Manufacturing method of three-dimensional stacked 3T0C DRAM (dynamic random access memory) based on ALD (atomic layer deposition) technology

By using ALD technology to realize the three-dimensional stacked 3T0C structure in DRAM, the existing 2T0C DRAM inflexible reading and low process utilization efficiency are solved, and flexible reading and high integration are achieved.

CN119012694APending Publication Date: 2024-11-22FUDAN UNIVERSITY +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411103093.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing 2T0C DRAM is inflexible to read, and its integration and process utilization efficiency are inefficient.

Method used

Using the three-dimensional stacking 3T0C DRAM manufacturing method based on ALD technology, two independent read transistors are made through a set of process processes, and two read transistors are controlled simultaneously by one write transistor to realize the three-dimensional stacking of read and write transistors. The read transistor adopts Double gate or back gate structure, the write transistor adopts a vertical channel structure.

Benefits of technology

It realizes flexible reading operations, which facilitates the reading transistors to connect different devices, improves chip area utilization and integration, and broadens the application range of capacitive DRAM.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119012694A_ABST
    Figure CN119012694A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a three-dimensional stacked 3T0C DRAM (dynamic random access memory) based on an ALD (atomic layer deposition) technology, and relates to the field of computer manufacturing. Two transistors are manufactured on the basis of one set of technological process, and two read transistors are controlled by one write transistor, so that more flexible device and storage application is realized. Meanwhile, read transistors with back gate and double-gate structures can be manufactured, and the process is more flexible. Three-dimensional stacking of a read transistor with a planar double-gate or back-gate structure and a write transistor with a vertical channel structure is realized, and the application scene and the process stability of the capacitance-free DRAM are improved. And the top gate device is manufactured on the basis of the back gate, so that the performance of the read transistor can be improved, flexible reading is realized, interconnection with other devices is more convenient, and the application range of the capacitance-free DRAM is widened. The process flow designed by the invention has better process feasibility and provides wider application possibility.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of computer manufacturing, and in particular to a method for manufacturing a three-dimensional stacked 3T0CDRAM based on ALD technology. Background Art

[0002] DRAM is an important type of volatile memory that caches data and performs dynamic storage functions in modern computer systems. In existing advanced integrated circuit processes, DRAM with a single transistor-single capacitor (1T1C) as the main structure has approached its size limit. In order to improve DRAM performance in a small-size process, dual-transistor (2T0C) DRAM based on thin-film transistors made of various new materials has been continuously developed to provide a solution for improving DRAM performance.

[0003] Some amorphous metal oxide semiconductor films have good uniformity and high mobility, using active electrons of elements such as In, Zn or Sn as carriers to achieve conductive functions, and can adjust the type and composition of metal elements to control the band structure, carrier concentration and conductivity. Atomic layer deposition (ALD) technology can grow metal oxide films at lower temperatures and better cover microstructures with high aspect ratios and small sizes through the principle of self-adsorption saturated chemical reactions. The metal element composition and oxygen vacancies can be adjusted by the ratio of the number of ALD sub-cycles, and the device function similar to MOSFET can be achieved with the help of semiconductor properties.

[0004] Therefore, technicians in this field are committed to developing a manufacturing method for a three-dimensional stacked 3T0C DRAM based on ALD technology. Based on the existing 2T0C DRAM structure, the device structure can be optimized using an improved patterning process under the same process, and the production of two transistors can be realized based on a set of process steps to form a capacitor-free DRAM with a 3T0C structure, using one write transistor to control two read transistors, and realizing more flexible devices and storage applications. At the same time, the improved process can also produce back-gate and dual-gate structure read transistors, which is more flexible in process.

[0005] The three-dimensional stacking of read transistors with a planar dual-gate or back-gate structure and write transistors with a vertical channel structure will help further improve the application scenarios of capacitor-free DRAM. The back-gate process is simpler than the dual-gate process, which helps reduce process complexity and improve process stability. Making top-gate devices based on back-gate can improve the performance of read transistors, achieve flexible reading, and more conveniently interconnect with other devices, broadening the application scope of capacitor-free DRAM. The designed process flow has good process feasibility and provides a wider range of application possibilities. Summary of the invention

[0006] In view of the above-mentioned defects of the prior art, the technical problem to be solved by the present invention is that the existing 2T0C DRAM is not flexible in reading, and has low integration and process utilization efficiency.

[0007] To achieve the above objectives, the present invention provides a method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology, in which two transistors are manufactured based on a set of process steps.

[0008] Furthermore, one write transistor controls two read transistors simultaneously.

[0009] Furthermore, the working states of the read transistors are independent of each other.

