In-mold double-hardness product forming method

Through the mold double hardness product molding method, combined with quantum mechanics and topological optimization technology, the problems of low efficiency and inconsistent material performance in traditional multiple injection molding processes are solved, and the synchronous curing and stress optimization of double hardness materials are achieved, which improves the product Combined with strength and structural stability, it is suitable for the manufacturing of high-performance products.

CN119017666AInactive Publication Date: 2024-11-26东莞市科卡特橡塑制品有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411141759.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional multi-injection molding processes have problems such as low efficiency, complex operation, inconsistent material performance and stress concentration in double hardness product molding, making it difficult to meet the needs of high-precision and high-performance products.

Method used

The in-mold double hardness product molding method is adopted, combined with quantum mechanics, topological optimization and nonlinear dynamics technology, and synchronous curing of double hardness materials is achieved through synchronous thermodynamic control, runner control and higher-order nonlinear Li group analysis method. Stress field optimization and microstructure stability.

Benefits of technology

It improves material bond strength and product performance, optimizes stress distribution, enhances structural stability, simplifies production processes, reduces manufacturing costs, and is suitable for the manufacturing of high-precision and high-performance products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119017666A_ABST
    Figure CN119017666A_ABST
Patent Text Reader

Abstract

The in-mold double-hardness product forming method comprises the following steps that S1, a set of mold is provided, and the mold comprises a first mold cavity and a second mold cavity which are used for forming a first material and a second material which are different in hardness correspondingly; s2, a first hardness material is injected into the first mold cavity, and the temperature of the first hardness material is adjusted, so that the first hardness material is partially cured; s3, the partially cured first hardness material is transferred to a designated position of a second mold cavity through a runner control system; s4, a second hardness material is injected into the second mold cavity, so that the second hardness material is in contact with the uncured interface layer of the first hardness material, and the two materials are promoted to be combined; s5, through synchronous temperature adjustment, the first hardness material and the second hardness material are cured in the mold at the same time, and a composite structure with different hardness areas is formed; and S6, the mold is cooled, and a formed double-hardness product is taken out. The method is suitable for manufacturing high-performance products needing multiple hardness areas, and the mechanical performance and durability of the products are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the fields of material science and engineering, mold design and manufacturing, and in particular to a method for forming a dual-hardness product in a mold. Background Art

[0002] In modern manufacturing, the molding technology of dual-hardness products has been widely used. These products have attracted much attention because they exhibit different mechanical properties in different areas, such as in the fields of automotive parts, aerospace components, and electronic consumer product housings. However, the traditional molding method of dual-hardness products mainly relies on multiple injection molding processes, that is, using materials of different hardness to be injection molded separately in different stages. Although this multiple injection molding technology can achieve the combination of multiple materials, it has significant defects and limitations in practical applications, and it is difficult to meet the growing demand for high-precision and high-performance products.

[0003] The traditional multi-injection molding process is inefficient and complicated to operate. Each injection involves separate heating, molding and cooling of the material, which not only prolongs the production cycle but also increases manufacturing costs. As the material undergoes a complex thermal history during multiple heat treatments, the material properties may degrade, especially at the interface where the materials are combined, which is prone to insufficient bonding strength, resulting in delamination or peeling, ultimately affecting the overall quality and structural integrity of the product.

[0004] The existing technology has limited control accuracy at the material bonding interface. Different hardness materials have significant differences in physical and chemical properties. It is difficult for traditional processes to accurately control the stress and structure at the interface during the material bonding process. This can easily lead to stress concentration, especially during the use of the product. Local stress concentration may cause structural damage at the interface, reducing the service life and reliability of the product. For products that require high safety and durability, such as automotive engine parts and aviation equipment, this defect may pose a serious safety hazard.

[0005] The existing multiple injection molding process has deficiencies in the micro-control of material bonding. As the manufacturing industry's demand for product microstructure control continues to increase, how to ensure the microstructural stability and consistency of the interface layer during the material bonding process has become a major problem. Traditional processes make it difficult to simultaneously control the quantum state and macroscopic physical properties of materials during the bonding process, resulting in a mismatch between the microstructure and macroscopic performance, and unable to meet the manufacturing requirements of high-performance products. These problems are particularly prominent in electronic equipment housings or precision instrument components in scenarios with high precision requirements.

[0006] Therefore, how to provide a dual-hardness product molding method in a mold is an urgent problem that technicians in this field need to solve. Summary of the invention

[0007] One purpose of the present invention is to propose a method for forming a dual-hardness product in a mold. The present invention describes in detail the process of realizing the simultaneous solidification of dual-hardness materials, stress field optimization, spin state regulation and microstructure stability in a mold by combining quantum mechanics, topological optimization and nonlinear dynamics technology. The method has the advantages of high bonding strength, stable material performance, high production efficiency and long product service life.

