ΔU)max=0.533[‰ / kV] (required ≤1[‰ / kV]). All the above electrical test data meet the technical standard requirements of imported Alstom products.
[0030] Example 2 A 220MW generator stator bar anti-corona manufacturing process comprises the following steps: Step 1: On the automatic blanking machine platform, the stator wire rod strands are cut, pressed, transposed and bent, and transposed and braided to obtain a formed stator wire rod.
[0031] Step 2: Attach the semiconductor board to the outside of the semi-conductive adhesive strip to make an adhesive semiconductor board, and attach the inner sides of the two conductive adhesive strips of the adhesive semiconductor board to the two sides of the slot of the formed stator wire rod respectively, and then heat it to 165°C in a curing mold for gelation. The gelation time is 20 minutes, and the equipotential layer is completed to obtain a gelled stator wire rod.
[0032] Step 3: Clean the sharp corners of the gelled stator wire rods, and wipe the dust, debris and other debris on the surface of the gelled stator wire rods with a rag dipped in alcohol. Use an automatic tape wrapping machine to wrap the main insulation mica tape on the outside of the gelled stator wire rods with an overlap of 1 / 2.
[0033] Step 4: Wrap a low-resistance anti-corona tape on the core slot of the gelled stator wire rod wrapped with the main insulating mica tape, overlapping 1 / 3. The low-resistance anti-corona tape is a fully cured polyester-glass braided tape coated with conductive graphite on the surface. The surface resistance of the low-resistance anti-corona tape is 1000-3000Ω.
[0034] Step 5: Wrap the high resistance anti-corona tape between the two sides of the low resistance anti-corona tape and the end copper blocks at both ends of the gelled stator wire rod by overlapping 2 / 3. The high resistance anti-corona tape is a fully cured polyester fiber tape coated with silicon carbide. The surface resistance of the high resistance anti-corona tape at a DC voltage of 5000V is 10 9 -10 13 Ω, the overlapping length of the high resistance anti-corona tape and the low resistance anti-corona tape is 20mm.
[0035] Step 6: Wrap the low resistance isolation anti-corona tape on the outside of the low resistance anti-corona tape in the opposite direction of the wrapping direction of the low resistance anti-corona tape by overlapping 1 / 3 to obtain the anti-corona stator wire rod. During the wrapping process, the low resistance isolation anti-corona tape should avoid being pressed on the top of the high resistance anti-corona tape. The distance between the side edges of the low resistance isolation anti-corona tape and the side edges of the near high resistance anti-corona tape is 2mm. The low resistance isolation anti-corona tape is a fully cured polyester glass braided tape with a large amount of conductive graphite coated on the surface. The surface resistance of the low resistance isolation anti-corona tape is 200-2000Ω.
[0036] Step 7: Wrap the outer side of the anti-corona stator wire rod with a porous polytetrafluoroethylene release tape with a pore diameter of 0.7-0.8mm by overlapping 1 / 3. The number of pores per unit area of the porous polytetrafluoroethylene release tape is about 300 / dm 2 .
[0037] Step 8: Place the anti-corona stator wire rod wrapped with polytetrafluoroethylene demoulding tape into a mold, and dry it in a drying kiln at 120° C. for 6 hours to obtain a pretreated stator wire rod.
[0038] Step 9: Vacuum dip varnish treatment is performed on the pre-treated stator wire rod in the VPI dipping tank. The vacuum dip varnish treatment includes vacuum drying treatment and pressure dip varnish treatment. During vacuum drying, the vacuum degree reaches below 0.2 mbar and the vacuum is maintained for 12 hours. During pressure dip varnish treatment, the pressure is 3.0 bar and the pressure is maintained for 18 hours. After vacuum dip varnishing, the stator wire rod is transferred to the drying kiln and heated and cured at 120°C for 26 hours to obtain the dip varnished stator wire rod. After vacuum dip varnishing treatment, the surface resistance of the core slot of the dip varnished stator wire rod is 1000-8000Ω at multiple points.
[0039] Step 10: Remove the mold of the varnished stator wire rod, clean the polytetrafluoroethylene demoulding tape and resin chips of the varnished stator wire rod, obtain the finished stator wire rod, and transfer the finished stator wire rod to the quality inspection for the equipotential layer resistance value and the electrical performance test of the whole wire rod. The test results are as follows: (1) The resistance value of the equipotential layer of the finished stator wire rod meets the standard requirement of less than 100kΩ, mainly concentrated in 20-80kΩ; (2) The surface anti-corona resistance of the finished stator wire rod in the low-resistance anti-corona area meets the requirement of 1000-8000Ω, mainly concentrated in 2000-6500Ω; ( 3) AC power frequency withstand voltage corona test, 1.5 times the corona condition was observed, far exceeding the requirement of 1.5Un (Un=18kV) without corona, and generally reached above 40kV; (4) AC power frequency withstand voltage test: without protective resistor, test voltage 48.6kV, 1 minute, passed; (5) AC power frequency withstand voltage test: with protective resistor, test voltage 64.8kV, 1 minute, passed; (6) Dielectric loss test: tgδ0.2Un=5.38‰ (required ≤30‰); (Δtgδ / ΔU)max=0.064[‰ / kV] (required ≤1[‰ / kV]). All the above electrical test data meet the technical standards for imported Alstom products.