[0010] Furthermore, each of the read transistors has a lead-out wiring.

[0011] Furthermore, the read transistors are respectively connected to different devices.

[0012] Furthermore, the read transistors are stacked in three dimensions.

[0013] Furthermore, the read transistor has a dual-gate structure.

[0014] Furthermore, the read transistor has a back gate structure.

[0015] Furthermore, the transistors are stacked three-dimensionally.

[0016] Furthermore, the write transistor has a vertical channel structure.

[0017] The existing 2T0C DRAM is not flexible to read and has low process efficiency. The present invention designs a 3T0C DRAM structure that uses a set of process steps to make two read transistors. One write transistor is used to control two read transistors at the same time, and the working states of the two transistors are independent of each other.

[0018] The existing dual-gate read transistor has a large area, the read and write transistors are located in the same plane, and the integration is low. The present invention adopts a three-dimensional stacked read and write transistor geometric layout, places the read and write transistors in the same plane area, and manufactures a dual-gate or back-gate structure of the read transistor to achieve three-dimensional stacking. The dual-gate has better gate control capability, the back-gate process is simple, and the device can be flexibly manufactured as needed during the process manufacturing.

[0019] Compared with the prior art, the present invention has the following obvious substantial features and significant advantages:

[0020] 1. The present invention can flexibly lead out the wiring of two read transistors to achieve flexible reading, and facilitate the two read transistors to be connected to different devices respectively, thereby achieving a wider range of applications.

[0021] 2. The read and write transistors of the present invention are located in the same plane, which is convenient for wiring according to the process layer, thereby improving chip area utilization and integration.

[0022] The concept, specific structure and technical effects of the present invention will be further described below in conjunction with the accompanying drawings to fully understand the purpose, characteristics and effects of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 is a schematic diagram of embodiment 1 of the present invention;

[0024] Figure 2 is a schematic diagram of embodiment 2 of the present invention;

[0025] Figure 3 is a schematic diagram of embodiment 3 of the present invention;

[0026] Figure 4 is a schematic diagram of embodiment 4 of the present invention;

[0027] Figure 5 is a schematic diagram of embodiment 5 of the present invention;

[0028] Figure 6 is a schematic diagram of embodiment 6 of the present invention;

[0029] Figure 7 It is a schematic diagram of Example 7 of the present invention. DETAILED DESCRIPTION

[0030] The following describes several preferred embodiments of the present invention with reference to the drawings in the specification, so that the technical content is clearer and easier to understand. The present invention can be embodied in many different forms of embodiments, and the protection scope of the present invention is not limited to the embodiments mentioned in the text.

[0031] In the drawings, components with the same structure are indicated by the same numerical reference numerals, and components with similar structures or functions are indicated by similar numerical reference numerals. The size and thickness of each component shown in the drawings are arbitrarily shown, and the present invention does not limit the size and thickness of each component. In order to make the illustration clearer, the thickness of the components is appropriately exaggerated in some places in the drawings.

[0032] Embodiment 1, as Figure 1 As shown, on a medium-heavy doped Si substrate 101 with 50-100nm silicon dioxide 102, a 50-300nm thick metal film material 103 is deposited by magnetron sputtering (PVD) technology, a write transistor gate region is defined by photolithography, and the metal and gate dielectric outside the write transistor gate region are etched.

[0033] The oxide film on the medium and heavily doped Si substrate used can select other high-k materials, such as aluminum oxide, hafnium oxide, etc., to expand the range of choices; the photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc., to expand the range of choices; the metal material used here can be Al, Cr, Ti, Ni or W, and the above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, and can also be replaced with transparent conductive oxides such as ITO to expand the range of choices; the PVD technology here can be replaced with electron beam evaporation (EBE) technology to expand the range of choices.

[0034] Embodiment 2, as Figure 2 As shown. A heavily doped silicon substrate 201 and a metal 203. A 10-200 nm thick silicon dioxide gate dielectric film material 202 is deposited by atomic layer deposition (ALD) technology; a write transistor active region is defined by photolithography, and the gate dielectric material in the write transistor active region is etched.

[0035] The silicon dioxide gate dielectric used here can be replaced with high-k dielectrics such as aluminum oxide or hafnium oxide to expand the range of options; the photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and EBL, etc.; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process to expand the range of options.

[0036] Embodiment 3, as Figure 3 As shown. A heavily doped silicon substrate 301, silicon dioxide or high-k dielectric 302. A layer of 10-200nm thick amorphous metal oxide semiconductor thin film material 304 is deposited by ALD technology, and then a layer of 50-300nm thick metal thin film material 303 is deposited by PVD technology. The drain and channel regions of the transistor are defined by photolithography, and the metal and amorphous metal oxide semiconductor materials outside the drain and channel regions are etched.