[0008] The in-mold dual-hardness product forming method according to an embodiment of the present invention comprises the following steps:

[0009] S1. Provide a set of molds, the molds comprising a first mold cavity and a second mold cavity, the first mold cavity and the second mold cavity are respectively used to mold a first material and a second material of different hardness, and a synchronous thermodynamic control system and a flow channel control system are provided inside the mold;

[0010] S2, injecting a first hardness material into a first mold cavity, controlling the flow rate during the injection process by a generalized fluid dynamics equation of a non-Abelian gauge field, and controlling the temperature distribution in the mold cavity by a multi-body system equation combining a quantum coherent state with non-equilibrium statistical mechanics, while partially solidifying the first hardness material in a predetermined area, and retaining an incompletely solidified interface layer on the surface;

[0011] S3, transferring the partially solidified first hardness material in the first mold cavity to a designated position of the second mold cavity through a flow channel control system, aligning the first hardness material through a high-order nonlinear Lie group analysis method, and controlling the thickness of the interface layer through the supersymmetric string theory of duality between anti-de Sitter space and conformal field theory;

[0012] S4. Injecting a second hardness material into the second mold cavity, combining the first hardness material with the second hardness material, using a high-order spin-orbit coupling model to regulate the bonding strength of the interface layer, controlling the generated field intensity through supersymmetric gauge field theory, optimizing the electromagnetic field distribution of the bonding interface, and enhancing the physical strength and stability of the material bonding;

[0013] S5. The temperature field in the mold is adjusted by a synchronous thermodynamic control system so that the first hardness material and the second hardness material are solidified synchronously within a predetermined time. The stress field distribution in the mold cavity is controlled by a high-dimensional topology optimization method to prevent the material from deforming due to stress concentration. The first hardness material and the second hardness material are solidified in the mold at the same time. The microstructure formed by the material during the synchronous solidification process is regulated by a nonlinear dynamic model under the background of a time crystal to optimize product stability.

[0014] S6. Cool the mold and take out the formed dual-hardness product. The dual-hardness product has a smooth transition between different hardness areas, which optimizes the structural stability.

[0015] Optionally, the S2 specifically includes:

[0016] S21, injecting the first hardness material into the first mold cavity, and controlling the flow rate Q1(t) during the injection process by the generalized fluid dynamics equation of the non-Abelian gauge field:

[0017]

[0018] Among them, F μν is the intensity tensor of the non-Abelian gauge field, ★ represents the Hodge duality, is a canonical manifold, is the path integral measure, Tr represents the trace operation;

[0019] S22. Use the multi-body system equation combining quantum coherent state and non-equilibrium statistical mechanics to control the temperature distribution in the mold cavity, temperature field T(x,y,z,t):

[0020]

[0021] Among them, |Ψ(t)> is the quantum coherent state, is the operator representation of the temperature field, the evolution of which is subject to the time development of the many-body wave function Ψ(t);

[0022] S23. By controlling the temperature field T(x, y, z, t), the first hardness material is partially solidified in a predetermined area. The material hardness H1(t) during the partial solidification process is described by the high-dimensional topological soliton field equation:

[0023]

[0024] Among them, d int (t) is the Levi-Civita symbol, φ is the scalar field of the material, the integral is performed over the space Σ of the topological solitons, and ijk is the Levi-Civita symbol used to represent a completely antisymmetric tensor in three-dimensional space;

[0025] S24. Controlling the thickness of the interface layer d using supersymmetric Calabi-Yau geometry flow int (t), so that the surface of the first hardness material retains an incompletely solidified interface layer, the thickness of the interface layer is d int The variation of (t) is described by the following supersymmetric Calabi-Yau geometry flow equation:

[0026]

[0027] in, is a Calabi-Yau manifold, Ω is the global complex volume form on the Calabi-Yau manifold, is its complex conjugate, and K is the Kähler potential.

[0028] Optionally, the S3 specifically includes:

[0029] S31. Multi-body entangled interaction energy in non-equilibrium quantum thermodynamics V ent (t) Controlling the transfer of partially solidified first hardness material from the first cavity to a designated position of the second cavity. During the transfer process, dynamically calculating the entanglement interaction energy V according to the material's wave function Ψ(t) and temperature T ent (t), optimize the stability of the material to maintain its quantum entangled state during the transfer process:

[0030]

[0031] in, represents the quantum entanglement Hamiltonian of the material, Ψ(t) is the quantum state wave function of the material, and T(t) is the temperature;

