Lead back-etching manufacturing method
Through the double-layer screen printing technology of the dot blocking and specific screen T number, the thickness of the photosensitive ink and selective exposure and development are controlled, and the problems of thermally cured ink and dry film in lead re-etching are solved, and the lead is realized The accuracy and completeness of re-erosion enhances practicality and promotional significance.
Patent Information
- Application Number
- CN202411220497.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-11-26
AI Technical Summary
In the prior art, thermally cured inks can easily lead to oil-resistance plating of the electroless pad during the screen printing process, and when using a press-dry film protection, it is impossible to completely fill the window due to small holes and poor fluidity, resulting in gas residue and dryness. The film expands and breaks, causing the lead to oxidation and inability to re-corrode, and the ink bonding force with the dry film is increased, resulting in difficulty in removing.
Double-layer screen printing is performed using dot blocking mesh and a specific number of wire mesh Ts to control the thickness of the photosensitive ink, and through selective exposure and development, avoiding the problems caused by ink plating and dry film, ensuring that the ink is removed cleanly after electroless plating.
It has achieved the avoidance of impurity of plating and film removal caused by thermally cured inks and dry films, ensured the accuracy and completeness of lead re-etching, and improved the practicality and promotional significance of lead re-etching.
Smart Images

Figure CN119031603A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of circuit boards, and in particular to a method for manufacturing lead etch-back. Background Art
[0002] The current selective electroplating solder mask window etching lead production process is: ... circuit transfer--solder mask--lead protection--electroplating--D / F--electroplating--film stripping. Before the solder mask window is completed with chemical plating, there are generally two ways to make electroplated lead protection: one is to screen print thermosetting ink at the solder mask window position, and the other is to press dry film protection at the solder mask window position. Both methods have the following defects that cannot be solved. One is that the thermosetting ink will "bounce" during the screen printing process, resulting in oil resist plating on the pad that needs chemical plating; the second is to use the method of pressing dry film. Since the solder mask window hole is relatively small, the dry film has poor fluidity and cannot completely fill the window, and there is gas residue. After being heated during the chemical plating process, the dry film expands, cracks, and falls off, resulting in gold on the lead, and the lead is severely oxidized and cannot be etched back; and the bonding strength between the dry film and the ink is enhanced, resulting in the problem that the dry film on the ink cannot be removed. Summary of the invention
[0003] Based on this, it is necessary to provide a method for manufacturing lead etch-back in view of the shortcomings in the prior art.
[0004] A method for manufacturing a lead etch-back includes the following steps:
[0005] Step 1: Processing the inner and outer layers of the printed circuit board;
[0006] Step 2: Opening windows for ink: After the surface of the printed circuit board is covered with solder resist ink, solder resist exposure is performed to expose the pads that need chemical plating and the leads that need to be etched back through the opening windows;
[0007] Step 3, printing photosensitive selective plating ink; on the window that needs to be etched back, use the dot screen to print the photosensitive selective plating oil layer for the first time, then pre-bake, and then use the dot screen to print the photosensitive selective plating oil layer for the second time; wherein, the first screen printing is 51T screen when printing photosensitive selective plating ink, first screen print one side of the ink, pre-bake at 73±2℃ for 10min, the second screen printing ink, pre-bake at 73±2℃ for 15min, the third screen printing ink, pre-bake at 73±2℃ for 10min, the fourth screen printing ink, pre-bake at 73±5℃ for 30min, so as to control the oil thickness between 18-30um;
[0008] Step 4: Expose and develop the printed photosensitive material by oil coating;
[0009] Step 5: After the chemical plating is completed, the photosensitive plating oil is removed with chemical solution and the lead is etched back.
[0010] Furthermore, in this embodiment, the printed circuit board includes a PP layer, a core material layer, and a copper clad layer on each layer after inner and outer layer processing is completed.
[0011] Furthermore, when exposing the selected plated ink, the exposure scale is controlled at level 5-7.
[0012] Furthermore, in step one, a copper clad laminate is opened, and a high-density arbitrary interconnection process of the inner layer of the printed circuit board is completed by using a layer-building process on the copper clad laminate, and the outer layer of the printed circuit board is processed until the inner and outer layer graphics are completed.
[0013] In summary, the present invention uses a dot grid and a specific screen T number to perform double-layer screen printing to accurately control the thickness of the photosensitive ink, which not only avoids the ink resistance plating problem of thermosetting oil, but also eliminates the problems of unclean gold etching on the leads and unclean film stripping on the solder mask ink caused by the use of dry film. In addition, the selective exposure method can not only avoid the ink resistance plating of the pads that require chemical plating, but also improve the phenomenon of unclean gold on the leads and film stripping caused by the use of dry film. The present invention is highly practical and has a strong promotional significance. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 The present invention is a schematic flow chart of a method for manufacturing a lead etch-back process. DETAILED DESCRIPTION
[0015] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0016] like Figure 1 As shown, the present invention provides a method for making lead etch-back, which is to improve the problem of chemical plating ink resistance plating and the inability to etch gold on the lead.
