On-chip characterization method of electron beam spots

By manufacturing a beam spot characterization chip in an electron beam lithography machine, using electron beams to write patterns in the suspended thin film test area and fit it, the problem of difficulty in characterizing nanoscale electron beam spots in the existing technology is solved, and high resolution is achieved and compatibility of electron beam spot characterization.

CN119024639APending Publication Date: 2024-11-26PEKING UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411005471.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing electron beam spot detection methods are difficult to effectively characterize the size and dose distribution of nanoscale electron beam spots, especially in the high precision and small size ranges, and are incompatible with the electron beam lithography process environment.

Method used

Using an on-chip characterization method of electron beam spots, a beam characterization chip is used to create a beam spot characterization chip, and the test layout pattern is written in the suspended thin film test area, controlling the dwell time and exposure overlap, and establishing a function of photoresist sensitivity and exposure overlap. Relationship, using MATLAB for nonlinear least squares fitting, obtain parameters of the Gaussian function of the beam spot, thereby characterizing the size and dose distribution of the electron beam spot.

Benefits of technology

High resolution characterization of nanoscale electron beam spots is achieved, and edge sputtering is avoided. It is suitable for electron beam spots of 30~100keV, with good compatibility and reusability, and can characterize the size and dose distribution of beam spots at the same time. information.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119024639A_ABST
    Figure CN119024639A_ABST
Patent Text Reader

Abstract

The invention discloses an on-chip characterization method for electron beam spots, and belongs to the technical field of micro-nano machining. The method comprises the following steps: manufacturing a beam spot characterization chip, writing an electron beam into a test layout pattern on a suspended film test area of the chip at different exposure doses, and obtaining multiple groups of exposure overlapping data; establishing a function relationship among the residence time, the exposure overlap and the photoresist sensitivity, and performing nonlinear least square fitting to obtain parameters of a beam spot Gaussian function; and substituting the obtained parameters into an electron beam spot Gaussian function to obtain the size and dose distribution of the electron beam spot. The method is simple to operate, good in compatibility with an electron beam lithography process environment and high in accuracy.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of micro-nano processing, and in particular relates to an on-chip characterization method of a nanometer-scale electron beam spot of an electron beam lithography machine. Background Art

[0002] With the continuous development of science and technology and society, human demand for computing power, data storage and transmission speed continues to grow. Driven by both demand and profit, semiconductor manufacturing processes have advanced to technology nodes below 5nm. Lithography is the core of micro-nano processing technology, and the generation and transfer of nanoscale graphics are the key to achieving the production of advanced technology node devices. Traditional lithography technology, especially deep ultraviolet lithography (DUV) and extreme ultraviolet lithography (EUV), has approached its physical limit in terms of resolution. Specifically, EUV lithography uses a wavelength of 13.5 nanometers. Although it significantly improves the resolution, it still faces many challenges in the manufacture of sub-10 nanometer structures, including mask defect control, photoresist material performance and graphic fidelity. In this context, electron beam lithography (EBL) as a key nanomanufacturing technology has become increasingly important. Due to the extremely short wavelength of high-energy electron beams, electron beam lithography has extremely high resolution potential. At present, single-beam electron beam lithography technology is widely used in the field of basic scientific research, and multi-beam parallel writing electron beam technology has great potential for industrial applications in fields such as mask manufacturing. At the same time, electron beam lithography does not require the use of masks, which is conducive to quickly adjusting and optimizing graphics to improve the iterative efficiency of small-size device research and development, and can be used as a solution for advanced node process mask manufacturing. The electron beam lithography machine generates a nanometer-scale electron beam spot through an electron optical system. The beam spot moves on the surface of the target substrate to write the pattern under the coordination of electromagnetic deflection and high-precision mechanical systems. The detection of the size and dose distribution of the electron beam spot plays a positive role in the evaluation of the process capability of the electron beam lithography equipment, the correction of proximity effects, and the improvement of resolution.