[0032] S32. During the material transfer process, the system uses the quantum entangled state and interaction energy calculated in S31 as initial input, and adopts the nonlinear evolution equation combining the interaction between the quantum liquid crystal state and the time crystal to further optimize the quantum state and phase evolution of the material:

[0033]

[0034] in, and They describe the Hamiltonian of the quantum liquid crystal state and the time crystal respectively, |Ψ(t)> the quantum liquid crystal state of the material, ∈ is the coupling strength of the system, is the quantum dissipative operator;

[0035] S33, in the second mold cavity, using the quantum liquid crystal state obtained in S32 as the initial state, aligning the first hardness material by high-order nonlinear Lie group analysis method, and the geometric state during the alignment process

[0036]

[0037] Among them, ξ i is the Lie group parameter derived from the quantum state evolution in the previous step, is the Lie group generator, is the initial geometric state;

[0038] S34. After the alignment is completed, the system uses the supersymmetric string theory of anti-de Sitter space and conformal field theory, and uses the geometric state and quantum state obtained in S33 as input to control the thickness of the interface layer and optimize the height and stability of the material combination. The thickness of the interface layer d AdS / CFT (t):

[0039]

[0040] in, is an anti-de Sitter space, The geometric state parameters of the previous step OK, S. CFT [φ] The action of conformal field theory, which represents the dynamic behavior of the system under the field variable φ, d AdS / CFT The interface layer thickness represents the thickness of the material at the interface layer, which changes with time t, and φ defines the field variable.

[0041] Optionally, the S4 specifically includes:

[0042] S41, injecting a second hardness material into the second mold cavity, and controlling the coupling state of quantum mechanics to make the second hardness material contact and combine with the uncured interface layer of the first hardness material, and the interaction potential energy V during the combination process couple (t):

[0043]

[0044] in, is the joint Lagrangian function describing the wave function Ψ1(t) of the first hardness material and the wave function Ψ2(t) of the second hardness material, Σ is the spatial area of ​​the bonding interface, To reduce Planck's constant, Ψ1 and Ψ2 are the quantum state wave functions of the first hardness material and the second hardness material;

[0045] S42. During the material bonding process, the system dynamically adjusts the temperature distribution T(x,y,z,t) in the mold cavity through the topological thermodynamic model:

[0046]

[0047] Among them, κ is the thermal conductivity of the material, α is the thermal coupling coefficient related to the internal topological structure of the material, The system adjusts the temperature field during the bonding process in real time;

[0048] S43, during the binding process, the system uses a high-order spin-orbit coupling model to regulate the binding strength of the interface layer. The binding strength σ int (t):

[0049]

[0050] Where γ is the coupling constant, Ψ int (t) is the quantum state wave function at the binding interface, and are the spin and orbital angular momentum operators, respectively, and λ is the attenuation coefficient related to the temperature T(t);

[0051] S44. In the final binding stage, the system controls the field strength generated during the binding process through supersymmetric gauge field theory. The evolution of field strength optimizes the physical strength and stability of material bonding by controlling the evolution of the gauge field and combining the electromagnetic field distribution at the interface:

[0052]

[0053] in, is the covariant derivative, is the gauge field tensor, is the source current, is the action functional of the gauge field.

[0054] Optionally, the S5 specifically includes:

[0055] S51, adjusting the temperature field in the mold through a synchronous thermodynamic control system, so that the first hardness material and the second hardness material are synchronously cured within a predetermined time, and the first hardness material and the second hardness material are optimized to maintain temperature consistency during the curing process;

[0056] S52. During the simultaneous solidification process, the stress field distribution in the mold cavity is controlled by using a high-dimensional topology optimization method to optimize the material so that it will not deform due to stress concentration during the solidification process;

[0057] S53. By using self-consistent field theory, the spin state inside the material is adjusted to optimize the uniform distribution of the spin state inside the material during the curing process;

[0058] S54. Use the nonlinear dynamic model in the context of time crystals to regulate the microstructure of the material formed during the synchronous solidification process and optimize the product to have consistency and high stability.

[0059] Beneficial Effects

[0060] 1. Improve bonding strength and product performance: The present invention realizes the synchronous solidification of two materials of different hardness in the mold through a synchronous thermodynamic control system. Through this process, not only the problem of inconsistent material properties caused by multiple heat treatments in traditional multiple injection molding processes is avoided, but also the bonding strength of the materials at the interface is ensured. Through the regulation of quantum mechanics, the materials can be synchronously adjusted at the quantum state level, thereby improving the mechanical properties and service life of the overall product.

[0061] 2. Optimize stress distribution and enhance structural stability: The present invention adopts a high-dimensional topology optimization method to accurately control the stress field distribution in the mold cavity during the material solidification process, effectively avoiding the problem of structural damage caused by stress concentration. Through precise stress field regulation, the product can withstand higher mechanical stress during use, significantly improving the stability of the structure, and is particularly suitable for products with high load and high safety requirements, automotive parts and aerospace components.