[0037] The ALD technology is used to fill high aspect ratio grooves in cycles, and the filling of the grooves to a certain depth is the standard. The amorphous metal oxide semiconductor film can be IGZO, ITZO, IHO, ITGO, IGO and other metal oxide semiconductors that can be grown by ALD technology, expanding the range of choices; the metal material used here can be Al, Cr, Ti, Ni or W. The above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, and can also be replaced with transparent conductive oxides such as ITO to expand the range of choices; the PVD technology here can be replaced with EBE technology to expand the range of choices.

[0038] Embodiment 4, as Figure 4As shown, a heavily doped silicon substrate 401 and a metal 403 are provided. A 10-200 nm thick silicon dioxide gate dielectric film material 402 is deposited by ALD technology; and a 10-200 nm thick amorphous metal oxide semiconductor film material 404 is deposited by ALD technology.

[0039] The silicon dioxide gate dielectric used here can be replaced with high-k dielectrics such as aluminum oxide or hafnium oxide to expand the range of options; the amorphous metal oxide semiconductor film used here can be IGZO, ITZO, IHO, ITGO, IGO and other metal oxide semiconductors that can be grown using ALD technology to expand the range of options.

[0040] Embodiment 5, as Figure 5 As shown. Heavily doped silicon substrate 501, silicon dioxide or high-k dielectric 502, metal 503, metal oxide semiconductor 504. Two read transistor active regions are defined by photolithography, and amorphous metal oxide semiconductor material outside the read transistor active region is etched. This step can realize the structure of two transistors being simultaneously fabricated in the second layer.

[0041] The photolithography process used here includes ultraviolet lithography (UV, DUV, EUV) and EBL, etc., which expands the range of options; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process, which expands the range of options.

[0042] Embodiment 6, as Figure 6 As shown. Heavily doped silicon substrate 601, silicon dioxide or high-k dielectric 602, metal oxide semiconductor 604. The source and drain regions of two read transistors are defined by photolithography, a layer of 50-300nm thick metal film material 603 is deposited by PVD technology, and the metal outside the source and drain regions of the read transistor is stripped off. This step makes the source and drain electrodes of the upper multiple transistor structures.

[0043] The photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and EBL, etc., which expand the range of options; the metal materials used here can be Al, Cr, Ti, Ni or W, and the above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, and can also be replaced with transparent conductive oxides such as ITO to expand the range of options; the PVD technology here can be replaced with EBE technology to expand the range of options. This step produces the upper multiple transistor structure gate electrodes.

[0044] Embodiment 7, as Figure 7As shown. A heavily doped silicon substrate 701 and a metal oxide semiconductor 704. A 10-200nm thick silicon dioxide gate dielectric film material 702 is deposited by ALD technology; the top gate regions of two read transistors are defined by photolithography, a 50-300nm thick metal film material 703 is deposited by PVD technology, and the metal outside the gate region of the read transistor is stripped.

[0045] This process step can be omitted when making a back-gate read transistor structure; the silicon dioxide gate dielectric used here can be replaced with a high-k dielectric such as aluminum oxide or hafnium oxide to expand the range of options; the metal material used here can be Al, Cr, Ti, Ni or W, and the above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, or can be replaced with transparent conductive oxides such as ITO to expand the range of options; the PVD technology here can be replaced with EBE technology to expand the range of options; the photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and EBL, etc., to expand the range of options.

[0046] The preferred specific embodiments of the present invention are described in detail above. It should be understood that ordinary technicians in the field can make many modifications and changes based on the concept of the present invention without creative work. Therefore, all technical solutions that can be obtained by technicians in the technical field based on the concept of the present invention through logical analysis, reasoning or limited experiments on the basis of the prior art should be within the scope of protection determined by the claims.

Claims

1. A method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology, characterized in that: Two transistors are made based on one process.

2. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 1, characterized in that: One write transistor controls two read transistors simultaneously.

3. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 2, characterized in that: The working states of the read transistors are independent of each other.

4. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 2, characterized in that: The read transistors are each led out to wiring.

5. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology as claimed in claim 2, characterized in that: The read transistors are each connected to a different device.

6. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 2, characterized in that: The read transistors are three-dimensionally stacked.

7. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 6, characterized in that: The read transistor has a double-gate structure.

8. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 6, characterized in that: The read transistor has a back gate structure.

9. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 1, characterized in that: Writing transistors in three dimensions.

10. The method for manufacturing a three-dimensional stacked 3T0C DRAM based on ALD technology according to claim 9, characterized in that: The write transistor has a vertical channel structure.