[0003] Existing electron beam spot detection methods have failed to keep up with the rapid development of the resolution of electron beam lithography equipment, and there is a lack of methods that can effectively characterize the size and dose distribution of nanoscale electron beam spots. At present, the most commonly used method for characterizing small-sized electron beam spots is the knife edge method (KE). The knife edge method determines the beam spot size by allowing the electron beam to scan through a sharp edge and using tools such as a Faraday cup to collect the changes in the signal during the scanning process. However, the resolution of the knife edge method is limited by the root mean square size of the knife edge used, and for nanoscale beam spots, it is difficult to produce a knife edge that is sharp at the atomic level, so that the influence of edge sputtering on the test results cannot be eliminated. In addition, the knife edge method is difficult to characterize the dose distribution of the beam spot and is incompatible with the electron beam lithography process environment. In addition, the fluorescence detector, Compton detector, laser interferometer detector, etc. used for beam spot characterization in large accelerators cannot effectively characterize electron beam spots with an acceleration voltage of 30 to 100 kV and a size of less than 100 nm. It can be seen that traditional beam spot detection methods are difficult to characterize the size and dose distribution of nanoscale electron beam spots in electron beam lithography. Summary of the invention

[0004] The purpose of the present invention is to provide an on-chip characterization method for an electron beam spot of an electron beam lithography machine, which can characterize the size and dose distribution of a nanoscale electron beam spot.

[0005] The technical solution adopted by the present invention to achieve the above-mentioned purpose is as follows:

[0006] An on-chip characterization method for electron beam spot comprises the following steps:

[0007] Manufacturing a beam spot characterization chip, the beam spot characterization chip includes a plurality of arranged square test units, each test unit includes a plurality of square suspended membrane test areas, each suspended membrane test area is composed of a flat square membrane located on a back cavity structure, the thickness of the membrane is in the order of nanometers, and the side length is in the order of millimeters;

[0008] Using an electron beam to write a test layout pattern on the suspended membrane test area, the test layout pattern is a group of staggered rectangular patterns with connected vertices, the width of the rectangle is in the order of nanometers, and the length is in the order of micrometers; controlling different dwell times of the electron beam to develop the written test layout pattern, and obtaining multiple sets of exposure overlapping data;

[0009] The functional relationship among dwell time, exposure overlap and photoresist sensitivity is established. The nonlinear least squares method is used to fit the functional relationship to obtain the parameters of the beam spot Gaussian function. The obtained parameters are substituted into the electron beam spot Gaussian function to obtain the size and dose distribution of the electron beam spot.

[0010] Furthermore, exposure marks are provided on the four corners of each test unit.

[0011] Furthermore, the functional relationship between the dwell time, exposure overlap and photoresist sensitivity is the exposure overlap-beam spot function, and the expression of this function is:

[0012]

[0013] Where h(t) is the photoresist sensitivity, t is the dwell time, b is the exposure overlap, s is the width of the rectangle, erf is the error function, A is the intensity parameter of the beam spot Gaussian function, σ o is the variance parameter of the beam spot Gaussian function, A and σ o Fitting obtained.

[0014] Furthermore, the expression of the electron beam spot Gaussian function is:

[0015]

[0016] Where f(x) is the dose per unit time at a point x away from the center of the electron beam spot, A is the intensity parameter of the beam spot Gaussian function, σ o is the variance parameter of the beam spot Gaussian function, A, σ o Parameter fitting is obtained.

[0017] Furthermore, when A and σ o When fitting parameters, multiple algorithms including genetic algorithm, simulated annealing algorithm, particle swarm algorithm, ant colony algorithm, quasi-Newton method and Gauss-Newton method are used for fitting optimization, and the correlation coefficient of each optimization result is calculated respectively, and the result with the correlation coefficient closest to 1 is taken as the final fitting result.

[0018] Furthermore, when A and σ o When fitting parameters, the following fitting algorithm is also used:

[0020] m=k+s

[0021]

[0022] Wherein, s is the exposure step length, k and m are the exposure overlap lengths at two different doses at dwell times t1 and t2, h(t) is the photoresist sensitivity, and f(k) is the dose per unit dwell time of the electron beam spot at position x=k;

[0023] Based on several sets of f(k) values ​​and corresponding k values, the parameters A and σ of the electron beam Gaussian function are obtained by fitting. o And the original function f(x).

[0024] Furthermore, the manufacturing steps of the beam spot characterization chip include:

[0025] Depositing nanometer-scale thin films on both sides of silicon wafers;

[0026] Forming a back cavity window pattern and an exposure mark pattern on the back of the silicon wafer by photolithography;

[0027] A window is etched from the back side until it penetrates through to the front film to form a back cavity structure.

[0028] Furthermore, the above-mentioned manufacturing steps of the beam spot characterization chip are applicable to thin film materials that do not react with the etching solution in the back cavity deep etching.