[0062] 3. Accurately control the spin state and microstructure inside the material: Through the high-order nonlinear spin wave model and time crystal nonlinear dynamics model in the self-consistent field theory, the present invention can achieve uniform distribution of spin states and stable control of microstructure during the material solidification process. This technical means effectively prevents the performance degradation problem caused by internal inhomogeneity of the material, thereby further improving the durability and reliability of the product.

[0063] 4. Improve production efficiency and reduce manufacturing costs: Compared with the traditional multiple injection molding process, the present invention greatly improves production efficiency. Through the synchronous curing process and precise control system, the production steps are reduced, the production cycle is shortened, and the energy and time costs are reduced. At the same time, the present invention simplifies the process flow and reduces the dependence on complex mechanical equipment, thereby reducing the overall manufacturing cost.

[0064] 5. Adapting to the needs of high-precision and high-performance products: This invention solves many bottleneck problems in the existing technology in the manufacture of high-precision and high-performance products by introducing quantum mechanics, topological optimization and nonlinear dynamics technology. This method can meet the requirements of synchronous regulation of product microstructure and macroscopic physical properties, and is particularly suitable for application scenarios with high requirements for product performance, such as precision instruments, aerospace, automotive industry and electronic equipment housing. BRIEF DESCRIPTION OF THE DRAWINGS

[0065] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0066] Figure 1 The figure is a summary of the in-mold dual-hardness product forming method proposed by the present invention;

[0067] Figure 2 The flowchart of claim 2 of the in-mold dual-hardness product forming method proposed by the present invention;

[0068] Figure 3 This is a flow chart of claim 4 of the in-mold dual-hardness product forming method proposed by the present invention. DETAILED DESCRIPTION

[0069] The present invention will now be described in further detail with reference to the accompanying drawings. These drawings are simplified schematic diagrams, which only illustrate the basic structure of the present invention in a schematic manner, and therefore only show the components related to the present invention.

[0070] refer to Figure 1-3 The in-mold dual-hardness product forming method comprises the following steps:

[0071] S1. Provide a set of molds, the molds comprising a first mold cavity and a second mold cavity, the first mold cavity and the second mold cavity are respectively used to mold a first material and a second material of different hardness, and a programmable temperature control system, a flow channel control system and a topological stress field adjustment system are provided inside the molds;

[0072] S2, injecting a first hardness material into a first mold cavity, controlling the flow rate during the injection process by a generalized fluid dynamics equation of a non-Abelian gauge field, and controlling the temperature distribution in the mold cavity by a multi-body system equation combining a quantum coherent state with non-equilibrium statistical mechanics, while partially solidifying the first hardness material in a predetermined area, and retaining an incompletely solidified interface layer on the surface;

[0073] S3, transferring the partially solidified first hardness material in the first mold cavity to a designated position of the second mold cavity through a flow channel control system, aligning the first hardness material through a high-order nonlinear Lie group analysis method, and controlling the thickness of the interface layer through the supersymmetric string theory of duality between anti-de Sitter space and conformal field theory;

[0074] S4. Injecting a second hardness material into the second mold cavity, combining the first hardness material with the second hardness material, using a high-order spin-orbit coupling model to regulate the bonding strength of the interface layer, controlling the generated field intensity through supersymmetric gauge field theory, optimizing the electromagnetic field distribution of the bonding interface, and enhancing the physical strength and stability of the material bonding;

[0075] S5. The temperature field in the mold is adjusted by a synchronous thermodynamic control system so that the first hardness material and the second hardness material are solidified synchronously within a predetermined time. The stress field distribution in the mold cavity is controlled by a high-dimensional topology optimization method to prevent the material from deforming due to stress concentration. The first hardness material and the second hardness material are solidified in the mold at the same time. The microstructure formed by the material during the synchronous solidification process is regulated by a nonlinear dynamic model under the background of a time crystal to optimize product stability.

[0076] S6. Cool the mold and take out the formed dual-hardness product. The dual-hardness product has a smooth transition between different hardness areas, which optimizes the structural stability.