[0040] Although the present invention has been described in detail with reference to the accompanying drawings and in combination with the preferred embodiments, the present invention is not limited thereto. Without departing from the spirit and essence of the present invention, a person of ordinary skill in the art may make various equivalent modifications or substitutions to the embodiments of the present invention, and these modifications or substitutions shall be within the scope of the present invention. Any person of ordinary skill in the art may easily think of changes or substitutions within the technical scope disclosed by the present invention, and these shall be within the scope of protection of the present invention.
Claims
1. A large-capacity steam turbine generator stator bar anti-corona manufacturing process, characterized in that: The steps include: Step 1: Transpose the stator wire rods and weave them into shape to obtain a formed stator wire rod; Step 2: Use a semi-conductive adhesive strip to stick the semiconductor plates to both sides of the slot of the formed stator wire bar, and then heat to 150-170°C for gelation. The gelation time is 10-40 minutes, and the equipotential layer is completed to obtain a gelled stator wire bar; Step 3: Wrap the main insulation mica tape on the outside of the gelled stator bar with an overlap of 1 / 2; Step 4: Wrap the low-resistance anti-corona tape on the core slot of the gelled stator wire bar wrapped with the main insulation mica tape, overlapping 1 / 3; Step 5: Wrap the high resistance anti-corona tape between the two side edges of the low resistance anti-corona tape and the end copper blocks at both ends of the gelled stator wire rods with an overlap of 2 / 3; Step 6: Wrap the low-resistance isolation anti-corona tape on the outside of the low-resistance anti-corona tape by overlapping 1 / 3 to obtain the anti-corona stator wire rod. The wrapping direction of the resistance isolation anti-corona tape is opposite to that of the low-resistance anti-corona tape. Step 7: Wrap the polytetrafluoroethylene release tape on the outer side of the anti-corona stator wire rod by 1 / 3 overlap; Step 8: Put the anti-corona stator wire rod wrapped with polytetrafluoroethylene demoulding tape into the mold, and dry it at 100-120° C. for 4-8 hours to obtain a pretreated stator wire rod; Step nine: vacuum dip varnish treatment is performed on the pretreated stator wire rod, and then heat-cured at 100-120° C. for at least 24 hours to obtain a dip varnished stator wire rod; Step 10: Remove the mold of the paint-impregnated stator wire rod, clean the polytetrafluoroethylene demoulding tape and resin chips of the paint-impregnated stator wire rod, obtain the finished stator wire rod, and transfer the finished stator wire rod to the quality inspection for electrical performance test.
2. A large-capacity steam turbine generator stator bar anti-corona manufacturing process as claimed in claim 1, characterized in that: In step 2, the volume resistivity of the semi-conductive rubber strip is less than 5000Ω·m, and the volume resistivity of the semiconductor plate is 2000-20000Ω·cm.
3. The anti-corona manufacturing process for stator wire rods of a large-capacity steam turbine generator according to claim 1, characterized in that: In step three, the main insulating mica tape is a low-resistance mica tape.
4. The anti-corona manufacturing process for stator wire rods of a large-capacity steam turbine generator according to claim 1, characterized in that: In step 4, the low-resistance anti-corona tape is a fully-cured polyester-glass woven tape with a surface coated with conductive graphite, and the surface resistance of the fully-cured polyester-glass woven tape with a surface coated with conductive graphite is 1000-3000Ω.
5. The anti-corona manufacturing process for stator wire rods of a large-capacity steam turbine generator according to claim 1, characterized in that: In step 5, the high resistance anti-corona tape is a fully cured polyester fiber tape coated with silicon carbide on the surface, and the surface resistance of the fully cured polyester fiber tape coated with silicon carbide under a DC voltage of 5000V is 10 9 -10 13 Ω, the overlapping length of the high resistance anti-corona tape and the low resistance anti-corona tape is 20mm.
6. The anti-corona manufacturing process for stator wire rods of a large-capacity steam turbine generator according to claim 1, characterized in that: In step six, the low resistance isolation anti-corona tape is a fully cured polyester glass woven tape with a surface coated with conductive graphite, and the surface resistance of the fully cured polyester glass woven tape with a surface coated with conductive graphite is 200-2000Ω.
7. A large-capacity steam turbine generator stator bar anti-corona manufacturing process as claimed in claim 6, characterized in that: The distance between the side edge of the low-resistance isolation anti-corona belt and the side edge of the proximal high-resistance anti-corona belt is 1-3 mm.
8. The anti-corona manufacturing process for stator wire rods of a large-capacity steam turbine generator according to claim 1, characterized in that: In step seven, the tetrafluoroethylene demoulding tape has a porous structure with uniform pore distribution, and the pore diameter of the tetrafluoroethylene demoulding tape is 0.7-0.8 mm.
9. The anti-corona manufacturing process for stator wire rods of a large-capacity steam turbine generator according to claim 1, characterized in that: In step nine, the vacuum dipping treatment includes vacuum drying treatment and pressure dipping treatment, and the surface resistance of the core slot portion of the dipping stator bar is 1000-8000Ω.
Citation Information
Patent Citations
Manufacturing process of stator bar of turbo generator
CN101577470A
Stator coil of rotary electric machine
JP2003259589A