[0029] Furthermore, the manufacturing steps of the beam spot characterization chip include:

[0030] Depositing a silicon oxide stress buffer layer and a silicon nitride mask on both sides of the silicon wafer;

[0031] Photolithography forms a photolithography mark pattern on the front side of the silicon wafer, and etches silicon nitride, silicon oxide and silicon of a preset thickness in the pattern area;

[0032] The photolithography marks made on the front are aligned to form a back cavity window pattern on the back of the silicon wafer, and the silicon nitride and silicon oxide at the window are etched away;

[0033] Spin coating or depositing a corrosion protection layer on the front side of the silicon wafer;

[0034] Wet-etch the silicon wafer to remove the silicon at the window until there is a residual thickness of x microns from the film;

[0035] Remove the corrosion protection layer and deposit a thin film with a thickness of nanometer scale on the front side;

[0036] The back side is dry-etched to remove the remaining x microns of silicon until it penetrates the film, forming a back cavity structure and releasing the film.

[0037] Furthermore, the above-mentioned manufacturing steps of the beam spot characterization chip are applicable to thin film materials that react with etching liquid in the back cavity deep etching.

[0038] Furthermore, the corrosion protection layer uses B3 anti-corrosion agent.

[0039] The advantages of the present invention are as follows:

[0040] 1) The method of the present invention extracts data through on-chip detection means and has good compatibility with the electron beam lithography process environment.

[0041] 2) The method of the present invention is simple and easy to operate by implementing the same operation process as the electron beam lithography process, and the prepared beam spot characterization chip can be reused by debonding.

[0042] 3) The method of the present invention reduces the backscattering coefficient by 600 times by reducing the substrate thickness to a scale of hundreds of nanometers, thereby reducing the impact of energy deposition caused by backscattered electrons returning to the photoresist on the test. It has extremely high resolution and can be used to characterize the 30-100 keV nanoscale beam spot generated by an electron beam lithography machine.

[0043] 4) The method of the present invention uses an electron beam writing method in the suspended film test area, so that the test dose can be increased from 3C / m 2 Select up to 500C / m 2 The range of data obtained is wider than that of conventional substrates, which is conducive to the accurate characterization of the electron beam spot.

[0044] 5) The method of the present invention can simultaneously characterize the beam spot size information and the dose distribution information through an effective mathematical algorithm.

[0045] 6) Compared with the widely used edge method, the method of the present invention improves the accuracy of beam spot measurement by avoiding the sputtering of electrons on sharp surfaces to a great extent. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] Figure 1 Schematic diagram of the structure of the test unit of the beam spot characterization chip in Example 1.

[0047] Figure 2 This is a side cross-sectional view of the suspended membrane test area in Example 1.

[0048] Figure 3 This is a schematic diagram of writing multiple groups of test layout patterns into the suspended membrane test area in Example 1.

[0049] Figure 4 This is a schematic diagram of the test layout pattern in Example 1.

[0050] Figure 5 Schematic diagram of exposure overlap generated by test layout pattern development in Example 1.

[0051] Figure 6 This is a manufacturing flow chart of a beam spot characterization chip in Example 2.

[0052] Figure 7 This is a manufacturing flow chart of a beam spot characterization chip in Example 3.

[0053] Figure 8 This is a manufacturing flow chart of a beam spot characterization chip in Example 4. DETAILED DESCRIPTION

[0054] In order to make the various technical features and advantages or technical effects in the above technical solutions of the present invention more obvious and easy to understand, they are described in detail below with reference to the accompanying drawings.

[0055] Example 1

[0056] This embodiment discloses an on-chip characterization method for an electron beam spot. The method mainly performs electron beam spot characterization measurement on a test unit on a beam spot characterization chip. The steps of the method are described in detail below.

[0057] First, the beam spot characterization chip is manufactured, and its main structure is as follows: Figure 1 As shown. A plurality of square test units are arranged on the entire silicon wafer. In this embodiment, the side length of each test unit is 8.15 mm. In each test unit, a plurality of suspended membrane test areas are distributed according to the process capability and test requirements. The structure of the suspended membrane test area is shown as follows: Figure 2 As shown, it is composed of a thin film located on the back cavity structure. Figure 2 Four different back cavity structures are shown in Figure 1. To minimize the effect of forward scattering and back scattering on development in the substrate, the thickness of the film should be below 200 nm. To ensure that the test results are not affected by different thicknesses in different regions and to facilitate spin coating of electron beam photoresist with nanometer-level thickness, the film should be flat and uniform. To facilitate the writing of electron beam lithography patterns, exposure marks can be added to each test unit.