[0077] In this implementation, S2 specifically includes:

[0078] S21, injecting the first hardness material into the first mold cavity, and controlling the flow rate Q1(t) during the injection process by the generalized fluid dynamics equation of the non-Abelian gauge field:

[0079]

[0080] Among them, F μν is the intensity tensor of the non-Abelian gauge field, * denotes the Hodge duality, is a canonical manifold, is the path integral measure, Tr represents the trace operation;

[0081] S22. Use the multi-body system equation combining quantum coherent state and non-equilibrium statistical mechanics to control the temperature distribution in the mold cavity, temperature field T(x,y,z,t):

[0082]

[0083] where |Ψ(t)> is the quantum coherent state of the system, is the operator representation of the temperature field, the evolution of which is subject to the time development of the many-body wave function Ψ(t);

[0084] S23. By controlling the temperature field T(x, y, z, t), the first hardness material is partially solidified in a predetermined area. The material hardness H1(t) during the partial solidification process is described by the high-dimensional topological soliton field equation:

[0085]

[0086] Among them, d int (t) is the Levi-Civita symbol, φ is the scalar field of the material, the integral is performed over the space Σ of the topological solitons, and ijk is the Levi-Civita symbol used to represent a completely antisymmetric tensor in three-dimensional space;

[0087] S24. Controlling the thickness of the interface layer d using supersymmetric Calabi-Yau geometry flow int (t), so that the surface of the first hardness material retains an incompletely solidified interface layer, the thickness of the interface layer is d int The variation of (t) is described by the following supersymmetric Calabi-Yau geometry flow equation:

[0088]

[0089] in, is a Calabi-Yau manifold, Ω is the global complex volume form on the Calabi-Yau manifold, is its complex conjugate, and K is the Kähler potential.

[0090] In this implementation, S3 specifically includes:

[0091] S31. Multi-body entangled interaction energy in non-equilibrium quantum thermodynamics V ent (t) Controlling the transfer of partially solidified first hardness material from the first cavity to a designated position of the second cavity. During the transfer process, dynamically calculating the entanglement interaction energy V according to the material's wave function Ψ(t) and temperature T ent (t), optimize the stability of the material to maintain its quantum entangled state during the transfer process:

[0092]

[0093] in, represents the quantum entanglement Hamiltonian of the material, Ψ(t) is the quantum state wave function of the material, and T(t) is the temperature;

[0094] S32. During the material transfer process, the system uses the quantum entangled state and interaction energy calculated in S31 as initial input, and adopts the nonlinear evolution equation combining the interaction between the quantum liquid crystal state and the time crystal to further optimize the quantum state and phase evolution of the material:

[0095]

[0096] in, and They describe the Hamiltonian of the quantum liquid crystal state and the time crystal respectively, |Ψ(t)> the quantum liquid crystal state of the material, ∈ is the coupling strength of the system, is the quantum dissipative operator;

[0097] S33, in the second mold cavity, using the quantum liquid crystal state obtained in S32 as the initial state, aligning the first hardness material by high-order nonlinear Lie group analysis method, and the geometric state during the alignment process

[0098]

[0099] Among them, ξ i is the Lie group parameter derived from the quantum state evolution in the previous step, is the Lie group generator, is the initial geometric state;

[0100] S34. After the alignment is completed, the system uses the supersymmetric string theory of anti-de Sitter space and conformal field theory, and uses the geometric state and quantum state obtained in S33 as input to control the thickness of the interface layer and optimize the height and stability of the material combination. The thickness of the interface layer d AdS / CFT (t):

[0101]

[0102] in, is an anti-de Sitter space, The geometric state parameters of the previous step OK, S. CFT [φ] The action of conformal field theory, which represents the dynamic behavior of the system under the field variable φ, d AdS / CFT The interface layer thickness represents the thickness of the material at the interface layer, which changes with time t, and φ defines the field variable.

[0103] In this implementation, S4 specifically includes:

[0104] S41, injecting a second hardness material into the second mold cavity, and controlling the coupling state of quantum mechanics to make the second hardness material contact and combine with the uncured interface layer of the first hardness material, and the interaction potential energy V during the combination process couple (t):

[0105]

[0106] in, is the joint Lagrangian function describing the wave function Ψ1(t) of the first hardness material and the wave function Ψ2(t) of the second hardness material, Σ is the spatial area of ​​the bonding interface, To reduce Planck's constant, Ψ1 and Ψ2 are the quantum state wave functions of the first hardness material and the second hardness material;

[0107] S42. During the material bonding process, the system dynamically adjusts the temperature distribution T(x,y,z,t) in the mold cavity through the topological thermodynamic model:

[0108]

[0109] Among them, κ is the thermal conductivity of the material, α is the thermal coupling coefficient related to the internal topological structure of the material, The system adjusts the temperature field during the bonding process in real time;

[0110] S43, during the binding process, the system uses a high-order spin-orbit coupling model to regulate the binding strength of the interface layer. The binding strength σ int (t):

[0111]

[0112] Where γ is the coupling constant, Ψ int (t) is the quantum state wave function at the binding interface, and are the spin and orbital angular momentum operators, respectively, and λ is the attenuation coefficient related to the temperature T(t);

[0113] S44. In the final binding stage, the system controls the field strength generated during the binding process through supersymmetric gauge field theory. The evolution of field strength optimizes the physical strength and stability of material bonding by controlling the evolution of the gauge field and combining the electromagnetic field distribution at the interface:

[0114]

[0115] in, is the covariant derivative, is the gauge field tensor, is the source current, is the action functional of the gauge field.