[0017] The method for manufacturing a lead etch-back method specifically comprises the following steps:
[0018] Step 1: Open a copper clad board, use the layer-adding processing method to complete the high-density arbitrary interconnection processing of the inner layer of the printed circuit board, and perform outer layer processing on the printed circuit board until the inner and outer layer patterns are completed. In this embodiment, the printed circuit board includes a PP layer 11 and a core material layer 12 stacked in sequence from top to bottom, and a copper clad 13 on each layer after the inner and outer layer processing is completed;
[0019] Step 2: After the inner and outer layer patterns are completed, the surface of the printed circuit board is covered with solder resist ink 20 and then solder resist exposure is performed to expose the pads that need chemical plating and the leads that need to be etched back through the opening window 30, laying the foundation for the implementation of subsequent processes;
[0020] Step 3: On the window that needs to be etched back, use the dot screen to print the photosensitive selective plating oil layer 40 on both sides for the first time. After pre-baking, use the dot screen to print the photosensitive selective plating oil layer on both sides again;
[0021] The first screen printing is mainly to fill the ink opening of the window to a certain extent. In order to ensure that the photosensitive ink is not attacked by the solution and falls off during chemical plating, and the gold coating and de-sensitization of the photosensitive ink are smooth, you need to choose 51T mesh when selecting the photosensitive plating ink for screen printing. First, screen print the first ink on one side, pre-bake at 73±2℃ for 10min, screen print the second ink, pre-bake at 73±2℃ for 15min, screen print the third ink, pre-bake at 73±2℃ for 10min, and screen print the fourth ink, pre-bake at 73±5℃ for 30min, so that the oil thickness is controlled between 18-30um.
[0022] Step 4: Expose and develop the printed photosensitive selective plating oil; when exposing the selective plating ink, it is necessary to control the exposure scale at 5-7 levels. If it is greater than 7, there is a risk of incomplete oil removal, and if it is less than 5, there is a risk of ink falling off; thereby completing the removal of ink after chemical plating.
[0023] Step 5: After the chemical plating is completed, the photosensitive plating oil is removed with chemical solution and the lead is etched back.
[0024] In summary, the present invention uses a dot grid and a specific screen T number to perform double-layer screen printing to accurately control the thickness of the photosensitive ink, which not only avoids the ink resistance plating problem of thermosetting oil, but also eliminates the problems of unclean gold etching on the leads and unclean film stripping on the solder mask ink caused by the use of dry film. In addition, the selective exposure method can not only avoid the ink resistance plating of the pads that require chemical plating, but also improve the phenomenon of unclean gold on the leads and film stripping caused by the use of dry film. The present invention is highly practical and has a strong promotional significance.
[0025] The above-mentioned embodiment only expresses one implementation mode of the present invention, and its description is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.
Claims
1. A method for making lead etch-back, It is characterized in that The steps include: Step 1: Processing the inner and outer layers of the printed circuit board; Step 2: Opening windows for ink: After the surface of the printed circuit board is covered with solder resist ink, solder resist exposure is performed to expose the pads that need chemical plating and the leads that need to be etched back through the opening windows; Step 3, printing photosensitive selective plating ink; on the window that needs to be etched back, use the dot screen to print the photosensitive selective plating oil layer for the first time, then pre-bake, and then use the dot screen to print the photosensitive selective plating oil layer for the second time; wherein, the first screen printing is 51T screen when printing photosensitive selective plating ink, first screen print one side of the ink, pre-bake at 73±2℃ for 10min, the second screen printing ink, pre-bake at 73±2℃ for 15min, the third screen printing ink, pre-bake at 73±2℃ for 10min, the fourth screen printing ink, pre-bake at 73±5℃ for 30min, so as to control the oil thickness between 18-30um; Step 4: Expose and develop the printed photosensitive material by oil coating; Step 5: After the chemical plating is completed, the photosensitive plating oil is removed with chemical solution and the lead is etched back.
2. A method for manufacturing a lead etch-back as claimed in claim 1, Features: The printed circuit board comprises a PP layer and a core material layer stacked in sequence from top to bottom, and copper cladding arranged on each layer after inner and outer layer processing is completed.
3. A method for manufacturing a lead etch-back as claimed in claim 1, Features: When exposing the selected plating ink, control the exposure scale at level 5-7.
4. A method for manufacturing a lead etch-back as claimed in claim 1, Features: In step one, a copper clad laminate is opened, and a high-density arbitrary interconnection process of the inner layer of the printed circuit board is completed by using a build-up layer processing method, and the outer layer of the printed circuit board is processed until the inner and outer layer graphics are completed.