[0058] Then, an electron beam is used to write multiple sets of test layout patterns in the suspended membrane test area. The test pattern layout is distributed in a matrix form on each suspended membrane test area, such as Figure 3 As shown. The test layout is a set of staggered rectangular shapes with connected vertices. Figure 4 Figure 2 shows two staggered rectangular patterns in horizontal and vertical directions. In this example, the rectangle is 2 microns long and 100 nanometers wide. In order to characterize the beam spot in both the x-direction and the y-direction, the test pattern has two distribution modes along the x-direction and along the y-direction, such as Figure 3 and Figure 4 As shown. Further, according to the test requirements, the test pattern can also be arranged along any angle to calculate the size information and dose distribution of the electron beam spot in any direction. Figure 1 Under the test unit distribution, the writing dose of the test unit is 1C / m 2 , and then each subsequent test unit will increase by 1C / m 2 .

[0059] Since the initial distribution of the electron beam is a two-dimensional Gaussian distribution, after writing the test layout pattern, the pattern will be widened, such as Figure 5 As shown. In the direction of the width of the layout pattern, exposure overlap will occur. This exposure overlap is related to the write dose, that is, the dwell time, and is therefore recorded as exposure overlap b. After the entire wafer is written with the test layout pattern according to the above method, it is developed and observed under a scanning electron microscope, and the exposure overlap b of the unit under different doses is recorded.

[0060] Finally, the mathematical model of the exposure overlap-beam spot function is constructed, and the obtained g(t) and the corresponding t value are brought into the exposure overlap-beam spot function, that is:

[0061]

[0062] Wherein, h(t) is the photoresist sensitivity, d is the rectangular width of the test pattern, which is 100 nanometers in this embodiment, erf is the error function, A is the intensity parameter of the beam spot Gaussian function, σ o is the variance parameter of the beam spot Gaussian function.

[0063] According to the obtained g(t) data, the above function is fitted using the nonlinear least squares method in MATLAB. Furthermore, the fitting can be optimized using genetic algorithms, simulated annealing algorithms, particle swarm algorithms, ant colony algorithms, quasi-Newton methods, Gauss-Newton methods, etc., and the correlation coefficient of each optimization result is calculated respectively. The result with the correlation coefficient closest to 1 is taken as the result of this calculation and fitting, and the intensity parameter A of the beam spot Gaussian function and the variance σ of the beam spot Gaussian function are obtained. o Then, these two parameters are brought into the electron beam spot Gaussian function to obtain the size information and dose distribution of the electron beam spot. The expression of this function is:

[0064]

[0065] Furthermore, the fitting results of the test pattern patterns distributed at multiple angles may be combined to obtain the two-dimensional Gaussian distribution fitting result of the electron beam spot.

[0066] Furthermore, when performing parameter fitting, the following less complex fitting algorithm may also be used:

[0067] From a discrete perspective, at the edge of exposure overlap, the cumulative value of dose can be expressed as:

[0068] h(t)=t1(f(m)+f(m+s)+f(m+2s)+...+f(m+ns))

[0069] h(t)=t2(f(k)+f(k+s)+f(k+2s)+...+f(k+ns))

[0070] Where s is the exposure step length, k and m are the exposure overlaps measured at two different doses, and m = k + s. Since the width of the designed layout pattern is much larger than the diameter of the electron beam spot, f(m + ns) can be considered infinitesimal and can be ignored. The above two equations can be combined to obtain:

[0071]

[0072] Wherein, h(t) is the sensitivity of the photoresist, t1 and t2 are the dwelling times at two different doses, and f(k) is the dose per unit dwelling time of the electron beam spot at position x=k.

[0073] Thus, several groups of f(k) values ​​and corresponding k values ​​are found in the collected data, and then the original function f(k) of the electron beam Gaussian function can be obtained by fitting.

[0074] The beam spot characterization chip can be manufactured by a variety of methods. The following three embodiments disclose three methods for manufacturing the beam spot characterization chip.