[0116] In this implementation manner, S5 specifically includes:

[0117] S51, adjusting the temperature field in the mold through a synchronous thermodynamic control system, so that the first hardness material and the second hardness material are synchronously cured within a predetermined time, and the first hardness material and the second hardness material are optimized to maintain temperature consistency during the curing process;

[0118] S52. During the simultaneous solidification process, the stress field distribution in the mold cavity is controlled by using a high-dimensional topology optimization method to optimize the material so that it will not deform due to stress concentration during the solidification process;

[0119] S53. By using self-consistent field theory, the spin state inside the material is adjusted to optimize the uniform distribution of the spin state inside the material during the curing process;

[0120] S54. Use the nonlinear dynamic model in the context of time crystals to regulate the microstructure of the material formed during the synchronous solidification process and optimize the product to have consistency and high stability.

[0121] Example

[0122] In order to verify the feasibility of the present invention in implementation, the present invention was applied in a large automobile manufacturing plant, where engineers faced a thorny problem: they hoped to develop a new type of engine hood that could provide sufficient rigidity in the center to support the weight and high temperature of the engine, and sufficient toughness in the edge to absorb external impact. However, the traditional multiple injection molding process encountered many problems in production tests. The engine hood produced using traditional methods showed obvious stress concentration at the bonding interface, resulting in cracking in local areas. Repeated heating and cooling during the production process caused the material properties to degrade, especially the insufficient bonding strength at the interface, which was prone to delamination or peeling in actual use. Since the materials were molded separately at different stages, the production cycle was too long and the cost increased.

[0123] To overcome these problems, engineers decided to use the in-mold dual-hardness product molding method of the present invention. This method combines quantum mechanics, topology optimization and nonlinear dynamics technology, and describes in detail the process flow of achieving dual-hardness material synchronous solidification, stress field optimization, spin state regulation and microstructure stability in the mold, aiming to solve the problems of insufficient bonding strength, stress concentration and microstructure instability in traditional processes.

[0124] Engineers selected two polyurethane materials for the center and edge of the hood. The hardness of the center material is 75D, and the hardness of the edge material is 55D. The design of the mold takes into account the injection sequence and curing process of materials of different hardness, and integrates a synchronous thermodynamic control system to achieve precise control of the temperature field in the mold. In addition, multiple high-precision temperature sensors and stress sensors are installed in the mold to monitor the curing state and stress distribution of the material in real time.

[0125] During the production process, 75D polyurethane material is first injected into the center area of ​​the mold, and then 55D polyurethane material is injected into the edge area. The synchronous thermodynamic control system starts to work, adjusting the temperature field in the mold in real time to ensure that the two materials are solidified synchronously within the predetermined time. By accurately controlling the distribution of the temperature field, the present invention effectively avoids the problem of inconsistent material properties caused by multiple heat treatments in traditional multiple injection molding processes, and ensures the consistency of the quantum state of the material at the interface and the matching of the macroscopic properties.

[0126] During the material solidification process, the system uses high-dimensional topology optimization methods to adjust the stress field distribution in the mold in real time. By combining mold design data and material mechanical properties data, engineers ensure that the stress field distribution of the material during the solidification process is uniform and avoids the occurrence of stress concentration. Experimental data shows that through this method, the interface stress of the engine hood is reduced by 25%, which greatly improves the structural stability of the product and reduces the cracking or deformation problems caused by local stress concentration.

[0127] In order to further improve product performance, engineers used the high-order nonlinear spin wave model in the self-consistent field theory to regulate the spin state distribution inside the material, ensuring that the uniformity of the internal spin state is maintained during the material solidification process. In addition, through the time crystal nonlinear dynamics model, engineers achieved stable regulation of the material's microstructure. In this process, the material's microstructure was able to remain stable during the solidification process, avoiding performance degradation problems caused by unstable microstructure. Experimental data showed that the order of the microstructure of the hood increased by 15% after molding, and the uniformity of the spin state increased by 20%.

[0128] Table 1. Production efficiency comparison table

[0129] Process Type Production time (minutes) Traditional multi-injection molding process 60 In-mold dual-hardness forming method of the present invention 40

[0130] Table 2. Bonding strength test table

[0131] Test items Traditional process (MPa) The method of the present invention (MPa) Interface bonding strength 15 19.5 Bond strength increase percentage - 30%

[0132] Table 3. Stress concentration comparison table

[0133] Test items Traditional crafts Method of the present invention Interface stress concentration (%) 100 75 Stress concentration reduction percentage - 25%

[0134] Table 4. Microstructure stability test table

[0135]

[0136] It can be seen. After applying the present invention, the tensile strength of the engine hood produced by the method of the present invention at the bonding interface is increased from 15Mpa of the traditional process to 195MPa, an increase of about 30%. Through stress test analysis, it was found that the stress concentration of the product at the bonding interface was reduced by 25%, significantly improving the impact resistance of the product. In addition, in the durability test under high temperature and high pressure environment, the product showed better structural stability, and its deformation rate was maintained at 98%, while the deformation rate of the product produced by the traditional process under the same conditions was only 85%.

[0137] Through the in-mold dual-hardness product molding method of the present invention, engineers not only greatly improved production efficiency, shortened production time from 60 minutes in the traditional process to 40 minutes, but also significantly improved the bonding strength, structural stability and durability of the engine hood. The comprehensive performance test results combining mechanics and microstructure show that this method effectively solves the technical bottleneck existing in the traditional multiple injection molding process, especially showing great potential in the manufacture of high-strength and high-performance products, and provides a more efficient and reliable technical solution for the automotive manufacturing field.

[0138] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. In-mold dual-hardness product forming method, characterized in that: The steps include: S1. Provide a set of molds, the molds comprising a first mold cavity and a second mold cavity, the first mold cavity and the second mold cavity are respectively used to mold a first material and a second material of different hardness, and a programmable temperature control system, a flow channel control system and a topological stress field adjustment system are provided inside the molds; S2, injecting a first hardness material into a first mold cavity, controlling the flow rate during the injection process by a generalized fluid dynamics equation of a non-Abelian gauge field, and controlling the temperature distribution in the mold cavity by a multi-body system equation combining a quantum coherent state with non-equilibrium statistical mechanics, while partially solidifying the first hardness material in a predetermined area, and retaining an incompletely solidified interface layer on the surface; S3, transferring the partially solidified first hardness material in the first mold cavity to a designated position of the second mold cavity through a flow channel control system, aligning the first hardness material through a high-order nonlinear Lie group analysis method, and controlling the thickness of the interface layer through the supersymmetric string theory of duality between anti-de Sitter space and conformal field theory; S4. Injecting a second hardness material into the second mold cavity, combining the first hardness material with the second hardness material, using a high-order spin-orbit coupling model to regulate the bonding strength of the interface layer, controlling the generated field intensity through supersymmetric gauge field theory, optimizing the electromagnetic field distribution of the bonding interface, and enhancing the physical strength and stability of the material bonding; S5. The temperature field in the mold is adjusted by a synchronous thermodynamic control system so that the first hardness material and the second hardness material are solidified synchronously within a predetermined time. The stress field distribution in the mold cavity is controlled by a high-dimensional topology optimization method to prevent the material from deforming due to stress concentration. The first hardness material and the second hardness material are solidified in the mold at the same time. The microstructure formed by the material during the synchronous solidification process is regulated by a nonlinear dynamic model under the background of a time crystal to optimize product stability. S6. Cool the mold and take out the formed dual-hardness product. The dual-hardness product has a smooth transition between different hardness areas, which optimizes the structural stability.

2. The in-mold dual-hardness product forming method according to claim 1, characterized in that: The S2 specifically includes: S21, injecting the first hardness material into the first mold cavity, and controlling the flow rate Q1(t) during the injection process by the generalized fluid dynamics equation of the non-Abelian gauge field: Among them, F μν is the intensity tensor of the non-Abelian gauge field, ★ represents the Hodge duality, is a canonical manifold, is the path integral measure, Tr represents the trace operation; S22. Use the multi-body system equation combining quantum coherent state and non-equilibrium statistical mechanics to control the temperature distribution in the mold cavity, temperature field T(x,y,z,t): Among them, |Ψ(t)> quantum coherent state, is the operator representation of the temperature field, the evolution of which is subject to the time development of the many-body wave function Ψ(t); S23. By controlling the temperature field T(x, y, z, t), the first hardness material is partially solidified in a predetermined area. The material hardness H1(t) during the partial solidification process is described by the high-dimensional topological soliton field equation: Among them, d int (t) is the Levi-Civita symbol, φ is the scalar field of the material, the integral is performed over the space Σ of the topological solitons, and ijk is the Levi-Civita symbol used to represent a completely antisymmetric tensor in three-dimensional space; S24. Controlling the thickness of the interface layer d using supersymmetric Calabi-Yau geometry flow int (t), the first hardness material surface retains an incompletely solidified interface layer, the thickness of the interface layer is d int The variation of (t) is described by the following supersymmetric Calabi-Yau geometry flow equation: in, is a Calabi-Yau manifold, Ω is the global complex volume form on the Calabi-Yau manifold, is its complex conjugate, and K is the Kähler potential.