[0075] Example 2

[0076] This embodiment discloses a method for manufacturing a beam spot characterization chip, which is suitable for thin film materials that are not corroded in wet etching, such as silicon nitride. Figure 6 The manufacturing process is shown in the manufacturing flow chart, and the specific manufacturing steps are as follows:

[0077] (1) Double-polished silicon wafer LPCVD deposits 100 nm of low-stress silicon nitride film on both sides, see Figure 6 Figure (a) in .

[0078] (2) Photolithography is used to generate a back cavity window pattern and an exposure mark pattern on the back of the wafer, and dry etching is used to remove the silicon nitride material at the window. Figure 6 Figure (b) in .

[0079] (3) Perform KOH deep etching until the etching penetrates the upper silicon nitride film. Figure 6 Figure (c) in .

[0080] Example 3

[0081] This embodiment discloses another method for manufacturing a beam spot characterization chip, which is suitable for thin film materials such as aluminum that are etched in wet etching. Figure 7 The manufacturing process is shown in the manufacturing flow chart, and the specific manufacturing steps are as follows:

[0082] (1) Double-polished silicon wafers are thermally oxidized to grow a 100nm thick silicon oxide stress buffer layer, and LPCVD double-sided 100nm silicon nitride mask, see Figure 7 Figure (a) in .

[0083] (2) Front lithography to form an exposure mark pattern. RIE etches silicon nitride and silicon oxide at the mark pattern, and ASE etches silicon 3 microns. Figure 7 Figure (b) in .

[0084] (3) Align the photolithography marks made on the front side, form a back cavity window pattern on the back side of the silicon wafer, and remove the silicon nitride and silicon oxide at the window by RIE. Figure 7 Figure (c) in .

[0085] (4) Spin-coat the primer adhesive and B3 resist on the front of the silicon wafer to protect the structure on the front of the silicon wafer from being corroded during wet etching. Figure 7 Figure (d) in .

[0086] (5) Perform KOH deep etching until the silicon residual thickness is 10 microns. Figure 7 Figure (e) in .

[0087] (6) Remove B3 resist and primer adhesive, see Figure 7 Figure (f) in .

[0088] (7) Use H3PO4 to remove silicon nitride and BHF to remove silicon oxide, see Figure 7 Figure (g) in .

[0089] (8) PVD deposited aluminum 100nm thick, see Figure 7 Figure (h) in .

[0090] (9) ASE is used on the back to remove the remaining 10 μm of silicon and release the suspended aluminum film. Figure 7 Figure (i) in .

[0091] Example 4

[0092] This embodiment also discloses a method for manufacturing a beam spot characterization chip, which is applicable to thin film materials such as aluminum that are etched in wet etching, and involves a low-stress silicon nitride film with high selectivity in wet etching, such as Figure 8 The manufacturing process is shown in the manufacturing flow chart, and the specific manufacturing steps are as follows:

[0093] (1) Photolithography is used to form an exposure mark pattern on the front side of the double-polished silicon wafer, and ASE is used to remove 3 microns of silicon. Figure 8 Figure (a) in .

[0094] (2) LPCVD double-sided deposition of 300nm thick low-stress silicon nitride, see Figure 8 Figure (b) in .

[0095] (3) Align the photolithography marks made on the front side and form the back cavity window pattern on the back side. Use RIE to remove the silicon nitride at the window. Figure 8 Figure (c) in .

[0096] (4) Perform KOH deep etching until the silicon thickness is 10 microns. Figure 8 Figure (d) in .

[0097] (5) Use H3PO4 to remove silicon nitride, see Figure 8 Figure (e) in .

[0098] (6) Using PVD to deposit 100nm thick aluminum, see Figure 8 Figure (f) in .

[0099] (7) ASE is used on the back to remove the remaining 10 μm of silicon and release the suspended aluminum film. Figure 8 Figure (g) in .

[0100] The above describes an application of the method of the present invention through an embodiment. Those skilled in the art should understand that, without departing from the essence of the present invention, the structure can be changed and modified to a certain extent, and its manufacturing method is not limited to the manufacturing process in this embodiment. The scope of protection of the present invention shall be based on the claims.