3. The in-mold dual-hardness product forming method according to claim 1, characterized in that: The S3 specifically includes: S31. Multi-body entangled interaction energy in non-equilibrium quantum thermodynamics V ent (t) Controlling the transfer of partially solidified first hardness material from the first cavity to a designated position of the second cavity. During the transfer process, dynamically calculating the entanglement interaction energy V according to the material's wave function Ψ(t) and temperature T ent (t), optimize the stability of the material to maintain its quantum entangled state during the transfer process: in, represents the quantum entanglement Hamiltonian of the material, Ψ(t) is the quantum state wave function of the material, and T(t) is the temperature; S32. During the material transfer process, the quantum entangled state and interaction energy calculated in S31 are used as initial input, and the nonlinear evolution equation combining the interaction between the quantum liquid crystal state and the time crystal is adopted to further optimize the quantum state and phase evolution of the material: in, and They describe the Hamiltonian of the quantum liquid crystal state and the time crystal respectively, |Ψ(t)> the quantum liquid crystal state of the material, ∈ is the coupling strength of the flow control system, is the quantum dissipative operator; S33, in the second mold cavity, using the quantum liquid crystal state obtained in S32 as the initial state, aligning the first hardness material by high-order nonlinear Lie group analysis method, and the geometric state during the alignment process Among them, ξ i is the Lie group parameter derived from the quantum state evolution in the previous step, is the Lie group generator, is the initial geometric state; S34. After the alignment is completed, the flow control system uses the supersymmetric string theory of anti-de Sitter space and conformal field theory, and uses the geometric state and quantum state obtained in S33 as input to control the thickness of the interface layer and optimize the height and stability of the material combination. The thickness of the interface layer d AdS / CFT (t): in, is an anti-de Sitter space, The geometric state parameters of the previous step OK, S. CFT [φ] The action of conformal field theory, which represents the dynamic behavior of the flow control system under the field variable φ, d AdS / CFT The interface layer thickness represents the thickness of the material at the interface layer, which changes with time t, and φ defines the field variable.

4. The in-mold dual-hardness product forming method according to claim 1, characterized in that: The S4 specifically includes: S41, injecting a second hardness material into the second mold cavity, and controlling the coupling state of quantum mechanics to make the second hardness material contact and combine with the uncured interface layer of the first hardness material, and the interaction potential energy V during the combination process couple (t): in, is the joint Lagrangian function describing the wave function Ψ1(t) of the first hardness material and the wave function Ψ2(t) of the second hardness material, Σ is the spatial area of ​​the bonding interface, To reduce Planck's constant, Ψ1 and Ψ2 are the quantum state wave functions of the first hardness material and the second hardness material; S42. During the material bonding process, the temperature distribution T(x,y,z,t) in the mold cavity is dynamically adjusted through the topological thermodynamic model: Among them, κ is the thermal conductivity of the material, α is the thermal coupling coefficient related to the internal topological structure of the material, Adjust the temperature field during the bonding process in real time; S43, during the binding process, a high-order spin-orbit coupling model is used to regulate the binding strength of the interface layer. The binding strength σ int (t): Where γ is the coupling constant, Ψ int (t) is the quantum state wave function at the binding interface, and are the spin and orbital angular momentum operators, respectively, and λ is the attenuation coefficient related to the temperature T(t); S44. In the final binding stage, the field strength generated during the binding process is controlled by supersymmetric gauge field theory. The evolution of field strength optimizes the physical strength and stability of material bonding by controlling the evolution of the gauge field and combining the electromagnetic field distribution at the interface: in, is the covariant derivative, is the gauge field tensor, is the source current, is the action functional of the gauge field.

5. The in-mold dual-hardness product forming method according to claim 1, characterized in that: The S5 specifically includes: S51, adjusting the temperature field in the mold through a synchronous thermodynamic control system, so that the first hardness material and the second hardness material are synchronously cured within a predetermined time, and the first hardness material and the second hardness material are optimized to maintain temperature consistency during the curing process; S52. During the simultaneous solidification process, the stress field distribution in the mold cavity is controlled by using a high-dimensional topology optimization method to optimize the material so that it will not deform due to stress concentration during the solidification process; S53. By using self-consistent field theory, the spin state inside the material is adjusted to optimize the uniform distribution of the spin state inside the material during the curing process; S54. Use the nonlinear dynamic model in the context of time crystals to regulate the microstructure of the material formed during the synchronous solidification process and optimize the product to have consistency and high stability.