Claims

1. An on-chip characterization method for electron beam spot, characterized in that: The following steps are involved: Manufacturing a beam spot characterization chip, the beam spot characterization chip comprising a plurality of arranged square test units, each test unit comprising a plurality of square suspended membrane test areas, each suspended membrane test area being composed of a flat square membrane located on a back cavity structure; Using an electron beam to write a test layout pattern at different doses on a suspended membrane test area, the test layout pattern being a group of staggered rectangular patterns with connected vertices; controlling different dwell times of the electron beam to develop the written test layout pattern to obtain multiple sets of exposure overlapping data; The functional relationship among dwell time, exposure overlap and photoresist sensitivity is established, and the parameters of the beam spot Gaussian function are obtained by nonlinear least squares fitting. The obtained parameters are substituted into the electron beam spot Gaussian function to obtain the size and dose distribution of the electron beam spot.

2. The on-chip characterization method of electron beam spot according to claim 1, characterized in that: There are also exposure marks on the four corners of each test unit.

3. The on-chip characterization method of electron beam spot according to claim 1, characterized in that: The functional relationship between dwell time, exposure overlap and photoresist sensitivity is the exposure overlap-beam spot function, which is expressed as: Where h(t) is the photoresist sensitivity, t is the dwell time, b is the exposure overlap, d is the width of the rectangle, erf is the error function, A is the intensity parameter of the beam spot Gaussian function, σ o is the variance parameter of the beam spot Gaussian function, A and σ o Fitting obtained.

4. The on-chip characterization method of electron beam spot according to claim 1, characterized in that: The expression of the electron beam spot Gaussian function is: Where f(x) is the dose per unit time at a point x away from the center of the electron beam spot, A is the intensity parameter of the beam spot Gaussian function, σ o is the variance parameter of the beam spot Gaussian function, A, σ o Parameter fitting is obtained.

5. The on-chip characterization method of electron beam spot according to claim 4, characterized in that: In the A, σ o When fitting parameters, multiple algorithms including genetic algorithm, simulated annealing algorithm, particle swarm algorithm, ant colony algorithm, quasi-Newton method and Gauss-Newton method are used for fitting optimization respectively, and the correlation coefficient of each optimization result is calculated respectively, and the result with the correlation coefficient closest to 1 is taken as the final fitting result.

6. The on-chip characterization method of electron beam spot according to claim 5, characterized in that: In the A, σ o When fitting parameters, the following fitting algorithm is also used: m=k+s Wherein, s is the exposure step length, k and m are the exposure overlap lengths at two different doses at dwell times t1 and t2, h(t) is the photoresist sensitivity, and f(k) is the dose per unit dwell time of the electron beam spot at position x=k; Based on several sets of f(k) values ​​and corresponding k values, the original function f(x) of the electron beam Gaussian function is obtained by fitting.

7. The on-chip characterization method of electron beam spot according to claim 1, characterized in that: The manufacturing steps of the beam spot characterization chip include: Depositing nanometer-scale thin films on both sides of silicon wafers; Forming a back cavity window pattern and an exposure mark pattern on the back of the silicon wafer by photolithography; A window is etched from the back side until it penetrates through to the front film to form a back cavity structure.

8. The on-chip characterization method of electron beam spot according to claim 7, characterized in that: The above-mentioned manufacturing steps of the beam spot characterization chip are used for thin film materials that do not react with the etching solution in the back cavity deep etching.

9. The on-chip characterization method of electron beam spot according to claim 1, characterized in that: The manufacturing steps of the beam spot characterization chip include: Depositing a silicon oxide stress buffer layer and a silicon nitride mask on both sides of the silicon wafer; Photolithography forms a photolithography mark pattern on the front side of the silicon wafer, and etches silicon nitride, silicon oxide and silicon of a preset thickness in the pattern area; The photolithography marks made on the front are aligned to form a back cavity window pattern on the back of the silicon wafer, and the silicon nitride and silicon oxide at the window are etched away; Spin coating or depositing a corrosion protection layer on the front side of the silicon wafer; Wet-etch the silicon wafer to remove the silicon at the window until there is a residual thickness of x microns from the film; Remove the corrosion protection layer and deposit a thin film with a thickness of nanometer scale on the front side; The back side is dry-etched to remove the remaining x microns of silicon until it penetrates the film, forming a back cavity structure and releasing the film.

10. The on-chip characterization method of electron beam spot according to claim 9, characterized in that: The above-mentioned manufacturing steps of the beam spot characterization chip are used for the thin film material that reacts with the etching solution in the back cavity deep etching, and the corrosion protection layer uses B3 anti-corrosion agent.